Display panel and method for manufacturing the same

By setting an isolation layer in the display panel, gases such as water and oxygen in the pixel definition layer are prevented from entering the light emitting layer, the problem of light emitting layer failure is solved, the performance and service life of the display panel are improved, and the preparation process is simplified.

CN114335101BActive Publication Date: 2024-11-22SHENZHEN CHINA STAR OPTOELECTRONICS SEMICON DISPLAY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111621633.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-28
Publication Date
2024-11-22
Estimated Expiration
2041-12-28

AI Technical Summary

Technical Problem

Gas such as water and oxygen released from the pixel definition layer in the existing display panel enter the luminescent layer, causing the luminescent layer to fail, causing defects such as pixel shrinkage, picture color shift and dark spots, affecting product yield and service life.

Method used

An isolation layer is provided in the display panel. The isolation layer is located between the light emitting layer and the pixel definition layer to prevent gases such as water and oxygen from entering the light emitting layer. A metal layer is used as an isolation layer, and an oxide layer is formed on its surface to enhance the isolation effect.

Benefits of technology

It effectively avoids failure of the light emitting layer, prevents pixel shrinkage, improves the performance and service life of the display panel, and simplifies the preparation process and reduces costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114335101B_ABST
    Figure CN114335101B_ABST
Patent Text Reader

Abstract

The present application discloses a display panel and a preparation method thereof. The display panel includes a substrate, a pixel definition layer and a light-emitting layer. The pixel definition layer is disposed on the substrate. The pixel definition layer is provided with a first through hole, the first through hole penetrates the pixel definition layer, the light-emitting layer is disposed in the first through hole, and an isolation layer is disposed between the light-emitting layer and the pixel definition layer. In the present application, an isolation layer is disposed between the light-emitting layer and the pixel definition layer to prevent water and oxygen in the pixel definition layer from entering the light-emitting layer, thereby preventing the light-emitting layer from failing, thereby improving the performance of the display panel.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of display technology, and in particular to a display panel and a method for preparing the same. Background Art

[0002] At present, the pixel definition layer (Bank) is usually made of organic materials, which will release gases such as water and oxygen under certain environmental factors such as temperature or pressure. Figure 1 In the existing device structure, the light-emitting layer is usually in direct contact with the bank. The water, oxygen and other gases released by the bank can directly enter the light-emitting layer and react with the light-emitting material, causing the light-emitting layer to fail, thereby causing pixel shrinkage. The main manifestation of pixel shrinkage is darkening around the pixel. In severe cases, it will cause defects such as color deviation and dark spots on the screen, affecting the product yield and service life. Summary of the invention

[0003] The embodiments of the present application provide a display panel and a method for manufacturing the same, so as to solve the problem in the prior art that gases such as water and oxygen in a pixel definition layer enter into a light-emitting layer, causing the light-emitting layer to fail.

[0004] The present application provides a display panel, comprising:

[0005] substrate;

[0006] a pixel definition layer, wherein the pixel definition layer is disposed on the substrate, the pixel definition layer is provided with a first through hole, and the first through hole penetrates the pixel definition layer; and

[0007] A light-emitting layer is disposed in the first through hole, and an isolation layer is disposed between the light-emitting layer and the pixel definition layer.

[0008] Optionally, in some embodiments of the present application, the isolation layer includes a metal layer.

[0009] Optionally, in some embodiments of the present application, the display panel is provided with a display area and a non-display area arranged around the display area, the isolation layer also includes an insulating oxide layer, the oxide layer is arranged on a side of the metal layer away from the substrate, and the oxide layer is located at an end of the metal layer away from the display area, the display panel also includes an upper electrode and an electronic functional layer, the electronic functional layer is arranged on the light-emitting layer and the metal layer, the upper electrode is arranged on the electronic functional layer and the oxide layer, and the end of the upper electrode away from the display area is connected to the oxide layer.

[0010] Optionally, in some embodiments of the present application, the material of the oxide layer is a metal oxide of the material of the metal layer, and the metal layer and the oxide layer are integrally formed.

[0011] Optionally, in some embodiments of the present application, the isolation layer covers the pixel definition layer and fills the first through hole.

[0012] Optionally, in some embodiments of the present application, the isolation layer is provided with a first via hole, the first via hole is located between adjacent light-emitting layers, and the first via hole passes through the isolation layer.

[0013] Optionally, in some embodiments of the present application, the display panel further includes a transistor layer, a planarization layer and a self-repairing layer, the transistor layer is arranged on the substrate, the planarization layer is arranged on the transistor layer, the pixel definition layer is arranged on the planarization layer, the pixel definition layer is also provided with a second through hole, the display panel is provided with a display area and a non-display area arranged around the display area, the second through hole is located in at least one of the display area and the non-display area, the second through hole is spaced apart from the first through hole, the second through hole is connected with the first through hole, the second through hole passes through the pixel definition layer and the planarization layer to expose the transistor layer, the isolation layer extends into the second through hole and contacts the transistor layer, and the self-repairing layer is arranged on the isolation layer and extends into the second through hole and contacts the transistor layer.

[0014] Optionally, in some embodiments of the present application, the isolation layer covers the sidewalls of the first through hole.

[0015] Optionally, in some embodiments of the present application, the display panel further includes a transistor layer and a self-repairing layer, the transistor layer is disposed on the substrate, the pixel definition layer is disposed on the transistor layer, and the self-repairing layer is disposed in the transistor layer or on the isolation layer.

[0016] Optionally, in some embodiments of the present application, the self-repairing layer includes a self-repairing material, and the self-repairing material includes one or a combination of microcapsule self-repairing polymer materials, hollow fiber self-repairing polymer materials, nanoparticle self-repairing polymer materials and microvascular self-repairing polymer materials.

[0017] Optionally, in some embodiments of the present application, the surface of the material of the self-healing layer away from the substrate is a hydrophobic surface.

[0018] Accordingly, the present application also provides a method for preparing a display panel, comprising:

[0019] providing a substrate;

[0020] forming a pixel definition layer on the substrate, wherein the pixel definition layer is provided with a first through hole, and the first through hole penetrates the pixel definition layer to expose the substrate;

[0021] forming an isolation layer on the pixel definition layer and located on the sidewall of the first through hole; and

[0022] A light emitting layer is disposed in the first through hole, and the isolation layer is located between the light emitting layer and the pixel definition layer.

[0023] Optionally, in some embodiments of the present application, the display panel is provided with a display area and a non-display area provided around the display area, and the step of forming an isolation layer on the pixel definition layer includes:

[0024] Disposing metal on the pixel definition layer, and patterning the metal to form a metal layer of an isolation layer, wherein the metal layer is located on a side wall of the first through hole;

[0025] The end of the metal layer is located at a side of the metal layer away from the display area, and the surface of the end of the metal layer away from the substrate is oxidized to form an oxide layer of the isolation layer, and the upper surface of the end of the metal layer forms an insulating oxide layer;

[0026] After the step of providing the light-emitting layer in the first through hole, the method further comprises:

[0027] Disposing an electronic functional layer on the light-emitting layer and the pixel definition layer;

[0028] An upper electrode is arranged on the electronic functional layer and the oxide layer, an end of the upper electrode is located at a side of the upper electrode away from the display area, and the end of the upper electrode is connected to the oxide layer.

[0029] The present application discloses a display panel and a preparation method thereof. The display panel includes a substrate, a pixel definition layer and a light-emitting layer. The pixel definition layer is disposed on the substrate. The pixel definition layer is provided with a first through hole. The first through hole penetrates the pixel definition layer. The light-emitting layer is disposed in the first through hole. An isolation layer is disposed between the light-emitting layer and the pixel definition layer. In the present application, an isolation layer is disposed between the light-emitting layer and the pixel definition layer to prevent water and oxygen in the pixel definition layer from entering the light-emitting layer, thereby preventing the light-emitting layer from failing, thereby preventing the problem of darkening or shrinking around the pixel, and thus improving the performance of the display panel. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For those skilled in the art, other drawings can be obtained based on these drawings without creative work.

[0031] Figure 1 It is a schematic electron microscope diagram of a light-emitting layer in a display panel provided in the prior art.

[0032] Figure 2 It is a plan view of a display panel provided in an embodiment of the present application.

[0033] Figure 3 yes Figure 2 A schematic cross-sectional view of the display panel along line AB is provided in FIG.

[0034] Figure 4 It is a schematic diagram of the principle of the self-repairing layer repairing film cracks provided in an embodiment of the present application.

[0035] Figure 5 It is a schematic diagram of the process of the method for preparing a display panel provided in an embodiment of the present application.

[0036] Figure 6-Figure 12 It is a schematic diagram of the steps of the method for preparing a display panel provided in an embodiment of the present application. DETAILED DESCRIPTION

[0037] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without making creative work are within the scope of protection of the present application. In addition, it should be understood that the specific implementation methods described herein are only used to illustrate and explain the present application, and are not used to limit the present application. In the present application, unless otherwise stated, the directional words used, such as "upper" and "lower", generally refer to the upper and lower parts of the device in actual use or working state, specifically the drawing direction in the accompanying drawings; and "inside" and "outside" refer to the outline of the device. In the present application, "reaction" can be a chemical reaction or a physical reaction.

[0038] The embodiment of the present application provides a display panel and a method for manufacturing the same, wherein the display panel includes a substrate, a pixel definition layer, a light-emitting layer, and an isolation layer. The pixel definition layer is disposed on the substrate, the pixel definition layer is provided with a first through hole, the first through hole penetrates the pixel definition layer, the light-emitting layer is disposed in the first through hole, and an isolation layer is disposed between the light-emitting layer and the pixel definition layer.

[0039] In the present application, by setting an isolation layer between the light-emitting layer and the pixel definition layer, gases such as water and oxygen in the pixel definition layer can be prevented from entering the light-emitting layer, thereby preventing the light-emitting layer from failing due to water and oxygen erosion, thereby avoiding the problem of pixel shrinkage, thereby improving the performance of the display panel.

[0040] The following are detailed descriptions:

[0041] See also Figure 2 and Figure 3The present application provides a display panel 10. The display panel 10 includes a substrate 100, a transistor layer 200, a planar layer 300, a lower electrode 400, a pixel definition layer 500, an isolation layer 600, a light emitting layer 700, a self-repairing layer 800, an electronic functional layer 900, an upper electrode 1000 and an encapsulation layer 1100, which are stacked in sequence. The display panel 10 is provided with a display area 11 and a non-display area 12 arranged around the display area 11.

[0042] There are multiple transistor layers 200. Each transistor layer 200 is arranged at intervals on the substrate 100. Specifically, each transistor layer 200 includes a light shielding layer 210, a buffer layer 220, an active layer 230, an insulating layer 240, a gate 250, an interlayer dielectric layer 260, a connecting portion 270, a source 280, a drain 290 and a passivation layer 299. The light shielding layer 210 is arranged on the substrate 100. The light shielding layer 210 includes a light shielding portion 210a and a metal portion 210b arranged at intervals. The light shielding layer 210 is used to block external light to prevent the light from affecting the active layer 230, thereby improving the performance of the transistor. The metal portion 210b is a part of the first plate of the capacitor. The buffer layer 220 covers the light shielding layer 210 and the substrate 100. The active layer 230 is arranged on the buffer layer 220. The active layer 230 includes an active portion 230a and a conducting portion 230b which are spaced apart from each other. The active portion 230a is located on the light shielding portion 210a. The conducting portion 230b is located on the metal portion 210b, and the active portion 230a includes a semiconductor portion and a conductor portion disposed on both sides of the semiconductor portion. The conducting portion 230b is a second plate of the capacitor. The insulating layer 240 is disposed on the active portion 230a and is located on the semiconductor portion. The gate 250 is disposed on the insulating layer 240. The interlayer dielectric layer 260 covers the active layer 230, the insulating layer 240 and the gate 250. The source 280, the drain 290 and the connecting portion 270 are in the same layer and spaced apart on the interlayer dielectric layer 260, wherein the connecting portion 270 is located on the conducting portion 230b, and the connecting portion 270 extends into a connecting hole to connect with the metal portion 210b. The source electrode 280 extends into another connection hole and is connected to a conductor. The drain electrode 290 extends into another connection hole and is connected to another conductor. The connection portion 270 is a part of the first plate of the storage capacitor. The passivation layer 299 covers the buffer layer 220, the connection portion 270, the source electrode 280 and the drain electrode 290.

[0043] In the present application, the metal portion 210 b and the connecting portion 270 form a first electrode plate of the capacitor, so that the overlapping area between the first electrode plate and the second electrode plate is increased, the capacitance value of the storage capacitor is increased, and thus the performance of the display panel 10 is improved.

[0044] The planar layer 300 is disposed on the passivation layer 299 . The planar layer 300 is provided with a connection hole, and the connection hole of the planar layer 300 penetrates the planar layer 300 and the passivation layer 299 to expose the drain electrode 290 .

[0045] The lower electrode 400 is disposed on the planar layer 300 and extends into the connection hole of the planar layer 300 to be connected to the drain electrode 290 . Optionally, the lower electrode 400 may be an anode.

[0046] The pixel definition layer 500 is disposed on the lower electrode 400 and the planar layer 300. The pixel definition layer 500 is provided with a first through hole 501 and a second through hole 502. The first through hole 501 penetrates the pixel definition layer 500 to expose the lower electrode 400. The second through hole 502 penetrates the pixel definition layer 500 and the planar layer 300 to expose the passivation layer 299.

[0047] In the present application, a second through hole 502 is provided on the pixel definition layer 500. In the present application, by providing the second through hole 502 in the pixel definition layer 500, stress occurring during use or preparation can be buffered, thereby avoiding the problem of breakage of the film layer in the display panel 10, thereby improving the performance of the display panel 10.

[0048] The isolation layer 600 is disposed between the light-emitting layer 700 and the pixel definition layer 500. Specifically, the isolation layer 600 covers the sidewall of the first through hole 501. Optionally, the isolation layer 600 includes a metal layer 610. The metal layer 610 is disposed between the pixel definition layer 500 and the light-emitting layer 700. Optionally, the isolation layer 600 may also be made of other materials, such as an inorganic material having the ability to isolate gases such as water and oxygen.

[0049] In the present application, metal is used to form the metal layer 610 in the isolation layer 600 between the pixel definition layer 500 and the light-emitting layer 700, so that the isolation layer 600 can prevent gases such as water and oxygen in the pixel definition layer 500 from entering the light-emitting layer 700. At the same time, the metal layer 610 in the isolation layer 600 is formed of metal, so that the metal layer 610 has a reflective effect, thereby preventing the emitted light from diverging to the surroundings, thereby improving the light output rate of the display panel 10, and then improving the display effect of the display panel 10.

[0050] In one embodiment, the isolation layer 600 covers the pixel definition layer 500 and fills the first through hole 501 . At this time, the subsequent light emitting layer 700 is disposed on the metal layer 610 , that is, the subsequent light emitting layer 700 is in direct contact with the metal layer 610 .

[0051] In one embodiment, when the isolation layer 600 covers the pixel definition layer 500 and fills the first through hole 501, the isolation layer 600 is provided with a first via hole 601. The first via hole 601 penetrates the isolation layer 600 to expose the passivation layer 299, and the first via hole 601 is connected to the second through hole 502.

[0052] In the present application, when the isolation layer 600 covers the pixel definition layer 500 and fills the first through hole 501, the first via hole 601 is set on the isolation layer 600, so that the isolation layer 600 is disconnected, thereby forming a plurality of spaced-apart spacers, that is, forming a plurality of spaced-apart metal portions, thereby preventing the metal layer 610 from contacting the lower electrode 400, thereby preventing the adjacent lower electrodes 400 from being conductive, thereby avoiding a short circuit. At the same time, when a sub-pixel fails due to gases such as water and oxygen, the gases such as water and oxygen cannot pass through the isolation layer to affect other sub-pixels due to the spaced-apart isolation portions, thereby ensuring the normal operation of other sub-pixels, thereby improving the performance of the display panel 10.

[0053] In one embodiment, when the isolation layer 600 covers the pixel definition layer 500 and fills the first through hole 501, the isolation layer 600 is also provided with a second via hole 602, and the second via hole 602 penetrates the isolation layer 600 to expose the lower electrode 400, that is, the second via hole 602 penetrates the metal layer 610, and the second via hole 602 is connected to the first through hole 501.

[0054] In the present application, when the isolation layer 600 covers the pixel definition layer 500 and fills the first through hole 501, a second through hole 602 is also provided in the isolation layer 600 to penetrate the first through hole 501, so that the subsequent light-emitting layer 700 can be provided in the first through hole 501 and the second through hole 602 to be connected with the lower electrode 400, that is, the light-emitting layer 700 is in direct contact with the lower electrode 400, so that the energy levels between the subsequent light-emitting layer 700 and the lower electrode 400 and the metal layer 610 are matched, so that holes are easily injected, thereby improving the light extraction efficiency of the display panel 10, and at the same time, avoiding the influence of the microcavity effect.

[0055] In one embodiment, the material of the metal layer 610 is an easily oxidizable metal.

[0056] It should be noted that the easily oxidizable metal refers to a metal that is more likely to undergo oxidation reaction in the air.

[0057] In one embodiment, the material of the metal layer 610 includes one or a combination of aluminum, magnesium, zinc, nickel, lead, silver, copper and iron.

[0058] In one embodiment, the thickness H of the metal layer 610 is 50-800 nanometers.

[0059] The oxide layer 620 is disposed on a side of the metal layer 610 away from the substrate 100 . The oxide layer 620 is located at an end C of the metal layer 610 away from the display area 11 . The end C of the metal layer 610 is located on a side of the metal layer 610 away from the light emitting layer 700 .

[0060] In the present application, an oxide layer 620 is arranged on the side of the metal layer 610 away from the substrate 100 to prevent the subsequent upper electrode 1000 from being connected to the metal layer 610 when the subsequent electronic functional layer 900 does not completely cover the lower electrode 400, thereby avoiding a short circuit problem, thereby ensuring the performance of the display panel 10, and the oxide layer 620 is only arranged at the end C of the metal layer 610 away from the display area 11, which can reduce costs.

[0061] In one embodiment, an oxide layer 620 is provided on one side of the metal layer 610 away from the substrate 100, where the isolation layer 600 refers to the metal layer 610 and the oxide layer 620, and the first via 601 penetrates the oxide layer 620 and the metal layer 610 to expose the passivation layer 299, and the first via 601 is connected to the second through hole 502, and the second via 602 is connected to the first through hole 501, so that the metal layer 610 forms a plurality of spaced metal portions and the oxide layer 620 forms a plurality of spaced oxide portions.

[0062] In the present application, an oxide layer 620 is provided on the side of the metal layer 610 away from the substrate 100, that is, the oxide layer 620 is provided on the surface of the entire metal layer 610, which simplifies the preparation process of the display panel 10 and prevents the metal layer 610 from contacting the subsequent upper electrode 1000, thereby ensuring the performance of the display panel 10.

[0063] In one embodiment, the material of the oxide layer 620 includes one or a combination of aluminum oxide, magnesium oxide, zinc oxide, nickel oxide, tin oxide, lead oxide, iron oxide, silver oxide, and copper oxide.

[0064] In one embodiment, the material of the oxide layer 620 is a metal oxide of the material of the metal layer 610, and the material of the oxide layer 620 includes one or a combination of aluminum oxide, magnesium oxide, zinc oxide, nickel oxide, tin oxide, lead oxide, iron oxide, silver oxide, and copper oxide. As an example, the material of the metal layer is aluminum, and the material of the oxide layer is aluminum oxide; or, the material of the metal layer is lead, and the material of the oxide layer is lead oxide; or, the material of the metal layer is silver, and the material of the oxide layer is silver oxide, etc.

[0065] In the present application, the material of the oxide layer 620 is the metal oxide of the material of the metal layer 610, so that when the metal layer 610 and the oxide layer 620 are prepared, the metal layer 610 and the oxide layer 620 can be formed as one piece, which simplifies the preparation process of the isolation layer 600, is conducive to the rapid preparation of the isolation layer 600, and reduces production costs.

[0066] In one embodiment, the thickness h of the oxide layer 620 is 10-20 nanometers.

[0067] The light-emitting layer 700 is arranged in the first through hole 501 and the second through hole 602 to be connected to the lower electrode 400, that is, the light-emitting layer 700 is in direct contact with the lower electrode 400, thereby reducing the energy level difference between the light-emitting layer 700 and the lower electrode 400 and the metal layer 610, making it easy for holes to be injected into the light-emitting layer 700, thereby improving the light extraction efficiency of the display panel 10 and avoiding the influence of the microcavity effect.

[0068] The self-repairing layer 800 is disposed on the isolation layer 600 and extends into the second through hole 502 to contact the transistor layer 200. Specifically, when the oxide layer 620 is disposed on one side of the metal layer 610 away from the substrate 100, the self-repairing layer 800 is disposed on the oxide layer 620 and extends into the first through hole 601 and the second through hole 502 to contact the passivation layer 299, and the self-repairing layer 800 is disposed around the first through hole 501 to form a plurality of self-repairing portions disposed at intervals.

[0069] In the present application, a self-repairing layer 800 is arranged on the isolation layer 600, and extends into the first via hole 601 and the second via hole 502 to contact the passivation layer 299, so that the self-repairing layer 800 can automatically repair cracks that appear in the display panel 10 during the manufacturing and use process, thereby avoiding the problem of film layer breakage. At the same time, the second through hole 502 and the first through hole 601 are arranged to buffer the stress that appears during the use or preparation process, thereby avoiding the problem of film layer breakage in the display panel 10, thereby improving the performance of the display panel 10.

[0070] In one embodiment, the self-repairing layer 800 includes a repairing agent. The repairing agent is also a self-repairing material. The repairing agent includes one or several combinations of exogenous self-repairing polymer materials and intrinsic self-repairing polymer materials. Specifically, the exogenous self-repairing polymer materials include one or several combinations of microcapsule self-repairing polymer materials, hollow fiber self-repairing polymer materials, nanoparticle self-repairing polymer materials, microvascular self-repairing polymer materials, and carbon nanotube self-repairing polymer materials. Microcapsule self-repairing polymer materials include one or several combinations of dicyclopentadiene (DCPD) self-repairing agent system polymer materials and epoxy resin self-repairing agent systems. The repairing agent is a low-viscosity liquid and has good wettability with the fracture surface, so that the repairing agent can be coated in the particles.

[0071] In one embodiment, the material of the self-repairing layer 800 also includes a curing agent. The curing agent is a room temperature curing agent. The curing agent includes one or more combinations of aliphatic amines, thiols, boron trifluoride, polythiol-pentaerythritol tetramercaptopropionate, benzyldimethylamine, azobisisobutyronitrile (AIBN) and metal ruthenium (Grubbs). The curing agent can be encapsulated in particles containing the self-repairing agent, or not disposed in particles containing the self-repairing agent. It should be noted that the curing agent does not react with the film layer.

[0072] See also Figure 4 Repair principle: The crack expansion in the film layer causes the particles containing the repair agent to rupture. The repair agent in the particles flows to the crack under the action of capillary action. Under the action of the curing agent, the repair agent undergoes a polymerization reaction, thereby repairing the crack.

[0073] For example, the polymer material of the dicyclopentadiene (DCPD) self-healing agent system is dicyclopentadiene (DCPD) and a metal ruthenium-based (Grubbs) catalyst. DCPD can undergo a ring-opening metathesis polymerization reaction with the Grubbs catalyst to repair cracks and achieve self-healing.

[0074] In one embodiment, the surface of the self-repairing layer 800 away from the substrate 100 is a hydrophobic surface. The material of the hydrophobic surface is a hydrophobic material. The hydrophobic material includes a compound containing fluorine. In the present application, a hydrophobic material is added to the self-repairing layer 800. During the use or preparation of the display panel 10, the hydrophobic material will float on the surface of the self-repairing layer 800 to form a hydrophobic surface, so that the surface of the self-repairing layer 800 forms a hydrophobic surface with a hydrophobic effect, thereby avoiding the color mixing phenomenon between adjacent light-emitting layers 700 during the preparation of the light-emitting layer 700, thereby improving the performance of the display panel 10.

[0075] In one embodiment, the mass ratio of the hydrophobic material to the repairing agent is 1-5%: 1. Within this range, the hydrophobic effect of the self-repairing layer 800 can be improved, thereby improving the performance of the display panel 10.

[0076] In another embodiment, the self-repairing layer 800 is disposed in the transistor layer 200 , between the substrate 100 and the transistor layer 200 , and between the transistor layer 200 and the pixel definition layer 500 .

[0077] In another embodiment, a self-repairing layer 800 is further disposed in the transistor layer 200 , between the substrate 100 and the transistor layer 200 , between the transistor layer 200 and the pixel definition layer 500 , or between the pixel definition layer 500 and the isolation layer 600 .

[0078] In the present application, a self-repairing layer 800 is further arranged in the transistor layer 200, between the substrate 100 and the transistor layer 200, and between the transistor layer 200 and the pixel definition layer 500, so that the self-repairing layer 800 can also repair cracks in film layers other than those adjacent to the self-repairing layer 800, thereby further improving the bending performance of the display panel 10.

[0079] The electronic functional layer 900 is disposed on the light emitting layer 700 and the metal layer 610, the upper electrode 1000 is disposed on the electronic functional layer 900 and the oxide layer 620, and the end C of the upper electrode 1000 away from the display area 11 is connected to the oxide layer 620. Specifically, the electronic functional layer 900 includes an electron injection layer and an electron transport layer, the electron transport layer covers the oxide layer 620, the light emitting layer 700 and the self-repairing layer 800, the electron injection layer is disposed on the electron transport layer, and the upper electrode 1000 is disposed on the electron injection layer and the oxide layer 620. The upper electrode 1000 may be a cathode.

[0080] The encapsulation layer 1100 is disposed on the upper electrode 1000 .

[0081] It should be noted that the substrate 100 , the transistor layer 200 , the planar layer 300 , the lower electrode 400 , the self-repairing layer 800 , the electronic functional layer 900 , the upper electrode 1000 and the encapsulation layer 1100 in the display panel 10 may be removed as needed.

[0082] The present application provides a display panel 10, which prevents gases such as water and oxygen in the pixel definition layer 500 from entering the light-emitting layer 700 by setting an isolation layer 600 between the light-emitting layer 700 and the pixel definition layer 500, thereby preventing the light-emitting layer 700 from failing, thereby preventing the pixel from shrinking, and thus improving the performance of the display panel 10; a self-repairing layer 800 is set in the display panel 10, so that the self-repairing layer 800 can repair cracks that appear in the display panel 10 during use or preparation, thereby improving the bending performance of the display panel 10, thereby improving the performance of the display panel 10.

[0083] The present application also provides a method for preparing a display panel, comprising:

[0084] B11. Provide a substrate.

[0085] B12. Form a pixel definition layer on the substrate, wherein the pixel definition layer is provided with a first through hole, and the first through hole penetrates the pixel definition layer to expose the substrate.

[0086] B13. Form an isolation layer on the pixel definition layer and locate it on the side wall of the first through hole.

[0087] B14. A light-emitting layer is disposed in the first through hole, and an isolation layer is located between the light-emitting layer and the pixel definition layer.

[0088] In the present application, by setting an isolation layer between the light-emitting layer and the pixel definition layer, gases such as water and oxygen in the pixel definition layer can be prevented from entering the light-emitting layer, thereby preventing the light-emitting layer from failing, thereby preventing the pixel from shrinking, and thus improving the performance of the display panel.

[0089] The specific instructions are as follows:

[0090] See also Figure 5 and Figure 6-Figure 12 , the present application also provides a method for preparing a display panel.

[0091] B11. Provide a substrate.

[0092] In one embodiment, after B11, the following is further included:

[0093] See also Figure 6 . A plurality of transistor layers 200 are formed on the substrate 100, and each transistor layer 200 is spaced apart on the substrate 100. Each transistor layer 200 includes a light shielding layer 210, a buffer layer 220, an active layer 230, an insulating layer 240, a gate 250, an interlayer dielectric layer 260, a connecting portion 270, a source 280, a drain 290 and a passivation layer 299. The light shielding layer 210 is disposed on the substrate 100. The light shielding layer 210 includes a light shielding portion 210a and a metal portion 210b spaced apart from each other. The light shielding layer 210 is used to block external light to prevent the light from affecting the active layer 230, thereby improving the performance of the transistor. The metal portion 210b is a part of the first plate of the capacitor. The buffer layer 220 covers the light shielding layer 210 and the substrate 100. The active layer 230 is disposed on the buffer layer 220. The active layer 230 includes an active portion 230a and a conducting portion 230b which are spaced apart from each other. The active portion 230a is located on the light shielding portion 210a. The conducting portion 230b is located on the metal portion 210b, and the active portion 230a includes a semiconductor portion and a conductor portion arranged on both sides of the semiconductor portion. The conducting portion 230b is a second plate of the capacitor. The insulating layer 240 is arranged on the active layer 230 and is located on the semiconductor portion. The gate 250 is arranged on the insulating layer 240. The interlayer dielectric layer 260 covers the active layer 230, the insulating layer 240 and the gate 250. The source 280, the drain 290 and the connecting portion 270 are in the same layer and spaced apart on the interlayer dielectric layer 260, wherein the connecting portion 270 is located on the conducting portion 230b, and the connecting portion 270 extends into a connecting hole to connect with the metal portion 210b. The source electrode 280 extends into another connection hole and is connected to a conductor. The drain electrode 290 extends into another connection hole and is connected to another conductor. The connection portion 270 is a part of the first plate of the storage capacitor. The passivation layer 299 covers the buffer layer 220, the connection portion 270, the source electrode 280 and the drain electrode 290.

[0094] In one embodiment, after forming the transistor layer 200 on the substrate 100, the method further includes:

[0095] The planarization layer 300 is formed on the passivation layer 299. The planarization layer 300 is provided with a connection hole penetrating the planarization layer 300 and the passivation layer 299 to expose the drain electrode 290.

[0096] In one embodiment, after forming the planar layer 300 on the passivation layer 299, the method further includes:

[0097] The lower electrode 400 is formed on the planar layer 300 and extends into the connection hole of the planar layer 300 to be connected to the drain electrode 290 .

[0098] B12. Form a pixel definition layer on the substrate, wherein the pixel definition layer is provided with a first through hole, and the first through hole penetrates the pixel definition layer.

[0099] Please continue reading Figure 6 Specifically, a pixel definition layer 500 is formed on the planar layer 300 and the lower electrode 400, and the pixel definition layer 500 is half-etched so that the pixel definition layer 500 forms a pre-made hole 203 and a second through hole 502. The pre-made hole 203 penetrates the pixel definition layer 500 to expose the lower electrode 400, and is located above the lower electrode 400, and the pixel definition layer 500 located above the lower electrode 400 is retained. The second through hole 502 penetrates the pixel definition layer 500 and the planar layer 300 to expose the passivation layer 299.

[0100] In the present application, the pixel definition layer 500 located on the lower electrode 400 is retained to avoid damage to the lower electrode 400 during subsequent etching, thereby ensuring the performance of the display panel 10 .

[0101] B13. Form an isolation layer on the pixel definition layer and locate it on the side wall of the first through hole.

[0102] See also Figure 7 and Figure 8 Specifically, a layer of metal is deposited on the lower electrode 400 , the passivation layer 299 and the pixel definition layer 500 by magnetron sputtering or evaporation, and patterned to form the metal layer 610 in the isolation layer 600 . The metal layer 610 extends into the second through hole 502 and contacts the passivation layer 299 .

[0103] Then, the metal layer 610 of the isolation layer 600 located on the lower electrode 400 and the flat layer 300 is removed by etching or the like, and the prefabricated hole 203 forms the first through hole 501 and the second through hole 602, and the lower electrode 400 is exposed; then, the metal layer 610 is treated by plasma on the upper surface of the metal layer 610, and an insulating oxide layer 620 is formed on the upper surface of the metal layer 610, that is, the upper surface of the metal layer 610 is oxidized. The isolation layer 600 is provided with a first through hole 601 and a second through hole 602, where the isolation layer 600 refers to the metal layer 610 and the oxide layer 620, the first through hole 601 penetrates the oxide layer 620 and the metal layer 610 to expose the passivation layer 299, and the first through hole 601 is connected to the second through hole 502, and the second through hole 602 is connected to the first through hole 501, so that the metal layer 610 forms a plurality of metal parts arranged at intervals and the oxide layer 620 forms a plurality of oxide parts arranged at intervals.

[0104] In one embodiment, the isolation layer 600 except the sidewall of the first through hole 501 may be removed, that is, only the isolation layer 600 on the sidewall of the first through hole 501 is retained, so that the raw material of the isolation layer 600 can be saved.

[0105] In one embodiment, the material of the metal layer 610 is an easily oxidizable metal.

[0106] In one embodiment, the material of the metal layer 610 includes one or a combination of aluminum, magnesium, zinc, nickel, lead, silver, copper and iron.

[0107] In one embodiment, the thickness H of the metal layer 610 is 50-800 nanometers.

[0108] In one embodiment, the material of the oxide layer 620 is a metal oxide of the material of the metal layer 610, and the material of the oxide layer 620 includes one or a combination of aluminum oxide, magnesium oxide, zinc oxide, nickel oxide, tin oxide, lead oxide, iron oxide, silver oxide, and copper oxide. As an example, the material of the metal layer is aluminum, and the material of the oxide layer is aluminum oxide; or, the material of the metal layer is lead, and the material of the oxide layer is lead oxide; or, the material of the metal layer is silver, and the material of the oxide layer is silver oxide, etc.

[0109] In another embodiment, the method of forming the oxide layer 620 also includes: directly disposing an insulating oxide layer 620 on the metal layer 610, that is, the oxide layer 620 is not formed by oxidation of the metal layer 610. As an example, the material of the metal layer is lead, and the material of the oxide layer is aluminum oxide; or, the material of the metal layer is aluminum, and the material of the oxide layer is lead oxide; or, the material of the metal layer is iron, and the material of the oxide layer is silver oxide, etc.

[0110] In one embodiment, after B13, the method further includes:

[0111] See also Fig. 9 A self-repairing layer 800 is formed on the oxide layer 620, and extends into the first via hole 601 and the second via hole 502 to contact the passivation layer 299. Specifically, the self-repairing layer 800 is disposed on the oxide layer 620, extends into the first via hole 601 and the second via hole 502 to contact the passivation layer 299, and the self-repairing layer 800 is disposed around the first via hole 501 to form a plurality of self-repairing portions disposed at intervals.

[0112] In one embodiment, the material of the self-repairing layer 800 includes a repairing agent. The repairing agent includes one or several combinations of exogenous self-repairing polymer materials and intrinsic self-repairing polymer materials. Specifically, the exogenous self-repairing polymer materials include one or several combinations of microcapsule self-repairing polymer materials, hollow fiber self-repairing polymer materials, nanoparticle self-repairing polymer materials, microvascular self-repairing polymer materials, and carbon nanotube self-repairing polymer materials. Microcapsule self-repairing polymer materials include one or several combinations of dicyclopentadiene (DCPD) self-repairing agent system polymer materials and epoxy resin self-repairing agent systems. The repairing agent is a low-viscosity liquid and has good wettability with the fracture surface, so that the repairing agent can be coated in the particles.

[0113] In one embodiment, the material of the self-repairing layer 800 also includes a curing agent. The curing agent is a room temperature curing agent. The curing agent includes one or more combinations of aliphatic amines, thiols, boron trifluoride, polythiol-pentaerythritol tetramercaptopropionate, benzyldimethylamine, azobisisobutyronitrile (AIBN) and metal ruthenium (Grubbs). The curing agent can be encapsulated in particles containing the self-repairing agent, or not disposed in particles containing the self-repairing agent. It should be noted that the curing agent does not react with the film layer.

[0114] B14. A light-emitting layer is disposed in the first through hole, and an isolation layer is located between the light-emitting layer and the pixel definition layer.

[0115] See also Fig.10 Specifically, the light emitting layer 700 is disposed in the first through hole 501 , and the light emitting layer 700 is in contact with the lower electrode 400 and the isolation layer 600 .

[0116] In one embodiment, after B14, the method further includes:

[0117] See also Fig.11 and Fig.12 An electron transport layer in the electronic functional layer 900 is formed on the oxide layer 620 , the light emitting layer 700 , and the self-repairing layer 800 ; then, an electron injection layer in the electronic functional layer 900 is formed on the electron transport layer; then, an upper electrode 1000 is formed on the electron injection layer; then, an encapsulation layer 1100 is formed on the upper electrode 1000 .

[0118] In one embodiment, an end C of the upper electrode 1000 away from the light emitting layer 700 is connected to the oxide layer 620 .

[0119] The present application provides a display panel 10 and a preparation method thereof, wherein an isolation layer 600 is provided between a light-emitting layer 700 and a pixel definition layer 500 to prevent gases such as water and oxygen in the pixel definition layer 500 from entering the light-emitting layer 700, thereby preventing the light-emitting layer 700 from failing, thereby preventing the problem of pixel periphery shrinkage, and thus improving the performance of the display panel 10; a self-repairing layer 800 is provided in the display panel 10, so that the self-repairing layer 800 can repair cracks that appear in the display panel 10 during use or preparation, thereby improving the bending performance of the display panel 10, thereby improving the performance of the display panel 10.

[0120] The above is a detailed introduction to a display panel and a preparation method thereof provided in an embodiment of the present application. Specific examples are used herein to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the method of the present application and its core idea. At the same time, for technical personnel in this field, according to the idea of ​​the present application, there will be changes in the specific implementation method and application scope. In summary, the content of this specification should not be understood as a limitation on the present application.

Claims

1. A display panel, characterized in that: The display panel comprises a display area and a non-display area arranged around the display area; the display panel comprises: substrate; A pixel definition layer, wherein the pixel definition layer is disposed on the substrate, and the pixel definition layer is provided with a first through hole, and the first through hole penetrates the pixel definition layer; a light-emitting layer, the light-emitting layer being arranged in the first through hole, an isolation layer being arranged between the light-emitting layer and the pixel definition layer, the isolation layer comprising a metal layer and an insulating oxide layer arranged on a side of the metal layer away from the substrate, the oxide layer being located at an end of the metal layer away from the display area; An upper electrode and an electronic functional layer, wherein the electronic functional layer is arranged on the light-emitting layer and the metal layer, the upper electrode is arranged on the electronic functional layer and the oxide layer, and the end of the upper electrode away from the display area is connected to the oxide layer.

2. The display panel according to claim 1, characterized in that: The material of the oxide layer is the metal oxide of the material of the metal layer, and the metal layer and the oxide layer are integrally formed.

3. The display panel according to claim 1, characterized in that: The isolation layer covers the sidewall of the first through hole.

4. The display panel according to claim 1, characterized in that: The display panel further includes a transistor layer and a self-repairing layer, wherein the transistor layer is disposed on the substrate, the pixel definition layer is disposed on the transistor layer, and the self-repairing layer is disposed in the transistor layer or on the isolation layer.

5. The display panel according to claim 4, characterized in that: The self-repairing layer comprises a self-repairing material, and the self-repairing material comprises one or a combination of microcapsule self-repairing polymer materials, hollow fiber self-repairing polymer materials, nanoparticle self-repairing polymer materials and microvascular self-repairing polymer materials.

6. The display panel according to claim 5, characterized in that: The surface of the self-repairing layer away from the substrate is a hydrophobic surface.

7. A display panel, characterized in that: The display panel comprises a display area and a non-display area arranged around the display area; the display panel comprises: substrate; A pixel definition layer, wherein the pixel definition layer is disposed on the substrate, and the pixel definition layer is provided with a first through hole, and the first through hole penetrates the pixel definition layer; a light-emitting layer, wherein the light-emitting layer is disposed in the first through hole, an isolation layer is disposed between the light-emitting layer and the pixel definition layer, the isolation layer covers the pixel definition layer and fills the first through hole, a first via hole is disposed in the isolation layer, the first via hole is located between adjacent light-emitting layers, and the first via hole penetrates the isolation layer; A transistor layer is disposed on the substrate; a planar layer, disposed on the transistor layer, the pixel definition layer disposed on the planar layer, the pixel definition layer further disposed with a second through hole, the second through hole being located in at least one of the display area and the non-display area, the second through hole being spaced apart from the first through hole, the second through hole being connected with the first through hole, the second through hole penetrating the pixel definition layer and the planar layer to expose the transistor layer, the isolation layer extending into the second through hole to contact the transistor layer; The self-repairing layer is disposed on the isolation layer and extends into the second through hole to contact the transistor layer.

8. The display panel according to claim 7, characterized in that: The isolation layer covers the sidewall of the first through hole.

9. The display panel according to claim 8, characterized in that: The self-repairing layer comprises a self-repairing material, and the self-repairing material comprises one or a combination of microcapsule self-repairing polymer materials, hollow fiber self-repairing polymer materials, nanoparticle self-repairing polymer materials and microvascular self-repairing polymer materials.

10. The display panel according to claim 9, characterized in that: The surface of the self-repairing layer away from the substrate is a hydrophobic surface.

11. A method for preparing a display panel, characterized in that: include: providing a substrate; forming a pixel definition layer on the substrate, wherein the pixel definition layer is provided with a first through hole, and the first through hole penetrates the pixel definition layer; forming an isolation layer on the pixel definition layer and located on the sidewall of the first through hole; and A light-emitting layer is disposed in the first through hole, and the isolation layer is located between the light-emitting layer and the pixel definition layer; The display panel is provided with a display area and a non-display area arranged around the display area, and the step of forming an isolation layer on the pixel definition layer and located on the side wall of the first through hole includes: Disposing metal on the pixel definition layer, and patterning the metal to form a metal layer of an isolation layer, wherein the metal layer is located on a side wall of the first through hole; The end of the metal layer is located at a side of the metal layer away from the display area, and the surface of the end of the metal layer away from the substrate is oxidized to form an insulating oxide layer; After the step of providing the light-emitting layer in the first through hole, the method further comprises: Disposing an electronic functional layer on the light-emitting layer and the pixel definition layer; An upper electrode is arranged on the electronic functional layer and the oxide layer, an end of the upper electrode is located at a side of the upper electrode away from the display area, and the end of the upper electrode is connected to the oxide layer.