A method for preparing β-boramide based on chitosan functionalized copper material
The catalytic synthesis of β-boramide through chitosan functionalized copper material in pure water solves the problems of complex reactions and difficult catalyst recovery in the existing technology, and realizes green, efficient and economical synthesis of β-boramide, meeting the needs of Sustainable development needs of industrial production.
Patent Information
- Application Number
- CN202210251675.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-15
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2042-03-15
AI Technical Summary
The existing technology has problems such as complex reactions, many additives, unrecoverable catalysts, and the use of toxic solvents and alkali when synthesizing organoborides, and cannot meet the needs of green, environmentally friendly and economical industrial production.
Chitosan functionalized copper material is used as a catalyst, and through its biocompatibility and complexation of amino, hydroxyl and imine bonds, β-boramide is synthesized in pure water, avoiding the addition of strong alkali and Organic solvents are used, and the catalyst can be recycled multiple times.
Efficient synthesis of β-boramide in pure water is achieved, which reduces industrial costs and environmental pollution. The catalyst has good reusability, wide substrate applicability, simple reaction components, and avoids the addition of additional bases and complex ligands. .
Smart Images

Figure CN114605451B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of organic synthesis, and in particular to a method for preparing beta-boron amide based on chitosan functionalized copper material. Background Art
[0002] Organoboron compounds have important applications in organic synthesis, materials, biomedicine and other fields, and can also be used as organic functional polymers to prepare a variety of useful compounds. In the past few years, scientists have developed a variety of methods for constructing organoboron compounds. However, the existing reports all have their own limitations and cannot meet the needs of diverse synthesis. Therefore, it is worth further exploring new methods and new pathways for the synthesis of organoboron compounds. At the same time, amide bonds are one of the most common structural units in natural and synthetic molecules, and have many applications in the pharmaceutical, agrochemical and polymer industries. The traditional method for synthesizing amide bonds is to obtain them through the dehydration condensation of amines and carboxylic acids mediated by carefully designed coupling agents. This method causes excessive waste of raw materials and is expensive. With the increasing concern for the environment and the economy, atom-economical and widely applicable methods are more needed, and cheap reagents are preferred. In the past decade, some innovative methods have been designed to achieve these goals, but there are few reports on the design and synthesis of amide boron compounds using amide substrates.
[0003] In 2020, the document (J.Am.Chem.Soc.2020,142,623-632) used ethylene and isocyanate as raw materials and copper as catalyst for carboxylation reaction, which provided a direct and practical way to construct chiral secondary amides containing borate. In this reaction, a copper-catalyzed boryl carboxylation reaction of vinylene was successfully prepared using chiral phosphine amine ligands. However, the reaction has a series of problems such as complex copper source, ligand addition, and base addition, and it is not economical and cannot be green recycled. In the same year, the document (Chem.Commun.,2020,56,7483) studied the copper-catalyzed boronization amidation reaction of vinylene with isocyanate and bis-pinacol boron. This new scheme can be effectively implemented, and the resulting product can reach the gram scale, which provides a practical scheme for industrial application. This method uses isocyanate as a simple precursor to provide a series of boryl amides, which can synthesize valuable amides and borates. However, the scope of substrates applied by this method is limited. The group changes of isocyanate cannot meet the synthesis of a wider range of boron amide substrates, and the reaction requires the addition of bases, complex catalysts, and toxic solvents. Therefore, it is necessary to develop a new method that uses pure water as a solvent, has low cost, mild conditions, wider substrate applicability, and is green and efficient. Summary of the invention
[0004] The purpose of the present invention is to solve the shortcomings of the above-mentioned background technology and provide a method for preparing β-boramide based on chitosan functionalized copper material, thereby overcoming the problems of complex reaction, additives, specific ligands, and catalyst recovery in the existing method.
[0005] The invention uses chitosan Schiff base copper functional material to prepare beta-boramide compounds, utilizes the biocompatibility of chitosan Schiff base copper functional material and the complexing effect of amino, hydroxyl and imine bonds on metal ions, changes the complexing effect on ordinary chitosan, and has higher catalytic activity. Meanwhile, the amino groups on chitosan show an alkaline environment in the reaction system, and no strong base needs to be added in the reaction system. The reaction can be carried out only in pure water, and the catalyst can be recycled for multiple times. Therefore, the method is more green and environmentally friendly, and meets the concept of sustainable industrial production.
[0006] The technical solution of the present invention is: a method for preparing β-boramide based on chitosan functionalized copper material, characterized in that it comprises the following steps:
[0007] 1) Adding α-acrylamide compound I, bipyraclostrobin and chitosan Schiff base copper functional material CX@Cu into water, mixing and stirring at room temperature for 8 to 16 hours, wherein the molar ratio of α-acrylamide compound I, bipyraclostrobin and material CX@Cu loaded copper is 1:(1 to 2):(0.01 to 0.05);
[0008] 2) After the reaction is completed, the reaction is filtered, and the obtained filtrate is separated and purified to obtain the β-boronamide compound II. The precipitate is washed and dried to obtain the recovered chitosan Schiff base copper functional material catalytic material CX@Cu, which is then recycled for the next use.
[0009] The chemical reaction equation is as follows:
[0010]
[0011] Wherein, R is phenyl, p-methylphenyl, p-methoxyphenyl, p-bromophenyl, p-alkynylphenyl or naphthyl.
[0012] Preferably, in step 1), the copper content in the chitosan Schiff base copper functional material CX@Cu is 0.6-1.6 mmol / g.
[0013] Preferably, in step 1), the molar ratio of the α-acrylamide compound I, the bipyraclostrobin and the material CX@Cu loaded copper is 1:2:0.0167-0.025.
[0014] Preferably, in step 1), the ratio of the amount of copper loaded to water in the chitosan Schiff base copper functional material CX@Cu is 0.005 mmol: 1-2 ml.
[0015] Preferably, in step 1), the mixture is stirred and reacted at room temperature for 16 hours.
[0016] Preferably, the filtrate obtained in step 2) is separated and purified to obtain β-boramide compound II, specifically comprising: extracting the filtrate with ethyl acetate to obtain an organic phase containing the product, then drying over anhydrous Na2SO4, filtering, and rotary evaporation to remove excess organic solvent, and purifying the obtained crude product by column chromatography with a mixed solvent of ethyl acetate and petroleum ether to obtain β-boramide compound II.
[0017] Preferably, in step 1), the chitosan Schiff base copper functional material CX@Cu is prepared by the following steps:
[0018] a. Mix glacial acetic acid and anhydrous ethanol in a volume ratio of 1:5-8 to obtain an acetic acid ethanol solution, add chitosan and aldehyde to the acetic acid ethanol solution, and stir and react at 25-50°C for 8-16 hours, wherein the aldehyde is one of 4-imidazolecarboxaldehyde, 4-cyanobenzaldehyde, and 2-quinolinecarboxaldehyde, and the molar ratio of amino group -NH2 in chitosan to aldehyde group -CHO in the aldehyde compound is 1:3-4;
[0019] b. After the reaction is completed, the chitosan Schiff base material is separated and washed to obtain the chitosan Schiff base material;
[0020] c. placing the chitosan Schiff base material in a copper sulfate solution and stirring at 25-50°C for 8-16 hours to promote the adsorption of divalent copper ions;
[0021] d. After the adsorption is completed, the chitosan Schiff base copper functional material is obtained by separation and washing.
[0022] The chemical formula for preparing chitosan Schiff base material is:
[0023]
[0024] L is: One of them.
[0025] Furthermore, in step a, glacial acetic acid and anhydrous ethanol are mixed at a volume ratio of 1:7.5 to obtain an acetic acid ethanol solution, and the molar ratio of amino group -NH2 in chitosan to aldehyde group -CHO in aldehyde compound is 1:4. The acetic acid of the present invention adopts commercially available glacial acetic acid product.
[0026] Further, the copper sulfate solution in step c contains Cu 2+ The molar ratio of the amino group to the amino group-NH2 in the chitosan is at least 1:1, and the concentration of copper ions in the copper sulfate solution in step c is 0.16-0.24 mol / L.
[0027] Furthermore, the separation and washing treatments in steps b and d both include: after filtering, washing the precipitate repeatedly and alternately with water and ethanol, and drying in an oven at 50° C. for 12 hours.
[0028] During the preparation of chitosan Schiff base copper functional materials, copper sulfate solution provides sufficient copper ions to the chitosan Schiff base material, so that it can adsorb copper ions through its own adsorption capacity, which is a routine operation in the art.
[0029] In the present invention, the CB bond of the biboric acid pinacol ester is broken under the catalysis of the active divalent copper in the chitosan Schiff base copper functional material CX@Cu to form a copper borane complex and a corresponding byproduct Bpin-OH. The intermediate undergoes an unsaturated compound conjugate addition reaction with the α-acrylamide compound through the electron-guiding effect of the carbonyl group. In the reaction, the proton source comes from pure water, and the desired target product is obtained after protonation. The catalytic material is regenerated and can be recycled for the next time. The water in the reaction has a dual role, acting as a proton source and a solvent. The O atom adjacent to the N atom and the hydroxyl group in the material reacts with the Cu 2+ A strong complexation occurs and the protonation process is affected, giving the catalyst stable properties.
[0030] The beneficial effects of the present invention are:
[0031] 1. Chitosan Schiff base copper functional materials can be applied to pure water phase reactions, avoiding the use of organic reagents, and achieving green, environmental protection and pollution-free. Through the chitosan modified with Schiff base, the copper particles can be more firmly fixed on the catalytic material, and at the same time have a longer cycle life. The chitosan Schiff base copper functional material can be separated by simple filtration of the solid and liquid phases after the reaction, and can be recycled again after repeated washing, and the reusability performance is maintained well, which can reduce the cost of industrial reactions and reduce damage to the environment.
[0032] 2. This method can achieve a high conversion rate with a smaller amount of catalyst.
[0033] 3. The reaction components in this method are simple, pure water is used as the solvent, and no additional base and complex ligands are required.
[0034] 4. This method has wide substrate applicability and can successfully prepare different types of β-boronamide compounds.
[0035] 5. Chitosan Schiff base materials for Cu 2+ The adsorption is mainly based on the complexation of imine bonds, and a small amount of free amino groups are complexed:
[0036] Complexation:
[0037] Electrostatic attraction:
[0038] 6. After the chitosan is subjected to the Schiff base reaction, the surface area and porosity of the catalytic material are increased. The R'NH2 group on the chitosan reacts with the R2C=O group to generate a R2C=NR' bond, and a connection is formed at different amino positions inside the chitosan. Although the Schiff base reaction reduces the free amino groups of the chitosan, an imine bond is generated, which can also adsorb copper ions and bind to the O atom Cu in the hydroxyl group adjacent to the N atom. 2+ A related complexation reaction is generated to produce a conjugated surface, and through the double adsorption of chemical adsorption and physical adsorption, the complexation between the material and copper ions is made stronger. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] Figure 1 is the H NMR spectrum of the target product in Example 2;
[0040] Figure 2 It is the NMR carbon spectrum of the target product in Example 2. DETAILED DESCRIPTION
[0041] The following specific examples further illustrate the present invention in detail. The drugs used in the examples are all commercially available products unless otherwise specified, and the methods used are all conventional methods in the art unless otherwise specified.
[0042] Example 1
[0043] Chitosan Schiff base copper functional material is prepared by the following method:
[0044] a. Mix glacial acetic acid and anhydrous ethanol in a volume ratio of 1:7.5 to obtain an acetic ethanol solution, add 1 g of chitosan and aldehyde (4-imidazolecarboxaldehyde) to the acetic ethanol solution, and stir and react at 50°C for 12 hours, wherein 1.0 g of chitosan contains about 6.2 mmol -NH2, and the molar ratio of amino -NH2 in chitosan to aldehyde group -CHO in aldehyde compound is 1:4;
[0045] b. After the reaction is completed, the reaction solution is filtered, the resulting precipitate is repeatedly washed with water and ethanol alternately, and dried in an oven at 50°C for 12h to obtain the chitosan Schiff base material CX1;
[0046] c. Add the chitosan Schiff base material CX1 obtained in step b to 30 mL of copper sulfate solution (prepared with 1.6 g of copper sulfate pentahydrate, containing about 6.4 mmol Cu 2+ ) and stirred at 50 °C for 12 h to promote the adsorption of divalent copper ions;
[0047] d. After the adsorption is completed, the reaction solution is filtered and the precipitate is repeatedly washed with water and ethanol alternately, and then dried in an oven at 50°C for 12 h to obtain the chitosan Schiff base copper functional material CX1@Cu. The relative content of copper in the CX1@Cu catalytic material was detected by ICP to be 1.6 mmol / g.
[0048] When the aldehyde in step a of the above preparation method is replaced with 4-cyanobenzaldehyde, a chitosan Schiff base copper functional material CX2@Cu is obtained (the copper content is 0.6 mmol / g as determined by ICP);
[0049] When the aldehyde in step a of the above preparation method is replaced by 2-quinolinecarboxaldehyde, a chitosan Schiff base copper functional material CX3@Cu is obtained (the copper content is 0.9 mmol / g as determined by ICP).
[0050] In step a of the above preparation method, no aldehyde is added, only chitosan is added to the acetic acid ethanol solution, and the other steps remain unchanged to obtain a comparative material CX0@Cu (the copper content is 1.6 mmol / g as determined by ICP).
[0051] Example 2
[0052] This embodiment provides a method for preparing β-boramide by catalysis of chitosan Schiff base copper functional material, comprising the following steps:
[0053] 1) Add α-acrylamide compound I, bipyraclostrobin reagent, chitosan Schiff base copper functional materials CX1@Cu, CX2@Cu, CX3@Cu containing different aldehydes, and blank control chitosan copper material CX0@Cu (prepared in Example 1), wherein 0.3 mmol of α-acrylamide compound I, 0.6 mmol of bipyraclostrobin, and 0.005 mmol of copper loaded on chitosan Schiff base copper functional material are added to 2 ml of water, and the mixture is stirred at room temperature for 16 h. In this embodiment, R in α-acrylamide compound I is phenyl;
[0054] 2) After the reaction is completed, the precipitate is filtered, and the precipitate is repeatedly washed with water and ethanol alternately and dried, and the chitosan Schiff base copper functional material is recovered and recycled, and the filtrate is extracted with ethyl acetate three times to obtain an organic phase containing the product, and then dried with anhydrous Na2SO4 to remove water in the system, filtered, and rotary evaporated to remove excess organic solvent. The crude product is used as a developing solvent with a volume ratio of petroleum ether / ethyl acetate mixed solvent = 4:1, and column chromatography is purified to obtain β-boronamide compound II (R is phenyl).
[0055]
[0056] CX0@Cu, CX1@Cu, CX2@Cu, and CX3@Cu catalytic materials were used in the reaction, and the final yields were 45%, 89%, 80%, and 81%, respectively.
[0057] After the CX1@Cu catalytic material was used for 5 cycles, it was applied to the boron addition reaction of N,2-diphenylacrylamide for the 6th time, and the yield of the obtained product was 85%.
[0058] The NMR hydrogen spectrum and carbon spectrum of the target product are shown below. Figure 1 and Figure 2 :
[0059] 1 H NMR (400MHz, Chloroform-d); δ=7.42-7.23(m,5H),7.30-7.23(m,4H),7.08-7.03(m,2 H),3.89-3.85(q,1H),1.70-1.63(q,1H),1.32-1.26(q,1H),1.21(s,6H),1.19(s,6H).
[0060] 13 C NMR (100MHz, Chloroform-d); δ=172.85,141.95,138.49,129.47,129.29,128.43,127.85,124.44,119.92,83.78,50.39,25.25,25.12.
[0061] Example 3
[0062] This embodiment provides a method for preparing β-boramide by catalysis of chitosan Schiff base copper functional material, comprising the following steps:
[0063] 1) 0.20 mmol of α-acrylamide compound I, 0.4 mmol of biboric acid pinacol ester, and 0.005 mmol of copper-loaded chitosan Schiff base copper functional material CX1@Cu were added to 2.0 ml of water, and the mixture was stirred and reacted at room temperature for 16 h. In this embodiment, the α-acrylamide compound I is 2-phenyl-N-(p-tolyl) acrylamide (R is p-tolyl);
[0064] 2) After the reaction is completed, the filtrate is filtered and extracted with ethyl acetate three times to obtain an organic phase containing the product, which is then dried over anhydrous Na2SO4, filtered, and rotary evaporated to remove excess organic solvent. The crude product is used as a developing solvent with a volume ratio of petroleum ether / ethyl acetate mixed solvent = 4:1, and purified by column chromatography to obtain β-boronamide compound II, with a product yield of 85%.
[0065]
[0066] The NMR hydrogen spectrum and carbon spectrum of the target product are shown below:
[0067] 1 H NMR (400MHz, Chloroform-d); δ=7.35-7.34(m,3H),7.29-7.27(m,4H),7.08-7.04(d,2H),7.01(s,1 H),3.88-3.84(q,1H),2.27(s,1H),1.69-1.59(q,1H),1.31-1.25(q,1H),1.21(s,6H),1.19(s,6H).
[0068] 13 C NMR (100MHz, Chloroform-d); δ=172.71,142.04,135.93,133.97,129.73,129.39,128.40,127.75,119.97,83.72,50.28,25.23,25.09,21.25.
[0069] The results of this example show that when the CX1@Cu catalytic material provided in Example 1 of the present invention participates in the boron addition reaction, the conversion rate of 2-phenyl-N-(p-tolyl) acrylamide is high, and the yield of its boron addition product reaches 85%.
[0070] Example 4
[0071] This embodiment provides a method for preparing β-boramide by catalysis of chitosan Schiff base copper functional material, comprising the following steps:
[0072] 1) 0.20 mmol of α-acrylamide compound I, 0.4 mmol of biboric acid pinacol ester, and chitosan Schiff base copper functional material CX1@Cu loaded with 0.005 mmol of copper were added into 2.0 ml of water, and the mixture was stirred and reacted at room temperature for 16 h. In this embodiment, the α-acrylamide compound I is N-(4-methoxyphenyl)-2-phenylacrylamide (R is p-methoxyphenyl);
[0073] 2) After the reaction is completed, the filtrate is filtered and extracted with ethyl acetate three times to obtain an organic phase containing the product, which is then dried over anhydrous Na2SO4, filtered, and rotary evaporated to remove excess organic solvent. The crude product is used as a developing solvent with a volume ratio of petroleum ether / ethyl acetate mixed solvent = 6:1, and purified by column chromatography to obtain β-boronamide compound II, with a product yield of 87%.
[0074]
[0075] The H NMR spectrum and C NMR spectrum of the target product β-boronamide compound II of this example are as follows:
[0076] 1 H NMR (400MHz, Chloroform-d); δ=7.36-7.26(m,7H),6.97(s,1H),6.80-6.78(q,2H),3.88-3.83(q ,1H),3.76(s,3H),3.62(s,1H),1.69-1.61(q,1H),1.31-1.25(q,1H),1.21(s,6H),1.19(s,6H).
[0077] 13 C NMR (100MHz, Chloroform-d); δ=172.67,156.59,142.09,131.66,129.43,128.44,127.79,121.75,114.40,83.73,55.90,50.19,25.26,25.13.
[0078] The results of this example show that when the CX1@Cu catalytic material provided in Example 1 of the present invention participates in the boron addition reaction, the conversion rate of N-(4-methoxyphenyl)-2-phenylacrylamide is high, and the yield of its boron addition product reaches 87%.
[0079] Example 5
[0080] This embodiment provides a method for preparing β-boramide by catalysis of chitosan Schiff base copper functional material, comprising the following steps:
[0081] 1) 0.20 mmol of α-acrylamide compound I, 0.4 mmol of biboric acid pinacol ester, and chitosan Schiff base copper functional material CX1@Cu loaded with 0.005 mmol of copper were added into 2.0 ml of water, and the mixture was stirred and reacted at room temperature for 16 h. In this embodiment, the α-acrylamide compound I is N-(4-bromophenyl)-2-phenylacrylamide (R is p-bromophenyl);
[0082] 2) After the reaction is completed, the filtrate is filtered and extracted with ethyl acetate three times to obtain an organic phase containing the product, which is then dried over anhydrous Na2SO4 to remove water in the system, filtered, and rotary evaporated to remove excess organic solvent. The obtained crude product is used as a developing solvent with a volume ratio of petroleum ether / ethyl acetate mixed solvent = 4:1, and column chromatography is used to purify the β-boronamide compound II, and the product yield is 78%.
[0083]
[0084] The H NMR spectrum and C NMR spectrum of the target product β-boronamide compound II of this example are as follows:
[0085] 1 H NMR (400MHz, Chloroform-d); δ=7.37-7.27(m,9H),7.08(s,1H),3.88-3.84(q,1H),1.30-1.25(q,1H),1.21(s,6H),1.18(s,6H).
[0086] 13 C NMR (100MHz, Chloroform-d); δ=172.94,141.69,137.54,132.23,129.53,128.38,127.96,121.48,116.94,83.83,50.37,25.26,25.11.
[0087] As shown in the results of Example 5, when the CX1@Cu catalytic material provided in Example 1 of the present invention participates in the boron addition reaction, the conversion rate of N-(4-bromophenyl)-2-phenylacrylamide is high, and the yield of its boron addition product reaches 78%.
[0088] Example 6
[0089] This embodiment provides a method for preparing β-boramide by catalysis of chitosan Schiff base copper functional material, comprising the following steps:
[0090] 1) 0.20 mmol of α-acrylamide compound I, 0.4 mmol of biboric acid pinacol ester, and chitosan Schiff base copper functional material CX1@Cu loaded with 0.005 mmol of copper were added into 2.0 ml of water, and the mixture was stirred and reacted at room temperature for 16 h. In this embodiment, the α-acrylamide compound I is N-(4-ethynylphenyl)-2-phenylacrylamide (R is p-alkynylphenyl);
[0091] 2) After the reaction is completed, the filtrate is filtered and extracted with ethyl acetate three times to obtain an organic phase containing the product, which is then dried over anhydrous Na2SO4 to remove water in the system, filtered, and rotary evaporated to remove excess organic solvent. The obtained crude product is used as a developing solvent with a mixed solvent of petroleum ether / ethyl acetate in a volume ratio of 4:1, and purified by column chromatography to obtain β-boronamide compound II, with a product yield of 70%.
[0092]
[0093] The H NMR spectrum and C NMR spectrum of the target product β-boronamide compound II of this example are as follows:
[0094] 1H NMR (400MHz, Chloroform-d); δ=7.30-7.18(m,9H),7.08(s,1H),3.81-3.77(q,1H),2.93(s,1H),1.23-1.17(q,1H),1.13(s,6H),1.10(s,6H).
[0095] 13 C NMR (100MHz, Chloroform-d); δ=172.95,141.66,138.93,133.26,129.53,128.39,127.97,127.13,119.46,117.75,83.84,50.43,25.25,25.10.
[0096] As shown in the results of Example 6, when the CX1@Cu catalytic material provided in Example 1 of the present invention participates in the boron addition reaction, the conversion rate of N-(4-ethynylphenyl)-2-phenylacrylamide is high, and the yield of its boron addition product reaches 70%.
[0097] Example 7
[0098] This embodiment provides a method for preparing β-boramide by catalysis of chitosan Schiff base copper functional material, comprising the following steps:
[0099] 1) 0.20 mmol of α-acrylamide compound I, 0.4 mmol of biboric acid pinacol ester, and chitosan Schiff base copper functional material CX1@Cu loaded with 0.005 mmol of copper were added into 2.0 ml of water, and the mixture was stirred and reacted at room temperature for 16 h. In this embodiment, the α-acrylamide compound I is N-(naphthalene-2-yl)-2-phenylacrylamide (R is naphthyl);
[0100] 2) After the reaction is completed, the filtrate is filtered and extracted with ethyl acetate three times to obtain an organic phase containing the product, which is then dried over anhydrous Na2SO4 to remove water in the system, filtered, and rotary evaporated to remove excess organic solvent. The crude product is used as a developing solvent with a volume ratio of petroleum ether / ethyl acetate mixed solvent = 4:1, and purified by column chromatography to obtain β-boronamide compound II, with a product yield of 72%.
[0101]
[0102] The H NMR spectrum and C NMR spectrum of the target product β-boronamide compound II of this example are as follows:
[0103] 1H NMR (400MHz, Chloroform-d); δ=7.79-7.77(d,2H),7.64-7.62(d,2H),7.48-7.44(d,2H),7.73-7 .17(m,10H),3.94-3.90(q,1H),1.65-1.59(q,1H),1.24-1.19(q,1H),1.08(s,6H),1.05(s,6H).
[0104] 13 C NMR (100MHz, Chloroform-d); δ=173.30,142.14,134.35,132.77,129.61,129.05,128.56,12 8.01,127.18,126.46,126.16,126.14,125.69,120.61,120.38,83.73,50.35,25.21,25.13.
[0105] As shown in the results of Example 7, when the CX1@Cu catalytic material provided in Example 1 of the present invention participates in the boron addition reaction, the conversion rate of N-(naphthalene-2-yl)-2-phenylacrylamide is high, and the yield of its boron addition product reaches 72%.
Claims
1. A method for preparing β-boramide based on chitosan functionalized copper material, It is characterized in that The following steps are involved: 1) Adding α-acrylamide compound I, bipyraclostrobin and chitosan Schiff base copper functional material CX@Cu into water, mixing and stirring at room temperature for 8 to 16 hours, wherein the molar ratio of α-acrylamide compound I, bipyraclostrobin and material CX@Cu loaded copper is 1:(1 to 2):(0.01 to 0.05); 2) After the reaction is completed, filtering is performed, and the obtained filtrate is separated and purified to obtain β-boronamide compound II. After the precipitate is washed and dried, the recovered chitosan Schiff base copper functional material catalytic material CX@Cu is obtained, and it is recycled for the next use; The chemical reaction equation is as follows: Wherein, R is phenyl, p-methylphenyl, p-methoxyphenyl, p-bromophenyl, p-alkynylphenyl or naphthyl; Chitosan Schiff base copper functional material CX@Cu is prepared by the following steps: a. Mix glacial acetic acid and anhydrous ethanol in a volume ratio of 1:5-8 to obtain an acetic acid ethanol solution, add chitosan and aldehyde to the acetic acid ethanol solution, and stir the reaction at 25-50°C for 8-16 hours, wherein the aldehyde is one of 4-imidazolecarboxaldehyde, 4-cyanobenzaldehyde, and 2-quinolinecarboxaldehyde, and the amino-NH 2 The molar ratio of the aldehyde group-CHO in the aldehyde compound is 1:3-4; b. After the reaction is completed, the chitosan Schiff base material is separated and post-processed to obtain the chitosan Schiff base material; c. placing the chitosan Schiff base material in a copper sulfate solution and stirring at 25-50°C for 8-16 hours to promote the adsorption of divalent copper ions; d. After the adsorption is completed, the chitosan Schiff base copper functional material is obtained by separation and washing.
2. The method for preparing β-boramide based on chitosan functionalized copper material according to claim 1, It is characterized in that In step 1), the copper content in the chitosan Schiff base copper functional material CX@Cu is 0.6-1.6 mmol / g.
3. The method for preparing β-boramide based on chitosan functionalized copper material according to claim 1, It is characterized in that In step 1), the molar ratio of α-acrylamide compound I, bipyraclostrobin and material CX@Cu loaded copper is 1:2:0.0167-0.
025.
4. The method for preparing β-boramide based on chitosan functionalized copper material according to claim 1, It is characterized in that Step 1) The ratio of the amount of copper loaded to water in the chitosan Schiff base copper functional material CX@Cu is 0.005mmol:1-2ml.
5. The method for preparing β-boramide based on chitosan functionalized copper material according to claim 1, It is characterized in that In step 1), the mixture was stirred and reacted at room temperature for 16 h.
6. The method for preparing β-boramide based on chitosan functionalized copper material according to claim 1, It is characterized in that The filtrate obtained in step 2) is separated and purified to obtain β-boronamide compound II, which specifically comprises: extracting the filtrate with ethyl acetate to obtain an organic phase containing the product, and then subjecting the organic phase to anhydrous Na 2 SO 4 The residue was dried, filtered and rotary evaporated to remove the excess organic solvent. The obtained crude product was purified by column chromatography using a mixed solvent of ethyl acetate and petroleum ether to obtain β-boronamide compound II.
7. The method for preparing β-boramide based on chitosan functionalized copper material according to claim 1, It is characterized in that In step a, glacial acetic acid and anhydrous ethanol are mixed in a volume ratio of 1:7.5 to obtain an acetic acid ethanol solution. 2 The molar ratio of aldehyde to the aldehyde group -CHO in the aldehyde compound is 1:
4.
8. The method for preparing β-boramide based on chitosan functionalized copper material according to claim 1, It is characterized in that The copper sulfate solution in step c contains Cu 2+ With chitosan amino-NH 2 The molar ratio is at least 1:1, and the copper ion concentration in the copper sulfate solution in step c is 0.16-0.24 mol / L.
9. The method for preparing β-boramide based on chitosan functionalized copper material according to claim 1, It is characterized in that The separation and washing treatments in steps b and d both include: filtering, washing with water and ethanol repeatedly and alternately, and drying in an oven at 50° C. for 12 hours.
Citation Information
Patent Citations
Methods of preparing organic boron compound and beta-carbonyl compound by catalyzing copper ion loaded chitosan microspheres
CN107573370A
Preparation method for preparing beta-boryl ketone with substituent group at alpha position under catalysis of chitosan-loaded copper material
CN113563370A