Method for producing an internal stop in a tube member
Through axial cold forming and multi-step mold forming technology, the problems of time-consuming manufacturing of the internal stop portion of the pipe member and high tool cost are solved, and efficient and precise molding of high-strength steel alloy materials are achieved.
Patent Information
- Application Number
- CN202111494951.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-12-09
- Filing Date
- 2021-12-08
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2041-12-08
AI Technical Summary
The prior art consumes a long time and has high tool technology cost when manufacturing the internal stop portion of the pipe member, especially in the rolling process of high-strength steel alloys, which can easily lead to surface rupture or rolling impurities.
Using the axial cold forming method, the inner diameter of the tube member is reduced through a multi-step mold forming process, forming a conical transition area and compensating the depression and protrusions thereon, and then using the internal mold to widen and calibrate the precise interior. The stop portion avoids the use of radially offset dies and external dies.
The manufacturing process is simplified, tool cost and time consumption is reduced, and the accuracy and quality of the internal stop is improved, especially suitable for high-strength steel alloy materials.
Smart Images

Figure CN114618926B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for producing an internal stop in a pipe component. Background Art
[0002] DE102018108546A1 discloses a pipe element for a gas pressure container. The pipe element has a plurality of longitudinal sections. Recesses can be arranged between the sections. The recesses can be produced by roll forming, crimping or extrusion.
[0003] DE102018105445A1 discloses a housing for a gas generator module of an airbag system for a motor vehicle, wherein the tubular housing has a plurality of embossings pointing to the interior of the housing, which act as stops for internal components. To produce the embossings, an inner mandrel is used, and each embossing is pressed inward from the outside at points.
[0004] DE102018123316A1 discloses a pipe element for a gas pressure vessel and a method for producing the same. The production is carried out in multiple stages including at least one warm forming method step, which is implemented as axial compression. Different tools are used for the individual method steps. The axial compression is used to produce radially outwardly pointing projections, which are formed by material thickening.
[0005] Known rolling processes for producing depressions and similar geometric structures of the inner stop are relatively time-consuming processes. The production of the individual depressions distributed over the circumference is relatively complex in terms of tool technology. Furthermore, in the rolling process, especially of high-strength steel alloys, so-called rolling burnishing and rolling over have proven to be disadvantageous, which in the worst case can lead to surface cracks or pitting and / or the rolling in of foreign matter. Summary of the invention
[0006] The object of the present invention is to improve a method for producing an inner stop both with regard to the time consumption and with regard to the outlay in tool technology.
[0007] To this end, the present invention proposes a method for manufacturing an internal stopper in a pipe component, the method comprising the following steps:
[0008] a) providing a tubular member made of steel comprising a first end and a second end;
[0009] b) reducing the inner diameter D4 of the first end by means of a relative movement between the tube and a first die receiving the tube internally, the first die having an inner diameter D2 smaller than the outer diameter D1 of the tube, and for forming the tube, the relative movement being carried out in the axial direction of the tube, wherein a conical first region between the first end with the reduced inner diameter D4 and the second end is produced;
[0010] c) forming the conical first region by means of a relative movement of a further die in the axial direction of the tube component in the direction of the second end, thereby producing a circumferential depression on the outside and a projection on the inside with an inner diameter D5 in a longitudinal section of the conical first region, wherein the inner diameter D5 is smaller than the inner diameter D4 of the first end, and forming the conical second region in the direction of the second end following the depression by the further die;
[0011] d) While the tube component is supported on the outside in the mold cavity of the external mold, the first end is widened by means of at least one internal mold which is axially introduced into the first end, and an inner contour including an internal stop is formed by placing the radial outer surface of the first end in flat contact with the mold cavity for calibration, wherein, in order to produce the internal stop during the calibration process, the mold cavity has an inwardly protruding circumferential projection, which engages in a concave recess in the outer surface in the area of the recess, so that the at least one internal mold is pressed against the projection and the tube component is pressed against the projection.
[0012] The method according to the invention is used for producing an inner stop in a tubular component and has a plurality of steps, which can be regarded as only axial forming and in particular axial cold forming.
[0013] First, a steel tube component having a first end and a second end is provided. In the context of the method described here, the second end should not be deformed. It can be used as a support. Shaping takes place only in the region of the first end. The invention does not exclude that further method steps are carried out on the second end, as described, for example, in DE 10 2018 123 316 A1.
[0014] The inner diameter of the first end is reduced. This is done by a relative movement between the tube member and a first die that receives the tube member internally. For this purpose, the die has an inner diameter that is smaller than the outer diameter of the tube member at least in one region.
[0015] The relative movement is carried out in particular in the following manner: the die is moved relative to the fixed tube component. This involves axial shaping. In this axial shaping, the diameter is reduced only in the region of the first end. A conical transition is produced between the first and second ends, determined by the different diameter regions of the die. On the inlet side, the die has such a large diameter that the tube component can be accommodated in the die in particular. At a distance from the end on the inlet side, the inner diameter of the die is reduced in the conical transition region, corresponding to the desired outer diameter and the corresponding desired contour of the first end.
[0016] The next manufacturing step can be called compensation setting (Nachsetzen) with respect to the previously manufactured conical area of the tube component. Another die is used, which of course does not act on the already formed cylindrical first longitudinal section of the first end, but only on the conical area in the transition between the formed first end and the unformed second end. This conical area is deformed in that it is radially displaced inwards by the die that moves only axially. The conical second area is formed by the die at a distance from the conical area that is pressed radially inwards during this period. The steel used here is arched inwards in the area of the initial conical area, so that a recess that surrounds the outside radially is produced. The recess determines the surrounding bulge that protrudes inwards.
[0017] In the next step, the first end is widened by means of at least one inner die. The inner die is introduced into the first end and moved in the axial direction. The first end is located in the die cavity of the outer die. The inner contour with the desired inner stop should be formed by the radial outer surface of the first end being flatly placed in contact with the die cavity (calibrated).
[0018] By means of this final calibration with the aid of the inner mold, the final inner contour with the desired inner stop is produced. The inner contour is calibrated in such a way that the material of the tube component bears on the inner side with its outer surface on the mold cavity. In order to produce the inner stop during the calibration process, the mold cavity has a peripheral projection protruding inwards, which engages in a concave recess in the outer surface in the region of the recess. As a result, the inner mold can be pressed against the projection and the tube component can be pressed against the projection, and the inner contour is thus precisely defined, i.e. calibrated.
[0019] At least one radially circumferential stepped shoulder should be produced by means of the second inner mold. The stepped shoulder is spaced apart from the end side of the first end. The inner stop is formed in the transition region between the step portion with a smaller inner diameter and the step portion with a larger inner diameter of the stepped shoulder. The step portion with a smaller inner diameter is at a greater distance from the first end. The diameter of the step portion increases towards the first end, i.e. in the molding direction opposite to the axial direction.
[0020] All inner diameters changed by the forming according to the method according to the invention are preferably set smaller in the finished component than the inner diameter of the longitudinal section of the tubular component that has not been formed in this way. In other words, the inner diameter of the formed first end is smaller than the inner diameter of the unformed second end, even if the inner diameter of the first end is widened again in the second half of the method.
[0021] With regard to the step shape of the inner diameter, the area with the smallest inner diameter is the farthest from the first end. Therefore, the step with a larger inner diameter is upstream of the smaller step in the forming direction. This makes it possible to use a relatively simple internal mold as a calibration tool, which can be produced without undercuts. Due to the only axial forming, there is no need to provide a complex external mold including a radially deflectable die (the external mold causes radial deformation of the tube component from the outside). The stepped shoulder enables precise calibration in a relatively short length region.
[0022] For calibration, i.e. during the last forming stage, the mold cavity of the outer mold is constructed in such a way that the desired inner contour can be realized. At the same time, the outer contour is determined, which also depends on the desired wall thickness in the corresponding area. By forming in the area of the step with a larger diameter, a slightly larger wall thickness than in the undeformed longitudinal section of the tube member can be set. The step with a larger inner diameter is compressed slightly before the bulge to a certain extent during calibration in the last forming step. Preferably, the wall thickness difference is preferably very small (<5% of the wall thickness) and is especially only a few tenths of a millimeter in absolute terms over the entire forming area. Preferably, the wall thickness is substantially constant.
[0023] The inner stop formed as a radially surrounding projection does not necessarily have to extend in an axial plane. It can also be rounded in particular. The rounded area can be manufactured more simply, requires less forming force, and also produces less material stress in the tube component.
[0024] The pipe member should preferably be made of a high-strength steel alloy having a strength of Rm>780MPa, especially Rm>1050MPa. The pipe member can be seamless or welded. A preferred tempering treatment (hardening and annealing) is provided for the seamless pipe member provided by the method. The tempering treatment can be performed before or after the cold drawing of the pipe. When the cold drawing of the pipe is performed after the tempering treatment, the pipe is optionally annealed in a low-stress manner. After the stress-relieving annealing, the pipe is sheared to a desired length. When the tempering treatment is performed after the cold drawing, it is preferably sheared after the tempering treatment. The pipe member provided to the method according to the present invention is preferably a part of a pipe that has been heat-treated and cold-drawn as described above.
[0025] In summary, according to the method arrangement of the present invention, the initial inner diameter of the tube component is first reduced, and in the region of the conical transition, an inwardly directed protrusion and recess are formed by a compensating arrangement, and then the first end is widened again for the most part by an especially conical internal die and finally a desired inner contour with a stop is formed, which is feasible by the recess / protrusion previously manufactured by the compensating arrangement. The method steps (reduction, compensating arrangement, widening, calibration) are preferably all implemented as cold forming. The simple cold forming without additional active heat introduction shortens the duration of the manufacturing process, is low-cost and can be realized relatively simply. Combined with simple axial forming, the tool cost is reduced at the same time.
[0026] In an advantageous further development of the invention, the tubular component is manufactured as a housing of a gas generator module, and the stop produced by the method is used or produced for the positional orientation of the internal components of the gas generator module. The axial forming according to the invention, in particular as a simple cold forming, is preferably carried out on the combustion chamber side of the housing to be produced. The combustion chamber side or the first end has a different function than the opposite second end of the housing.
[0027] The housing is essentially a cylindrical tube component that is partially molded. The tube component must withstand very high loads for a short period of time when the gas generator is triggered, that is, it must be particularly rupture-proof. When the outer diameter is about 30 mm, the typical wall thickness is in the range of about 2 mm. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] The method according to the invention is explained below with reference to an exemplary embodiment shown in the merely schematic drawings. In the drawings:
[0029] Figure 1 A simplified illustration of a longitudinal section through a profiled region of a tube component serving as a housing for a gas generator module;
[0030] Figures 2.1 to 2.4 The chronological sequence of the four manufacturing steps in the first forming die is shown;
[0031] Figures 3.1 to 3.4 The chronological sequence of the four production steps in the second forming tool is shown:
[0032] Figures 4.1 to 4.4 shows the temporal sequence of four manufacturing steps in the third forming die;
[0033] Figures 5.1 to 5.4 shows the temporal sequence of four manufacturing steps in a fourth forming die;
[0034] Figure 6 showing a formed first end portion of a tube member;
[0035] Figure 7 Show Figure 6 Details of VII. DETAILED DESCRIPTION
[0036] Figure 1 The longitudinal section of a partial region of a tubular housing 2 of a gas generator module is shown. The tubular housing 2 is produced from an initially cylindrical tube component 1, wherein the Figures 2.1 to 5.4 Explain the further manufacturing steps of axial cold forming. Figure 1 The depression 8 is shown, which is formed radially outwardly and circumferentially and has different diameter regions (inner diameters D6 and D7 ) at the steps 23 , 24 of the step shoulder 21 , wherein the stop 22 is formed between the steps 23 , 24 .
[0037] According to the method of the present invention, a pipe component 1 made of high-strength steel (Rm>780MPa) is used. Figure 2.1 The first die 4 has an inner diameter D2 ( Figure 2.2 ), the inner diameter is smaller than the outer diameter D1 of the tube member 1. The second end 5 is axially supported and / or held in a manner not further shown. The first die 4 moves axially in the direction of the arrow P1. The initial inner diameter D3 of the tube member 1 is reduced to a smaller inner diameter D4.
[0038] Figure 2.3 The lower end position of the first mold 4 is shown. Figure 2.4 It is shown how the die 4 is moved back to the starting position in the direction of the arrow P2. The inner contour of the first die 4, which is stepped in the inner diameter D2, has been transferred to the tube component 1. A conical first region 6 is formed, which is located between the undeformed second end 5 and the deformed first end 3. The first end 3 is slightly stretched by this shaping. The transition between the conical region 6 and the first end 3 or the second end 5 is rounded.
[0039] In the second forming stage ( Figures 3.1 to 3.4 ). This means that the already formed cylindrical part of the first end 3 is no longer formed, but the conical region 6 is formed. For this purpose, a further mold 7 is used, which also has a stepped shape, so that only the conical first region 6 is reshaped. Figure 3.2 It is shown how the further die 7 is moved in the axial direction in the direction of the arrow P1 . Figure 3.3 The mold is shown in the lower end position. The conical first region 6 is deformed, wherein a circumferential depression 8 and an inwardly protruding projection 25 are now produced in the initial length region of the conical first region 6. The wall region is offset radially inwards at the height of the depression 8. The inner diameter D5 of the projection 25 is smaller than the inner diameter D4 of the already formed cylindrical first end 3.
[0040] In the axial direction, the radially outer circumferential depression 8 is followed by a widening conical second region 9, which is formed by the die 7 and forms the transition to the still undeformed second end 5. The transition is smooth. The conical second region 9 is steeper than the conical first region 6, which is due to the corresponding shaping of the further die 7, such as by means of Figure 2.4 and 3.4 This can be seen from the comparison. Figure 2.4 and 3.4 The molds 4 and 7 are each shown in an upward movement in the direction of the arrow P2 and simultaneously the tube component 1 as a result of the corresponding forming phase.
[0041] Figures 4.1 to 4.4 The next manufacturing step is shown. Figure 3.4 The tube component 1 with a contour is placed in an outer mold 10 having a mold cavity 11. The mold cavity 11 is contoured, ie not only cylindrical, and determines the later outer shape of the tube component 1.
[0042] The inner mold 12 is introduced into the tube component 1 from the first end 3 in the direction of the arrow P1, whereby the tube component 1 is widened. The first inner mold 12 has a truncated cone-shaped tip 13, which is followed by a cylindrical shaft 14. According to the contour of the first inner mold 12, a cylindrical contour is produced in the upper region of the first end 3 and a conical contour is produced in the region where the tip 13 comes into contact with the tube component 1, for example, up to the height of the depression 8 or the inwardly directed protrusion 25.
[0043] Figure 4.3 The lower end position of the first inner mold 12 is shown. Figure 4.4 The upward movement of the first inner mold 12 in the outer mold 10 (arrow P2 ) and the contour of the tube component 1 after completion of this production step are shown again.
[0044] Figure 4.4 It is also shown that the tube component 1 lies with its cylindrical outer surface 15 on the mold cavity 11 in the region of the first end 3. In the more heavily contoured region, adjacent to the depression 8, the tube component 1 does not yet lie on the mold cavity 11 of the outer mold 10.
[0045] The final calibration is done with Figures 5.1 to 5.4 Explanation. Figure 4.4 The profile of the pipe member 1 in Figure 5.1 The second internal mold 16 has a head 17 ( Figure 5.2 A thinner shaft 18 is connected to the head 17 ( Figure 5.3). The second inner mold 16 has three graded diameter regions as the active surface for forming. The region with the largest diameter of the head 17 first contacts the first end 3 of the tube member 1 and calibrates the inner diameter of the first end 3 over most of its length.
[0046] The smaller diameter region of the head is upstream in the axial direction and in the forming direction. Two further smaller diameter regions are also provided in the mold cavity 11 corresponding to the contour of the head 17. The mold cavity 11 has a projection 19 in the region of the depression 8, which engages in the depression 8.
[0047] Figure 5.3 The lower end position of the second inner mold 16 is shown. In the region of the projection 19, the depression 8 in the wall of the tube component 1 is pressed outwardly toward the mold cavity 11. The material is pressed in particular against the projection 19 of the mold cavity 11. As a result, the region with the smallest inner diameter is formed, thereby producing an inner contour 20 with a circumferential stepped shoulder 21, as shown in FIG. Figure 5.4 As shown in .
[0048] exist Figure 5.4 , the second inner mold 16 is in the stage of upward movement in the direction of the arrow P2. The formed pipe component 1 can now be removed from the outer mold 10.
[0049] FIG. 2 shows an enlarged view of the finished stepped shoulder 21 , which is connected to the end side 26 ( Figure 5.4 ). The step shoulder 21 has an inner stop 22, which is arranged at the transition area between a smaller step 23 in the inner diameter D6 and a larger step 24 in the inner diameter D7 via a transition section. The larger step 24 is upstream of the smaller step 23 corresponding to the contour of the second inner mold 16.
[0050] Figure 6 and 7 Further details are shown in the region of the step shoulder 21. The larger step 24 has a greater axial length L1 than the rounded stop 22, which has a length L2. Furthermore, the length L1 of the larger step 24 is also greater than the length L3 of the smaller step 23 in diameter. The length L3 of the smaller step 23 is greater than the length L2 of the stop.
[0051] Figure 6 and 7It is also shown that the substantially cylindrical length region of the end face of the first end 3 upstream of the formed step shoulder 21 has a larger inner diameter D8 than the larger step D7. At the same time, the wall thickness W1 is substantially constant over the entire formed region. Only a small thickening is given in the region of the larger step 24, which in this embodiment is approximately 1 / 10 mm. In the case of a wall thickness W1 of 1.5 mm to 3 mm and a thickening of 15% to 20% of the wall thickness W, the outer diameter D1 is preferably in the range of 20 mm to 50 mm.
[0052] Figure 6 and 7 The radius R is also shown. The radius R is not the same size. Except between the stop 22 and the smaller step 23, all transitions are smooth. The diameter is only indicated in the essentially cylindrical region. The outer diameter D9 in the region of the largest deformation in diameter is smaller than the outer diameter D10 of the larger step 24. In addition, the ratio between the outer diameters D1, D9 in the undeformed second end 5 and in the deformed region can be indicated by the following equation: D9=0.9-1.0xD1.
[0053] In the region of the length of the stop 22, the depression 8 has a rounded transition radially outward to a larger step 24 in the outer diameter D10. The depth T1 of the depression 8 relative to the outer diameter D10 of the larger step 24 is in the range of 0.3 mm to 1 mm. The rounded depression 8 transitions into the undeformed region of the second end 5 via another rounded transition with a radius R.
[0054] Reference numerals list
[0055] 1. Pipe components
[0056] 2 Shell
[0057] The first end of 31
[0058] 4First mold
[0059] The second end of 51
[0060] 61 cone-shaped first area
[0061] 7 Additional molds
[0062] The depression in 81
[0063] 91 conical second area
[0064] 10 External mold
[0065] 1110 mold cavity
[0066] 12First internal mold
[0067] 1312 Tip
[0068] 1412 Axis
[0069] The outer surface of 151
[0070] 16 Second internal mold
[0071] 1716 Head
[0072] 1816 Axis
[0073] The Bulge of 1910
[0074] Inner contour of 201
[0075] 211 stepped shoulder
[0076] 221 stopper
[0077] The smaller step section of 2321
[0078] The larger step section of 2421
[0079] 25 in 8 of the bulges
[0080] 263 end side
[0081] D11 initial outer diameter
[0082] D24 inner diameter
[0083] D31 initial inner diameter
[0084] Reduced inner diameter of D41
[0085] D5 is the inner diameter of 1 in the recess 8
[0086] Inner diameter of D623
[0087] Inner diameter of D724
[0088] Inner diameter of D83
[0089] Outer diameter of D93
[0090] The outer diameter of D1024
[0091] Axial length of L124
[0092] Axial length of L222
[0093] Axial length of L323
[0094] P1 axial movement direction
[0095] P2 axial movement direction
[0096] R Radius
[0097] T18's Depth About D10
[0098] Wall thickness of W11
Claims
1. A method for manufacturing an internal stopper (22) in a pipe component (1), the method comprising the following steps: a) providing a tube member (1) made of steel comprising a first end (3) and a second end (5); b) reducing the inner diameter D4 of the first end portion (3) by means of a relative movement between the tube member (1) and a first die (4) receiving the tube member (1) therein, the first die (4) having an inner diameter D2 smaller than the outer diameter D1 of the tube member (1), and for forming the tube member (1), the relative movement is performed in the axial direction of the tube member (1), wherein: Producing a conical first region (6) between the first end (3) and the second end (5) with a reduced inner diameter D4; c) forming the conical first region (6) by means of a relative movement of a further die (7) in the axial direction of the tube component (1) in the direction of the second end (5), thereby generating a circumferential depression (8) on the outside and a projection (25) with an inner diameter D5 on the inside in a longitudinal section of the conical first region (6), wherein the inner diameter D5 is smaller than the inner diameter D4 of the first end (3), and forming a conical second region (9) in the direction of the second end (5) following the depression (8) by the further die (7); d) While the tube component (1) is supported on the outside in a mold cavity (11) of an external mold (10), the first end (3) is widened by means of at least one internal mold which is axially introduced into the first end (3), and an inner contour (20) including an internal stop (22) is formed by placing the radial outer surface (15) of the first end (3) flatly in contact with the mold cavity (11) for calibration, wherein, in order to produce the internal stop (22) during the calibration process, the mold cavity (11) has an inwardly protruding circumferential projection (19), which engages in a concave recess in the outer surface in the region of the recess (8), so that the at least one internal mold is pressed against the projection (25) and the tube component (1) is pressed against the projection (19).
2. The method according to claim 1, characterized in that The widening of the first end (3) is carried out by means of a first inner tool (12) and the shaping of the inner contour (20) is subsequently carried out in the region of the projection (25) by means of a second inner tool (16).
3. The method according to claim 2, characterized in that When the inner contour (20) is formed, at least one circumferential stepped shoulder (21) is produced, which is spaced apart from the end side (26) of the first end (3), and the inner stop (22) is formed in the transition area between the step (23) with a smaller inner diameter D6 and the adjacent step (24) with a larger inner diameter D7.
4. The method according to claim 3, characterized in that The inner diameter D7 of the larger step portion (24) is adjusted to be smaller than the inner diameter D8 of the first end portion (3), which is located upstream of the larger step portion (24).
5. The method according to claim 3 or 4, characterized in that: By forming in the region of the step ( 24 ) with a larger inner diameter D7 , a greater wall thickness W1 is provided than in the undeformed longitudinal section of the tube component ( 1 ).
6. The method according to any one of claims 1 to 4, characterized in that The inner stop (22) is rounded or chamfered.
7. The method according to claim 3, characterized in that The axial length L1 of the step portion (24) with a larger inner diameter D7 is greater than the length L3 of the step portion (23) with a smaller inner diameter D6.
8. The method according to any one of claims 1 to 4, characterized in that A pipe component (1) is provided which is made of a high-strength steel alloy having a strength of Rm>780 MPa.
9. The method according to any one of claims 1 to 4, characterized in that At least one of the forming operations is performed as cold forming.
10. The method according to any one of claims 1 to 4, characterized in that The tube component (1) is manufactured as a housing (2) of a gas generator module, wherein the inner stop (22) is manufactured for the positional orientation of an inner component of the gas generator module.
11. The method according to claim 10, characterized in that The method is carried out on the combustion chamber side of the housing (2) to be produced.
12. The method according to claim 2, characterized in that When the inner contour (20) is formed with a second inner mold (16), at least one circumferential stepped shoulder (21) is produced, which is spaced apart from the end side (26) of the first end (3), and the inner stop (22) is formed in the transition area between the step (23) with a smaller inner diameter D6 and the adjacent step (24) with a larger inner diameter D7.
13. The method according to any one of claims 1 to 4, characterized in that A pipe component (1) is provided which is made of a high-strength steel alloy having a strength of Rm>1050 MPa.