FinFET devices and methods
By introducing an air gap in FinFET devices and sealing the air gap with a low dielectric constant material, the problem of increased capacitance between the gate stack and the contacts is solved, thereby improving the high-speed operation performance and reliability of the devices.
Patent Information
- Application Number
- CN202110307154.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2021-01-15
- Filing Date
- 2021-03-23
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2041-03-23
AI Technical Summary
As the minimum feature size of semiconductor devices decreases, problems arise such as increased capacitance between gate stacks and contacts in FinFET devices, leading to decreased high-speed operation performance.
Introducing an air gap in FinFET devices and sealing the upper region of the air gap with a low dielectric constant material reduces the possibility of conductive material entering the air gap, thereby reducing the capacitance between the gate stack and the contacts.
It improves the high-speed operation performance of FinFET, reduces the possibility of electrical short circuits and leakage, and enhances the overall performance of the device.
Smart Images

Figure CN114551400B_ABST
Abstract
Description
Technical Field
[0001] This disclosure generally relates to FinFET devices and methods. Background Technology
[0002] Semiconductor devices are used in a variety of electronic applications, such as personal computers, cell phones, digital cameras, and other electronic devices. Semiconductor devices are typically manufactured by sequentially depositing insulating or dielectric layers, conductive layers, and semiconductor layers of material on a semiconductor substrate, and using photolithography to pattern the individual material layers to form circuit components and elements thereon.
[0003] The semiconductor industry is continuously increasing the integration density of various electronic components (e.g., transistors, diodes, resistors, capacitors, etc.) by constantly reducing the minimum feature size, which allows more components to be integrated into a given area. However, as the minimum feature size decreases, other problems arise that need to be addressed. Summary of the Invention
[0004] According to one embodiment of this disclosure, a semiconductor device is provided, comprising: a fin extending from a semiconductor substrate; a gate stack over the fin; a spacer on a sidewall of the gate stack; a source / drain region adjacent to the spacer in the fin; an interlayer dielectric layer (ILD) extending over the gate stack, the spacer, and the source / drain region; a contact plug extending through the ILD and contacting the source / drain region; the dielectric layer including a first portion located on a top surface of the ILD and a second portion extending between the ILD and the contact plug, wherein the top surface of the second portion is closer to the substrate than the top surface of the ILD; and an air gap between the spacer and the contact plug, wherein the second portion of the dielectric layer seals the top of the air gap.
[0005] According to another embodiment of this disclosure, a method for forming a semiconductor device is provided, comprising: forming a fin protruding from a substrate; forming a gate structure over a channel region of the fin; forming a gate spacer along a sidewall of the gate structure; forming an epitaxial region in the fin adjacent to the channel region; depositing a first dielectric layer over the gate structure and the gate spacer, the first dielectric layer comprising a first dielectric material; forming a contact plug extending through the first dielectric layer and contacting the epitaxial region, wherein an air gap separates the contact plug and the gate spacer; depositing a second dielectric layer over the first dielectric layer and over the contact plug, including sealing a lower region of the air gap with the second dielectric layer, wherein the second dielectric layer comprises a second dielectric material different from the first dielectric material; etching the second dielectric layer to expose the contact plug, wherein after etching the second dielectric layer, the remaining portion of the second dielectric layer seals the lower region of the air gap; and depositing a conductive material on the contact plug, including depositing the conductive material between the contact plug and the first dielectric material and on the remaining portion of the second dielectric layer. According to another embodiment of this disclosure, a method for forming a semiconductor device is provided, comprising: forming a gate stack on a semiconductor fin; forming an epitaxial source / drain region in the semiconductor fin adjacent to the gate stack; depositing a first dielectric layer on the gate stack and on the epitaxial source / drain region; forming an opening in the first dielectric layer to expose the epitaxial source / drain region; depositing a sacrificial material in the opening; depositing a first conductive material on the sacrificial material in the opening; removing the sacrificial material to form a gap; depositing a second dielectric layer on the first dielectric layer, on the conductive material, and on the gap, wherein the second dielectric layer extends a first distance into the gap; and etching the second dielectric layer to expose the first conductive material, wherein a first portion of the second dielectric layer remains in the gap after the etching. Attached Figure Description
[0006] The various aspects of this disclosure can be best understood from the following detailed description taken in conjunction with the accompanying drawings. Note that, according to industry standard practice, the various features are not drawn to scale. In fact, for clarity of discussion, the dimensions of the various features may be arbitrarily increased or decreased.
[0007] Figure 1 An example of FinFET according to some embodiments is shown in a 3D view.
[0008] Figure 2 , Figure 3 , Figure 4, Figure 5 , Figure 6 , Figure 7 , Figure 8A , Figure 8B , Figure 9A , Figure 9B , Figure 10A , Figure 10B , Figure 10C , Figure 10D , Figure 11A , Figure 11B , Figure 12A , Figure 12B , Figure 13A , Figure 13B , Figure 14A , Figure 14B , Figure 14C , Figure 15A and Figure 15B This is a cross-sectional view of an intermediate stage in the fabrication of a FinFET according to some embodiments.
[0009] Figure 16 , Figure 17 , Figure 18 , Figure 19 , Figure 20 , Figure 21 , Figure 22 , Figure 23A , Figure 23B , Figure 24A , Figure 24B , Figure 25A , Figure 25B , Figure 26A , Figure 26B , Figure 27A , Figure 27B and Figure 28 This is a cross-sectional view of an intermediate stage in the fabrication of a FinFET with an air gap, according to some embodiments. Detailed Implementation
[0010] The following disclosure provides numerous different embodiments or examples for implementing various features of the invention. Specific examples of components and arrangements are described below to simplify this disclosure. Of course, these are merely examples and not intended to be limiting. For example, in the following description, forming a first feature above or on a second feature may include embodiments in which the first and second features are formed in direct contact, and may also include embodiments in which an additional feature may be formed between the first and second features such that the first and second features do not need to be in direct contact. Furthermore, reference numerals and / or letters may be repeated in various examples. This repetition is for simplicity and clarity and does not in itself indicate a relationship between the various embodiments and / or configurations discussed.
[0011] In addition, spatially related terms (e.g., "below," "below," "lower than," "above," "upper") may be used herein to readily describe the relationship of one element or feature shown in the figures relative to another element(s) or feature(s). These spatially related terms are intended to cover different orientations of the device in use or operation other than those shown in the figures. The device may be oriented in other ways (rotated 90 degrees or in other orientations), and the spatially related descriptors used herein shall be interpreted accordingly.
[0012] According to some embodiments, an air gap is formed around the contacts to the source / drain epitaxial regions of the FinFET device. The low dielectric constant (k value) of the air gap can reduce the capacitance between the gate stack and the contacts of the FinFET device, which can improve the high-speed (e.g., "AC") operation of the FinFET. In some embodiments, the deposition process of the etch stop layer above is controlled such that a portion of the etch stop layer extends into the air gap and seals the upper region of the air gap. For example, using a lower precursor dose during the ALD process allows the material of the etch stop layer to grow in the upper region of the air gap and seal the lower region of the air gap. In some embodiments, the distance by which the etch stop layer extends into the air gap can be controlled by controlling this dose. By sealing the air gap, the possibility of subsequently deposited conductive material entering the air gap is reduced or eliminated. Therefore, the possibility of leakage or electrical short circuit due to the presence of conductive material in the air gap is reduced or eliminated.
[0013] Figure 1 An example of a FinFET according to some embodiments is shown in a three-dimensional view. The FinFET includes a fin 52 on a substrate 50 (e.g., a semiconductor substrate). Isolation regions 56 are disposed in the substrate 50, and the fin 52 protrudes above these isolation regions from between adjacent isolation regions 56. Although the isolation regions 56 are described / shown as separate from the substrate 50, as used herein, the term "substrate" may be used to refer to a semiconductor substrate alone or a semiconductor substrate including the isolation regions. Furthermore, although the fin 52 is shown as a single continuous material like the substrate 50, the fin 52 and / or the substrate 50 may comprise a single material or a combination of materials. In this context, fin 52 refers to the portion extending between adjacent isolation regions 56.
[0014] A gate dielectric layer 92 runs along the sidewall of fin 52 and is located above the top surface of fin 52, and a gate electrode 94 is located above the gate dielectric layer 92. Source / drain regions 82 are disposed on the opposite side of fin 52 relative to the gate dielectric layer 92 and the gate electrode 94. Figure 1Further illustrations show reference cross sections used in the following figures. Cross section AA is along the longitudinal axis of the gate electrode 94 and in a direction perpendicular to, for example, the direction of current flow between the source / drain regions 82 of the FinFET. Cross section BB is perpendicular to cross section AA and along the longitudinal axis of the fin 52 in the direction of current flow between, for example, the source / drain regions 82 of the FinFET. Cross section CC is parallel to cross section AA and extends through the source / drain regions of the FinFET. For clarity, subsequent figures refer to these reference cross sections.
[0015] Some embodiments discussed herein are described in the context of FinFETs formed using a gate-last process. In other embodiments, a gate-first process may be used. Furthermore, some embodiments contemplate aspects used in planar devices (e.g., planar FETs).
[0016] Figures 2 to 28 This includes cross-sectional views of intermediate stages in the fabrication of a FinFET according to some embodiments. Figures 2 to 7 It shows Figure 1 The reference cross-section AA shown is different in that it has multiple fins / FinFETs. Figure 8A , Figure 9A , Figure 10A , Figure 11A , Figure 12A , Figure 13A , Figure 14A , Figure 15A , Figure 24A , Figure 25A , Figure 26A and Figure 27A Along Figure 1 The reference cross section AA is shown, and Figure 8B , Figure 9B , Figure 10B , Figure 11B , Figure 12B , Figure 13B , Figure 14B , Figure 14C , Figure 15B , Figure 16 , Figure 17 , Figure 18 , Figure 19 , Figure 20 , Figure 21 , Figure 22 , Figure 23A , Figure 23B , Figure 24B , Figure 25B , Figure 26B , Figure 27B and Figure 28 Along Figure 1The similar cross-section BB shown is illustrated, but the difference lies in the multiple fins / FinFETs. Figure 10C and Figure 10D Along Figure 1 The reference cross-section CC shown is different in that it has multiple fins / FinFETs.
[0017] exist Figure 2 In this embodiment, a substrate 50 is provided. The substrate 50 may be a semiconductor substrate, such as a bulk semiconductor, a semiconductor-on-insulator (SOI) substrate, etc., which may be doped (e.g., doped with p-type or n-type dopants) or undoped. The substrate 50 may be a wafer, such as a silicon wafer. Typically, an SOI substrate is a layer of semiconductor material formed on an insulating layer. For example, the insulating layer may be a buried oxide (BOX) layer, a silicon oxide layer, etc. The insulating layer is disposed on a substrate (typically a silicon substrate or a glass substrate). Other substrates may also be used, such as multilayer substrates or gradient substrates. In some embodiments, the semiconductor material of the substrate 50 may include: silicon; germanium; compound semiconductors, including silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, and / or indium antimonide; alloy semiconductors, including silicon germanium, gallium arsenide phosphide, aluminum indium arsenide, aluminum gallium arsenide, gallium indium arsenide, gallium indium phosphide, and / or gallium arsenide phosphide; or combinations thereof.
[0018] Substrate 50 has region 50N and region 50P. Region 50N can be used to form an n-type device, such as an NMOS transistor (e.g., an n-type FinFET). Region 50P can be used to form a p-type device, such as a PMOS transistor (e.g., a p-type FinFET). Region 50N can be physically separated from region 50P (as shown by separator 51), and any number of device features (e.g., other active devices, doped regions, isolation structures, etc.) can be formed between region 50N and region 50P.
[0019] exist Figure 3 In this embodiment, fins 52 are formed in the substrate 50. Fins 52 are semiconductor strips. In some embodiments, fins 52 can be formed in the substrate 50 by etching trenches in the substrate 50. The etching can be any acceptable etching process, such as reactive ion etching (RIE), neutral beam etching (NBE), or a combination thereof. The etching can be anisotropic.
[0020] The fins can be patterned using any suitable method. For example, one or more photolithography processes, including dual-patterning or multi-patterning processes, can be used to pattern the fins. Typically, dual-patterning or multi-patterning processes combine photolithography and self-alignment processes, allowing the creation of patterns with, for example, smaller pitches than that achievable using a single direct photolithography process. For example, in one embodiment, a sacrificial layer is formed on a substrate and patterned using a photolithography process. Spacers are formed alongside the patterned sacrificial layer using a self-alignment process. The sacrificial layer is then removed, and the remaining spacers can then be used to pattern the fins. In some embodiments, a mask (or other layer) may be retained on the fin 52.
[0021] exist Figure 4 An insulating material 54 is formed on the substrate 50 and between adjacent fins 52. The insulating material 54 can be an oxide (e.g., silicon oxide), a nitride, or a combination thereof, and can be formed by high-density plasma chemical vapor deposition (HDP-CVD), flowable CVD (FCVD) (e.g., CVD-based material deposition and post-curing in a remote plasma system to convert it into another material (e.g., oxide)), or a combination thereof. Other insulating materials formed by any acceptable process can be used. In the illustrated embodiment, the insulating material 54 is silicon oxide formed by an FCVD process. Once the insulating material is formed, an annealing process can be performed. In the embodiment, the insulating material 54 is formed such that an excess of the insulating material 54 covers the fins 52. Although the insulating material 54 is shown as a single layer, some embodiments may utilize multiple layers. For example, in some embodiments, a liner (not shown) can be formed first along the surfaces of the substrate 50 and the fins 52. A filler material, such as the filler material described above, can then be formed on the liner.
[0022] exist Figure 5 In this process, a removal process is applied to the insulating material 54 to remove excess insulating material 54 over the fin 52. In some embodiments, a planarization process such as chemical mechanical polishing (CMP), etch-back, or a combination thereof may be used. This planarization process exposes the fin 52 such that, after the planarization process is completed, the top surfaces of the fin 52 and the insulating material 54 are flush. In embodiments where a mask remains on the fin 52, the planarization process may expose or remove the mask such that, after the planarization process is completed, the mask or the top surfaces of the fin 52 and the insulating material 54 are flush, respectively.
[0023] exist Figure 6In this process, insulating material 54 is recessed to form shallow trench isolation (STI) regions 56. The insulating material 54 is recessed such that the upper portions of fins 52 in regions 50N and 50P protrude between adjacent STI regions 56. Furthermore, the top surface of the STI region 56 can have a flat surface (as shown), a convex surface, a concave surface (e.g., dish-shaped), or a combination thereof. The top surface of the STI region 56 can be formed as flat, convex, and / or concave by appropriate etching. Acceptable etching processes can be used to recess the STI regions 56, such as etching processes selectively targeting the material of the insulating material 54 (e.g., etching the material of the insulating material 54 at a faster rate than the material of the fins 52). For example, an oxide employing, for example, dilute hydrofluoric acid (dHF) can be used for removal.
[0024] about Figures 2 to 6 The described process is merely one example of how fin 52 can be formed. In some embodiments, the fin can be formed by an epitaxial growth process. For example, a dielectric layer can be formed over the top surface of the substrate 50, and trenches can be etched through the dielectric layer to expose the underlying substrate 50. Homoethelic structures can be epitaxially grown in the trenches, and the dielectric layer can be recessed such that the homoethelic structure protrudes from the dielectric layer to form the fin. Furthermore, in some embodiments, heteroethelic structures can be used for fin 52. For example, Figure 5 The fin 52 can be recessed, and a different material can be epitaxially grown on the recessed fin 52. In such an embodiment, the fin 52 comprises a recessed material and an epitaxial growth material disposed on the recessed material. In another embodiment, a dielectric layer can be formed on the top surface of the substrate 50, and trenches can be etched through the dielectric layer. A heteroepitaxial structure can then be epitaxially grown in the trench using a material different from that of the substrate 50, and the dielectric layer can be recessed such that the heteroepitaxial structure protrudes from the dielectric layer to form the fin 52. In some embodiments in which homoepitaxial or heteroepitaxial structures are epitaxially grown, the epitaxially grown material can be in-situ doped during growth, which avoids prior and subsequent implantation, but in-situ doping and implantation doping can be used together.
[0025] Furthermore, it may be advantageous to epitaxially grow a material different from that in region 50P (e.g., the PMOS region) in region 50N (e.g., the NMOS region). In various embodiments, the upper portion of fin 52 may be made of silicon-germanium (Si). x Ge 1-x(where x can be in the range of 0 to 1), silicon carbide, pure or substantially pure germanium, III-V compound semiconductors, II-VI compound semiconductors, etc. For example, materials that can be used to form III-V compound semiconductors include, but are not limited to: indium arsenide, aluminum arsenide, gallium arsenide, indium phosphide, gallium nitride, indium gallium arsenide, indium aluminum arsenide, gallium antimonide, aluminum antimonide, aluminum phosphide, gallium phosphide, etc.
[0026] Further in Figure 6 In this process, suitable wells (not shown) may be formed in fin 52 and / or substrate 50. In some embodiments, a P-well may be formed in region 50N and an N-well may be formed in region 50P. In some embodiments, either a P-well or an N-well may be formed in both region 50N and region 50P.
[0027] In embodiments with different well types, photoresist or other masks (not shown) can be used to implement different implantation steps for regions 50N and 50P. For example, photoresist can be formed over fin 52 and STI region 56 in region 50N. The photoresist is patterned to expose region 50P of substrate 50, such as a PMOS region. The photoresist can be formed using spin coating techniques, and the photoresist can be patterned using acceptable photolithography techniques. Once the photoresist is patterned, n-type impurity implantation is performed in region 50P, and the photoresist can be used as a mask to substantially prevent n-type impurities from being implanted into region 50N, such as an NMOS region. The n-type impurity can be phosphorus, arsenic, antimony, etc., implanted into the region, with a concentration equal to or less than 10. 18 cm -3 For example, in about 10 16 cm -3 With about 10 18 cm -3 Between. After implantation, the photoresist is removed, for example, through an acceptable ashing process.
[0028] Following implantation in region 50P, a photoresist is formed over fin 52 and STI region 56 in region 50P. The photoresist is patterned to expose region 50N of substrate 50, such as an NMOS region. The photoresist can be formed using spin coating and can be patterned using acceptable photolithography techniques. Once the photoresist is patterned, p-type impurity implantation can be performed in region 50N, and the photoresist can be used as a mask to substantially prevent p-type impurities from being implanted into region 50P, such as a PMOS region. The p-type impurity can be boron, boron fluoride, indium, etc., implanted into the region, with a concentration equal to or less than 10. 18 cm -3 For example, in about 1016 cm -3 Peace Treaty 10 18 cm -3 Between. After injection, the photoresist can be removed, for example, by an acceptable ashing process.
[0029] Following implantation in regions 50N and 50P, annealing can be performed to repair implantation damage and activate the implanted p-type and / or n-type impurities. In some embodiments, the growth material of the epitaxial fins can be in-situ doped during growth, which can avoid implantation, but in-situ doping and implantation doping can be used together.
[0030] exist Figure 7 In this process, a dummy dielectric layer 60 is formed on fin 52. For example, the dummy dielectric layer 60 can be silicon oxide, silicon nitride, a combination thereof, etc., and can be deposited or thermally grown according to acceptable techniques. A dummy gate layer 62 is formed on the dummy dielectric layer 60, and a mask layer 64 is formed on the dummy gate layer 62. The dummy gate layer 62 can be deposited on the dummy dielectric layer 60 and then planarized, for example, by CMP. The mask layer 64 can be deposited on the dummy gate layer 62. The dummy gate layer 62 can be a conductive or non-conductive material and can be selected from the group consisting of amorphous silicon, polysilicon, poly-SiGe, metal nitrides, metal silicides, metal oxides, and metals. The dummy gate layer 62 can be deposited by physical vapor deposition (PVD), CVD, sputtering deposition, or other techniques known in the art for depositing the selected material. The dummy gate layer 62 can be made of other materials that have high etch selectivity relative to the etching of the isolation region. For example, mask layer 64 may include silicon nitride, silicon oxynitride, etc. In this example, a single dummy gate layer 62 and a single mask layer 64 are formed across regions 50N and 50P. Note that, for illustrative purposes only, dummy dielectric layer 60 is shown to cover only fin 52. In some embodiments, dummy dielectric layer 60 may be deposited such that dummy dielectric layer 60 covers STI region 56, extending between dummy gate layer 62 and STI region 56.
[0031] Figures 8A to 15B Various additional steps for manufacturing the devices of the embodiments are shown. Figures 8A to 15B Features in either region 50N or region 50P are shown. For example, Figures 8A to 15B The structure shown can be applied to both Region 50N and Region 50P. Differences in the structure between Region 50N and Region 50P (if any) are described in the text of each figure.
[0032] exist Figure 8A and Figure 8BIn this process, acceptable photolithography and etching techniques can be used to pattern the mask layer 64 (see...). Figure 7 A mask 74 is formed. The pattern of the mask 74 can then be transferred to the dummy gate layer 62. In some embodiments (not shown), the pattern of the mask 74 can also be transferred to the dummy dielectric layer 60 by an acceptable etching technique to form the dummy gate 72. The dummy gate 72 covers the corresponding channel region 58 of the fin 52. The pattern of the mask 74 can be used to separate each dummy gate 72 from the adjacent dummy gate entity. The dummy gate 72 may also have a length direction substantially perpendicular to the length direction of the corresponding epitaxial fin 52.
[0033] Further in Figure 8A and Figure 8B In this process, a gate sealing spacer 80 can be formed on the exposed surfaces of the dummy gate 72, mask 74, and / or fin 52. The gate sealing spacer 80 can be formed by thermal oxidation or deposition followed by anisotropic etching. The gate sealing spacer 80 can be formed from silicon oxide, silicon nitride, silicon oxynitride, etc.
[0034] After the gate sealing spacer 80 is formed, implantation for the lightly doped source / drain (LDD) region (not explicitly shown) can be performed. Similar to the above, this process may be performed in embodiments with different device types. Figure 6 The implantation discussed earlier can involve forming a mask (e.g., photoresist) over region 50N while exposing region 50P, and implanting an impurity of an appropriate type (e.g., p-type) into the exposed fins 52 in region 50P. The mask can then be removed. The n-type impurity can be any of the previously discussed n-type impurities, and the p-type impurity can be any of the previously discussed p-type impurities. The lightly doped source / drain regions can have a doping density of approximately 10. 15 cm -3 To about 10 19 cm -3 The concentration of impurities. Annealing can be used to repair injection damage and reactivate the injected impurities.
[0035] exist Figure 9A and Figure 9B In this process, a gate spacer 86 is formed on a gate sealing spacer 80 along the sidewalls of the dummy gate 72 and the mask 74. The gate spacer 86 can be formed by conformally depositing an insulating material and then anisotropically etching the insulating material. The insulating material of the gate spacer 86 can be silicon oxide, silicon nitride, silicon oxynitride, silicon carbonitride, or combinations thereof.
[0036] Note that the above disclosure generally describes a process for forming spacers and LDD regions. Other processes and sequences can be used. For example, fewer or additional spacers can be used, different step sequences can be used, such as not etching the gate sealing spacer 80 before forming the gate spacer 86 to create an "L-shaped" gate sealing spacer, forming and removing spacers, etc. Furthermore, different structures and steps can be used to form n-type and p-type devices. For example, the LDD region of an n-type device can be formed before forming the gate sealing spacer 80, while the LDD region of a p-type device can be formed after forming the gate sealing spacer 80.
[0037] exist Figure 10A and Figure 10B In some embodiments, epitaxial source / drain regions 82 are formed in fin 52. In some cases, the epitaxial source / drain regions 82 may be formed to apply strain in the corresponding channel regions 58, thereby improving performance. The epitaxial source / drain regions 82 are formed in fin 52 such that each dummy gate 72 is disposed between corresponding adjacent pairs of epitaxial source / drain regions 82. In some embodiments, the epitaxial source / drain regions 82 may extend into fin 52 and may also extend through fin 52. In some embodiments, gate spacers 86 are used to separate the epitaxial source / drain regions 82 from the dummy gates 72 by an appropriate lateral distance such that the epitaxial source / drain regions 82 do not short-circuit the subsequently formed gate of the resulting FinFET.
[0038] The epitaxial source / drain region 82 in region 50N (e.g., an NMOS region) can be formed by masking region 50P (e.g., a PMOS region) and etching the source / drain region of fin 52 in region 50N to form a groove in fin 52. The epitaxial source / drain region 82 in region 50N is then epitaxially grown in the groove. The epitaxial source / drain region 82 can comprise any acceptable material, such as a material suitable for an n-type FinFET. For example, if fin 52 is silicon, the epitaxial source / drain region 82 in region 50N can comprise a material to which tensile strain is applied in channel region 58, such as silicon, silicon carbide, phosphorus-doped silicon carbide, silicon-phosphorus, etc. The epitaxial source / drain region 82 in region 50N can have a surface protruding from the corresponding surface of fin 52 and can have a facet.
[0039] The epitaxial source / drain region 82 in region 50P (e.g., a PMOS region) can be formed by masking region 50N (e.g., an NMOS region) and etching the source / drain region of fin 52 in region 50P to form a groove in fin 52. The epitaxial source / drain region 82 in region 50P is then epitaxially grown in the groove. The epitaxial source / drain region 82 can include any acceptable material, such as a material suitable for a p-type FinFET. For example, if fin 52 is silicon, the epitaxial source / drain region 82 in region 50P can include a material to which compressive strain is applied in channel region 58, such as silicon-germanium, boron-doped silicon-germanium, germanium, germanium-tin, etc. The epitaxial source / drain region 82 in region 50P can also have a surface protruding from the corresponding surface of fin 52 and can have a facet.
[0040] The epitaxial source / drain regions 82 and / or fins 52 can be formed by implanting dopant, similar to the previously discussed process for forming lightly doped source / drain regions, followed by annealing. The source / drain regions may have a density of approximately 10... 19 cm -3 Peace Treaty 10 21 cm -3 The impurity concentrations between these values. The n-type and / or p-type impurities used for the source / drain regions can be any of the impurities discussed above. In some embodiments, the epitaxial source / drain regions 82 can be doped in situ during growth.
[0041] As a result of the epitaxial process used to form the epitaxial source / drain regions 82 in regions 50N and 50P, the upper surface of the epitaxial source / drain regions has small facets that extend laterally outward beyond the sidewalls of the fin 52. In some embodiments, these small facets cause adjacent source / drain regions 82 of the same FinFET to merge, such as... Figure 10C As shown. In other embodiments, adjacent source / drain regions 82 remain separated after the epitaxial process is completed, as... Figure 10D As shown. In Figure 10C and Figure 10D In the illustrated embodiment, the gate spacer 86 is formed to cover the portion of the sidewall of the fin 52 extending above the STI region 56, thereby preventing epitaxial growth. In some other embodiments, the spacer etching used to form the gate spacer 86 may be adjusted to remove spacer material, allowing the epitaxial growth region to extend to the surface of the STI region 56.
[0042] exist Figure 11A and Figure 11B In some embodiments, in Figure 10A and Figure 10BA first interlayer dielectric (ILD) 88 is deposited on the structure shown. The first ILD 88 can be formed of a dielectric material and can be deposited by any suitable method such as CVD, plasma-enhanced CVD (PECVD), or FCVD. The dielectric material may include phosphosilicate glass (PSG), borosilicate glass (BSG), boron-doped phosphosilicate glass (BPSG), undoped silicate glass (USG), etc. Other insulating materials formed by any acceptable process can be used. In some embodiments, a contact etch stop layer (CESL) 87 is disposed between the first ILD 88 and the epitaxial source / drain region 82, mask 74, and gate spacer 86. CESL 87 may include a dielectric material, such as silicon nitride, silicon oxide, silicon oxynitride, etc., and may have a different etch rate than the material of the first ILD 88 described above. In some embodiments, CESL 87 may be formed to have a thickness between about 2 nm and about 5 nm, for example, about 3 nm. In some cases, controlling the thickness of CESL 87 can control the dimensions (e.g., width or height) of the subsequently formed source / drain contacts 118 and / or the dimensions (e.g., width or height) of the air gap 120 (see [reference]). Figure 17-22 ).
[0043] exist Figure 12A and Figure 12B In this process, a planarization process (e.g., CMP) can be performed to make the top surface of the first ILD 88 flush with the top surface of the dummy gate 72 or the mask 74. This planarization process may also remove the mask 74 over the dummy gate 72, as well as portions of the gate sealing spacers 80 and 86 along the sidewalls of the mask 74. After this planarization process, the top surfaces of the dummy gate 72, the gate sealing spacers 80, the gate spacers 86, and the first ILD 88 are flush. Therefore, the top surface of the dummy gate 72 is exposed through the first ILD 88. In some embodiments, the mask 74 may be retained, in which case the planarization process makes the top surface of the first ILD 88 flush with the top surface of the mask 74.
[0044] exist Figure 13A and Figure 13BIn one or more etching steps, the dummy gate 72 and mask 74 (if present) are removed to form a recess 90. A portion of the dummy dielectric layer 60 within the recess 90 may also be removed. In some embodiments, only the dummy gate 72 is removed, and the dummy dielectric layer 60 remains and is exposed by the recess 90. In some embodiments, the dummy dielectric layer 60 is removed from the recess 90 in a first region of the die (e.g., a core logic region) and retained in the recess 90 in a second region of the die (e.g., an input / output region). In some embodiments, the dummy gate 72 is removed by an anisotropic dry etching process. For example, the etching process may include a dry etching process using one or more reactive gases that selectively etch the dummy gate 72 without etching the first ILD 88, gate spacer 86, or CESL 87. Each recess 90 exposes and / or overlays a channel region 58 on the corresponding fin 52. Each channel region 58 is disposed between adjacent pairs of epitaxial source / drain regions 82. During removal, the dummy dielectric layer 60 can be used as an etch stop layer when etching the dummy gate 72. The dummy dielectric layer 60 can then be optionally removed after the dummy gate 72 has been removed.
[0045] exist Figure 14A and Figure 14B In this process, a gate dielectric layer 92 and a gate electrode 94 are formed to replace the gate. Figure 14C It shows Figure 14B A detailed view of region 89. A gate dielectric layer 92 is conformally deposited in the recess 90, for example, on the top surface and sidewalls of fin 52 and on the sidewalls of gate sealing spacer 80 / gate spacer 86. The gate dielectric layer 92 may also be formed on the top surface of the first ILD 88. According to some embodiments, the gate dielectric layer 92 comprises silicon oxide, silicon nitride, or multiple layers thereof. In some embodiments, the gate dielectric layer 92 comprises a high-k dielectric material, and in these embodiments, the gate dielectric layer 92 may have a k value greater than about 7.0, and may comprise metal oxides or silicates of hafnium, aluminum, zirconium, lanthanum, manganese, barium, titanium, lead, and combinations thereof. Methods for forming the gate dielectric layer 92 may include molecular beam deposition (MBD), ALD, PECVD, etc. In embodiments in which a portion of the dummy dielectric layer 60 remains in the recess 90, the gate dielectric layer 92 comprises the material of the dummy dielectric layer 60 (e.g., silicon oxide).
[0046] Gate electrodes 94 are deposited on the gate dielectric layer 92 and fill the remaining portion of the trench 90. Gate electrodes 94 may comprise a metallic material, such as titanium nitride, titanium oxide, tantalum nitride, tantalum carbide, cobalt, ruthenium, aluminum, tungsten, combinations thereof, or multiples thereof. For example, although in Figure 14BA single-layer gate electrode 94 is shown, but the gate electrode 94 may include any number of liner layers 94A, any number of work function adjustment layers 94B, and filler material 94C, such as Figure 14C As shown. After filling the recess 90, a planarization process such as CMP can be performed to remove excess material from the gate electrode 94 and the gate dielectric layer 92 above the top surface of the first ILD 88. The remaining material from the gate electrode 94 and the gate dielectric layer 92 thus form the replacement gate of the resulting FinFET. The gate electrode 94 and the gate dielectric layer 92 can be collectively referred to as the “gate stack”. The gate and the gate stack can extend along the sidewalls of the channel region 58 of the fin 52.
[0047] The formation of the gate dielectric layer 92 in regions 50N and 50P can occur simultaneously, such that the gate dielectric layer 92 in each region is formed of the same material, and the formation of the gate electrode 94 can occur simultaneously, such that the gate electrode 94 in each region is formed of the same material. In some embodiments, the gate dielectric layer 92 in each region can be formed using different processes, such that the gate dielectric layer 92 can be made of different materials, and / or the gate electrode 94 in each region can be formed using different processes, such that the gate electrode 94 can be made of different materials. When using different processes, various masking steps can be used to mask and expose appropriate regions.
[0048] exist Figure 15A and Figure 15B In some embodiments, a second ILD 108 is deposited on top of the first ILD 88. In some embodiments, the second ILD 108 is a flowable film formed by a flowable CVD method. In some embodiments, the second ILD 108 is formed of a dielectric material such as PSG, BSG, BPSG, USG, silicon oxide, etc., and can be deposited by any suitable method such as CVD, PECVD, etc. A planarization process such as CMP can be performed to planarize the surface of the second ILD 108. In some embodiments, the second ILD 108 may be formed having a thickness T1 between about 10 nm and about 30 nm, but other thicknesses are possible.
[0049] According to some embodiments, a hard mask 96 is deposited on the structure prior to the deposition of the second ILD 108. The hard mask 96 may comprise one or more layers of dielectric material, such as silicon nitride, silicon oxynitride, etc., and may have a different etch rate than the material of the second ILD 108 above. In some embodiments, the hard mask 96 may be formed to have a thickness between about 2 nm and about 4 nm. In some embodiments, the hard mask 96 is formed of the same material as CESL 87, or is formed to have approximately the same thickness as CESL 87. The source / drain contacts 118 are subsequently formed (see...). Figure 20 () Through hard mask 96 and CESL 87 to contact the top surface of epitaxial source / drain region 82, and gate contact 132 (see Figure 27A It passes through the hard mask 96 to contact the top surface of the gate electrode 94.
[0050] Figures 16 to 22 A source / drain contact 118 having an air gap 120 is shown according to some embodiments (see [reference]). Figure 22 The intermediate step of the process. The source / drain contact 118 physically contacts and electrically contacts the epitaxial source / drain region 82. The source / drain contact 118 may also be referred to as "contact 118" or "contact plug 118". For clarity, Figures 16 to 22 Shown as Figure 15B Detailed view of area 111. Figure 16 It shows Figure 15B Region 111, which has the same structure as shown.
[0051] exist Figure 17In some embodiments, openings 110 are formed in the first ILD 88 and the second ILD 108 to expose the epitaxial source / drain regions 82. The openings 110 can be formed using suitable photolithography and etching techniques. For example, a photoresist (e.g., a single-layer or multi-layer photoresist structure) can be formed over the second ILD 108. The photoresist can then be patterned to expose the second ILD 108 in the regions corresponding to the openings 110. Then, using the patterned photoresist as an etching mask, one or more suitable etching processes can be performed to etch the openings 110. These one or more etching processes can include wet etching processes and / or dry etching processes. In some embodiments, CESL 87 and / or a hard mask 96 can be used as etch stop layers when forming the openings 110. In some embodiments, portions of CESL 87 extending over the epitaxial source / drain regions 82 can also be removed. In some embodiments where the opening extends through CESL 87, the opening 110 may extend below the top surface of the epitaxial source / drain region 82 and into the epitaxial source / drain region 82. In some embodiments, the one or more etching processes may remove material from the first ILD 88 to expose CESL 87, and may also partially etch the portion of CESL 87 above the epitaxial source / drain region 82. The opening 110 may have, for example, […]. Figure 17 The tapered sidewalls shown may also have sidewalls with different profiles (e.g., vertical sidewalls). In some embodiments, the opening 110 may have a width W1 between about 10 nm and about 30 nm, but other widths are also possible. The width W1 may be measured across the top of the opening 110, across the bottom of the opening 110, or across the opening 110 at any other location. In some cases, controlling the width W1 may control the dimensions of the subsequently formed source / drain contacts 118 and / or the air gap 120 (see [link to documentation]). Figure 22 ).
[0052] exist Figure 18In some embodiments, a dummy spacer layer 112 is formed over the opening 110. In some embodiments, an etching process is first performed to remove the CESL 87 over the epitaxial source / drain region 82. This etching process may include, for example, an anisotropic dry etching process. This etching process may extend the opening 110 below the top surface of the epitaxial source / drain region 82 and into the epitaxial source / drain region 82. Then, in some embodiments, the dummy spacer layer 112 may be formed as a blanket layer extending over the second ILD 108, CESL 87, and the epitaxial source / drain region 82. The dummy spacer layer 112 may include materials such as silicon, polycrystalline silicon, amorphous silicon, etc., or combinations thereof. In some embodiments, the dummy spacer layer 112 is a material that can be etched with high selectivity relative to other layers (e.g., the second ILD 108, CESL 87, or contact spacer layer 114 (described below)). The dummy spacer layer 112 can be deposited by PVD, CVD, ALD, etc. In some embodiments, the dummy spacer layer 112 can be formed to have a thickness between about 3 nm and about 9 nm, but other thicknesses are also possible. In some embodiments, the thickness of the dummy spacer layer 112 approximately corresponds to the width W2 of the subsequently formed air gap 120 (see...). Figure 22 ).
[0053] exist Figure 19 In some embodiments, a contact spacer layer 114 is formed on the dummy spacer layer 112. Prior to forming the contact spacer layer 114, a suitable anisotropic dry etching process may be performed to remove the region of the dummy spacer layer 112 extending laterally over the second ILD 108 and the epitaxial source / drain region 82. Due to the anisotropy of this dry etching process, the region of the dummy spacer layer 112 extending along the sidewalls of the opening 110 is retained. In some embodiments, the anisotropic dry etching process may also etch the material of the epitaxial source / drain region 82, thus extending the opening 110 further into the epitaxial source / drain region 82.
[0054] In some embodiments, the contact spacer layer 114 may be formed as a blanket layer extending over the second ILD 108, the dummy spacer layer 112, and the epitaxial source / drain region 82. The contact spacer layer 114 may comprise one or more layers of material, such as silicon oxide, silicon nitride, silicon oxynitride, silicon carbonitride, or combinations thereof. The contact spacer layer 114 may be deposited by PVD, CVD, ALD, or the like. In some embodiments, the contact spacer layer 114 may be formed with a thickness between about 2 nm and about 5 nm, for example, about 3 nm, but other thicknesses are also possible. After forming the contact spacer layer 114, a suitable anisotropic dry etching process may be performed to remove the laterally extending regions of the contact spacer layer 114 over the second ILD 108, the dummy spacer layer 112, and the epitaxial source / drain region 82. Due to the anisotropy of this dry etching process, the area of the contact spacer layer 114 extending along the sidewall of the opening 110 (e.g., along the dummy spacer layer 112) is preserved. In some cases, controlling the thickness of the contact spacer layer 114 can control the size of the subsequently formed source / drain contacts 118 and / or the size of the air gap 120 (see [link to documentation]). Figure 22 ).
[0055] Go to Figure 20 According to some embodiments, one or more conductive materials are deposited in the opening 110 to form source / drain contacts 118. In some embodiments, the conductive material of the source / drain contacts 118 includes a liner (not shown separately) conformally deposited on the surface of the opening 110 (e.g., on the contact spacer layer 114), and a conductive filler material deposited on the liner to fill the opening 110. In some embodiments, the liner includes titanium, cobalt, nickel, titanium nitride, titanium oxide, tantalum nitride, tantalum oxide, etc., or combinations thereof. In some embodiments, the conductive filler material includes cobalt, tungsten, copper, aluminum, gold, silver, alloys thereof, etc., or combinations thereof. The liner or conductive filler material can be deposited using one or more suitable processes, such as CVD, PVD, ALD, sputtering, plating, etc.
[0056] In some embodiments, a silicide region 116 may also be formed on the upper portion of the epitaxial source / drain region 82 to improve the electrical connection between the epitaxial source / drain region 82 and the source / drain contact 118. In some embodiments, the silicide region 116 may be formed by reacting the upper portion of the epitaxial source / drain region 82 with the liner. In some embodiments, a separate material may be deposited on the epitaxial source / drain region 82, which reacts with the epitaxial source / drain region 82 to form the silicide region 116. The silicide region 116 may include titanium silicide, nickel silicide, etc., or combinations thereof. In some embodiments, one or more annealing processes are performed to promote the silicide formation reaction. After depositing the conductive filler material for the source / drain contact 118, excess material may be removed by using a planarization process such as CMP to form a top surface of the source / drain contact 118 that is coplanar with the top surface of the second ILD 108.
[0057] Go to Figure 21 According to some embodiments, the material of the dummy spacer layer 112 is removed to form the initial air gap 120'. A suitable etching process, such as a dry etching process, can be used to remove the material of the dummy spacer layer 112. This etching process can be selective for the material of the dummy spacer layer 112 above the material of the second ILD 108, CESL 87, or contact spacer layer 114. For example, in embodiments where the dummy spacer layer 112 comprises silicon and the contact spacer layer 114 comprises silicon nitride, the etching process can include using HBr, O2, He, CH3F, H2, etc., or combinations thereof, as process gases in a plasma etching process that selectively etches the silicon of the dummy spacer layer 112. Other materials or etching processes are also possible.
[0058] In some embodiments, the initial air gap 120' may be formed with a width W2 between about 0.5 nm and about 4 nm, but other widths are also possible. In some cases, forming an initial air gap 120' with a larger width W2 can reduce capacitance and improve device performance, as will be described in more detail below. The initial air gap 120' may have a substantially uniform width, or the width may vary along its vertical length (e.g., the length extending away from the substrate 50). For example, the width of the initial air gap 120' may taper, for example, having a smaller width near the bottom (e.g., near the epitaxial source / drain region 82) than near the top (e.g., near the second ILD 108). In some embodiments, the bottom of the initial air gap 120' may extend into the epitaxial source / drain region 82 (e.g., as shown below). Figure 21(As shown), or the bottom of the initial air gap 120' may be at or above the top surface of the epitaxial source / drain region 82. The initial air gap 120' may extend at an angle relative to the vertical axis, such as... Figure 21 As shown, it can extend substantially along the vertical axis. In some embodiments, the initial air gap 120' can extend at a vertical height H1 (e.g., a distance H1 along the vertical axis) between about 15 nm and about 80 nm, but other heights are also possible.
[0059] In some cases, an initial air gap 120' is formed between the source / drain contact 118 and the gate stack 92 / 94 (and Figure 22 The subsequently formed air gap 120 (shown) reduces the capacitance between the source / drain contacts 118 and the gate stack 92 / 94. Compared to other spacer materials such as oxides and nitrides, air's low dielectric constant (k value), approximately k=1, allows for this reduction in capacitance. By using the air gap 120 to reduce capacitance, FinFET devices can exhibit faster response times and improved performance at higher frequencies.
[0060] Go to Figure 22 An etch stop layer (ESL) 122 is formed over the second ILD 108, the source / drain contact 118, and the initial air gap 120'. The ESL 122 may be formed as a blanket layer extending across the initial air gap 120', such that the initial air gap 120' is closed and forms the air gap 120. In some embodiments, some material of the ESL 122 extends partially into the initial air gap 120'. The ESL 122 may subsequently serve as an etch stop layer during the formation of conductive features 136 on the source / drain contact 118, as described below. Figure 26A -B and Figure 27A -B is described.
[0061] ESL 122 may comprise one or more layers of material, such as silicon nitride, silicon oxynitride, silicon carbonitride, silicon carbonitride, etc., or combinations thereof, and may be deposited using, for example, an ALD process (e.g., thermal ALD or plasma-enhanced ALD (PEALD) process). In some embodiments, ESL 122 may be formed having a thickness T2 between about 3 nm and about 30 nm on top of the second ILD 108, but other thicknesses are also possible. In some embodiments, ESL 122 may be deposited such that the material of ESL 122 extends into and seals the initial air gap 120'. The portion of ESL 122 extending into the initial air gap 120' is... Figure 22This is indicated as a sealing region 123' in subsequent figures. In some embodiments, the sealing region 123' may extend into the initial air gap 120' by a vertical distance D1, which is between approximately 2 nm and approximately 20 nm, but other distances are also possible. In some cases, the distance D1 may be less than, approximately equal to, or greater than the thickness T1 of the second ILD 108. In some embodiments, the distance D1 can be controlled by controlling parameters of the ESL 122 material deposition process, as described in more detail below.
[0062] The remaining portion of the initial air gap 120' sealed by the sealing region 123' is in Figure 22 This is indicated as air gap 120 in subsequent figures. In some embodiments, air gap 120 may extend at a vertical height H2 between about 10 nm and about 80 nm, but other distances are also possible. By controlling the deposition of ESL 122 to extend the sealing region 123' into the initial air gap 120', the conductive material of the subsequently deposited conductive feature 136 (see [reference]) can be prevented from being deposited. Figure 27B The air gap 120 is filled or partially filled, thus preserving the capacitive benefits of the air gap while reducing the likelihood of leakage between the conductive feature 136 and the gate stack 92 / 94. For example, forming an air gap 120 between the source / drain contact 118 and the gate stack 92 / 94 of a FinFET device can reduce the parasitic capacitance between the source / drain contact 118 and the gate stack 92 / 94, which can improve the high-speed operation of the FinFET. Furthermore, the presence of the air gap 120 reduces the amount of conductive feature 136 between the source / drain contact 118 and the gate stack 92 / 94, or subsequently formed (see [link to relevant documentation]). Figure 27B The possibility of leakage between the gate stack 92 / 94 and the sealing region 123'. The size of the subsequently formed air gap 120 can be controlled by controlling the distance D1 of the sealing region 123'. For example, in some cases, a smaller distance D1 can allow for a larger air gap 120, which can further reduce parasitic capacitance or leakage.
[0063] In some embodiments where the ALD process is used to deposit the material of ESL 122, parameters of the ALD process can be controlled to control the distance D1 by which the sealing region 123' extends into the initial air gap 120'. In some embodiments, the distance D1 can be controlled by controlling the dosage (e.g., pressure and / or pulse duration) of one or more precursors in the ALD process. For example, a larger dosage of the precursor may allow the precursor to reach and react with a deeper surface within the initial air gap 120'. In this way, a larger dosage of the precursor may allow the material of ESL 122 to grow on a surface that extends further into the initial air gap 120'. Correspondingly, a smaller dosage of the precursor may restrict the growth of the material of ESL 122 to a surface near the top of the initial air gap 120'. In this way, by controlling the dosage of one or more precursors, the distance by which the material of ESL 122 grows into the initial air gap 120' can be controlled, and therefore the distance D1 by which the sealing region 123' extends into the initial air gap 120' can be controlled.
[0064] In some embodiments, by using a smaller dose of the precursor, which may not reach all surfaces (e.g., the bottom) of the initial air gap 120' during an ALD half-cycle, and therefore not all possible surface reaction sites react with the precursor during the ALD half-cycle. In this way, the ALD process is not limited by the saturation of surface reaction sites, but by the precursor dose, and the ALD process described herein can be considered an “unsaturated” or “low-dose” ALD process. Furthermore, by using a smaller precursor dose, the material of ESL 122 can be controlled to not fill the initial air gap 120', but instead grow on the upper surface of the initial air gap 120' to form an air gap 120 sealed by the sealing region 123'. In this way, the unsaturated ALD process described herein can seal the initial air gap 120', thereby reducing the risk of filling the initial air gap 120' with material.
[0065] Figure 23A and Figure 23B It shows the relationship with Figure 22 The structures shown are similar, but Figure 23A An embodiment in which a sealing region 123' with a small distance D1 is formed is shown, and Figure 23B An embodiment is shown in which a sealing region 123' with a large distance D1 is formed. In some embodiments, parameters of the unsaturated ALD process described herein can be controlled to control the distance D1 of the sealing region 123'. For example, the dose of the precursor (e.g., pressure and / or pulse duration) of half a cycle can be controlled to control the formation of the sealing region 123'. Using a smaller precursor dose (e.g., a smaller precursor pressure and / or a shorter pulse duration) can form a sealing region 123' extending a smaller distance D1 into the initial air gap 120', similar to Figure 23A The sealing region 123' is shown. Using a larger precursor dose (e.g., a larger precursor pressure and / or a longer pulse duration), a sealing region 123' extending a larger distance D1 into the initial air gap 120' can be formed, similar to... Figure 23B The sealing region 123' is shown. In this way, controlling the precursor dosage can control the distance D1 by which the sealing region 123' extends into the initial air gap 120'.
[0066] As another example, in an embodiment where the ALD process is a PEALD process, the duration of the applied RF power during a half-cycle can be controlled to control the formation of the sealing region 123'. By reducing the RF duration, the amount of reactive precursor material generated is reduced, and a shorter RF power duration can form a sealing region 123' extending a smaller distance D1, similar to... Figure 23A The sealing region 123' is shown. A longer RF power duration can create a sealing region 123' that extends a greater distance D1, similar to... Figure 23B The sealing region 123' is shown. In some embodiments, a shorter precursor pulse duration combined with a shorter RF power duration can form a sealing region 123' with a smaller distance D1 compared to a longer precursor pulse duration combined with a longer RF power duration. These are examples, and precursor pressure, pulse duration, RF power duration, and / or other parameters can be controlled in other combinations or variations to control the formation of the sealing region 123'. Parameters or precursors for different portions of the ALD cycle can be controlled in this way, and in some embodiments, the same portions of different ALD cycles of the deposition process may have different parameters. Figure 22 , Figure 23A and Figure 23B The sealing region 123' and the corresponding distance D1 shown are illustrative examples, and the sealing region 123' may be formed to have a different distance D1 than shown.
[0067] As an illustrative example, the PEALD process can be used to deposit an ESL 122 (and a sealing region 123') comprising silicon nitride. Silicon formation precursors (e.g., SiH4, SiH2Cl2, SiH2I2, etc., or combinations thereof) can be used in the silicon formation half-cycle, and nitrogen formation precursors, such as N2, NH3, etc., or combinations thereof, can be used during the nitrogen formation half-cycle in which plasma is generated. Other precursors besides these can be used in other embodiments. Deposition can be performed in the process chamber at process temperatures between about 250°C and about 400°C, but other temperatures may also be used. In some embodiments, during the silicon formation half-cycle, the silicon formation precursor can be pulsed into the process chamber at a flow rate between about 5 sccm and about 100 sccm, with pulse durations between about 0.1 seconds and 0.5 seconds. The pressure during the silicon formation half-cycle can be between about 10 Torr and about 30 Torr. After the silicon formation precursor is pulsed, a purge can be performed for about 0.1 seconds to about 5 seconds. In some embodiments, during the nitrogen formation half-cycle, the nitrogen formation precursor can be pulsed into the process chamber at a flow rate between about 10 sccm and about 500 sccm, with the pulse duration between about 0.1 s and 1 s. The pressure during the nitrogen formation half-cycle can be between about 10 Torr and about 30 Torr. Plasma can be generated by RF power between about 0.1 s and about 1 s. Plasma can be generated by RF power between about 100 watts and about 800 watts. After the nitrogen formation precursor is pulsed, a purging period of about 0.1 s to about 1 s can be performed. These are example parameter values, and other parameter values or combinations thereof may be used in other embodiments.
[0068] Figures 24A to 27B This is a cross-sectional view of an additional stage in the fabrication of a FinFET according to some embodiments. Figures 24A to 27B It shows Figure 15A and Figure 15B The same cross-sectional view of the structure shown. Figure 24A and Figure 24B The structure after ESL 122 deposition is shown, similar to Figure 22 The structure shown.
[0069] Go to Figure 25A and Figure 25BAccording to some embodiments, a dielectric layer 134 may be formed on the ESL 122. The dielectric layer 134 may be formed of a suitable dielectric material, such as a low-k dielectric material, a polymer (e.g., polyimide), silicon oxide, silicon nitride, silicon carbide, silicon carbonitride, silicon carbonitride, etc., or combinations thereof. The dielectric layer 134 may be formed using suitable processes such as spin coating, CVD, PVD, ALD, etc. In some embodiments, the dielectric layer 134 may be formed in a manner similar to the previously described first ILD 88 or second ILD 108.
[0070] exist Figure 26A and Figure 26B In some embodiments, an opening 138 and a recess 139 may be formed. The opening 138 extends through the dielectric layer 134 and ESL 122 to expose the source / drain contact 118. Figure 26B An embodiment is shown in which a single opening 138 exposes two adjacent source / drain contacts 118; however, in other embodiments, a single opening 138 may expose a single source / drain contact 118 or more than two source / drain contacts 118. The opening 138 and the recess 139 can be formed using suitable photolithography and etching techniques. For example, a photoresist (e.g., a single-layer or multi-layer photoresist structure) can be formed over a dielectric layer 134. The photoresist can then be patterned to expose the dielectric layer 134 in the region corresponding to the opening 138. Then, using the patterned photoresist as an etching mask, one or more suitable etching processes can be performed to etch the opening 138. These one or more etching processes may include wet etching processes and / or dry etching processes. In some embodiments, ESL 122 can be used as an etch stop layer during the formation of the opening 138. The opening 138 may have, for example, Figure 26B The tapered sidewalls shown may also have sidewalls with different profiles (e.g., vertical sidewalls).
[0071] Still referencing Figure 26B Alternatively, a portion of the sealing region 123' can be removed by etching (one or more) processes to form an extension to the initial air gap 120' (see [link]). Figure 21The groove 139 is located in the initial air gap 120. The etching process(s) can be controlled such that after the opening 138 is formed, the air gap 120 remains sealed by the remaining portion of the sealing region 123'. The remaining portion of the sealing region 123' can be referred to as "seal 123". Because of the remaining portion of the seal 123' forming the sealing region 123', using the sealing region 123' to seal the air gap 120 prevents exposure of the air gap 120 during the formation of the opening 138. In some embodiments, the groove 139 may extend to a vertical distance D2 in the initial air gap 120', which is between approximately 0 nm and approximately 15 nm, but other distances are also possible. Possible dimensions of the seal 123 are described below for... Figure 28 To describe in more detail.
[0072] Furthermore, the presence of the seal 123 protects the air gap 120 and prevents subsequently formed conductive material from entering the air gap 120, which can reduce the subsequent formation of conductive features 136 (see [link]). Figure 27B The possibility of leakage between the gate stack 92 / 94 and the gate stack. For example, although Figure 26B The diagram shows that the opening 138 is patterned to extend over the air gap 120, but in other cases, the opening 138 may not be desired to extend over the air gap 120 due to, for example, lithographic misalignment. Thus, the seal 123 prevents subsequently deposited material from entering the air gap 120. This is achieved by a vertical distance D1 relative to the sealing region 123' (see...). Figure 22 The depth D2 of the groove 139 can be controlled to control the position and size of the seal 123, which may depend on the specific application or desired structure. For example, a larger seal 123 may provide more protection against leakage, or a smaller seal 123 may allow for a larger air gap 120, thereby further reducing parasitic capacitance. These are examples, and other configurations or considerations are possible.
[0073] exist Figure 27A and Figure 27B In some embodiments, conductive feature 136 is formed as a contact source / drain contact 118. Figure 28 It shows Figure 27B A detailed view of region 135. Conductive feature 136 may include one or more metal wires and / or vias making physical and electrical contact with source / drain contacts 118. Conductive feature 136 may be, for example, a redistribution layer. Any suitable technique may be used to form conductive feature 136.
[0074] In some embodiments, the material used to form the conductive feature 136 may be a single damascene process and / or a dual damascene process, a via-first process, or a metal-first process. In some embodiments, a liner 137, such as a diffusion barrier layer, an adhesive layer, etc., is formed in the opening 138 and the recess 139. Figure 28 (As shown). The liner may include titanium, titanium nitride, tantalum, tantalum nitride, etc., which can be formed using deposition processes such as CVD, ALD, etc. A conductive material can then be formed on the liner 137. The conductive material may be copper, copper alloy, silver, gold, tungsten, cobalt, aluminum, nickel, etc., or combinations thereof. The conductive material may be formed on the liner 137 in the opening 138 and the groove 139 by, for example, electrochemical coating processes, CVD, ALD, PVD, etc., or combinations thereof. The material of the liner 137 and / or the conductive material is prevented from entering the air gap 120 by the seal 123. A planarization process such as CMP may be performed to remove excess material from the surface of the dielectric layer 134. The remaining liner 137 and conductive material form the conductive feature 136. In other embodiments, other techniques may be used to form the conductive feature 136. The seal 123 may be separated from the remaining portion of the ESL 122 (e.g., the portion on the second ILD 108) by the conductive feature 136, as Figure 28 As shown.
[0075] Figure 27A A gate contact 132, physically coupled and electrically coupled to a gate electrode 94, is also shown. The gate contact 132 can be formed, for example, by forming an opening exposing the gate electrode 94 using a suitable photolithography and etching process, and then depositing an optional liner and conductive material within the opening. The gate contact 132 can be formed before or after the formation of the dielectric layer 134. The source / drain contacts 118 and the gate contact 132 can be formed using different processes or the same process. In some embodiments, some conductive features 136 (conductive features) in contact with the gate contact 132 can also be formed. Figure 27A (Not shown in the image).
[0076] refer to Figure 28 Each seal 123 may be formed to have a width approximately the same as the width W2 of the initial air gap 120' described previously. The width of the seal 123 may be substantially constant, or the seal 123 may have a concave, convex, tapered, or irregular sidewall profile. The seal 123 may have substantially vertical sidewalls, or may have sidewalls that are at least partially angled, such as... Figure 28As shown. In some embodiments, the seal 123 may extend to a vertical height H3 between about 1 nm and about 15 nm, but other heights are also possible. In some embodiments, the height H3 of the seal 123 may be between about 1% and about 150% of the thickness T1 of the second ILD 108, but other fractions are also possible. In some cases, a larger height H3 may provide improved sealing of the air gap 120, as well as improved protection against electrical short circuits or leakage. In some embodiments, the top surface of the seal 123 may be above the gate stack (e.g., above the gate dielectric layer 92 and the gate electrode 94) at a vertical distance D4, which is between about 0 nm and about 35 nm, but other distances are also possible. The top surface of the seal 123 may be above the gate stack, below the gate stack, or substantially flush with the gate stack. In some cases, a larger vertical distance D4 between the top surface of the seal 123 and the gate stack may allow for improved protection against leakage or short circuits between the conductive feature 136 and the gate stack. In some embodiments, the seal 123 may have a width-to-height ratio (width:height) between about 4:1 and about 1:30, but other aspect ratios are also possible. In some cases, a seal 123 with a relatively wide aspect ratio may allow for a larger air gap 120, which can improve capacitance reduction. In some embodiments, the seal 123 may have a substantially flat top surface and / or a substantially flat bottom surface, which may be substantially horizontal (e.g., parallel to the plane of the substrate 50) or may be angled relative to the horizontal. Figure 28 An embodiment is shown in which the top and bottom surfaces of the seal 123 are substantially flat and substantially horizontal. In other embodiments, the top and / or bottom surfaces of the seal 123 may be convex, concave, circular, irregular, or have another shape.
[0077] refer to Figure 28 The portion of the filling groove 139 of the conductive feature 136 may have a width W3 between about 0.5 nm and about 4 nm, but other widths are also possible. The width W3 may be approximately the same as the width W2 of the initial air gap 120' previously described. The width of the conductive feature 136 within the groove 139 may be substantially constant, or may have concave, convex, tapered, or irregular sidewall profiles. The conductive feature 136 within the groove 139 may have substantially vertical sidewalls or may have sidewalls that are at least partially angled, such as... Figure 28 As shown. In some embodiments, the conductive feature 136 within the groove 139 may extend a vertical distance D3 below the top surface of the second ILD 108, the vertical distance D3 being between about 0 nm and about 15 nm, but other distances are also possible. The vertical distance D3 may be related to the... Figure 26BThe vertical distance D2 of the described groove 139 is approximately the same. In some embodiments, the vertical distance D3 can be between about 0% and about 150% of the thickness T1 of the second ILD 108, but other fractions are also possible. In some cases, a smaller vertical distance D3 can allow for the formation of a larger air gap 120, and thus can allow for improved capacitance reduction. In some embodiments, the conductive feature 136 within the groove 139 may have an aspect ratio (width:height) between about 10:1 and about 1:30, but other aspect ratios are also possible. In some cases, a relatively wide aspect ratio can allow for a larger air gap 120, which can improve capacitance reduction. In some embodiments, the conductive feature 136 within the groove 139 may have a substantially flat bottom surface, which may be substantially horizontal (e.g., parallel to the plane of the substrate 50) or may be angled relative to the horizontal. Figure 28 An embodiment is shown in which the bottom surface of the conductive feature 136 within the groove 139 is substantially flat and substantially horizontal. In other embodiments, the bottom surface of the conductive feature 136 within the groove 139 may be convex, concave, circular, irregular, or have another shape.
[0078] The embodiments can achieve advantages. By forming an air gap between the source / drain contacts and the gate stack of a FinFET device, the capacitance between the source / drain contacts and the gate stack can be reduced. Reducing this capacitance can improve the speed or high-frequency operation of the FinFET device. Additionally, the top of the air gap is sealed by the remainder of the dielectric layer above, which may be an etch stop layer. Sealing the air gap prevents unwanted material from entering and degrading device performance or causing process defects. For example, sealing the portion of the dielectric layer can improve the isolation between the source / drain contacts and the gate of the FinFET. In some cases, controlling the dose of the ALD process used to form the dielectric layer and / or the RF time of the PEALD process can control the size or depth of the remainder of the dielectric layer within the air gap.
[0079] In some embodiments, a device includes: a fin extending from a semiconductor substrate; a gate stack above the fin; a spacer on the sidewalls of the gate stack; a source / drain region adjacent to the spacer in the fin; an interlayer dielectric layer (ILD) extending above the gate stack, the spacer, and the source / drain region; a contact plug extending through the ILD and contacting the source / drain region; a dielectric layer including a first portion on the top surface of the ILD and a second portion extending between the ILD and the contact plug, wherein the top surface of the second portion is closer to the substrate than the top surface of the ILD; and an air gap between the spacer and the contact plug, wherein the second portion of the dielectric layer seals the top of the air gap. In one embodiment, the device includes: a conductive material extending over the ILD, the second portion, and the contact plug. In one embodiment, the conductive material is separated from the air gap by the second portion. In one embodiment, the first portion is separated from the second portion by the conductive material. In one embodiment, the dielectric layer includes silicon nitride. In one embodiment, the top surface of the second portion is in the range of 0 nm to 15 nm below the top surface of the ILD. In one embodiment, the vertical thickness of the second portion is in the range of 1 nm to 15 nm. In one embodiment, the width of the second portion is in the range of 0.5 nm to 4 nm. In one embodiment, the vertical thickness of the first portion is in the range of 3 nm to 30 nm. In one embodiment, the bottom surface of the second portion is further away from the substrate than the bottom surface of the ILD.
[0080] In some embodiments, a method includes: forming a fin protruding from a substrate; forming a gate structure over a channel region of the fin; forming a gate spacer along a sidewall of the gate structure; forming an epitaxial region in the fin adjacent to the channel region; depositing a first dielectric layer over the gate structure and the gate spacer, the first dielectric layer comprising a first dielectric material; forming a contact plug extending through the first dielectric layer and contacting the epitaxial region, wherein an air gap separates the contact plug and the gate spacer; depositing a second dielectric layer over the first dielectric layer and over the contact plug, including sealing a lower region of the air gap with the second dielectric layer, wherein the second dielectric layer comprises a second dielectric material different from the first dielectric material; etching the second dielectric layer to expose the contact plug, wherein after etching the second dielectric layer, the remaining portion of the second dielectric layer seals the lower region of the air gap; and depositing a conductive material on the contact plug, including depositing a conductive material between the contact plug and the first dielectric material and on the remaining portion of the second dielectric layer. In one embodiment, an upper region of the air gap separates the first dielectric layer and the contact plug. In one embodiment, the remaining portion of the second dielectric layer is less thick than the first dielectric layer. In one embodiment, the remaining portion of the second dielectric layer is closer to the substrate than the top surface of the first dielectric layer. In one embodiment, depositing conductive material includes depositing conductive material on the top surface of the first dielectric layer. In one embodiment, the remaining portion of the second dielectric layer extends from the first dielectric layer to a spacer layer on the contact plug.
[0081] In some embodiments, a method includes: forming a gate stack over a semiconductor fin; forming an epitaxial source / drain region adjacent to the gate stack in the semiconductor fin; depositing a first dielectric layer over the gate stack and over the epitaxial source / drain region; forming an opening in the first dielectric layer to expose the epitaxial source / drain region; depositing a sacrificial material within the opening; depositing a first conductive material over the sacrificial material within the opening; removing the sacrificial material to form a gap; depositing a second dielectric layer over the first dielectric layer, over the conductive material, and over the gap, wherein the second dielectric layer extends a first distance into the gap; and etching the second dielectric layer to expose the first conductive material, wherein a first portion of the second dielectric layer remains within the gap after etching. In one embodiment, depositing the second dielectric layer includes depositing silicon nitride using a plasma-enhanced atomic layer deposition (PEALD) process. In one embodiment, etching the second dielectric layer includes etching a second portion of the second dielectric layer within the gap. In one embodiment, the method includes depositing a second conductive material on the first conductive material and on the first portion of the second dielectric layer.
[0082] The foregoing has outlined features of several embodiments to enable those skilled in the art to better understand various aspects of this disclosure. Those skilled in the art should understand that they can readily use this disclosure as a basis for designing or modifying other processes and structures to achieve the same purposes and / or the same advantages of the embodiments described herein. Those skilled in the art should also recognize that such equivalent constructions do not depart from the spirit and scope of this disclosure, and that various changes, substitutions, and modifications can be made herein without departing from the spirit and scope of this disclosure.
[0083] Example 1 is a semiconductor device comprising: a fin extending from a semiconductor substrate; a gate stack above the fin; a spacer on a sidewall of the gate stack; a source / drain region in the fin adjacent to the spacer; an interlayer dielectric layer (ILD) extending above the gate stack, the spacer, and the source / drain region; a contact plug extending through the ILD and contacting the source / drain region; a dielectric layer including a first portion located on a top surface of the ILD and a second portion extending between the ILD and the contact plug, wherein the top surface of the second portion is closer to the substrate than the top surface of the ILD; and an air gap between the spacer and the contact plug, wherein the second portion of the dielectric layer seals the top of the air gap.
[0084] Example 2 is the device described in Example 1, further comprising: a conductive material extending over the ILD, the second portion, and the contact plug.
[0085] Example 3 is the device described in Example 2, wherein the conductive material is separated from the air gap by the second portion.
[0086] Example 4 is the device described in Example 2, wherein the first portion is separated from the second portion by the conductive material.
[0087] Example 5 is the device described in Example 1, wherein the dielectric layer comprises silicon nitride.
[0088] Example 6 is the device described in Example 1, wherein the top surface of the second portion is in the range of 0 nm and 15 nm below the top surface of the ILD.
[0089] Example 7 is the device described in Example 1, wherein the vertical thickness of the second portion is in the range of 1 nm to 15 nm.
[0090] Example 8 is the device described in Example 1, wherein the width of the second portion is in the range of 0.5 nm and 4 nm.
[0091] Example 9 is the device described in Example 1, wherein the vertical thickness of the first portion is in the range of 3 nm to 30 nm.
[0092] Example 10 is the device described in Example 1, wherein the bottom surface of the second portion is further away from the substrate than the bottom surface of the ILD.
[0093] Example 11 is a method for forming a semiconductor device, comprising: forming a fin protruding from a substrate; forming a gate structure over a channel region of the fin; forming a gate spacer along a sidewall of the gate structure; forming an epitaxial region in the fin adjacent to the channel region; depositing a first dielectric layer over the gate structure and the gate spacer, the first dielectric layer comprising a first dielectric material; forming a contact plug extending through the first dielectric layer and contacting the epitaxial region, wherein an air gap separates the contact plug and the gate spacer; depositing a second dielectric layer over the first dielectric layer and over the contact plug, including sealing a lower region of the air gap with the second dielectric layer, wherein the second dielectric layer comprises a second dielectric material different from the first dielectric material; etching the second dielectric layer to expose the contact plug, wherein, after etching the second dielectric layer, the remaining portion of the second dielectric layer seals the lower region of the air gap; and depositing a conductive material on the contact plug, including depositing the conductive material between the contact plug and the first dielectric material and on the remaining portion of the second dielectric layer.
[0094] Example 12 is the method described in Example 11, wherein the upper region of the air gap separates the first dielectric layer and the contact plug.
[0095] Example 13 is the method described in Example 11, wherein the thickness of the remaining portion of the second dielectric layer is less than the thickness of the first dielectric layer.
[0096] Example 14 is the method described in Example 11, wherein the remaining portion of the second dielectric layer is closer to the substrate than the top surface of the first dielectric layer.
[0097] Example 15 is the method of Example 11, wherein depositing the conductive material includes depositing the conductive material on the top surface of the first dielectric layer.
[0098] Example 16 is the method of Example 11, wherein the remaining portion of the second dielectric layer extends from the first dielectric layer to the spacer layer on the contact plug.
[0099] Example 17 is a method for forming a semiconductor device, comprising: forming a gate stack over a semiconductor fin; forming an epitaxial source / drain region in the semiconductor fin adjacent to the gate stack; depositing a first dielectric layer over the gate stack and over the epitaxial source / drain region; forming an opening in the first dielectric layer to expose the epitaxial source / drain region; depositing a sacrificial material within the opening; depositing a first conductive material over the sacrificial material within the opening; removing the sacrificial material to form a gap; depositing a second dielectric layer over the first dielectric layer, over the conductive material, and over the gap, wherein the second dielectric layer extends a first distance into the gap; and etching the second dielectric layer to expose the first conductive material, wherein a first portion of the second dielectric layer remains within the gap after the etching.
[0100] Example 18 is the method described in Example 17, wherein depositing the second dielectric layer includes depositing silicon nitride using a plasma-enhanced atomic layer deposition (PEALD) process.
[0101] Example 19 is the method of Example 17, wherein etching the second dielectric layer includes etching a second portion of the second dielectric layer within the gap.
[0102] Example 20 is the method of Example 17, further comprising depositing a second conductive material on the first conductive material and on a first portion of the second dielectric layer.
Claims
1. A semiconductor device, comprising: Fins extend from the semiconductor substrate; Gate stacks are located on the fin; Spacers are located on the sidewalls of the gate stack. The source / drain region is adjacent to the spacer in the fin; An interlayer dielectric layer (ILD) extends over the gate stack, the spacers, and the source / drain regions; The contact plug extends through the ILD and contacts the source / drain region; A dielectric layer comprising a first portion located on the top surface of the ILD and a second portion extending between the ILD and the contact plug, wherein the top surface of the second portion is closer to the substrate than the top surface of the ILD, and the first portion is separate from the second portion; and An air gap exists between the spacer and the contact plug, wherein a second portion of the dielectric layer seals the top of the air gap.
2. The device according to claim 1, further comprising: A conductive material extends over the ILD, the second portion, and the contact plug.
3. The device according to claim 2, wherein, The conductive material is separated from the air gap through the second portion.
4. The device according to claim 2, wherein, The first part is separated from the second part by the conductive material.
5. The device according to claim 1, wherein, The dielectric layer comprises silicon nitride.
6. The device according to claim 1, wherein, The top surface of the second part is located between 0 nm and 15 nm below the top surface of the ILD.
7. The device according to claim 1, wherein, The vertical thickness of the second part is in the range of 1 nm to 15 nm.
8. The device according to claim 1, wherein, The width of the second part is in the range of 0.5 nm to 4 nm.
9. The device according to claim 1, wherein, The vertical thickness of the first part is in the range of 3 nm to 30 nm.
10. The device according to claim 1, wherein, The bottom surface of the second portion is further away from the substrate than the bottom surface of the ILD.
11. A method for forming a semiconductor device, comprising: Forming fins that protrude from the substrate; A gate structure is formed above the channel region of the fin; A gate spacer is formed along the sidewall of the gate structure; An extensional region adjacent to the channel region is formed in the fin; A first dielectric layer is deposited on the gate structure and the gate spacer, the first dielectric layer comprising a first dielectric material; A contact plug is formed, the contact plug extending through the first dielectric layer and contacting the epitaxial region, wherein an air gap separates the contact plug and the gate spacer; Depositing a second dielectric layer on top of the first dielectric layer and on top of the contact plug, including sealing the lower region of the air gap with the second dielectric layer, wherein the second dielectric layer comprises a second dielectric material different from the first dielectric material; Etching the second dielectric layer to expose the contact plug, wherein, after etching the second dielectric layer, a first portion of the second dielectric layer is located on the top surface of the first dielectric layer, a second portion of the second dielectric layer seals the lower region of the air gap, and the first portion is separated from the second portion; and Depositing conductive material on the contact plug includes depositing the conductive material between the contact plug and the first dielectric material and on a second portion of the second dielectric layer.
12. The method according to claim 11, wherein, The upper region of the air gap separates the first dielectric layer and the contact plug.
13. The method according to claim 11, wherein, The thickness of the second portion of the second dielectric layer is less than the thickness of the first dielectric layer.
14. The method according to claim 11, wherein, The second portion of the second dielectric layer is closer to the substrate than the top surface of the first dielectric layer.
15. The method according to claim 11, wherein, Depositing the conductive material includes depositing the conductive material on the top surface of the first dielectric layer.
16. The method according to claim 11, wherein, A second portion of the second dielectric layer extends from the first dielectric layer to the spacer layer on the contact plug.
17. A method for forming a semiconductor device, comprising: A gate stack is formed on the semiconductor fin; An epitaxial source / drain region adjacent to the gate stack is formed in the semiconductor fin; A first dielectric layer is deposited on the gate stack and on the epitaxial source / drain regions; An opening is formed in the first dielectric layer to expose the epitaxial source / drain region; Deposit sacrificial material within the opening; A first conductive material is deposited on the sacrificial material within the opening; Remove the sacrificial material to form a gap; A second dielectric layer is deposited over the first dielectric layer, over the first conductive material, and over the gap, wherein the second dielectric layer extends a first distance into the gap; and The second dielectric layer is etched to expose the first conductive material, wherein, after the etching, a first portion of the second dielectric layer is located on the top surface of the first dielectric layer, a second portion of the second dielectric layer remains within the gap, and the first portion is separated from the second portion.
18. The method according to claim 17, wherein, Depositing the second dielectric layer involves depositing silicon nitride using a plasma-enhanced atomic layer deposition (PEALD) process.
19. The method of claim 17, wherein, Etching the second dielectric layer includes etching a portion of the second dielectric layer within the gap.
20. The method of claim 17, further comprising depositing a second conductive material on the first conductive material and on a second portion of the second dielectric layer.
Citation Information
Patent Citations
Integrated circuit devices
CN109390337A
Inverse t-shaped contact structures having air gap spacers
US20190334011A1
Semiconductor device with linerless contacts
US20200303246A1