A four-electrode device for measuring leakage current of suspension composite insulator samples

By designing a four-electrode device of high-voltage first electrode, surface electrode, interface electrode and body electrode, the lossless problem of interface current measurement of composite insulator test samples is solved, and the accurate measurement of the surface, interface and body current of composite insulator is achieved, and the improvement of the improvement of the surface, interface and body current of composite insulator is achieved. Measurement efficiency.

CN114594406BActive Publication Date: 2024-11-29HAINAN POWER GRID CO LTD ELECTRIC POWER RES INST
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202210244685.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-03-14
Publication Date
2024-11-29
Estimated Expiration
2042-03-14

AI Technical Summary

Technical Problem

The prior art cannot directly measure the interface current at the sheath-mand rod of the composite insulator test sample without loss, and there are errors in the measurement of surface current and body current.

Method used

A four-electrode device including a high-voltage first electrode, a surface electrode, an interface electrode and a body electrode are designed, through which the surface current, interface current and body current of the suspended composite insulator sample are measured separately, and the second electrode is fixed using an insulating substrate. , the diameter and thickness of the electrodes are optimized to ensure accurate measurement.

Benefits of technology

Accurate measurement of the surface current, interface current and body current of the composite insulator sample is achieved, which improves working efficiency and avoids the anatomical and completeness damage of the test sample.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114594406B_ABST
    Figure CN114594406B_ABST
Patent Text Reader

Abstract

The invention discloses a four-electrode device for measuring leakage current of a suspension composite insulator sample, comprising: a first electrode, arranged at a first end of the suspension composite insulator sample, wherein the first electrode is a high-voltage electrode; a second electrode, arranged at a second end of the suspension composite insulator sample; and an insulating substrate, used for fixing the second electrode. The invention uses a high-voltage electrode, a surface electrode, an interface electrode and a body electrode to simultaneously measure the surface current, the interface current and the body current of the composite insulator sample, without dissecting the composite insulator, thereby greatly improving the working efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of high-voltage power transmission and transformation, and in particular to a four-electrode device for measuring leakage current of a suspension composite insulator sample. Background Art

[0002] Since the 1980s, composite insulators have been widely used in my country, and the history of composite insulators in my country has been nearly 40 years. With the increase in the number and time of composite insulator operation, and the long-term exposure to electric fields, mechanical loads and complex and changeable environmental effects, composite insulators gradually age, and accidents such as surface flashover, abnormal heating, and breakdown and fracture occur. Among them, abnormal heating failures have occurred most frequently in recent years, and large-scale abnormal temperature rise has occurred many times, seriously threatening the safe and stable operation of the power grid. In the study of abnormal heating of composite insulators, it is very important to measure the leakage current of composite insulators. In the study of the heating mechanism of composite insulators, the surface current, interface current and body current of composite insulators can be used as key criteria. Therefore, accurately measuring the surface current, interface current and body current of composite insulators is of great significance for studying the abnormal temperature rise of composite insulators, protecting the safe operation of power systems, and ensuring people's production and life.

[0003] Cited documents: Patent No. CN202110122114.3 "A test method and device for the interface resistivity between the sheath and core rod of a composite insulator" When measuring the surface current, interface current and volume current of a composite insulator, it is necessary to first completely peel off the sheath and core rod of the composite insulator, and then measure the sheath current and core rod current respectively. This will destroy the integrity of the sample, causing measurement errors, and the interface current cannot be directly measured. Patent No. CN202010734326.2 "Test sample preparation method and sample preparation auxiliary device for rod-shaped composite insulators" uses an inner electrode, an inner ring electrode and an outer ring electrode as the second electrode. The inner electrode collects the volume current of the sample, the inner ring electrode collects the surface current of the sample, and the outer ring electrode acts as a uniform surface electric field. This patent cannot measure the interface current at the sheath-core rod of the sample. In summary, the existing technologies cannot directly measure the interface current at the sheath-core rod of the composite insulator sample in a non-destructive manner. There is an urgent need for a four-electrode device for measuring the leakage current of a suspended composite insulator sample to solve the existing technical problems. Summary of the invention

[0004] In order to solve the above problems, the purpose of the present invention is to provide a four-electrode device for measuring the leakage current of a suspension composite insulator sample, comprising:

[0005] A first electrode is arranged at a first end of the suspension composite insulator sample, wherein the first electrode is a high voltage electrode;

[0006] A second electrode is arranged at a second end of the suspension composite insulator sample;

[0007] The insulating substrate is used to fix the second electrode.

[0008] Preferably, the second electrode comprises a surface electrode, an interface electrode and a body electrode;

[0009] The diameter of the body electrode is 2 / 3 of the core rod diameter of the composite insulator sample;

[0010] The inner diameter of the interface electrode is 2 mm smaller than the overall diameter of the composite insulator sample;

[0011] The outer diameter of the interface electrode is 2 mm larger than the overall diameter of the composite insulator sample;

[0012] The outer diameter of the surface electrode is the same as the diameter of the first electrode;

[0013] The inner diameter of the surface electrode is 1 mm smaller than the overall diameter of the composite insulator specimen.

[0014] Preferably, the radial thickness of the interface electrode is 2 mm.

[0015] Preferably, the insulating substrate is polytetrafluoroethylene;

[0016] The body electrode, the interface electrode and the surface electrode are coaxially embedded on the insulating substrate.

[0017] Preferably, the upper surfaces of the body electrode, the interface electrode and the surface electrode are 1-2 mm higher than the substrate.

[0018] Preferably, the second electrode has a height of 8-10 mm.

[0019] Preferably, the diameter of the first electrode is 80 mm, and the axial thickness of the electrode is 20 mm.

[0020] Preferably, the first electrode and the second electrode are pure copper.

[0021] Preferably, the length of the suspension composite insulator specimen for a line not greater than 110 kV is 3-4 cm;

[0022] The length of suspension composite insulator specimens for lines greater than 110 kV and not greater than 500 kV is 5-6 cm;

[0023] The length of suspension composite insulator specimens for lines greater than 500kV is 7-8cm.

[0024] Preferably, the method for measuring the leakage current of a suspension composite insulator sample using a four-electrode device comprises the following steps:

[0025] Step 1: After removing the head and tail fittings of the rod-shaped suspension composite insulator, the portion between any two sheds is segmented in a direction perpendicular to the core rod axis, so that the cutting surface is perpendicular to the core rod axis to generate a suspension composite insulator segment;

[0026] Step 2: pre-treating the suspension composite insulator segment to remove protrusions on the cross section of the suspension composite insulator segment sample and dirt on the sheath surface, wherein the pre-treated suspension composite insulator segment is placed in a constant temperature drying oven for 72 hours to obtain a suspension composite insulator sample;

[0027] Step 3: Use the first electrode and the second electrode to clamp the two end sections of the suspension composite insulator sample respectively, so that there is no gap between the electrode and the sample, and the center of the sample coincides with the center of the electrode. Pressurize the first electrode, and measure the surface current, interface current and body current of the suspension composite insulator sample through the surface electrode, interface electrode and body electrode.

[0028] The present invention discloses the following technical effects:

[0029] The present invention uses high voltage electrodes, surface electrodes, interface electrodes and body electrodes to simultaneously measure the surface current, interface current and body current of a composite insulator sample without dissecting the composite insulator, thereby greatly improving work efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0031] Figure 1 It is a schematic diagram of a short-edge sample of a suspended composite insulator according to the present invention;

[0032] Figure 2 is a schematic diagram of the four-electrode system of the present invention;

[0033] Figure 3 It is a schematic cross-sectional view of a short-edge sample of a suspended composite insulator using the four-electrode system described in the present invention. DETAILED DESCRIPTION

[0034] In order to make the purpose, technical scheme and advantages of the embodiments of the present application clearer, the technical scheme in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all of the embodiments. The components of the embodiments of the present application generally described and shown in the drawings here can be arranged and designed in various different configurations. Therefore, the following detailed description of the embodiments of the present application provided in the drawings is not intended to limit the scope of the application claimed for protection, but merely represents the selected embodiments of the present application. Based on the embodiments of the present application, all other embodiments obtained by those skilled in the art without making creative work belong to the scope of protection of the present application.

[0035] like Figure 1-3 As shown, the present invention provides a four-electrode device for measuring leakage current of a suspension composite insulator sample, comprising:

[0036] A first electrode is arranged at a first end of the suspension composite insulator sample, wherein the first electrode is a high voltage electrode;

[0037] A second electrode is arranged at a second end of the suspension composite insulator sample;

[0038] The insulating substrate is used to fix the second electrode.

[0039] Further preferably, the second electrode includes a surface electrode, an interface electrode and a body electrode;

[0040] The diameter of the body electrode is 2 / 3 of the core rod diameter of the composite insulator sample;

[0041] The inner diameter of the interface electrode is 2 mm smaller than the overall diameter of the composite insulator sample;

[0042] The outer diameter of the interface electrode is 2 mm larger than the overall diameter of the composite insulator sample;

[0043] The outer diameter of the surface electrode is the same as the diameter of the first electrode;

[0044] The inner diameter of the surface electrode is 1 mm smaller than the overall diameter of the composite insulator specimen.

[0045] Further preferably, the radial thickness of the interface electrode is 2 mm.

[0046] Further preferably, the insulating substrate is polytetrafluoroethylene;

[0047] The body electrode, the interface electrode and the surface electrode are coaxially embedded on the insulating substrate.

[0048] Further preferably, the upper surfaces of the body electrode, the interface electrode and the surface electrode are 1-2 mm higher than the substrate.

[0049] Further preferably, the second electrode has a height of 8-10 mm.

[0050] Further preferably, the diameter of the first electrode is 80 mm, and the axial thickness of the electrode is 20 mm.

[0051] Further preferably, the first electrode and the second electrode are made of pure copper.

[0052] Further preferably, the length of the suspension composite insulator sample for a line not greater than 110 kV is 3-4 cm;

[0053] The length of suspension composite insulator specimens for lines greater than 110 kV and not greater than 500 kV is 5-6 cm;

[0054] The length of suspension composite insulator specimens for lines greater than 500kV is 7-8cm.

[0055] Further preferably, the method for measuring the leakage current of a suspension composite insulator sample using a four-electrode device comprises the following steps:

[0056] Step 1: After removing the head and tail fittings of the rod-shaped suspension composite insulator, the portion between any two sheds is segmented in a direction perpendicular to the core rod axis, so that the cutting surface is perpendicular to the core rod axis to generate a suspension composite insulator segment;

[0057] Step 2: pre-treating the suspension composite insulator segment to remove protrusions on the cross section of the suspension composite insulator segment sample and dirt on the sheath surface, wherein the pre-treated suspension composite insulator segment is placed in a constant temperature drying oven for 72 hours to obtain a suspension composite insulator sample;

[0058] Step 3: Use the first electrode and the second electrode to clamp the two end sections of the suspension composite insulator sample respectively, so that there is no gap between the electrode and the sample, and the center of the sample coincides with the center of the electrode. Pressurize the first electrode, and measure the surface current, interface current and body current of the suspension composite insulator sample through the surface electrode, interface electrode and body electrode.

[0059] The present invention is composed of an electrode unit and an insulating substrate, wherein the electrode unit is composed of a first electrode and a second electrode, wherein the first electrode is a high voltage electrode, and the second electrode is composed of a surface electrode, an interface electrode and a body electrode, wherein (1) the diameter of the body electrode is smaller than the core rod diameter of the composite insulator sample, and its diameter is 2 / 3 of the core rod diameter; so that when the composite insulator sample is placed on the second electrode, the range of the body electrode can include most of the core rod cross section, but cannot include the sheath-core rod interface. (2) The inner diameter of the interface electrode is 2 mm smaller than the overall diameter of the composite insulator sample, and the outer diameter is 2 mm larger than the overall diameter of the composite insulator sample, that is, the radial thickness of the interface electrode is 2 mm, so that when the composite insulator sample is placed on the second electrode, the range of the interface electrode can include the entire sheath-core rod interface, but as little as possible including the core rod and sheath part; (3) The outer diameter of the surface electrode is consistent with the diameter of the first electrode, and the inner diameter is 1 mm larger than the overall diameter of the composite insulator sample, so that when the composite insulator sample is placed on the second electrode, the edge of the sheath of the composite insulator sample can be just within the range of the body electrode, but cannot include the sheath-core rod interface. (4) The above-mentioned body electrode, interface electrode and surface electrode are coaxially embedded and fixed on the polytetrafluoroethylene insulation substrate, the upper surface of the electrode is 1-2 mm higher than the substrate, the lower surface is embedded in the substrate, and the overall height of the second electrode is 8-10 mm. (5) The diameter of the first electrode is 80 mm, and the axial thickness of the electrode is 20 mm. (6) The materials of the above-mentioned upper and second electrodes are both pure copper.

[0060] For example, for the FXBW-500 / 300 type 500kV composite insulator sample, the sample core rod diameter is 30mm, the sheath thickness is 3mm, the overall sample diameter is 36mm, and the length is 80mm. Figure 1 As shown. The structural dimensions of the four-electrode system for measuring the sample are: the high-voltage electrode has a diameter of 80 mm and a thickness of 20 mm; the body electrode has a diameter of 20 mm, the interface electrode has a diameter of 32 mm, the surface electrode has a diameter of 80 mm, the body electrode and the interface electrode are spaced 4 mm apart, and the interface electrode and the surface electrode are spaced 1 mm apart. Figure 2 shown.

[0061] The present invention also includes a method for measuring leakage current of a suspension composite insulator sample using a four-electrode device, comprising the following steps:

[0062] Step 1: After removing the head and tail fittings of the rod-shaped composite insulator, cut the part between any two sheds in sections along the direction perpendicular to the core rod axis, so that the cutting surface is perpendicular to the core rod axis;

[0063] Step 2: pre-treating the composite insulator segment to remove protrusions on the cross section of the composite insulator sample and dirt on the surface of the sheath; the composite insulator sample is placed in a constant temperature drying oven for 72 hours;

[0064] Step 3: Use a metal first electrode and a metal second electrode to clamp the two end sections of the pre-treated composite insulator segment, respectively, so that there is no gap between the electrode and the sample, and the center of the sample coincides with the center of the electrode. When the high-voltage electrode is pressurized, the composite insulator sample will generate leakage current. The surface electrode, interface electrode and body electrode in the four-electrode system simultaneously measure the surface current, interface current and body current of the composite insulator sample.

[0065] When cutting the line suspension composite insulator in the step 1, the length of the suspension composite insulator segment for lines not exceeding 110kV is 3-4cm; the length of the suspension composite insulator segment for lines exceeding 110kV and not exceeding 500kV is 5-6cm; the length of the suspension composite insulator segment for lines exceeding 500kV is 7-8cm.

[0066] It should be noted that similar numbers and letters represent similar items in the following figures. Therefore, once an item is defined in one figure, it does not need to be further defined and explained in subsequent figures. In addition, the terms "first", "second", "third", etc. are only used to distinguish the description and are not to be understood as indicating or implying relative importance.

[0067] Finally, it should be noted that the above-described embodiments are only specific implementations of the present invention, which are used to illustrate the technical solutions of the present invention, rather than to limit them. The protection scope of the present invention is not limited thereto. Although the present invention is described in detail with reference to the above-described embodiments, those skilled in the art should understand that any person skilled in the art can still modify the technical solutions described in the above-described embodiments within the technical scope disclosed by the present invention, or can easily think of changes, or perform equivalent replacements on some of the technical features thereof; and these modifications, changes or replacements do not make the essence of the corresponding technical solutions deviate from the spirit and scope of the technical solutions of the embodiments of the present invention. They should all be covered within the protection scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the protection scope of the claims.

Claims

1. A four-electrode device for measuring leakage current of suspension composite insulator samples, characterized in that: include: A first electrode is arranged at a first end of the suspension composite insulator sample, wherein the first electrode is a high voltage electrode; The second electrode is arranged at the second end of the suspension composite insulator sample; the second electrode includes a surface electrode, an interface electrode and a body electrode; the diameter of the body electrode is 2 / 3 of the core rod diameter of the composite insulator sample; the inner diameter of the interface electrode is 2 mm smaller than the overall diameter of the composite insulator sample; the outer diameter of the interface electrode is 2 mm larger than the overall diameter of the composite insulator sample; the outer diameter of the surface electrode is the same as the diameter of the first electrode; the inner diameter of the surface electrode is 1 mm smaller than the overall diameter of the composite insulator sample; The insulating substrate is used to fix the second electrode.

2. A four-electrode device for measuring leakage current of a suspension composite insulator sample according to claim 1, characterized in that: The radial thickness of the interface electrode is 2 mm.

3. A four-electrode device for measuring leakage current of a suspension composite insulator sample according to claim 2, characterized in that: The insulating substrate is polytetrafluoroethylene; The body electrode, the interface electrode and the surface electrode are coaxially embedded on an insulating substrate.

4. A four-electrode device for measuring leakage current of a suspension composite insulator sample according to claim 3, characterized in that: The upper surfaces of the body electrode, the interface electrode and the surface electrode are 1-2 mm higher than the substrate.

5. A four-electrode device for measuring leakage current of a suspension composite insulator sample according to claim 4, characterized in that: The second electrode has a height of 8-10 mm.

6. A four-electrode device for measuring leakage current of a suspension composite insulator sample according to claim 5, characterized in that: The diameter of the first electrode is 80 mm, and the axial thickness of the electrode is 20 mm.

7. A four-electrode device for measuring leakage current of a suspension composite insulator sample according to claim 6, characterized in that: The first electrode and the second electrode are made of pure copper.

8. A four-electrode device for measuring leakage current of a suspension composite insulator sample according to claim 7, characterized in that: The length of the suspension composite insulator sample for a line not greater than 110 kV is 3-4 cm; The length of the suspension composite insulator sample for lines greater than 110 kV and not greater than 500 kV is 5-6 cm; The length of the suspension composite insulator sample for a line greater than 500 kV is 7-8 cm.

9. A four-electrode device for measuring leakage current of a suspension composite insulator sample according to claim 8, characterized in that: The method for measuring the leakage current of the suspension composite insulator sample using the four-electrode device comprises the following steps: Step 1: After removing the head and tail fittings of the rod-shaped suspension composite insulator, the portion between any two sheds is segmented in a direction perpendicular to the core rod axis, so that the cutting surface is perpendicular to the core rod axis to generate a suspension composite insulator segment; Step 2: pre-treating the suspension composite insulator segment to remove protrusions on the cross section of the suspension composite insulator segment sample and dirt on the sheath surface, wherein the pre-treated suspension composite insulator segment is placed in a constant temperature drying oven for 72 hours to obtain the suspension composite insulator sample; Step 3: Use the first electrode and the second electrode to clamp the two end sections of the suspension composite insulator sample respectively, so that there is no gap between the electrode and the sample, and the center of the sample coincides with the center of the electrode, pressurize the first electrode, and measure the surface current, interface current and body current of the suspension composite insulator sample respectively through the surface electrode, the interface electrode and the body electrode.

Citation Information

Patent Citations

  • Composite insulator sheath and core rod interface resistivity test method and device

    CN112698102A

  • Manufacturing method for test sample of rod-shaped composite insulator and sample manufacturing auxiliary device