Method for detecting dislocation of gallium nitride crystal
By using a mixed acid solution to etch gallium nitride crystals at 250°C to 400°C, and combining it with scanning electron microscopy analysis, the problems of complex detection, high cost, and inability to observe small-size dislocations in the existing technology have been solved, and nitrogen detection has been achieved. Fast and accurate characterization of dislocations in gallium crystals suitable for routine detection.
Patent Information
- Application Number
- CN202210080468.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-01-24
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2042-01-24
AI Technical Summary
Existing gallium nitride crystal dislocation detection methods have problems such as complex sample preparation, high cost, inability to directly observe the type and shape of dislocations, high heating temperature and difficulty in control. It is difficult to be suitable for routine detection, especially for small-sized dislocations. Not very good at detection.
Use a mixed sulfuric acid, hydrochloric acid and phosphoric acid solution with a volume ratio of (1.1~2.9):(0.1~1.9) to prepare an acid solution, etch the gallium nitride sample at 250℃~400℃, and combine it with scanning electron microscopy analysis to quickly and accurately Observe the size, shape, distribution and density of dislocations.
It achieves direct, rapid and accurate characterization of micron- or nano-scale dislocations, is suitable for detection of small-sized dislocations, meets conventional detection conditions, has simple steps, high testing efficiency and low cost.
Smart Images

Figure CN114594119B_ABST
Abstract
Citation Information
Patent Citations
GaN-based epitaxial material dislocation defect determination method
CN104502351A
Dislocation defect analysis method
CN112067402A
Method for evaluating dislocation of crystal, method for evaluating crystal growth method, and crystal growth method
JP2009008500A