A method and system for determining the effective diffusion coefficient of a porous electrode.

By constructing a porous rotating disk electrode model using the finite element method and combining it with the velocity field and diffusion equation, the problem of difficulty in determining the mass transfer capacity of porous electrodes was solved, enabling more accurate determination of the diffusion coefficient and improvement of catalytic effect.

CN114021216BActive Publication Date: 2024-11-29SHANGHAI UNIV
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202111356136.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-11-16
Publication Date
2024-11-29
Estimated Expiration
2041-11-16

AI Technical Summary

Technical Problem

Existing technologies make it difficult to accurately determine the mass transfer capacity of porous electrodes, resulting in even electrode materials with strong catalytic activity failing to achieve good catalytic effects.

Method used

Using the finite element method, a geometric model of a porous rotating disk electrode is constructed. By combining the velocity field simulation solution and the convection-diffusion equation, the effective diffusion coefficient of the porous electrode is determined, and its mass transfer capacity is evaluated.

Benefits of technology

This improves the accuracy of calculating the effective diffusion coefficient of the porous electrode, enabling more accurate measurement of mass transfer capacity, avoiding reliance on empirical formulas, and enhancing the catalytic effect of the porous electrode.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114021216B_ABST
    Figure CN114021216B_ABST
Patent Text Reader

Abstract

The present invention discloses a method and system for determining the effective diffusion coefficient of a pore electrode, the method comprising: calculating the velocity field simulation solution corresponding to the pore rotating disk electrode geometric model at different speeds; the pore rotating disk electrode geometric model is constructed based on the rotating disk electrode electrochemical experiment, and the diffusion coefficient of the reactant in the reactant solution and the diffusion coefficient of the reactant in the boundary layer are input during operation; according to the velocity field simulation solution, the convection-diffusion equation is solved using finite element calculation software to determine the simulated current curve at different speeds; according to the simulated current curve at different speeds and the experimental current curve, the diffusion coefficient of the reactant in the reactant solution and the diffusion coefficient of the reactant in the boundary layer are adjusted; finally, according to the adjusted diffusion coefficient of the reactant in the boundary layer, the effective diffusion coefficient of the pore electrode is determined. The present invention can accurately determine the effective diffusion coefficient of the pore electrode, and then measure the mass transfer capacity of the pore electrode.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of electrode mass transfer capacity determination, and in particular to a method and system for determining an effective diffusion coefficient of a pore electrode. Background Art

[0002] Compared with flat electrodes, porous electrodes can provide a larger specific surface area, thereby increasing the reaction rate and improving the electron transfer capacity. However, the surface structure and catalytic performance of different porous electrodes are different. The catalytic ability of the porous electrode is determined by the electrode surface structure and catalytic performance. If the mass transfer capacity of a porous electrode is poor, even if the electrode material itself has strong catalytic activity, it will not ultimately achieve a good catalytic effect. Therefore, it is particularly important to judge the mass transfer capacity of the porous electrode (if the catalytic activity is low due to the structure of the material itself, there is no need to look for new materials, only the geometric structure of the existing material needs to be changed, saving a lot of manpower and material resources), but how to judge the mass transfer capacity of the porous electrode is a difficult problem. Summary of the invention

[0003] The purpose of the present invention is to provide a method and system for determining the effective diffusion coefficient of a pore electrode, which can accurately determine the effective diffusion coefficient of the pore electrode and further measure the mass transfer capacity of the pore electrode.

[0004] To achieve the above object, the present invention provides the following solutions:

[0005] A method for determining an effective diffusion coefficient of a pore electrode, comprising:

[0006] Calculate the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different rotation speeds; the porous rotating disk electrode geometric model includes the porous rotating disk electrode geometric structure and related parameters; the porous rotating disk electrode geometric structure includes a beaker, a reactant solution arranged inside the beaker, a porous rotating disk electrode arranged inside the beaker, and a boundary layer arranged above the porous rotating disk electrode; wherein, below the porous rotating disk electrode is an adsorption layer, below the adsorption layer is an adsorption process, and above the adsorption layer is an electrochemical reaction process; the related parameters include the diffusion coefficient of the reactant in the reactant solution and the diffusion coefficient of the reactant in the boundary layer;

[0007] According to the velocity field simulation solution, the convection-diffusion equation is solved using finite element calculation software to determine the simulated current curves at different rotation speeds;

[0008] Comparing the first difference with the first interval; the first difference is the difference between the spacing of the limiting diffusion current corresponding to the simulation current curve at different speeds and the spacing of the limiting diffusion current corresponding to the experimental current curve;

[0009] When the first difference is greater than the maximum value of the first interval, the diffusion coefficient of the reactant in the reactant solution is reduced, and the step of calculating the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different speeds is returned; when the first difference is less than the minimum value of the first interval, the diffusion coefficient of the reactant in the reactant solution is increased, and the step of calculating the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different speeds is returned; when the first difference is within the first interval, the second difference is compared with the second interval; the second difference is the difference between the value of the limiting diffusion current corresponding to the simulated current curve at different speeds and the value of the limiting diffusion current corresponding to the experimental current curve;

[0010] When the second difference is greater than the maximum value of the second interval, the diffusion coefficient of the reactant in the boundary layer is reduced, and the process returns to the velocity field simulation solution step corresponding to the porous rotating disk electrode geometric model at different speeds; when the second difference is less than the minimum value of the second interval, the diffusion coefficient of the reactant in the boundary layer is increased, and the process returns to the velocity field simulation solution step corresponding to the porous rotating disk electrode geometric model at different speeds; when the second difference is within the second interval, the effective diffusion coefficient of the porous electrode is determined based on the diffusion coefficient of the reactant in the boundary layer corresponding to the simulated current curve.

[0011] Optionally, the process of determining the experimental current curve is:

[0012] preparing the porous material into a porous rotating disk electrode;

[0013] A plurality of rotating disk electrode electrochemical experiments are carried out on the porous rotating disk electrode at different rotation speeds to obtain experimental current curves at different rotation speeds; wherein the rotation speed set when carrying out the rotating disk electrode electrochemical experiment is the same as the rotation speed when simulating the porous rotating disk electrode geometric model.

[0014] Optionally, the calculation of the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different rotation speeds specifically includes:

[0015] Based on the rotating disk electrode electrochemical experiment, a porous rotating disk electrode geometric structure is constructed;

[0016] Setting relevant parameters; the relevant parameters include: viscosity of reactant solution, concentration of reactant solution, diffusion coefficient of reactant in reactant solution, diffusion coefficient of reactant in boundary layer, reaction pre-exponential factor, transfer coefficient, adsorption rate, rotation speed of porous rotating disk electrode, Reynolds number and boundary conditions; the boundary conditions are that the surface of porous rotating disk electrode is set as a no-slip wall and the walls around beaker are set as solid walls;

[0017] determining a velocity field type according to the Reynolds number;

[0018] Based on the velocity field type and the porous rotating disk electrode geometric model, the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different rotation speeds is calculated.

[0019] Optionally, the Reynolds number calculation process is:

[0020] The Reynolds number is calculated according to the parameters set when performing the rotating disk electrode electrochemical experiment; wherein, when the Reynolds number is greater than a set threshold, the velocity field type is a turbulent model, and when the Reynolds number is less than or equal to the set threshold, the velocity field type is a laminar model.

[0021] Optionally, the method of solving the convection-diffusion equation using finite element calculation software according to the velocity field simulation solution to determine the simulated current curves at different speeds specifically includes:

[0022] According to the velocity field simulation solution, the convection-diffusion equation is solved by using finite element calculation software to determine the concentration gradient of the reactant on the surface of the porous rotating disk electrode and the concentration gradient of the product on the surface of the porous rotating disk electrode;

[0023] According to the concentration gradient of the reactant on the surface of the porous rotating disk electrode and the concentration gradient of the product on the surface of the porous rotating disk electrode, the Butler-Volmer model is used to calculate the instantaneous current generated on the surface of the porous rotating disk electrode at different times;

[0024] The instantaneous current at different times is integrated to obtain simulated current curves at different rotation speeds.

[0025] A system for determining an effective diffusion coefficient of a pore electrode, comprising:

[0026] A velocity field simulation solution calculation module is used to calculate the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different rotation speeds; the porous rotating disk electrode geometric model includes a porous rotating disk electrode geometric structure and related parameters; the porous rotating disk electrode geometric structure includes a beaker, a reactant solution arranged inside the beaker, a porous rotating disk electrode arranged inside the beaker, and a boundary layer arranged above the porous rotating disk electrode; wherein, below the porous rotating disk electrode is an adsorption layer, below the adsorption layer is an adsorption process, and above the adsorption layer is an electrochemical reaction process; the related parameters include a diffusion coefficient of the reactant in the reactant solution and a diffusion coefficient of the reactant in the boundary layer;

[0027] A simulation current curve determination module is used to solve the convection-diffusion equation using finite element calculation software according to the velocity field simulation solution to determine the simulation current curve at different rotation speeds;

[0028] A comparison module, used for comparing the first difference with the first interval; the first difference is the difference between the spacing of the limiting diffusion current corresponding to the simulation current curve at different speeds and the spacing of the limiting diffusion current corresponding to the experimental current curve;

[0029] The first comparison result determination module is used to:

[0030] When the first difference is greater than the maximum value of the first interval, reducing the diffusion coefficient of the reactant in the reactant solution, and returning to the velocity field simulation solution calculation module;

[0031] When the first difference is less than the minimum value of the first interval, the diffusion coefficient of the reactant in the reactant solution is increased, and the velocity field simulation solution calculation module is returned;

[0032] When the first difference is within the first interval, the second difference is compared with the second interval; the second difference is the difference between the limiting diffusion current value corresponding to the simulation current curve at different speeds and the limiting diffusion current value corresponding to the experimental current curve;

[0033] The second comparison result determination module is used to:

[0034] When the second difference is greater than the maximum value of the second interval, the diffusion coefficient of the reactant in the boundary layer is reduced, and the velocity field simulation solution calculation module is returned;

[0035] When the second difference is less than the minimum value of the second interval, the diffusion coefficient of the reactant in the boundary layer is increased, and the velocity field simulation solution calculation module is returned;

[0036] When the second difference is within the second interval, the effective diffusion coefficient of the pore electrode is determined according to the diffusion coefficient of the reactant in the boundary layer corresponding to the simulated current curve.

[0037] Optionally, an experimental device is also included; the experimental device is used to:

[0038] preparing the porous material into a porous rotating disk electrode;

[0039] A plurality of rotating disk electrode electrochemical experiments are carried out on the porous rotating disk electrode at different rotation speeds to obtain experimental current curves at different rotation speeds; wherein the rotation speed set when carrying out the rotating disk electrode electrochemical experiment is the same as the rotation speed when simulating the porous rotating disk electrode geometric model.

[0040] Optionally, the velocity field simulation solution calculation module specifically includes:

[0041] Aperture Rotating Disk Electrode geometry model building unit for:

[0042] Based on the rotating disk electrode electrochemical experiment, a porous rotating disk electrode geometric structure is constructed;

[0043] Setting relevant parameters; the relevant parameters include: viscosity of reactant solution, concentration of reactant solution, diffusion coefficient of reactant in reactant solution, diffusion coefficient of reactant in boundary layer, reaction pre-exponential factor, transfer coefficient, adsorption rate, rotation speed of porous rotating disk electrode, Reynolds number and boundary conditions; the boundary conditions are that the surface of porous rotating disk electrode is set as a no-slip wall and the walls around beaker are set as solid walls;

[0044] A velocity field type determination unit, used to determine the velocity field type according to the Reynolds number;

[0045] The velocity field simulation solution calculation unit is used to calculate the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different rotation speeds based on the velocity field type and the porous rotating disk electrode geometric model.

[0046] Optionally, in the velocity field type determination unit, the Reynolds number calculation process is:

[0047] The Reynolds number is calculated according to the parameters set when performing the rotating disk electrode electrochemical experiment; wherein, when the Reynolds number is greater than a set threshold, the velocity field type is a turbulent model, and when the Reynolds number is less than or equal to the set threshold, the velocity field type is a laminar model.

[0048] Optionally, the simulated current curve determination module specifically includes:

[0049] A concentration gradient calculation unit is used to solve the convection-diffusion equation using finite element calculation software according to the velocity field simulation solution to determine the concentration gradient of the reactant on the surface of the porous rotating disk electrode and the concentration gradient of the product on the surface of the porous rotating disk electrode;

[0050] An instantaneous current generating unit, used to calculate the instantaneous current generated on the surface of the porous rotating disk electrode at different times using the Butler-Volmer model according to the concentration gradient of the reactant on the surface of the porous rotating disk electrode and the concentration gradient of the product on the surface of the porous rotating disk electrode;

[0051] The simulated current curve determining unit is used to perform integration processing on the instantaneous current at different moments to obtain simulated current curves at different rotation speeds.

[0052] According to the specific embodiments provided by the present invention, the present invention discloses the following technical effects:

[0053] First, the introduction of the boundary layer allows the characteristics of the porous structure to be expressed using an equivalent diffusion coefficient, so that when exploring the mass transfer capacity of the pore structure, we are no longer limited to empirical formulas, but can fully combine them with experimental results to improve the accuracy of calculating the effective diffusion coefficient of the pore electrode.

[0054] Second, the global numerical solution can simulate the velocity field, concentration field and current curve in the entire porous rotating disk electrode without using an approximate analytical solution, further improving the accuracy of the calculation of the effective diffusion coefficient of the porous electrode. BRIEF DESCRIPTION OF THE DRAWINGS

[0055] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0056] Figure 1 Schematic diagram of the geometric structure of the rotating disk electrode of the present invention;

[0057] Figure 2 A schematic flow chart of a method for determining an effective diffusion coefficient of a pore electrode according to the present invention;

[0058] Figure 3 It is a structural schematic diagram of a system for determining an effective diffusion coefficient of a pore electrode according to the present invention; DETAILED DESCRIPTION

[0059] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0060] The rotating disk electrode can effectively eliminate concentration polarization and measure the intrinsic reaction rate more accurately. Therefore, the pore electrode is prepared into a porous rotating disk electrode (PRDE), which can effectively perform electrochemical characterization of the pore electrode.

[0061] On this basis, the present invention constructs the global reaction process through the finite element method, fits the current curve, and obtains the effective diffusion coefficient of the porous rotating disk electrode, thereby judging the mass transfer capacity of different porous electrode materials.

[0062] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.

[0063] In order to study the distribution of current density on the electrode surface and reduce or eliminate the influence of factors such as the diffusion layer, electrochemical researchers have developed a high-speed rotating electrode by comparing various electrodes and stirring methods. Since the end face of this electrode is like a disk, it is also called a rotating disk electrode (RDE), or simply a rotating disk electrode or a rotating disk electrode. Figure 1 shown. Figure 1 Where R1 and H1 represent the radius and height of the electrode rotor immersed in the solution, respectively; R2 and H2 represent the radius and height of the beaker containing the reactant solution, respectively.

[0064] In mathematics, the finite element method (FEM) is a technique for solving boundary value problems of partial differential equations and obtaining approximate solutions. When solving, the entire problem area is decomposed, and each sub-area becomes a simple part, which is called a finite element. In the simulation of the rotating disk electrode, the finite element method can better calculate the fluid-structure interaction model.

[0065] The rotating disk electrode is simplified by axial symmetry and two-dimensional infinite distance mass transfer assumptions to obtain the Levich formula, i L =0.62nFAD 2 / 3 v -1 / 6 ω 1 / 2 c b Among them, the parameter i L , n, F, A, v, ω, D, c b They are limiting diffusion current, number of transferred electrons, Faraday constant, surface area of ​​rotating disk electrode, viscosity of reactant solution, rotating disk electrode speed, reactant diffusion coefficient and reactant solution concentration. This formula can approximate the limiting diffusion current of rotating disk electrode at different speeds. Under this assumption, the limiting diffusion current is proportional to the 1 / 2 power of the rotating disk electrode speed, but this formula is only applicable to rotating disk electrodes with medium speeds, and it is difficult to predict the limiting diffusion current of porous structures.

[0066] In the Butler-Volmer model, the instantaneous current i generated on the rotating disk electrode surface is calculated as: i = FAk 0 [C O (0,t)e -αFη / RT -C R (0,t)e (1-α)Fη / RT]. Among them, F, A, k 0 , C O (0,t),C R (0, t), α, η, R, T are respectively the Faraday constant, the surface area of ​​the rotating disk electrode, the reaction pre-exponential constant, the reactant concentration on the electrode surface at time t, the product concentration on the electrode surface at time t, the transfer coefficient, the overvoltage, the Boltzmann constant and the temperature. It can be seen from the above formula that as the overvoltage continues to increase, the forward reaction rate will become faster and faster, and the instantaneous current generated will also become larger and larger, but the reactant concentration near the rotating disk electrode is also decreasing, so the instantaneous current will not reach infinity.

[0067] The Reynolds number is a dimensionless number that can be used to characterize fluid flow conditions. In a rotating disk electrode, the Reynolds number is calculated as Where ω, r, and v are the rotation speed of the disk electrode, the electrode radius, and the kinematic viscosity of the solution, respectively. The Reynolds number can be used to determine whether turbulent motion occurs in the flow field. It is generally believed that when the Reynolds number is greater than 20,000, the flow field of the rotating disk electrode will produce turbulence.

[0068] Today, the methods for comparing the mass transfer capabilities of different pore structures are all empirical formulas, as shown below:

[0069]

[0070] Among them, D e,j is the effective diffusion coefficient of the reactant in the pore structure, D F,j is the diffusion coefficient of the reactant in the solution, ε p is the porosity, τ F,j is the tortuosity coefficient. The biggest difficulty of this formula is the determination of the tortuosity coefficient. When applied to pore electrodes, the Millington and Quirk model and the Bruggeman model are mainly adopted, taking τ F,j =ε p -1 / 3 and τ F,j =ε p -1 / 2 It can be seen that there is still room for improvement when exploring the effective diffusion coefficient of pore electrodes.

[0071] Although the rotating disk electrode can effectively eliminate concentration polarization and is widely used by many researchers, the study of the velocity field in the rotating disk electrode is based on the analytical solution of Von Karman and Cochran. The solution of the velocity field does not change with time. In fact, with the development of high-speed cameras, it is found in the velocity field experiment of the rotating disk electrode that the solution of the velocity field is non-steady, especially at the central symmetry axis, where the flow field often swings. Scholars once believed that increasing the rotation speed would better overcome the mass transfer limitation, but people found that as the rotation speed gradually increases, turbulence will gradually occur in the reaction pool, which in turn limits the mass transfer. This makes the velocity field of the calculated analytical solution have a certain error with the actual velocity field, and the applicability of the analytical solution is limited to a certain range, which does not conform to the actual situation, and it is difficult for people to know the distribution of the concentration field of the product and reactant, as well as the reaction mode on the electrode surface.

[0072] On the surface of the rotating disk electrode, due to the difference in velocity field distribution, the concentration field is unevenly distributed along the axial direction. However, in the original analytical solution, the treatment method is the one-dimensional plane assumption, that is, the concentration field distribution does not change with the axial direction, which is inconsistent with the actual situation. In addition, in the original analytical solution, it is assumed that the electrode surface is completely smooth, that is, the reactants will be consumed immediately after reaching the electrode surface under extremely high overvoltage, which is also inconsistent with many real experimental situations (in actual situations, due to the roughness of the electrode surface, the apparent diffusion coefficients of the reactants and products on the electrode surface will be inconsistent with their intrinsic diffusion coefficients). In fact, in some fields, people pursue the roughness of materials. For example, in the problem of porous catalysis, porous materials have a larger specific surface area and more reaction sites. When simulating the current of the rotating disk electrode, people try to set zero flux on the electrode surface to solve the reactant concentration and reaction current problems, but these assumptions are still different from the actual situation, and the polarization current curve cannot be reproduced, and it is difficult to simulate and explore the mechanism of the rotating disk electrode in more depth.

[0073] In summary, in the rotating disk electrode, there are errors in the calculation of both the velocity field and the concentration field, and it is difficult to reproduce a complete and correct voltage-current curve. Therefore, the global numerical solution method is considered to improve the entire electrochemical reaction process of the rotating disk electrode.

[0074] The porous rotating disk electrode prepared by the pore electrode has a larger specific surface area. In order to better analyze the CV curve of the porous rotating disk electrode, it is necessary to have a deep understanding of the mass transfer and reaction steps of the porous rotating disk electrode.

[0075] In finite element simulation, the most ideal situation is to use CT scanning to obtain the three-dimensional morphology of the electrode material, and perform three-dimensional modeling to simulate the adsorption and reaction processes of the reactants. However, the microscopic scale of the porous material is at the micrometer level, while the scale of the entire rotating disk electrode is at the centimeter level. Building the entire model requires a huge amount of computing power support, which is very difficult to achieve.

[0076] In view of the above problems, the present invention adopts a finite element calculation method to solve the steady-state velocity field of a rotating disk electrode in a two-dimensional axisymmetric case, and on this basis adopts a pore boundary diffusion layer model to add adsorption reaction and electrochemical reaction to the electrode surface, thereby coupling and solving the generated current on the electrode surface at different speeds. In the Butler-Volmer equation for the generated current, the Faraday constant, electrode surface area, reaction pre-exponential factor constant, transfer coefficient, overpotential, Boltzmann constant and temperature can all be obtained by looking up a table or according to experimental conditions, but the concentration of reactants on the electrode surface at time t and the concentration of products on the electrode surface at time t need to be obtained by numerical solution. In order to obtain accurate reactant concentrations and product concentrations on the electrode surface that vary with time, it is necessary to solve the convection-diffusion equation. And if you want to accurately solve the convection-diffusion equation, you need to know the velocity distribution in the beaker of the rotating disk electrode, that is, the velocity of each divided area in the beaker, so you need to solve the Navier-Stokes equation. In the boundary diffusion layer, the only way of material transfer is diffusion, and there is no influence of the velocity field. Therefore, it is only necessary to solve the convection-diffusion equation without solving the Navier-Stokes equation in advance.

[0077] The model can well restore the current curve obtained from the electrochemical experiment of the pore electrode material. In the process of reducing the current curve, it is necessary to set the diffusion coefficient of the reactant in the beaker and the equivalent diffusion coefficient of the reactant in the pore electrode diffusion layer structure. Comparing the equivalent diffusion coefficient of the pore electrode diffusion layer structure can effectively compare the mass transfer capacity of different structures.

[0078] Embodiment 1

[0079] This embodiment provides a method for determining the effective diffusion coefficient of a pore electrode based on numerical simulation of a rotating disk, which specifically includes:

[0080] (1) Preparation of porous rotating disk electrode: First, a porous rotating disk electrode is prepared using a porous material, and then a rotating disk electrode electrochemical experiment is carried out on the porous rotating disk electrode at different rotation speeds (hereinafter referred to as the actual experiment), thereby obtaining multiple sets of current curves at different rotation speeds.

[0081] (2) Construction of the geometric model of the porous rotating disk electrode: Based on the beaker and rotor (i.e., the porous rotating disk electrode) used in the actual experiment, a geometric model that is exactly the same as the actual experiment is reproduced in the finite element software; the geometric model includes a beaker, a reactant solution arranged inside the beaker, a porous rotating disk electrode arranged inside the beaker, and a boundary region (i.e., the boundary layer, also called the diffusion layer) arranged above the porous rotating disk electrode and with a height of 0.01 mm.

[0082] (3) Assigning material properties: According to the reactant solution taken in the actual experiment, set the viscosity and concentration of the reactant solution in the finite element software.

[0083] (4) Setting of electrochemical reaction parameters: Based on the actual experiment, the rotation speed of the porous rotating disk electrode, the viscosity of the reactant solution, the concentration of the reactant solution, the voltage scanning rate, the diffusion coefficient of the reactant in the reactant solution, the diffusion coefficient of the reactant in the boundary layer, the reaction pre-exponential factor, the transfer coefficient, the adsorption rate of the adsorption process, etc. are input into the finite element software. Among them, the diffusion coefficient of the reactant in the reactant solution can be obtained by looking up the table to obtain this range.

[0084] (5) Set boundary conditions according to the actual conditions of the actual experiment; set the electrode surface as a no-slip wall, the rotation speed of which is v = ω*r, ω is the electrode rotation speed, and r is the distance from the point on the electrode to the rotation center. The bottom of the electrode is the adsorption layer. The adsorption process is set below the adsorption layer, and the reactant consumption is set above the adsorption layer. The rate of reactant consumption is equal to the rate of current generation by the Butler-Volmer equation. Set the top of the beaker as the pressure outlet, and set the walls around the beaker as solid walls.

[0085] (6) Flow field calculation: The Reynolds number Re is calculated based on the actual experimental parameters. If the Reynolds number is greater than 20,000, a turbulent model is used, otherwise a laminar model is used. The corresponding flow field is calculated using the finite element method, the Navier-Stokes equation and the continuity equation are solved, and the numerical solution of the velocity field in the reaction beaker at the first speed of the simulation is obtained.

[0086] (7) Solving multiple groups of speed flow fields: After obtaining the numerical solution of the velocity field in the reaction beaker under the first speed condition corresponding to the actual experiment, keep other reaction parameters unchanged in the simulation software, only change the electrode speed to make it consistent with the speed selected in the experiment in (1), and repeat process (6) to obtain the numerical solution of the velocity field in the reaction beaker of the simulation experiment at different speeds.

[0087] (8) Chemical reaction calculation: With the velocity field results, the convection-diffusion equation can be solved. Based on the velocity field results of (7), the convection-diffusion equation is solved using finite element calculation software to obtain the concentration gradients of the reactants and products on the electrode surface, and then the instantaneous current is calculated based on the Butler-Volmer equation.

[0088] (9) Result processing: Process the result of (8), integrate the current generated on the electrode surface, obtain the current of the entire electrode surface, and thus obtain a simulated current curve.

[0089] (10) Compare the generated current curves at different speeds with the experimental current curves. If the spacing between the limiting diffusion currents at different speeds is too wide, the bulk solution diffusion coefficient needs to be reduced, otherwise it needs to be increased. When the spacing is equal, increasing the diffusion coefficient in the porous electrode diffusion layer will increase the limiting diffusion current as a whole, otherwise it will decrease. Based on these two principles, repeating processes (8)-(9) can obtain a reaction current distribution that is completely consistent with the experimental current in (1), that is, the diffusion coefficient in the porous electrode diffusion layer of the experimental electrode is obtained.

[0090] (11) By comparing the diffusion coefficients in the diffusion layers of porous electrodes of different materials, we can obtain the equivalent diffusion coefficients of different porous materials. The higher the effective diffusion coefficient, the better the mass transfer capacity of the material.

[0091] In this embodiment, the following innovations are provided:

[0092] (1) Boundary layer method: the porous electrode diffusion layer on the electrode surface replaces the uneven surface of the porous electrode, and the effective diffusion coefficient in the boundary layer is used to characterize the mass transfer capacity of the material.

[0093] (2) The global numerical solution method couples the velocity field, concentration field, and mass transfer and electrochemical reaction processes of the rotating disk electrode to reproduce the complete voltage-current curve of the rotating disk electrode.

[0094] Other things that need to be stated are:

[0095] 1. Flow field calculation can adopt CFD and finite volume method.

[0096] 2. The concept of mass transfer capacity of porous layer can be described by porosity or other quantitative descriptions.

[0097] Embodiment 2

[0098] like Figure 2 As shown, this embodiment provides a method for determining an effective diffusion coefficient of a pore electrode, comprising:

[0099] Step 201: Calculate the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different rotation speeds; the porous rotating disk electrode geometric model includes a porous rotating disk electrode geometric structure and related parameters; the porous rotating disk electrode geometric structure includes a beaker, a reactant solution arranged inside the beaker, a porous rotating disk electrode arranged inside the beaker, and a boundary layer arranged above the porous rotating disk electrode; wherein, below the porous rotating disk electrode is an adsorption layer, below the adsorption layer is an adsorption process, and above the adsorption layer is an electrochemical reaction process; the related parameters include a diffusion coefficient of the reactant in the reactant solution and a diffusion coefficient of the reactant in the boundary layer.

[0100] Step 202: According to the velocity field simulation solution, the convection-diffusion equation is solved using finite element calculation software to determine the simulated current curves at different rotation speeds.

[0101] Step 203: Compare the first difference with the first interval; the first difference is the difference between the spacing of the limiting diffusion current corresponding to the simulation current curve at different speeds and the spacing of the limiting diffusion current corresponding to the experimental current curve.

[0102] Step 204: When the first difference is greater than the maximum value of the first interval, the diffusion coefficient of the reactant in the reactant solution is reduced, and the step of returning to the velocity field simulation solution step corresponding to the porous rotating disk electrode geometric model at different speeds is returned; when the first difference is less than the minimum value of the first interval, the diffusion coefficient of the reactant in the reactant solution is increased, and the step of returning to the velocity field simulation solution step corresponding to the porous rotating disk electrode geometric model at different speeds is returned; when the first difference is within the first interval, the second difference is compared with the second interval; the second difference is the difference between the value of the limiting diffusion current corresponding to the simulated current curve at different speeds and the value of the limiting diffusion current corresponding to the experimental current curve.

[0103] Step 205: When the second difference is greater than the maximum value of the second interval, the diffusion coefficient of the reactant in the boundary layer is reduced, and the process returns to the step of calculating the velocity field simulation solution corresponding to the geometric model of the porous rotating disk electrode at different speeds; when the second difference is less than the minimum value of the second interval, the diffusion coefficient of the reactant in the boundary layer is increased, and the process returns to the step of calculating the velocity field simulation solution corresponding to the geometric model of the porous rotating disk electrode at different speeds; when the second difference is within the second interval, the effective diffusion coefficient of the porous electrode is determined based on the diffusion coefficient of the reactant in the boundary layer corresponding to the simulated current curve.

[0104] In this embodiment, the process of determining the experimental current curve is as follows:

[0105] The porous material is prepared into a porous rotating disk electrode.

[0106] At different rotation speeds, multiple groups of rotating disk electrode electrochemical experiments were performed on the porous rotating disk electrode to obtain experimental current curves at different rotation speeds.

[0107] It should be noted that the rotation speed set when performing the rotating disk electrode electrochemical experiment is the same as the rotation speed when simulating the porous rotating disk electrode geometric model.

[0108] Furthermore, step 201 specifically includes:

[0109] Based on the rotating disk electrode electrochemical experiment, a porous rotating disk electrode geometric structure was constructed.

[0110] Set relevant parameters; the relevant parameters include: viscosity of reactant solution, concentration of reactant solution, diffusion coefficient of reactant in reactant solution, diffusion coefficient of reactant in boundary layer, reaction pre-exponential factor, transfer coefficient, adsorption rate, rotation speed of porous rotating disk electrode, Reynolds number and boundary conditions; the boundary conditions are that the surface of porous rotating disk electrode is set as a no-slip wall and the walls around beaker are set as solid walls.

[0111] The velocity field type is determined according to the Reynolds number; the Reynolds number calculation process: the Reynolds number is calculated according to the parameters set when the rotating disk electrode electrochemical experiment is performed; wherein, when the Reynolds number is greater than a set threshold, the velocity field type is a turbulence model, and when the Reynolds number is less than or equal to the set threshold, the velocity field type is a laminar model.

[0112] Based on the velocity field type and the porous rotating disk electrode geometric model, the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different rotation speeds is calculated.

[0113] Furthermore, step 202 specifically includes:

[0114] According to the velocity field simulation solution, the convection-diffusion equation is solved using finite element calculation software to determine the concentration gradient of the reactant on the surface of the porous rotating disk electrode and the concentration gradient of the product on the surface of the porous rotating disk electrode.

[0115] According to the concentration gradient of the reactant on the surface of the porous rotating disk electrode and the concentration gradient of the product on the surface of the porous rotating disk electrode, the Butler-Volmer model is used to calculate the instantaneous current generated on the surface of the porous rotating disk electrode at different times.

[0116] The instantaneous current at different times is integrated to obtain simulated current curves at different rotation speeds.

[0117] Embodiment 3

[0118] like Figure 3 As shown, this embodiment provides a system for determining an effective diffusion coefficient of a pore electrode, comprising:

[0119] The velocity field simulation solution calculation module 301 is used to calculate the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different rotation speeds; the porous rotating disk electrode geometric model includes the porous rotating disk electrode geometric structure and related parameters; the porous rotating disk electrode geometric structure includes a beaker, a reactant solution arranged inside the beaker, a porous rotating disk electrode arranged inside the beaker, and a boundary layer arranged above the porous rotating disk electrode; wherein, below the porous rotating disk electrode is an adsorption layer, below the adsorption layer is an adsorption process, and above the adsorption layer is an electrochemical reaction process; the related parameters include the diffusion coefficient of the reactant in the reactant solution and the diffusion coefficient of the reactant in the boundary layer.

[0120] The simulated current curve determination module 302 is used to solve the convection-diffusion equation using finite element calculation software according to the velocity field simulation solution to determine the simulated current curves at different rotation speeds.

[0121] The comparison module 303 is used to compare the first difference with the first interval; the first difference is the difference between the spacing of the limiting diffusion current corresponding to the simulation current curve at different speeds and the spacing of the limiting diffusion current corresponding to the experimental current curve.

[0122] The first comparison result determination module 304 is used to:

[0123] When the first difference is greater than the maximum value of the first interval, the diffusion coefficient of the reactant in the reactant solution is reduced, and the method returns to the velocity field simulation solution calculation module.

[0124] When the first difference is less than the minimum value of the first interval, the diffusion coefficient of the reactant in the reactant solution is increased, and the method returns to the velocity field simulation solution calculation module.

[0125] When the first difference is within the first interval, the second difference is compared with the second interval; the second difference is the difference between the limiting diffusion current corresponding to the simulation current curve at different speeds and the limiting diffusion current corresponding to the experimental current curve.

[0126] The second comparison result determination module 305 is used to:

[0127] When the second difference is greater than the maximum value of the second interval, the diffusion coefficient of the reactant in the boundary layer is reduced, and the method returns to the velocity field simulation solution calculation module.

[0128] When the second difference is less than the minimum value of the second interval, the diffusion coefficient of the reactant in the boundary layer is increased, and the method returns to the velocity field simulation solution calculation module.

[0129] When the second difference is within the second interval, the effective diffusion coefficient of the pore electrode is determined according to the diffusion coefficient of the reactant in the boundary layer corresponding to the simulated current curve.

[0130] Furthermore, the system described in this embodiment also includes an experimental device; the experimental device is used to:

[0131] The porous material is prepared into a porous rotating disk electrode.

[0132] A plurality of rotating disk electrode electrochemical experiments are carried out on the porous rotating disk electrode at different rotation speeds to obtain experimental current curves at different rotation speeds; wherein the rotation speed set when carrying out the rotating disk electrode electrochemical experiment is the same as the rotation speed when simulating the porous rotating disk electrode geometric model.

[0133] The velocity field simulation solution calculation module 301 specifically includes:

[0134] Aperture Rotating Disk Electrode geometry model building unit for:

[0135] Based on the rotating disk electrode electrochemical experiment, a porous rotating disk electrode geometric structure is constructed;

[0136] Set relevant parameters; the relevant parameters include: viscosity of reactant solution, concentration of reactant solution, diffusion coefficient of reactant in reactant solution, diffusion coefficient of reactant in boundary layer, reaction pre-exponential factor, transfer coefficient, adsorption rate, rotation speed of porous rotating disk electrode, Reynolds number and boundary conditions; the boundary conditions are that the surface of porous rotating disk electrode is set as a no-slip wall and the walls around beaker are set as solid walls.

[0137] A velocity field type determination unit is used to determine the velocity field type according to the Reynolds number; the Reynolds number calculation process: the Reynolds number is calculated according to the parameters set when performing the rotating disk electrode electrochemical experiment; wherein, when the Reynolds number is greater than a set threshold, the velocity field type is a turbulence model, and when the Reynolds number is less than or equal to the set threshold, the velocity field type is a laminar model.

[0138] The velocity field simulation solution calculation unit is used to calculate the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different rotation speeds based on the velocity field type and the porous rotating disk electrode geometric model.

[0139] The simulated current curve determination module 302 specifically includes:

[0140] The concentration gradient calculation unit is used to solve the convection-diffusion equation based on the velocity field simulation solution using finite element calculation software to determine the concentration gradient of the reactant on the surface of the porous rotating disk electrode and the concentration gradient of the product on the surface of the porous rotating disk electrode.

[0141] The instantaneous current generating unit is used to calculate the instantaneous current generated on the surface of the porous rotating disk electrode at different times according to the concentration gradient of the reactant on the surface of the porous rotating disk electrode and the concentration gradient of the product on the surface of the porous rotating disk electrode using the Butler-Volmer model.

[0142] The simulated current curve determining unit is used to perform integration processing on the instantaneous current at different moments to obtain simulated current curves at different rotation speeds.

[0143] In this specification, each embodiment is described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the embodiments can be referred to each other. For the system disclosed in the embodiment, since it corresponds to the method disclosed in the embodiment, the description is relatively simple, and the relevant parts can be referred to the method part.

[0144] The principles and implementation methods of the present invention are described in this article using specific examples. The description of the above embodiments is only used to help understand the method and core idea of ​​the present invention. At the same time, for those skilled in the art, according to the idea of ​​the present invention, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as limiting the present invention.

Claims

1. A method for determining the effective diffusion coefficient of a pore electrode, characterized in that: include: Calculate the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different rotation speeds; the porous rotating disk electrode geometric model includes the porous rotating disk electrode geometric structure and related parameters; the porous rotating disk electrode geometric structure includes a beaker, a reactant solution arranged inside the beaker, a porous rotating disk electrode arranged inside the beaker, and a boundary layer arranged above the porous rotating disk electrode; wherein, below the porous rotating disk electrode is an adsorption layer, below the adsorption layer is an adsorption process, and above the adsorption layer is an electrochemical reaction process; the related parameters include the diffusion coefficient of the reactant in the reactant solution and the diffusion coefficient of the reactant in the boundary layer; According to the velocity field simulation solution, the convection-diffusion equation is solved using finite element calculation software to determine the simulated current curves at different rotation speeds; Comparing the first difference with the first interval; the first difference is the difference between the spacing of the limiting diffusion current corresponding to the simulation current curve at different speeds and the spacing of the limiting diffusion current corresponding to the experimental current curve; When the first difference is greater than the maximum value of the first interval, the diffusion coefficient of the reactant in the reactant solution is reduced, and the step of calculating the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different speeds is returned; when the first difference is less than the minimum value of the first interval, the diffusion coefficient of the reactant in the reactant solution is increased, and the step of calculating the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different speeds is returned; when the first difference is within the first interval, the second difference is compared with the second interval; the second difference is the difference between the value of the limiting diffusion current corresponding to the simulated current curve at different speeds and the value of the limiting diffusion current corresponding to the experimental current curve; When the second difference is greater than the maximum value of the second interval, the diffusion coefficient of the reactant in the boundary layer is reduced, and the process returns to the velocity field simulation solution step corresponding to the porous rotating disk electrode geometric model at different speeds; when the second difference is less than the minimum value of the second interval, the diffusion coefficient of the reactant in the boundary layer is increased, and the process returns to the velocity field simulation solution step corresponding to the porous rotating disk electrode geometric model at different speeds; when the second difference is within the second interval, the effective diffusion coefficient of the porous electrode is determined based on the diffusion coefficient of the reactant in the boundary layer corresponding to the simulated current curve.

2. The method for determining the effective diffusion coefficient of a pore electrode according to claim 1, characterized in that: The determination process of the experimental current curve is: preparing the porous material into a porous rotating disk electrode; A plurality of rotating disk electrode electrochemical experiments are carried out on the porous rotating disk electrode at different rotation speeds to obtain experimental current curves at different rotation speeds; wherein the rotation speed set when carrying out the rotating disk electrode electrochemical experiment is the same as the rotation speed when simulating the porous rotating disk electrode geometric model.

3. The method for determining the effective diffusion coefficient of a pore electrode according to claim 2, characterized in that: The calculation of the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different speeds specifically includes: Based on the rotating disk electrode electrochemical experiment, a porous rotating disk electrode geometric structure is constructed; Setting relevant parameters; the relevant parameters include: viscosity of reactant solution, concentration of reactant solution, diffusion coefficient of reactant in reactant solution, diffusion coefficient of reactant in boundary layer, reaction pre-exponential factor, transfer coefficient, adsorption rate, rotation speed of porous rotating disk electrode, Reynolds number and boundary conditions; the boundary conditions are that the surface of porous rotating disk electrode is set as a no-slip wall and the walls around beaker are set as solid walls; determining a velocity field type according to the Reynolds number; Based on the velocity field type and the porous rotating disk electrode geometric model, the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different rotation speeds is calculated.

4. The method for determining the effective diffusion coefficient of a pore electrode according to claim 3, characterized in that: The calculation process of the Reynolds number is: The Reynolds number is calculated according to the parameters set when performing the rotating disk electrode electrochemical experiment; wherein, when the Reynolds number is greater than a set threshold, the velocity field type is a turbulent model, and when the Reynolds number is less than or equal to the set threshold, the velocity field type is a laminar model.

5. The method for determining the effective diffusion coefficient of a pore electrode according to claim 1, characterized in that: The method of solving the convection-diffusion equation using finite element calculation software according to the velocity field simulation solution to determine the simulated current curves at different speeds specifically includes: According to the velocity field simulation solution, the convection-diffusion equation is solved by using finite element calculation software to determine the concentration gradient of the reactant on the surface of the porous rotating disk electrode and the concentration gradient of the product on the surface of the porous rotating disk electrode; According to the concentration gradient of the reactant on the surface of the porous rotating disk electrode and the concentration gradient of the product on the surface of the porous rotating disk electrode, the Butler-Volmer model is used to calculate the instantaneous current generated on the surface of the porous rotating disk electrode at different times; The instantaneous current at different times is integrated to obtain simulated current curves at different rotation speeds.

6. A system for determining the effective diffusion coefficient of a pore electrode, characterized in that: include: A velocity field simulation solution calculation module is used to calculate the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different rotation speeds; the porous rotating disk electrode geometric model includes a porous rotating disk electrode geometric structure and related parameters; the porous rotating disk electrode geometric structure includes a beaker, a reactant solution arranged inside the beaker, a porous rotating disk electrode arranged inside the beaker, and a boundary layer arranged above the porous rotating disk electrode; wherein, below the porous rotating disk electrode is an adsorption layer, below the adsorption layer is an adsorption process, and above the adsorption layer is an electrochemical reaction process; the related parameters include a diffusion coefficient of the reactant in the reactant solution and a diffusion coefficient of the reactant in the boundary layer; A simulation current curve determination module is used to solve the convection-diffusion equation using finite element calculation software according to the velocity field simulation solution to determine the simulation current curve at different rotation speeds; A comparison module, used for comparing the first difference with the first interval; the first difference is the difference between the spacing of the limiting diffusion current corresponding to the simulation current curve at different speeds and the spacing of the limiting diffusion current corresponding to the experimental current curve; The first comparison result determination module is used to: When the first difference is greater than the maximum value of the first interval, reducing the diffusion coefficient of the reactant in the reactant solution, and returning to the velocity field simulation solution calculation module; When the first difference is less than the minimum value of the first interval, the diffusion coefficient of the reactant in the reactant solution is increased, and the velocity field simulation solution calculation module is returned; When the first difference is within the first interval, the second difference is compared with the second interval; the second difference is the difference between the limiting diffusion current value corresponding to the simulation current curve at different speeds and the limiting diffusion current value corresponding to the experimental current curve; The second comparison result determination module is used to: When the second difference is greater than the maximum value of the second interval, the diffusion coefficient of the reactant in the boundary layer is reduced, and the velocity field simulation solution calculation module is returned; When the second difference is less than the minimum value of the second interval, the diffusion coefficient of the reactant in the boundary layer is increased, and the velocity field simulation solution calculation module is returned; When the second difference is within the second interval, the effective diffusion coefficient of the pore electrode is determined according to the diffusion coefficient of the reactant in the boundary layer corresponding to the simulated current curve.

7. A system for determining the effective diffusion coefficient of a pore electrode according to claim 6, characterized in that: Also included is an experimental device; the experimental device is used for: preparing the porous material into a porous rotating disk electrode; A plurality of rotating disk electrode electrochemical experiments are carried out on the porous rotating disk electrode at different rotation speeds to obtain experimental current curves at different rotation speeds; wherein the rotation speed set when carrying out the rotating disk electrode electrochemical experiment is the same as the rotation speed when simulating the porous rotating disk electrode geometric model.

8. A system for determining the effective diffusion coefficient of a pore electrode according to claim 7, characterized in that: The velocity field simulation solution calculation module specifically includes: Aperture Rotating Disk Electrode geometry model building unit for: Based on the rotating disk electrode electrochemical experiment, a porous rotating disk electrode geometric structure is constructed; Setting relevant parameters; the relevant parameters include: viscosity of reactant solution, concentration of reactant solution, diffusion coefficient of reactant in reactant solution, diffusion coefficient of reactant in boundary layer, reaction pre-exponential factor, transfer coefficient, adsorption rate, rotation speed of porous rotating disk electrode, Reynolds number and boundary conditions; the boundary conditions are that the surface of porous rotating disk electrode is set as a no-slip wall and the walls around beaker are set as solid walls; A velocity field type determination unit, used to determine the velocity field type according to the Reynolds number; The velocity field simulation solution calculation unit is used to calculate the velocity field simulation solution corresponding to the porous rotating disk electrode geometric model at different rotation speeds based on the velocity field type and the porous rotating disk electrode geometric model.

9. A system for determining the effective diffusion coefficient of a pore electrode according to claim 8, characterized in that: In the velocity field type determination unit, the Reynolds number calculation process is: The Reynolds number is calculated according to the parameters set when performing the rotating disk electrode electrochemical experiment; wherein, when the Reynolds number is greater than a set threshold, the velocity field type is a turbulent model, and when the Reynolds number is less than or equal to the set threshold, the velocity field type is a laminar model.

10. A system for determining the effective diffusion coefficient of a pore electrode according to claim 6, characterized in that: The simulated current curve determination module specifically includes: A concentration gradient calculation unit is used to solve the convection-diffusion equation using finite element calculation software according to the velocity field simulation solution to determine the concentration gradient of the reactant on the surface of the porous rotating disk electrode and the concentration gradient of the product on the surface of the porous rotating disk electrode; An instantaneous current generating unit, used to calculate the instantaneous current generated on the surface of the porous rotating disk electrode at different times using the Butler-Volmer model according to the concentration gradient of the reactant on the surface of the porous rotating disk electrode and the concentration gradient of the product on the surface of the porous rotating disk electrode; The simulated current curve determining unit is used to perform integration processing on the instantaneous current at different moments to obtain simulated current curves at different rotation speeds.

Citation Information

Patent Citations

  • Method and system for establishing computational fluid mechanical model for simulating cigarette combustion

    CN107679314A

  • CFD-based heavy metal wastewater sulfuration precipitation reactor optimization method

    CN110277141A