A Mg-doped enhanced transition metal sulfide-based visible light detector and preparation method thereof
By combining Mg-doped transition metal sulfide and InGaN materials to form a heterogeneous p-n junction, the problem of difficulty in forming p-type doping of transition metal sulfide materials in the existing technology is solved, and high-performance optoelectronics for visible light communications are realized. The detector improves the response speed and sensitivity of the device.
Patent Information
- Application Number
- CN202111347895.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-11-15
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2041-11-15
AI Technical Summary
Existing transition metal sulfide materials naturally have n-type electronic characteristics, and it is difficult to control the preparation process to form p-type doping, which limits the improvement of device performance, especially when forming a strong heterojunction built-in electric field with traditional III-V materials. difficult problem.
The van der Waals heterogeneous p-n junction is prepared by combining Mg-doped transition metal sulfide with InGaN semiconductor material, and the Mg-doped transition metal sulfide layer is prepared on the Si-based InGaN epitaxial wafer using chemical vapor deposition and molecular beam evaporation. And a Ti/Au electrode is formed on it to achieve in-situ doping and electrode deposition, form a deep main energy level, and regulate the carrier type and concentration.
The p-type doping of TMDs materials is achieved, which reduces the dark current, enhances the rectification ratio and response speed, and improves the performance and sensitivity of photodetectors for visible light communications.
Smart Images

Figure CN114242817B_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of photoelectric detectors for visible light communication, and in particular relates to a Mg-doped enhanced transition metal sulfide (TMDs)-based visible light detector and a preparation method thereof. Background Art
[0002] In recent years, with the rapid development of solid-state lighting, visible light communication technology has also made great progress. Visible light communication is a wireless optical communication technology based on white light emitting diode technology. It can realize two functions, lighting and high-speed data transmission, and has the characteristics of high signal density coverage, high confidentiality and security, anti-electromagnetic interference, and wide spectrum range. It can achieve high-speed, stable and safe communication transmission. As an unrestricted white spectrum area, it has no interference with traditional radio waves in terms of signals, opening up the spectrum of the next generation of broadband communication.
[0003] Transition metal sulfide is a two-dimensional van der Waals semiconductor material with the characteristics of high carrier mobility, high thermal stability, good chemical stability, and adjustable bandgap width with the number of layers. It can achieve an adjustable bandgap width of 1.4-2.0eV, corresponding to the detection of visible light with a wavelength of 620-950nm. In recent years, the size of traditional Si-based detectors has continued to decrease, the density of transistors has increased exponentially, and the short channel effect of transistors has limited the further improvement of their own performance. Compared with Si-based detectors, two-dimensional detectors have the advantages of small size, easy to carry, easy to integrate, and high breakdown electric field, which has promoted the further development of visible light detectors.
[0004] Existing transition metal sulfides exhibit natural n-type electronic properties, and it is difficult to form a strong heterojunction built-in electric field with traditional III-V materials. Because S vacancies are difficult to eliminate, this n-type electronic property is difficult to change through preparation process regulation. Therefore, p-type doping of transition metal sulfides is a difficult problem.
[0005] The present invention combines doped TMDs and InGaN semiconductor materials to prepare a van der Waals heterogeneous pn junction, thereby further improving the performance of the device. Summary of the invention
[0006] In order to overcome the shortcomings and deficiencies of the prior art, the object of the present invention is to provide a Mg-doped enhanced transition metal sulfide-based visible light detector and a preparation method thereof. The present invention combines Mg-doped TMDs (transition metal sulfides) with InGaN semiconductor materials to prepare a van der Waals heterojunction, thereby improving the performance of the device. The method of the present invention is simple and easy to operate.
[0007] The purpose of the present invention is achieved through the following technical solutions:
[0008] A Mg-doped enhanced transition metal sulfide (TMDs)-based visible light detector comprises a Si substrate layer, an InGaN epitaxial layer (InGaN layer), a Mg-doped transition metal sulfide (TMDs) layer and an electrode layer arranged in sequence from bottom to top. The electrode layer is a first electrode layer and a second electrode layer; the first electrode layer is a Ti / Au layer, and the second electrode layer is a Ti / Au layer.
[0009] The Mg-doped transition metal sulfide layer partially covers the InGaN epitaxial layer, and a mesa is formed on the upper surface of the InGaN epitaxial layer.
[0010] A first electrode layer is arranged on the table of the InGaN epitaxial layer, and the electrode layer is not in contact with the Mg-doped transition metal sulfide layer. The Ti layer in the first electrode layer is arranged on the table of the InGaN epitaxial layer. The Au layer is arranged on the Ti layer.
[0011] A second electrode layer is arranged on the Mg-doped transition metal sulfide layer. The second electrode layer partially covers the Mg-doped transition metal sulfide layer. The Ti layer in the second electrode layer is arranged on the Mg-doped transition metal sulfide layer. The Au layer is arranged on the Ti layer.
[0012] The transition metal sulfide is also called a transition metal chalcogenide, and has a chemical formula of MX2, where M refers to a transition metal element (eg, molybdenum, tungsten, niobium, rhenium, titanium), and X refers to a chalcogen element (eg, sulfur, selenium, tellurium).
[0013] The method for preparing the Mg-doped enhanced transition metal sulfide (TMDs)-based visible light detector comprises the following steps:
[0014] 1) preparing a Mg-doped transition metal sulfide (TMDs) layer on a Si-based InGaN epitaxial wafer by chemical vapor deposition, and annealing;
[0015] 2) preparing an electrode layer on the annealed Mg-doped transition metal sulfide (TMDs) layer and on the InGaN layer not covered by the Mg-doped transition metal sulfide (TMDs) layer.
[0016] The specific steps of the preparation method are:
[0017] 1) Spin-coating a positive photoresist on a Si-based InGaN epitaxial wafer, and photolithography out a vapor deposition area of the Mg layer, where the vapor deposition area is located at one end of the upper surface of the epitaxial wafer;
[0018] 2) using molecular beam evaporation to deposit a layer of metal Mg in the evaporation area, stripping off the unexposed photoresist, and obtaining an epitaxial wafer device containing a Mg layer;
[0019] 3) preparing an epitaxial Mg-doped TMDs layer on an epitaxial wafer device containing a Mg layer by chemical vapor deposition using transition metal oxides and chalcogenide sources as precursors, and performing annealing to obtain a doped TMDs / InGaN layer device; wherein the Mg-doped TMDs layer partially covers the InGaN layer in the device;
[0020] 4) Spin-coating photoresist on the doped TMDs / InGaN layer device, and photolithography out an electrode deposition area of a desired shape; the electrode deposition area is located on the Mg-doped TMDs layer and on the InGaN layer not covered by the Mg-doped TMDs layer;
[0021] 5) A metal electrode is evaporated in the deposition area by molecular beam evaporation, and the unexposed photoresist is stripped off to obtain a Mg-doped enhanced transition metal sulfide (TMDs)-based visible light detector.
[0022] In step 3), the transition metal oxide is an oxide of molybdenum, tungsten, niobium, rhenium, or titanium, such as molybdenum trioxide or tungsten trioxide; the chalcogen source is sulfur, selenium, or tellurium powder;
[0023] The chemical vapor deposition was carried out under an argon atmosphere at standard atmospheric pressure.
[0024] The chemical vapor deposition equipment in step 3) is a tube furnace; the chemical vapor deposition conditions are: the growth environment is an argon atmosphere of 700-780 Torr; the transition metal oxide and the chalcogen source are heated at different temperatures, the heating temperatures are 650-750° C. and 100-140° C. respectively; the growth time is 2-6 min;
[0025] The thickness of the Mg-doped TMDs layer is 1-100 nm; the Mg doping concentration in the Mg-doped TMDs layer is 2×10 18 ~6×10 18 cm -3 .
[0026] Step 3) the annealing treatment: the temperature is 600-750°C, and the annealing time is 0.5-2h.
[0027] (A large amount of Mg will be lost and evaporated during the preparation process)
[0028] In step 5), the metal electrode is a Ti / Au electrode, the Ti layer is disposed on the Mg-doped transition metal sulfide layer, and the Au layer is disposed on the Ti layer.
[0029] The Si-based InGaN substrate in step 1) is an InGaN single crystal or epitaxial wafer, the Si layer thickness is 300-400um, and the InGaN epitaxial wafer thickness is 1-3um.
[0030] Step 2) The thickness of the Mg layer is 10-100 nm.
[0031] The thickness of the deposited Ti and gold electrodes in step 5) are 30-60nm / 60-150nm respectively.
[0032] The Mg-doped p-type TMDs layer forms a pn heterojunction with the intrinsic n-type InGaN substrate layer.
[0033] The Mg-doped TMDs layer in the device of the present invention introduces a large number of acceptor energy levels, realizes p-type doping of TMDs, and regulates the carrier concentration. The regulated carriers optimize the barrier height between the material and the electrode, reduce the dark current, enhance the rectification ratio, and improve the response speed of the device, which is of great significance for realizing high-performance and high-sensitivity photodetectors for visible light communication.
[0034] Compared with the prior art, the present invention has the following advantages:
[0035] The present invention utilizes molecular beam evaporation equipment to selectively evaporate the Mg layer, realizes in-situ doping during the growth process, forms a deep acceptor energy level, regulates the carrier type and concentration, and realizes P-type TMDs material. By combining with n-type InGaN material to construct a 2D / 3D heterojunction, the device performance is further improved. This method has the advantages of high in-situ doping efficiency and simple process, and is of great significance for realizing high-sensitivity photodetector devices for visible light communication. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Figure 1 This is a schematic diagram of the structure of the Mg-doped enhanced TMDs-based visible light detector of the present invention; 1-substrate, 2-InGaN layer, 3-Mg-doped TMDs layer, 4-electrode layer;
[0037] Figure 2 The flow chart of the preparation of the Mg-doped enhanced TMDs-based visible light detector of the present invention; 1-substrate, 2-InGaN layer, 3-Mg-doped TMDs layer, 4-electrode layer; 30-Mg layer;
[0038] Figure 3 This is a Raman characterization image of the epitaxially grown Mg-doped TMDs film on InGaN according to Example 1 of the present invention;
[0039] Figure 4 This is the current-voltage curve (365 nm) of the Mg-doped enhanced TMDs-based visible light detector prepared in Example 1 of the present invention under different ultraviolet light intensities. DETAILED DESCRIPTION
[0040] The following figures and examples further illustrate the future implementation of the present invention, but the implementation and protection of the present invention are not limited thereto. It should be noted that if there are any details not particularly described below, they can be implemented or understood by scientific researchers and technicians in this field with reference to the prior art.
[0041] The schematic diagram of the structure of the Mg-doped enhanced TMDs-based visible light detector of the present invention is as follows: Figure 1 As shown, it includes, from bottom to top, a Si substrate layer 1, an InGaN epitaxial layer 2, a Mg-doped transition metal sulfide (TMDs) layer 3, and an electrode layer 4. The electrode layer 4 is a first electrode layer and a second electrode layer; the first electrode layer is a Ti / Au layer, and the second electrode layer is a Ti / Au layer.
[0042] The Mg-doped transition metal sulfide layer 3 partially covers the InGaN epitaxial layer 2, and a mesa is formed on the upper surface of the InGaN epitaxial layer.
[0043] A first electrode layer is disposed on the table of the InGaN epitaxial layer 2, and the electrode layer is not in contact with the Mg-doped transition metal sulfide layer. The Ti layer in the first electrode layer is disposed on the table of the InGaN epitaxial layer. The Au layer is disposed on the Ti layer.
[0044] A second electrode layer is disposed on the Mg-doped transition metal sulfide layer 3. The second electrode layer partially covers the Mg-doped transition metal sulfide layer. In the second electrode layer, the Ti layer is disposed on the Mg-doped transition metal sulfide layer. The Au layer is disposed on the Ti layer.
[0045] Figure 2 The present invention is a flow chart for preparing a Mg-doped enhanced TMDs-based visible light detector; 1-substrate, 2-InGaN layer, 3-Mg-doped TMDs layer, 4-electrode layer; 30-Mg layer.
[0046] Example 1
[0047] This embodiment provides a Mg-doped enhanced transition metal sulfide (TMDs)-based visible light detector, comprising, from bottom to top, a Si substrate layer, an InGaN layer, a Mg-doped TMDs layer, a Ti electrode layer and a gold electrode layer.
[0048] This embodiment also provides a method for preparing a Mg-doped enhanced transition metal sulfide (TMDs)-based visible light detector, comprising the following steps:
[0049] 1) Spin-coating photoresist on the Si-based InGaN epitaxial wafer, and photolithography out the Mg layer evaporation area device (the Mg evaporation area is located at one end of the upper surface of the InGaN epitaxial wafer, partially covering the InGaN);
[0050] 2) using a molecular beam evaporation device to evaporate a layer of metal Mg on the evaporation area of step 1), wherein the thickness of the metal Mg is 10 nm, to obtain an epitaxial wafer device containing a metal Mg layer;
[0051] 3) stripping and cleaning the unexposed photoresist of the device containing the metallic Mg layer in step (2) to obtain a stripped Mg layer device;
[0052] 4) The Mg layer device of step (3) was subjected to single-zone chemical vapor deposition equipment, and the air in the tube was purged several times with argon gas. In an argon atmosphere at standard atmospheric pressure, molybdenum oxide and sulfur powder were used as precursors, and the precursors were heated to 730°C and 130°C, respectively, and epitaxially grown for 4 minutes to prepare an epitaxial Mg-doped MoS2 layer, thereby obtaining a Mg-doped MoS2 / InGaN layer device, and the Mg doping concentration was 2×10 18 ~6×10 18 cm -3 ; The Mg-doped MoS2 layer partially covers the InGaN layer, and the Mg-doped MoS2 layer is located at the other end of the upper surface of the InGaN layer;
[0053] 5) annealing the doped TMDs / InGaN layer device in step 4) in a sulfur atmosphere at an annealing temperature of 600° C. for 2 hours to obtain an annealed doped TMDs / InGaN layer device;
[0054] 6) Spin-coating a photoresist on the Mg-doped MoS2 layer and the InGaN layer not covered by the Mg-doped MoS2 layer in the MoS2 / InGaN layer device of step 5), and photolithography out an area of a desired electrode shape;
[0055] 7) using a molecular beam evaporation device to deposit Ti / Au electrodes with a thickness of 30 / 60 nm respectively on the device containing the electrode shape in step 6) to obtain a device containing an electrode layer;
[0056] 8) Stripping and cleaning the unexposed photoresist of the device containing the electrode layer in step (7) to obtain the Mg-doped enhanced MoS2 / InGaN visible light detector device.
[0057] Figure 3 This is a Raman characterization image of the epitaxially grown Mg-doped TMDs film on InGaN according to Example 1 of the present invention;
[0058] Figure 4 This is the current-voltage curve (365 nm) of the Mg-doped enhanced TMDs-based visible light detector prepared in Example 1 of the present invention under different ultraviolet light intensities.
[0059] Example 2
[0060] This embodiment provides a Mg-doped enhanced transition metal sulfide (TMDs)-based visible light detector, comprising, from bottom to top, a Si substrate layer, an InGaN layer, a Mg-doped TMDs layer, a Ti electrode layer and a gold electrode layer.
[0061] This embodiment also provides a method for preparing a Mg-doped enhanced transition metal sulfide (TMDs)-based visible light detector, comprising the following steps:
[0062] 1) Spin-coating photoresist on the Si-based InGaN epitaxial wafer and photolithography out the Mg layer evaporation area; the evaporation area is located at one end of the upper surface of the InGaN layer;
[0063] 2) using a molecular beam evaporation device to evaporate a layer of metal Mg on the evaporation area of step 1), wherein the thickness of the metal Mg is 20 nm, to obtain an epitaxial wafer device containing a metal Mg layer;
[0064] 3) stripping and cleaning the unexposed photoresist of the device containing the metal Mg layer in step 2) to obtain a stripped Mg layer device;
[0065] 4) The Mg layer device of step 3) was prepared by using a single temperature zone chemical vapor deposition device, and the air in the tube was purged several times with argon gas. In an argon atmosphere at standard atmospheric pressure, tungsten oxide and sulfur powder were used as precursors, and the precursors were heated to 750°C and 130°C, respectively, and epitaxially grown for 3 minutes to prepare an epitaxial Mg-doped WS2 layer, thereby obtaining a doped WS2 / InGaN layer device, and the Mg doping concentration was 2×10 18 ~6×10 18 cm -3 ; The Mg-doped WS2 layer partially covers the InGaN layer;
[0066] 5) annealing the doped WS2 / InGaN layer device in step 4) in a sulfur atmosphere at an annealing temperature of 700° C. for 1 h to obtain an annealed doped TMDs / InGaN layer device;
[0067] 6) Spin-coating photoresist on the doped WS2 / InGaN layer device described in step (5) to photoetch out a device containing an electrode shape;
[0068] 7) using a molecular beam evaporation device to deposit Ti / Au electrodes with a thickness of 40 / 80 nm respectively on the device containing the electrode shape in step 6) to obtain a device containing an electrode layer;
[0069] 8) Stripping and cleaning the unexposed photoresist of the device containing the electrode layer in step 7) to obtain the Mg-doped enhanced WS2 / InGaN visible light detector device.
[0070] Example 3
[0071] The present embodiment provides a Mg-doped enhanced transition metal sulfide (TMDs)-based visible light detector, comprising, from bottom to top, a Si substrate layer, an InGaN layer, a Mg-doped MoS2 layer, a Ti electrode layer and an Au electrode layer.
[0072] This embodiment also provides a method for preparing a Mg-doped enhanced transition metal sulfide (TMDs)-based visible light detector, comprising the following steps:
[0073] 1) Spin-coat photoresist on the Si-based InGaN epitaxial wafer and photolithograph the Mg layer evaporation area device;
[0074] 2) using a molecular beam evaporation device to deposit a layer of metal Mg on the device in step 1), wherein the thickness of the metal Mg is 50 nm, to obtain an epitaxial wafer device containing a metal Mg layer;
[0075] 3) stripping and cleaning the unexposed photoresist of the device containing the metal Mg layer in step 2) to obtain a stripped Mg layer device;
[0076] 4) The Mg layer device of step 3) was prepared by using a single temperature zone chemical vapor deposition device, and the air in the tube was purged several times with argon gas. In an argon atmosphere at standard atmospheric pressure, molybdenum oxide and sulfur powder were used as precursors, and the precursors were heated to 750°C and 140°C, respectively, and epitaxially grown for 4 minutes to prepare an epitaxial Mg-doped MoS2 layer, thereby obtaining a Mg-doped MoS2 / InGaN layer device, and the Mg doping concentration was 2×10 18 ~6×10 18 cm -3 ; The Mg-doped MoS2 layer partially covers the InGaN layer;
[0077] 5) annealing the Mg-doped MoS2 / InGaN layer device in step 4) in a sulfur atmosphere at an annealing temperature of 750° C. for 0.5 h to obtain an annealed MoS2 / InGaN layer device;
[0078] 6) Spin-coating the doped MoS2 / InGaN layer device in step 5) with photoresist, and photolithography out a device containing an electrode shape;
[0079] 7) using a molecular beam evaporation device to deposit Ti / Au electrodes with a thickness of 40 / 100 nm on the device containing the electrode shape in step 6) to obtain a device containing an electrode layer;
[0080] 8) Stripping and cleaning the unexposed photoresist of the device containing the electrode layer in step 7) to obtain the Mg-doped enhanced TMDs-based visible light detector device.
Claims
1. A Mg-doped enhanced transition metal sulfide-based visible light detector, characterized in that: It includes a Si substrate layer, an InGaN layer, a Mg-doped transition metal sulfide layer and an electrode layer arranged in sequence from bottom to top; the electrode layer is a first electrode layer and a second electrode layer; The Mg-doped transition metal sulfide layer partially covers the InGaN layer, and a mesa is formed on the upper surface of the InGaN layer; A first electrode layer is provided on the table of the InGaN layer, and the first electrode layer is not in contact with the Mg-doped transition metal sulfide layer; A second electrode layer is disposed on the Mg-doped transition metal sulfide layer; the second electrode layer partially covers the Mg-doped transition metal sulfide layer; The first electrode layer is a Ti / Au layer, and the second electrode layer is a Ti / Au layer; In the first electrode layer, a Ti layer is arranged on the table of the InGaN layer; and an Au layer is arranged on the Ti layer; In the second electrode layer, the Ti layer is disposed on the Mg-doped transition metal sulfide layer; and the Au layer is disposed on the Ti layer; The transition metal sulfide is also called a transition metal chalcogenide, and has a chemical formula of MX2, where M is one of molybdenum, tungsten, niobium, rhenium, and titanium, and X refers to a chalcogen element, specifically one of sulfur, selenium, and tellurium; the Mg doping concentration in the Mg-doped transition metal sulfide layer is 2×10 18 ~ 6×10 18 cm -3 .
2. The method for preparing the Mg-doped enhanced transition metal sulfide-based visible light detector according to claim 1, characterized in that: Specific steps: S1) spin-coating a positive photoresist on a Si-based InGaN epitaxial wafer, and photolithography out a vapor deposition area of the Mg layer, where the vapor deposition area is located at one end of the upper surface of the epitaxial wafer; S2) using molecular beam evaporation to deposit a layer of metal Mg in the evaporation area, stripping off the unexposed photoresist, and obtaining an epitaxial wafer device containing a Mg layer; S3) preparing an epitaxial Mg-doped TMDs layer on an epitaxial wafer device containing a Mg layer by chemical vapor deposition using transition metal oxides and chalcogenide sources as precursors, and performing annealing to obtain a doped TMDs / InGaN layer device; wherein the Mg-doped TMDs layer partially covers the InGaN layer in the device; S4) Spin-coating a photoresist on the doped TMDs / InGaN layer device, and photolithography out an electrode deposition area of a desired shape; the electrode deposition area is located on the Mg-doped TMDs layer and on the InGaN layer not covered by the Mg-doped TMDs layer; the Mg-doped TMDs layer refers to a Mg-doped transition metal sulfide layer; S5) using molecular beam evaporation to deposit a metal electrode in the deposition area, stripping off the unexposed photoresist, and obtaining a Mg-doped enhanced transition metal sulfide-based visible light detector; In step S3), the transition metal oxide is an oxide of molybdenum, tungsten, niobium, rhenium or titanium; the chalcogen source is sulfur, selenium or tellurium powder; The chemical vapor deposition is carried out in an argon atmosphere at standard atmospheric pressure; The chemical vapor deposition equipment in step S3) is a tube furnace; Chemical vapor deposition conditions: growth environment is 700 - 780 Torr argon atmosphere; transition metal oxide and chalcogenide source are heated at different temperatures, heating temperatures are 650 - 750 ° C, 100 - 140 ° C respectively; growth time is 2 - 6 minutes; The thickness of the Mg-doped TMDs layer is 1-100 nm; the Mg doping concentration in the Mg-doped TMDs layer is 2×10 18 ~ 6×10 18 cm -3 ; Step 3) annealing treatment: temperature is 600-750 °C, annealing time is 0.5-2 h; In step S5), the metal electrode is a Ti / Au layer, the Ti layer is disposed on the Mg-doped transition metal sulfide layer; the Au layer is disposed on the Ti layer; the thickness of the Ti layer and the Au layer are 30-60 nm and 60-150 nm respectively; The Si-based InGaN epitaxial wafer in step S1) is an InGaN single crystal or epitaxial wafer, the Si layer thickness is 300-400 um, and the InGaN epitaxial wafer thickness is 1-3 um; Step S2) The thickness of the Mg layer is 10-100 nm.
3. The use of the Mg-doped enhanced transition metal sulfide-based visible light detector according to claim 1, characterized in that: The Mg-doped enhanced transition metal sulfide-based visible light detector is used to prepare a photoelectric detector for visible light communication.
Citation Information
Patent Citations
Metal element-doped molybdenum disulfide film material and preparation method thereof
CN109467126A
2D WS2 / InGaN II type heterojunction self-driven blue light detector and preparation method and application thereof
CN113224198A
Transition metal dichalcogenides (TMDCS) over iii-nitride heteroepitaxial layers
US20180350921A1
Methods to deposit and etch controlled thin layers of transition metal dichalcogenides
US20190279870A1
Doped metal-chalcogenide thin film and method of manufacturing the same
US20200152477A1