Lead compound, preparation method, use and lubricating oil composition thereof
A lead compound with alkylbenzene carboxylic acid structures addresses solubility and stability issues in polyalkyl cyclopentane lubricants, providing enhanced anti-wear and friction reduction for land and space machinery.
Patent Information
- Application Number
- CN202011183654.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-10-30
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2040-10-30
AI Technical Summary
Existing lead cyclopentaneate compounds exhibit poor oil solubility and stability in polyalkyl cyclopentane-based space lubricants, leading to stratification and precipitation, and there is a need for improved anti-wear and friction reduction properties in both land and space lubricants.
A lead compound with specific alkylbenzene carboxylic acid structures is synthesized through saponification or double decomposition reactions, enhancing solubility and stability, and a lubricating oil composition is formulated with these compounds in various base oils.
The lead compound demonstrates improved solubility, anti-wear, and friction reduction properties, ensuring long-term stability and performance in both terrestrial and space machinery lubricants without stratification or precipitation.
Smart Images

Figure CN114436825B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a lead compound, in particular to a lead compound with excellent anti-wear and anti-oxidation properties and a preparation method thereof. Background Art
[0002] Lead naphthenate is an extreme pressure anti-wear agent with excellent performance. It forms a lead-containing extreme pressure film on the surface of the friction pair through chemical reaction, which can reduce the shear strength of the contact surface of the friction pair and the friction coefficient during relative motion, so that mechanical equipment can work normally. Therefore, it is widely used in industrial lubricants, greases and space lubricants.
[0003] Chinese Patent 201410581489.6 "An Antioxidant Lubricant for Automobiles" discloses an antioxidant lubricant for automobiles, comprising dienyl succinimide, alkylated diphenylamine, lead cyclopentaneate, polymethacrylate, petroleum barium borate, poly-α-olefin, methyl silicone oil, antimony diisopropyl dithiophosphate, oleyl glycerol and base oil.
[0004] Chinese patent 201210177400.0 "A method for preparing a metal cutting fluid with good extreme pressure resistance" discloses a method for preparing a metal cutting fluid with good extreme pressure resistance, the preparation method comprising: 1) synthesizing diethanolamine boric acid polycarboxylic acid complex ester, 2) synthesizing diethanolamine boric acid maleic anhydride complex ester, 3) adding lead cyclopentaneate, oleic acid, barium petroleum sulfonate, triethanolamine, borax, sodium silicate, nitrobenzoic acid in sequence under stirring, continuing to stir for 20 to 40 minutes after all are added, cooling to 50 to 60°C, adding sodium molybdate and boric acid, stirring for 20 to 30 minutes, adding methyl silicone oil, stirring for 10 to 20 minutes; 4) mixing the products of steps 1 to 3 to obtain the final product. The purpose of this invention is to propose a method for preparing a metal cutting fluid with good extreme pressure resistance.
[0005] Chinese patent CN85100213A "High-load extreme-pressure lithium-based grease" discloses a high-load extreme-pressure lithium-based grease, which is characterized by containing a group of sulfur, lead, molybdenum, and amine-type composite extreme-pressure additives, including 2.0% to 10.0% sulfurized olefin cottonseed oil, 0.3% to 3.0% lead cyclopentaneate, 0.1% to 0.5% benzotriazole octadecylamine, 0.3% to 0.4% dibutyl dithiocarbamate lead and 0.5% to 5.0% dibutyl dithiocarbamate molybdenum oxysulfide.
[0006] Lead cyclopentaneate anti-wear agent can also be used to prepare space lubricants. The prepared lubricants are mainly used for lubrication of moving parts of space devices. Since space parts are in a high vacuum space environment, they need to have excellent low volatility and lubrication properties to ensure long-term and stable operation of lubricated parts. The base oils used in space lubricants generally include silicone oil, perfluoropolyether oil, PAO, polyalkyl cyclopentane, etc. Among them, polyalkyl cyclopentane has comprehensive performance and is the main base oil for space lubricants. The lubricating oil composition prepared from lead cyclopentaneate and polyalkyl cyclopentane base oils has extremely low volatility and saturated vapor pressure, good viscosity-temperature properties and lubrication properties, especially good extreme pressure and anti-wear properties under boundary lubrication conditions, and is a good lubricant for space equipment.
[0007] However, the existing lead cyclopentane has poor oil solubility in polyalkylcyclopentane and will undergo stratification and precipitation after dissolution, which affects its extreme pressure and anti-wear effects.
[0008] At the same time, the extreme pressure anti-wear and friction reduction properties of existing lead-containing anti-wear agents used in land machinery transmission lubricants need to be further improved. Summary of the invention
[0009] In order to overcome the defects in the prior art, the present invention provides a lead compound and a preparation method and use thereof, and a lubricating oil composition containing the lead compound, including the following aspects.
[0010] In a first aspect, the present invention provides a lead compound.
[0011] The lead compound of the present invention has a structure as shown in formula (I):
[0012]
[0013] The A group in formula (I) is selected from the group represented by formula (II) and / or the group represented by formula (III);
[0014]
[0015] In formula (II), the R0 group is C 1~6 A straight or branched alkylene group; x is an integer between 0 and 4, and x R1 groups are each independently selected from C 2~40 A straight chain or branched alkyl group; The ring group is (x+1) valent C 3~20 The cycloalkyl group, The ring group is a cycloalkyl group having 1 to 5 rings;
[0016] In formula (III), the R2 group is C 2~30 A straight chain or branched chain alkyl group.
[0017] According to the present invention, preferably, The ring group is (x+1) valent C 3~10 The cycloalkyl group, The ring group is a cycloalkyl group with 1 to 3 rings, and the R0 group is C 1~5 A straight or branched alkylene group; x is an integer between 1 and 3, and the x R1 groups are each independently selected from C 2~30 A straight chain or branched alkyl group; R2 group is C 8~24 A straight chain or branched chain alkyl group.
[0018] According to the present invention, the lead compound can be selected from one or more of the following lead compounds:
[0019] (1) Alkylbenzene carboxylic acid lead cyclopentanoate, its structure is:
[0020]
[0021] Where R a0 C8~C 24 Alkyl, R a1 is C1~C3 alkylene, R a2 C8~C 24 alkyl;
[0022] (2) Alkylbenzene carboxylic acid lead cyclohexane acid, its structure is:
[0023]
[0024] Where R b0 C8~C 24 Alkyl, R b1 is C1~C3 alkylene, R b2 C8~C 24 alkyl;
[0025] (3) Alkylbenzene carboxylic acid biscyclopentanoate lead, its structure is:
[0026]
[0027] Where R c0 C8~C 24 Alkyl, R c1 is C1~C3 alkylene, R c2 C8~C 24 alkyl;
[0028] (4) Alkylbenzene carboxylic acid biscyclohexane lead, its structure is:
[0029]
[0030] Where R d0 C8~C 24 Alkyl, Rd1 is C1~C3 alkylene, R d2 C8~C 24 alkyl;
[0031] (5) Alkylbenzene carboxylic acid bicycloalkanoic acid lead, its structure is:
[0032]
[0033] Where R e0 C8~C 24 Alkyl, R e1 is C1~C3 alkylene, R e2 C8~C 24 alkyl;
[0034] (6) Alkylbenzene carboxylic acid tricycloalkanoic acid lead, its structure is:
[0035]
[0036] Where R f0 C8~C 24 Alkyl, R f1 is C1~C3 alkylene, R f2 C8~C 24 alkyl;
[0037] (7) Alkylbenzene carboxylic acid tricycloalkanoic acid lead, its structure is:
[0038]
[0039] Where R g0 C8~C 24 Alkyl, R g1 is C1~C3 alkylene, R g2 C8~C 24 alkyl.
[0040] The lead compound of the present invention has excellent oil solubility, anti-wear property and friction reduction property, and is an anti-wear agent with excellent performance. It can be used for lubrication of vehicle gears, industrial gears and transmission of other mechanical parts, and can also be used for lubrication of space moving parts. In particular, it can solve the problem that the existing extreme pressure anti-wear agent has poor solubility and low stability in space lubricants based on polyalkyl cyclopentane oil, and is difficult to meet the requirements of space lubricants.
[0041] In a second aspect, the present invention provides a method for preparing the lead compound described in the first aspect.
[0042] The method for preparing the lead compound of the first aspect comprises a saponification reaction or a double decomposition reaction;
[0043] The saponification reaction is a step of reacting the compound represented by formula (α) and / or the compound represented by formula (β) with lead oxide;
[0044]
[0045] In formula (α), the R0 group is C 1~6 A straight or branched alkylene group; x is an integer between 0 and 4, and x R1 groups are each independently selected from C 2~40 A straight chain or branched alkyl group; The ring group is (x+1) valent C 3~20 The cycloalkyl group The ring group is a cycloalkyl group with 1 to 5 rings; in formula (β), the R2 group is C 2~30 A straight chain or branched alkyl group;
[0046] The double decomposition reaction is a step of reacting the compound represented by formula (α') and / or the compound represented by formula (β') with a lead salt;
[0047]
[0048] In formula (α'), the R0 group is C 1~6 A straight or branched alkylene group; x is an integer between 0 and 4, and x R1 groups are each independently selected from C 2~40 A straight chain or branched alkyl group; The ring group is (x+1) valent C 3~20 The cycloalkyl group The ring group is a cycloalkyl group with 1 to 5 rings; in formula (β'), the R2 group is C 2~30 wherein M in formula (α') and formula (β') is independently Na or K.
[0049] According to the preparation method of the present invention, preferably, The ring group is (x+1) valent C 3~10 The cycloalkyl group The ring group is a cycloalkyl group with 1 to 3 rings, and the R0 group is C 1~5 A straight or branched alkylene group; x is an integer between 1 and 3, and the x R1 groups are each independently selected from C 2~30 A straight chain or branched alkyl group; R2 group is C 8~24 A straight chain or branched alkyl group; M is Na.
[0050] According to the preparation method of the present invention, the lead oxide can be selected from melathione and / or chrysanthemum, preferably chrysanthemum. The melathione is a red tetragonal crystal, and the chrysanthemum is a yellow orthorhombic crystal.
[0051] According to the preparation method of the present invention, the lead salt can be selected from one or more of lead nitrate, lead chloride and lead acetate, preferably lead acetate.
[0052] According to the preparation method of the present invention, in the saponification reaction, the molar ratio of the compound represented by formula (α) and / or the compound represented by formula (β) to lead oxide is 0.6-1.6:0.3-0.8, preferably 0.8-1.4:0.4-0.7, most preferably 0.9-1.1:0.45-0.55, preferably, the molar ratio between the compound represented by formula (α) and the compound represented by formula (β) is 0.5-6:1, preferably 0.8-3:1, most preferably 1.5-2.5:1. In the reaction of the compound represented by formula (α) and / or the compound represented by formula (β) with lead oxide, the compound represented by formula (α) and / or the compound represented by formula (β) and lead oxide can be added once or multiple times, for example, can be added in 1 to 5 times, preferably 1 to 3 times, most preferably 2 to 3 times.
[0053] According to the preparation method of the present invention, in the saponification reaction, in the reaction between the compound represented by formula (α) and / or the compound represented by formula (β) and lead oxide, a promoter may be added. The promoter may be one or more of low molecular alcohol, acid and water, preferably low molecular alcohol and / or acid, most preferably low molecular alcohol. The low molecular alcohol is C 1~5 Alcohol, preferably C 1~3 Alcohol, most preferably C 2~3 The amount of the accelerator added is preferably 0.01% to 1% of the total mass of the compound represented by formula (α) and / or the compound represented by formula (β) and lead oxide, and more preferably 0.05% to 0.8%.
[0054] According to the preparation method of the present invention, in the saponification reaction, the temperature for reacting the compound represented by formula (α) and / or the compound represented by formula (β) with lead oxide can be 40 to 300°C, preferably 60 to 200°C, and most preferably 100 to 150°C, and the reaction time can be 2 to 10 hours, preferably 3 to 8 hours, and most preferably 4 to 6 hours.
[0055] According to the preparation method of the present invention, for the saponification reaction, a filtering operation can be performed after the reaction of the compound represented by formula (α) and / or the compound represented by formula (β) with lead oxide is completed to remove unreacted lead oxide. Before the filtering operation, a solvent may be added or not, but preferably a solvent is added. The solvent is preferably a hydrocarbon solvent, for example, one or more of solvent gasoline, n-octane and xylene.
[0056] According to the preparation method of the present invention, in the double decomposition reaction, the molar ratio of the compound represented by formula (α') and / or the compound represented by formula (β') to the lead salt is 0.6-1.6:0.3-0.8, preferably 0.8-1.4:0.4-0.7, most preferably 0.9-1.1:0.45-0.55, preferably, the molar ratio between the compound represented by formula (α') and the compound represented by formula (β') is 0.5-6:1, preferably 0.8-3:1, most preferably 1.5-2.5:1. In the reaction of the compound represented by formula (α') and / or the compound represented by formula (β') with the lead salt, the compound represented by formula (α') and / or the compound represented by formula (β') and the lead salt can be added once or multiple times, for example, can be added in 1 to 5 times, preferably 1 to 3 times, most preferably 2 to 3 times.
[0057] According to the preparation method of the present invention, in the double decomposition reaction, the temperature for reacting the compound represented by formula (α') and / or the compound represented by formula (β') with the lead salt can be 40 to 300°C, preferably 60 to 200°C, and most preferably 100 to 150°C, and the reaction time can be 2 to 10 hours, preferably 3 to 8 hours, and most preferably 4 to 6 hours.
[0058] According to the preparation method of the present invention, for the double decomposition reaction, a filtering operation can be performed after the reaction of the compound represented by formula (α') and / or the compound represented by formula (β') with the lead salt is completed to remove the generated by-products and unreacted reactants. Before the filtering operation, a solvent may be added or not, preferably a solvent is added. The solvent is preferably a hydrocarbon solvent, for example, one or more of solvent gasoline, n-octane and xylene.
[0059] The preparation method of the invention is simple and efficient, and the reaction process does not require the purification of cyclohexane acid or water washing, and the discharge of three wastes is greatly reduced. The lead-containing anti-wear agent prepared according to the method of the invention has good compatibility with the base oil and has excellent anti-wear, friction-reducing and antioxidant properties.
[0060] In a third aspect, the present invention provides the use of the lead compound described in any of the above aspects.
[0061] The lead compound described in any of the above aspects can be used as a lubricant with excellent extreme pressure and anti-wear properties, and can be used for lubrication of gears and bearings in mechanical transmission parts on land, and can also be used as a lubricant for the operation of space machinery and equipment. In particular, when used as a space lubricant, it can solve the problem that the existing extreme pressure and anti-wear agents have poor solubility and low stability in space lubricants based on polyalkyl cyclopentane, and are difficult to meet the requirements of space lubricants.
[0062] In a fourth aspect, the present invention provides a lubricating oil composition.
[0063] The lubricating oil composition of the present invention comprises the lead compound and lubricating base oil as described in any of the above aspects. The lead compound preferably accounts for 0.1% to 15% of the total mass of the lubricating oil composition, preferably 0.3% to 10%. The lubricating base oil can be one or more of API I, II, III, IV and V lubricating base oils, preferably API V lubricating base oil.
[0064] According to the present invention, the API I, II, III class lubricating base oil preferably has a kinematic viscosity of 2 to 30 mm at 100°C. 2 / s lubricating base oil, for example, one or more of 100SN, 150SN, 200SN, 500SN, 650SN, 150BS lubricating oils processed by the old three sets of processes and 100N, 150N, 200N, 500N, 600N hydrorefined oils and lubricating oil bases prepared by high pressure hydrocracking process can be selected.
[0065] According to the present invention, the API IV class lubricating base oil preferably has a kinematic viscosity of 2 to 30 mm at 100°C. 2 / s polyalphaolefin lubricating oil, for example, one or more of PAO2, PAO4, PAO6, PAO8 and PAO10 can be selected.
[0066] According to the present invention, the API V lubricating base oil can be selected from polyalkyl cyclopentane and / or ester oil, preferably polyalkyl cyclopentane. The polyalkyl cyclopentane and / or ester oil can be prepared by conventional methods in the art or purchased commercially, and there is no particular limitation.
[0067] According to the present invention, the lead compound described in any of the above aspects has good solubility, compatibility, extreme pressure and anti-wear properties and retention performance in the polyalkyl cyclopentane, and does not cause problems such as stratification and precipitation.
[0068] The lubricating oil composition of the present invention has good lubricity, friction reduction, wear resistance and oxidation resistance, and can ensure the normal operation of ground and space machinery.
[0069] In a fifth aspect, the present invention provides a space lubricant composition.
[0070] The space lubricant composition of the present invention comprises the lead compound and polyalkyl cyclopentane as described in any one of the above aspects. The lead compound preferably accounts for 0.1% to 15% of the total mass of the space lubricant composition, preferably 0.3% to 10%.
[0071] The space lubricant composition of the present invention has excellent stability, does not produce stratification, additive precipitation and the like during long-term operation, has good lubricity, friction reduction, wear resistance and oxidation resistance, and can ensure the normal operation of space machinery. The lead compound therein has good solubility, extreme pressure and wear resistance in various base oils, especially in polyalkyl cyclopentane.
[0072] The present invention unexpectedly discovered that, compared with lead cyclopentaneate prepared by a conventional process, the lead compound of the present invention has a longer wear resistance retention time at the same dosage. This is related to the fact that the introduction of alkylphenylcarboxylic acid groups and cyclopentaneic acid groups improves the stability of the lead compound in the friction pair and reduces the rate at which lead soap decomposes to form inorganic lead salts, so that the lead compound of the present invention exerts an anti-wear and friction-reducing effect for a longer period of time, thereby being able to reduce the amount of the lead compound added to the formula. It is also unexpectedly discovered that, after the introduction of alkylphenylcarboxylic acid groups, the lead compound of the present invention has improved oxidation resistance. DETAILED DESCRIPTION
[0073] The present invention will be further described below by way of examples, but the present invention is not limited thereto.
[0074] Unless otherwise specified, the percentages mentioned below are all mass percentages.
[0075] Source of raw materials:
[0076] Cyclohexane A
[0077] Crude acid value: 88mgKOH / g, pure acid value: 120mgKOH / g, average relative molecular mass: 467, purity: 73.33%, density: 0.9710g / cm 3 , 100℃ kinematic viscosity: 94.6mm 2 / s, industrial products
[0078] Cyclohexane acid B
[0079] Crude acid value: 257.3mgKOH / g, pure acid value: 292.42mgKOH / g, average relative molecular mass: 192, purity: 88%, density: 0.950g / cm 3 , Industrial products
[0080] Cyclohexane acid C
[0081] Crude acid value: 220.8mgKOH / g, pure acid value: 253.8mgKOH / g, average relative molecular mass: 221, purity: 87%, density: 0.949g / cm 3 , Industrial products
[0082] Tetradecylbenzoic acid, the preparation method thereof is as follows:
[0083] 1) Preparation of Tetradecylacetophenone
[0084] In a 1000 ml three-necked flask with temperature control and stirring, add 350 ml CCl4, 50 g anhydrous AlCl3 and 50 g acetyl chloride (0.637 mol), add 174 g (0.634 mol) of tetradecylbenzene dropwise, control the dropping speed so that the material temperature is between 0 and 5 ° C. After the addition is completed, react at 20 to 25 ° C for 1 hour, then separate the organic layer from the reaction mixture, wash with acid and water until neutral, dry with anhydrous sodium sulfate, filter, and evaporate the solvent to obtain tetradecylacetophenone.
[0085] 2) Oxidation of tetradecyl acetophenone to alkyl benzoic acid
[0086] At room temperature, add 200 ml of chloroform, 120 ml of NaOCl and 20 g of NaOH mixed solution into a 1000 ml three-necked flask. Add 31.65 g (0.1 mol) of p-tetradecylacetophenone dropwise. After the addition is complete, heat and reflux for 1.5 hours. Distill off the solvent under reduced pressure, wash with water, and filter to obtain 32.5 g of tetradecylbenzoic acid with an acid value of 167.04 mgKOH / g and a purity of 95%.
[0087] Hexadecylbenzoic acid
[0088] 1) Preparation of hexadecyl acetophenone
[0089] In a 1000 ml three-necked flask with temperature control and stirring, add 350 ml CCl4, 50 g anhydrous AlCl3 and 50 g acetyl chloride (0.637 mol), add 191.8 g (0.634 mol) of hexadecylbenzene dropwise, control the dropping speed so that the material temperature is between 0 and 5 °C, after the addition is completed, react at 20 to 25 °C for 1 hour, then separate the organic layer from the reaction mixture, wash with acid and water until neutral, dry with anhydrous sodium sulfate, filter, and evaporate the solvent to obtain hexadecylacetophenone.
[0090] 2) Hexadecylacetophenone is oxidized to p-alkylbenzoic acid
[0091] At room temperature, add 200 ml of chloroform, 120 ml of NaOCl and 20 g of NaOH mixed solution into a 1000 ml three-necked flask. Add 34 g (0.1 mol) of p-hexadecylacetophenone dropwise. After the addition is complete, heat and reflux for 1.5 hours. Distill off the solvent under reduced pressure, wash with water, and filter to obtain 35.5 g of hexadecylbenzoic acid with an acid value of 151.9 mgKOH / g and a purity of 94%.
[0092] Lead oxide, propanol, and ethylene glycol were purchased from Beijing Chemical Reagent Company and were of analytical grade.
[0093] No. 120 solvent gasoline:
[0094] Distillation range is 80℃~120℃, industrial product
[0095] 150SN lubricating base oil:
[0096] The kinematic viscosity at 40°C is 30.21 mm 2 / s, kinematic viscosity at 100℃ is 5.62mm 2 / s, pour point, -12℃, PetroChina Dalian Petrochemical Company
[0097] No. 6 Hydrogenated Oil:
[0098] The kinematic viscosity at 40°C is 31.85 mm 2 / s, kinematic viscosity at 100℃ is 6.23mm 2 / s, Sinopec Shanghai Gaoqiao Petrochemical Company
[0099] PAO6
[0100] The kinematic viscosity at 40°C is 29 mm 2 / s, kinematic viscosity at 100℃ is 5.7mm 2 / s, Preparation Example 1 of Industrial Polyalkyl Cyclopentane
[0101] This preparation example is used to illustrate the preparation method of polyalkylcyclopentane used in the following examples.
[0102] After the n-decyl alcohol, solid potassium hydroxide and dicyclopentadiene are mixed, they are added into a flask equipped with a stirrer, a separatory funnel, a condenser, a water separator and a thermometer for heating reaction. The reaction temperature is 220-250° C. When no more water is generated in the water separator, the reaction is stopped. The reaction product is washed with water, dried and filtered to obtain poly-n-decylcyclopentadiene. Poly-n-decylcyclopentadiene is prepared into a solution with a dilution of 10% with n-heptane. 200 g of this solution is mixed with 3.6 g of amorphous nickel catalyst and then put into a high-pressure reactor. Hydrogen is introduced until the hydrogen pressure reaches 5 MPa. The mixture is heated to 155° C. under stirring and reacted for 20 hours. The reaction product is cooled and filtered to remove the solvent to obtain poly-n-decylcyclopentane.
[0103] Example 1
[0104] In a 1000 ml three-necked flask with temperature control, water cooling and stirring, 127.5 g (0.27 mol) of cyclohexane acid A and 63.6 g (0.2 mol) of tetradecylbenzoic acid (total acid value is 167 mgKOH / g, mass fraction is 95%, average relative molecular mass is 318) were first added, and the materials were stirred. When the material temperature rose to 115°C, 35.7 g (0.16 mol) of lead oxide and 1.7 g of propanol were slowly added within 30 minutes. After 2 hours of constant temperature reaction, 100 g (0.21 mol) of cyclohexane acid A was added, and 35.7 g (0.16 mol) of lead oxide was slowly added within 30 minutes, and then reacted for 4 hours. When there were no solid particles of lead oxide in the material and the material was transparent, the temperature was lowered, 200 g of No. 120 solvent gasoline was added at 60°C, and the material was diluted and filtered. The filtrate was distilled to obtain 348 g of viscous dark brown extreme pressure anti-wear agent A (theoretical product amount is 357 g), with a yield of 97.5%. The mass fraction of Pb in the product is 18.5%.
[0105] Example 2
[0106] In a 1000 ml three-necked flask with temperature control, water cooling and stirring, 76.8 g (0.4 mol) of cyclohexane acid B and 95.4 g (0.3 mol) of tetradecylbenzoic acid (total acid value is 167 mgKOH / g, mass fraction is 95%, average relative molecular mass is 318) were first added, and the materials were stirred. When the material temperature rose to 120°C, 61.4 g (0.275 mol) of lead oxide and 1.8 g of ethylene glycol were slowly added within 40 minutes. After 3 hours of constant temperature reaction, 76.8 g (0.4 mol) of cyclohexane acid B was added, and 62.5 g (0.28 mol) of lead oxide was slowly added within 30 minutes, and then reacted for 3 hours. When there were no solid particles of lead oxide in the material and the material was transparent, the temperature was lowered, 300 g of No. 120 solvent gasoline was added at 60°C, and the material was diluted and filtered. The filtrate was distilled to obtain 353 g of viscous dark brown extreme pressure anti-wear agent B (theoretical product amount is 363 g), with a yield of 97.2%. The mass fraction of Pb in the product is 29.3%.
[0107] Example 3
[0108] In a 1000 ml three-necked flask with temperature control, water cooling and stirring, 88 g (0.4 mol) of cyclohexane acid C and 127.2 g (0.4 mol) of tetradecylbenzoic acid (total acid value is 167 mgKOH / g, mass fraction is 95%, average relative molecular mass is 318) were first added, and the materials were stirred. When the material temperature rose to 120°C, 93.66 g (0.42 mol) of lead oxide and 3.4 g of propanol were slowly added within 30 minutes. After 4 hours of constant temperature reaction, 44 g (0.2 mol) of cyclohexane acid C was added, and 23.4 g (0.1 mol) of lead oxide was slowly added within 30 minutes, and then reacted for 2 hours. When there were no solid particles of lead oxide in the material and the material was transparent, the temperature was lowered, 200 g of No. 120 solvent gasoline was added at 60°C, and the material was diluted and filtered. The filtrate was distilled to obtain 350.2 g of viscous dark brown extreme pressure anti-wear agent C (theoretical product amount is 366.9 g), and the yield was 95.5%. The mass fraction of Pb in the product is 29.8%.
[0109] Example 4
[0110] In a 1000 ml three-necked flask with temperature control, water cooling and stirring, 127.5 g (0.27 mol) of cyclohexane acid A and 69.2 g (0.2 mol) of hexadecylbenzoic acid (total acid value is 151.9 mgKOH / g, mass fraction is 94%, average relative molecular mass is 346) were first added, and the materials were stirred. When the material temperature rose to 121°C, 35.7 g (0.160 mol) of lead oxide and 1.7 g of propanol were slowly added within 35 minutes. After 3 hours of constant temperature reaction, 100 g (0.21 mol) of cyclohexane acid A was added, and 35.7 g (0.160 mol) of lead oxide was slowly added within 30 minutes, and then reacted for 3 hours. When there were no solid particles of lead oxide in the material and the material was transparent, the temperature was lowered, 180 g of No. 120 solvent gasoline was added at 60°C, and the material was diluted and filtered. The filtrate was distilled to obtain 351 g of viscous dark brown extreme pressure anti-wear agent D (theoretical product amount is 362.3 g), and the yield was 96.9%. The mass fraction of Pb in the product is 17.9%.
[0111] Comparative Example 1
[0112] First, add 219.5 g (0.47 mol) of cyclopentane acid A to a 1000 ml three-necked flask with temperature control, water cooling and stirring, stir the material, and when the material temperature rises to 115°C, slowly add 35.7 g (0.16 mol) of lead oxide and 1.7 g of propanol within 30 minutes. After constant temperature reaction for 2 hours, then add 100 g (0.21 mol) of cyclopentane acid A, slowly add 35.7 g (0.16 mol) of lead oxide within 30 minutes, and then react for 4 hours. When there are no solid particles of lead oxide in the material and the material is transparent, cool it down, add 200 g of No. 120 solvent gasoline at 60°C, filter after dilution, and distill the filtrate to obtain 365.9 g (theoretical product amount is 385.1 g) of viscous dark brown extreme pressure anti-wear agent A-1, with a yield of 95%. The mass fraction of Pb in the product is 17.3%.
[0113] Comparative Example 2
[0114] First, add 134.4 g (0.7 mol) of cyclopentane acid B to a 1000 ml three-necked flask with temperature control, water cooling and stirring, stir the material, and when the material temperature rises to 120°C, slowly add 61.4 g (0.275 mol) of lead oxide and 1.8 g of ethylene glycol within 40 minutes. After constant temperature reaction for 3 hours, add 76.8 g (0.4 mol) of cyclopentane acid B, slowly add 62.5 g (0.28 mol) of lead oxide within 30 minutes, and then react for 3 hours. When there are no solid particles of lead oxide in the material and the material is transparent, cool it down, add 300 g of No. 120 solvent gasoline at 60°C, filter after dilution, and distill the filtrate to obtain 316.6 g (theoretical product amount is 325.1 g) of viscous dark brown extreme pressure anti-wear agent B-1, with a yield of 97.3%. The mass fraction of Pb in the product is 34.8%.
[0115] Comparative Example 3
[0116] In a 1000 ml three-necked flask with temperature control, water cooling and stirring, add the refined acid of cyclohexane acid C for distillation (cyclohexane acid C is distilled under reduced pressure, the vacuum degree is 3torr, and the refined acid with a distillation temperature of 130℃~145℃ is obtained), then add a 10% sodium hydroxide solution by mass for saponification reaction (the molar ratio of cyclohexane acid to sodium hydroxide is 1:1), the saponification temperature is 85℃, the saponification time is 1h, and then add toluene to fully dissolve it, stir, add a 15% lead acetate solution by mass under toluene reflux conditions (the molar ratio of cyclohexane acid to lead acetate is 1:0.5), and react for 2h to generate lead cyclohexane acid. After the reaction is completed, the aqueous phase is discarded, the organic phase is washed 4 times with 80℃ hot water, and after dehydration, it is distilled under reduced pressure to obtain 262 grams of extreme pressure anti-wear agent C-1, and the mass fraction of Pb in the product is 26.9%.
[0117] Performance Evaluation of Lead Compounds
[0118] The lead compounds of Examples 1 to 4 and Comparative Examples 1 to 3 were dissolved in 150SN, No. 6 hydrogenated oil, PAO4, and polyalkyl cyclopentane base oil at a dosage of 8% to examine the solubility of the antiwear agent in the base oil. The results are shown in Table 1.
[0119] The above base oils were selected respectively, and lead compounds were modulated into lubricating oil compositions with a lead content of 0.1%. The wear spot diameter values and PDSC oxidation induction periods of these lubricating oil compositions after 1 hour and 2 hours of testing were examined. The results are shown in Tables 2, 3 and 4.
[0120] The anti-wear test method is the lubricating oil anti-wear performance determination method (four-ball method) SH / T0189.
[0121] The antioxidant activity was determined by the PDSC test, which was performed on a TA 5000DSC 2910 thermal analyzer under the following conditions: a heating rate of 100°C / min, a constant temperature of 60 min, and a pressure of 3.5 MPa.
[0122] As can be seen from Table 1, the lead compound of the present invention exhibits excellent oil solubility in petroleum-based and polyalkyl cyclopentane base oils, wherein the turbidity in 150SN base oil at -15°C is due to the high pour point of the base oil itself and has nothing to do with the lead compound of the present invention.
[0123] It can be seen from Tables 2 and 3 that the lead compound of the present invention has better wear resistance, especially under longer wear time, the wear spot diameter is significantly smaller than that of the comparative example, indicating that the anti-wear duration of the lead compound of the present invention is longer.
[0124] It can be seen from Table 4 that the lead compound of the present invention has better antioxidant performance.
[0125] Table 1 Solubility test of antiwear agents in different base oils
[0126]
[0127] Table 2 1-hour wear test results of different lubricating oil compositions (unit: mm)
[0128]
[0129] Table 3 2-hour wear test results of different lubricating oil compositions (unit: mm)
[0130]
[0131] Table 4 PDSC oxidation induction period test results of different lubricating oil compositions (unit: min)
[0132] additive 150SN No. 6 Hydrogenated Oil PAO4 Polyalkyl cyclopentane Example 1 17.2 16.2 18.9 17.4 Example 2 17.6 16.1 18.3 16.9 Example 3 17.8 15.9 17.5 17.1 Example 4 18.2 16.3 17.2 16.9 Comparative Example 1 9.8 8.6 10.3 9.7 Comparative Example 2 8.7 7.4 9.8 9.5 Comparative Example 3 6.9 7.6 10.3 10.6
Claims
1. A method for preparing a lead compound, comprising the step of reacting a mixture of cyclohexane acid and a compound represented by formula (β) with lead oxide; In formula (β), R 2 The group is C 8~24 The straight chain or branched alkyl group; the lead oxide is selected from linalool and / or yellow lead; the molar ratio of the mixture of cycloalkane acid and the compound represented by formula (β) to the lead oxide is 0.6-1.6:0.3-0.
8.
2. The preparation method according to claim 1, It is characterized in that The temperature for the reaction of the mixture of the cycloalkane acid and the compound represented by the formula (β) with lead oxide is 40 to 300°C.
3. The preparation method according to claim 1, It is characterized in that A promoter is added to the reaction between the mixture of the cyclohexane acid and the compound represented by the formula (β) and lead oxide.
4. The lead compound prepared by the method according to any one of claims 1 to 3 is used as an extreme pressure antiwear agent.
5. A lubricating oil composition comprising a lead compound prepared according to the method of any one of claims 1 to 3 and a lubricating base oil.
6. A space lubricant composition comprising a lead compound prepared according to the method of any one of claims 1 to 3 and a polyalkyl cyclopentane.