A kind of semi-solid rapid pulping method of aluminum alloy

By setting a cooling runner on the stirring head and using a mechanical manual automation operation, combined with rotating shaft and blade design, the problems of low pulping efficiency and insufficient safety in the existing aluminum alloy pulping technology are solved, and fast and safe Aluminum alloy semi-solid pulping process.

CN114309493BActive Publication Date: 2024-11-22ANHUI XISU MACHINERY TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111392612.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-11-23
Publication Date
2024-11-22
Estimated Expiration
2041-11-23

AI Technical Summary

Technical Problem

The existing aluminum alloy pulping technology has low pulping efficiency and is unsafe, which can easily lead to melt splashing and affect production safety.

Method used

A semi-solid rapid pulping method of aluminum alloy is adopted. By setting a cooling runner on the stirring head and using mechanical manual automation, the stirring head and the container are moved with each other, combining the rotating shaft and blade design to generate shear force and cooling. The effect is to reduce the temperature of the aluminum alloy melt and the formation time of dendrites.

Benefits of technology

Improves pulping speed and safety, reduces workers' labor intensity and potential damage risks, avoids the harm of metal molten steam to the operator, and increases the cooling area and shear force, so that the dendrites are more evenly dispersed, improving pulping efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114309493B_ABST
    Figure CN114309493B_ABST
Patent Text Reader

Abstract

The present invention discloses a semi-solid rapid slurrying method for aluminum alloy, comprising: placing aluminum alloy melt in a container, extending a stirring head below the liquid level of the aluminum alloy melt in the container and rotating around the axis of the stirring head to stir the aluminum alloy melt; a cooling flow channel is formed on the stirring head, the cooling flow channel is at least partially located below the liquid level of the aluminum alloy melt, and the upper part of the stirring head has a cooling inlet and a cooling outlet connected to the cooling flow channel; during the rotation of the stirring head, the cooling medium flows in the cooling flow channel and exchanges heat with the aluminum alloy melt to reduce the temperature of the aluminum alloy melt, and the fluid in the cooling flow channel does not directly contact the aluminum alloy melt during the heat exchange process. Compared with the prior art, the present invention arranges a cooling flow channel inside the rotating shaft, so that the stirring head generates shear force when stirring the aluminum alloy melt, and heat is exchanged by the fluid flowing through the cooling flow channel inside the stirring head, thereby promoting the generation of dendrites, so that the slurrying process is faster.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of aluminum alloy pulping, and in particular to a semi-solid rapid pulping method for an aluminum alloy. Background Art

[0002] Semi-solid forming technology refers to the process of performing certain technical treatments on the metal during the solidification process (such as mechanical stirring, adding grain refiners, etc.) to change the nucleation and growth mode of the primary solid phase or to fully break up the formed dendrites to obtain a semi-solid slurry containing a nearly spherical or rose-shaped primary solid phase.

[0003] When preparing the slurry, the shear force generated by stirring is used to fully break up and free the dendrites formed during the solidification process, so that a large number of fine grains are evenly distributed in the molten metal. The slurrying methods based on stirring mainly include mechanical stirring, electromagnetic stirring, and later ultrasonic vibration, gas stirring, air-cooling stirring, etc. The slurrying rate is slow if it is achieved only by mechanical stirring.

[0004] The gas stirring method was first proposed by Wannas in et al. of Prince of Songkla University in Thailand and has now been successfully commercialized. The main process of the gas induction method is: using porous graphite media to input fine inert bubbles into the molten metal to rapidly cool the molten metal. The melt temperature is cooled from a few degrees above the liquidus line to a certain temperature below the liquidus line. The stirring effect caused by the bubbles acts on the melt to produce a nearly spherical structure. This process is mainly for semi-solid slurries with a lower solid phase ratio. However, this method is prone to cause melt splashing, which creates unsafe factors in production.

[0005] In view of this, the applicant conducted in-depth research on the above-mentioned defects in the prior art, which resulted in the present case. Summary of the invention

[0006] The main purpose of the present invention is to provide a semi-solid rapid pulping method for aluminum alloy, solve the problem of low pulping efficiency of the existing pulping technology, and provide a pulping method with good safety and high pulping speed.

[0007] In order to achieve the above object, the solution of the present invention is:

[0008] A method for rapid semi-solid slurrying of an aluminum alloy, comprising placing an aluminum alloy melt in a container, extending a stirring head below the liquid level of the aluminum alloy melt in the container and rotating around the axis of the stirring head to stir the aluminum alloy melt; a cooling channel is formed on the stirring head, the cooling channel is at least partially located below the liquid level of the aluminum alloy melt, and the upper portion of the stirring head has a cooling inlet and a cooling outlet connected to the cooling channel; during the rotation of the stirring head, a cooling medium flows in the cooling channel and exchanges heat with the aluminum alloy melt to reduce the temperature of the aluminum alloy melt, and during the heat exchange process, the fluid in the cooling channel does not directly contact the aluminum alloy melt.

[0009] Furthermore, the container is connected to a first manipulator, which drives the container to move in space. The first manipulator drives the container to hold the aluminum alloy melt and move it under the stirring head to pour out the aluminum alloy melt after slurrying.

[0010] Furthermore, the stirring head is mounted on a second manipulator, and the second manipulator drives the stirring head to move in space so as to extend the stirring head below the liquid level of the aluminum alloy melt in the cavity.

[0011] Furthermore, the stirring head includes a rotating shaft and a blade arranged on the rotating shaft, the rotating shaft is formed with a first flow channel and a second flow channel respectively arranged along the axial direction of the rotating shaft, and the blade is formed with a third flow channel; the first flow channel, the second flow channel and the third flow channel constitute a cooling flow channel; the first flow channel is connected to the cooling inlet, the second flow channel is connected to the cooling outlet, the cooling medium enters the first flow channel from the cooling inlet, the third flow channel is connected to the first flow channel and the second flow channel respectively, and the cooling medium then flows from the second flow channel to the cooling outlet.

[0012] Furthermore, a coil is formed outside the blade, the coil is fixedly connected to the blade, and the third flow channel is formed inside the coil.

[0013] Furthermore, a side of the coil close to the rotating shaft is fixedly connected to the rotating shaft by welding through a first connecting block, and an end of the coil away from the rotating shaft is connected to the blade by welding through a second connecting block.

[0014] Further, the third flow channel is formed inside the blade, and the thermal conductivity of the blade is greater than the thermal conductivity of the rotating shaft.

[0015] Furthermore, the blades are made of copper, the rotating shaft is made of steel, and the blades are welded to the rotating shaft.

[0016] Furthermore, the connection points between the third flow channel and the first flow channel and the second flow channel are both located at the lowest point of the third flow channel.

[0017] Further, the cooling inlet includes a first annular flow channel formed on the upper part of the rotating shaft and a first through hole connected to the first flow channel; the cooling outlet includes a second annular flow channel formed on the upper part of the rotating shaft and a second through hole connected to the second flow channel; the first annular flow channel and the second annular flow channel are spaced apart in the axial direction of the rotating shaft; a first connecting ring is rotatably sealed and connected to the rotating shaft outside the first annular flow channel, and an input pipe is connected to the first connecting ring; a second connecting ring is rotatably sealed and connected to the rotating shaft outside the second annular flow channel, and an output pipe is connected to the second connecting ring; when the rotating shaft rotates, the first connecting ring and the second connecting ring remain relatively fixed to the main shaft mounting seat that fixes the rotating shaft and do not rotate with the rotating shaft.

[0018] After adopting the above structure, the semi-solid rapid pulping method of aluminum alloy according to the present invention has at least the following beneficial effects:

[0019] 1. The rotation of the stirring head generates shear force on the aluminum alloy melt in the container, thereby breaking and separating the dendrites formed during the solidification process. At the same time, a cooling flow channel is arranged in the stirring head, through which a cooling fluid flows, which accelerates the cooling of the aluminum alloy melt and promotes the formation of dendrites, thereby reducing the time required for slurrying.

[0020] Second, by setting the first manipulator and the second manipulator, the container and the stirring head can be moved in space to cooperate with each other, and the stirring head can be automatically extended into or extended from the container, which reduces the labor intensity of the workers and avoids the risk of high temperature burns, while also avoiding the potential harm of the molten metal steam to the operator through breathing. The stirring head can also be fixed on the frame, and the relative movement of the stirring head and the container can be achieved only by the first manipulator driving the container to move.

[0021] 3. The stirring head includes a rotating shaft and blades arranged on the rotating shaft. By arranging a plurality of blades, the blades can not only increase the shear force generated by the stirring head, but also provide installation space for the cooling channel. The cooling fluid flowing through the first channel flows into the third channel, which greatly increases the heat exchange area between the cooling fluid and the aluminum alloy melt.

[0022] Fourth, the third flow channel can be formed inside the blade, and the third flow channel exchanges heat with the aluminum alloy melt through the blade. The blade is preferably made of a material with a thermal conductivity greater than that of the rotating shaft, such as copper. The rotating shaft is made of steel to ensure the rigidity of the rotating shaft and the stability during rotation.

[0023] Fifth, the third flow channel can also be formed by a coil, the coil is connected to the outer edge of the blade in an S shape, and the coil is welded to the rotating shaft and the blade through a first connecting block and a second connecting block. In this way, the outer surface of the coil is in contact with the aluminum alloy melt, and the contact area is large. In addition, the coil can also shear the aluminum alloy melt, and the coil and the blade cooperate to generate a greater shear force.

[0024] 6. The upper part of the rotating shaft is provided with a first annular flow channel and a second annular flow channel, and the first connecting ring and the second connecting ring are connected respectively, so that the cooling fluid is input through the input pipe, and the cooling fluid is continuously transported to the first flow channel through the first annular flow channel. The fluid in the second flow channel is continuously discharged to the second connecting ring through the second annular flow channel, and the rotation of the rotating shaft will not affect the arrangement of the input pipe and the output pipe, and the overall structure is simple and compact, which is convenient for installation.

[0025] Compared with the prior art, the present invention provides a cooling channel inside the rotating shaft, so that the stirring head generates shear force when stirring the aluminum alloy melt, and heat is exchanged by passing fluid through the cooling channel inside the stirring head, thereby promoting the generation of dendrites. The mechanical action of the shear force of stirring makes the dendrites more dispersed, and the combination of the two makes the semi-solid slurrying process of the aluminum alloy melt faster. Since the fluid is inside the stirring head, the fluid does not contact the aluminum alloy melt, and it is not easy to cause the aluminum alloy melt to splash. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 The present invention relates to a schematic diagram of the use status of a stirring head and a container used in a method for rapid semi-solid slurrying of an aluminum alloy.

[0027] Figure 2 It is a front view structural schematic diagram of the stirring head of the first embodiment.

[0028] Figure 3 It is a schematic cross-sectional structural diagram of the stirring head of the first embodiment.

[0029] Figure 4 for Figure 3 Schematic diagram of the enlarged structure at point A in the middle.

[0030] Figure 5 It is a schematic diagram of the three-dimensional structure of the stirring head of the first embodiment.

[0031] Figure 6 and Figure 7 Schematic diagram of the three-dimensional structure of the rotating shaft with coils on blades at different angles.

[0032] Figure 8 It is a schematic diagram of a partially enlarged structure of a rotating shaft with a coil on a blade.

[0033] Fig. 9 It is a schematic cross-sectional structure diagram of the blade of the second embodiment.

[0034] In the figure:

[0035] Container 1; aluminum alloy melt 11;

[0036] Stirring head 2; cooling channel 20; rotating shaft 21; sealing plug 211; first bearing 212; second bearing 213; C-shaped retaining ring 214; gear 215;

[0037] Cooling inlet 22; first annular flow channel 221; first through hole 222; first connecting ring 223; input pipe 224; one-way valve 225;

[0038] Cooling outlet 23; second annular flow channel 231; second through hole 232; second connecting ring 233; output pipe 234; first flow channel 24; second flow channel 25;

[0039] Blade 3; coil 31; first connection block 311; second connection block 312; third flow channel 32; reinforcing rib 33. DETAILED DESCRIPTION

[0040] In order to further explain the technical solution of the present invention, the present invention is described in detail below through specific embodiments.

[0041] like Figures 1 to 9 As shown, it is a semi-solid rapid slurrying method of aluminum alloy involved in the present invention, comprising: placing an aluminum alloy melt 11 in a container 1, extending a stirring head 2 below the liquid level of the aluminum alloy melt 11 in the container 1 and rotating around the axis of the stirring head 2 to stir the aluminum alloy melt 11; a cooling flow channel is formed on the stirring head 2, and the cooling flow channel is at least partially located below the liquid level of the aluminum alloy melt 11, and the upper part of the stirring head 2 has a cooling inlet 22 and a cooling outlet 23 connected to the cooling flow channel; during the rotation of the stirring head 2, the cooling medium flows in the cooling flow channel and exchanges heat with the aluminum alloy melt 11 to reduce the temperature of the aluminum alloy melt 11, and the fluid in the cooling flow channel does not directly contact the aluminum alloy melt 11 during the heat exchange process.

[0042] Thus, the invention relates to a method for rapid semi-solid slurrying of aluminum alloys. The rotation of the stirring head 2 generates shear force on the aluminum alloy melt 11 in the container 1, thereby breaking and separating the dendrites formed during the solidification process. At the same time, a cooling flow channel 20 is provided in the stirring head 2, in which a cooling fluid flows, accelerating the cooling of the aluminum alloy melt 11 and promoting the formation of dendrites, thereby reducing the time required for slurrying. Since the shear force is generated by stirring while the temperature is lowered by the stirring head 2, the dendrites are dispersed by the stirring head 2 after they are generated, and the dendrites are more evenly distributed in the aluminum alloy melt 11.

[0043] Preferably, the container 1 is connected to a first manipulator (not shown in the figure), the first manipulator drives the container 1 to move in space, the first manipulator drives the container 1 to hold the aluminum alloy melt 11 and move it below the stirring head 2 and pour out the aluminum alloy melt 11 after slurrying. The stirring head 2 is installed on a second manipulator (not shown in the figure), and the second manipulator drives the stirring head 2 to move in space to extend the stirring head 2 below the liquid level of the aluminum alloy melt 11 in the cavity. By setting the first manipulator and the second manipulator, the container 1 and the stirring head 2 can be moved in space to cooperate with each other, and the stirring head 2 can be automatically extended from the container 1, which reduces the labor intensity of the workers and avoids the risk of high temperature burns, and also avoids the metal vapor of the molten metal from causing potential harm to the operator through breathing. The stirring head 2 can also be fixedly installed on the frame, and the relative movement of the stirring head 2 and the container 1 can be achieved only by the first manipulator driving the container 1 to move.

[0044] The first manipulator and the second manipulator are multi-degree-of-freedom servo manipulators, which can operate with high accuracy and for a long time through programmed stored programs.

[0045] Preferably, if Figure 3 and Fig. 9 As shown, the stirring head 2 includes a rotating shaft 21 and a blade 3 arranged on the rotating shaft 21, the rotating shaft 21 is formed with a first flow channel 24 and a second flow channel 25 respectively arranged along the axial direction of the rotating shaft 21, and a third flow channel 32 is formed on the blade 3; the first flow channel 24, the second flow channel 25 and the third flow channel 32 constitute a cooling flow channel 20; the first flow channel 24 is connected to the cooling inlet 22, the second flow channel 25 is connected to the cooling outlet 23, the cooling medium enters the first flow channel 24 from the cooling inlet 22, the third flow channel 32 is connected to the first flow channel 24 and the second flow channel 25 respectively, and the cooling medium then flows from the second flow channel 25 to the cooling outlet 23. The stirring head 2 includes a rotating shaft 21 and blades 3 arranged on the rotating shaft 21. By arranging a plurality of blades 3, the blades 3 can not only increase the shear force generated by the stirring head 2, but also provide an installation space for the cooling channel 20. The cooling fluid flowing through the first channel 24 flows into the third channel 32, which greatly increases the heat exchange area between the cooling fluid and the aluminum alloy melt 11.

[0046] Furthermore, a protective coating is provided on the surface of the rotating shaft and the blades; the protective coating plays an anti-corrosion role, thereby extending the service life of the rotating shaft and the blades, and preventing iron elements from entering the aluminum liquid, resulting in an excessively high iron content in the aluminum liquid.

[0047] Preferably, if Figures 2 to 8As shown, a coil 31 is formed on the outside of the blade 3 (preferably, a protective coating is also provided on the surface of the coil), the coil 31 is fixedly connected to the blade 3, and the third flow channel 32 is formed in the coil 31. Preferably, the side of the coil 31 close to the rotating shaft 21 is welded and fixedly connected to the rotating shaft 21 through a first connecting block 311, and the end of the coil 31 away from the rotating shaft 21 is welded and connected to the blade 3 through a second connecting block 312. The third flow channel 32 can be formed by means of a coil 31, the coil 31 is connected to the outer edge of the blade 3 in an S shape, and the coil 31 is welded and connected to the rotating shaft 21 and the blade 3 through a first connecting block 311 and a second connecting block 312. In this way, the outer surface of the coil 31 contacts the aluminum alloy melt 11, and the contact area is large. Moreover, the coil 31 can also shear the aluminum alloy melt 11, and the coil 31 cooperates with the blade 3 to generate a greater shear force.

[0048] Furthermore, the blade 3 includes two symmetrical parts, and a reinforcing rib 33 is provided between the left and right blades 3, and the reinforcing rib 33 is provided perpendicular to the blade 3. Preferably, the coil 31 is a copper coil 31, and the coil 31 includes two parts, a left part and a right part, according to the layout of the blade 3, and the upper ends of the left and right coils 31 are connected to each other through a pipe. In this way, the connection between the blade 3 and the rotating shaft 21 is more secure, and can withstand a greater reaction force of the aluminum alloy melt 11 on the blade 3.

[0049] As a second implementation of the third flow channel 32, Fig. 9 As shown, preferably, the third flow channel 32 is formed inside the blade 3, and the thermal conductivity of the blade 3 is greater than the thermal conductivity of the rotating shaft 21. The third flow channel 32 can be formed inside the blade 3, and the third flow channel 32 exchanges heat with the aluminum alloy melt 11 through the blade 3. The blade 3 is preferably made of a material with a thermal conductivity greater than that of the rotating shaft 21, such as copper. In order to facilitate the molding of the third flow channel 32, the blade 3 is pre-molded and the third flow channel 32 is then welded and fixedly connected to the rotating shaft 21. Preferably, the material of the blade 3 is copper, and the rotating shaft 21 is steel, and the blade 3 is welded and connected to the rotating shaft 21. The rotating shaft 21 is made of steel to ensure the rigidity of the rotating shaft 21 and the stability during rotation. The third flow channel 32 is formed inside the blade 3, such as Fig. 9 As shown, the third flow channels 32 in the uppermost blades 3 on the left and right sides are connected by pipes.

[0050] The fluid in the cooling channel 20 may be gas or liquid, preferably liquid, such as water. After the liquid enters the cooling channel 20, part or all of the liquid vaporizes to absorb heat, thereby better cooling the aluminum alloy melt 11. The temperature of the fluid transported to the cooling channel is room temperature or lower than room temperature (25 degrees Celsius), or the temperature of the fluid transported to the cooling channel is between the solidification point of the fluid and 100 degrees Celsius.

[0051] In order to prevent the fluid entering the cooling channel 20 from flowing back out from the cooling inlet 22, a one-way valve 225 is provided on the pipe connected to the cooling inlet 22. When the aluminum alloy melt is contained in the container, the temperature of the aluminum alloy melt is above the liquidus (0-50 degrees Celsius above the liquidus). After being stirred and cooled by the stirring head, the temperature drops below the liquidus. Taking ZL101 aluminum alloy as an example, its liquidus temperature is 615°C and its solidus temperature is 567°C. The aluminum alloy is heated to 700°C, and the container takes out the aluminum alloy melt from the heating furnace. After being stirred and cooled by the stirring head, its temperature drops to below 567°C.

[0052] Preferably, the connection between the third flow channel 32 and the first flow channel 24 and the second flow channel 25 is located at the lowest point of the third flow channel 32. In this way, the liquid fluid will reach the lowest point of the first flow channel 24 under the action of gravity, so as to more conveniently enter the third flow channel 32. When in use, with the one-way blocking effect of the one-way valve 225, if the pressure generated by the expansion of the liquid fluid drives the fluid to flow into the third flow channel 32, and then enter the second flow channel 25 from the third flow channel 32.

[0053] Preferably, the cooling inlet 22 includes a first annular flow channel 221 formed on the upper part of the rotating shaft 21 and a first through hole 222 connected to the first flow channel 24; the cooling outlet 23 includes a second annular flow channel 231 formed on the upper part of the rotating shaft 21 and a second through hole 232 connected to the second flow channel 25; the first annular flow channel 221 and the second annular flow channel 231 are spaced apart in the axial direction of the rotating shaft 21; a first connecting ring 223 is rotatably sealed and connected to the rotating shaft 21 outside the first annular flow channel 221, and an input pipe 224 is connected to the first connecting ring 223; a second connecting ring 233 is rotatably sealed and connected to the rotating shaft 21 outside the second annular flow channel 231, and an output pipe 234 is connected to the second connecting ring 233; when the rotating shaft 21 rotates, the first connecting ring 223 and the second connecting ring 233 remain relatively fixed to the spindle mounting seat (not shown in the figure) that fixes the rotating shaft 21 and do not rotate with the rotating shaft 21.

[0054] Furthermore, the first flow channel 24 and the second flow channel 25 are in communication with the upper end surface of the rotating shaft 21, and the upper end surface of the rotating shaft 21 is provided with a sealing plug 211 for blocking the first flow channel 24 and the second flow channel 25. In this way, when processing the first flow channel 24 and the second flow channel 25, the processing can be performed from the upper end surface of the rotating shaft 21, and when the processing is completed and the first flow channel 24 and the second flow channel 25 are used, the sealing plug 211 is used for blocking and sealing.

[0055] The first annular flow channel 221 and the second annular flow channel 231 are provided on the upper part of the rotating shaft 21, and are respectively connected with the first connecting ring 223 and the second connecting ring 233, so that the cooling fluid is input through the input pipe 224, and the cooling fluid is continuously transported to the first flow channel 24 through the first annular flow channel 221. The fluid in the second flow channel 25 is continuously discharged to the second connecting ring 233 through the second annular flow channel 231, and the rotation of the rotating shaft 21 will not affect the arrangement of the input pipe 224 and the output pipe 234, and the overall structure is simple and compact, which is convenient for installation. The one-way valve 225 can be installed on the input pipe 224.

[0056] The input pipe 224 and the output pipe 234 are fixed to the spindle mounting seat by a fixing structure (not shown in the figure), and the fixing structure can be a detachable connection component such as a buckle. The first connecting ring 223 and the second connecting ring 233 in the figure are only schematic connection relationships. In order to ensure sealing, a sealing structure can be provided between the first connecting ring 223 and the second connecting ring 233 and the rotating shaft 21 to ensure sealing of the upper and lower sides of the annular flow channel.

[0057] Furthermore, a gear 215 for driving the rotating shaft 21 to rotate is fixedly connected to the upper end of the rotating shaft 21, and the first connecting ring 223 and the upper and lower sides of the second connection are respectively installed with the first bearing 212 and the second bearing 213, and the rotating shaft 21 is connected to the main shaft mounting seat through the first bearing 212 and the second bearing 213.

[0058] like Figure 4 As shown, the first bearing 212, the first connecting ring 223, the second connecting ring 233 and the second bearing 213 are sequentially installed from top to bottom, and the inner diameter of the second bearing 213 is larger than the inner diameter of the first bearing 212. For the convenience of installation, a stepped shaft is provided at the upper end of the rotating shaft 21, and the first bearing 212, the first connecting ring 223, the second connecting ring 233 and the second bearing 213 are sequentially sleeved on the rotating shaft 21 from top to bottom. The upper ends of the first bearing 212 and the second bearing 213 are both provided with a C-shaped retaining ring 214.

[0059] Compared with the prior art, the present invention provides a cooling channel 20 inside the rotating shaft 21, so that the stirring head 2 stirs the aluminum alloy melt 11 to generate shear force, and at the same time, heat is exchanged by passing fluid through the cooling channel 20 inside the stirring head 2, thereby promoting the generation of dendrites. The mechanical action of the shear force of stirring makes the dendrites more dispersed, and the combination of the two makes the semi-solid slurrying process of the aluminum alloy melt 11 faster. Since the fluid is inside the stirring head 2, the fluid does not contact the aluminum alloy melt 11, and it is not easy to cause the aluminum alloy melt 11 to splash.

[0060] The above embodiments and drawings do not limit the product form and style of the present invention. Any appropriate changes or modifications made by ordinary technicians in the relevant technical field should be deemed to be within the patent scope of the present invention.

Claims

1. A method for rapid semi-solid slurrying of aluminum alloy, characterized in that: The invention comprises: placing an aluminum alloy melt in a container, extending a stirring head below the liquid level of the aluminum alloy melt in the container and rotating around the axis of the stirring head to stir the aluminum alloy melt; a cooling channel is formed on the stirring head, and the cooling channel is at least partially located below the liquid level of the aluminum alloy melt, and the upper part of the stirring head has a cooling inlet and a cooling outlet connected to the cooling channel; during the rotation of the stirring head, a cooling medium flows in the cooling channel and exchanges heat with the aluminum alloy melt to reduce the temperature of the aluminum alloy melt, and during the heat exchange process, the fluid in the cooling channel does not directly contact the aluminum alloy melt; The container is connected to a first manipulator, and the first manipulator drives the container to move in space, and the first manipulator drives the container to hold the aluminum alloy melt and move it under the stirring head and pour out the aluminum alloy melt after slurrying; The stirring head is mounted on a second manipulator, and the second manipulator drives the stirring head to move in space so as to extend the stirring head below the liquid level of the aluminum alloy melt in the cavity; The stirring head includes a rotating shaft and a blade arranged on the rotating shaft, the rotating shaft is formed with a first flow channel and a second flow channel respectively arranged along the axial direction of the rotating shaft, and the blade is formed with a third flow channel; the first flow channel, the second flow channel and the third flow channel constitute a cooling flow channel; the first flow channel is connected to the cooling inlet, the second flow channel is connected to the cooling outlet, the cooling medium enters the first flow channel from the cooling inlet, the third flow channel is communicated with the first flow channel and the second flow channel respectively, and the cooling medium then flows from the second flow channel to the cooling outlet; The connection points of the third flow channel with the first flow channel and the second flow channel are both located at the lowest point of the third flow channel; the fluid in the cooling flow channel is liquid; a one-way valve is provided on the pipeline connected to the cooling inlet; the liquid fluid will reach the lowest point of the first flow channel under the action of gravity, and the pressure generated by the expansion of the liquid fluid drives the fluid to flow into the third flow channel, and then enter the second flow channel from the third flow channel; The cooling inlet includes a first annular flow channel formed on the upper part of the rotating shaft and a first through hole connected to the first flow channel; the cooling outlet includes a second annular flow channel formed on the upper part of the rotating shaft and a second through hole connected to the second flow channel; the first annular flow channel and the second annular flow channel are spaced apart in the axial direction of the rotating shaft; a first connecting ring is rotatably sealed and connected to the rotating shaft outside the first annular flow channel, and an input pipe is connected to the first connecting ring; a second connecting ring is rotatably sealed and connected to the rotating shaft outside the second annular flow channel, and an output pipe is connected to the second connecting ring; when the rotating shaft rotates, the first connecting ring and the second connecting ring remain relatively fixed to the main shaft mounting seat that fixes the rotating shaft and do not rotate with the rotating shaft; A coil is formed outside the blade, the coil is fixedly connected to the blade, and the third flow channel is formed inside the coil; The side of the coil close to the rotating shaft is fixedly connected to the rotating shaft by welding through a first connecting block, and the end of the coil away from the rotating shaft is connected to the blade by welding through a second connecting block; A protective coating is provided on the surface of the rotating shaft and the blades; the blades include two symmetrical parts, a reinforcing rib is provided between the left and right blades, and the reinforcing rib is arranged perpendicular to the blades; the coil is a copper coil, and a protective coating is also provided on the surface of the coil. The coil includes two parts, a left side and a right side, according to the layout of the blades, and the upper ends of the left and right coils are connected to each other through pipes.