Lithium-ion battery modeling method and device

By obtaining the three-dimensional spatial structure of the negative electrode material particles of lithium-ion battery and determining their size and shape distribution, a negative electrode lithium-ion weighted solid phase diffusion equation was established, which solved the problem of neglecting the shape of the negative electrode material in the single-particle model and improved the lithium-ion battery Model accuracy and performance prediction capabilities.

CN114139429BActive Publication Date: 2024-11-12CHINA AVIATION LITHIUM BATTERY RES INST CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202111438230.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-11-29
Publication Date
2024-11-12
Estimated Expiration
2041-11-29

AI Technical Summary

Technical Problem

In the existing lithium-ion battery modeling method, the single-particle model ignores the diffusion of lithium ions in solution, and the graphite sheet layer structure of the negative electrode material is not accurate enough, resulting in the low accuracy of the lithium-ion battery model.

Method used

By obtaining the three-dimensional spatial structure of multiple material particles in the negative electrode sheet of the lithium-ion battery, determining their size distribution and shape distribution, and establishing the negative electrode lithium-ion weighted solid phase diffusion equation, thereby building a more accurate lithium-ion battery model.

Benefits of technology

The accuracy of the lithium-ion battery model is improved, making the negative electrode material particles in the model closer to the actual morphology, and enhancing the predictive ability of lithium-ion battery performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114139429B_ABST
    Figure CN114139429B_ABST
Patent Text Reader

Abstract

The present invention provides a lithium-ion battery modeling method and device, the method comprising: obtaining the three-dimensional spatial structure of multiple material particles of the negative electrode plate of the lithium-ion battery; determining the size distribution and / or shape distribution of the multiple material particles according to the three-dimensional spatial structure of the multiple material particles; determining the weighted solid-phase diffusion equation of negative-electrode lithium ions in the lithium-ion battery according to the size distribution and / or shape distribution of the multiple material particles; and establishing a lithium-ion battery model according to the weighted solid-phase diffusion equation of negative-electrode lithium ions in the lithium-ion battery. By taking the size distribution and / or shape distribution of the negative-electrode material particles of the lithium-ion battery into consideration when establishing the model, the simplified negative-electrode material particles in the model are closer to the actual negative-electrode material particles, rather than the single spherical shape in the prior art, thereby improving the accuracy of the established lithium-ion battery model.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of battery technology, and in particular to a lithium-ion battery modeling method and device. Background Art

[0002] With the development of science and technology, lithium-ion batteries are widely used in various fields such as spacecraft, electric vehicles, and portable electronic devices due to their advantages such as small size, light weight, high energy density, and long life. In order to improve battery performance, lithium-ion battery modeling analysis is usually performed before lithium-ion battery manufacturing. Therefore, it is becoming increasingly important to improve the accuracy of the established lithium-ion battery model.

[0003] In the prior art, a simplified electrochemical model, namely the single particle (SP) model, is generally used to simulate lithium-ion batteries. The single particle model ignores the diffusion of lithium ions in the solution and focuses on the impact of solid-phase diffusion on the performance of lithium batteries. The existing single particle model simply considers both positive and negative electrode particles as a single sphere, which is more applicable to positive electrode materials. However, since the graphite of negative electrode materials has a lamellar structure, most negative electrode material particles deviate from the spherical shape. Therefore, for negative electrode materials, simplifying the material particles into a single sphere is not applicable, resulting in the low accuracy of the established lithium-ion battery model. Summary of the invention

[0004] An object of the present invention is to provide a lithium ion battery modeling method capable of improving the accuracy of the established lithium ion battery model.

[0005] To achieve the above object, the present invention provides a lithium ion battery modeling method, which comprises:

[0006] Obtaining the three-dimensional spatial structure of multiple material particles of the negative electrode plate of the lithium-ion battery;

[0007] Determining a size distribution and / or a shape distribution of the plurality of material particles according to the three-dimensional spatial structure of the plurality of material particles;

[0008] Determining a weighted solid phase diffusion equation of negative electrode lithium ions in a lithium ion battery according to a size distribution and / or a shape distribution of a plurality of material particles;

[0009] A lithium-ion battery model is established according to the negative electrode lithium ion weighted solid phase diffusion equation.

[0010] By obtaining the three-dimensional spatial structure of multiple material particles of the negative electrode plate of the lithium-ion battery; determining the size distribution and / or shape distribution of the multiple material particles according to the three-dimensional spatial structure of the multiple material particles; determining the weighted solid-phase diffusion equation of negative electrode lithium ions in the lithium-ion battery according to the size distribution and / or shape distribution of the multiple material particles; and establishing a lithium-ion battery model according to the above-mentioned weighted solid-phase diffusion equation of negative electrode lithium ions. By taking the size distribution and / or shape distribution of the negative electrode material particles of the lithium-ion battery into account when establishing the model, the simplified negative electrode material particles in the model are closer to the actual negative electrode material particles, rather than the single spherical shape in the prior art, thereby improving the accuracy of the established lithium-ion battery model.

[0011] Another object of the present invention is to provide a lithium ion battery modeling device capable of improving the accuracy of the established lithium ion battery model.

[0012] To achieve the above object, the present invention also provides a lithium ion battery modeling device, which comprises:

[0013] A spatial structure acquisition module, used to acquire the three-dimensional spatial structure of multiple material particles of the negative electrode plate of the lithium-ion battery;

[0014] A particle distribution determination module, used to determine the size distribution and / or shape distribution of the plurality of material particles according to the three-dimensional spatial structure of the plurality of material particles;

[0015] A solid phase diffusion determination module, used to determine a weighted solid phase diffusion equation of negative electrode lithium ions in a lithium ion battery according to a size distribution and / or a shape distribution of a plurality of material particles;

[0016] The model building module is used to build a lithium-ion battery model based on the weighted solid phase diffusion equation of negative electrode lithium ions in the lithium-ion battery.

[0017] The three-dimensional spatial structure of multiple material particles of the negative electrode sheet of the lithium-ion battery is obtained by setting a spatial structure acquisition module; a particle distribution determination module is set to determine the size distribution and / or shape distribution of multiple material particles according to the three-dimensional spatial structure of multiple material particles; a solid phase diffusion determination module is set to determine the weighted solid phase diffusion equation of negative electrode lithium ions in the lithium-ion battery according to the size distribution and / or shape distribution of multiple material particles; a model construction module is set to establish a lithium-ion battery model according to the weighted solid phase diffusion equation of negative electrode lithium ions in the lithium-ion battery. When establishing the model, the size distribution and / or shape distribution of the negative electrode material particles of the lithium-ion battery are taken into account, so that the simplified negative electrode material particles in the model are closer to the actual negative electrode material particles, rather than the single sphere in the prior art, thereby improving the accuracy of the established lithium-ion battery model.

[0018] Another object of the present invention is to provide a computer device capable of improving the accuracy of the established lithium-ion battery model.

[0019] To achieve the above objectives, an embodiment of the present invention further provides a computer device, comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor implements the above lithium-ion battery modeling method when executing the computer program.

[0020] From the above description, it can be known that the computer device provided by the embodiment of the present invention obtains the three-dimensional spatial structure of multiple material particles of the negative electrode plate of the lithium-ion battery; determines the size distribution and / or shape distribution of the multiple material particles according to the three-dimensional spatial structure of the multiple material particles; determines the weighted solid-phase diffusion equation of negative electrode lithium ions in the lithium-ion battery according to the size distribution and / or shape distribution of the multiple material particles; and establishes a lithium-ion battery model according to the above-mentioned weighted solid-phase diffusion equation of negative electrode lithium ions. By taking into account the size distribution and / or shape distribution of the negative electrode material particles of the lithium-ion battery when establishing the model, the simplified negative electrode material particles in the model are closer to the actual negative electrode material particles, rather than the single sphere in the prior art, thereby improving the accuracy of the established lithium-ion battery model.

[0021] Another object of the present invention is to provide a computer-readable storage medium capable of improving the accuracy of an established lithium-ion battery model.

[0022] To achieve the above object, an embodiment of the present invention further provides a computer-readable storage medium, wherein the computer-readable storage medium stores a computer program for executing the above lithium-ion battery modeling method.

[0023] The computer-readable storage medium provided by the embodiment of the present invention obtains the three-dimensional spatial structure of multiple material particles of the negative electrode plate of the lithium-ion battery; determines the size distribution and / or shape distribution of the multiple material particles according to the three-dimensional spatial structure of the multiple material particles; determines the weighted solid-phase diffusion equation of negative electrode lithium ions in the lithium-ion battery according to the size distribution and / or shape distribution of the multiple material particles; and establishes a lithium-ion battery model according to the above-mentioned weighted solid-phase diffusion equation of negative electrode lithium ions. By taking into account the size distribution and / or shape distribution of the negative electrode material particles of the lithium-ion battery when establishing the model, the simplified negative electrode material particles in the model are closer to the actual negative electrode material particles, rather than the single sphere in the prior art, thereby improving the accuracy of the established lithium-ion battery model. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] The following drawings are intended only to illustrate and explain the present invention, and are not intended to limit the scope of the present invention.

[0025] Figure 1This is a schematic diagram of the positive and negative electrode material particles in the traditional single particle model of lithium-ion batteries;

[0026] Figure 2 This is a schematic diagram of the true morphology of the negative electrode material particles of lithium-ion batteries;

[0027] Figure 3 is a schematic diagram of a lithium-ion battery modeling method in an embodiment of the present invention;

[0028] Figure 4 is a schematic diagram of a process for determining the size distribution of multiple material particles in a specific embodiment of the present invention;

[0029] Figure 5 is a schematic diagram of a process for determining shape distribution of multiple material particles in yet another specific embodiment of the present invention;

[0030] Figure 6 is an example diagram of the histogram distribution of the sphericity of the negative electrode material particles in a specific example of the present invention;

[0031] Figure 7 is a schematic diagram of 25 negative electrode material particles of different shapes and volumes in a specific example of the present invention;

[0032] Figure 8 is a schematic diagram of the implementation process of step 304 in a specific embodiment of the present invention;

[0033] Fig. 9 is a schematic diagram of volume histogram distribution of negative electrode material particles in a specific example of the present invention;

[0034] Fig.10 is a graph showing the relationship between battery voltage and time obtained by simulation in a specific example of the present invention;

[0035] Fig.11 is a schematic structural diagram of a lithium-ion battery modeling device according to an embodiment of the present invention;

[0036] Fig.12 is a schematic diagram of the structure of the particle distribution determination module 1102 in a specific embodiment of the present invention;

[0037] Fig.13 It is a structural schematic diagram of a computer device in an embodiment of the present invention. DETAILED DESCRIPTION

[0038] The present application is further described in detail below through the accompanying drawings and examples. Through these descriptions, the characteristics and advantages of the present application will become clearer and more specific. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0039] The word "exemplary" is used exclusively herein to mean "serving as an example, embodiment, or illustration." Any embodiment described herein as "exemplary" is not necessarily to be construed as preferred or advantageous over other embodiments. Although various aspects of the embodiments are shown in the drawings, the drawings are not necessarily drawn to scale unless otherwise noted.

[0040] In addition, the technical features involved in different embodiments of the present application described below can be combined with each other as long as they do not conflict with each other.

[0041] like Figure 1 FIG. 1 shows a conventional single particle model, which includes, from left to right: negative electrode current collector 101, negative electrode material particles 102, separator 103, positive electrode material particles 104, and positive electrode current collector 105. It can be seen that the conventional single particle model treats the positive and negative electrode material particles as uniform spheres, while the inventors found that the positive electrode material particles are approximately spherical, and in FIG. Figure 2 In the electron microscope photograph shown, the negative electrode material particles are irregular in shape and are far from spherical. Therefore, the traditional single particle model is not applicable to the negative electrode material particles, resulting in the low accuracy of the lithium-ion battery model established based on the traditional single particle model.

[0042] In order to improve the accuracy of the established lithium-ion battery model, an embodiment of the present invention provides a lithium-ion battery modeling method, such as Figure 3 As shown, including:

[0043] Step 301: obtaining a three-dimensional spatial structure of a plurality of material particles of a negative electrode plate of a lithium-ion battery;

[0044] Step 302: determining the size distribution and / or shape distribution of the plurality of material particles according to the three-dimensional spatial structure of the plurality of material particles;

[0045] Step 303: determining a weighted solid phase diffusion equation of negative electrode lithium ions in a lithium ion battery according to the size distribution and / or shape distribution of the plurality of material particles;

[0046] Step 304: Establish a lithium-ion battery model based on the negative electrode lithium ion weighted solid phase diffusion equation.

[0047] From the above steps, it can be seen that by obtaining the three-dimensional spatial structure of multiple material particles of the negative electrode plate of the lithium-ion battery; determining the size distribution and / or shape distribution of the multiple material particles according to the three-dimensional spatial structure of the multiple material particles; determining the weighted solid-phase diffusion equation of negative electrode lithium ions in the lithium-ion battery according to the size distribution and / or shape distribution of the multiple material particles; and establishing a lithium-ion battery model according to the above weighted solid-phase diffusion equation of negative electrode lithium ions. By taking the size distribution and / or shape distribution of the negative electrode material particles of the lithium-ion battery into account when establishing the model, the simplified negative electrode material particles in the model are closer to the actual negative electrode material particles, rather than the single sphere in the prior art, thereby improving the accuracy of the established lithium-ion battery model.

[0048] First, the three-dimensional spatial structure of multiple material particles of the negative electrode sheet of the lithium-ion battery is obtained. In the specific implementation, the three-dimensional spatial structure of multiple material particles of the material used for the negative electrode sheet of the ion battery is obtained by using the focused ion beam FIB (Focused Ion Beam) three-dimensional imaging technology, that is, the three-dimensional structure of the material particles is extracted using the FIB technology. And because FIB has the advantage of more realistically reflecting the detailed morphology of the material surface, the three-dimensional spatial structure of the obtained multiple material particles has higher clarity, which can provide more accurate data for subsequent calculations, thereby helping to further improve the accuracy of the established lithium-ion battery model.

[0049] Specifically, since FIB three-dimensional imaging is performed on all material particles in the negative electrode plate to determine the spatial structure of all material particles, the amount of calculation is too large and the calculation process is complicated. In a specific embodiment, at least two or more representative material particles in the plate can be selected. Generally, under the premise of ensuring the accuracy of the final model, in order to reduce the amount of calculation as much as possible and improve the efficiency of modeling, the negative electrode plate is sampled, and FIB three-dimensional imaging is performed on the sampled samples to determine the spatial structure of the material particles in the sample. In specific implementation, the sampling size can be 100μm×100μm×100μm, or 50μm×50μm×50μm. The specific sampling size is determined according to the actual situation, and this application does not limit it here.

[0050] After obtaining the three-dimensional spatial structure of multiple material particles of the negative electrode sheet of the lithium-ion battery, the size distribution and / or shape distribution of the multiple material particles are determined according to the three-dimensional spatial structure of the multiple material particles. In specific implementation, the size distribution of the multiple material particles is determined according to the three-dimensional spatial structure of the multiple material particles, such as Figure 4 As shown, including:

[0051] Step 401: determining the volume of each material particle according to the three-dimensional spatial structure of the plurality of material particles;

[0052] Step 402: Counting the multiple material particles according to their volumes to obtain volume distribution of the multiple material particles;

[0053] Step 403: Determine the size distribution of the plurality of material particles according to the volume distribution of the plurality of material particles.

[0054] Specifically, in order to more intuitively obtain the volume distribution law and distribution of multiple material particles, the multiple material particles are counted according to their volumes to obtain the volume distribution of the multiple material particles, including:

[0055] Statistical analysis is performed on the volumes of the plurality of material particles to determine the grouping intervals of the volume histogram distribution, thereby obtaining volume histogram distribution data of the plurality of material particles including a plurality of volume groups.

[0056] By obtaining the above volume histogram distribution data, it is possible to intuitively obtain the volume distribution of multiple material particles in several groups of value ranges and the number of particles in each group of value ranges, thereby determining the different sizes of the multiple material particles.

[0057] In specific implementation, after using FIB technology to extract the three-dimensional structure of multiple negative electrode material particles, the volume of each negative electrode material particle can be obtained, and all material particles are counted according to the volume size, and the number of groups and the group interval of the histogram distribution are determined to obtain the volume histogram distribution of multiple material particles. Since the particle size is positively correlated with the volume, the volume can be used to characterize the size relationship of the particles. Therefore, the volume histogram distribution of multiple material particles is used as the size distribution of multiple material particles.

[0058] In specific implementation, the amount of calculation can be further reduced by determining the representative material particles of the group according to the median of the volume of each group in the volume histogram distribution data of multiple material particles; integrating the representative material particles of all groups as the size distribution of multiple material particles. That is, it is equivalent to normalizing all the material particles in a group to the particle size represented by the median of the volume of the group. Since the volume values ​​in a group are not much different, this simplification is reasonable and will not have a great impact on the final modeling results, but it can greatly simplify the calculations in the modeling process.

[0059] After determining the size distribution of multiple material particles, the weighted solid phase diffusion equation of negative electrode lithium ions in the lithium ion battery can be determined according to the size distribution of the multiple material particles, and a lithium ion battery model can be established according to the weighted solid phase diffusion equation of negative electrode lithium ions.

[0060] In another specific embodiment, similarly, determining the shape distribution of the plurality of material particles according to the three-dimensional spatial structure of the plurality of material particles includes:

[0061] Determine the sphericity of each material particle according to the three-dimensional spatial structure of the plurality of material particles;

[0062] Counting multiple material particles according to sphericity to obtain sphericity distribution of the multiple material particles;

[0063] The shape distribution of the plurality of material particles is determined according to the sphericity distribution of the plurality of material particles.

[0064] The volume shape of material particles is very irregular, and it is impossible to count the distribution of different particle shapes. Therefore, in order to count the distribution of material particles with different shapes, the circumscribed sphere is taken for particles with different shapes. According to the sphericity, material particles with different shapes can be classified to determine the shape distribution of multiple material particles.

[0065] In specific implementation, the sphericity of each material particle is determined according to the following formula:

[0066] S=V a / V b

[0067] Where S represents the sphericity of a material particle; V a Indicates the volume of the material particles; V b Represents the volume of the sphere circumscribing the material particle.

[0068] After extracting the three-dimensional structure of multiple negative electrode material particles using FIB technology, not only the volume of each negative electrode material particle can be obtained, but also the volume of the circumscribed sphere of each negative electrode material particle can be obtained. Then, using the above formula, the sphericity of each negative electrode material particle can be obtained. The sphericity distribution of multiple material particles is used as the shape distribution of multiple material particles.

[0069] After determining the shape distribution of multiple material particles, the weighted solid phase diffusion equation of negative electrode lithium ions in the lithium ion battery can be determined according to the shape distribution of the multiple material particles, and a lithium ion battery model can be established according to the weighted solid phase diffusion equation of negative electrode lithium ions.

[0070] Since the shapes of negative electrode material particles are different, even if the volume of the particles is the same, the particle shapes are likely to be different. In a specific embodiment, the size distribution of multiple material particles can be considered alone, or the shape distribution of multiple material particles can be considered alone. However, in order to be more precise and maximize the accuracy of the constructed model, the optimal embodiment chooses to consider the size distribution and shape distribution of multiple material particles, that is, when determining to construct a lithium-ion battery model, the size distribution and shape distribution of the material particles are considered at the same time.

[0071] In another specific embodiment of the present invention, when determining the size distribution and shape distribution of the plurality of material particles according to the three-dimensional spatial structure of the plurality of material particles, after determining the size distribution according to the steps shown in steps 401 to 403, Figure 5 The steps shown determine the shape distribution and include:

[0072] Step 501: determining the sphericity of each material particle in each volume group according to the three-dimensional spatial structure of a plurality of material particles;

[0073] Step 502: Counting the material particles in each volume group according to the sphericity to obtain the sphericity distribution corresponding to the multiple volume groups;

[0074] Step 503: Determine the shape distribution of multiple material particles according to the above sphericity distribution.

[0075] The specific implementation process of step 502 includes:

[0076] The sphericity of the material particles in each volume group is counted, and the group interval of the sphericity histogram distribution of the material particles corresponding to each volume group is determined to obtain the sphericity histogram distribution data corresponding to each volume group;

[0077] The sphericity histogram distribution data corresponding to each volume grouping is integrated to obtain the sphericity histogram distribution data corresponding to multiple volume groupings.

[0078] In specific implementation, the amount of calculation can be further reduced by determining the representative material particles of the sphericity grouping according to the median sphericity of each grouping in the above-mentioned sphericity histogram distribution data, and integrating the representative sphericity particles as the size distribution of multiple material particles. That is, it is equivalent to normalizing all the material particles in a grouping to the particle size represented by the median sphericity of the grouping. Since the sphericity values ​​in a grouping are not much different, this simplification is reasonable and will not have a great impact on the final modeling results, but it can greatly simplify the calculations in the modeling process.

[0079] Accordingly, the specific implementation process of step 503 includes:

[0080] In the sphericity histogram distribution data corresponding to each volume grouping, a representative material particle of each sphericity grouping corresponding to the volume grouping is determined according to the sphericity medians of multiple sphericity groups corresponding to the volume grouping;

[0081] The representative material particles of each group of sphericity corresponding to all volume groups are integrated to obtain the shape distribution of the plurality of material particles.

[0082] In a specific implementation, for multiple groups of volume histogram distribution of multiple material particles, for example, volume distribution groups 1-5, after determining the sphericity of each material particle in each volume group, the sphericity of the material particles in each volume group is statistically analyzed to determine the group interval of the sphericity histogram distribution of the material particles corresponding to each volume group, and obtain the sphericity histogram distribution data corresponding to each volume group. In the sphericity histogram distribution data corresponding to each volume group, the representative material particles of each sphericity group corresponding to the volume group are determined according to the sphericity median of multiple groups of sphericity corresponding to the volume group; the representative material particles of each group of sphericity corresponding to all volume groups are integrated to obtain the shape distribution of multiple material particles.

[0083] For example, the sphericity of 68 material particles in volume distribution group 1 is determined, and the 68 material particles are counted according to the sphericity, and the group interval of the sphericity histogram distribution is determined to obtain the sphericity histogram distribution of the 68 material particles, including sphericity groups 1 to 4. The medians of the sphericity of sphericity group 1, sphericity group 2, sphericity group 3, and sphericity group 4 are taken as representative particles of sphericity groups 1 to 4, and the representative particles of the sphericity corresponding to volume distribution group 1 can be obtained by integration. Similarly, the representative particles of the sphericity corresponding to volume distribution groups 2 to 5 can be obtained respectively, and the shape distribution of multiple material particles can be obtained by sorting.

[0084] For example Figure 6 This is a histogram of the number of particles with different sphericity corresponding to a certain volume group obtained in a specific example of the present invention. This figure classifies the material particles of different shapes that cannot be counted by sphericity to obtain the number of particles with different sphericity (essentially the distribution of particles of different shapes).

[0085] After determining the size distribution and shape distribution of the plurality of material particles, the weighted solid phase diffusion equation of the negative electrode lithium ions in the lithium ion battery is determined according to the size distribution and shape distribution of the plurality of material particles. Specifically, the weighted solid phase diffusion equation of the negative electrode lithium ions in the lithium ion battery is determined as:

[0086]

[0087] The boundary conditions are:

[0088]

[0089] Among them, c so,n Indicates the lithium ion concentration in the negative electrode material particles, mol / m 3 ;D so,n represents the negative electrode solid phase diffusion coefficient, m 2 / s; t represents the discharge time, s; x represents the coordinate of the x-axis in the spatial coordinate system xyz, m; y represents the coordinate of the y-axis in the spatial coordinate system xyz, m; z represents the coordinate of the z-axis in the spatial coordinate system xyz, m; N represents the number of volume distribution groups; M represents the number of sphericity distribution groups; α i represents the frequency of the i-th volume distribution group in the volume histogram distribution; β i,j represents the frequency of the jth sphericity distribution group corresponding to the i-th volume distribution group in the sphericity histogram distribution; c so,n | (x,y,z)on surface Represents the solid phase concentration at the coordinate (x, y, z) on the surface of the negative electrode of the lithium battery, mol / m 3 ;j n represents the negative electrode ion current density, mol×m -2 ×s -1 .

[0090] The spatial coordinate system xyz is a reference for describing the space inside the lithium-ion battery for the convenience of calculation. There is no restriction when setting it, but in order to make it simple and quick to set up, the long axis direction of the material particles is generally selected as the x-axis direction, the short axis direction of the material particles is selected as the y-axis direction, and the direction perpendicular to these two directions is the z-axis direction.

[0091] like Figure 7 Shown are 25 different shapes and volumes of negative electrode material particles obtained by considering size distribution and shape distribution in a specific example of the present invention, i represents the volume distribution group number, j represents the sphericity distribution group number, i.e. 5 sizes and 5 shape types, there are 25 situations after combining.

[0092] In particular, if the weighted solid phase diffusion equation of negative electrode lithium ions in lithium-ion batteries is determined based only on the size distribution of multiple material particles, it is only necessary to replace the β i,j The value of can be 1, that is, it is assumed that all material particles have the same shape. If the weighted solid phase diffusion equation of negative electrode lithium ions in lithium-ion batteries is determined based only on the shape distribution of multiple material particles, it is only necessary to replace α in the above formula i The value of can be 1, which means that the size of all material particles is the same by default.

[0093] The traditional single-particle model combines the solid-phase diffusion equation of positive lithium ions and the solid-phase diffusion equation of negative lithium ions in lithium-ion batteries to obtain the solid-phase diffusion equation of lithium ions in lithium-ion batteries. Since the lithium-ion single-particle model is used to describe the mechanism reaction process and physical properties in lithium-ion batteries, the lithium-ion single-particle model includes the lithium-ion solid-phase diffusion equation, the Butler-Volmer kinetic equation and the terminal voltage expression. In the embodiment of the present application, a weighted solid-phase diffusion equation of negative lithium ions is established. Therefore, by combining the established weighted solid-phase diffusion equation of positive lithium ions, the solid-phase diffusion equation of positive lithium ions in the above-mentioned lithium-ion battery, the Butler-Volmer kinetic equation and the terminal voltage expression, a more accurate battery single-particle model can be established as the lithium-ion battery model in the specific embodiment of the present invention.

[0094] In the embodiment of the present invention, after the weighted solid-phase diffusion equation of the negative electrode lithium ions in the lithium-ion battery is determined, a lithium-ion battery model is established according to the weighted solid-phase diffusion equation of the negative electrode lithium ions. The specific process is as follows: Figure 8 As shown, including:

[0095] Step 801: Determine the solid phase diffusion equation of positive electrode lithium ions in a lithium ion battery;

[0096] Step 802: Establishing the Butler-Volmer kinetic equation and terminal voltage expression;

[0097] Step 803: According to the Butler-Volmer kinetic equation, the terminal voltage expression, the positive electrode lithium ion solid phase diffusion equation and the above-mentioned negative electrode lithium ion weighted solid phase diffusion equation, a single particle model of the lithium ion battery is established to obtain a lithium ion battery model.

[0098] After constructing the weighted solid-phase diffusion equation of negative electrode lithium ions in lithium-ion batteries, the solid-phase diffusion equation of positive electrode lithium ions in lithium-ion batteries is determined as follows:

[0099]

[0100] The boundary conditions are:

[0101]

[0102]

[0103] Among them, c so,p Indicates the lithium ion concentration in the positive electrode material particles, mol / m 3 ;D so,p represents the positive electrode solid phase diffusion coefficient, m 2 / s; t represents the discharge time, s; r represents the distance from any point in the particle to the center of the sphere, m; R so,p represents the radius of the positive electrode solid phase particle, m; jp represents the positive electrode ion current density, mol×m -2 ×s -1 .

[0104] The reactive ion current density at the boundary of the positive and negative current collectors is calculated according to the following formula:

[0105]

[0106]

[0107] Where I represents current, A; R so,p Represents the average size of positive electrode particles, m; R so,n represents the average size of negative electrode particles, m; F represents the Faraday constant, C / mol; Vcell represents the battery volume, m 3 ; εpj represents the volume fraction of the positive electrode sheet; εp represents the volume fraction of the positive electrode active material; εnj represents the volume fraction of the negative electrode sheet; εn represents the volume fraction of the negative electrode active material.

[0108] In a specific embodiment of the present invention, the Butler-Volmor kinetic equation is used to express the relationship between the reaction overpotential and the ion current density, and the Butler-Volmor kinetic equation is established as:

[0109]

[0110]

[0111] Among them, k p Indicates the positive electrode reaction rate, m / s; c so,p,max Indicates the maximum lithium ion concentration in the positive electrode solid phase, mol / m 3 ;c so,p,surf Indicates the lithium ion concentration on the positive electrode solid surface, mol / m 3 ;c p Indicates the lithium ion concentration in the positive electrode area, mol / m 3 ; R represents the ideal gas constant: 8.314 J×mol -1 ×K -1 ; T represents temperature, K; η p represents the positive electrode overpotential, V; k n Indicates the negative electrode reaction rate, m / s; c so,n,max Indicates the maximum lithium ion concentration in the negative electrode solid phase, mol / m 3 ;c so,n,surf Indicates the lithium ion concentration on the negative electrode solid surface, mol / m 3 ;c n Indicates the lithium ion concentration in the negative electrode area, mol / m 3 ; η nRepresents the negative electrode overpotential, V.

[0112] The expression of terminal voltage V is established as:

[0113] V=E-η p -η n -Rsol×I×A

[0114] Where E represents the open circuit potential, V; Rsol represents the liquid phase resistance, Ω; A represents the battery electrode area, m 2 ; I represents current, A; η p represents the positive electrode overpotential, V; η n Represents the negative electrode overpotential, V.

[0115] The open circuit potential E in the formula is:

[0116] Among them, E p Represents the OCV (Open Circuit Voltage) ~ SOC (state of charge) curve of the positive electrode material; E n Represents the OCV~SOC curve of the negative electrode material; c so,p,surf Indicates the lithium ion concentration on the positive electrode surface, mol / m 3 ;c so,n,surf Indicates the lithium ion concentration on the negative electrode surface, mol / m 3 ;c so,p,max Indicates the maximum lithium ion concentration of the positive electrode, mol / m 3 ;c so,n,max Indicates the maximum lithium ion concentration of the negative electrode, mol / m 3 .

[0117] Lithium ion concentration on the negative electrode surface c so,n,surf Solve according to the following formula:

[0118] c so,n,surf,i,j represents the lithium ion concentration on the negative electrode surface of the representative material particle corresponding to the i-th row and the j-th column, mol / m 3 .

[0119] From the above process, it can be seen that by taking the size distribution, shape distribution, or size distribution and shape distribution of the negative electrode material particles into consideration in the simplification of the negative electrode material particles, and establishing the corresponding negative electrode lithium ion weighted solid phase diffusion equation, the final constructed battery single particle model is more in line with the actual lithium ion battery, thereby improving the accuracy of the established lithium ion battery model.

[0120] In a specific embodiment of the present invention, based on the single particle model established above, the single particle model can also be used to perform simulation calculations of lithium-ion batteries, so as to predict the performance data of the lithium-ion battery, thereby determining the performance of the lithium-ion battery and further applying it to guide industrial production.

[0121] In order to better illustrate how the lithium-ion battery modeling method provided by the embodiment of the present invention is applied to actual industrial production, the following specific example is provided:

[0122] When conducting industrial production of lithium-ion batteries, the materials of the positive and negative electrodes affect the performance of the final manufactured battery. Therefore, a small portion of the negative electrode material to be tested can be used to make electrode samples according to the electrode manufacturing process.

[0123] The FIB technology is used to extract the three-dimensional spatial structure of the electrode sample, obtain the three-dimensional spatial structure of the negative electrode material particles, and calculate the volume of multiple negative electrode material particles. According to the volume, the multiple negative electrode material particles are counted to obtain the volume histogram of multiple negative electrode material particles, such as Fig. 9 shown.

[0124] Furthermore, in order to simplify the calculation, when determining the shape distribution of multiple negative electrode material particles, based on Fig. 9 The data in the histogram shown in the figure are used to solve the corresponding circumscribed sphere volume for each material particle in each volume histogram distribution group, thereby calculating the corresponding sphericity. According to the sphericity of the material particles, the following is obtained: Figure 6 shown Fig. 9 Histogram of the sphericity of material particles corresponding to a certain volume grouping in .

[0125] The volume median of each group in the volume histogram is selected as the volume value of the representative particle of the group, and the sphericity median of each group in the sphericity histogram is selected as the sphericity value of the representative particle of the group. After the combination, there are as follows Figure 7 The 25 negative electrode material particles shown.

[0126] Based on the above 25 kinds of negative electrode material particles, the weighted solid phase diffusion equation of negative electrode lithium ions in lithium-ion batteries is constructed. Combined with the solid phase diffusion equation of positive electrode lithium ions in ion batteries, the Butler-Volmer kinetic equation and the terminal voltage expression, a single particle model of a lithium-ion battery with the above-mentioned electrode samples as the negative electrode is established.

[0127] Then, based on the single particle model established above, the battery performance of the lithium-ion battery with the above-mentioned pole piece sample as the negative electrode can be simulated using the Comsol software. Specifically, the single particle model established above is imported into the Comsol software in the form of a PDE custom equation in Comsol, and the relevant parameters required for simulation such as porosity, diffusion coefficient, positive and negative electrode OCV curves, reaction rate constant, etc. are input into the Comsol software. Among them, the above-mentioned relevant parameters can be set manually, or in order to improve the simulation accuracy, actual experiments can be conducted on the lithium-ion battery with the above-mentioned pole piece sample as the negative electrode to measure the required relevant parameters.

[0128] In the COMSOL software, the simulation calculation of lithium-ion battery performance is carried out through the process of defining solution type - drawing - defining material properties of each solution domain - setting loads and boundary conditions - mesh part - solving model - post-processing and reporting results - modification and optimization. It can predict the lithium ion concentration distribution in solid particles, positive and negative electrode potential curves and Fig.10 The battery charge and discharge curve is shown. Based on the prediction results, the performance data of the lithium-ion battery with the above-mentioned electrode sample as the negative electrode is analyzed, so that the structure-activity relationship between the microscopic morphology of the negative electrode material particles and the battery performance can be constructed for artificial regulation, thereby guiding the actual battery manufacturing.

[0129] For example, the performance data of lithium-ion batteries with the above-mentioned pole piece samples as negative electrodes can be compared with the expected performance standards. If the expected performance standards are met, it is considered that the negative electrode material can be used to actually produce lithium batteries; if not, replace the new negative electrode material, remake the pole piece, re-establish the corresponding lithium-ion battery model, and re-simulate. It can be used for material selection during actual battery manufacturing. Before actual manufacturing, it can be determined whether this batch of materials can produce lithium-ion batteries with the expected effect. This not only prevents material waste and saves manufacturing costs, but also avoids the process of re-manufacturing and improves industrial production efficiency. At the same time, according to the simulation results, it can be decided whether to optimize and debug battery devices when manufacturing batteries, which greatly reduces the trial and error costs in the development of lithium batteries and shortens the development cycle.

[0130] In addition, it can also be used to find high-quality battery manufacturing materials. The more uniform the material, the better the consistency of the charge and discharge performance of each particle. However, the gaps between particles are relatively large. For example, if stones are piled up, sand can be filled into the gaps. Therefore, the capacity of lithium batteries can be increased by using non-uniform materials. At the same time, the charge and discharge performance of each particle of non-uniform materials is different, and some particles may have side reactions. Therefore, there must be a compromise solution. The lithium-ion battery model provided by the embodiment of the present invention can be used in conjunction with the physical model of geometric stacking to find this compromise solution, so that the battery capacity is as large as possible without side reactions and without affecting the battery life.

[0131] The implementation of the above specific application is only an example, and the remaining implementation methods will not be described in detail one by one.

[0132] Based on the same inventive concept, the embodiment of the present invention also provides a lithium-ion battery modeling device. Since the principle of the problem solved by the lithium-ion battery modeling device is similar to that of the lithium-ion battery modeling method, the implementation of the lithium-ion battery modeling device can refer to the implementation of the lithium-ion battery modeling method, and the repeated parts will not be repeated. The specific structure is as follows: Fig.11 As shown:

[0133] A spatial structure acquisition module 1101 is used to acquire a three-dimensional spatial structure of a plurality of material particles of a negative electrode plate of a lithium-ion battery;

[0134] A particle distribution determination module 1102 is used to determine the size distribution and / or shape distribution of the plurality of material particles according to the three-dimensional spatial structure of the plurality of material particles;

[0135] A solid phase diffusion determination module 1103 is used to determine a weighted solid phase diffusion equation of negative electrode lithium ions in a lithium ion battery according to a size distribution and / or a shape distribution of a plurality of material particles;

[0136] The model building module 1104 is used to build a lithium-ion battery model according to the weighted solid-phase diffusion equation of negative electrode lithium ions in the lithium-ion battery.

[0137] The three-dimensional spatial structure of multiple material particles of the negative electrode sheet of the lithium-ion battery is obtained by setting a spatial structure acquisition module 1101; a particle distribution determination module 1102 is set to determine the size distribution and / or shape distribution of multiple material particles according to the three-dimensional spatial structure of multiple material particles; a solid phase diffusion determination module 1103 is set to determine the weighted solid phase diffusion equation of negative electrode lithium ions in the lithium-ion battery according to the size distribution and / or shape distribution of multiple material particles; a model construction module 1104 is set to establish a lithium-ion battery model according to the weighted solid phase diffusion equation of negative electrode lithium ions in the lithium-ion battery. When establishing the model, the size distribution and / or shape distribution of the negative electrode material particles of the lithium-ion battery are taken into account, so that the simplified negative electrode material particles in the model are closer to the actual negative electrode material particles, rather than the single sphere in the prior art, thereby improving the accuracy of the established lithium-ion battery model.

[0138] In specific implementation, the spatial structure acquisition module 1101 is specifically used for:

[0139] The three-dimensional spatial structure of multiple material particles used for the negative electrode plate of the ion battery is obtained by using focused ion beam three-dimensional imaging technology.

[0140] In a specific embodiment, the structure of the particle distribution determination module 1102 is as follows: Fig.12 As shown, specifically including:

[0141] The size distribution determination unit 1201 is used to:

[0142] According to the three-dimensional spatial structure of multiple material particles, the volume of each material particle is counted;

[0143] Counting the multiple material particles according to their volumes to obtain volume distribution of the multiple material particles;

[0144] A size distribution of the plurality of material particles is determined based on the volume distribution of the plurality of material particles.

[0145] The size distribution determination unit 1201 is specifically used to: perform statistical analysis on the volumes of multiple material particles, determine the grouping intervals of the volume histogram distribution, and obtain volume histogram distribution data of the multiple material particles including multiple volume groups.

[0146] The shape distribution determining unit 1202 is used to:

[0147] Determining the sphericity of each material particle in each volume grouping according to the three-dimensional spatial structure of the plurality of material particles;

[0148] Counting the material particles in each volume group according to the sphericity, and obtaining the sphericity distribution corresponding to the multiple volume groups;

[0149] Based on the sphericity distribution, the shape distribution of the plurality of material particles is determined.

[0150] Specifically, the sphericity of each material particle is determined according to the following formula:

[0151] S=V a / V b

[0152] Where S represents the sphericity of a material particle; V a Indicates the volume of the material particles; V b Represents the volume of the sphere circumscribing the material particle.

[0153] In a specific embodiment, the shape distribution determination unit 1402 is specifically used to: perform statistics on the sphericity of the material particles in each volume group, determine the group interval of the sphericity histogram distribution of the material particles corresponding to each volume group, and obtain the sphericity histogram distribution data corresponding to each volume group;

[0154] The sphericity histogram distribution data corresponding to each volume grouping is integrated to obtain the sphericity histogram distribution data corresponding to multiple volume groupings.

[0155] Accordingly, the shape distribution determining unit 1402 is specifically configured to:

[0156] In the sphericity histogram distribution data corresponding to each volume grouping, a representative material particle of each sphericity grouping corresponding to the volume grouping is determined according to the sphericity medians of multiple sphericity groups corresponding to the volume grouping;

[0157] The representative material particles of each group of sphericity corresponding to all volume groups are integrated to obtain the shape distribution of the plurality of material particles.

[0158] In a specific embodiment, the solid phase diffusion determination module 1103 is specifically used to:

[0159] According to the size distribution and shape distribution of multiple material particles, the weighted solid phase diffusion equation of negative electrode lithium ions in lithium-ion batteries is determined as follows:

[0160]

[0161] The boundary conditions are:

[0162]

[0163] Among them, c so,n Indicates the lithium ion concentration in the negative electrode material particles, mol / m 3 ;D so,n represents the negative electrode solid phase diffusion coefficient, m 2 / s; t represents the discharge time, s; x represents the coordinate of the x-axis in the spatial coordinate system xyz, m; y represents the coordinate of the y-axis in the spatial coordinate system xyz, m; z represents the coordinate of the z-axis in the spatial coordinate system xyz, m; N represents the number of volume distribution groups; M represents the number of sphericity distribution groups; α o represents the frequency of the i-th volume distribution group in the volume histogram distribution; β o,j represents the frequency of the jth sphericity distribution group corresponding to the i-th volume distribution group in the sphericity histogram distribution; c so,n | (x,y,z)on surface Represents the solid phase concentration at the coordinate (x, y, z) on the surface of the negative electrode of the lithium battery, mol / m 3 ;j n represents the negative electrode ion current density, mol×m -2 ×s -1 .

[0164] In a specific embodiment, the model building module 1104 is specifically used to:

[0165] Determine the solid phase diffusion equation of positive lithium ions in lithium-ion batteries;

[0166] Establish the Butler-Volmer kinetic equation and terminal voltage expression;

[0167] According to the Butler-Volmer kinetic equation, the terminal voltage expression, the positive electrode lithium ion solid phase diffusion equation and the above-mentioned negative electrode lithium ion weighted solid phase diffusion equation, a single particle model of the lithium ion battery is established to obtain a lithium ion battery model.

[0168] An embodiment of the present invention further provides a computer device, Fig.13 Schematic diagram of a computer device in an embodiment of the present invention. The computer device can implement all steps in the lithium-ion battery modeling method in the above embodiment. The computer device specifically includes the following contents:

[0169] Processor (processor) 1301, memory (memory) 1302, communication interface (CommunicationsInterface) 1303 and communication bus 1304;

[0170] The processor 1301, the memory 1302, and the communication interface 1303 communicate with each other through the communication bus 1304; the communication interface 1303 is used to realize information transmission between related devices;

[0171] The processor 1301 is used to call the computer program in the memory 1302, and the processor implements the lithium-ion battery modeling method in the above embodiment when executing the computer program.

[0172] An embodiment of the present invention further provides a computer-readable storage medium, wherein the computer-readable storage medium stores a computer program for executing the above-mentioned lithium-ion battery modeling method.

[0173] In summary, the lithium-ion battery modeling method and device provided by the embodiments of the present invention have the following advantages:

[0174] By obtaining the three-dimensional spatial structure of multiple material particles of the negative electrode plate of the lithium-ion battery; determining the size distribution and / or shape distribution of the multiple material particles according to the three-dimensional spatial structure of the multiple material particles; determining the weighted solid-phase diffusion equation of negative electrode lithium ions in the lithium-ion battery according to the size distribution and / or shape distribution of the multiple material particles; and establishing a lithium-ion battery model according to the above-mentioned weighted solid-phase diffusion equation of negative electrode lithium ions. By taking the size distribution and / or shape distribution of the negative electrode material particles of the lithium-ion battery into account when establishing the model, the simplified negative electrode material particles in the model are closer to the actual negative electrode material particles, rather than the single spherical shape in the prior art, thereby improving the accuracy of the established lithium-ion battery model.

[0175] Although the present invention provides method operation steps as described in the embodiments or flowcharts, more or fewer operation steps may be included based on conventional or non-creative labor. The order of steps listed in the embodiments is only one way of executing the order of many steps and does not represent the only execution order. When the actual device or client product is executed, it can be executed in sequence or in parallel according to the method shown in the embodiments or the drawings (for example, in a parallel processor or multi-threaded processing environment).

[0176] It should be understood by those skilled in the art that the embodiments of this specification may be provided as methods, devices (systems) or computer program products. Therefore, the embodiments of this specification may take the form of complete hardware embodiments, complete software embodiments or embodiments combining software and hardware. Moreover, the present invention may take the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program codes.

[0177] The present invention is described with reference to flowcharts and / or block diagrams of methods, apparatus (systems) and computer program products according to embodiments of the present invention. It should be understood that each process and / or block in the flowchart and / or block diagram, as well as a combination of processes and / or blocks in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor or other programmable data processing device to produce a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.

[0178] These computer program instructions may also be stored in a computer-readable memory capable of directing a computer or other programmable data processing device to operate in a specific manner, so that the instructions stored in the computer-readable memory produce an article of manufacture comprising an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.

[0179] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process. Figure 1 A process or multiple processes and / or boxes Figure 1 The steps for the functions specified in one or more boxes.

[0180] Each embodiment in this specification is described in a progressive manner, and the same and similar parts between the embodiments can be referred to each other, and each embodiment focuses on the differences from other embodiments. In particular, for the system embodiment, since it is basically similar to the method embodiment, the description is relatively simple, and the relevant parts can be referred to the partial description of the method embodiment. In this article, relational terms such as first and second are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply that there is any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such a process, method, article or device. The orientation or position relationship indicated by the terms "upper", "lower", etc. is based on the orientation or position relationship shown in the drawings, which is only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present invention. Unless otherwise expressly specified and limited, the terms "installed", "connected" and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be a connection between the two components. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to the specific circumstances. It should be noted that the embodiments of the present invention and the features in the embodiments can be combined with each other in the absence of conflict. The present invention is not limited to any single aspect, nor to any single embodiment, nor to any combination and / or permutation of these aspects and / or embodiments. Moreover, each aspect and / or embodiment of the present invention can be used alone or in combination with one or more other aspects and / or embodiments thereof.

[0181] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein by equivalents. These modifications or replacements do not make the essence of the corresponding technical solutions deviate from the scope of the technical solutions of the embodiments of the present invention, and they should all be included in the scope of the claims and specification of the present invention.

Claims

1. A lithium-ion battery modeling method, characterized in that: include: Obtaining the three-dimensional spatial structure of multiple material particles of the negative electrode plate of the lithium-ion battery; Determining a size distribution and / or a shape distribution of the plurality of material particles according to the three-dimensional spatial structure of the plurality of material particles; Determining a weighted solid phase diffusion equation of negative electrode lithium ions in a lithium ion battery according to a size distribution and / or a shape distribution of a plurality of material particles; Establishing a lithium-ion battery model according to the negative electrode lithium ion weighted solid phase diffusion equation; The step of determining the size distribution of the plurality of material particles according to the three-dimensional spatial structure of the plurality of material particles comprises: Determine the volume of each material particle according to the three-dimensional spatial structure of the plurality of material particles; Counting the multiple material particles according to their volumes to obtain volume distribution of the multiple material particles; Determining a size distribution of the plurality of material particles according to a volume distribution of the plurality of material particles; The step of determining the shape distribution of the plurality of material particles according to the three-dimensional spatial structure of the plurality of material particles comprises: Determine the sphericity of each material particle according to the three-dimensional spatial structure of the plurality of material particles; Counting multiple material particles according to sphericity to obtain sphericity distribution of the multiple material particles; determining a shape distribution of the plurality of material particles according to a sphericity distribution of the plurality of material particles; According to the size distribution and / or shape distribution of the plurality of material particles, the weighted solid phase diffusion equation of the negative electrode lithium ions in the lithium ion battery is determined as follows: The boundary conditions are: Among them, c so,n Indicates the lithium ion concentration in the negative electrode material particles; D so,n represents the negative electrode solid phase diffusion coefficient; t represents the discharge time; x represents the coordinate of the x-axis in the spatial coordinate system xyz; y represents the coordinate of the y-axis in the spatial coordinate system xyz; z represents the coordinate of the z-axis in the spatial coordinate system xyz; N represents the number of volume distribution groups; M represents the number of sphericity distribution groups; α i represents the frequency of the i-th volume distribution group in the volume histogram distribution; β i,j represents the frequency of the jth sphericity distribution group corresponding to the i-th volume distribution group in the sphericity histogram distribution; c so,n | (x,y,z)onsurface represents the solid phase concentration at the coordinate (x, y, z) on the surface of the negative electrode of the lithium battery; j n It represents the negative electrode ion current density.

2. The lithium-ion battery modeling method according to claim 1, characterized in that: The volume distribution of the multiple material particles is obtained by counting the multiple material particles according to their volumes, including: Statistical analysis is performed on the volumes of the plurality of material particles to determine the grouping intervals of the volume histogram distribution, thereby obtaining volume histogram distribution data of the plurality of material particles including a plurality of volume groups.

3. The lithium-ion battery modeling method according to claim 2, characterized in that: According to the three-dimensional spatial structure of the plurality of material particles, the shape distribution of the plurality of material particles is determined, including: Determining the sphericity of each material particle in each volume grouping according to the three-dimensional spatial structure of the plurality of material particles; Counting the material particles in each volume group according to the sphericity, and obtaining the sphericity distribution corresponding to the multiple volume groups; Based on the sphericity distribution, a shape distribution of a plurality of material particles is determined.

4. The lithium-ion battery modeling method according to claim 3, characterized in that: Determine the sphericity of each material particle according to the following formula: S=V a / V b Where S represents the sphericity of a material particle; V a Indicates the volume of the material particles; V b Represents the volume of the sphere circumscribing the material particle.

5. The lithium-ion battery modeling method according to claim 3, characterized in that: The material particles in each volume group are counted according to the sphericity to obtain the sphericity distribution corresponding to multiple volume groups, including: The sphericity of the material particles in each volume group is counted, and the group interval of the sphericity histogram distribution of the material particles corresponding to each volume group is determined to obtain the sphericity histogram distribution data corresponding to each volume group; The sphericity histogram distribution data corresponding to each volume grouping is integrated to obtain the sphericity histogram distribution data corresponding to multiple volume groupings.

6. The lithium-ion battery modeling method according to claim 5, characterized in that: Determining the shape distribution of a plurality of material particles according to the sphericity distribution includes: In the sphericity histogram distribution data corresponding to each volume grouping, a representative material particle of each sphericity grouping corresponding to the volume grouping is determined according to the sphericity medians of multiple sphericity groups corresponding to the volume grouping; The representative material particles of each group of sphericity corresponding to all volume groups are integrated to obtain the shape distribution of the plurality of material particles.

7. The lithium-ion battery modeling method according to claim 1, characterized in that: According to the negative electrode lithium ion weighted solid phase diffusion equation, a lithium ion battery model is established, including: Determine the solid phase diffusion equation of positive lithium ions in lithium-ion batteries; Establish the Butler-Volmer kinetic equation and terminal voltage expression; According to the Butler-Volmer kinetic equation, the terminal voltage expression, the positive electrode lithium ion solid phase diffusion equation and the negative electrode lithium ion weighted solid phase diffusion equation, a single particle model of the lithium ion battery is established to obtain a lithium ion battery model.

8. The lithium-ion battery modeling method according to claim 1, characterized in that: Obtain the three-dimensional spatial structure of multiple material particles of the negative electrode plate of the lithium-ion battery, including: The three-dimensional spatial structure of multiple material particles used for the negative electrode plate of the ion battery is obtained by using focused ion beam three-dimensional imaging technology.

9. A lithium-ion battery modeling device, characterized in that: include: A spatial structure acquisition module, used to acquire the three-dimensional spatial structure of multiple material particles of the negative electrode plate of the lithium-ion battery; A particle distribution determination module, used to determine the size distribution and / or shape distribution of the plurality of material particles according to the three-dimensional spatial structure of the plurality of material particles; A solid phase diffusion determination module, used to determine a weighted solid phase diffusion equation of negative electrode lithium ions in a lithium ion battery according to a size distribution and / or a shape distribution of a plurality of material particles; A model building module is used to build a lithium-ion battery model based on the weighted solid phase diffusion equation of negative electrode lithium ions in lithium-ion batteries; The particle distribution determination module is also used for: Determine the volume of each material particle according to the three-dimensional spatial structure of the plurality of material particles; Counting the multiple material particles according to their volumes to obtain volume distribution of the multiple material particles; Determining a size distribution of the plurality of material particles according to a volume distribution of the plurality of material particles; The particle distribution determination module is also used for: Determine the sphericity of each material particle according to the three-dimensional spatial structure of the plurality of material particles; Counting multiple material particles according to sphericity to obtain sphericity distribution of the multiple material particles; determining a shape distribution of the plurality of material particles according to a sphericity distribution of the plurality of material particles; The solid phase diffusion determination module is also used to determine the weighted solid phase diffusion equation of negative electrode lithium ions in the lithium ion battery according to the size distribution and / or shape distribution of multiple material particles: The boundary conditions are: Among them, c so,n Indicates the lithium ion concentration in the negative electrode material particles; D so,n represents the negative electrode solid phase diffusion coefficient; t represents the discharge time; x represents the coordinate of the x-axis in the spatial coordinate system xyz; y represents the coordinate of the y-axis in the spatial coordinate system xyz; z represents the coordinate of the z-axis in the spatial coordinate system xyz; N represents the number of volume distribution groups; M represents the number of sphericity distribution groups; α i represents the frequency of the i-th volume distribution group in the volume histogram distribution; β i,j represents the frequency of the jth sphericity distribution group corresponding to the i-th volume distribution group in the sphericity histogram distribution; c so,n | (x,y,z)onsurface represents the solid phase concentration at the coordinate (x, y, z) on the surface of the negative electrode of the lithium battery; j n It represents the negative electrode ion current density.

10. A computer device comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, characterized in that: When the processor executes the computer program, the method according to any one of claims 1 to 8 is implemented.

11. A computer-readable storage medium, characterized in that: The computer-readable storage medium stores a computer program for executing the method according to any one of claims 1 to 8.

Citation Information

Patent Citations

  • Mechanism modeling method for lithium ion battery

    CN104899439A

  • Electric vehicle lithium ion battery lithium precipitation diagnostic method with data drive

    CN109143083A

  • Determination method for stress between electrode particles during lithium ion battery discharge process based on electrochemical-mechanical coupling model

    CN109991301A