A method for continuous extraction and purification of sorbic acid hydrolyzate

Through the continuous extraction and purification method of sorbic acid hydrolysate and organic solvent, problems such as cumbersome operation, low yield and low purity in the existing process are solved, and efficient sorbic acid purification is achieved, improving the yield and quality of the product.

CN114478238BActive Publication Date: 2024-11-19NANTONG ACETIC ACID CHEM
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111639206.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-29
Publication Date
2024-11-19
Estimated Expiration
2041-12-29

AI Technical Summary

Technical Problem

The existing sorbic acid hydrolysis and purification process has problems such as many operating steps, low product yield and low purity.

Method used

The continuous extraction and purification method of sorbic acid hydrolysate and organic solvent is adopted. Through the separation, evaporation and crystallization steps of layered tower, the cooling and centrifugation process are reduced, and the yield and quality of sorbic acid are improved.

Benefits of technology

It reduces the loss of sorbic acid, improves product yield and purity, reduces equipment investment, and avoids activated carbon decolorization and refining, achieving efficient sorbic acid purification.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114478238B_ABST
    Figure CN114478238B_ABST
Patent Text Reader

Abstract

The invention discloses a method for continuous extraction and purification of sorbic acid hydrolyzate, and belongs to the field of chemical industry. The hydrochloric acid hydrolyzate obtained by hydrolyzing polyester with hydrochloric acid and an organic solvent are pumped into a dissolving kettle in proportion for continuous dissolution; the dissolved material is then pumped into a layering tower for separation, the upper layer is an organic layer containing sorbic acid, the organic layer material obtained in the upper layer is washed with residual hydrochloric acid by a water washing tower at 80-85°C, a solvent layer is obtained at the top of the tower, and the solvent layer is then pumped into a first evaporator at a certain flow rate for evaporation separation, and the kettle liquid of the first evaporator is then pumped into a second evaporator, and the tower top material of the second evaporator is cooled and crystallized to obtain a sorbic acid semi-finished product; the organic solvent is an organic solvent with a boiling point of 130-260°C. The SA content in the washed sorbic acid semi-finished product is 90-99.5%, and the solvent content is ≤1%, which reduces the cooling, centrifugation, and washing processes, and reduces equipment investment.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for continuous extraction and purification of sorbic acid hydrolyzate, belonging to the field of chemical industry. Background Art

[0002] Sorbic acid, scientific name 2,4-hexadienoic acid, English name: Sorbic Acid, white needle-shaped or powdery crystals, slightly soluble in water, soluble in a variety of organic solvents, structural formula is Sorbic acid is an unsaturated fatty acid with conjugated dienes. It can effectively inhibit the activity of molds, yeasts and aerobic bacteria. Its inhibitory effect on the development and reproduction of harmful microorganisms is stronger than its bactericidal effect. It is a preservative recommended by the Food and Agriculture Organization of the United Nations to countries around the world. Its safety is twice that of salt. Sorbic acid has been widely used in the preservation and preservation of various foods, vegetables, fruits, medicines, rubber, papermaking, animal feed, cosmetics, paints, tobacco, beverages and other industries.

[0003] The hydrolysis of polyester is the fundamental process for producing sorbic acid. At present, most industries use hydrochloric acid to hydrolyze polyester to prepare sorbic acid. Polyester hydrolysis produces a total of 4 types of 2,4-hexadienoic acid, only the trans-trans isomer is the effective ingredient sorbic acid, and the other isomers account for 20% of the total product content. These isomers have a lower melting point than sorbic acid and are oily; they are easily oxidized by oxygen, and are prone to gelation and discoloration. The presence of isomers affects the sorbic acid content and reduces the reaction yield. Therefore, only when the polyester is completely hydrolyzed can a high yield of sorbic acid be obtained. The prior art discloses a method for producing and purifying sorbic acid, wherein distilled polyester and 33% hydrochloric acid by mass are added to a hydrolysis kettle, the mixture is stirred at 65-70°C for 1h, then heated to 80-85°C and stirred for 1.5h, filtered, washed with water and centrifuged to obtain crude sorbic acid, and the crude sorbic acid is washed with alcohol before entering the refining process. This production process is an intermittent production process with a long reaction time and complicated operation. Alcohol washing will dissolve a large amount of sorbic acid, resulting in product loss. Moreover, the alcohol washing effect is general, resulting in a decrease in the purity of the sorbic acid product and a deterioration in color. Activated carbon decolorization and refining are required, generating a large amount of solid waste. Summary of the invention

[0004] [Technical issues]

[0005] The existing sorbic acid hydrolysis and purification process has the problems of multiple operation steps, low product yield and low purity.

[0006] [Technical solution]

[0007] In order to solve the above problems, the present invention provides a method for continuous extraction and purification of sorbic acid hydrolyzate, wherein the present invention performs continuous layering after mixing the uncooled hydrochloric acid hydrolyzate with a solvent after the reaction, washes the solvent layer on the upper layer and then performs evaporation separation, and then cools, crystallizes and filters to obtain SA semi-finished products. Compared with the traditional process, the method of the present invention reduces the process of cooling and centrifugation, and improves economic benefits. The sorbic acid product is separated by evaporation and crystallization, while reducing the loss of sorbic acid, thereby improving the yield and quality of the sorbic acid product.

[0008] The present invention provides a method for continuous extraction and purification of sorbic acid hydrolyzate, the method comprising the following steps:

[0009] First, hydrochloric acid hydrolyzate obtained by hydrolyzing polyester with hydrochloric acid and an organic solvent are pumped into a dissolving kettle in a certain ratio for continuous dissolution; then the dissolved materials are pumped into a layering tower for separation, the upper layer is an organic layer containing sorbic acid, and the lower layer is an acid layer, the organic layer material obtained from the upper layer is passed through a water washing tower at 80-85° C. to remove residual hydrochloric acid, a solvent layer is obtained at the top of the tower, and a water layer is obtained at the bottom of the tower, the water layer is treated as waste water or for other purposes, and then the solvent layer is pumped into a first evaporator at a certain flow rate for evaporation and separation, and then the kettle liquid of the first evaporator is pumped into a second evaporator, and the tower top material of the second evaporator is cooled and crystallized to obtain a sorbic acid semi-finished product;

[0010] Wherein, the organic solvent is an organic solvent with a boiling point of 130 to 250°C.

[0011] In one embodiment of the present invention, the method is a continuous production method.

[0012] In one embodiment of the present invention, the solid content of the hydrochloric acid hydrolyzate is 20-30 wt%.

[0013] In one embodiment of the present invention, the hydrochloric acid hydrolyzate is preferably an uncooled hydrochloric acid hydrolyzate obtained by hydrolyzing polyester with hydrochloric acid.

[0014] In one embodiment of the present invention, the mass ratio of the hydrolyzate to the organic solvent is 1:1 to 2.5.

[0015] In one embodiment of the present invention, the organic solvent is a substance that can produce an azeotrope with sorbic acid; preferably, the organic solvent includes one or more organic solvents such as esters, cyclic esters, aromatic hydrocarbons, ethers, alkanes, heterocycles, and unsaturated carboxylic acids.

[0016] In one embodiment of the present invention, the ester organic solvent is a product obtained by dehydration of an organic carboxylic acid and an alcohol, preferably including but not limited to methyl anthranilate, ethyl hexanoate or ethyl 2-dimethylbutyrate.

[0017] In one embodiment of the present invention, the cyclic ester organic solvent includes but is not limited to δ-valerolactone or mevalonolactone.

[0018] In one embodiment of the present invention, the ether organic solvent includes but is not limited to anisole, butyl ether or diphenyl ether.

[0019] In one embodiment of the present invention, the alkane organic solvent includes but is not limited to undecane or dodecane.

[0020] In one embodiment of the present invention, the heterocyclic organic solvent includes but is not limited to pyrrole or indole.

[0021] In one embodiment of the present invention, the unsaturated carboxylic acid organic solvent includes but is not limited to crotonic acid or butynedioic acid.

[0022] In one embodiment of the present invention, the dissolution temperature is 70-90° C., and the residence time is 5 min-1 h.

[0023] In one embodiment of the present invention, the content of sorbic acid in the organic layer containing sorbic acid is 8 to 30 wt %.

[0024] In one embodiment of the present invention, the HCl content in the solvent layer is 0.1-0.5 wt %.

[0025] In one embodiment of the present invention, the system pressure of the first evaporator is -0.09 to -0.05 MPa, and the residence time is 0.1 to 2 hours.

[0026] In one embodiment of the present invention, the system pressure of the second evaporator is -0.1 to -0.08 MPa, and the residence time is 0.5 to 3 hours.

[0027] In one embodiment of the present invention, the kettle liquid of the second evaporator is tar, which can be processed after being discharged.

[0028] In one embodiment of the present invention, the operating parameters of the cooling crystallization are that the distilled solution is reduced from 60-100°C to 5-20°C at a rate of 5-20°C / h.

[0029] In one embodiment of the present invention, the sorbic acid content in the obtained sorbic acid semi-finished product is 90-99.5%, and the solvent content is ≤1%.

[0030] In one embodiment of the present invention, the method further comprises refining the semi-finished sorbic acid product.

[0031] In one embodiment of the present invention, the method specifically comprises the following steps: first, the uncooled hydrochloric acid hydrolyzate and the solvent are continuously injected into a dissolution kettle in a certain proportion for continuous dissolution, wherein the solid content of the hydrolyzate is 20-30%, the mass ratio of the hydrolyzate to the solvent is 1:1-2.5, the residence time of the dissolution is 5min-1h, and the dissolution temperature is 70-90°C; the dissolved material is injected into a layering tower for continuous separation, the upper layer is a solvent layer with a SA content of 8-30%, and the lower layer is an acid layer, and the organic layer material separated from the upper layer is passed through a water washing tower at 80-85°C to remove the residual Hydrochloric acid, a solvent layer is continuously discharged from the top of the tower, and a water layer is continuously discharged from the bottom of the tower. The HCl content in the solvent layer after water washing is 0.1%-0.5%, and the water layer is treated as waste water; the washed solvent layer is then continuously pumped into the first evaporator at a certain flow rate for evaporation separation, low-boiling substances are continuously discharged from the top of the first evaporator, the kettle liquid of the first evaporator is continuously pumped into the second evaporator, tar is continuously discharged from the kettle of the second evaporator, and the material continuously evaporated from the top of the second evaporator is then pumped into a crystallizer for cooling and crystallization. The SA content of the washed sorbic acid semi-finished product is 90-99.5%, and the solvent content is ≤1%. The semi-finished product enters the refining process.

[0032] The invention also provides application of the method in the field of antiseptic or fresh-keeping.

[0033] Compared with the prior art, the present invention has the following advantages and effects:

[0034] 1) The present invention directly adds an organic solvent to the hydrolyzed material to dissolve sorbic acid. Compared with the process of dissolving crude sorbic acid, the cooling, centrifugation and washing processes are reduced, and the equipment investment is reduced.

[0035] 2) This process can separate sorbic acid from the solvent by continuous distillation, and high-boiling impurities are discharged in the kettle residue. The sorbic acid content in the kettle residue is low, which greatly reduces the loss of sorbic acid. The yield of sorbic acid obtained in the purification process is 99%-99.9%;

[0036] 3) Distillation is performed in a two-stage continuous manner, with chlorine-containing low-boiling substances being continuously separated in the first stage and tar being continuously separated in the second stage. The two-stage continuous distillation process ensures the quality of the semi-finished product;

[0037] 4) Compared with the industrial production process, this process does not require activated carbon decolorization, and the concentration of the refined SA solution is stable, which is easy for continuous production. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] Figure 1 A schematic process flow diagram of a method for continuous extraction and purification of sorbic acid hydrolyzate of the present invention. DETAILED DESCRIPTION

[0039] The present invention provides a method for continuous extraction and purification of sorbic acid hydrolyzate, the method comprising the following steps:

[0040] First, the uncooled hydrochloric acid hydrolyzate and the solvent are continuously pumped into a dissolving kettle in a certain proportion for continuous dissolution, wherein the solid content of the hydrolyzate is 20-30%, the mass ratio of the hydrolyzate to the solvent is 1:1-2.5, the residence time of the dissolution is 5min-1h, and the dissolution temperature is 70-90°C; the dissolved material is pumped into a layering tower for continuous separation, the upper layer is a solvent layer with an SA content of 8-30%, and the lower layer is an acid layer, the organic layer material separated from the upper layer is passed through a water washing tower at 80-85°C to remove residual hydrochloric acid, and the solvent layer is continuously discharged from the top of the tower, The water layer is continuously discharged from the bottom of the tower, and the HCl content in the solvent layer after water washing is 0.1% to 0.5%, and the water layer is treated as wastewater; the washed solvent layer is then continuously pumped into the first evaporator at a certain flow rate for evaporation separation, the low boiling point is continuously discharged from the top of the first evaporator, the first evaporator kettle liquid is continuously pumped into the second evaporator, tar is continuously discharged from the second evaporator kettle, and the material continuously evaporated from the top of the second evaporator is then pumped into the crystallizer for cooling and crystallization, and the SA content of the washed sorbic acid semi-finished product is 90-99.5%, the solvent content is ≤1%, and the semi-finished product enters the refining process. The present invention is further described below in conjunction with the examples, but the embodiments of the present invention are not limited thereto.

[0041] Example 1

[0042] First, the uncooled hydrochloric acid hydrolyzate and δ-valerolactone are continuously pumped into a dissolving kettle in a certain ratio for continuous dissolution, wherein the solid content of the hydrolyzate is 20%, the mass ratio of the hydrolyzate to the solvent δ-valerolactone is 1:2.5, the residence time of the dissolution is 5 minutes, and the dissolution temperature is 70°C; the dissolved material is pumped into a layering tower for continuous separation, the upper layer is a solvent layer with an SA content of 8%, the lower layer is an acid layer, the organic layer material separated from the upper layer is passed through an 80°C water washing tower to remove residual hydrochloric acid, the solvent layer is continuously discharged from the top of the tower, and the water layer is continuously discharged from the bottom of the tower. The HCl content in the solvent layer after water washing is 0.1%, and the water layer is treated as waste water; then the washed solvent layer is continuously pumped into a first evaporator 1 at a certain flow rate for evaporation separation, the system pressure of the first evaporator 1 is -0.06MPa, the residence time is 1h, low boiling is continuously discharged from the top of the tower, and the kettle liquid is continuously pumped into a second evaporator 2, the system pressure of the second evaporator 2 is -0.09MPa, and the residence time is 1.5h. Tar is continuously discharged from the bottom of the tower, and the material continuously evaporated from the top of the tower is then pumped into a crystallizer for cooling and crystallization (reduced to 10°C at a rate of 10°C / h). The SA content of the washed sorbic acid semi-finished product is 94.5%, and the solvent content is ≤1%. The semi-finished product then enters the refining process.

[0043] The yield of sorbic acid was 99.2%.

[0044] Example 2

[0045] First, the uncooled hydrochloric acid hydrolyzate and dodecane are continuously pumped into a dissolving kettle in a certain ratio for continuous dissolution, wherein the solid content of the hydrolyzate is 24%, the mass ratio of the hydrolyzate to the solvent dodecane is 1:1.5, the residence time of the dissolution is 20 minutes, and the dissolution temperature is 80°C; the dissolved material is pumped into a layering tower for continuous separation, the upper layer is a solvent layer with a 24% SA content, the lower layer is an acid layer, the organic layer material separated from the upper layer is passed through an 82°C water washing tower to remove residual hydrochloric acid, the solvent layer is continuously discharged from the top of the tower, and the water layer is continuously discharged from the bottom of the tower. After washing, the HCl content in the solvent layer is 0.2%, and the water layer is treated as waste water; then the washed solvent layer is continuously pumped into the first evaporator 1 at a certain flow rate for evaporation separation, the system pressure of the first evaporator 1 is -0.09MPa, the residence time is 1h, the low boiling point is continuously discharged from the top of the tower, and the kettle liquid is continuously pumped into the second evaporator 2, the system pressure of the second evaporator 2 is -0.1MPa, and the residence time is 1h. Tar is continuously discharged from the bottom of the tower, and the material continuously evaporated from the top of the tower is then pumped into a crystallizer for cooling and crystallization (the evaporated solution is reduced to 10°C at a rate of 6°C / h). The SA content of the washed sorbic acid semi-finished product is 90.5%, and the solvent content is ≤1%. The semi-finished product then enters the refining process.

[0046] The yield of sorbic acid was 99.0%.

[0047] Example 3

[0048] First, the uncooled hydrochloric acid hydrolyzate and crotonic acid are continuously pumped into a dissolving kettle in a certain proportion for continuous dissolution, wherein the solid content of the hydrolyzate is 30%, the mass ratio of the hydrolyzate to the solvent crotonic acid is 1:1, the residence time of the dissolution is 1h, and the dissolution temperature is 90°C; the dissolved material is pumped into a layering tower for continuous separation, the upper layer is a solvent layer with a 30% SA content, the lower layer is an acid layer, the organic layer material separated from the upper layer is passed through an 85°C water washing tower to remove residual hydrochloric acid, the solvent layer is continuously discharged from the top of the tower, and the water layer is continuously discharged from the bottom of the tower. The HCl content in the solvent layer after water washing is 0.5%, and the water layer is treated as waste water; then the washed solvent layer is continuously pumped into the first evaporator 1 at a certain flow rate for evaporation separation, the system pressure of the first evaporator 1 is -0.05MPa, the residence time is 2h, the low boiling point is continuously discharged from the top of the tower, and the kettle liquid is continuously pumped into the second evaporator 2, the system pressure of the second evaporator 2 is -0.08MPa, and the residence time is 3h. Tar is continuously discharged from the bottom of the tower, and the material continuously evaporated from the top of the tower is then pumped into a crystallizer for cooling and crystallization (the evaporated solution is reduced to 10°C at a rate of 15°C / h). The SA content of the washed sorbic acid semi-finished product is 99.5%, and the solvent content is ≤1%. The semi-finished product then enters the refining process.

[0049] The yield of sorbic acid was 99.9%.

[0050] Example 4

[0051] First, the uncooled hydrochloric acid hydrolyzate and diphenyl ether are continuously pumped into a dissolving kettle in a certain proportion for continuous dissolution, wherein the solid content of the hydrolyzate is 24%, the mass ratio of the hydrolyzate to the solvent diphenyl ether is 1:1, the residence time of the dissolution is 20 minutes, and the dissolution temperature is 80°C; the dissolved material is pumped into a layering tower for continuous separation, the upper layer is a solvent layer with a 24% SA content, the lower layer is an acid layer, the organic layer material separated from the upper layer is passed through an 80°C water washing tower to remove residual hydrochloric acid, the solvent layer is continuously discharged from the top of the tower, and the water layer is continuously discharged from the bottom of the tower. The HCl content in the solvent layer after water washing is 0.2%, and the water layer is treated as waste water; then the washed solvent layer is continuously pumped into the first evaporator 1 at a certain flow rate for evaporation separation, the system pressure of the first evaporator 1 is -0.05MPa, the residence time is 2h, the low boiling point is continuously discharged from the top of the tower, and the kettle liquid is continuously pumped into the second evaporator 2, the system pressure of the second evaporator 2 is -0.1MPa, and the residence time is 0.5h. Tar is continuously discharged from the bottom of the tower, and the material continuously evaporated from the top of the tower is then pumped into a crystallizer for cooling and crystallization (the evaporated solution is reduced to 10°C at a rate of 5°C / h). The SA content of the washed sorbic acid semi-finished product is 96%, and the solvent content is ≤1%. The semi-finished product then enters the refining process.

[0052] The yield of sorbic acid was 99.5%.

[0053] Example 5

[0054] When the organic solvent in Example 4 was replaced by pyrrole, other parameters and steps were consistent with Example 4, the SA content of the obtained sorbic acid semi-finished product was 94.5%, the solvent content was ≤1%, and the temperature of the distilled solution was reduced to 10° C. at a rate of 5° C. / h. The yield of sorbic acid was 99.3%.

[0055] Example 6

[0056] First, the uncooled hydrochloric acid hydrolyzate and diphenyl ether solvent are continuously pumped into a dissolving kettle in a certain proportion for continuous dissolution, wherein the solid content of the hydrolyzate is 30%, the mass ratio of the hydrolyzate to the solvent diphenyl ether is 1:2.5, the residence time of the dissolution is 1h, and the dissolution temperature is 90°C; the dissolved material is pumped into a layering tower for continuous separation, the upper layer is a solvent layer with an SA content of 8%, the lower layer is an acid layer, the organic layer material separated from the upper layer is passed through an 80°C water washing tower to remove residual hydrochloric acid, the solvent layer is continuously discharged from the top of the tower, and the water layer is continuously discharged from the bottom of the tower. After washing, the HCl content in the solvent layer is 0.2%, and the water layer is treated as waste water; then the washed solvent layer is continuously pumped into the first evaporator 1 at a certain flow rate for evaporation separation, the system pressure of the first evaporator 1 is -0.05MPa, the residence time is 2h, the low boiling point is continuously discharged from the top of the tower, and the kettle liquid is continuously pumped into the second evaporator 2, the system pressure of the second evaporator 2 is -0.1MPa, and the residence time is 0.5h. Tar is continuously discharged from the tower bottom, and the material continuously distilled from the top of the tower is then pumped into the crystallizer for cooling and crystallization. The distilled solution is cooled to 10°C at a rate of 5°C / h. The SA content of the washed sorbic acid semi-finished product is 96.2%, and the solvent content is ≤1%. The semi-finished product enters the refining process.

[0057] The yield of sorbic acid was 99.6%.

[0058] When other organic solvents such as esters, cyclic esters, aromatic hydrocarbons, ethers, alkanes, heterocycles, unsaturated carboxylic acids defined in the present invention are used, the other operating parameters are consistent with the above embodiment, and a sorbic acid semi-finished product with a sorbic acid content of 90-99.5% and a solvent content of ≤1% can be obtained, with a yield of not less than 99%, and the sorbic acid product can be prepared after subsequent refining.

[0059] Comparative Example 1

[0060] When the organic solvent in Example 4 was replaced with ethanol or acetone, it was found that it could not form an azeotrope with sorbic acid, and the purification process could not be achieved. Sorbic acid still remained in the kettle, and the distilled liquid was difficult to collect.

[0061] Comparative Example 2

[0062] First, the uncooled hydrochloric acid hydrolyzate and diphenyl ether are continuously pumped into a dissolving kettle in a certain proportion for continuous dissolution, wherein the solid content of the hydrolyzate is 24%, the mass ratio of the hydrolyzate to the solvent diphenyl ether is 1:1, the residence time of the dissolution is 20 minutes, and the dissolution temperature is 80°C; the dissolved material is pumped into a layering tower for continuous separation, the upper layer is a solvent layer with a 24% SA content, the lower layer is an acid layer, the organic layer material separated from the upper layer is passed through a washing tower hydrochloric acid at 80°C, the solvent layer is continuously discharged from the top of the tower, and the water layer is continuously discharged from the bottom of the tower. After washing, the HCl content in the solvent layer is 0.2%, and the water layer is treated as waste water; then the washed solvent layer is continuously pumped into the first evaporator 1 at a certain flow rate for evaporation separation, the system pressure of the first evaporator 1 is -0.04MPa, the residence time is 2h, the low boiling point is continuously discharged from the top of the tower, and the kettle liquid is continuously pumped into the second evaporator 2, the system pressure of the second evaporator 2 is -0.07MPa, and the residence time is 0.5h. Tar is continuously discharged from the bottom of the tower, and the material continuously distilled from the top of the tower is then pumped into the crystallizer for cooling and crystallization. The distilled solution is cooled from 60°C to 10°C at a rate of 5°C / h. The SA content of the washed sorbic acid semi-finished product is 98%, and the solvent content is ≤1%. The semi-finished product enters the refining process.

[0063] The yield of sorbic acid was 80%.

[0064] Although the present invention has been disclosed as above in the form of a preferred embodiment, it is not intended to limit the present invention. Anyone familiar with this technology can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention should be based on the definition of the claims.

Claims

1. A method for continuous extraction and purification of sorbic acid hydrolyzate, characterized in that: The method steps are as follows: First, hydrochloric acid hydrolyzate obtained by hydrolyzing polyester with hydrochloric acid and an organic solvent are pumped into a dissolving kettle in a certain ratio for continuous dissolution; then the dissolved materials are pumped into a layering tower for separation, the upper layer is an organic layer containing sorbic acid, and the lower layer is an acid layer, the organic layer material obtained from the upper layer is passed through a water washing tower at 80-85° C. to remove residual hydrochloric acid, a solvent layer is obtained at the top of the tower, and a water layer is obtained at the bottom of the tower, the water layer is treated as waste water or for other purposes, and then the solvent layer is pumped into a first evaporator at a certain flow rate for evaporation and separation, and then the kettle liquid of the first evaporator is pumped into a second evaporator, and the tower top material of the second evaporator is cooled and crystallized to obtain a sorbic acid semi-finished product; The solid content of the hydrochloric acid hydrolyzate is 20-30 wt %; the mass ratio of the hydrolyzate to the organic solvent is 1:1-2.5; The organic solvent is δ-valerolactone, diphenyl ether, dodecane or crotonic acid; The system pressure of the first evaporator is -0.09~-0.05 MPa, and the residence time is 0.1~2h; the system pressure of the second evaporator is -0.1~-0.08 MPa, and the residence time is 0.5~3h.

2. The method for continuous extraction and purification of sorbic acid hydrolyzate according to claim 1, characterized in that: The dissolving temperature is 70-90° C., and the residence time is 5 min-1 h.

3. The method for continuous extraction and purification of sorbic acid hydrolyzate according to claim 1, characterized in that: The operating parameters of the cooling crystallization are that the distilled solution is cooled from 60-100° C. to 5-20° C. at a rate of 5-20° C. / h.

4. The method for continuous extraction and purification of sorbic acid hydrolyzate according to claim 1, characterized in that: The method further comprises refining the semi-finished sorbic acid product.