Method for preparing aldehydes and separating catalyst systems by membrane separation
By performing gas exchange before membrane separation and increasing the partial pressure fraction of carbon monoxide or hydrogen, the problem of catalyst loss during the membrane separation process is solved, and the rejection rate of the catalyst and the economy of the hydroformylation process are improved.
Patent Information
- Application Number
- CN202110864052.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-07-30
- Filing Date
- 2021-07-29
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2041-07-29
AI Technical Summary
In the existing hydroformylation method, the uniformly dissolved catalyst is easily lost during the membrane separation process, resulting in increased economic costs.
Gas exchange is performed before membrane separation to increase the partial pressure fraction of carbon monoxide or hydrogen, thereby improving the retention efficiency of the catalyst and reducing catalyst loss.
By increasing the partial pressure fraction of carbon monoxide or hydrogen, the rejection rate of the catalyst is significantly increased, the loss of the catalyst is reduced, and the economy of the hydroformylation process is improved.
Abstract
Description
Technical Field
[0001] The present invention relates to a method for preparing aldehydes from C2 to C20 olefins using a subsequent membrane separation of a catalyst system that separates a uniformly dissolved catalyst system, wherein before the membrane separation, a gas exchange for increasing the partial pressure fraction of carbon monoxide or hydrogen is performed to improve the retention of the catalyst by the membrane. Background Art
[0002] Hydroformylation processes for preparing aldehydes are well known to those skilled in the art. In these processes, olefins are converted into the corresponding aldehydes by reaction with synthesis gas (a mixture of carbon monoxide (CO) and hydrogen (H2)) in the presence of a catalyst system. Hydroformylation is a commonly used industrial process that can produce hundreds of kilotonnes (kt) of aldehydes per year in factories. The catalyst systems commonly used here are homogeneously dissolved catalyst systems and include transition metal complexes, usually cobalt or rhodium as metal and phosphorus-containing ligands.
[0003] On the scale of hundreds of kt, the ability to run such hydroformylation methods economically depends on multiple factors. An important factor is the metal in the catalyst system of uniform dissolution, because rhodium and cobalt and compounds thereof used as catalyst precursors are relatively expensive raw materials. Therefore, the core purpose of the operation of industrialized hydroformylation methods is to minimize the loss of catalyst during operation. A known measure is to separate the catalyst system of uniform dissolution from the reaction output, and the catalyst system is recycled to the reaction zone. For example, it can be completed by known membrane separation methods (for example, referring to WO 2010 / 097376A1). Known membrane separation methods are performed here, so that the reaction output using synthesis gas pressurization is supplied to membrane separation or first the reaction output is subjected to thermal separation (distillation, evaporation in thin film evaporator (TFE)), wherein the reaction output must first be decompressed, and then membrane separation is performed thereafter, optionally when inert gas (such as nitrogen) is pressurized.
[0004] However, catalyst losses may also occur during or before the known separation processes, either through adhesion of clusters on the part of the system (caused by precipitation of insoluble transition metal compounds in the system) or through inadequate separation of the catalyst system from the reactor output. Summary of the invention
[0005] It was therefore an object of the present invention to provide a process for preparing aldehydes in which, compared with the known processes, the losses of catalyst are reduced during the separation of the homogeneously dissolved catalyst system by membrane separation.
[0006] It has been surprisingly found that this purpose can be achieved by gas exchange after the actual reaction but before the membrane separation. In this method, synthesis gas, i.e. a mixture mainly comprising carbon monoxide and hydrogen, is at least partially replaced by carbon monoxide or hydrogen, with the result that the partial pressure fraction of carbon monoxide or hydrogen is increased. Therefore, the output obtained from the reaction output containing the product or from the thermal separation provided upstream of the membrane separation is pressurized using a gas different from the composition in the reaction, or using a gas mixture with different blends to pressurize, which causes an increase in interception in the subsequent membrane separation and thus better separation of the catalyst system of uniform dissolution.
[0007] Therefore, the present invention achieves this object by a process for preparing an aldehyde, said process comprising at least:
[0008] Hydroformylation by reacting C2 to C20 olefins, preferably C2 to C17 olefins, more preferably C3 to C14 olefins, and most preferably C6 to C14 olefins, with synthesis gas in at least one reaction zone in the presence of a homogeneously dissolved catalyst system comprising at least Co or Rh and preferably a phosphorus-containing ligand, to obtain a liquid reaction output containing the product, wherein the partial pressure fraction of CO or H2 in the hydroformylation does not exceed 75% of the total gas pressure, preferably does not exceed 70% of the total gas pressure, more preferably does not exceed 65% of the total gas pressure, the total gas pressure being the sum of the pressures arising from all gaseous species present, and
[0009] Membrane separation for separating homogeneously dissolved catalyst systems, the method being characterized in that
[0010] Prior to membrane separation, gas exchange is carried out with CO or H2, with the result that the partial pressure fraction of CO or H2 accounts for more than 80% of the total gas pressure, preferably more than 85% of the total gas pressure, more preferably more than 90% of the total gas pressure. DETAILED DESCRIPTION
[0011] The first part of the inventive method is the hydroformylation of C2-C20 olefins, preferably C2 to C17 olefins, more preferably C3 to C14 olefins, and most preferably C6 to C14 olefins. In principle, pure olefins can be used in this method. However, hydrocarbon streams comprising suitable olefins are preferably used. The olefin content in the hydrocarbon stream should naturally be high enough so that the hydroformylation can be operated economically. The olefin-containing feed mixture is preferably virtually free of other unsaturated compounds or polyunsaturated compounds, such as dienes or acetylene derivatives.
[0012] The hydrocarbon stream that can be used in the process of the invention may include olefins with terminal and / or internal carbon-carbon double bonds. In addition, the hydrocarbon stream may include olefins with the same or different numbers of carbon atoms. Suitable olefins are in particular ethylene, propylene, 1- or 2-butene or mixtures thereof, isobutylene, 1- or 2-pentene or mixtures thereof, isopentene, 1-, 2- or 3-hexene, 1-heptene, linear heptenes with internal double bonds (2-heptene, 3-heptene, etc.), mixtures of linear heptenes, 2- or 3-methyl-1-hexene, 1-octene, linear octenes with internal double bonds, mixtures of linear octenes, 2- or 3-methylheptene, 1-nonene, 1-hexadecene, linear hexadecene with an internal double bond, and a mixture of linear hexadecenes.
[0013] Propylene is industrially produced by naphtha cracking and is a readily available basic chemical. C5 olefins, i.e. pentenes, are present in the light petroleum fractions of refineries or crackers. The technical grade mixture comprising straight-chain C4 olefins, n-butenes and isobutenes is a mixture from the light petroleum fractions of refineries, from the C4 fractions of FC crackers or logistic crackers, from the mixture of Fischer-Tropsch synthesis, from the mixture of butane dehydrogenation, and from the mixture of metathesis or other industrial processes. For example, a straight-chain butene mixture suitable for the method of the present invention is obtained from the C4 fraction of a logistic cracker.
[0014] By oligomerization, for example dimerization, trimerization or tetramerization, higher olefins can be obtained especially.In addition, suitable hydrocarbon stream is the mixture of isomeric hexene (two propylenes) produced by propylene dimerization, the mixture of isomeric octenes (two butenes) produced by butene dimerization, the mixture of isomeric nonene (three propylenes) produced by propylene trimerization, the mixture of isomeric dodecene (tetrapropylene or tributylene) produced by propylene tetramerization or butene trimerization, the isomeric hexadecene (tetrabutylene) produced by butene tetramerization and the olefin mixture produced by the olefin co-oligomerization with different number of carbon atoms (preferably 2 to 4 carbon atoms), optionally after being separated by distillation into the cut with the same or different number of carbon atoms.Also olefins or olefin mixtures that can be produced using the Fischer-Tropsch synthesis method.In addition, the olefins that can also be produced using olefin metathesis or other industrialized methods.
[0015] The olefins used in the process are hydroformylated using synthesis gas in the presence of a homogeneously dissolved catalyst system. The molar ratio of synthesis gas to feed mixture should be between 6:1 and 1:1, preferably between 3:1 and 1:1, more preferably between 2:1 and 1:1. The hydroformylation can optionally be carried out in the presence of solvents known to those skilled in the art, but preferably no solvent is used.
[0016] The homogeneous catalyst system used in the process of the invention comprises or consists of Co or Rh (preferably Rh) and preferably a phosphorus-containing ligand. In a particularly preferred embodiment, the catalyst system of the invention comprises Rh and a phosphorus-containing ligand. Suitable ligands for the catalyst system of the invention are well known to the person skilled in the art (see, for example, the textbook "Rhodium Catalyzed Hydroformylation" by PWNM van Leeuwen (2002) or A. and R. Franke, “Hydroformylation–Fundamentals, Processes and Applications in Organic Synthesis” (2016).
[0017] The phosphorus-containing ligand of the catalyst system of the invention is preferably a phosphine, such as TPP (triphenylphosphine), a monophosphite, such as Alkanox 240 (tris(2,4-di-tert-butylphenyl)phosphite), or a bisphosphite, such as BiPhePhos. Mixtures of ligands can also be used.
[0018] The hydroformylation is preferably carried out under the following conditions: The temperature in the hydroformylation is preferably in the range of 80 to 250° C., more preferably in the range of 90 to 225° C., and particularly preferably in the range of 100 to 210° C. The pressure in the hydroformylation is preferably in the range of 10 to 350 bar, more preferably in the range of 30 to 325 bar, and particularly preferably in the range of 45 to 300 bar.
[0019] According to the invention, the hydroformylation is carried out in at least one reaction zone. The reaction zone for the purposes of the invention comprises at least one reactor in which the hydroformylation is carried out. The reaction zone may also comprise more than one reactor, in particular two or three reactors, which may be connected in parallel or in series, or a mixture of parallel and series arrangements.
[0020] The pressure in the hydroformylation generally corresponds to the total gas pressure. The total gas pressure in the context of the present invention is understood to mean the sum of the pressures resulting from all gaseous substances present, i.e. the pressure of the (total) gas phase. In the present invention, this corresponds in particular to the sum of the H2 partial pressures, i.e. the total gas pressure and then the synthesis gas pressure. In the hydroformylation according to the invention, the partial pressure fraction of CO or H2 does not exceed 70% of the total gas pressure, preferably does not exceed 60% of the total gas pressure, more preferably does not exceed 55% of the total gas pressure.
[0021] The liquid reaction output obtained in the hydroformylation, which contains the product, is therefore also under the pressure present during the hydroformylation. After the hydroformylation, a thermal separation or a membrane separation is carried out. However, the thermal separation is optional here, that is to say it does not need to be carried out, while the process according to the invention always includes a membrane separation. It is also possible to carry out the thermal separation only after the membrane separation has been carried out. In certain cases, the membrane separation can be carried out before and after the thermal separation.
[0022] When this optional step is carried out, the thermal separation can be carried out before or after the membrane separation. The thermal separation can consist of a single process step or a plurality of process steps. The thermal separation comprises at least one thermal separation method, preferably selected from thin film evaporation, distillation, falling film evaporation and short path evaporation.
[0023] In a preferred embodiment of the invention, thermal separation takes place before membrane separation, but the gas exchange according to the invention takes place after thermal separation and before membrane separation.
[0024] The membrane separation carried out after the hydroformylation, optionally before or after the thermal separation as described above, serves to separate off the homogeneously dissolved catalyst system.
[0025] Before membrane separation, and optionally before thermal separation upstream of membrane separation, gas exchange is performed with CO or H2, so that the partial pressure fraction of CO or H2 accounts for more than 80% of the total gas pressure, preferably more than 85% of the total gas pressure, and more preferably more than 90% of the total gas pressure. By this gas exchange, the partial pressure fraction of CO or H2 is selectively increased, while the partial pressure fraction of the respective other components is reduced. Possible gas exchange methods are known to those skilled in the art.
[0026] As described above, due to the presence of synthesis gas, after hydroformylation, the liquid reaction output containing the product is still under pressure. If thermal separation occurs before membrane separation, different or additional gases, such as inert gases, may also be present. Gas exchange occurs before membrane separation, for example, by at least partially venting the gases present, i.e., depressurizing the reaction output or the output from the thermal separation and then pressurizing with CO or H2 until the desired CO or H2 partial pressure fraction is reached, i.e., more than 80% of the total gas pressure is present, preferably more than 85% of the total gas pressure, more preferably more than 90% of the total gas pressure. In another variant, the output from the reaction or the output from the thermal separation is depressurized and then pressurized with CO or H2 using a mixing zone and / or a bubble column until the desired CO or H2 partial pressure fraction is reached, i.e., more than 80% of the total gas pressure is present, preferably more than 85% of the total gas pressure, more preferably more than 90% of the total gas pressure.
[0027] The decompression of the gas discharge / liquid reaction output or the output from the thermal separation and the subsequent pressurization of CO or H2, optionally using a mixing zone and / or a bubble column, can be carried out successively once or twice or more to set the desired partial pressure fraction. After the gas exchange, the total gas pressure is preferably 1 to 70 bar, more preferably 2 to 30 bar, and particularly preferably 4 to 20 bar.
[0028] After the gas exchange, the liquid reaction output or the output from the upstream thermal separation is subjected to membrane separation to separate the homogeneous catalyst system. The membrane separation is preferably carried out at a transmembrane pressure of 5 to 100 bar, more preferably 10 to 80 bar, and particularly preferably 20 to 50 bar. In a preferred embodiment, the membrane separation is also carried out at a temperature of 0° C. to 200° C., more preferably 20° C. to 160° C.
[0029] The membrane material used in membrane separation is preferably selected from polydimethylsiloxane, polyimide, partially fluorinated polymer, fully fluorinated polymer, perfluoropolymer, amorphous fluoropolymer (e.g. ), amorphous or partially crystalline perfluoroalkoxy polymers (e.g. ), block copolymers of the above materials, polymers with intrinsic microporosity (PIM), polyaryletherketones (especially polyetheretherketone and polyetherketoneketone), polybenzimidazoles and polyethers. Polymers with intrinsic microporosity (PIM) with different monomer compositions, especially polymers containing spirobifluorene groups, are also suitable. The membrane material is preferably polydimethylsiloxane (PDMS) or a perfluoroalkoxy polymer, such as
[0030] In a preferred embodiment, the membrane material used is intrinsically stable in the reaction output / in the mixture present after thermal separation, ie it does not require any additional crosslinking of the polymer chains.
[0031] The method of the present invention can be carried out continuously or batchwise. In a preferred embodiment, the method is carried out continuously.
[0032] The present invention is explained below in conjunction with examples. However, these examples do not constitute any limitation and are only used for illustration.
[0033] Example
[0034] Example 1 - Gas Exchange with Hydrogen and Carbon Monoxide in Toluene
[0035] Experimental setup
[0036] Dicarbonyl (acetylacetonato) rhodium (I) (1.97 g, 7.63 mmol) as a precursor of the transition metal of the catalyst system and a phosphorus-containing ligand 240 (tris(2,4-di-tert-butylphenyl)phosphite) (98.74 g, 152.6 mmol) was dissolved in toluene (2612.1 g) with a rhodium:ligand molar ratio of 1:20 and a Rh concentration of 300 ppm (by mass).
[0037] This solution was subjected to membrane separation in a closed-loop membrane test apparatus, where the permeate and excess retentate were recycled back into the feed. This continuous circulation mode ensured that the membrane separation conditions (such as feed concentration and viscosity) remained similar during the experiment. The membrane area was 84.5 cm 2 The test membrane is sealed in a flat channel test cell. The membrane material used is cross-linked polydimethylsiloxane (PDMS).
[0038] The catalyst was first run at 60°C and 40 bar synthesis gas pressure in a reactor without membrane separation. The reactor was then depressurized to a total gas pressure of 20 bar, the temperature dropped to 30°C, and the flat channel test cell was then put into operation. The membrane cycle was run at 30°C, a feed pressure of 50 bar and a permeate pressure of 21 bar.
[0039] Measurement of interception
[0040] The first measurement, measurement 1, was carried out at a reactor pressure of 20 bar synthesis gas (CO:H2 mixture = about 50:50). In each case, samples of the feed, retentate and permeate were collected and investigated for rhodium concentration therein by ICP-MS to determine the rhodium retention therein (rhodium retention = 1 - (Rh concentration in permeate / Rh concentration in retentate)). The rhodium retention was 73%.
[0041] Following the operation of the membrane separation, a gas exchange is then carried out in which the reactor is repeatedly depressurized to 2 bar and then pressurized to 20 bar with hydrogen. This pressure exchange consisting of depressurization and hydrogen repressurization is repeated three times. Thereafter, the partial pressure fraction of hydrogen accounts for more than 90% of the total gas pressure. This feed is then used for measurement 2. Samples of the feed and permeate are collected and the rhodium concentration therein is studied to determine the rhodium retention therein. After hydrogen pressurization, the rhodium retention is 80%. This shows that the retention of rhodium in membrane separation can be significantly increased by pre-pressurizing with hydrogen instead of synthesis gas.
[0042] Subsequently, the starting situation was restored by a reverse gas exchange from hydrogen to synthesis gas pressure, analogously to the gas exchange from synthesis gas to hydrogen (measurement 3). Thereafter, the rhodium retention was 70%.
[0043] A further gas exchange was then carried out in a similar manner, but this time with carbon monoxide (measurement 4). The rhodium retention was then 78%. This shows that the retention of rhodium in the membrane separation can be significantly increased by prepressurizing with carbon monoxide instead of synthesis gas.
[0044] The results are again summarized in the following table:
[0045] Measurement Rhodium retention by the membrane 1(Synthesis gas) 73% 2 (Hydrogen) 80% 3(Synthesis gas) 70% 4 (Carbon monoxide) 78%
[0046] Example 2 - Gas Exchange with Hydrogen and Carbon Monoxide in Isotridecaldehyde
[0047] The experiment described in Example 1 was repeated using isotridecanal instead of toluene. For this purpose, dicarbonyl(acetylacetonato)rhodium(I) (1.174 g, 4.55 mmol) and 240 (tris (2,4-di-tert-butylphenyl) phosphite) (58.31 g, 152.6 mmol) was dissolved in isotridecanal (2492.02 g) at a rhodium:ligand molar ratio of 1:20 and a Rh concentration of 300 ppm (by mass). The experimental setup and procedure were carried out as described in Example 1.
[0048] Here, it is also found that the membrane rejection is higher than the comparison range with synthesis gas, whether after pressurization with hydrogen or after pressurization with carbon monoxide.
[0049] The results using isotridecanal as solvent are summarized in the following table:
[0050] Measurement Rhodium retention by the membrane 1(Synthesis gas) 30% 2 (Hydrogen) 45% 3(Synthesis gas) 21% 4 (Carbon monoxide) 40%
[0051] Example 3 - Gas Exchange of Hydrogen and Carbon Monoxide in Toluene Using Membranes Made of Polyetheretherketone
[0052] The experiment described in Example 1 was repeated using toluene and using a membrane made of polyetheretherketone (PEEK) instead of a membrane made of crosslinked PDMS. The membrane made of PEEK (Example 1) was prepared according to WO 2015 / 110843 A1.
[0053] Dicarbonyl(acetylacetonato)rhodium(I) (1.824 g, 7.07 mmol) and 240 (tris (2,4-di-tert-butylphenyl) phosphite) (90.85 g, 140.4 mmol) was dissolved in toluene (2431 g) at a rhodium:ligand molar ratio of 1:20 and a Rh concentration of 300 ppm (by mass). The experimental setup and procedure were carried out as described in Example 1.
[0054] Here, it is also found that the membrane rejection is higher than the comparison range with synthesis gas, whether after pressurization with hydrogen or after pressurization with carbon monoxide.
[0055] The results for the membranes made with toluene as solvent and PEEK are summarized in the following table:
[0056] Measurement Rhodium retention by the membrane 1(Synthesis gas) 89% 2 (Hydrogen) 96% 3(Synthesis gas) 90% 4 (Carbon monoxide) 95%
[0057] Example 4 - Gas Exchange of Hydrogen and Carbon Monoxide in Toluene Using SolSep NF030306
[0058] The experiment described in Example 1 was repeated using the commercially available membrane NF030306 from SolSep BV.
[0059] Dicarbonyl(acetylacetonato)rhodium(I) (1.825 g, 7.07 mmol) and 240 (tris (2,4-di-tert-butylphenyl) phosphite) (90.90 g, 140.5 mmol) was dissolved in toluene (2448 g) at a rhodium:ligand molar ratio of 1:20 and a Rh concentration of 300 ppm (by mass). The experimental setup and procedure were carried out as described in Example 1.
[0060] Here, it is also found that the membrane rejection is higher than the comparison range with synthesis gas, whether after pressurization with hydrogen or after pressurization with carbon monoxide.
[0061] The results with toluene as solvent and membrane SolSep NF030306 are summarized in the following table:
[0062] Measurement Rhodium retention by the membrane 1(Synthesis gas) 63% 2 (Hydrogen) 74% 3(Synthesis gas) 66% 4 (Carbon monoxide) 71%
Claims
1. A method for preparing an aldehyde, the method comprising at least: Hydroformylation, which is carried out in at least one reaction zone by reacting C2 to C20 olefins with synthesis gas in the presence of a homogeneously dissolved catalyst system comprising at least Co or Rh, to obtain a liquid reaction output containing products, wherein the partial pressure fraction of CO or H2 in the hydroformylation does not exceed 75% of the total gas pressure, the total gas pressure being the sum of the pressures generated by all gaseous substances present, and membrane separation to separate the homogeneously dissolved catalyst system, The method is characterized in that Prior to the membrane separation, gas exchange is performed with CO or H2, with the result that the partial pressure fraction of CO or H2 accounts for more than 80% of the total gas pressure.
2. The method according to claim 1, wherein the C2 to C20 olefin is a C2 to C17 olefin.
3. The method according to claim 1, wherein the C2 to C20 olefin is a C3 to C14 olefin.
4. The method according to claim 1, wherein the C2 to C20 olefin is a C6 to C14 olefin.
5. The method of claim 1, wherein the homogeneously dissolved catalyst system further comprises a phosphorus-containing ligand.
6. The method according to claim 1, wherein the partial pressure fraction of CO or H2 in the hydroformylation accounts for no more than 70% of the total gas pressure.
7. The method according to claim 1, wherein the partial pressure fraction of CO or H2 in the hydroformylation accounts for no more than 65% of the total gas pressure.
8. The method according to claim 1, wherein before the membrane separation, gas exchange with CO or H2 is performed, as a result of which the partial pressure fraction of the CO or H2 accounts for more than 85% of the total gas pressure.
9. The method according to claim 1, wherein before the membrane separation, gas exchange with CO or H2 is performed, as a result of which the partial pressure fraction of the CO or H2 accounts for more than 90% of the total gas pressure.
10. The process according to claim 1, wherein the hydroformylation is carried out at a pressure of 10 to 350 bar.
11. The process according to any one of claims 1 to 10, wherein the hydroformylation is carried out at a temperature of 80 to 250°C.
12. The method according to any one of claims 1 to 10, wherein the homogeneously dissolved catalyst system comprises at least Rh and a phosphorus-containing ligand.
13. The method of claim 5, wherein the phosphorus-containing ligand is a phosphine, a monophosphite, a bisphosphite, or a mixture thereof.
14. The method according to any one of claims 1 to 10, wherein the total gas pressure after the gas exchange is 1 to 70 bar.
15. The method according to claim 14, wherein the total gas pressure after the gas exchange is 2 to 30 bar.
16. The method according to claim 14, wherein the total gas pressure after the gas exchange is 4 to 20 bar.
17. The method according to any one of claims 1 to 10, wherein the membrane separation is performed at a transmembrane pressure of 5 to 100 bar.
18. The method according to claim 17, wherein the membrane separation is performed at a transmembrane pressure of 10 to 80 bar.
19. The method according to claim 17, wherein the membrane separation is performed at a transmembrane pressure of 20 to 50 bar.
20. The method according to any one of claims 1 to 10, wherein the membrane separation is performed at a temperature of 0°C to 200°C.
21. The method according to claim 20, wherein the membrane separation is performed at a temperature of 20°C to 160°C.
22. The method according to any one of claims 1 to 10, wherein at least one thermal separation is performed before or after the membrane separation.
23. The method according to claim 22, wherein the thermal separation comprises at least one thermal separation method selected from thin film evaporation, distillation, falling film evaporation and short path evaporation.
24. The method of claim 22, wherein the thermal separation occurs before the membrane separation, but the gas exchange occurs after the thermal separation and before the membrane separation.
25. The method according to any one of claims 1 to 10, wherein the method is carried out continuously.
26. The process of any one of claims 1 to 10, wherein the reaction zone comprises at least one reactor.
27. The method according to any one of claims 1 to 10, wherein the membrane separation uses a membrane material selected from the group consisting of polydimethylsiloxane, polyimide, partially fluorinated polymer, fully fluorinated polymer, block copolymers of the above materials, polyaryletherketone, polybenzimidazole and polyether.
28. The method according to any one of claims 1 to 10, wherein the membrane separation uses a membrane material selected from the group consisting of polymers having intrinsic microporosity.
29. The method according to any one of claims 1 to 10, wherein the membrane separation uses a membrane material selected from the group consisting of amorphous fluoropolymers.
30. The method according to any one of claims 1 to 10, wherein the membrane separation uses a membrane material selected from the group consisting of an amorphous or partially crystalline perfluoroalkoxy polymer.
31. The method of claim 27, wherein the polyaryletherketone is selected from the group consisting of polyetheretherketone and polyetherketoneketone.
32. The method of claim 29, wherein the amorphous fluoropolymer is Cytop.
33. The method of claim 30, wherein the amorphous or partially crystalline perfluoroalkoxy polymer is Hyflon.
34. The process according to claim 22, wherein the membrane material used is intrinsically stable in the reaction output / in the mixture present after the thermal separation, ie it does not require any additional cross-linking of the polymer chains.