Metal foam extrusion method and articles made therefrom

By injecting metal foam powder into the conduit and using a hot-pressure combination for activation, the problem of low efficiency and high cost of the existing metal foaming process is solved, achieving more efficient metal foam manufacturing and improving the impact absorption capacity of vehicle parts.

CN114273657BActive Publication Date: 2024-10-11GM GLOBAL TECHNOLOGY OPERATIONS LLC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110458253.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-10-01
Filing Date
2021-04-27
Publication Date
2024-10-11
Estimated Expiration
2041-04-27

AI Technical Summary

Technical Problem

The existing metal foaming process has challenges between improving the impact absorption capacity of vehicle components and reducing costs, and the existing process is not efficient.

Method used

The metal foam is formed by injecting metal foam powder into the conduit and activating it using a combination of heat and pressure. This specifically includes injecting metal foam powder into the cavity of the conduit, increasing the temperature through an induction coil or convection furnace, and applying pressure to promote Foam.

Benefits of technology

A more efficient metal foam manufacturing process is achieved, improving the impact absorption capabilities of vehicle components while reducing manufacturing costs and improving manufacturing efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114273657B_ABST
    Figure CN114273657B_ABST
Patent Text Reader

Abstract

A method for making a foam in a conduit includes extruding a metal conduit. A metal foam powder is injected into a cavity of the metal conduit. The metal foam powder is activated to form a metal foam in the cavity of the metal conduit. An apparatus for making a foamed metal includes an extruder including one or more screws for extruding metal through a die to form the conduit. The die includes a plurality of ports for injecting the metal foam powder into a central cavity or a wall cavity of the conduit. The apparatus includes a pressurizing portion for increasing the pressure on the metal foam powder and a heating portion for increasing the temperature of the metal foam powder to promote its expansion into a metal foam.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to methods of metal foam extrusion and articles made therefrom. In particular, the present disclosure relates to a method of extruding a metal foam inside a conduit or as part of a conduit wall. Background Art

[0002] Metal foams are often used to make reinforced components for vehicles that transport people or goods. Such vehicles include cars, bicycles and motorcycles, locomotives, aircraft, ships and boats. This reinforcement allows for greater energy absorption, thereby reducing damage to the vehicle and its occupants.

[0003] It would be desirable to improve the metal foaming process to make the process more efficient and less expensive while increasing the impact absorption capabilities of components used in vehicles. Summary of the invention

[0004] In one embodiment, a method for making a foam in a conduit includes extruding a metal conduit, injecting a metal foam powder into a cavity of the metal conduit, and activating the metal foam powder to form a metal foam in the cavity of the metal conduit.

[0005] In another embodiment, the cavity is a central cavity located concentrically relative to the catheter wall(s).

[0006] In yet another embodiment, the cavity is a central cavity disposed eccentrically relative to the catheter wall(s).

[0007] In yet another embodiment, the cavity is a wall cavity between an inner wall and an outer wall of the metal conduit.

[0008] In yet another embodiment, the metal conduit and the metal foam comprise the same metal.

[0009] In yet another embodiment, the metal conduit comprises a metal different from the metal foam.

[0010] In yet another embodiment, activation includes increasing the temperature and / or pressure of the metal foam powder.

[0011] In yet another embodiment, the temperature is 200 to 650°C.

[0012] In yet another embodiment, the temperature increase during the extrusion process is facilitated by an induction coil located at the extruder die and inside the conduit.

[0013] In another embodiment, the increase in pressure is achieved by a ram that enters the conduit and travels in the opposite direction to the direction of travel of the extrudate.

[0014] In yet another embodiment, the metal conduit and the metal foam include aluminum.

[0015] In one embodiment, an apparatus for making a foamed metal includes an extruder including one or more screws for extruding metal through a die to form a conduit. The die includes a plurality of ports for injecting a metal foam powder into a central cavity or a wall cavity of the conduit. The apparatus includes a pressurizing portion for increasing the pressure on the metal foam powder and a heating portion for increasing the temperature of the metal foam powder to promote its expansion into a metal foam.

[0016] In one embodiment, the pressurizing section comprises a roller mill or a press head that travels in the opposite direction to the extrudate.

[0017] In yet another embodiment, the heating portion includes a convection oven or an induction coil.

[0018] In yet another embodiment, the induction coil is close to the mold.

[0019] In one embodiment, an article includes a conduit containing a first metal. The conduit includes one or more cavities. At least one cavity contains a metal foam. The conduit wall surrounds the metal foam. The metal foam includes a second metal.

[0020] In one embodiment, the first metal is the same as the second metal.

[0021] In yet another embodiment, the first metal and the second metal are aluminum.

[0022] In yet another embodiment, one or more cavities are located between the inner wall and the outer wall of the conduit.

[0023] In yet another embodiment, the one or more lumens are concentrically positioned relative to the catheter wall.

[0024] The above features and advantages and other features and advantages of the present disclosure will become apparent from the following detailed description when taken in conjunction with the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Other features, advantages and details appear by way of example only in the following detailed description, which refers to the accompanying drawings, in which:

[0026] Figure 1 is an exemplary illustration of a catheter whose cavity is filled with metal foam;

[0027] Figure 2 An exemplary process for making a catheter having a central cavity filled with a metal foam is described; and

[0028] Figure 3 Another exemplary process for making a catheter having a wall cavity filled with a metal foam is depicted. DETAILED DESCRIPTION

[0029] The following description is merely exemplary in nature and is not intended to limit the present disclosure, its application, or uses.

[0030] Disclosed herein is a method for making a metal foam surrounded by a metal sheath. The metal sheath preferably forms a wall around the foam and encapsulates the foam. In one embodiment, the metal sheath is a conduit wall containing the foam; the foam is located in the central cavity of the conduit. In another embodiment, the foam may be contained in a cavity in the conduit wall (hereinafter referred to as a "wall cavity"). In another embodiment, the foam may be located in the central cavity of the conduit, in the wall cavity, and in both the central cavity and the wall cavity. The density of the metal foam is 3 to 15 percent of the density of the unfoamed metal and may or may not have the same metal component as the conduit wall.

[0031] The method includes extruding a conduit having one or more cavities containing foam. The extrusion of the conduit and the foaming of the metal in the cavity occur simultaneously. The foaming occurs by injecting metal foam powder into the one or more cavities of the conduit and activating the metal foam powder by using a combination of heat and pressure.

[0032] Figure 1 An exemplary catheter 100 is depicted, which includes a foam 106 located in a central cavity 102 and a wall cavity 104 of the catheter 100. The catheter can have a cross-sectional geometry that is circular, oval, square, triangular, rectangular, polygonal, or a combination thereof. It can also have an irregular cross-sectional geometry if desired. Although Figure 1 The foam is depicted as being disposed in the central cavity 102 as well as the wall cavity 104, but it should be noted that the foam may be located in one or more of these locations as desired. The central cavity 102 is located concentrically relative to the conduit wall(s). The central cavity 102 may also be located eccentrically relative to the conduit wall(s). The conduit is preferably made of a first metal and the foam is made of a second metal. The first metal may be the same or different than the second metal. In a preferred embodiment, the first metal is the same as the second metal.

[0033] When the first metal is different from the second metal, it is desirable that the melting point of the first metal (forming the conduit wall) is higher than the melting point of the second metal (forming the foam).

[0034] Now refer to it again Figure 1 , the conduit 100 can be divided into an inner wall 103 and an outer wall 105, and the wall cavity 104 between the inner wall and the outer wall can be filled with foam 106. The division of the conduit 100 will be discussed in detail later. It should be noted that the foam 106 in the central cavity 102 can be the same as or different from the foam in the wall cavity 104. For example, the central cavity 102 can contain a first metal foam that is different from the second metal foam contained in the wall cavity 104.

[0035] In another embodiment, the conduit 100 can be divided into multiple walls (2 or more walls), some or all of which can be filled with metal foam. For example, the conduit can be divided into an inner wall, an outer wall and 2 to 5 intermediate walls (the intermediate walls are located between the inner wall and the outer wall), and if necessary, the cavities therebetween are filled with metal foam.

[0036] In one embodiment, the foamed first metal and / or the foamed second metal may contain additional foaming polymer. The average pore size of the polymer foam is preferably smaller than the average pore size of the metal foam. The presence of the foamed polymer in the foamed metal improves the impact absorption capacity of any component made from the metal foam.

[0037] The first metal and the second metal include transition metals or alloys containing transition metals. The metals referred to herein are preferably in their elemental form. Examples of suitable first and / or second metals include iron, aluminum, copper, titanium, tungsten, nickel, cobalt, tin, lead, silicon, magnesium, manganese, vanadium, molybdenum, gallium, indium, thallium, gold, silver, etc., or combinations thereof. In one embodiment, aluminum is a preferred first metal. In another embodiment, aluminum is also a preferred second metal.

[0038] Alloys may also be extruded into conduits containing metal foams. Suitable alloys are stainless steel, carbon steel, titanium aluminum alloy, iron alloy, ferroboron, ferrochrome (chromium), iron magnesium, ferromanganese, ferromolybdenum, ferronickel, ferrophosphorus, ferrotitanium, ferrovanadium, ferrosilicon, aluminum-lithium (aluminum, lithium, and sometimes mercury), aluminum nickel cobalt (aluminum, nickel, copper), duralumin (copper, aluminum), magnesium aluminum (aluminum, 5 percent magnesium), Magnox (magnesium oxide, aluminum), Nambe (aluminum plus seven other unspecified metals), silicon aluminum (aluminum, silicon), Billon (copper, silver), brass (copper, zinc), calamine brass (copper, zinc), Chinese silver (copper, zinc), Dutch metal (copper, zinc), gold plated metal (copper, zinc), Muntz metal (copper, zinc), Pinchbeck (copper, zinc), Prince's metal (copper, zinc), metal) (copper, zinc), Tombach (copper, zinc), Bronze (copper, tin, aluminum or any other element), Alumel (nickel, manganese, aluminum, silicon), Chromel (nickel, chromium), Cupronickel (nickel, bronze, copper), German silver (nickel, copper, zinc), Hastelloy (nickel, molybdenum, chromium and sometimes tungsten), Inconel (nickel, chromium, iron), Monel metal (copper, nickel, iron, manganese), Mu metal (nickel, iron), Nickel-Carbon (nickel, carbon), Nichrome (chromium, iron, nickel), Nichrome (nickel, chromium, silicon, magnesium), Nisil (nickel, silicon), Nitinol (nickel, titanium, shape memory alloy).

[0039] The preferred metal for the conduit 100 and the foam 106 contained therein is aluminum.

[0040] The metal foam may include open cells, closed cells, or a combination thereof. In one embodiment, the metal foam may include 5 to 95 volume percent, preferably 20 to 80 volume percent, of open cells, with the remainder being closed cells.

[0041] The metal foam preferably includes a plurality of open cells. The foam also has some closed cells disposed between the open cells. However, the majority of cells in the metal foam are open cells. For a given density, the open cell foam provides the foam with higher energy absorption properties.

[0042] In one embodiment, at least 80% of the cells are open cells, preferably at least 90% of the cells are open cells, and more preferably at least 95% of the cells are open cells. The average pore size of the metal foam is 0.5 micrometers to 10 millimeters, preferably 50 micrometers to 5 millimeters, and more preferably 100 micrometers to 2 millimeters. The volume porosity of the metal foam is 50 to 95 volume percent, preferably 70 to 90 volume percent, based on the total volume of the metal foam.

[0043] Preferred aluminum foams have a density of 0.069 to 0.54 g / cm3, an average pore size of 25 μm to 3 μm, and a wall thickness of 50 to 85 μm. The average cell size is inversely proportional to the average cell wall thickness and density.

[0044] The metal foam 106 is made of metal foam powder. The metal foam powder may include a) metal powder with a foaming agent, and / or b) metal hollow spheres, which include organic spheres with a metal powder-binder suspension disposed thereon. Each of these is described in detail below.

[0045] When the viscosity of the molten metal is properly established, metal foam is obtained by adding a foaming agent to the molten metal. The foaming agent is usually a powder of a metal hydride, such as TiH 2 , decomposes to form hydrogen when heated above 400°C. Other metal hydrides with decomposition temperatures between 280 and 600°C, such as zirconium and magnesium hydrides, can also be used as blowing agents.

[0046] When the foaming agent comes into contact with the molten metal, the molten metal decomposes immediately and therefore there is insufficient time to achieve a uniform distribution of the gas-forming particles.

[0047] Non-ferrous metal foams use conventional blowing agents and metal powders. Commercially available powders (e.g., aluminum, zinc, tin, or lead) are mixed with the blowing agent by conventional means, such as a drum mixer. After mixing, the powder mixture is compacted to obtain a dense, almost non-porous object. Several compaction methods can be used, such as uniaxial pressing, powder extrusion, and even roller compaction. When this dense mass is heated to a temperature near the melting point, it expands into a highly porous cellular body. Various blowing agents have been shown to produce good results.

[0048] The blowing agents used include metal hydrides, such as titanium, zirconium and magnesium hydrides, which have decomposition temperatures between 280 and 600°C.

[0049] Metallic hollow sphere (MHS) foam structure provides a new type of foam metal. This technology ensures controlled manufacturing of single pores to single MHS and reproducible structure of customized parts. First, various metals (such as nickel, cobalt and copper) are electrodeposited on a spherical substrate.

[0050] An organic spherical substrate made primarily of foamed polystyrene is used as a cell-forming undercoat. A metal powder-binder suspension is atomized onto the exterior of the organic sphere substrate. A heat treatment process produces metal foam, while the binder and organic sphere substrate are removed by subsequent heat treatment. There are several methods to merge individual hollow spheres into MHS parts, including sintering, brazing, and bonding.

[0051] The metal foam powder is injected into a suitable cavity during the extrusion process and is transformed into metal foam by using appropriate high temperature and high pressure.

[0052] Figure 2 and Figure 3 An exemplary process for producing a metal foam in a catheter is described. Figure 2 An exemplary process for making a conduit 100 using an extruder 202 is described, wherein the central cavity 102 (defined by the conduit wall 104) of the conduit 100 is filled with a metal foam 106. The extruder has a die 204 attached thereto, which facilitates the extrusion of the conduit 100. As indicated by the arrow, the direction of travel of the extrudate 500 is from right to left (facing the observer of the paper). The die 204 includes a port 206 through which a metal foam powder 101 can be fed into the interior 102 of the conduit 100. The die 204 can also be provided with a separate heating device, such as an induction coil 208, which can heat the metal foam powder 101 to produce the metal foam 106. Alternatively, the extrudate (conduit 100) can pass through a convection oven 210, which heats the metal foam powder 101 to convert it into the metal foam 106 in the conduit 100. Pressure 212 can be applied to the metal foam powder in the conduit through the open end of the conduit 100 to facilitate the foaming process. For example, a plunger or ram (not shown) may be directed to apply pressure to the metal foam powder from the open end of the conduit toward the extruder inside the conduit, thereby converting it into metal foam. In other words, the increase in pressure on the foam powder is achieved by the ram entering the conduit and traveling in the opposite direction of travel of the extrudate. Applying high temperature and high pressure to the metal foam powder 101 converts it into metal foam 106.

[0053] The metal foam 106 is produced by heating the metal foam powder 101 to a temperature of 200 to 640°C, preferably 250 to 620°C, and more preferably 300 to 600°C.

[0054] A pressure of 20 to 120 kPa, preferably 30 to 100 kPa, may be applied to the metal foam powder in the central cavity of the conduit to convert it into metal foam.

[0055] Figure 3A process is described for making a catheter 100 having a wall with a cavity 104 filled with a metal foam 106. The process uses an extruder 202 with a die 204 to make a catheter 100 having multiple walls 103, 105. The extruder may be a single screw or a multi-screw extruder. Figure 3 A mold 204 is depicted, which can make two walls in the conduit 100, an inner wall 103 and an outer wall 105. The mold 204 includes a splitter 205, which splits an initial stream 207 of molten metal into two streams 209 and 211. Stream 209 forms the inner wall 103, while stream 211 forms the outer wall 105. A stream of metal foam powder 101 can be injected into the wall cavity 104 through, for example, a port 212 in the splitter 205. Then, in the device 214, the conduit 100 containing the metal foam powder 101 in the cavity 104 between the inner tube 103 and the outer tube 105 is subjected to high temperature and pressure. The device 214 can include a roller mill combined with a convection oven. The roller mill can be used to apply pressure on the conduit, while the convection oven can be used to increase the temperature of the conduit to activate the metal foam powder, thereby promoting its conversion into metal foam 106. The metal foam 106 is contained between the inner wall 103 and the outer wall 105. The temperature and pressure used to foam the metal foam powder 101 within the wall cavity are the same as detailed above.

[0056] In one embodiment (not shown), the metal foam may be produced simultaneously in the central cavity 102 and the wall cavity 104. In other words, Figure 2 The embodiments described in detail in Figure 3 It should be noted that although Figure 2 and Figure 3 The process in is a continuous process, but foam metal parts can also be manufactured in a batch process. Continuous processes are preferred because of their lower energy costs and because the manufacturing speed is increased.

[0057] from Figure 2 and Figure 3 It can be seen that the apparatus for making metal foam in a conduit includes an extruder, a device or part for increasing the pressure on the metal foam powder, and a heating part for increasing the temperature on the metal foam powder. The extruder includes one or more screws for extruding metal through a die to form a conduit.

[0058] The mold includes one or more ports for injecting metal foam powder into the central cavity or wall cavity of the conduit. In one embodiment, the mold includes a plurality of ports for injecting metal foam powder into the central cavity or wall cavity of the conduit.

[0059] The pressurizing section increases the pressure on the metal foam powder. The pressurizing section includes a pressure head or plunger that travels in a direction opposite to the direction of travel of the extrudate 500. In one embodiment, the pressurizing section may include a roller mill. The heating section increases the temperature of the metal foam powder to promote its expansion into metal foam. The heating section includes a convection oven or an induction coil. The induction coil is located on or near the die (of the extruder).

[0060] In one embodiment, metal foam powder can be mixed with expandable polymer powder (eg, EXPANCEL) to produce metal foam interspersed with polymer foam. The combination of metal foam and polymer foam will give the foam part improved impact performance and sound absorption capabilities.

[0061] Examples of polymer foams include polystyrene, polyurethane, polyacrylate, polycarbonate, polyolefin, etc., or combinations thereof.

[0062] Metal foams made in the manner detailed herein have many advantages. They can be made continuously in one step, thereby reducing manufacturing costs. Aluminum foam can be formed only on certain walls of the conduit to fine-tune performance. The use of metal foams (e.g., aluminum foam) will allow product designs that can take advantage of higher wall stiffness without significantly increasing mass by using metal foams in critical areas for energy attenuation.

[0063] Articles made in the manner described herein may be used in vehicles, such as automobiles, bicycles and motorcycles, aircraft, locomotives, ships and other marine vessels.

[0064] Although the above disclosure has been described with reference to exemplary embodiments, it will be appreciated by those skilled in the art that various changes may be made and equivalents may be substituted for its elements without departing from the scope of the present invention. In addition, many modifications may be made to adapt specific circumstances or materials to the teachings of the present disclosure without departing from the basic scope of the present disclosure. Therefore, it is intended that the present disclosure is not limited to the specific embodiments disclosed, but will include all embodiments falling within its scope.

Claims

1. A device for producing foamed metal, comprising: Mould Extruder, including: one or more screws for extruding metal through the die to form the conduit; in, The mold includes a plurality of ports for injecting metal foam powder into the central cavity or the wall cavity of the catheter; a pressurizing section downstream of the die and configured to provide pressure in the central cavity or the wall cavity of the conduit for applying pressure to the metal foam powder from the open end of the conduit toward the extruder; and The heating part is used to increase the temperature of the metal foam powder to promote its expansion into metal foam.

2. A method of forming a metal conduit having a metal foam in a cavity using the apparatus of claim 1, comprising: extruding a metal conduit having a cavity; injecting metal foam powder into the cavity of the metal conduit; and The metal foam powder is activated by applying pressure to the metal foam powder in the cavity from the open end of the conduit toward the extruder and increasing the temperature of the metal foam to form a metal foam in the cavity of the metal conduit.

3. The method of claim 2, wherein the cavity is a central cavity located concentrically relative to the catheter wall. The method of claim 2 , wherein the cavity is a central cavity located eccentrically relative to the catheter wall.

5. The method of claim 2, wherein the cavity is a wall cavity between an inner wall and an outer wall of the metal conduit.

6. The method of claim 2, wherein the metal conduit and the metal foam comprise the same metal.

7. The method of claim 2, wherein the temperature is 200 to 650°C.

8. The method according to claim 7, characterized in that During the extrusion process, an induction coil located at the extrusion die and inside the tube assists in increasing the temperature, and wherein the increase in pressure is achieved by a ram that enters the tube and travels in the opposite direction to the travel of the extruded metal tube.