wafer fabrication methods
By forming a modified layer and a crack separation starting point on the back of the wafer, forming a groove along a predetermined dividing line and peeling off the chip, the problem of difficulty in efficiently forming chips of desired thickness in the prior art is solved, and a high-efficiency, low-damage processing process is achieved.
Patent Information
- Application Number
- CN202111001450.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-09-04
- Filing Date
- 2021-08-30
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2041-08-30
AI Technical Summary
Existing technologies are difficult to efficiently form chips of the desired thickness, and may damage the device during the formation process.
A laser beam is used to locate a focal point on the back of the wafer, forming a modified layer and cracks to create a separation starting point. Grooves are then formed along predetermined dividing lines through these starting points, ultimately peeling off the chip and avoiding direct damage to the device.
It enables efficient fabrication of chips of desired thickness, reduces damage to devices, lowers production costs, and simplifies the process flow.
Smart Images

Figure CN114141707B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to a method for processing wafers into chips from wafers. Background Technology
[0002] It is known that there are methods for forming chips from wafers by grinding and cutting wafers (for example, see Patent Document 1).
[0003] Patent Document 1: Japanese Patent Application Publication No. 2008-218599
[0004] However, a new method is desired to form chips of a desired thickness from wafers. Summary of the Invention
[0005] Therefore, the object of the present invention is to provide a new wafer processing method for forming a chip of desired thickness from a wafer.
[0006] According to the present invention, a method for processing a wafer is provided, wherein a chip is formed from a wafer having a plurality of predetermined dividing lines formed along a first direction and a second direction intersecting the first direction and a plurality of chip regions divided by the predetermined dividing lines, characterized in that the wafer processing method comprises the following steps: a trench forming step, wherein a trench with a depth greater than or equal to the desired chip thickness is formed along the predetermined dividing lines from the front side of the wafer; a separation starting point forming step, wherein a focal point of a laser beam of a wavelength that is transparent to the wafer is positioned from the back side of the wafer at a depth equivalent to the thickness of the chip to be formed, and the laser beam is irradiated while the focal point is moved relative to the wafer to form a modified layer and a crack extending from the modified layer, thereby forming a separation starting point parallel to the front side; and a chip peeling step, wherein the chip is peeled from the wafer using the separation starting point.
[0007] Preferably, in the separation starting point forming step, the laser beam is positioned at a depth corresponding to at least two different chip thicknesses for each chip region; in the groove forming step, a groove with a depth greater than the desired chip thickness is formed in the chip region where the groove is to be formed; and in the chip peeling step, chips with at least two different thicknesses are formed for each chip region.
[0008] Preferably, a device is formed in each of the chip regions, and in the chip region where the device is determined to be defective, the trench forming step, the separation starting point forming step, and the chip stripping step are performed.
[0009] This invention provides a novel wafer fabrication method for forming chips of desired thickness from wafers. Attached Figure Description
[0010] Figure 1This is a flowchart illustrating an example of the processing sequence of the wafer fabrication method according to the first embodiment.
[0011] Figure 2 It is shown as Figure 1 A perspective view of an example of a wafer being processed using a wafer processing method.
[0012] Figure 3 It is shown Figure 1 A cross-sectional view of the separation starting point formation step.
[0013] Figure 4 It is shown Figure 1 A top view of the separation starting point formation steps.
[0014] Figure 5 It is shown Figure 1 A cross-sectional view of the first example of the groove forming step.
[0015] Figure 6 It is shown Figure 1 A top view of the first example of the groove forming step.
[0016] Figure 7 It is shown Figure 1 A cross-sectional view of the second example of the groove forming step.
[0017] Figure 8 It is shown Figure 1 A cross-sectional view of the chip stripping process.
[0018] Figure 9 This is a cross-sectional view of the first example of the groove forming step in the wafer processing method of the first modified example.
[0019] Figure 10 This is a top view of the first example of the groove forming step in the wafer processing method of the first modified example.
[0020] Figure 11 This is a cross-sectional view of a second example of the groove forming step in the wafer processing method of the first modified example.
[0021] Figure 12 This is a cross-sectional view showing the separation start point formation step of the wafer processing method of the first modified example.
[0022] Figure 13 This is a top view showing the separation start point formation step of the wafer processing method of the first modified example.
[0023] Figure 14 This is a cross-sectional view showing the separation start point formation step of the wafer processing method according to the second embodiment.
[0024] Figure 15This is a top view showing the separation start point formation step of the wafer processing method according to the second embodiment.
[0025] Figure 16 This is a cross-sectional view showing a first example of the groove forming step in the wafer processing method of the second embodiment.
[0026] Figure 17 This is a top view showing a first example of the groove forming step in the wafer processing method of the second embodiment.
[0027] Figure 18 This is a cross-sectional view showing a second example of the groove forming step in the wafer processing method of the second embodiment.
[0028] Figure 19 This is a cross-sectional view showing the chip stripping step of the wafer processing method of the second embodiment.
[0029] Figure 20 This is a flowchart illustrating an example of the processing sequence of the wafer fabrication method according to the third embodiment.
[0030] Figure 21 It is shown Figure 20 A cross-sectional view of the separation starting point formation step.
[0031] Figure 22 It is shown Figure 20 A top view of the separation starting point formation steps.
[0032] Figure 23 It is shown Figure 20 A cross-sectional view of the first example of the groove forming step.
[0033] Figure 24 It is shown Figure 20 A top view of the first example of the groove forming step.
[0034] Figure 25 It is shown Figure 20 A cross-sectional view of the second example of the groove forming step.
[0035] Figure 26 It is shown Figure 20 A cross-sectional view of the chip stripping process.
[0036] Figure 27 It is shown Figure 20 A top view of the chip stripping process.
[0037] Figure 28 It is shown Figure 20 A cross-sectional view of the adhesive filling step.
[0038] Figure 29 It is shown Figure 20 A top view of the adhesive filling process.
[0039] Figure 30 It is shown Figure 20 A cross-sectional view of the chip fixing process.
[0040] Figure 31 It is shown Figure 20 A top view of the chip fixing process.
[0041] Label Explanation
[0042] 12: Laser beam; 13: Focusing point; 100: Wafer; 101: Front side; 102: Pre-defined dividing line; 103: Chip area; 104: Back side; 130, 130-1, 130-2: Thickness; 131: Modified layer; 132: Crack; 135: Separation starting point; 140, 150: Depth; 141: Cutting groove; 151: Laser processing groove; 160, 160-1, 160-2, 165: Chip. Detailed Implementation
[0043] Hereinafter, embodiments of the present invention will be described in detail with reference to the accompanying drawings. The present invention is not limited to the contents described in the following embodiments. Furthermore, the structural elements described below include substantially the same structural elements that can be readily conceived by those skilled in the art. In addition, the structures described below can be appropriately combined. Furthermore, various omissions, substitutions, or modifications to the structure can be made without departing from the spirit of the present invention.
[0044] [First Embodiment]
[0045] The wafer processing method of the first embodiment of the present invention will be described with reference to the accompanying drawings. Figure 1 As shown, the wafer processing method of the first embodiment includes a separation start point forming step 1001, a trench forming step 1002, and a chip stripping step 1003.
[0046] The wafer 100, which is the object of processing in the wafer processing method of the first embodiment, is, for example, a disc-shaped semiconductor wafer or optical device wafer made of silicon, sapphire, silicon carbide (SiC), gallium arsenide, or the like. Figure 2 As shown, the wafer 100 has, on its flat front side 101, multiple predetermined dividing lines 102 formed along a first direction and a second direction intersecting the first direction; and chip regions 103 divided by the multiple predetermined dividing lines 102. In the first embodiment, the wafer 100 forms a chip 160 (device, see reference 103) in each chip region 103. Figure 8 In the first embodiment, the first direction and the second direction of the wafer 100 are perpendicular to each other, and the multiple predetermined dividing lines 102 are formed in a grid pattern, but this is not the case in the present invention.
[0047] In the first embodiment, the wafer 100 is processed according to the following steps, such as Figure 2 As indicated by the arrows of reference numerals 110 and 120, adhesive tape 105 is pasted onto the front side 101 or the back side 104 opposite to the front side 101, and an annular frame 106 is installed on the outer edge of the adhesive tape 105 to perform the processing steps, but the present invention is not limited to this.
[0048] like Figure 3 As shown, the separation starting point formation step 1001 is the following step: the focusing point 13 of the laser beam 12 with a wavelength that is transparent to the wafer 100 is positioned from the back surface 104 of the wafer 100 onto the chip 160 to be formed (see reference). Figure 8 The laser beam 12 is irradiated while the focal point 13 is moved relative to the wafer 100 at a depth of 130 mm. Figure 3 and Figure 4 As shown, a modified layer 131 and cracks 132 extending from the modified layer 131 are formed at this depth, thereby forming a separation starting point 135 parallel to the front side 101.
[0049] In the separation origin formation step 1001, firstly, adhesive tape 105 is attached to the front side 101 of the wafer 100. Next, in the separation origin formation step 1001, as follows... Figure 3 As shown, the wafer 100 is held on the front side 101 by the holding stage 15 of the laser processing apparatus 10 via the holding surface 16 and the adhesive tape 105. Here, in the first embodiment, the holding stage 15 has, for example, a disc-shaped frame with a recess; and a disc-shaped adsorption part embedded in the recess, which is formed of porous ceramic or the like with a large number of pores. The upper surface of the adsorption part is the holding surface 16, which is used to attract and hold the wafer 100 by a negative pressure introduced by an attraction source (not shown).
[0050] In the separation starting point formation step 1001, then, as Figure 3 As shown, for example, by means of a lifting and moving unit (not shown) and a focusing unit (not shown), the vertical position of the focusing point 13 of the laser beam 12 emitted from the laser oscillator 11 of the laser processing apparatus 10 is positioned at a height above the front surface 101 of the wafer 100 on the chip 160 (see reference). Figure 8 The position of the laser beam 12 is determined by a thickness of 130, wherein the lifting and moving unit causes the laser oscillator 11 or the holding stage 15 to move vertically, and the focusing unit is disposed within the laser oscillator 11, which causes the focal position of the laser beam 12 to move vertically. Furthermore, in the first embodiment where the laser beam 12 is irradiated from the back surface 104 of the wafer 100, the position that is a thickness of 130 above the front surface 101 of the wafer 100 corresponds to a depth corresponding to the thickness of 130 of the chip 160.
[0051] In step 1001, where the separation starting point is formed, then, as follows: Figure 3 As shown, for example, by moving the laser oscillator 11 or a moving unit (not shown) that holds the stage 15 in a direction parallel to the front surface 101, the focusing point 13 and the wafer 100 are aligned in a predetermined direction parallel to the front surface 101. Figure 4 The laser beam 12 is moved relative to the back surface 104 of the wafer 100 while continuously and vertically irradiating the wafer 100 from the back surface 104 side, thereby creating a surface at a height of 160 (refer to the front surface 101 of the wafer 100) above the wafer 100. Figure 8 The modified layer 131 is formed in a straight line extending along the specified direction, with a thickness of 130. In the separation start point formation step 1001, for example, a pulsed laser beam 12 is irradiated onto the wafer 100 by the laser oscillator 11 of the laser processing apparatus 10.
[0052] The modified layer 131 formed in step 1001 through the separation starting point formation is a layer that makes the substrate of the wafer 100 amorphous at the focusing point 13 of the laser beam 12, and residual stress acts in a direction parallel to the front surface 101. In step 1001 through the separation starting point formation, through this residual stress, such as Figure 3 and Figure 4 As shown, a crack 132 is formed extending from the modified layer 131 in a direction intersecting the predetermined direction. Both the modified layer 131 and the crack 132 formed by the separation starting point formation step 1001 become the separation starting point 135 during the peeling process in the chip peeling step 1003 described later.
[0053] In step 1001, where the separation starting point is formed, as follows: Figure 4 As shown, multiple linear modified layers 131 are formed parallel to each other at intervals corresponding to the effective elongation length of the crack 132 from the modified layer 131 (in the first embodiment, the interval is approximately twice the effective elongation length (more than 1.9 times and less than 2.1 times)). This ensures that the separation starting point 135, parallel to the front face 101, is formed sufficiently and uniformly without creating large intervals or unevenness. In the separation starting point formation step 1001, in the first embodiment, for example, the modified layers 131 are formed at intervals of approximately 10 μm, and the effective elongation length of the crack 132 from the modified layer 131 is approximately 5 μm. Here, the effective elongation length of the crack 132 from the modified layer 131 is the length of the crack 132 from the modified layer 131 that fully and effectively functions as the separation starting point 135. In the separation starting point formation step 1001, in the first embodiment, according to... Figure 3 and Figure 4The arrows indicate that the laser beam 12 irradiates the entire surface of the wafer 100 to form the modified layer 131 and cracks 132. However, this invention is not limited to this; the modified layer 131 and cracks 132 may also be formed only in the region corresponding to the chip region 103. Furthermore, although multiple modified layers 131 are actually formed in the separation start point formation step 1001, in... Figure 4 and Figure 6 The text omits and only records a portion of the modified layer 131.
[0054] The groove forming step 1002 involves forming a chip 160 of a desired depth from the front side 101 along the predetermined dividing line 102 (see reference). Figure 8 The step of forming a trench with a thickness of 130 or more is called a half-cut. The trench forming step 1002 is a so-called half-cut that forms a trench with a depth of less than 100 of wafer thickness.
[0055] In trench forming step 1002, firstly, the adhesive tape 105, which was adhered to the front side 101 of the wafer 100 after the separation start point forming step 1001, is peeled off, and then the adhesive tape 105 is adhered to the back side 104 of the wafer 100. Next, in trench forming step 1002, as in the first example, ... Figure 5 As shown, the wafer 100 is held on the back side 104 side by the holding table 25 of the cutting processing apparatus 20, with the holding surface 26 holding it across the adhesive tape 105. In the second example, as... Figure 7 As shown, the back side 104 of the wafer 100 is held by the holding stage 35 of the laser processing apparatus 30 via the holding surface 36 and the adhesive tape 105. The holding stages 25 and 35 have the same structure as the holding stage 15.
[0056] Then, in the first example of groove forming step 1002, as Figure 5 As shown, while rotating the cutting tool 21 of the cutting processing apparatus 20, the wafer 100 is cut from the front side 101 to a depth 140 of thickness 130 or more. For example, the cutting tool 21 and the wafer 100 are moved relative to each other along the predetermined dividing line 102 by a moving unit (not shown) that moves the cutting tool 21 or the worktable 25 in a direction parallel to the front side 101, thereby cutting the wafer 100 and forming a cutting groove 141 of depth 140 along the predetermined dividing line 102. In the first example of the groove forming step 1002, cutting is performed on each predetermined dividing line 102, such as... Figure 6 As shown, a cutting groove 141 of depth 140 is formed along all the predetermined dividing lines 102. Additionally, in practice, as... Figure 6 As shown, the modified layer 131 formed by the separation starting point forming step 1001 is formed densely in a manner that is narrower than the cutting grooves 141 formed by the first example of the groove forming step 1002.
[0057] Additionally, in the second example of groove forming step 1002, such as Figure 7 As shown, while irradiating the wafer 100 with a laser beam 32 of a wavelength that absorbs the wafer 100 using the laser oscillator 31 of the laser processing apparatus 30, the laser beam 32 and the wafer 100 are moved relative to each other along the predetermined dividing lines 102, for example, by a moving unit (not shown) that moves the laser oscillator 31 or the stage 35 in a direction parallel to the front surface 101. This allows the laser beam 32 to perform a so-called ablation process on the wafer 100, causing it to sublimate or evaporate, thus forming a laser processing groove 151 with a thickness of 130 or more and a depth of 150 along the predetermined dividing lines 102. In a second example of groove forming step 1002, for example, a pulsed laser beam 32 is irradiated onto the wafer 100 using the laser oscillator 31 of the laser processing apparatus 30. In the second example of groove forming step 1002, the same as in the first example of groove forming step 1002, a laser processing groove 151 with a depth of 150 is formed along all the predetermined dividing lines 102.
[0058] like Figure 8 As shown, chip stripping step 1003 is a step of stripping chip 160 from wafer 100 using the separation point 135 formed through separation point formation step 1001. Figure 8 The example shown illustrates the chip stripping step 1003 performed after the first instance of trench forming step 1002, but the same applies to the case performed after the second instance of trench forming step 1002.
[0059] In chip stripping step 1003, firstly, as... Figure 8 As shown, the wafer 100 is held on the back side 104 side by the holding stage 45 of the chip stripping device 40 via the holding surface 46 and the adhesive tape 105. The holding stage 45 has the same structure as the holding stage 15.
[0060] In the chip stripping step 1003, after the adsorption plate 43 of the chip stripping device 40, located at the lower end of the ultrasonic amplitude transformer 41, comes into contact with the front side 101 of the chip region 103 of the wafer 100, the ultrasonic amplitude transformer 41 is subjected to ultrasonic waves by the ultrasonic oscillator 42, causing the ultrasonic amplitude transformer 41 to vibrate ultrasonically. The ultrasonic amplitude transformer 41, which has undergone ultrasonic vibration, is subjected to ultrasonic vibration on the chip region 103 of the wafer 100 through the adsorption plate 43, thereby destroying the separation starting point 135 of the chip region 103 and stripping the chip 160 formed in the chip region 103 from the wafer 100.
[0061] In chip stripping step 1003, the chip 160 stripped from the wafer 100 is picked up from above by adsorption and holding using the adsorption sheet 43, resulting in a monolithic chip 160. Here, in the first embodiment, a negative pressure is introduced to the surface of the adsorption sheet 43, for example, by an attraction source not shown, and the adsorption sheet 43 uses the negative pressure to adsorb and hold the chip 160 from above. In chip stripping step 1003, in the first embodiment, chip 160 is stripped and picked up according to each chip region 103, and all chips 160 formed on the wafer 100 are monolithicized. Alternatively, in chip stripping step 1003, if the chip 160 can be stripped solely by adsorption based on the adsorption sheet 43, it can also be implemented using a chip stripping device 40 without an ultrasonic oscillator 42.
[0062] In the wafer processing method of the first embodiment having the above-described structure, in the separation start point formation step 1001, the focus point 13 of a laser beam 12 with a wavelength that is transmissible to the wafer 100 is positioned along the bottom surface of the chip 160 at a depth corresponding to the desired thickness 130 of the chip 160, and the laser beam 12 is irradiated to form a separation start point 135. In the groove formation step 1002, a groove (a cutting groove 141 in the first example, and a laser processing groove 151 in the second example) is formed along the predetermined dividing line 102. In the chip peeling step 1003, the chip 160 is peeled from the wafer 100 starting from the separation start point 135. Therefore, the wafer processing method of the first embodiment has the following effect: by changing the positioning height of the focus point 13 of the laser beam 12 with a wavelength that is transmissible to the wafer 100, a chip 160 with a desired thickness 130 can be formed from the wafer 100. In addition, in the wafer processing method of the first embodiment, a separation layer connected to the separation starting point 135 is formed on the entire bottom surface of the chip 160. The separation starting point 135 is composed of a modified layer 131 and a crack 132 extending from the modified layer 131 in a plane direction parallel to the front surface 101 of the wafer 100, so the chip 160 can be effectively peeled off.
[0063] Furthermore, in the wafer processing method of the first embodiment, in the separation start point formation step 1001, a laser beam 12 of a wavelength that is transmissible to the wafer 100 is irradiated from the back side 104 side of the wafer 100, opposite to the front side 101 where the chip 160 is formed, to form a separation start point 135. Therefore, in the wafer processing method of the first embodiment, when a device (chip 160) is formed on the front side 101, the laser beam 12 is not obstructed, and the separation start point 135 can be formed well. In addition, in the wafer processing method of the first embodiment, when a device (chip 160) is formed on the front side 101, the damage to the chip 160 caused by the laser beam 12 irradiated to form the separation start point 135 can be reduced.
[0064] Furthermore, in the wafer processing method of the first embodiment, a chip 160 of the desired thickness can be formed without using a grinding device. Moreover, in the wafer processing method of the first embodiment, when the groove forming step 1002 is performed using the laser processing apparatus 30, a chip 161 of the desired thickness can be formed using only the laser processing apparatuses 10 and 30. By using identical laser processing apparatuses 10 and 30, the installation area of the apparatus can be reduced, and the production cost can be lowered. Additionally, conventionally, a step to reduce the adhesive strength of the adhesive tape is required when peeling off the chip. However, in the wafer processing method of the first embodiment, since the chip 160 is peeled off starting from the separation point 135 formed inside the wafer 100, the step to reduce the adhesive strength of the adhesive tape 105 is unnecessary. Furthermore, in the wafer processing method of the first embodiment, after the laser beam 12 is irradiated from the back side 104 side of the wafer 100 through the separation start point formation step 1001, the groove formation step 1002 and the chip peeling step 1003 are continuously performed from the front side 101 side of the wafer 100. Therefore, compared with the first modified example described later, which requires two re-attaching of the adhesive tape 105, the re-attaching of the adhesive tape 105 is only performed once after the separation start point formation step 1001, thus reducing the processing time.
[0065] [Example 1]
[0066] The wafer processing method of the first modified example of the present invention will be described with reference to the accompanying drawings. Figure 9 This is a cross-sectional view illustrating the first example of the groove forming step 1002 of the wafer processing method of the first modified example. Figure 10 This is a top view illustrating the first example of the groove forming step 1002 of the wafer processing method of the first modified example. Figure 10 Viewed from the front 101 side Figure 9 A diagram showing the state of the data. Figure 11 This is a cross-sectional view illustrating a second example of the groove forming step 1002 in the wafer processing method of the first modified example. Figure 12 This is a cross-sectional view illustrating the separation start point formation step 1001 of the wafer processing method of the first modified example. Figure 13 This is a top view illustrating the separation start point formation step 1001 of the wafer processing method of the first modified example. Figure 13 Viewed from the 104th side of the back Figure 12 A diagram of the state. In Figures 9 to 13 In this document, parts that are the same as those in the first embodiment are marked with the same reference numerals and their descriptions are omitted.
[0067] The wafer processing method of the first modification replaces the wafer processing method of the first embodiment by changing the execution order of the separation start point formation step 1001 and the trench formation step 1002; all other processes are the same as in the first embodiment. That is, in the wafer processing method of the first modification, the trench formation step 1002 is performed before the separation start point formation step 1001.
[0068] The groove forming step 1002 of the first modification, except for the point that adhesive tape 105 is first pasted on the back side 104 of the wafer 100, and as in the first example, as... Figure 9 and Figure 10 As shown in the second example Figure 11 Except for the fact that a groove (cutting groove 141 in the first example and laser processing groove 151 in the second example) is formed on the wafer 100 where the separation starting point 135 is not formed, it is the same as the first embodiment.
[0069] In the first variation of the wafer processing method, the separation start point forming step 1001, except that the adhesive tape 105 is peeled off from the back side 104 of the wafer 100 after the trench forming step 1002 and the adhesive tape 105 is attached to the front side 101 of the wafer 100, and as... Figure 12 and Figure 13 Except for the point where a separation starting point 135 is formed on the wafer 100 with grooves (cutting groove 141 in the first example, laser processing groove 151 in the second example), it is the same as in the first embodiment. Figure 12 and Figure 13 The example shown illustrates the separation start point formation step 1001 in the case where it is performed after the first instance of the groove formation step 1002, but the same applies in the case where the separation start point formation step 1001 is performed after the second instance of the groove formation step 1002.
[0070] The chip stripping step 1003 of the wafer processing method in the first variation is the same as in the first embodiment, except that it is performed after peeling off the adhesive tape 105 that is pasted on the front side 101 of the wafer 100 after the separation start point formation step 1001 and pasting the adhesive tape 105 onto the back side 104 of the wafer 100.
[0071] The wafer processing method of the first modified example having the above-described structure has changed the execution order of the separation start point formation step 1001 and the trench formation step 1002 in the first embodiment, thus achieving the same effect as the first embodiment.
[0072] [Second Implementation]
[0073] according to Figures 14 to 19 A wafer processing method according to the second embodiment of the present invention will be described. Figures 14 to 19 In this document, parts that are the same as those in the first embodiment are marked with the same reference numerals and their descriptions are omitted.
[0074] like Figure 19 As shown, the wafer processing method of the second embodiment is changed from the first embodiment to generate a chip 160-1 with a thickness of 130-1 from one half of the wafer 100, region 170, and a chip 160-2 with a thickness of 130-2 from the other half of the wafer 100, region 180. Other processing is the same as in the first embodiment. In the second embodiment, the thicknesses 130-1 and 130-2 are different.
[0075] In the second embodiment of the wafer processing method, the separation starting point formation step 1001 is as follows: In the first embodiment, the depth of forming the separation starting point 135 is changed according to the depth of the focusing point 13 of the positioning laser beam 12 for each region 170, 180 of the wafer 100, and other processes are the same as in the first embodiment. In the second embodiment of the wafer processing method, specifically, as follows: Figure 14 and Figure 15 As shown, in region 170, the focusing point 13 of the laser beam 12 is positioned at a point corresponding to the chip 160-1 to be generated (see reference). Figure 19 A laser beam 12 is irradiated at a depth of 130-1, forming a modified layer 131 and cracks 132 at this depth, thus creating a separation initiation point 135. In region 180, the focusing point 13 of the laser beam 12 is positioned at a point corresponding to the chip 160-2 to be generated (see reference). Figure 19 A laser beam 12 is irradiated at a depth of 130-2 mm in the thickness of the material, forming a modified layer 131 and a crack 132 at that depth, thereby forming a separation initiation point 135.
[0076] In the wafer processing method of the second embodiment, the trench forming step 1002 is as follows: In the first embodiment, in the first example, as shown in the first example... Figure 16 and Figure 17 As shown in example 2 Figure 18 As shown, the process is modified so that chips 160-1 and 160-2 with the desired depth (140 in the first example and 150 in the second example) are formed from the front side 101 (refer to...). Figure 19 The thicker one of the ) Figure 16 and Figure 18 In the example shown, the groove with a thickness of 130-1 or more is a chip 160-1 (cutting groove 141 in the first example and laser processing groove 151 in the second example), and the other processing is the same as in the first embodiment.
[0077] Furthermore, in the trench forming step 1002 of the wafer processing method in the second embodiment, it is not limited to the above-described manner. Alternatively, the depth (140 in the first example and 150 in the second example) of the trench (cutting trench 141 in the first example and laser processing trench 151 in the second example) surrounding the chip region 103 may be formed in the chip region 103 to be greater than or equal to the thickness (130-1 and 130-2) of the desired chip (chip 160-1, 160-2). In the trench forming step 1002 of the wafer processing method of the second embodiment, the depth of the trench (cutting trench 141 in the first example, laser processing trench 151 in the second example) may be changed according to the desired thickness (thickness 130-1, 130-2) of the desired chip (chip 160-1, 160-2) in the chip region 103 adjacent to the dividing predetermined line 102.
[0078] like Figure 19 As shown, in the first embodiment, the chip stripping step 1003 of the wafer processing method of the second embodiment is changed to stripping and picking up a chip 160-1 with a thickness of 130-1 in region 170 and stripping and picking up a chip 160-2 with a thickness of 130-2 in region 180. Other processes are the same as in the first embodiment.
[0079] In the second embodiment, two chips 160-1 and 160-2 with different thicknesses 130-1 and 130-2 are generated for each of the two regions 170 and 180 of the wafer 100. However, this is not a limitation in the present invention. For example, there may be more than three types, or at least two different thicknesses of chips may be generated for each chip region 103 of the wafer 100. In this case, in the separation start point forming step 1001, the laser beam 12 is irradiated with a focusing point 13 of the laser beam 12 at a depth corresponding to the thickness of at least two different chips to form a separation start point 135 according to each chip region 103 of the wafer 100. In the groove forming step 1002, a groove around the chip region 103 is formed to a depth greater than the desired chip thickness according to each chip region 103.
[0080] Conventionally, when forming chips of different thicknesses from a single wafer, an inefficient method was employed, such as varying the grinding thickness for each monolithically formed chip. However, in the wafer processing method of the second embodiment having the aforementioned structure, the depth at which the separation starting point 135 is formed is varied to two or more different depths according to each chip region 103. Figures 14 to 19 In the example, there are 2 types), which can form more than 2 types (in Figures 14 to 19In the example, there are two types of chips 160-1 and 160-2 with different thicknesses of 130-1 and 130-2. Therefore, compared with the conventional method, the wafer processing method of the second embodiment can efficiently form chips 160-1 and 160-2 with different thicknesses of 130-1 and 130-2 from a single wafer 100.
[0081] Alternatively, the wafer processing method of the second embodiment can also be applied to the first modification, by changing the execution order of the separation start point forming step 1001 and the trench forming step 1002.
[0082] [Third Implementation]
[0083] according to Figures 20 to 30 A wafer processing method according to the third embodiment of the present invention will be described. Figures 20 to 31 In this document, parts that are the same as those in the first and second embodiments are marked with the same reference numerals and their descriptions are omitted.
[0084] like Figure 20 As shown, the wafer processing method of the third embodiment includes a device determination step 1011, a separation start point formation step 1001, a trench formation step 1002, a chip peeling step 1003, an adhesive filling step 1004, and a chip fixing step 1005.
[0085] Device determination step 1011 is a step of detecting whether each chip 160 formed on wafer 100 is defective. Here, chip 160 being defective means that chip 160 does not meet the quality requirements for use as a product. In device determination step 1011, for example, multiple probes of a device detector (not shown) are brought into contact with electrodes formed on chip 160, and a tester (not shown) electrically connected to the probes inputs a predetermined electrical signal to chip 160 via the probes. Whether chip 160 is defective is detected based on the electrical signal returned from chip 160. Device determination step 1011 is not limited to this in the present invention, and various other known checks for detecting whether chip 160 is defective can also be implemented.
[0086] In the wafer processing method of the third embodiment, when it is determined in the device determination step 1011 that all chips 160 are not defective (the result is "No" in the device determination step 1011), the process ends. In the wafer processing method of the third embodiment, when it is determined in the device determination step 1011 that at least one chip 160 is defective (the result is "Yes" in the device determination step 1011), information such as the position of the defective chip 160 within the wafer 100, the size of the chip region 103, and the thickness 130 are sent to a control unit (not shown) that controls each device (laser processing device 10, cutting processing device 20, laser processing device 30, and chip stripping device 40) that performs each step of the wafer processing method of the third embodiment, so that the process enters the separation start point formation step 1001.
[0087] Furthermore, in the third embodiment, the control unit described above includes a computer system. The computer system included in the control unit includes: an arithmetic processing unit having a microprocessor such as a CPU (Central Processing Unit); a storage device having a memory such as ROM (Read Only Memory) or RAM (Random Access Memory); and an input / output interface device. The arithmetic processing unit of the control unit performs arithmetic processing according to a computer program stored in the storage device of the control unit, and outputs control signals for controlling the aforementioned devices to the structural elements of the aforementioned devices via the input / output interface device of the control unit.
[0088] like Figure 21 and Figure 22 As shown, in the first embodiment, the separation start point formation step 1001 of the wafer processing method of the third embodiment is changed to form a separation start point 135 at a depth equivalent to the thickness 130 of the chip 160 in the chip region 103 where the chip 160 determined to be defective by the device determination step 1011 is formed. Other processing is the same as in the first embodiment.
[0089] In the first case, as Figure 23 and Figure 24 As shown in example 2 Figure 25As shown, in the first embodiment, the groove forming step 1002 of the wafer processing method of the third embodiment is changed to forming a groove (cutting groove 141 in the first example and laser processing groove 151 in the second example) with a depth (140 in the first example and 150 in the second example) greater than the thickness 130 of the chip 160 in the second example, only in the portion surrounding the chip region 103 where the chip 160 is formed as a defective chip 160 determined by the device determination step 1011. The other processing is the same as in the first embodiment.
[0090] In addition, in the first example of the groove forming step 1002 of the wafer processing method of the third embodiment, specifically, a so-called cleaving cut is performed. That is, for each part of the dividing predetermined line 102, the cutting tool 21 is positioned on the part of the dividing predetermined line 102, and while rotating the cutting tool 21, the cutting tool 21 is lowered in the vertical direction to the height of the cutting groove 141 with a depth of 140 to perform cutting. Then, the cutting tool 21 is raised in the vertical direction and retracted. However, the present invention is not limited to cleaving cut. The cutting groove 141 with a depth of 140 can also be formed along the dividing predetermined line 102 surrounding the chip region 103 using the same method as in the first embodiment.
[0091] like Figure 26 and Figure 27 As shown, in the first embodiment, the chip stripping step 1003 of the wafer processing method of the third embodiment is modified to only strip and pick up chips 160 that are determined to be defective by the device determination step 1011, while other processes are the same as in the first embodiment. In the chip stripping step 1003 of the wafer processing method of the third embodiment, chips 160 that are determined to be defective by the device determination step 1011 are picked up, thereby forming a recess 162 with a depth corresponding to the thickness 130 of the chip 160 in the region including the chip region 103 of the wafer 100 on which the chip 160 is formed and the portion of the dividing predetermined line 102 surrounding the chip region 103.
[0092] In the past, when a chip was completely cut and peeled off along the thickness direction, the peeling process was required after reducing the adhesive force of the adhesive tape in the chip area to be peeled off. However, in the chip peeling step 1003 of the third embodiment, since the peeling is performed starting from the separation point 135 formed inside the wafer 100, the step of reducing the adhesive force of the adhesive tape 105 in the chip area 103 where the chip 160 to be peeled off is formed is not required.
[0093] like Figure 28 and Figure 29As shown, the adhesive filling step 1004 is a step in which adhesive 53 is supplied by the adhesive supply device 50 to the recess 162 formed in the chip peeling step 1003 to fill the recess. In the third embodiment, the adhesive 53 is used to fix the chip 165 subsequently provided in the chip fixing step 1005 (see reference). Figure 30 and Figure 31 The adhesive is a liquid resin that cures in the air, for example, preferably an adhesive containing known organic solvents, surfactants, etc.
[0094] In adhesive filling step 1004, as Figure 28 As shown, the back surface 104 side of the wafer 100 with the recess 162 is held by the holding stage 55 of the adhesive supply device 50 via the holding surface 56 and the adhesive tape 105. The holding stage 55 has the same structure as the holding stage 15 of the first embodiment. In the adhesive filling step 1004, adhesive 53 supplied from the adhesive supply source 52 of the adhesive supply device 50 is then supplied from the nozzle 51 to the recess 162, filling it to a depth to which the adhesive 53 will just not overflow from the recess 162 when the chip 165 is subsequently provided in the chip fixing step 1005.
[0095] like Figure 30 and Figure 31 As shown, chip fixing step 1005 involves providing chip 165 onto the adhesive 53 filled in the recess 162 in adhesive filling step 1004 using chip fixing device 60, and pressing and fixing chip 165 to adhesive 53. Furthermore, in the third embodiment, chip 165 has the same specifications, shape, and size as chip 160 peeled from wafer 100 in chip peeling step 1003, and is determined to be non-defective (qualified) using the same determination method as in device determination step 1011.
[0096] In chip fixing step 1005, such as Figure 30 As shown, the chip holding device 60 holds the back side 104 of the wafer 100, which is filled with adhesive 53 in the recess 162, through the holding stage 65 and the holding surface 66, with the adhesive tape 105 in between. The holding stage 65 has the same structure as the holding stage 15 in the first embodiment. In the chip holding step 1005, the adsorption part 61 of the chip holding device 60, which adsorbs and holds the chip 165, is positioned on the adhesive 53 in the recess 162. After pressing the chip 165 against the adhesive 53 with the adsorption part 61 until the upper surface of the chip 165 is at the same height as the front side 101 of the wafer 100, the adsorption and holding of the chip 165 is released.
[0097] Furthermore, in the chip fixing step 1005, the height of the upper surface of the chip 165, based on the bottom surface of the recess 162, is the height obtained by adding the thickness of the adhesive 53 to the thickness of the chip 165. Therefore, in the previously performed separation start point forming step 1001, the separation start point 135 can also be formed to a depth deeper than the thickness 130 of the chip 160. Alternatively, the following step may be performed: after performing the chip fixing step 1005, the front side 101 of the wafer 100 is held in the adhesive tape 105 while the back side 104 is ground.
[0098] In addition, Figures 21 to 31 In the example shown, the wafer processing method of the third embodiment determines that one chip 160 is defective, and performs the processing steps after the separation start point formation step 1001 in the chip region 103 where the defective chip 160 is formed. However, this invention is not limited to this, and multiple chips 160 may also be determined to be defective, and the processing steps after the separation start point formation step 1001 may be performed on each chip region 103 where these multiple defective chips 160 are formed.
[0099] In the past, in wafer-on-wafer (WOW) processes where multiple semiconductor device wafers are stacked together and interconnected by forming through electrodes that penetrate the stacked semiconductor devices, and then the stacked wafers are divided to form a stacked chip, if a defective chip exists on a certain wafer, the chips stacked on top of that defective chip are also unusable. However, in the wafer processing method of the third embodiment with the above-described structure, defective chips 160 (devices) are selectively removed, and qualified chips 165 are instead embedded in the removed chip regions 103. This allows all chips 160 and 165 formed in all chip regions 103 on the wafer 100 to be qualified, thus suppressing the generation of unusable chips 160 in the WOW process.
[0100] Alternatively, the wafer processing method of the third embodiment can also be applied to the first modification, by changing the execution order of the separation start point forming step 1001 and the trench forming step 1002.
[0101] Furthermore, the present invention is not limited to the embodiments described above. That is, various modifications can be made without departing from the spirit of the present invention.
Claims
1. A method for processing a wafer, forming a chip from a wafer, the wafer having a plurality of predetermined dividing lines formed along a first direction and a second direction intersecting the first direction, and a plurality of chip regions divided by the predetermined dividing lines, characterized in that, The wafer fabrication method comprises the following steps: In the trench forming step, a trench with a depth greater than the desired chip thickness is formed along the predetermined dividing line from the front side of the wafer. In the separation start-point formation step, a focal point of a laser beam with a wavelength that is transparent to the wafer is positioned from the back of the wafer at a depth equivalent to the thickness of the chip to be formed. The laser beam is irradiated while the focal point is moved relative to the wafer to form a modified layer and cracks extending from the modified layer, thereby forming a separation start-point parallel to the front side. as well as The chip stripping step utilizes this separation starting point to peel the chip off the wafer. Devices are formed in this chip region. In the chip area where the device is determined to be defective, the trench forming step, the separation starting point forming step, and the chip peeling step are performed to selectively remove the defective device. Instead, the qualified devices are embedded in the chip area where the defective devices have been removed.
2. The wafer processing method according to claim 1, characterized in that, In this separation initiation step, the laser beam is positioned at a depth corresponding to at least two different chip thicknesses for each chip region. In this trench forming step, a trench with a depth greater than the desired chip thickness is formed in the chip region where the trench is to be formed. In this chip stripping step, at least two different thicknesses of chips are formed for each chip region.
Citation Information
Patent Citations
Method and apparatus for processing wafer
JP2008218599A
Chip manufacturing method
CN103026468A
Processing apparatus and processing method
JP2017130638A