Coal mining machine gear carburizing process simulation method, system, equipment and storage medium
The cellular automaton-finite difference model is used to simulate the shearer gear carburization process, which solves the problem of difficulty in observing the carbide precipitation and grain growth process in the existing technology, and realizes the carbon concentration and structure of the carburized layer and core. Dynamic evolution prediction reduces process development costs and provides optimization guidance.
Patent Information
- Application Number
- CN202111503128.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-09
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2041-12-09
AI Technical Summary
It is difficult to observe and simulate the carbide precipitation and grain growth process in real time during the shearer gear carburizing process with existing technology, resulting in high process development costs and difficulty in optimizing the carburizing process.
The cellular automaton-finite difference model is used to simulate the austenite grain growth process by calculating the carbon diffusion process and carbide precipitation rules, and provide dynamic evolution information of the carbon concentration and structure of the carburized layer and core.
It achieves visual prediction of the carbon concentration and structure evolution of the carburizing layer and core under different carburizing process conditions, reduces the cost of carburizing process development, and provides theoretical guidance to optimize process parameters.
Smart Images

Figure CN114417651B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of coal mining machine gear carburizing process simulation, and in particular to a coal mining machine gear carburizing process simulation method, system, equipment and storage medium. Background Art
[0002] Carburizing is an essential chemical heat treatment method for key gears of coal mining machines to obtain a highly wear-resistant surface and a toughened core. During the carburizing process, the evolution of the carbon concentration distribution on the surface of the tooth surface and the precipitation law of carbides determine the hardness and wear resistance of the tooth surface; the grains in the core of the gear will inevitably grow, which can easily cause the core to have a high hardness and poor toughness after quenching. During the development of the carburizing process for coal mining machine gears, the experimental method can only compare and observe the microstructure of the tooth surface and the core before and after carburizing. It is difficult to observe the precipitation of carbides on the surface of the tooth surface and the grain growth process in the core in real time, and the carburizing experiment has the disadvantages of long cycle and high energy consumption.
[0003] The invention patent with the prior art publication number CN108959832A provides a grain growth prediction model for optimizing the carburizing and quenching process of M50NiL steel. It predicts the grain growth during the carburizing process by establishing the austenite grain growth model of M50NiL steel, thereby putting forward specific requirements for the grain size before each heat treatment. In order to achieve the specified carburizing layer depth and optimize the carburizing process parameters, it can not only save the process experiment time and reduce the cost, but also avoid the rapid growth of the grains of the parts during the long-term carburizing process, thereby improving the mechanical properties of the parts and extending their service life. However, it can only calculate the grain size according to the formula, and it is impossible to give the grain morphology image information and dynamic evolution information at different carburizing moments, and it is also impossible to give the evolution laws such as carbon concentration, carbide morphology, size, etc., and it is also impossible to predict the grain growth of other types of alloy steels, so it is difficult to provide theoretical guidance for the development and optimization of the actual carburizing process, resulting in a high cost of carburizing process development.
[0004] Therefore, there is an urgent need to provide a carburizing simulation method that can provide grain morphology images and dynamic evolution information as well as dynamic image information such as carbon concentration and carbide morphology. Summary of the invention
[0005] To this end, the technical problem to be solved by the present invention is to overcome the problems existing in the prior art and propose a method, system, equipment and storage medium for simulating the carburizing process of coal mining machine gears, which can reproduce and visualize the microstructural evolution process of carbon concentration gradient distribution, carbide precipitation, and austenite grain growth during carburizing for different gear alloy steels, predict the carbon concentration and structure of the carburized layer and core under different carburizing process conditions, provide theoretical guidance for the development and optimization of the actual carburizing process, and reduce the cost of carburizing process development.
[0006] In order to solve the above technical problems, the present invention provides a method for simulating the carburizing process of a coal mining machine gear, comprising the following steps:
[0007] S1: Determine a region to be simulated, and initialize simulation data of the region to be simulated, wherein the simulation data includes the number of cells, the cell size, the simulation temperature, the number of grains, the grain orientation, the carbon concentration, and the diffusion coefficient;
[0008] S2: calculating the carbon diffusion process of the area to be simulated based on the initialized simulation data to obtain the carbon concentration distribution in the area;
[0009] S3: when the carbon concentration of a local area of the area to be simulated exceeds a preset concentration threshold, calculating the growth process of carbides to simulate the law of carbide precipitation;
[0010] S4: according to the carbide precipitation law, the grain boundary migration velocity of the carbide is set to 0, the austenite grain boundary migration velocity is calculated, and the austenite solid phase fraction change is obtained to simulate the austenite grain growth process;
[0011] S5: Repeat S2-S4 to obtain simulation results at different times, wherein the simulation results include the carbon diffusion process, carbide precipitation law, and austenite grain growth process.
[0012] In one embodiment of the present invention, in S1, the region to be simulated is selected from an established cellular automaton-finite difference model.
[0013] In one embodiment of the present invention, in S2, calculating the carbon diffusion process of the area to be simulated based on the initialized simulation data includes:
[0014] The finite difference method is used to solve the carbon diffusion equation, which is: Where D is the carbon diffusion coefficient related to temperature T and carbon concentration u, and p is the conversion equation related to the carbide phase fraction (φ). The conversion equation p is in the form of Where k is the carbide-austenite partition coefficient with respect to carbon concentration;
[0015] Calculate the diffusion coefficient in the carbon diffusion equation, and the calculation formula is: Where R is the ideal gas constant.
[0016] In one embodiment of the present invention, in S3, calculating the growth process of carbides includes:
[0017] The precipitation and growth of carbides in the carburized layer is controlled by the movement of the austenite-carbide phase boundary. The formula for calculating the movement rate of the austenite-carbide phase boundary is v = MΔG, where ΔG is the effective phase transformation driving force, M is the interface mobility, and M = M0exp(–Q / RT), where M0 is the pre-exponential factor, Q is the activation energy, and T is the temperature (K);
[0018] The interface movement speed is obtained based on the movement rate formula and the interface mobility formula Where T M is the melting point of pure iron, V m is the molar volume of austenite, is the calculated maximum solubility of austenite for carbon;
[0019] The phase fraction increment of carbide in one time step is calculated according to the interface movement speed: Where G is the shape adjustment factor related to the state of the adjacent cells, and its calculation formula is:
[0020] In one embodiment of the present invention, in S4, calculating the austenite grain boundary migration velocity includes:
[0021] During carburizing, the growth of austenite grains is controlled by the migration of austenite grain boundaries. The migration rate of austenite grain boundaries is Where γ is the interface energy, K is the grain boundary curvature, D0 is the grain boundary self-diffusion coefficient, k is the Boltzmann constant, and b is the Burgers vector length.
[0022] In addition, the present invention also provides a coal mining machine gear carburizing process simulation system, comprising:
[0023] A data initialization module is used to determine a region to be simulated, and the data initialization module is used to initialize simulation data of the region to be simulated, wherein the simulation data includes the number of cells, the size of the cells, the simulation temperature, the number of grains, the orientation of the grains, the carbon concentration, and the diffusion coefficient;
[0024] A carbon diffusion process simulation module, wherein the carbon diffusion process simulation module is used to calculate the carbon diffusion process of the area to be simulated based on the initialized simulation data to obtain the carbon concentration distribution in the area;
[0025] A carbide precipitation simulation module, which is used to calculate the growth process of carbides to simulate the law of carbide precipitation when the carbon concentration of a local area of the area to be simulated exceeds a preset concentration threshold;
[0026] The grain growth simulation module is used to set the grain boundary migration velocity of carbides to 0 according to the carbide precipitation law, calculate the austenite grain boundary migration velocity, and obtain the change of austenite solid phase fraction to simulate the austenite grain growth process.
[0027] In one embodiment of the present invention, the carbon diffusion process simulation module includes:
[0028] A carbon diffusion calculation submodule, which is used to calculate the carbon diffusion process of the area to be simulated based on the initialized simulation data, includes:
[0029] The finite difference method is used to solve the carbon diffusion equation, which is: Where D is the carbon diffusion coefficient related to temperature T and carbon concentration u, and p is the carbon phase fraction The relevant conversion equation, the conversion equation p is in the form of Where k is the carbide-austenite partition coefficient with respect to carbon concentration;
[0030] Calculate the diffusion coefficient in the carbon diffusion equation, and the calculation formula is: Where R is the ideal gas constant.
[0031] In one embodiment of the present invention, the carbide precipitation simulation module includes:
[0032] The carbide growth process calculation submodule is used to calculate the carbide growth process, including:
[0033] The precipitation and growth of carbides in the carburized layer is controlled by the movement of the austenite-carbide phase boundary. The formula for calculating the movement rate of the austenite-carbide phase boundary is v = MΔG, where ΔG is the effective phase transformation driving force, M is the interface mobility, and M = M0exp(–Q / RT), where M0 is the pre-exponential factor, Q is the activation energy, and T is the temperature (K);
[0034] The interface movement speed is obtained based on the movement rate formula and the interface mobility formula Where T M is the melting point of pure iron, V m is the molar volume of austenite, is the calculated maximum solubility of austenite for carbon;
[0035] The phase fraction increment of carbide in one time step is calculated according to the interface movement speed: Where G is the shape adjustment factor related to the state of the adjacent cells, and its calculation formula is:
[0036] In addition, the present invention also provides a computer device, including a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor implements the steps of a method for simulating the carburizing process of coal mining machine gears when executing the program.
[0037] In addition, the present invention also provides a computer-readable storage medium having a computer program stored thereon, characterized in that when the program is executed by a processor, the steps of a method for simulating the carburizing process of coal mining machine gears are implemented.
[0038] The above technical solution of the present invention has the following advantages compared with the prior art:
[0039] The present invention can reproduce and visualize the carbon concentration gradient distribution, carbide precipitation, and microstructural evolution of austenite grain growth during carburizing for different gear alloy steels, predict the carbon concentration and structure of the carburized layer and core under different carburizing process conditions, provide theoretical guidance for the development and optimization of the actual carburizing process, and reduce the cost of carburizing process development. BRIEF DESCRIPTION OF THE DRAWINGS
[0040] In order to make the contents of the present invention more clearly understood, the present invention is further described in detail below based on specific embodiments of the present invention in conjunction with the accompanying drawings.
[0041] Figure 1 It is a schematic flow chart of the method for simulating the carburizing process of coal mining machine gears of the present invention.
[0042] Figure 2 This is the initialization grain morphology diagram of the present invention: (a) grain orientation display; (b) carbon concentration display.
[0043] Figure 3 Graphs showing changes in carburized layer thickness and average grain size over time at different carburizing temperatures of the present invention: (a) 920°C; (b) 950°C; (c) 980°C.
[0044] Figure 4 It is a graph showing the change of average carbon concentration with the distance from the left side at different carburizing temperatures of the present invention.
[0045] Figure 5 These are the simulation results of the carbide precipitation process on the tooth surface during carburizing at 950°C shown by the carbon concentration of the present invention: (a) 0.5s; (b) 100s; (c) 2000s.
[0046] Figure 6 Graphs showing the evolution of the grain morphology of the gear core at different carburizing temperatures of the present invention: (a) 920°C; (b) 950°C; (c) 980°C.
[0047] Figure 7 This is the austenite grain morphology evolution diagram when there is carbide distribution at 950°C of the present invention: (a) there are 20 carbides in the simulation area; (b) there are 40 carbides in the simulation area.
[0048] Figure 8 The relationship between the number of grains and the average grain size at different carburizing temperatures of the present invention is: (a) the relationship between time and the number of grains; (b) the relationship between time and the average grain size.
[0049] Fig. 9 This is the effect of the amount of carbides on the average grain size at 950°C of the present invention.
[0050] Fig.10 It is a hardware structure schematic diagram of the carburizing process simulation system of the coal mining machine gear of the present invention.
[0051] Fig.11 It is a structural schematic diagram of the computer device of the present invention.
[0052] The reference numerals are described as follows: 10, processor; 11, memory; 12, communication interface; 13, communication bus;
[0053] 20. Data initialization module; 21. Carbon diffusion process simulation module; 22. Carbide precipitation simulation module; 23. Grain growth simulation module. DETAILED DESCRIPTION
[0054] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments so that those skilled in the art can better understand the present invention and implement it, but the embodiments are not intended to limit the present invention.
[0055] Embodiment 1
[0056] See also Figure 1 and 2 As shown, this embodiment provides a method for simulating the carburizing process of a coal mining machine gear, comprising the following steps:
[0057] S1: Determine a region to be simulated, and initialize simulation data of the region to be simulated, wherein the simulation data includes the number of cells, the cell size, the simulation temperature, the number of grains, the grain orientation, the carbon concentration, and the diffusion coefficient;
[0058] S2: calculating the carbon diffusion process of the area to be simulated based on the initialized simulation data to obtain the carbon concentration distribution in the area;
[0059] S3: when the carbon concentration of a local area of the area to be simulated exceeds a preset concentration threshold, calculating the growth process of carbides to simulate the law of carbide precipitation;
[0060] S4: According to the carbide precipitation law, the grain boundary migration velocity of carbides is set to 0, the austenite grain boundary migration velocity is calculated, and the change of austenite solid phase fraction is obtained to simulate the austenite grain growth process;
[0061] S5: Repeat S2-S4 to obtain simulation results at different times, wherein the simulation results include the carbon diffusion process, carbide precipitation law, and austenite grain growth process.
[0062] In a method for simulating the carburizing process of a coal mining machine gear disclosed in the present invention, the area to be simulated is selected from an established cellular automaton-finite difference model.
[0063] Wherein, in S2, the carbon diffusion process of the area to be simulated is calculated based on the initialized simulation data, including:
[0064] S2.1: The carbon diffusion equation is solved by the finite difference method. The carbon diffusion equation is: Where D is the carbon diffusion coefficient related to temperature T and carbon concentration u, and p is the conversion equation related to the carbide phase fraction (φ). The conversion equation p is in the form of Where k is the carbide-austenite partition coefficient with respect to carbon concentration, which is calculated by the thermodynamic software Pandat;
[0065] S2.2: Calculate the diffusion coefficient in the carbon diffusion equation, and the calculation formula is: Where R is the ideal gas constant.
[0066] When simulating carbon diffusion in the above carburizing process, Robin boundary conditions are used for high carbon potential boundaries.
[0067] Among them, in S3, the growth process of carbides is calculated, including:
[0068] S3.1: The precipitation and growth of carbides in the carburized layer is controlled by the movement of the austenite-carbide phase boundary. The formula for calculating the austenite-carbide phase boundary movement rate is v = MΔG, where ΔG is the effective phase transformation driving force, M is the interface mobility, and M = M0exp(–Q / RT), where M0 is the pre-exponential factor, Q is the activation energy, and T is the temperature (K);
[0069] S3.2: Based on the dilute solution assumption, the interface migration velocity is obtained based on the migration rate formula and the interface mobility formula Where T M is the melting point of pure iron, V m is the molar volume of austenite, is the calculated maximum solubility of austenite for carbon;
[0070] S3.3: At the phase interface, the increment of the carbide phase fraction within one time step is calculated based on the interface movement velocity: Where G is the shape adjustment factor related to the state of the adjacent cells, and its calculation formula is:
[0071] Among them, in S4, the austenite grain boundary migration velocity is calculated, including:
[0072] During carburizing, the growth of austenite grains is controlled by the migration of austenite grain boundaries. The migration rate of austenite grain boundaries is Where γ is the interface energy, K is the grain boundary curvature, D0 is the grain boundary self-diffusion coefficient, k is the Boltzmann constant, and b is the Burgers vector length.
[0073] The present invention combines thermodynamic calculations and can reproduce and visualize the carbon concentration gradient distribution, carbide precipitation, and microstructural evolution of austenite grain growth during carburizing for different gear alloy steels, predict the carbon concentration and structure of the carburized layer and core under different carburizing process conditions, provide theoretical guidance for the development and optimization of the actual carburizing process, and reduce the cost of carburizing process development.
[0074] The following is a detailed description of a method for simulating the carburizing process of a coal mining machine gear according to the present invention using a specific simulation example and the simulation results obtained.
[0075] (1) Simulation results of carbon diffusion during carburizing of 18Cr2Ni4WA gear alloy steel
[0076] For 18Cr2Ni4WA gear alloy steel, the simulation area is a 400×20 square grid with a grid size of 5μm, the initial carbon concentration is 0.18wt.%, and the left boundary is a high carbon potential carburizing source. The initial simulation results are shown in Figure 2 As shown, Figure 2 (a) Different gray values represent different grain orientations. Figure 2 (b) Black indicates grain boundaries, and gray indicates the interior of the grain. The initial average grain size is 40.5 μm.
[0077] The changes of carburized layer thickness and grain size over time at different carburizing temperatures are shown in Figure 2. Figure 3As shown, the part with the largest gray value is the grain boundary, and the part with gray value between the maximum and minimum is the carburized layer. According to statistics, at the carburizing temperature of 920℃, the carburizing layer thickness at t=60s is 175μm, and the average grain size is 41.3μm; at the carburizing temperatures of 950℃ and 980℃, the carburizing layer thickness at t=60s is 225μm and 275μm respectively, and the average grain size is 42.0μm and 42.7μm. Under the same carburizing time, the higher the carburizing temperature, the faster the diffusion rate of carbon in austenite, the thicker the carburized layer, the better the carburizing effect, and the higher the surface hardness; but the average grain size will increase, making the internal structure grains coarse and the mechanical properties decreased. Figure 4 As shown in the figure, the average carbon concentration changes with the distance on the left side at different carburizing temperatures. The higher the carburizing temperature, the greater the average carbon concentration in the simulation area, which proves that the higher the temperature, the faster the diffusion rate of carbon, more carbon enters the austenite structure, and the carburizing thickness increases.
[0078] (2) Carbide precipitation simulation results
[0079] The calculation area is set to 500×100 grid calculation area, and the grid size is 0.2μm. It is set that a carbide nucleates and grows at the grain boundary, and the driving force for the growth of carbides comes from the difference between the maximum solubility of austenite to carbon and the actual carbon concentration. Figure 5 The simulation results of carbide precipitation on the gear surface during carburizing at 950°C are shown in carbon concentration. It can be seen that carbon diffuses into the calculation area from the left boundary of high carbon potential, and the carbide begins to grow after absorbing the diffused carbon element. Figure 5 (b) and Figure 5 As shown in (c), a low-carbon area is formed around the carbide. This is because the growth of the carbide consumes the carbon element in the matrix, and the carbon element in the matrix cannot replenish the consumed carbon element in time, forming a concentration gradient around the carbide. As carburization continues, the carbide continues to grow along the carbon concentration gradient in the matrix, that is, it grows towards the high carbon potential area. Figure 5 The evolution process of carbide precipitation is reproduced, and the simulation prediction of carbide precipitation under different process parameters can also be realized.
[0080] (3) Grain growth simulation results
[0081] The established model was used, and the calculation area was a 500×500 square grid with a grid size of 1 μm. Figure 6 (a) Figure 6 (b) and Figure 6 (c) The change of the grain morphology of the gear core with time during carburization at 920℃, 950℃, and 980℃. Different gray values represent different grain orientations. The initial grain size in the three examples is 20.2μm. Figure 6As can be seen in (a), when the carburizing temperature is 920℃ and the time is 100s, the grains are small and hexagonal in shape. The average grain size is 23.5μm. When the carburizing time reaches 1000s, the average grain size is 48.6μm. When the carburizing time reaches 2000s, the average grain size is 66.8μm. When the carburizing time reaches 3600s, the average grain size is 86.9μm. After 2000s of carburizing time, the grain size becomes 4.302 times the initial grain size, and the total growth rate is 330.2%. Similarly, if Figure 6 As shown in (b), when the carburizing time reaches 100s, the average grain size is 25.2μm; when the carburizing time reaches 1000s, the average grain size is 53.0μm; when the carburizing time reaches 2000s, the average grain size is 71.0μm; when the carburizing time reaches 3600s, the average grain size is 88.6μm. When the carburizing temperature is 980℃, the simulation results are as follows Figure 6 As shown in (c), when the carburizing time reaches 100s, the average grain size is 27.0μm; when the carburizing time reaches 1000s, the average grain size is 61.4μm; when the carburizing time reaches 2000s, the average grain size is 86.9μm; when the carburizing time reaches 3600s, the average grain size is 122.9μm. From the simulation results and statistical data, it can be seen that at the same temperature, with the increase of carburizing time, the average grain size increases rapidly; at the same carburizing time, with the increase of carburizing temperature, the grain size also increases.
[0082] When carbides exist at the austenite grain boundaries, the austenite grain morphology evolution diagram at 950°C is as follows: Figure 7 As shown, there are 20 carbides in group (a) and 40 carbides in group (b). According to statistics, when the carburizing time is 100s, 1000s, 2000s and 3600s, the average grain size of group (a) is 24.8μm, 42.6μm, 48.3μm and 51.1μm respectively; the average grain size of group (b) is 24.4μm, 36.4μm, 39.4μm and 41.4μm respectively. From the statistical data, it can be seen that with the increase of carburizing time, the grain size gradually increases, but because the carbides are at the grain boundaries, they play a pinning role on the grain boundaries and hinder the migration of the grain boundaries, resulting in the average grain size of the carbides with a large number being smaller than the average grain size of the carbides with a small number.
[0083] Figure 8 To statistically analyze the relationship between the average number and size of grains and carburizing time when there is no carbide in the simulation area at three different carburizing temperatures. Figure 8As shown in (a), the number of grains decreases with the increase of carburizing time. In the initial stage, due to the large number of grains, small size, large grain curvature and large surface energy, the phase change speed is fast and the number of grains decreases rapidly. In the later stage of carburizing, the number of grains in the simulation area tends to be stable. The higher the temperature, the lower the activation energy of grain boundary movement, the higher the average grain boundary mobility, and the faster the grain growth rate; at the same time, the number of grains in the simulation area is less. Figure 8 (b) is the relationship between carburizing time and grain size. It can be seen that with the increase of carburizing time, the grain size gradually increases. In the initial stage, the number of grains decreases rapidly, so the grain size increases rapidly; the rate of decrease in the number of grains gradually decreases, and the rate of increase in the average grain size gradually decreases.
[0084] The effect of carbide quantity on average grain size at 950℃ is as follows: Fig. 9 As shown. With the increase of carburizing time, the number of carbides will not affect the trend of grain size increase, but will affect the size of the average grain size. At the same carburizing temperature, the more carbides there are at the grain boundary, the greater the pinning effect on the grain boundary, which inhibits grain boundary migration and reduces the grain growth rate and the final average grain size. In the carburizing process of gear alloy steel, in order to obtain a core structure with fine grains, it is beneficial to have an appropriate number of dispersed carbides in the core.
[0085] Embodiment 2
[0086] A coal mining machine gear carburizing process simulation system disclosed in Embodiment 2 of the present invention is introduced below. The coal mining machine gear carburizing process simulation system described below and the coal mining machine gear carburizing process simulation method described above can refer to each other.
[0087] See also Fig.10 As shown, this embodiment discloses a coal mining machine gear carburizing process simulation system, including:
[0088] A data initialization module 20 is used to determine a region to be simulated, and the data initialization module 20 is used to initialize simulation data of the region to be simulated, wherein the simulation data includes the number of cells, the cell size, the simulation temperature, the number of grains, the grain orientation, the carbon concentration and the diffusion coefficient;
[0089] A carbon diffusion process simulation module 21, wherein the carbon diffusion process simulation module 21 is used to calculate the carbon diffusion process of the area to be simulated based on the initialized simulation data, wherein the carbon diffusion process includes carbon concentration distribution;
[0090] A carbide precipitation simulation module 22, which is used to calculate the growth process of carbides to simulate the carbide precipitation law when the carbon concentration of the local area of the area to be simulated exceeds a preset concentration threshold;
[0091] The grain growth simulation module 23 is used to set the grain boundary migration velocity of carbides to 0 according to the carbide precipitation law, calculate the austenite grain boundary migration velocity, and obtain the change of austenite solid phase fraction to simulate the austenite grain growth process.
[0092] Wherein, the carbon diffusion process simulation module 21 includes:
[0093] A carbon diffusion calculation submodule, which is used to calculate the carbon diffusion process of the area to be simulated based on the initialized simulation data, includes:
[0094] The finite difference method is used to solve the carbon diffusion equation, which is: Where D is the carbon diffusion coefficient related to temperature T and carbon concentration u, and p is the conversion equation related to the carbide phase fraction (φ). The conversion equation p is in the form of Where k is the carbide-austenite partition coefficient with respect to carbon concentration;
[0095] Calculate the diffusion coefficient in the carbon diffusion equation, and the calculation formula is: Where R is the ideal gas constant.
[0096] Wherein, the carbide precipitation simulation module 22 includes:
[0097] The carbide growth process calculation submodule is used to calculate the carbide growth process, including:
[0098] The precipitation and growth of carbides in the carburized layer is controlled by the movement of the austenite-carbide phase boundary. The formula for calculating the movement rate of the austenite-carbide phase boundary is v = MΔG, where ΔG is the effective phase transformation driving force, M is the interface mobility, and M = M0exp(–Q / RT), where M0 is the pre-exponential factor, Q is the activation energy, and T is the temperature (K);
[0099] The interface movement speed is obtained based on the movement rate formula and the interface mobility formula Where T M is the melting point of pure iron, V m is the molar volume of austenite, is the calculated maximum solubility of austenite for carbon;
[0100] The phase fraction increment of carbide in one time step is calculated according to the interface movement speed: Where G is the shape adjustment factor related to the state of the adjacent cells, and its calculation formula is:
[0101] The coal mining machine gear carburizing process simulation system of the present embodiment is used to implement the aforementioned coal mining machine gear carburizing process simulation method. Therefore, the specific implementation method of the system can be seen in the embodiment part of the coal mining machine gear carburizing process simulation method in the previous text. Therefore, its specific implementation method can refer to the description of the corresponding various parts of the embodiment, which will not be elaborated here.
[0102] In addition, since the coal mining machine gear carburizing process simulation system of this embodiment is used to implement the aforementioned coal mining machine gear carburizing process simulation method, its function corresponds to that of the aforementioned method and will not be repeated here.
[0103] Embodiment 3
[0104] A computer device and a storage medium disclosed in Embodiment 3 of the present invention are introduced below. The computer device and the storage medium described below and the method for simulating the carburizing process of a coal mining machine gear described above can be referred to each other.
[0105] An embodiment of the present invention further provides a computer device, including:
[0106] A memory for storing computer programs;
[0107] A processor is used to implement the steps of the above-mentioned method for simulating the carburizing process of coal mining machine gears when executing a computer program.
[0108] See also Fig.11 , which is a schematic diagram of the structure of a computer device, the computer device may include: a processor 10, a memory 11, a communication interface 12 and a communication bus 13. The processor 10, the memory 11 and the communication interface 12 communicate with each other through the communication bus 13.
[0109] In the embodiment of the present invention, the processor 10 may be a central processing unit (CPU), an application specific integrated circuit, a digital signal processor, a field programmable gate array or other programmable logic devices.
[0110] The processor 10 may call a program stored in the memory 11. Specifically, the processor 10 may execute operations in an embodiment of a method for simulating a carburizing process of a coal mining machine gear.
[0111] The memory 11 is used to store one or more programs. The program may include program codes, and the program codes include computer operation instructions.
[0112] In addition, the memory 11 may include a high-speed random access memory, and may also include a non-volatile memory, such as at least one disk storage device or other volatile solid-state storage device.
[0113] The communication interface 12 may be an interface of a communication module, and is used to connect to other devices or systems.
[0114] Of course, it should be noted that Fig.10 The structure shown does not constitute a limitation on the computer device in the embodiment of the present application. In actual applications, the computer device may include Fig.10 More or fewer components than shown, or combinations of certain components.
[0115] An embodiment of the present invention further provides a computer-readable storage medium, on which a computer program is stored. When the computer program is executed by a processor, the steps of the above-mentioned method for simulating the carburizing process of coal mining machine gears are implemented.
[0116] Those skilled in the art will appreciate that the embodiments of the present application may be provided as methods, systems, or computer program products. Therefore, the present application may adopt the form of a complete hardware embodiment, a complete software embodiment, or an embodiment in combination with software and hardware. Moreover, the present application may adopt the form of a computer program product implemented in one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) that include computer-usable program code.
[0117] The present application is described with reference to the flowcharts and / or block diagrams of the methods, devices (systems), and computer program products according to the embodiments of the present application. It should be understood that each process and / or box in the flowchart and / or block diagram, as well as the combination of the processes and / or boxes in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing device to generate a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.
[0118] These computer program instructions may also be stored in a computer-readable memory capable of directing a computer or other programmable data processing device to operate in a specific manner, so that the instructions stored in the computer-readable memory produce an article of manufacture comprising an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.
[0119] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process in the computer or other programmable device. Figure 1 A process or multiple processes and / or boxes Figure 1 A step that specifies a function in one or more boxes.
[0120] Obviously, the above embodiments are merely examples for clear explanation and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived from these are still within the protection scope of the invention.
Claims
1. A method for simulating the carburizing process of a coal mining machine gear, characterized in that: The following steps are involved: S1: Determine a region to be simulated, and initialize simulation data of the region to be simulated, wherein the simulation data includes the number of cells, the cell size, the simulation temperature, the number of grains, the grain orientation, the carbon concentration, and the diffusion coefficient; S2: Calculate the carbon diffusion process in the area to be simulated based on the initialized simulation data to obtain the carbon concentration distribution in the area; S3: when the carbon concentration of a local area of the area to be simulated exceeds a preset concentration threshold, calculating the growth process of carbides to simulate the law of carbide precipitation; S4: According to the carbide precipitation law, the grain boundary migration velocity of carbides is set to 0, the austenite grain boundary migration velocity is calculated, and the change of austenite solid phase fraction is obtained to simulate the austenite grain growth process; S5: repeating S2-S4 to obtain simulation results at different times, wherein the simulation results include the carbon diffusion process, the carbide precipitation law, and the austenite grain growth process; The step of calculating the carbon diffusion process of the area to be simulated based on the initialized simulation data includes: The finite difference method is used to solve the carbon diffusion equation, which is: Where D is the carbon diffusion coefficient related to temperature T and carbon concentration u, and p is the carbon phase fraction The relevant conversion equation, the conversion equation p is in the form of Where k is the carbide-austenite partition coefficient with respect to carbon concentration; Calculate the diffusion coefficient in the carbon diffusion equation, and the calculation formula is: Where R is the ideal gas constant; In S3, the carbide growth process is calculated, including: The precipitation and growth of carbides in the carburized layer is controlled by the movement of the austenite-carbide phase boundary. The formula for calculating the movement rate of the austenite-carbide phase boundary is v = MΔG, where ΔG is the effective phase transformation driving force, M is the interface mobility, and M = M0exp(–Q / RT), where M0 is the pre-exponential factor, Q is the activation energy, and T is the temperature; The interface movement speed is obtained based on the movement rate formula and the interface mobility formula Where T M is the melting point of pure iron, V m is the molar volume of austenite, is the calculated maximum solubility of austenite for carbon; The phase fraction increment of carbide in one time step is calculated according to the interface movement speed: Where G is the shape adjustment factor related to the state of the adjacent cells, and its calculation formula is:
2. The method for simulating the carburizing process of coal mining machine gear according to claim 1, characterized in that: In S1, the region to be simulated is selected from an established cellular automaton-finite difference model.
3. The method for simulating the carburizing process of coal mining machine gear according to claim 1, characterized in that: In S4, the austenite grain boundary migration velocity is calculated, including: During carburizing, the growth of austenite grains is controlled by the migration of austenite grain boundaries. The migration rate of austenite grain boundaries is Where γ is the interface energy, K is the grain boundary curvature, D0 is the grain boundary self-diffusion coefficient, k is the Boltzmann constant, and b is the Burgers vector length.
4. A coal mining machine gear carburizing process simulation system, characterized in that: include: A data initialization module is used to determine a region to be simulated, and the data initialization module is used to initialize simulation data of the region to be simulated, wherein the simulation data includes the number of cells, the size of the cells, the simulation temperature, the number of grains, the orientation of the grains, the carbon concentration, and the diffusion coefficient; A carbon diffusion process simulation module, wherein the carbon diffusion process simulation module is used to calculate the carbon diffusion process of the area to be simulated based on the initialized simulation data to obtain the carbon concentration distribution in the area; A carbide precipitation simulation module, which is used to calculate the growth process of carbides to simulate the law of carbide precipitation when the carbon concentration of a local area of the area to be simulated exceeds a preset concentration threshold; A grain growth simulation module, which is used to set the grain boundary migration velocity of carbides to 0 according to the carbide precipitation law, calculate the austenite grain boundary migration velocity, and obtain the austenite solid phase fraction change to simulate the austenite grain growth process; Wherein, the carbon diffusion process simulation module includes: A carbon diffusion calculation submodule, which is used to calculate the carbon diffusion process of the area to be simulated based on the initialized simulation data, includes: The finite difference method is used to solve the carbon diffusion equation, which is: Where D is the carbon diffusion coefficient related to temperature T and carbon concentration u, and p is the carbon phase fraction The relevant conversion equation, the conversion equation p is in the form of Where k is the carbide-austenite partition coefficient with respect to carbon concentration; Calculate the diffusion coefficient in the carbon diffusion equation, and the calculation formula is: Where R is the ideal gas constant; The carbide precipitation simulation module includes: The carbide growth process calculation submodule is used to calculate the carbide growth process, including: The precipitation and growth of carbides in the carburized layer is controlled by the movement of the austenite-carbide phase boundary. The formula for calculating the movement rate of the austenite-carbide phase boundary is v = MΔG, where ΔG is the effective phase transformation driving force, M is the interface mobility, and M = M0exp(–Q / RT), where M0 is the pre-exponential factor, Q is the activation energy, and T is the temperature (K); The interface movement speed is obtained based on the movement rate formula and the interface mobility formula Where T M is the melting point of pure iron, V m is the molar volume of austenite, is the calculated maximum solubility of austenite for carbon; The phase fraction increment of carbide in one time step is calculated according to the interface movement speed: Where G is the shape adjustment factor related to the state of the adjacent cells, and its calculation formula is:
5. A computer device comprising a memory, a processor and a computer program stored in the memory and executable on the processor, characterized in that: When the processor executes the program, the steps of the method according to any one of claims 1 to 3 are implemented.
6. A computer-readable storage medium having a computer program stored thereon, characterized in that: When the program is executed by a processor, the steps of the method according to any one of claims 1 to 3 are implemented.