A touch panel PCD routing design for FMLOC products

By designing PCD traces in the TMA layer of the OLED display panel and co-designing them as common traces with the backboard circuit layer, combining the overlapping traces and via connections of the TMA and TMB layers, the detection range in the prior art is solved. Limited problems enable comprehensive detection of Crack in the display area, improving detection efficiency and reliability.

CN114510901BActive Publication Date: 2024-11-12UNIV OF ELECTRONICS SCI & TECH OF CHINA
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202210061229.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-01-19
Publication Date
2024-11-12
Estimated Expiration
2042-01-19

AI Technical Summary

Technical Problem

When detecting cracks of OLED display panels, the existing PCD trace design has a limited detection range and cannot effectively detect Cracks in the display area, especially the Crack problems of FMLOC layer after bent or folded.

Method used

Design a touch panel PCD trace, use the TMA layer to route the display panel Panel-display AA area, and design it as a common PCD trace with the backboard circuit layer, and pass through the overlapping trace and through the TMA and TMB layers. Connect holes to reduce resistance, expand the detection range by straight lines, polylines and/or curves to ensure comprehensive inspection of Crack.

Benefits of technology

The range and detection rate of Crack detection are greatly improved, and the Crack from the edge of the Panel panel to the AA area can be effectively detected, including the Crack in the bent area, ensuring product reliability and quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114510901B_ABST
    Figure CN114510901B_ABST
Patent Text Reader

Abstract

The present invention belongs to the technical field of organic light-emitting display, and specifically relates to a PCD routing design for a touch panel applied to FMLOC products. The present invention designs the PCD routing of the TMA layer to the periphery of the Panel and the AA area. The PCD routing of the TMA layer in the AA area is designed below the TMB design pattern, and the design pattern at the bridge key of the AA area is avoided by a straight line, a broken line and / or a curve; the routing through the TMA layer has no effect on the TMB routing design and touch performance, and the detection range is greatly increased. Trace routing uses TMA and TMB overlapping routing, and the TMA layer of the trace routing is designed to be hollowed out at the crossover point between the PCD and the trace routing, and other areas are connected to the TMB through vias to reduce the trace routing resistance. The PCD routing of the present invention increases the crack detection range from the outermost periphery of the panel to the edge of the panel to the AA area, greatly improving the crack detection rate, especially the PCD crack in the right-angle bend area.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of organic light emitting display, and in particular relates to a PCD wiring design of a touch panel applied to an FMLOC product. Background Art

[0002] Active matrix organic light emitting diode AMOLED display is a device used to display images and colors. It is widely used in mobile phones and computers. During the manufacturing process, the flexible OLED substrate will crack due to foreign objects or external forces. Especially during the bonding process (referring to the bonding of the panel and the protective cover glass) or after bending, the film layer is more likely to crack due to stress. Therefore, a panel crack defect detection PCD (Panel Crack Defection) routing will be designed outside the display area of ​​the display panel to perform crack inspections to ensure product yield. PCD uses BP (Back Panel) layer metal routing. Due to the limitations of the peripheral wiring layout (drawing design), there are other circuits close to the display area. Usually, a circle of PCD routing is designed at the outermost edge of the Panel (display panel), and the detection range is limited (such as Figure 1 shown).

[0003] The FMLOC product of flexible multi-layer film touch panel is based on the AMOLED display screen. Metal and inorganic film patterns are made on its packaging layer. It is easy to crack from the FMLOC layer after bending or external force. When crack occurs from the FMLOC layer, it will cause problems such as touch failure or packaging failure. The existing PCD routing is only designed on the outermost side of the BP metal layer. The crack caused by bending and stress mismatch between film layers in the FMLOC layer or the display AA area cannot be detected by the PCD routing of the BP in the existing solution because it does not extend to the PCD routing of the BP peripheral circuit.

[0004] FMLOC is to make the Touch layer after the OLED backplane, evaporation and packaging processes are completed. The usual process of the Touch layer is: Packaging layer-Barrier layer (base layer)-TMA layer (Touch Metal A, touch layer A)-TLD layer (Touch Layer insulation layer)-TMB (Touch Metal B, touch layer B)-TOC (Touch Organic Layer touch organic protection layer); usually TMA (also called Metal1) forms a bridge key, and TMB layer (also called metal2) forms Tx (transmit or send touch signals) and Rx (receive touch signals) routing. The peripheral routing of the Touch panel is only the Trace routing, and the Trace routing is the routing in the non-display area, such as Figure 4As shown, in order to reduce resistance, metal1&metal2 are usually double-layered and connected through TLD vias.

[0005] The commonly used OLED backplane process flow is Buffer (substrate) - Poly (low temperature polysilicon) - GI (Gate Insulating gate insulation layer) - Gate1 (first gate) - Cst insulation layer (storage capacitor insulation layer) - Gate2 (second gate layer) - ILD (insulation layer through hole) - SD (source and drain source and drain metal layer) - PLN (planarization layer) - anode. The metal layer is Gate1 / Gate2 / SD, and the peripheral wiring units of the panel include Gate / EM GOA (backplane gate drive circuit), VSS (low level), vinit (initial level) and other units. PCD wiring usually uses Gate 2 layer metal wiring, such as Figure 1 As shown in the figure, Gate / EM GOA refers to the gate driver circuit on the backplane of the gate driver / emitter driver GOA (Gate Driver on array).

[0006] Products bent at large angles or folded products will bend the AA area. Since the crack in the bending area occurs in the FMLOC film layer, the PCD cannot detect it, resulting in reliability cracks. Figure 2 .

[0007] PCD inspection principle: Currently commonly used PCD routing designs are as follows: Figure 3 As shown, the PCD trace is divided into two loops on both sides of the panel. The two loops are connected to the resistance check IC (circuit board integrated circuit) through terminals. Usually the loop trace resistance is 40 kiloohms. If cracks appear, due to PCD trace breakage or micro-contact caused by fine cracks, the PCD resistance will rise to 100 kiloohms or infinity.

[0008] PCD is an effective means to solve the problem of cracks caused by foreign matter or external forces during the production of OLED, especially during the cutting and bonding process. However, because the current crack inspection lines are designed at the outermost periphery of the Panel BP layer, the crack detection range is small and can only detect cracks around the panel, and cracks in the display area cannot be detected. Summary of the invention

[0009] In view of the above problems or shortcomings, and to solve the problem of low efficiency of existing PCD in detecting device cracks, the present invention provides a touch panel PCD routing design applied to FMLOC products, so as to more comprehensively detect cracks in the display area of ​​FMLOC products.

[0010] A touch panel PCD routing design applied to FMLOC products.

[0011] The touch panel PCD routing is designed in the TMA layer in the AA area of ​​the display panel Panel-display. The TMA layer does not involve Trace routing, and the peripheral non-display area leads only leave the trace routing of the TMB layer; the PCD routing of the TMA layer in the AA area is designed below the TMB layer design pattern.

[0012] Furthermore, the touch panel PCD routing is designed together with the PCD routing of the backplane circuit layer as a common PCD routing for both FMLOC and the backplane circuit layer, so that cracks occurring in the BP / package / FMLOC film layer can be detected. That is, the backplane circuit layer and the touch panel use a common PCD routing to detect cracks.

[0013] Furthermore, the trace routing uses TMA layer and TMB layer to overlap the routing, the TMA layer of the trace routing is designed to be hollowed out at the intersection of PCD and trace routing, and other areas are connected to the TMB layer through vias to reduce the trace routing resistance. A non-base layer is sandwiched between TMA and TMB to separate the two metal layers. When the two metal layers need to be short-circuited, the two metal layers are connected together by digging holes to play a parallel connection to reduce resistance.

[0014] Furthermore, the PCD routing is a straight line, a folded line and / or a curve; the PCD routing in the AA area is arranged between pixels depending on the pixel arrangement in the AA area. The PCD routing starts at the edge of the display panel, that is, the outermost routing in the peripheral circuit, and extends to the display area. It is changed to a straight line, a folded line and / or a curve according to different pixel arrangements to expand the wiring area and improve the detection range.

[0015] The present invention designs the PCD routing of the TMA layer to the periphery of the panel and the AA area, and the PCD routing of the TMA layer in the AA area is designed below the TMB design pattern, and uses straight lines, broken lines and / or curves to avoid the design pattern of the AA area at the bridge key; routing through the TMA layer has no effect on the TMB routing design and touch performance, and greatly increases the detection range, such as Figure 6 As shown in Figure 1. Trace routing uses TMA and TMB overlapping routing, as shown in Figure 1. Figure 7 As shown, the TMA layer of the trace line is designed to be hollowed out at the point where the PCD and the trace line cross, and other areas are connected to the TMB through vias to reduce the trace line resistance.

[0016] In summary, compared with the prior art, the present invention increases the crack detection range from the outermost edge of the panel to the edge of the panel to the AA area by using the TMA layer of FMOLC to design PCD routing, which greatly improves the crack detection rate, especially PCD cracks in the right-angle bending area. It also provides a design idea of ​​using common PCD routing for FMLOC and backplane circuit layer, reuses PCD routing, and enables cracks occurring in BP / package / FMLOC film layer to be detected. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 This is a schematic diagram of the existing Panel peripheral wiring;

[0018] Figure 2 This is a schematic diagram of the crack leakage detection of the FMLOC film layer when the existing PCD routing reliability crack occurs;

[0019] Figure 3 This is a schematic diagram of the existing PCD routing;

[0020] Figure 4 Design a schematic diagram for the existing PCD;

[0021] Figure 5 The FMLOC jumper design of the present invention;

[0022] Figure 6 PCD routing case 1 of the present invention;

[0023] Figure 7 PCD routing case 2 of the present invention;

[0024] Figure 8 This is the FMLOC process flow chart;

[0025] Fig. 9 This is a schematic diagram of PCD routing. DETAILED DESCRIPTION

[0026] The present invention is further described in detail below with reference to the accompanying drawings and embodiments.

[0027] The common process flow of OLED backplane (LTPS as an example) is: Buffer buffer substrate layer → Poly low-temperature polysilicon → GIGate interlayer dielectric → Gate1 (gate) → Cst (storage capacitor) dielectric → Gate2 (forming Cst) → ILD (insulating layer) → SD → PLN (planar layer) → cathode cathode → PDL (Pixel defined layer) → PS (spacer unit formed by PhotoSpacer exposure). The panel peripheral wiring units include Gate / EM GOA, VSS, Vinit and other metal wirings. PCD wiring usually uses Gate 2 layer metal wiring, such as Figure 1 shown.

[0028] Figure 8 The process flow chart of FMLOC is as follows: Encapsulation layer CVD2 – Barrier layer (base layer) – TMA layer (Touch Metal A, touch layer A) – TLD layer (Touch Layer insulation layer) – TMB (Touch Metal B, touch layer B) – TOC (Touch Organic Layer touch organic protection layer). FMLOC makes the Touch layer after the OLED backplane, evaporation and encapsulation processes are completed. The usual process is TMA (forming bridge keys) insulation layer (forming capacitors) TMB (forming Tx, Rx routing). The peripheral routing of Touch is only Trace routing. Trace routing is as follows: Figure 3 As shown, in order to reduce resistance, double-layer routing is usually used for metal1 & metal2.

[0029] Currently, the commonly used OLED Panel peripheral routing units include Gate / EM GOA, VSS, Vinit and other metal routings. PCD routing usually uses Gate 2 layer metal routing, such as Figure 1 Commonly used PCD routing designs are as follows: Figure 2 As shown in the figure, the PCD wiring is divided into two loops on both sides of the panel, one end is connected to the Green Data line of the CT unit, and the other end is connected to the Data voltage of the CT or connected to the high level such as VGH of the FPC. During PCD detection, if a crack occurs on one side, a green bright line will be displayed on the black screen on the corresponding side; if there is no crack, the black screen is normal.

[0030] Embodiment 1:

[0031] 1) Use the TMA layer to design PCD routing in the Panel AA area, remove the TMA layer of the Trace routing, and only leave the TMB layer trace routing on the periphery. Because the TMA only has a graphic design pattern at the bridge key in the AA area, such as Figure 5The PCD routing of the TMA layer can be designed to the periphery of the panel and within the AA area. The PCD routing of the TMA layer in the AA area can be designed below the TMB graphic design pattern, which has no effect on the routing design and touch performance, greatly increasing the detection range. Figure 6 The PCD routing of the FMLOC layer is designed together with the PCD routing of the BP layer, so that cracks occurring in the BP / package / FMLOC film layer can be detected.

[0032] Embodiment 2:

[0033] In the AA area, the PCD detection routing is designed using the TMA layer, which is the same as in Example 1. The trace routing uses TMA and TMB overlapping routing, such as Figure 7 As shown, the TMA layer of the trace routing is designed to be hollowed out at the point where the PCD and the trace routing cross, and other areas are connected to the TMB through vias, which can also reduce the trace routing resistance.

[0034] Fig. 9 It shows that when the gap between the pixel arrangements is a straight line, the PCD routing is a straight line; when the gap between the pixel arrangements is a zigzag line, the PCD routing is a zigzag line, and the routing is performed according to different pixel architectures.

[0035] It can be seen from the above embodiments that the present invention designs PCD routing by utilizing the TMA layer of FMLOC. The layout range of this PCD routing is mainly in the AA area, avoiding the design pattern of the AA area at the bridge key; routing through the TMA layer has no effect on the TMB routing design and touch performance, greatly increasing the detection range. By using straight lines, broken lines and / or curves, the Crack detection range is increased from the outermost edge of the Panel to the edge of the Panel to the AA area, greatly increasing the routing range, thereby improving the Crack detection rate, especially PCD Crack inspection in right-angle bends or folded bends. Routing in the AA area is determined by the pixel arrangement in the AA area. The PCD routing on the left extends to 1 / 2 of the AA area at most, and the pattern is not limited to a straight line. The shape of the PCD routing can be changed according to the different pixel arrangements to increase the routing range.

Claims

1. A touch panel PCD routing design for FMLOC products. Features: The touch panel PCD routing is designed in the TMA layer in the AA area of ​​the display panel Panel-display. The TMA layer does not involve Trace routing, and the peripheral non-display area leads only leave the trace routing of the TMB layer; the PCD routing of the TMA layer in the AA area is designed below the TMB layer design pattern.

2. The touch panel PCD routing design applied to FMLOC products as claimed in claim 1, Features: The touch panel PCD routing is designed together with the PCD routing of the backplane circuit layer as a common PCD routing for both the FMLOC and the backplane circuit layer, so that cracks occurring in the BP / package / FMLOC film layer can be detected.

3. The PCD wiring design of the touch panel applied to the FMLOC product as claimed in claim 1, Features: The trace routing uses the TMA layer and the TMB layer to overlap the routing, the TMA layer of the trace routing is designed to be hollowed out at the crossing point between the PCD and the trace routing, and other areas are connected to the TMB layer through vias to reduce the trace routing resistance.

4. The touch panel PCD routing design applied to FMLOC products as claimed in claim 1, Features: The PCD routing line is a straight line, a broken line and / or a curved line. The PCD routing line in the AA area is arranged between pixels depending on the pixel arrangement in the AA area.

Citation Information

Patent Citations

  • Display panel, crack detection method thereof and display device

    CN111307867A

  • Display panel, crack detection method and preparation method thereof and display device

    CN112164711A

  • Display substrate and production method thereof, and display device

    CN113284935A

  • Display substrate and display device

    CN113552970A

  • Display panel and display device

    CN214505497U