A waste acid concentration treatment tower

By using multi-stage packing layers and hot air convection technology in the waste acid concentration treatment tower, the problems of impurity removal and concentration increase in sulfuric acid waste liquid are solved, efficient concentration of waste acid and resource reuse are achieved, and environmental pollution is reduced.

CN114588646BActive Publication Date: 2024-10-18JIANGSU YUHAO INTELLIGENT MFG CO LTD
View PDF 14 Cites 0 Cited by

Patent Information

Application Number
CN202110327745.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-03-26
Publication Date
2024-10-18
Estimated Expiration
2041-03-26

AI Technical Summary

Technical Problem

The sulfuric acid waste liquid produced in industrial production contains a large number of metal ions and organic impurities, causing environmental pollution. Existing treatment methods are difficult to effectively remove impurities and increase the concentration of sulfuric acid, affecting resource reuse.

Method used

A waste acid concentration treatment tower is designed, which adopts a multi-stage packing layer structure, including circular orifice plate corrugated packing, inorganic packing and metal mesh corrugated packing. It is combined with an ultrasonic generator and heating device, and uses hot air convection and surface treatment technology. Improve the concentration efficiency and specific gravity of waste acid.

Benefits of technology

It achieves efficient concentration of waste acid, meets recycling standards, reduces environmental pollution, and is conducive to energy conservation and environmental protection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0002995267680000071
    Figure BDA0002995267680000071
  • Figure BDA0002995267680000261
    Figure BDA0002995267680000261
  • Figure HDA0002995267690000011
    Figure HDA0002995267690000011
Patent Text Reader

Abstract

The invention belongs to the technical field of environmental protection, and particularly relates to a waste acid concentration treatment tower; the treatment tower comprises a tower body, an exhaust port, a packing layer, an air inlet, a feeding port, a discharging port, and other structures; the packing comprises three types of packing layers, namely, an upper, middle, and lower packing layer, and the multi-stage packing layer can improve the efficiency of waste acid concentration; a material with a large specific surface area is adopted, and an ionic liquid is used to perform surface treatment on the material, thereby increasing the acid and alkali resistance of the packing and obtaining a concentrated acid with a higher specific gravity; a metal packing layer is adopted in the lower layer, thereby increasing the specific gravity of waste acid concentration; by treating waste liquid with the waste acid concentration treatment tower of the invention, the recycling standard can be achieved, thereby realizing resource reuse, which is beneficial to energy conservation and environmental protection, which is a pollution problem that needs to be solved at present.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of environmental protection, and in particular relates to a waste acid concentration treatment tower. Background Art

[0002] Sulfuric acid is widely used in industrial production processes, which will produce a large amount of sulfuric acid waste liquid. Sulfuric acid waste liquid contains a large amount of metal ions and organic impurities, which pollutes the environment greatly. The current treatment methods used are recycling and neutralization treatment. In the recycling process, impurities in the waste liquid can be effectively removed, and the concentration of sulfuric acid can be increased, and the recycling standard can be met, thereby realizing resource reuse, which is beneficial to energy conservation and environmental protection, and is the pollution problem that needs to be solved at present. Summary of the invention

[0003] In order to solve the above technical problems, the first aspect of the present invention provides a waste acid concentration treatment tower, including a tower body 1, an exhaust port 2 is provided above the top of the tower body 1, a packing layer is provided in the middle of the tower body 1, an air inlet 6 is provided on one side below the tower body 1, and a heating device 9 is connected to the bottom of the tower body 1.

[0004] Preferably, the packing layer comprises a first packing layer 3, a second packing layer 4, and a third packing layer 5; the first packing layer 3, the second packing layer 4, and the third packing layer 5 are respectively located at the upper, middle, and lower positions of the packing layer.

[0005] Preferably, an ultrasonic generator 10 is connected to the bottom of the heating device 9; preferably, a feeding port 7 is provided on the lower side of the tower body 1; preferably, a discharge port 8 is provided on the lower side of the feeding port 7; preferably, the air inlet 6 is located on the lower side of the tower body 1 away from the feeding port 7 and the discharge port 8, and the height of the air inlet 6 is greater than the height of the feeding port 7; preferably, the heating temperature of the heating device 9 is 55-65°C.

[0006] Preferably, the height ratio of the first packing layer 3, the second packing layer 4 and the third packing layer 5 is (1.0-1.6):(1.6-2.5):1.

[0007] Preferably, the height ratio of the first packing layer 3, the second packing layer 4 and the third packing layer 5 is (1.2-1.4):(1.8-2.2):1.

[0008] Preferably, the filler of the second filler layer is an inorganic filler.

[0009] Beneficial Effects

[0010] 1. A waste acid concentration treatment tower provided by the present invention comprises three types of packing layers: upper, middle and lower. The multi-stage packing layer can improve the efficiency of waste acid concentration.

[0011] 2. In the present invention, the middle filler layer uses inorganic fillers, and the inorganic fillers use materials with large specific surface areas. At the same time, ionic liquids are used to treat the surface of the materials, which increases the acid and alkali resistance of the fillers and can obtain concentrated acids with higher specific gravity.

[0012] 3. The lower layer of the present invention adopts a metal filler layer, which increases the specific gravity of the waste acid concentration.

[0013] 4. By treating the waste liquid with the waste acid concentration treatment tower of the present invention, the recycling standard can be achieved, thereby realizing resource reuse, which is beneficial to energy conservation and environmental protection, which is the pollution problem that needs to be solved at present. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 It is a schematic structural diagram of the waste acid concentration treatment tower of the present invention.

[0015] In the figure: 1 tower body, 2 exhaust port, 3 first packing layer, 4 second packing layer, 5 third packing layer, 6 air inlet, 7 feeding port, 8 discharging port, 9 heating device, 10 ultrasonic generator. DETAILED DESCRIPTION

[0016] The following is a further clear and complete description of the technical features in the technical solution provided by the present invention in conjunction with specific implementation methods, which is not intended to limit the scope of protection thereof.

[0017] The words "preferred", "more preferred" and the like in the present invention refer to embodiments of the present invention that can provide certain beneficial effects in certain circumstances. However, other embodiments may also be preferred under the same circumstances or other circumstances. In addition, the description of one or more preferred embodiments does not imply that other embodiments are not applicable, nor is it intended to exclude other embodiments from the scope of the present invention.

[0018] A first aspect of the present invention provides a waste acid concentration treatment tower, comprising a tower body 1, an exhaust port 2 is provided above the top of the tower body 1, a packing layer is provided in the middle of the tower body 1, an air inlet 6 is provided on one side below the tower body 1, and a heating device 9 is connected below the bottom of the tower body 1.

[0019] In one embodiment, the packing layer is composed of a first packing layer 3, a second packing layer 4, and a third packing layer 5, which are respectively located at the upper, middle, and lower positions of the packing layer.

[0020] In one embodiment, an ultrasonic generator 10 is connected to the bottom of the heating device 9 .

[0021] In one embodiment, a feeding port 7 is provided on a lower side of the tower body 1 .

[0022] In one embodiment, a discharge port 8 is provided on one side below the feed port 7 .

[0023] In one embodiment, the air inlet 6 is located at a side of the lower side of the tower body 1 away from the feeding port 7 and the discharging port 8 , and the height of the air inlet 6 is greater than the height of the feeding port 7 .

[0024] Hot air is added through the air inlet 6, which is located above the other side of the feeding port 7 and the discharging port 8, which is beneficial to the convection of hot air on the water vapor of the dilute sulfuric acid.

[0025] In one embodiment, the heating temperature of the heating device 9 is 55-65°C.

[0026] In one embodiment, the height ratio of the first packing layer 3, the second packing layer 4, and the third packing layer 5 is (1.0-1.6):(1.6-2.5):1.

[0027] In a preferred embodiment, the height ratio of the first packing layer 3, the second packing layer 4, and the third packing layer 5 is (1.2-1.4):(1.8-2.2):1.

[0028] In a more preferred embodiment, the height ratio of the first packing layer 3 , the second packing layer 4 , and the third packing layer 5 is 1.25:2:1.

[0029] In one embodiment, the filler of the first filler layer is a circular perforated plate corrugated filler; the specific surface area of ​​the perforated plate corrugated filler is 200-400m 2 / m 3 , the void ratio is 90-98%.

[0030] In a preferred embodiment, the raw material of the orifice plate corrugated packing is polytetrafluoroethylene; the specific surface area of ​​the circular polytetrafluoroethylene orifice plate corrugated packing is 250m 2 / m 3 , the porosity is 97%.

[0031] In one embodiment, the circular polytetrafluoroethylene orifice plate corrugated packing is purchased from Jiangxi Pingxiang Kelong Petrochemical Equipment Packing Co., Ltd., model SB-250Y.

[0032] It was found in the experiment that the perforated plate corrugated packing has a large porosity and good wetting properties, which optimizes the treatment effect of waste acid concentration and can increase the proportion of recovered acid.

[0033] In one embodiment, the filler of the third filler layer is a circular metal wire mesh corrugated filler; the specific surface area of ​​the metal wire mesh corrugated filler is 600-800m 2 / m 3 , the void ratio is 80-95%.

[0034] In a preferred embodiment, the raw material of the metal wire mesh corrugated packing is chromium-nickel-molybdenum-copper alloy; the specific surface area of ​​the circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing is 700m 2 / m 3 , the void ratio is 87%.

[0035] In one embodiment, the circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing is purchased from Anping County Hualai Metal Wire Mesh Co., Ltd., and the model is 700 (CY).

[0036] The experiment found that the metal filler has high compressive strength, the chromium-nickel-molybdenum-copper alloy wire mesh corrugated filler has low pressure drop when used, large specific surface area, relatively high porosity, and high separation efficiency for impurities, which can enhance the effect of waste acid concentration.

[0037] In one embodiment, the filler of the second filler layer is an inorganic filler; the raw materials of the inorganic filler, by weight, include the following components: 37.5 parts of clay, 24 parts of calcined alumina, 9.6 parts of nanomaterials, 5.7 parts of layered materials, 3.2 parts of tea residue powder, and 2 parts of alloy.

[0038] In one embodiment, the raw material of the inorganic filler further includes an ionic liquid.

[0039] In one embodiment, the alloy is a cobalt-based alloy.

[0040] In one embodiment, the cobalt-based alloy is purchased from Nangong Yingtai Metal Materials Co., Ltd., and the specification model is Co6.

[0041] In one embodiment, the clay is composed of kaolin, attapulgite and montmorillonite in a weight ratio of (4-6):(1-2):1.

[0042] In a preferred embodiment, the clay is composed of kaolin, attapulgite and montmorillonite in a weight ratio of (4.5-5.5):(1.2-1.7):1.

[0043] In one embodiment, the clay consists of kaolin, attapulgite and montmorillonite in a weight ratio of 5:1.5:1.

[0044] In one embodiment, the particle size of the calcined alumina is 40-50 um.

[0045] In a preferred embodiment, the particle size of the calcined alumina is 45 um.

[0046] In one embodiment, the calcined alumina is purchased from Hebei Hengguang Mineral Products Co., Ltd., and the alumina content is greater than 99%.

[0047] In one embodiment, the particle size of the kaolin is 20-25 um.

[0048] In a preferred embodiment, the particle size of the kaolin is 23 um.

[0049] In one embodiment, the kaolin is purchased from Hebei Huanhe Mineral Products Co., Ltd., and the silicon dioxide content is 52%.

[0050] In one embodiment, the particle size of the attapulgite is 20-30 um.

[0051] In a preferred embodiment, the particle size of the attapulgite is 25 um.

[0052] In one embodiment, the attapulgite is purchased from the Qiangdong Mineral Products Processing Plant in Lingshou County, and the specification model is qd-015.

[0053] In one embodiment, the particle size of the montmorillonite is 0.2-1 um.

[0054] In a preferred embodiment, the particle size of the montmorillonite is 0.5 um.

[0055] In one embodiment, the montmorillonite purchasing manufacturer is Lingshou County Linda Mineral Products Processing Plant.

[0056] In one embodiment, the layered material is selected from at least one of graphene, talc, glass flakes, hydrotalcite, and mica powder.

[0057] In a preferred embodiment, the layered material is a composition of graphene, talc, and glass flakes, and the weight ratio thereof is (1.2-2):1:1.

[0058] In a more preferred embodiment, the weight ratio of graphene, talc and glass flakes is 1.8:1:1.

[0059] In a preferred embodiment, the graphene sheet diameter is 0.1-1 um.

[0060] In a more preferred embodiment, the graphene sheet diameter is 0.5 um.

[0061] In one embodiment, the graphene is purchased from Nanjing Jicang Nanotechnology Co., Ltd.

[0062] In a preferred embodiment, the talcum powder has a flake diameter of 1-10 um.

[0063] In a more preferred embodiment, the talcum powder has a flake diameter of 5 um.

[0064] In one embodiment, the talcum powder is purchased from Lingshou County Xingyuan Mineral Powder Processing Plant.

[0065] In a preferred embodiment, the diameter of the glass flakes is 1-10 um.

[0066] In a more preferred embodiment, the diameter of the glass flakes is 5 um.

[0067] In one embodiment, the glass flake purchasing manufacturer is Lingshou County Hengxin Mineral Products Processing Plant.

[0068] Glass flakes are a kind of filler with corrosion resistance, but the filler obtained by using glass flakes alone in this application has poor acid and alkali resistance; it may be because the individual glass flakes are easy to agglomerate in the system, destroying the internal structure of the filler and reducing its acid and alkali resistance. The applicant unexpectedly discovered that the use of a certain weight of graphene, talcum powder, and glass flakes in the system of the present invention can greatly increase the acid and alkali resistance of the filler. It may be because graphene and talcum powder have certain flexibility, which can be well combined with the flaky rigid glass flakes. The three can be well stacked in layers in the system, and there is almost no staggered stacking. It can be better resistant to acid and alkali. When the filler works in the tower, its internal structure will not be destroyed due to the long-term action of acid, which extends the service life of the filler.

[0069] In one embodiment, the raw materials of the filler further include 3-6 parts of glass fiber and carboxymethyl cellulose.

[0070] In a preferred embodiment, the weight ratio of the filler glass fiber and carboxymethyl cellulose is (2-4):1.

[0071] In a more preferred embodiment, the weight ratio of the filler glass fiber to carboxymethyl cellulose is 2.8:1.

[0072] In one embodiment, the glass fibers are chopped glass fibers.

[0073] In a preferred embodiment, the length of the chopped glass fibers is 1-5 mm.

[0074] In a more preferred embodiment, the length of the chopped glass fibers is 3 mm.

[0075] In one embodiment, the chopped glass fibers are purchased from Dongguan Qianzhao Composite Materials Co., Ltd.

[0076] In a preferred embodiment, the carboxymethyl cellulose is sodium carboxymethyl cellulose, and the content of the sodium carboxymethyl cellulose is greater than 99%.

[0077] In one embodiment, the sodium carboxymethyl cellulose is purchased from Jinan Kaisheng Chemical Co., Ltd.

[0078] Adding a certain amount of glass fiber to the system can increase the compressive strength of the filler. During the experiment, the applicant discovered that the use of a certain amount of carboxymethyl cellulose and glass fiber to work together can greatly increase the compressive strength of the filler. The applicant speculates that it may be because glass fiber can increase the resistance of the filler system to external forces to a certain extent, but its dispersibility with other components in the system is poor. Under the action of carboxymethyl cellulose, its dispersion in the system is increased. It may be because the long-chain alkyl on the carboxymethyl cellulose can drive the dispersion of glass fiber in the system to a certain extent, forming a force-bearing whole in the system, which increases the compressive strength of the filler.

[0079] Through a large number of studies, it is found that adding too much or too little glass fiber will affect the compressive strength of the filler. This may be because adding too much glass fiber will cause defects in the filler matrix and other raw material components in the filler cannot wrap it well, causing the glass fiber to form defects in the overall force-bearing structure in the system, thereby affecting the compressive strength of the filler.

[0080] In one embodiment, the nanomaterial includes nano-aluminum oxide and nano-silicon dioxide in a weight ratio of (2-5):1.

[0081] In a preferred embodiment, the nanomaterial includes nano-aluminum oxide and nano-silicon dioxide, and the weight ratio thereof is (3-4):1.

[0082] In a more preferred embodiment, the nano material includes nano-aluminum oxide and nano-silicon dioxide in a weight ratio of 3.2:1.

[0083] In a preferred embodiment, the aluminum oxide particle size is 10-100 nm.

[0084] In a more preferred embodiment, the particle size of aluminum oxide is 50 nm.

[0085] In one embodiment, the aluminum oxide is purchased from Hangzhou Hengna New Materials Co., Ltd.

[0086] In a preferred embodiment, the silica particle size is 10-30 nm.

[0087] In a more preferred embodiment, the silica particle size is 20 nm.

[0088] In one embodiment, the silicon dioxide is purchased from Shanghai Naio Nano Technology Co., Ltd.

[0089] In one embodiment, the nanomaterial further comprises nanomolecular sieve.

[0090] The nano molecular sieve is selected from one or more of silicon oxide nanospheres, titanium silicon molecular sieve TS-1, and SBA-15.

[0091] In one embodiment, the BET specific surface area of ​​the nanomolecular sieve is 550-600m 2 / g.

[0092] In a preferred embodiment, the nanomolecular sieve is SBA-15; the BET specific surface area of ​​the SBA-15 is 580 m 2 / g.

[0093] In one embodiment, the nano molecular sieve accounts for 20-50% of the weight of the nano material.

[0094] In a preferred embodiment, the nano molecular sieve accounts for 31.25% of the weight of the nano material.

[0095] In one embodiment, the SBA-15 is purchased from Jiangsu Xianfeng Nanomaterial Technology Co., Ltd.

[0096] In one embodiment, the raw material of the filler further includes an ionic liquid.

[0097] In one embodiment, the weight of the ionic liquid is 15-35% of the total weight of the nanomaterial and the glass fiber.

[0098] In a preferred embodiment, the weight of the ionic liquid is 20-30% of the total weight of the nanomaterial and the glass fiber.

[0099] In a more preferred embodiment, the weight of the ionic liquid is 25% of the total weight of the nanomaterial and the glass fiber.

[0100] In one embodiment, the anion of the ionic liquid is hexafluorophosphate or tetrafluoroborate.

[0101] In a preferred embodiment, the anion of the ionic liquid is hexafluorophosphate.

[0102] In one embodiment, the cation of the ionic liquid is an imidazolium ion.

[0103] In one embodiment, the structure of the ionic liquid is:

[0104]

[0105] In a preferred embodiment, R1 is (C6-C 16 ) is an alkyl group, and R2 is a methyl group.

[0106] In a preferred embodiment, the R1 is C 10 -C 14 of alkyl.

[0107] In a more preferred embodiment, said R1 is C 12 of alkyl.

[0108] In one embodiment, the ionic liquid is 1-dodecyl-3-methylimidazolium hexafluorophosphate; the CAS number of the 1-dodecyl-3-methylimidazolium hexafluorophosphate is 219947-93-0.

[0109] The applicant found that adding a certain proportion of nano-aluminum oxide and nano-silicon dioxide to the system can not only increase the acid and alkali resistance of the filler, but also increase the specific gravity of the final harvested acid solution. It may be because nano-aluminum oxide and nano-silicon dioxide have a large specific surface area, and dispersing them in the system makes the system have a higher interface effect, and the filler in the tower has a good mass transfer effect. The applicant unexpectedly found that when a certain amount of nano-molecular sieve is added as filler, the concentration effect of the waste acid is better. It may be because the nano-molecular sieve has good adsorption and desorption functions, can quickly transfer products, and its larger specific surface area further increases the surface effect.

[0110] The applicant found that the glass fiber and glass flakes are dispersed in the packing system, so that when the packing works in the tower, the specific gravity of the acid finally concentrated is reduced, which may be because the glass fiber and glass flakes belong to a rigid structure, which reduces the wettability of the packing to the acid solution. The applicant found that the wettability of the working acid solution with a certain long chain and methyl ionic liquid filler is used to obtain an acid with a higher specific gravity. It may be because the hydrophobic long-chain alkyl on the carboxymethyl cellulose and the ionic liquid with the same hydrophobic structure are mutually adsorbed, which realizes the dispersion of the glass fiber and the glass flake, and the ionic liquid with an anion of hexafluorophosphate or tetrafluoroboric acid has good thermal stability. In the process of high-temperature processing, it can open the graphene structure and talcum powder that are tightly packed together, and the wettability of the graphene and talcum powder with a high specific surface area is increased, thereby increasing the wettability of the packing. And the addition of ionic liquid also improves the service life of the packing to a certain extent, which may be because the ionic liquid with a cation of imidazole can increase the degradation temperature of clay and nanomaterials to a certain extent.

[0111] The preparation method of the second filler layer comprises the following steps:

[0112] ① Add ionic liquid, nanomaterial and layered material into a stirring device and mix for 5-30 minutes to obtain mixture A;

[0113] ② Add clay, calcined alumina, tea residue powder and alloy into mixture A and stir for 5-30 minutes to obtain mixture B;

[0114] ③Putting mixture B into a cemented carbide mold and pressing it to obtain a green body;

[0115] ④ Place the green body into a vacuum sintering furnace for calcination. The sintering furnace temperature is set to 1450°C and the holding time is 2 hours. Turn off the switch of the vacuum sintering furnace. After the temperature drops to room temperature, take out the prepared second filler layer.

[0116] Working principle of waste acid concentration treatment tower: dilute sulfuric acid is added into the tower body through the feeding port, the heating device of the tower body adjusts the temperature of the tower body to 55-65℃, and at the same time, the ultrasonic generator provides 80KHZ ultrasonic wave to turn the dilute sulfuric acid into mist-like dilute sulfuric acid water vapor, and hot air is added into the tower body through the hot air port to realize the convection of the dilute sulfuric acid water vapor. When the dilute sulfuric acid water vapor passes through the packing layer, part of the water vapor is cooled into a droplet state, refluxes to the bottom of the tower and mixes with the concentrated acid, and part of the water vapor directly enters the exhaust port in the form of water vapor.

[0117] Example

[0118] Example 1

[0119] A waste acid concentration treatment tower, such as Figure 1 As shown, it includes a tower body 1, an exhaust port 2 is provided on the top of the tower body 1, a packing layer is provided in the middle of the tower body 1, an air inlet 6 is provided on one side below the tower body 1, and a heating device 9 is connected to the bottom of the tower body 1.

[0120] The packing layer comprises a first packing layer 3, a second packing layer 4, and a third packing layer 5; the first packing layer 3, the second packing layer 4, and the third packing layer 5 are respectively located at the upper, middle, and lower positions of the packing layer.

[0121] An ultrasonic generator 10 is connected to the bottom of the heating device 9; a feeding port 7 is provided on the lower side of the tower body 1; a discharge port 8 is provided on the lower side of the feeding port 7; the air inlet 6 is located on the lower side of the tower body 1 away from the feeding port 7 and the discharge port 8, and the height of the air inlet 6 is greater than the height of the feeding port 7; the heating temperature of the heating device 9 is 60°C.

[0122] The height ratio of the first packing layer 3 , the second packing layer 4 , and the third packing layer 5 is 1.25:2:1.

[0123] The first packing layer is a circular polytetrafluoroethylene perforated plate corrugated packing; the packing of the second packing layer is an inorganic packing; and the third packing layer is a circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing.

[0124] The circular polytetrafluoroethylene orifice plate corrugated packing was purchased from Jiangxi Pingxiang Kelong Petrochemical Equipment Packing Co., Ltd., model SB-250Y; the circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing was purchased from Anping County Hualai Metal Wire Mesh Co., Ltd., model 700 (CY).

[0125] The raw materials of the inorganic filler include the following components by weight: 23.5 parts of kaolin, 7 parts of attapulgite, 4.5 parts of montmorillonite, 15 parts of calcined alumina, 1.5 parts of aluminum oxide, 0.5 parts of silicon dioxide, 3 parts of SBA-15, 1.7 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 1.95 parts of graphene, 1.05 parts of talc, 1.05 parts of glass flakes, 3 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy.

[0126] The preparation method of the second filler layer comprises the following steps:

[0127] ① Add 1.7 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 1.5 parts of aluminum oxide, 0.5 parts of silicon dioxide, 3 parts of SBA-15, 1.95 parts of graphene, 1.05 parts of talc, and 1.05 parts of glass flakes into a stirring device and mix for 20 minutes to obtain a mixture A;

[0128] ② Add 23.5 parts of kaolin, 7 parts of attapulgite, 4.5 parts of montmorillonite, 15 parts of calcined alumina, 3 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy to mixture A and stir for 10 minutes to obtain mixture B;

[0129] ③Putting mixture B into a cemented carbide mold and pressing it to obtain a green body;

[0130] ④ Place the green body into a vacuum sintering furnace for calcination. The sintering furnace temperature is set to 1450°C and the holding time is 2 hours. Turn off the switch of the vacuum sintering furnace. After the temperature drops to room temperature, take out the prepared second filler layer.

[0131] The weight ratio of the glass fiber to the carboxymethyl cellulose is 2.5:1.

[0132] The particle size of the kaolin is 23um; the particle size of the attapulgite is 25um; the particle size of the montmorillonite is 0.5um; the particle size of the calcined alumina is 45um; the particle size of the aluminum oxide is 50nm; the particle size of the silicon dioxide is 20nm; the BET specific surface area of ​​the SBA-15 is 580m2 / g; the flake diameter of the graphene is 0.5um; the flake diameter of the talcum powder is 5um; the flake diameter of the glass flake is 5um; the length of the chopped glass fiber is 3mm; the content of the sodium carboxymethyl cellulose is greater than 99%.

[0133] The kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the attapulgite was purchased from Lingshou County Qiangdong Mineral Products Processing Plant, with a specification of qd-015; the kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the calcined alumina was purchased from Hebei Hengguang Mineral Products Co., Ltd., with an alumina content greater than 99%; the aluminum oxide was purchased from Hangzhou Hengna New Materials Co., Ltd.; the silicon dioxide was purchased from Shanghai Naio Nano Technology Co., Ltd.; the SBA-15 was purchased from Jiangsu Xianfeng Nano Materials Technology Co., Ltd.; the graphene was purchased from Nanjing Jichang Nano Technology Co., Ltd.; the talc was purchased from Lingshou County Xingyuan Mineral Powder Processing Plant; the glass flakes were purchased from Lingshou County Hengxin Mineral Products Processing Plant; the chopped glass fiber was purchased from Dongguan Qianzhao Composite Materials Co., Ltd.; the sodium carboxymethyl cellulose was purchased from Jinan Kaisheng Chemical Co., Ltd.; the cobalt-based alloy was purchased from Nangong Yingtai Metal Materials Co., Ltd., with a specification of Co6.

[0134] Example 2

[0135] A waste acid concentration treatment tower, such as Figure 1 As shown, it includes a tower body 1, an exhaust port 2 is provided on the top of the tower body 1, a packing layer is provided in the middle of the tower body 1, an air inlet 6 is provided on one side below the tower body 1, and a heating device 9 is connected to the bottom of the tower body 1.

[0136] The packing layer comprises a first packing layer 3, a second packing layer 4, and a third packing layer 5; the first packing layer 3, the second packing layer 4, and the third packing layer 5 are respectively located at the upper, middle, and lower positions of the packing layer.

[0137] An ultrasonic generator 10 is connected to the bottom of the heating device 9; a feeding port 7 is provided on the lower side of the tower body 1; a discharge port 8 is provided on the lower side of the feeding port 7; the air inlet 6 is located on the lower side of the tower body 1 away from the feeding port 7 and the discharge port 8, and the height of the air inlet 6 is greater than the height of the feeding port 7; the heating temperature of the heating device 9 is 60°C.

[0138] The height ratio of the first packing layer 3 , the second packing layer 4 , and the third packing layer 5 is 1.25:2:1.

[0139] The first packing layer is a circular polytetrafluoroethylene perforated plate corrugated packing; the packing of the second packing layer is an inorganic packing; and the third packing layer is a circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing.

[0140] The circular polytetrafluoroethylene orifice plate corrugated packing was purchased from Jiangxi Pingxiang Kelong Petrochemical Equipment Packing Co., Ltd., model SB-250Y; the circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing was purchased from Anping County Hualai Metal Wire Mesh Co., Ltd., model 700 (CY).

[0141] The raw materials of the inorganic filler include the following components by weight: 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 2.7 parts of graphene, 1.5 parts of talc, 1.5 parts of glass flakes, 4.75 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy.

[0142] The preparation method of the second filler layer comprises the following steps:

[0143] ① Add 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 2.7 parts of graphene, 1.5 parts of talc, and 1.5 parts of glass flakes into a stirring device and mix for 20 minutes to obtain a mixture A;

[0144] ② Add 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 4.75 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy to mixture A and stir for 10 minutes to obtain mixture B;

[0145] ③Putting mixture B into a cemented carbide mold and pressing it to obtain a green body;

[0146] ④ Place the green body into a vacuum sintering furnace for calcination. The sintering furnace temperature is set to 1450°C and the holding time is 2 hours. Turn off the switch of the vacuum sintering furnace. After the temperature drops to room temperature, take out the prepared second filler layer.

[0147] The weight ratio of the glass fiber to the carboxymethyl cellulose is 2.8:1.

[0148] The particle size of the kaolin is 23um; the particle size of the attapulgite is 25um; the particle size of the montmorillonite is 0.5um; the particle size of the calcined alumina is 45um; the particle size of the aluminum oxide is 50nm; the particle size of the silicon dioxide is 20nm; the BET specific surface area of ​​the SBA-15 is 580m 2 / g; the flake diameter of the graphene is 0.5um; the flake diameter of the talcum powder is 5um; the flake diameter of the glass flake is 5um; the length of the chopped glass fiber is 3mm; the content of the sodium carboxymethyl cellulose is greater than 99%.

[0149] The kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the attapulgite was purchased from Lingshou County Qiangdong Mineral Products Processing Plant, with a specification of qd-015; the kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the calcined alumina was purchased from Hebei Hengguang Mineral Products Co., Ltd., with an alumina content greater than 99%; the aluminum oxide was purchased from Hangzhou Hengna New Materials Co., Ltd.; the silicon dioxide was purchased from Shanghai Naio Nano Technology Co., Ltd.; the SBA-15 was purchased from Jiangsu Xianfeng Nano Materials Technology Co., Ltd.; the graphene was purchased from Nanjing Jichang Nano Technology Co., Ltd.; the talc was purchased from Lingshou County Xingyuan Mineral Powder Processing Plant; the glass flakes were purchased from Lingshou County Hengxin Mineral Products Processing Plant; the chopped glass fiber was purchased from Dongguan Qianzhao Composite Materials Co., Ltd.; the sodium carboxymethyl cellulose was purchased from Jinan Kaisheng Chemical Co., Ltd.; the cobalt-based alloy was purchased from Nangong Yingtai Metal Materials Co., Ltd., with a specification of Co6.

[0150] Example 3

[0151] A waste acid concentration treatment tower, such as Figure 1 As shown, it includes a tower body 1, an exhaust port 2 is provided on the top of the tower body 1, a packing layer is provided in the middle of the tower body 1, an air inlet 6 is provided on one side below the tower body 1, and a heating device 9 is connected to the bottom of the tower body 1.

[0152] The packing layer comprises a first packing layer 3, a second packing layer 4, and a third packing layer 5; the first packing layer 3, the second packing layer 4, and the third packing layer 5 are respectively located at the upper, middle, and lower positions of the packing layer.

[0153] An ultrasonic generator 10 is connected to the bottom of the heating device 9; a feeding port 7 is provided on the lower side of the tower body 1; a discharge port 8 is provided on the lower side of the feeding port 7; the air inlet 6 is located on the lower side of the tower body 1 away from the feeding port 7 and the discharge port 8, and the height of the air inlet 6 is greater than the height of the feeding port 7; the heating temperature of the heating device 9 is 60°C.

[0154] The height ratio of the first packing layer 3 , the second packing layer 4 , and the third packing layer 5 is 1.25:2:1.

[0155] The first packing layer is a circular polytetrafluoroethylene perforated plate corrugated packing; the packing of the second packing layer is an inorganic packing; and the third packing layer is a circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing.

[0156] The circular polytetrafluoroethylene orifice plate corrugated packing was purchased from Jiangxi Pingxiang Kelong Petrochemical Equipment Packing Co., Ltd., model SB-250Y; the circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing was purchased from Anping County Hualai Metal Wire Mesh Co., Ltd., model 700 (CY).

[0157] The raw materials of the inorganic filler include the following components by weight: 33.5 parts of kaolin, 10 parts of attapulgite, 6.5 parts of montmorillonite, 30 parts of calcined alumina, 7 parts of aluminum oxide, 2 parts of silicon dioxide, 3 parts of SBA-15, 4.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 3.4 parts of graphene, 1.8 parts of talc, 1.8 parts of glass flakes, 6 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy.

[0158] The preparation method of the second filler layer comprises the following steps:

[0159] ① Add 4.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 7 parts of aluminum oxide, 2 parts of silicon dioxide, 3 parts of SBA-15, 3.4 parts of graphene, 1.8 parts of talc and 1.8 parts of glass flakes into a stirring device and mix for 20 minutes to obtain a mixture A;

[0160] ② Add 33.5 parts of kaolin, 10 parts of attapulgite, 6.5 parts of montmorillonite, 30 parts of calcined alumina, 6 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder and 2 parts of cobalt-based alloy to mixture A and stir for 10 minutes to obtain mixture B;

[0161] ③Putting mixture B into a cemented carbide mold and pressing it to obtain a green body;

[0162] ④ Place the green body into a vacuum sintering furnace for calcination. The sintering furnace temperature is set to 1450°C and the holding time is 2 hours. Turn off the switch of the vacuum sintering furnace. After the temperature drops to room temperature, take out the prepared second filler layer.

[0163] The weight ratio of the glass fiber to the carboxymethyl cellulose is 3.2:1.

[0164] The particle size of the kaolin is 23um; the particle size of the attapulgite is 25um; the particle size of the montmorillonite is 0.5um; the particle size of the calcined alumina is 45um; the particle size of the aluminum oxide is 50nm; the particle size of the silicon dioxide is 20nm; the BET specific surface area of ​​the SBA-15 is 580m 2 / g; the flake diameter of the graphene is 0.5um; the flake diameter of the talcum powder is 5um; the flake diameter of the glass flake is 5um; the length of the chopped glass fiber is 3mm; the content of the sodium carboxymethyl cellulose is greater than 99%.

[0165] The kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the attapulgite was purchased from Lingshou County Qiangdong Mineral Products Processing Plant, with a specification of qd-015; the kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the calcined alumina was purchased from Hebei Hengguang Mineral Products Co., Ltd., with an alumina content greater than 99%; the aluminum oxide was purchased from Hangzhou Hengna New Materials Co., Ltd.; the silicon dioxide was purchased from Shanghai Naio Nano Technology Co., Ltd.; the SBA-15 was purchased from Jiangsu Xianfeng Nano Materials Technology Co., Ltd.; the graphene was purchased from Nanjing Jichang Nano Technology Co., Ltd.; the talc was purchased from Lingshou County Xingyuan Mineral Powder Processing Plant; the glass flakes were purchased from Lingshou County Hengxin Mineral Products Processing Plant; the chopped glass fiber was purchased from Dongguan Qianzhao Composite Materials Co., Ltd.; the sodium carboxymethyl cellulose was purchased from Jinan Kaisheng Chemical Co., Ltd.; the cobalt-based alloy was purchased from Nangong Yingtai Metal Materials Co., Ltd., with a specification of Co6.

[0166] Example 4

[0167] A waste acid concentration treatment tower, such as Figure 1 As shown, it includes a tower body 1, an exhaust port 2 is provided on the top of the tower body 1, a packing layer is provided in the middle of the tower body 1, an air inlet 6 is provided on one side below the tower body 1, and a heating device 9 is connected to the bottom of the tower body 1.

[0168] The packing layer comprises a first packing layer 3, a second packing layer 4, and a third packing layer 5; the first packing layer 3, the second packing layer 4, and the third packing layer 5 are respectively located at the upper, middle, and lower positions of the packing layer.

[0169] An ultrasonic generator 10 is connected to the bottom of the heating device 9; a feeding port 7 is provided on the lower side of the tower body 1; a discharge port 8 is provided on the lower side of the feeding port 7; the air inlet 6 is located on the lower side of the tower body 1 away from the feeding port 7 and the discharge port 8, and the height of the air inlet 6 is greater than the height of the feeding port 7; the heating temperature of the heating device 9 is 60°C.

[0170] The height ratio of the first packing layer 3 , the second packing layer 4 , and the third packing layer 5 is 1.25:2:1.

[0171] The first packing layer is a circular polytetrafluoroethylene perforated plate corrugated packing; the packing of the second packing layer is an inorganic packing; and the third packing layer is a circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing.

[0172] The circular polytetrafluoroethylene orifice plate corrugated packing was purchased from Jiangxi Pingxiang Kelong Petrochemical Equipment Packing Co., Ltd., model SB-250Y; the circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing was purchased from Anping County Hualai Metal Wire Mesh Co., Ltd., model 700 (CY).

[0173] The raw materials of the inorganic filler include the following components by weight: 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 2.7 parts of graphene, 1.5 parts of talc, 1.5 parts of glass flakes, 4.75 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy.

[0174] The preparation method of the second filler layer comprises the following steps:

[0175] ① Add 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 2.7 parts of graphene, 1.5 parts of talc, and 1.5 parts of glass flakes into a stirring device and mix for 20 minutes to obtain a mixture A;

[0176] ② Add 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 4.75 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy to mixture A and stir for 10 minutes to obtain mixture B;

[0177] ③Putting mixture B into a cemented carbide mold and pressing it to obtain a green body;

[0178] ④ Place the green body into a vacuum sintering furnace for calcination. The sintering furnace temperature is set to 1450°C and the holding time is 2 hours. Turn off the switch of the vacuum sintering furnace. After the temperature drops to room temperature, take out the prepared second filler layer.

[0179] The weight ratio of the glass fiber to the carboxymethyl cellulose is 2.8:1.

[0180] The particle size of kaolin is 23um; the particle size of attapulgite is 25um; the particle size of montmorillonite is 0.5um; the particle size of calcined alumina is 45um; the particle size of aluminum oxide is 50nm; the particle size of silicon dioxide is 20nm; the flake diameter of graphene is 0.5um; the flake diameter of talcum powder is 5um; the flake diameter of glass flake is 5um; the length of chopped glass fiber is 3mm; the content of sodium carboxymethyl cellulose is greater than 99%.

[0181] The kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the attapulgite was purchased from Lingshou County Qiangdong Mineral Products Processing Plant, with a specification of qd-015; the kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the calcined alumina was purchased from Hebei Hengguang Mineral Products Co., Ltd., with an alumina content greater than 99%; the aluminum oxide was purchased from Hangzhou Hengna New Materials Co., Ltd.; the silicon dioxide was purchased from Shanghai Naio Nano Technology Co., Ltd.; the graphene was purchased from Nanjing Jichang Nano Technology Co., Ltd.; the talc was purchased from Lingshou County Xingyuan Mineral Powder Processing Plant; the glass flakes were purchased from Lingshou County Hengxin Mineral Products Processing Plant; the chopped glass fiber was purchased from Dongguan Qianzhao Composite Materials Co., Ltd.; the sodium carboxymethyl cellulose was purchased from Jinan Kaisheng Chemical Co., Ltd.; the cobalt-based alloy was purchased from Nangong Yingtai Metal Materials Co., Ltd., with a specification of Co6.

[0182] Example 5

[0183] A waste acid concentration treatment tower, such as Figure 1 As shown, it includes a tower body 1, an exhaust port 2 is provided on the top of the tower body 1, a packing layer is provided in the middle of the tower body 1, an air inlet 6 is provided on one side below the tower body 1, and a heating device 9 is connected to the bottom of the tower body 1.

[0184] The packing layer comprises a first packing layer 3, a second packing layer 4, and a third packing layer 5; the first packing layer 3, the second packing layer 4, and the third packing layer 5 are respectively located at the upper, middle, and lower positions of the packing layer.

[0185] An ultrasonic generator 10 is connected to the bottom of the heating device 9; a feeding port 7 is provided on the lower side of the tower body 1; a discharge port 8 is provided on the lower side of the feeding port 7; the air inlet 6 is located on the lower side of the tower body 1 away from the feeding port 7 and the discharge port 8, and the height of the air inlet 6 is greater than the height of the feeding port 7; the heating temperature of the heating device 9 is 60°C.

[0186] The height ratio of the first packing layer 3 , the second packing layer 4 , and the third packing layer 5 is 1.25:2:1.

[0187] The first packing layer is a circular polytetrafluoroethylene perforated plate corrugated packing; the packing of the second packing layer is an inorganic packing; and the third packing layer is a circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing.

[0188] The circular polytetrafluoroethylene orifice plate corrugated packing was purchased from Jiangxi Pingxiang Kelong Petrochemical Equipment Packing Co., Ltd., model SB-250Y; the circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing was purchased from Anping County Hualai Metal Wire Mesh Co., Ltd., model 700 (CY).

[0189] The raw materials of the inorganic filler include the following components by weight: 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 1.5 parts of glass flakes, 4.75 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy.

[0190] The preparation method of the second filler layer comprises the following steps:

[0191] ① Add 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, and 1.5 parts of glass flakes into a stirring device and mix for 20 minutes to obtain a mixture A;

[0192] ② Add 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 4.75 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy to mixture A and stir for 10 minutes to obtain mixture B;

[0193] ③Putting mixture B into a cemented carbide mold and pressing it to obtain a green body;

[0194] ④ Place the green body into a vacuum sintering furnace for calcination. The sintering furnace temperature is set to 1450°C and the holding time is 2 hours. Turn off the switch of the vacuum sintering furnace. After the temperature drops to room temperature, take out the prepared second filler layer.

[0195] The weight ratio of the glass fiber to the carboxymethyl cellulose is 2.8:1.

[0196] The particle size of the kaolin is 23um; the particle size of the attapulgite is 25um; the particle size of the montmorillonite is 0.5um; the particle size of the calcined alumina is 45um; the particle size of the aluminum oxide is 50nm; the particle size of the silicon dioxide is 20nm; the BET specific surface area of ​​the SBA-15 is 580m 2 / g; the diameter of the glass flakes is 5um; the length of the chopped glass fibers is 3mm; and the content of the sodium carboxymethyl cellulose is greater than 99%.

[0197] The kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the attapulgite was purchased from Lingshou County Qiangdong Mineral Products Processing Plant, with a specification of qd-015; the kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the calcined alumina was purchased from Hebei Hengguang Mineral Products Co., Ltd., with an alumina content greater than 99%; the aluminum oxide was purchased from Hangzhou Hengna New Materials Co., Ltd.; the silicon dioxide was purchased from Shanghai Naio Nano Technology Co., Ltd.; the SBA-15 was purchased from Jiangsu Xianfeng Nano Materials Technology Co., Ltd.; the glass flakes were purchased from Lingshou County Hengxin Mineral Products Processing Plant; the chopped glass fibers were purchased from Dongguan Qianzhao Composite Materials Co., Ltd.; the sodium carboxymethyl cellulose was purchased from Jinan Kaisheng Chemical Co., Ltd.; the cobalt-based alloy was purchased from Nangong Yingtai Metal Materials Co., Ltd., with a specification of Co6.

[0198] Example 6

[0199] A waste acid concentration treatment tower, such as Figure 1 As shown, it includes a tower body 1, an exhaust port 2 is provided on the top of the tower body 1, a packing layer is provided in the middle of the tower body 1, an air inlet 6 is provided on one side below the tower body 1, and a heating device 9 is connected to the bottom of the tower body 1.

[0200] The packing layer comprises a first packing layer 3, a second packing layer 4, and a third packing layer 5; the first packing layer 3, the second packing layer 4, and the third packing layer 5 are respectively located at the upper, middle, and lower positions of the packing layer.

[0201] An ultrasonic generator 10 is connected to the bottom of the heating device 9; a feeding port 7 is provided on the lower side of the tower body 1; a discharge port 8 is provided on the lower side of the feeding port 7; the air inlet 6 is located on the lower side of the tower body 1 away from the feeding port 7 and the discharge port 8, and the height of the air inlet 6 is greater than the height of the feeding port 7; the heating temperature of the heating device 9 is 60°C.

[0202] The height ratio of the first packing layer 3 , the second packing layer 4 , and the third packing layer 5 is 1.25:2:1.

[0203] The first packing layer is a circular polytetrafluoroethylene perforated plate corrugated packing; the packing of the second packing layer is an inorganic packing; and the third packing layer is a circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing.

[0204] The circular polytetrafluoroethylene orifice plate corrugated packing was purchased from Jiangxi Pingxiang Kelong Petrochemical Equipment Packing Co., Ltd., model SB-250Y; the circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing was purchased from Anping County Hualai Metal Wire Mesh Co., Ltd., model 700 (CY).

[0205] The raw materials of the inorganic filler include the following components by weight: 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 2.7 parts of graphene, 1.5 parts of talc, 1.5 parts of glass flakes, 7.25 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy.

[0206] The preparation method of the second filler layer comprises the following steps:

[0207] ① Add 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 2.7 parts of graphene, 1.5 parts of talc, and 1.5 parts of glass flakes into a stirring device and mix for 20 minutes to obtain a mixture A;

[0208] ② Add 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 7.25 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy to mixture A and stir for 10 minutes to obtain mixture B;

[0209] ③Putting mixture B into a cemented carbide mold and pressing it to obtain a green body;

[0210] ④ Place the green body into a vacuum sintering furnace for calcination. The sintering furnace temperature is set to 1450°C and the holding time is 2 hours. Turn off the switch of the vacuum sintering furnace. After the temperature drops to room temperature, take out the prepared second filler layer.

[0211] The weight ratio of the glass fiber to the carboxymethyl cellulose is 4.8:1.

[0212] The particle size of the kaolin is 23um; the particle size of the attapulgite is 25um; the particle size of the montmorillonite is 0.5um; the particle size of the calcined alumina is 45um; the particle size of the aluminum oxide is 50nm; the particle size of the silicon dioxide is 20nm; the BET specific surface area of ​​the SBA-15 is 580m 2 / g; the flake diameter of the graphene is 0.5um; the flake diameter of the talcum powder is 5um; the flake diameter of the glass flake is 5um; the length of the chopped glass fiber is 3mm; the content of the sodium carboxymethyl cellulose is greater than 99%.

[0213] The kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the attapulgite was purchased from Lingshou County Qiangdong Mineral Products Processing Plant, with a specification of qd-015; the kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the calcined alumina was purchased from Hebei Hengguang Mineral Products Co., Ltd., with an alumina content greater than 99%; the aluminum oxide was purchased from Hangzhou Hengna New Materials Co., Ltd.; the silicon dioxide was purchased from Shanghai Naio Nano Technology Co., Ltd.; the SBA-15 was purchased from Jiangsu Xianfeng Nano Materials Technology Co., Ltd.; the graphene was purchased from Nanjing Jichang Nano Technology Co., Ltd.; the talc was purchased from Lingshou County Xingyuan Mineral Powder Processing Plant; the glass flakes were purchased from Lingshou County Hengxin Mineral Products Processing Plant; the chopped glass fiber was purchased from Dongguan Qianzhao Composite Materials Co., Ltd.; the sodium carboxymethyl cellulose was purchased from Jinan Kaisheng Chemical Co., Ltd.; the cobalt-based alloy was purchased from Nangong Yingtai Metal Materials Co., Ltd., with a specification of Co6.

[0214] Example 7

[0215] A waste acid concentration treatment tower, such as Figure 1 As shown, it includes a tower body 1, an exhaust port 2 is provided on the top of the tower body 1, a packing layer is provided in the middle of the tower body 1, an air inlet 6 is provided on one side below the tower body 1, and a heating device 9 is connected to the bottom of the tower body 1.

[0216] The packing layer comprises a first packing layer 3, a second packing layer 4, and a third packing layer 5; the first packing layer 3, the second packing layer 4, and the third packing layer 5 are respectively located at the upper, middle, and lower positions of the packing layer.

[0217] An ultrasonic generator 10 is connected to the bottom of the heating device 9; a feeding port 7 is provided on the lower side of the tower body 1; a discharge port 8 is provided on the lower side of the feeding port 7; the air inlet 6 is located on the lower side of the tower body 1 away from the feeding port 7 and the discharge port 8, and the height of the air inlet 6 is greater than the height of the feeding port 7; the heating temperature of the heating device 9 is 60°C.

[0218] The height ratio of the first packing layer 3 , the second packing layer 4 , and the third packing layer 5 is 1.25:2:1.

[0219] The first packing layer is a circular polytetrafluoroethylene perforated plate corrugated packing; the packing of the second packing layer is an inorganic packing; and the third packing layer is a circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing.

[0220] The circular polytetrafluoroethylene orifice plate corrugated packing was purchased from Jiangxi Pingxiang Kelong Petrochemical Equipment Packing Co., Ltd., model SB-250Y; the circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing was purchased from Anping County Hualai Metal Wire Mesh Co., Ltd., model 700 (CY).

[0221] The raw materials of the inorganic filler include the following components by weight: 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 2.7 parts of graphene, 1.5 parts of talc, 1.5 parts of glass flakes, 3.25 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy.

[0222] The preparation method of the second filler layer comprises the following steps:

[0223] ① Add 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 2.7 parts of graphene, 1.5 parts of talc, and 1.5 parts of glass flakes into a stirring device and mix for 20 minutes to obtain a mixture A;

[0224] ② Add 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 3.25 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy to mixture A and stir for 10 minutes to obtain mixture B;

[0225] ③Putting mixture B into a cemented carbide mold and pressing it to obtain a green body;

[0226] ④ Place the green body into a vacuum sintering furnace for calcination. The sintering furnace temperature is set to 1450°C and the holding time is 2 hours. Turn off the switch of the vacuum sintering furnace. After the temperature drops to room temperature, take out the prepared second filler layer.

[0227] The weight ratio of the glass fiber to the carboxymethyl cellulose is 1.6:1.

[0228] The particle size of the kaolin is 23um; the particle size of the attapulgite is 25um; the particle size of the montmorillonite is 0.5um; the particle size of the calcined alumina is 45um; the particle size of the aluminum oxide is 50nm; the particle size of the silicon dioxide is 20nm; the BET specific surface area of ​​the SBA-15 is 580m 2 / g; the flake diameter of the graphene is 0.5um; the flake diameter of the talcum powder is 5um; the flake diameter of the glass flake is 5um; the length of the chopped glass fiber is 3mm; the content of the sodium carboxymethyl cellulose is greater than 99%.

[0229] The kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the attapulgite was purchased from Lingshou County Qiangdong Mineral Products Processing Plant, with a specification of qd-015; the kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the calcined alumina was purchased from Hebei Hengguang Mineral Products Co., Ltd., with an alumina content greater than 99%; the aluminum oxide was purchased from Hangzhou Hengna New Materials Co., Ltd.; the silicon dioxide was purchased from Shanghai Naio Nano Technology Co., Ltd.; the SBA-15 was purchased from Jiangsu Xianfeng Nano Materials Technology Co., Ltd.; the graphene was purchased from Nanjing Jichang Nano Technology Co., Ltd.; the talc was purchased from Lingshou County Xingyuan Mineral Powder Processing Plant; the glass flakes were purchased from Lingshou County Hengxin Mineral Products Processing Plant; the chopped glass fiber was purchased from Dongguan Qianzhao Composite Materials Co., Ltd.; the sodium carboxymethyl cellulose was purchased from Jinan Kaisheng Chemical Co., Ltd.; the cobalt-based alloy was purchased from Nangong Yingtai Metal Materials Co., Ltd., with a specification of Co6.

[0230] Example 8

[0231] A waste acid concentration treatment tower, such as Figure 1 As shown, it includes a tower body 1, an exhaust port 2 is provided on the top of the tower body 1, a packing layer is provided in the middle of the tower body 1, an air inlet 6 is provided on one side below the tower body 1, and a heating device 9 is connected to the bottom of the tower body 1.

[0232] The packing layer comprises a first packing layer 3, a second packing layer 4, and a third packing layer 5; the first packing layer 3, the second packing layer 4, and the third packing layer 5 are respectively located at the upper, middle, and lower positions of the packing layer.

[0233] An ultrasonic generator 10 is connected to the bottom of the heating device 9; a feeding port 7 is provided on the lower side of the tower body 1; a discharge port 8 is provided on the lower side of the feeding port 7; the air inlet 6 is located on the lower side of the tower body 1 away from the feeding port 7 and the discharge port 8, and the height of the air inlet 6 is greater than the height of the feeding port 7; the heating temperature of the heating device 9 is 60°C.

[0234] The height ratio of the first packing layer 3 , the second packing layer 4 , and the third packing layer 5 is 1.25:2:1.

[0235] The first packing layer is a circular polytetrafluoroethylene perforated plate corrugated packing; the packing of the second packing layer is an inorganic packing; and the third packing layer is a circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing.

[0236] The circular polytetrafluoroethylene orifice plate corrugated packing was purchased from Jiangxi Pingxiang Kelong Petrochemical Equipment Packing Co., Ltd., model SB-250Y; the circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing was purchased from Anping County Hualai Metal Wire Mesh Co., Ltd., model 700 (CY).

[0237] The raw materials of the inorganic filler include the following components by weight: 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 2.7 parts of graphene, 1.5 parts of talc, 1.5 parts of glass flakes, 4.75 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy.

[0238] The preparation method of the second filler layer comprises the following steps:

[0239] ① Add 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 2.7 parts of graphene, 1.5 parts of talc, and 1.5 parts of glass flakes into a stirring device and mix for 20 minutes to obtain a mixture A;

[0240] ② Add 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 4.75 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy to mixture A and stir for 10 minutes to obtain mixture B;

[0241] ③Putting mixture B into a cemented carbide mold and pressing it to obtain a green body;

[0242] ④ Place the green body into a vacuum sintering furnace for calcination. The sintering furnace temperature is set to 1450°C and the holding time is 2 hours. Turn off the switch of the vacuum sintering furnace. After the temperature drops to room temperature, take out the prepared second filler layer.

[0243] The weight ratio of the glass fiber to the carboxymethyl cellulose is 2.8:1.

[0244] The particle size of the kaolin is 23um; the particle size of the attapulgite is 25um; the particle size of the montmorillonite is 0.5um; the particle size of the calcined alumina is 45um; the particle size of the aluminum oxide is 50nm; the particle size of the silicon dioxide is 20nm; the BET specific surface area of ​​the SBA-15 is 580m 2 / g; the flake diameter of the graphene is 0.5um; the flake diameter of the talcum powder is 5um; the flake diameter of the glass flake is 5um; the length of the chopped glass fiber is 3mm; the content of the sodium carboxymethyl cellulose is greater than 99%.

[0245] The kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the attapulgite was purchased from Lingshou County Qiangdong Mineral Products Processing Plant, with a specification of qd-015; the kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the calcined alumina was purchased from Hebei Hengguang Mineral Products Co., Ltd., with an alumina content greater than 99%; the aluminum oxide was purchased from Hangzhou Hengna New Materials Co., Ltd.; the silicon dioxide was purchased from Shanghai Naio Nano Technology Co., Ltd.; the SBA-15 was purchased from Jiangsu Xianfeng Nano Materials Technology Co., Ltd.; the graphene was purchased from Nanjing Jichang Nano Technology Co., Ltd.; the talc was purchased from Lingshou County Xingyuan Mineral Powder Processing Plant; the glass flakes were purchased from Lingshou County Hengxin Mineral Products Processing Plant; the chopped glass fiber was purchased from Dongguan Qianzhao Composite Materials Co., Ltd.; the sodium carboxymethyl cellulose was purchased from Jinan Kaisheng Chemical Co., Ltd.; the cobalt-based alloy was purchased from Nangong Yingtai Metal Materials Co., Ltd., with a specification of Co6.

[0246] Example 9

[0247] A waste acid concentration treatment tower, such as Figure 1 As shown, it includes a tower body 1, an exhaust port 2 is provided on the top of the tower body 1, a packing layer is provided in the middle of the tower body 1, an air inlet 6 is provided on one side below the tower body 1, and a heating device 9 is connected to the bottom of the tower body 1.

[0248] The packing layer comprises a first packing layer 3, a second packing layer 4, and a third packing layer 5; the first packing layer 3, the second packing layer 4, and the third packing layer 5 are respectively located at the upper, middle, and lower positions of the packing layer.

[0249] An ultrasonic generator 10 is connected to the bottom of the heating device 9; a feeding port 7 is provided on the lower side of the tower body 1; a discharge port 8 is provided on the lower side of the feeding port 7; the air inlet 6 is located on the lower side of the tower body 1 away from the feeding port 7 and the discharge port 8, and the height of the air inlet 6 is greater than the height of the feeding port 7; the heating temperature of the heating device 9 is 60°C.

[0250] The height ratio of the first packing layer 3 , the second packing layer 4 , and the third packing layer 5 is 1.25:2:1.

[0251] The first packing layer is a circular polytetrafluoroethylene perforated plate corrugated packing; the packing of the second packing layer is an inorganic packing; and the third packing layer is a circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing.

[0252] The circular polytetrafluoroethylene orifice plate corrugated packing was purchased from Jiangxi Pingxiang Kelong Petrochemical Equipment Packing Co., Ltd., model SB-250Y; the circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing was purchased from Anping County Hualai Metal Wire Mesh Co., Ltd., model 700 (CY).

[0253] The raw materials of the inorganic filler include the following components by weight: 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 3.1 parts of 1-butyl-3-methylimidazole hexafluorophosphate, 2.7 parts of graphene, 1.5 parts of talc, 1.5 parts of glass flakes, 4.75 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy.

[0254] The preparation method of the second filler layer comprises the following steps:

[0255] ① Add 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 2.7 parts of graphene, 1.5 parts of talc, and 1.5 parts of glass flakes into a stirring device and mix for 20 minutes to obtain a mixture A;

[0256] ② Add 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 4.75 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy to mixture A and stir for 10 minutes to obtain mixture B;

[0257] ③Putting mixture B into a cemented carbide mold and pressing it to obtain a green body;

[0258] ④ Place the green body into a vacuum sintering furnace for calcination. The sintering furnace temperature is set to 1450°C and the holding time is 2 hours. Turn off the switch of the vacuum sintering furnace. After the temperature drops to room temperature, take out the prepared second filler layer.

[0259] The weight ratio of the glass fiber to the carboxymethyl cellulose is 2.8:1.

[0260] The particle size of the kaolin is 23um; the particle size of the attapulgite is 25um; the particle size of the montmorillonite is 0.5um; the particle size of the calcined alumina is 45um; the particle size of the aluminum oxide is 50nm; the particle size of the silicon dioxide is 20nm; the BET specific surface area of ​​the SBA-15 is 580m 2 / g; the flake diameter of the graphene is 0.5um; the flake diameter of the talcum powder is 5um; the flake diameter of the glass flake is 5um; the length of the chopped glass fiber is 3mm; the content of the sodium carboxymethyl cellulose is greater than 99%.

[0261] The kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the attapulgite was purchased from Lingshou County Qiangdong Mineral Products Processing Plant, with a specification of qd-015; the kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the calcined alumina was purchased from Hebei Hengguang Mineral Products Co., Ltd., with an alumina content greater than 99%; the aluminum oxide was purchased from Hangzhou Hengna New Materials Co., Ltd.; the silicon dioxide was purchased from Shanghai Naio Nano Technology Co., Ltd.; the SBA-15 was purchased from Jiangsu Xianfeng Nano Materials Technology Co., Ltd.; the graphene was purchased from Nanjing Jichang Nano Technology Co., Ltd.; the talc was purchased from Lingshou County Xingyuan Mineral Powder Processing Plant; the glass flakes were purchased from Lingshou County Hengxin Mineral Products Processing Plant; the chopped glass fiber was purchased from Dongguan Qianzhao Composite Materials Co., Ltd.; the sodium carboxymethyl cellulose was purchased from Jinan Kaisheng Chemical Co., Ltd.; the cobalt-based alloy was purchased from Nangong Yingtai Metal Materials Co., Ltd., with a specification of Co6.

[0262] Example 10

[0263] A waste acid concentration treatment tower, such as Figure 1 As shown, it includes a tower body 1, an exhaust port 2 is provided on the top of the tower body 1, a packing layer is provided in the middle of the tower body 1, an air inlet 6 is provided on one side below the tower body 1, and a heating device 9 is connected to the bottom of the tower body 1.

[0264] The packing layer comprises a first packing layer 3, a second packing layer 4, and a third packing layer 5; the first packing layer 3, the second packing layer 4, and the third packing layer 5 are respectively located at the upper, middle, and lower positions of the packing layer.

[0265] An ultrasonic generator 10 is connected to the bottom of the heating device 9; a feeding port 7 is provided on the lower side of the tower body 1; a discharge port 8 is provided on the lower side of the feeding port 7; the air inlet 6 is located on the lower side of the tower body 1 away from the feeding port 7 and the discharge port 8, and the height of the air inlet 6 is greater than the height of the feeding port 7; the heating temperature of the heating device 9 is 60°C.

[0266] The height ratio of the first packing layer 3 , the second packing layer 4 , and the third packing layer 5 is 1.25:2:1.

[0267] The first packing layer is a circular polytetrafluoroethylene perforated plate corrugated packing; the packing of the second packing layer is an inorganic packing; and the third packing layer is a circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing.

[0268] The circular polytetrafluoroethylene orifice plate corrugated packing was purchased from Jiangxi Pingxiang Kelong Petrochemical Equipment Packing Co., Ltd., model SB-250Y; the circular chromium-nickel-molybdenum-copper alloy wire mesh corrugated packing was purchased from Anping County Hualai Metal Wire Mesh Co., Ltd., model 700 (CY).

[0269] The raw materials of the inorganic filler include the following components by weight: 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 2.7 parts of graphene, 1.5 parts of talc, 1.5 parts of glass flakes, 3.5 parts of glass fiber, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy.

[0270] The preparation method of the second filler layer comprises the following steps:

[0271] ① Add 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 2.7 parts of graphene, 1.5 parts of talc, and 1.5 parts of glass flakes into a stirring device and mix for 20 minutes to obtain a mixture A;

[0272] ② Add 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 3.5 parts of glass fiber, 3.5 parts of tea residue powder and 2 parts of cobalt-based alloy to mixture A and stir for 10 minutes to obtain mixture B;

[0273] ③Putting mixture B into a cemented carbide mold and pressing it to obtain a green body;

[0274] ④ Place the green body into a vacuum sintering furnace for calcination. The sintering furnace temperature is set to 1450°C and the holding time is 2 hours. Turn off the switch of the vacuum sintering furnace. After the temperature drops to room temperature, take out the prepared second filler layer.

[0275] The particle size of the kaolin is 23um; the particle size of the attapulgite is 25um; the particle size of the montmorillonite is 0.5um; the particle size of the calcined alumina is 45um; the particle size of the aluminum oxide is 50nm; the particle size of the silicon dioxide is 20nm; the BET specific surface area of ​​the SBA-15 is 580m 2 / g; the flake diameter of the graphene is 0.5um; the flake diameter of the talcum powder is 5um; the flake diameter of the glass flake is 5um; and the length of the chopped glass fiber is 3mm.

[0276] The kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the attapulgite was purchased from Lingshou County Qiangdong Mineral Products Processing Plant, with a specification of qd-015; the kaolin was purchased from Hebei Huanhe Mineral Products Co., Ltd., with a silicon dioxide content of 52%; the calcined alumina was purchased from Hebei Hengguang Mineral Products Co., Ltd., with an alumina content greater than 99%; the aluminum oxide was purchased from Hangzhou Hengna New Materials Co., Ltd.; the silicon dioxide was purchased from Shanghai Naio Nano Technology Co., Ltd.; the SBA-15 was purchased from Jiangsu Xianfeng Nano Materials Technology Co., Ltd.; the graphene was purchased from Nanjing Jichang Nano Technology Co., Ltd.; the talc was purchased from Lingshou County Xingyuan Mineral Powder Processing Plant; the glass flakes were purchased from Lingshou County Hengxin Mineral Products Processing Plant; the chopped glass fiber was purchased from Dongguan Qianzhao Composite Materials Co., Ltd.; the cobalt-based alloy was purchased from Nangong Yingtai Metal Materials Co., Ltd., with a specification of Co6.

[0277] Experimental Testing

[0278] 1. Compressive strength test

[0279] Test method: 50 groups of second-layer fillers prepared in Examples 1-10 were randomly selected as test pieces. The compressive strength of the test pieces was measured by axial compression using a PMT-150C rock mechanics testing system, and the average value of the 50 groups was taken.

[0280] 2. Acid resistance test

[0281] Five groups of second-layer fillers prepared in Examples 1-10 were randomly selected, their mass m1 was measured, and they were immersed in a 96 wt % concentrated sulfuric acid solution and slightly boiled for 1 hour. The fillers were taken out, dried, and then their mass m2 was measured; the acid resistance was m2 / m1, and the average value of the five groups was taken.

[0282] 3. Alkali resistance test

[0283] Randomly select 5 groups of second-layer fillers prepared in Examples 1-10, measure their mass m1, soak them in 96wt% sodium hydroxide solution and slightly boil them for 1h, take out the fillers, dry them, and measure their mass m2; the alkali resistance is m2 / m1, and the average value of the 5 groups is taken.

[0284] 4. Specific gravity test of concentrated acid

[0285] Add dilute sulfuric acid with a specific gravity of 1.01 into the treatment tower in Example 1-10, take 3 groups of concentrated acids in Example 1-10, use a fast liquid concentration meter DA-300C to measure the specific gravity of the concentrated acids, and take the average value of the 3 groups.

[0286] The compressive strength, acid resistance, alkali resistance and specific gravity of concentrated acid collected in the treatment tower of the second layer filler in Examples 1-10 were tested. The test results are shown in Table 1.

[0287]

[0288] Table 1

[0289] The foregoing examples are merely illustrative and are used to explain some features of the method of the present invention. The appended claims are intended to claim the widest possible range that can be conceived, and the embodiments presented herein are only illustrations of selected implementations according to the combination of all possible embodiments. Therefore, it is the applicant's intention that the appended claims are not limited by the selection of examples that illustrate the features of the present invention. Some numerical ranges used in the claims also include sub-ranges within them, and changes in these ranges should also be interpreted as being covered by the appended claims where possible.

Claims

1. A waste acid concentration treatment tower, comprising a tower body (1), characterized in that: An exhaust port (2) is provided above the top of the tower body (1), a packing layer is provided in the middle of the tower body (1), an air inlet (6) is provided on one side below the tower body (1), and a heating device (9) is connected below the bottom of the tower body (1); The packing layer comprises a first packing layer (3), a second packing layer (4), and a third packing layer (5); the first packing layer (3), the second packing layer (4), and the third packing layer (5) are respectively located at the upper, middle, and lower positions of the packing layer; The filler of the second filler layer is an inorganic filler; The raw materials of the inorganic filler include the following components by weight: 23.5 parts of kaolin, 7 parts of attapulgite, 4.5 parts of montmorillonite, 15 parts of calcined alumina, 1.5 parts of aluminum oxide, 0.5 parts of silicon dioxide, 3 parts of SBA-15, 1.7 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 1.95 parts of graphene, 1.05 parts of talc, 1.05 parts of glass flakes, 3 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy; the weight ratio of the glass fiber to sodium carboxymethyl cellulose is 2.5:1; The preparation method of the second filler layer comprises the following steps: (1) 1.7 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 1.5 parts of aluminum oxide, 0.5 parts of silicon dioxide, 3 parts of SBA-15, 1.95 parts of graphene, 1.05 parts of talc, and 1.05 parts of glass flakes were added into a stirring device and mixed for 20 minutes to obtain a mixture A; (2) adding 23.5 parts of kaolin, 7 parts of attapulgite, 4.5 parts of montmorillonite, 15 parts of calcined alumina, 3 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy to mixture A and stirring for 10 minutes to obtain mixture B; (3) placing the mixture B into a cemented carbide mold and pressing it to obtain a green body; (4) placing the green body into a vacuum sintering furnace for calcination. The sintering furnace temperature is set to 1450°C. The holding time is 2 hours. The vacuum sintering furnace is turned off. After the temperature drops to room temperature, the prepared second filler layer is taken out. or, The raw materials of the inorganic filler include the following components by weight: 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 2.7 parts of graphene, 1.5 parts of talc, 1.5 parts of glass flakes, 4.75 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy; the weight ratio of the glass fiber to sodium carboxymethyl cellulose is 2.8:1; The preparation method of the second filler layer comprises the following steps: (1) 3.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 5.1 parts of aluminum oxide, 1.5 parts of silicon dioxide, 3 parts of SBA-15, 2.7 parts of graphene, 1.5 parts of talc, and 1.5 parts of glass flakes were added into a stirring device and mixed for 20 minutes to obtain a mixture A; (2) adding 25 parts of kaolin, 7.5 parts of attapulgite, 5 parts of montmorillonite, 24 parts of calcined alumina, 4.75 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy to mixture A and stirring for 10 minutes to obtain mixture B; (3) placing the mixture B into a cemented carbide mold and pressing it to obtain a green body; (4) placing the green body into a vacuum sintering furnace for calcination. The sintering furnace temperature is set to 1450°C. The holding time is 2 hours. The vacuum sintering furnace is turned off. After the temperature drops to room temperature, the prepared second filler layer is taken out. or, The raw materials of the inorganic filler include the following components by weight: 33.5 parts of kaolin, 10 parts of attapulgite, 6.5 parts of montmorillonite, 30 parts of calcined alumina, 7 parts of aluminum oxide, 2 parts of silicon dioxide, 3 parts of SBA-15, 4.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 3.4 parts of graphene, 1.8 parts of talc, 1.8 parts of glass flakes, 6 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy; the weight ratio of the glass fiber to sodium carboxymethyl cellulose is 3.2:1; The preparation method of the second filler layer comprises the following steps: (1) 4.1 parts of 1-dodecyl-3-methylimidazole hexafluorophosphate, 7 parts of aluminum oxide, 2 parts of silicon dioxide, 3 parts of SBA-15, 3.4 parts of graphene, 1.8 parts of talc, and 1.8 parts of glass flakes were added into a stirring device and mixed for 20 minutes to obtain a mixture A; (2) adding 33.5 parts of kaolin, 10 parts of attapulgite, 6.5 parts of montmorillonite, 30 parts of calcined alumina, 6 parts of glass fiber and sodium carboxymethyl cellulose, 3.5 parts of tea residue powder, and 2 parts of cobalt-based alloy to mixture A and stirring for 10 minutes to obtain mixture B; (3) placing the mixture B into a cemented carbide mold and pressing it to obtain a green body; (4) The green body is placed in a vacuum sintering furnace for calcination. The sintering furnace temperature is set to 1450°C and the holding time is 2 hours. The vacuum sintering furnace is turned off. After the temperature drops to room temperature, the prepared second filler layer is taken out.

2. A waste acid concentration treatment tower according to claim 1, characterized in that: The bottom of the heating device (9) is connected to an ultrasonic generator (10).

3. A waste acid concentration treatment tower according to claim 1, characterized in that: A feeding port (7) is provided on one side below the tower body (1).

4. A waste acid concentration treatment tower according to claim 3, characterized in that: A discharge port (8) is provided on one side below the feed port (7).

5. A waste acid concentration treatment tower according to claim 4, characterized in that: The air inlet (6) is located below the tower body (1) on a side away from the feeding port (7) and the discharging port (8), and the height of the air inlet (6) is greater than the height of the feeding port (7).

6. A waste acid concentration treatment tower according to claim 1, characterized in that: The heating temperature of the heating device (9) is 55-65°C.

7. The waste acid concentration treatment tower according to claim 1, characterized in that: The height ratio of the first packing layer (3), the second packing layer (4) and the third packing layer (5) is (1.0-1.6):(1.6-2.5):

1.

8. A waste acid concentration treatment tower according to claim 7, characterized in that: The height ratio of the first packing layer (3), the second packing layer (4) and the third packing layer (5) is (1.2-1.4):(1.8-2.2):1.

Citation Information

Patent Citations

  • Purification and reconcentration of waste sulphuric acid

    CA1259775A

  • Hot-air concentrating tower for purifying waste acid

    CN102430249A

  • Coloring agent for processing plastic products

    CN105199393A

  • Structured square-mesh ceramic packing

    CN105536681A

  • Process for purification and concentration of sulfuric acid

    CN1094013A