A dustproof film assembly and a method of using the same
By designing a ring-shaped dust-proof film component that is bonded on one side, the problems of delamination and residual glue in MEMS patch assembly are solved, the sound and air permeability performance is improved, and the components can be easily peeled off and efficiently bonded.
Patent Information
- Application Number
- CN202210110778.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-01-29
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2042-01-29
AI Technical Summary
During the assembly process of MEMS patches, dust-proof film components are prone to delamination and residual glue problems, which affect the air and sound permeability performance of MEMS.
Design a dust-proof film component with one-sided bonding. The adhesive piece has a ring-shaped structure and runs through it to form an opening along its thickness direction. It is only bonded to the PCB board in the edge area and the inner area is bonded to the dust-proof film, reducing Overall thickness to facilitate peeling, and avoid delamination and residual glue by controlling glue layer thickness and bond strength.
It effectively avoids delamination, ensures the sound and air permeability of MEMS, reduces the amount of residual glue, makes the contact area between the adhesive part and the PCB board moderate, and improves the operational convenience and bonding strength of the component.
Smart Images

Figure CN114745646B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of film materials, and in particular to a dustproof film component used in a surface mount technology (SMT) process and a use method thereof. Background Art
[0002] With the progress of society, people have higher and higher requirements for electronic products such as mobile phones and laptops. They not only hope that the performance of these electronic products will be higher and higher to meet people's various work needs, but also hope that the size of these electronic products will be smaller and smaller so that people can carry them more conveniently. Therefore, the size of the corresponding electronic parts also needs to be continuously reduced, while the performance and consistency need to be continuously improved.
[0003] In the above context, MEMS, an electronic component, has attracted much attention. MEMS is a micro-electromechanical system, also known as a micro-electromechanical system. It refers to a high-tech device with a size of several millimeters or even smaller. Its internal structure is generally in the micrometer or even nanometer level. It is an independent intelligent system. It is mainly composed of three parts: sensors, actuators, and micro-energy. MEMS involves multiple disciplines and engineering technologies such as physics, semiconductors, optics, and bioengineering, and has opened up a wide range of uses in the fields of intelligent systems, consumer electronics, and smart homes.
[0004] This product is suitable for the process protection of silicon microphones (MEMS mic) in surface mount assembly (SMT); the ASICs and MEMS of silicon microphones may be contaminated by dust (the cleanliness of SMT workshops is generally not high) and flux (such as rosin) during the SMT process, which may affect the integrity of the function or directly cause it to fail, so a dustproof film is needed to protect the process.
[0005] In the related art, a protective film, a first double-sided adhesive layer, a second double-sided adhesive layer and a dustproof film are interconnected to obtain a dustproof film assembly, wherein the bottom surface of the protective film is bonded to the upper surface of the first double-sided adhesive layer, the bottom surface of the first double-sided adhesive layer is bonded to the upper surface of the dustproof film, the bottom surface of the dustproof film is bonded to the upper surface of the second double-sided adhesive layer, and the bottom surface of the second double-sided adhesive layer is bonded to the PCB board; firstly, in order to ensure that the entire dustproof film assembly is stably fixed on the PCB board, the second double-sided adhesive layer needs to have a suitable contact area with the PCB board; this contact area cannot be too small, and after processes such as reflow soldering, the second double-sided adhesive layer will be tightly adhered to the PCB board. When the dustproof film assembly is torn off, the glue in the second double-sided adhesive layer remains on the PCB board, thereby affecting the air permeability and sound permeability of the MEMS on the PCB board; secondly, since the dustproof film assembly has a four-layer structure, when the dustproof film assembly needs to be torn off, stratification is likely to occur between its internal structures, making it difficult for the entire dustproof film assembly to be completely peeled off from the PCB board, thereby causing the entire MEMS to be scrapped. Summary of the invention
[0006] The object of the present invention is to provide a dustproof film assembly, the thickness of which is greatly reduced, which can better avoid the occurrence of stratification, does not produce residual glue, and has good sound permeability and air permeability.
[0007] To achieve the above object, the present invention adopts the following technical solutions:
[0008] A dustproof film assembly, used for protecting silicon microphones during patch assembly, comprising an adhesive member with single-side bonding and a dustproof film for dustproof and breathable use;
[0009] The adhesive member is an annular structure, and an opening is formed through the adhesive member along the thickness direction thereof;
[0010] The adhesive member includes a substrate layer and a glue layer arranged along the thickness direction thereof, and the edge area of the adhesive member is bonded to the PCB board through the glue layer; the remaining area is bonded to the dustproof film through the glue layer;
[0011] The diameter of the dustproof film is greater than the inner diameter of the adhesive member; the dustproof film covers the opening, and the dustproof film covers the PCB board.
[0012] In the related art, the occurrence of delamination and residual glue is reduced by selecting appropriate double-sided adhesive and dust-proof film; but it is not easy to think of changing the overall structure of the film assembly, that is, the structure formed by the single-sided adhesive and the dust-proof film provided by the present invention. The dust-proof film assembly provided by the present invention has a smaller volume, and the adhesive is provided with a glue layer only on one side of the adhesive, that is, one side of the adhesive is sticky, and the adhesive is respectively bonded to the dust-proof film and the PCB board through the glue layer. The adhesive and the dust-proof film form a two-layer structure. Compared with the four-layer structure in the prior art, the overall thickness of the dust-proof film assembly is greatly reduced; when the dust-proof film assembly needs to be torn off, the overall thickness of the dust-proof film assembly is reduced, so that it is easier to peel off the adhesive and the PCB board, and the dust-proof film assembly can be completely peeled off from the PCB board, which is better. To avoid the occurrence of stratification, secondly, in the related art, since the dust-proof film is bonded to the first double-sided tape and the second double-sided tape at the same time, when the stickiness on both sides of the dust-proof film exists but not at the same time, it is easy to cause stratification inside the dust-proof film assembly. The present invention uses an adhesive with a glue layer on one side, and the adhesive is bonded to the dust-proof film through the glue layer. At the same time, since the PCB board is not sticky, there is no bonding relationship between the PCB board and the dust-proof film, that is, there is no situation where the stickiness on both sides of the dust-proof film is different, which can effectively avoid the occurrence of stratification inside the dust-proof film assembly; the contact area between the PCB board and the glue layer in the adhesive is moderate, so that after the dust-proof film assembly is torn off, it is not easy for residual glue to appear on the PCB board, thereby making the MEMS arranged on the PCB board have better sound permeability and air permeability.
[0013] Preferably, a sticky protrusion is provided on the side of the adhesive member, and the dustproof film assembly further comprises a handle bonded to the protrusion.
[0014] The protrusion is sticky on one side, specifically, the side of the protrusion close to the PCB board is sticky. The protrusion can be of any shape, and the handle can be of any shape. The handle is adapted to the shape of the protrusion to reduce the adsorption of impurities. When the dustproof film assembly needs to be torn off, since the protrusion is a part of the adhesive, and the adhesive is bonded to the dustproof film through the glue layer, the entire adhesive and the dustproof film can be torn off from the PCB board by acting on the protrusion with the handle, which has better operational convenience compared with robot operation.
[0015] Preferably, the area where the edge of the adhesive member is bonded to the PCB board is the bonding area, the bonding area is annular, the average width of the bonding area is 0.2 mm-0.6 mm, and the thickness of the dustproof film is 2-20 μm.
[0016] In the dustproof film assembly provided by the present invention, the maximum width of the bonding area and the minimum width of the bonding area are equal or unequal. When they are equal, they are equal to the average width, which is convenient for operation and easy assembly; when they are unequal, it is suitable for certain special fields. The average width of the bonding area is the average of the sum of the maximum width of the bonding area and the minimum width of the bonding area. The average width of the bonding area cannot be too large or too small. The average width of the bonding area is preferably 0.2mm-0.6mm. While ensuring the bonding strength, no residual glue is generated. When the average width of the bonding area is less than 0.2mm, the area where the adhesive is directly bonded to the PCB board is too small, so that the adhesive is easy to fall off. When the average width of the bonding area is greater than 0.6mm, the bonding strength is too large, and after the dustproof film assembly is torn off, the residual glue is too large. The thickness of the dustproof film cannot be too large or too small. When the thickness of the dustproof film is greater than 20μm, a gap will be generated between the side of the adhesive with the handle and the PCB board, so that the contact area between the adhesive and the PCB board at this location is reduced. When the thickness of the dustproof film is less than 2μm, the dustproof effect on the PCB board will be reduced.
[0017] Preferably, the center of the dustproof film is offset from the center of the adhesive, and the center of the dustproof film is located on the side of the adhesive away from the handle; the width of the adhesive area close to the handle is greater than the width of the adhesive area away from the handle.
[0018] The dustproof film assembly provided by the present invention has a certain thickness for both the protrusion and the handle, so the bonding area close to the handle will first move downward and then upward, and the actual contact area between the PCB board and the bonding area close to the protrusion is reduced, resulting in weak bonding. Therefore, the present invention displaces the center of the dustproof film and the center of the adhesive so that the width of the bonding area close to the handle is greater than the width of the bonding area away from the handle, thereby obtaining a moderate size of the bonding area, so that the adhesive and the PCB board have a more suitable contact area.
[0019] Preferably, the width of the bonding area close to the handle is 0.3-0.8 mm, and the width of the bonding area away from the handle is 0.1-0.5 mm; the ratio of the width of the bonding area away from the handle to the outer diameter of the bonding piece is not less than 4%.
[0020] The dustproof film assembly provided by the present invention not only meets the bonding strength between the adhesive and the PCB board and does not generate residual glue, but also has a moderate size of the bonding area, so that the adhesive and the PCB board have a more suitable contact area; the width of the bonding area close to the handle is not equal to the width of the bonding area away from the handle. The width of the bonding area close to the handle, that is, the maximum width of the bonding area, when the width of the bonding area close to the handle is greater than 0.8mm, the bonding strength at this location is too large, and residual glue will be generated. When the width of the bonding area close to the handle is less than 0.3mm, a gap will be generated between the adhesive and the PCB board, so that the contact area between the PCB board and the adhesive at this location is too small; the width of the bonding area away from the handle, that is, the minimum width of the bonding area, when the width of the bonding area away from the handle is less than 0.1mm, and the ratio of the width of the bonding area away from the handle to the outer diameter of the adhesive is less than 4%, the contact area between the PCB board and the adhesive away from the handle is reduced, so that the bonding strength is reduced, and debonding will occur.
[0021] Preferably, the ratio of the average width of the bonding area to the outer diameter of the bonding element is 0.06-0.2:1.
[0022] The dustproof film assembly of the present invention has sufficient bonding strength between the adhesive member and the PCB board.
[0023] Preferably, the thickness of the glue layer is 5-80 μm, and the bonding strength of the glue layer is 5N / 25mm-30N / 25mm;
[0024] The high-temperature overflow of the glue layer is no more than 50 μm @ 280°C·3min;
[0025] The surface energy of the dustproof film is 15-30 mN / m.
[0026] The glue layer uses a pressure-sensitive adhesive, which has good viscosity at room temperature. During the reflow soldering process, the glue layer of the adhesive may be partially melted. The melted glue will become fluid and then penetrate into the dust-proof film. The glue will block the film pores, reducing the porosity of the dust-proof film, thereby affecting the sound permeability and air permeability. The dust-proof film assembly provided by the present invention can solve the above problems. The specific analysis is as follows:
[0027] First, by controlling the thickness of the glue layer to 5-80μm, not only the bonding strength is guaranteed, but also the reduction of the porosity of the dustproof film due to the melting of the glue layer can be avoided. The thickness of the glue layer should not be too large or too small. When the thickness of the glue layer is less than 5μm, the bonding strength is greatly reduced due to being too thin, and debonding is likely to occur. When the thickness of the glue layer is greater than 80μm, the glue layer is too thick, that is, the glue becomes more, which increases the amount of melted glue. The melted glue penetrates into the dustproof film, reducing the porosity of the dustproof film. rate, thereby affecting the sound permeability and air permeability; the bonding strength of the glue layer is controlled within 5N / 25mm-30N / 25mm, which not only has sufficient bonding strength, but also ensures that there is no residual glue on the PCB board after the dustproof film assembly is torn off, thereby making the MEMS arranged on the PCB board have good sound permeability and air permeability. When the bonding strength of the glue layer is less than 5N / 25mm, the viscosity is not enough and it is easy to debond. When the bonding strength of the glue layer is greater than 30N / 25mm, the bonding strength is too large and residual glue will be generated.
[0028] Secondly, the high-temperature overflow of the glue layer is set to be no more than 50μm@280℃·3min. The high-temperature overflow, i.e., the fluidity of the glue layer after melting at high temperature, is reflected by testing the length of the glue layer flowing after melting at high temperature. By making the glue layer flow more slowly at high temperature, the glue penetrating into the dustproof film can be reduced, thereby better ensuring the porosity of the dustproof film, and thereby making the MEMS arranged on the PCB board have better sound permeability and air permeability.
[0029] Finally, the surface energy of the dust-proof film is set to 15-30mN / m, and the oleophobic level of the dust-proof film surface is greater than or equal to level 6, so that the dust-proof film has good oleophobic performance, and further makes it difficult for the melted part of the glue layer to flow on the dust-proof film, and the glue is not easy to penetrate into the dust-proof film, thereby better ensuring the porosity of the dust-proof film. In addition, it can also prevent wetting by flux (rosin). When the surface energy of the dust-proof film surface is greater than 30mN / m and the oleophobic level of the dust-proof film surface is less than level 6, the oleophobic performance of the dust-proof film is poor, which will cause the melted part of the glue layer to flow on the dust-proof film, thereby affecting the porosity of the dust-proof film.
[0030] Preferably, the area where the adhesive member is bonded to the dustproof film is a mucosal area, the mucosal area is annular, and the average width of the mucosal area is 0.3-0.8 mm.
[0031] In the dustproof film assembly provided by the present invention, the average width of the mucous membrane area is the average of the sum of the maximum width of the mucous membrane area and the minimum width of the mucous membrane area. The average width of the mucous membrane area cannot be too large or too small. When the average width of the mucous membrane area is less than 0.3 mm, the area directly bonded to the dustproof film is too small, making the dustproof film easy to fall off.
[0032] Preferably, the ratio of the average width of the mucosal area to the diameter of the dustproof film is 0.2-0.4:1.
[0033] The dustproof film assembly provided by the present invention has a ratio of the average width of the adhesive film area to the diameter of the dustproof film of 0.2-0.4:1, and an adaptive contact area is provided between the adhesive and the dustproof film, so that the adhesive and the dustproof film have sufficient bonding strength.
[0034] Preferably, the thickness of the adhesive member is 20-200 μm; the outer diameter of the adhesive member is 2 mm-4 mm, and the inner diameter is 0.6-2 mm.
[0035] The dustproof film assembly provided by the present invention has a thickness of the adhesive member of 20-200 μm, so that the dustproof film assembly as a whole has a moderate thickness and can be easily peeled off from the PCB board, effectively avoiding the stratification of the dustproof film assembly; the outer diameter of the adhesive member is 2mm-4mm, and the inner diameter is 0.6-2mm, which can obtain a contact area that is compatible with the PCB board and the dustproof film, not only meeting the bonding strength but also without any residual glue.
[0036] Preferably, the elastic modulus of the substrate layer is 50-300 MPa, the elastic limit deformation of the substrate layer is 0.5%-5%; the tensile strength of the adhesive is 100N / 25mm-300N / 25mm; the shear strength of the adhesive is 150-350kPa;
[0037] The ratio of the thickness of the substrate layer to the thickness of the glue layer is 1-4:1.
[0038] The dustproof film assembly provided by the present invention has a great influence on the detection of sound transmission performance because the dustproof film is attached to the sound hole on the back side of the PCB board. The elastic modulus of the substrate layer is 50-300MPa, and its elastic limit deformation is 0.5%-5%. The tensile strength of the adhesive is 100N / 25mm-300N / 25mm, and the shear strength of the adhesive is 150-350kPa, which is beneficial to improving the sound transmission performance; the ratio of the thickness of the substrate layer to the thickness of the glue layer is 1-4:1. First, the glue layer cannot be too thick; secondly, it is effectively ensured that the adhesive as a whole has good mechanical strength, so that the dustproof film assembly has good mechanical strength and can meet the needs of practical applications.
[0039] Preferably, the pore size of the dustproof film is 0.02-2μm, so that the dustproof film assembly has good sound permeability and air permeability; the diameter of the dustproof film is 1mm-3mm, so that the dustproof film and the adhesive have an adaptive contact area and sufficient bonding strength; the ratio of the thickness of the dustproof film to the thickness of the adhesive is 1:2-1:12, and the adhesive can provide sufficient bonding strength to effectively prevent stratification between the adhesive and the dustproof film when the dustproof film assembly is torn off.
[0040] Preferably, the dustproof film is a polytetrafluoroethylene film; the handle is polyimide; and the substrate layer is polyimide;
[0041] The thickness of the dustproof film assembly is 24-215 μm;
[0042] The sound loss of the dustproof membrane assembly is less than 1dB@1kHz.
[0043] The air permeability of the dustproof membrane assembly is 5000-150000ml / (min*cm 2 )@7KPa.
[0044] Polytetrafluoroethylene film is selected, and polyimide is selected for the handle and the base material. Firstly, the mechanical strength is high, and the entire dustproof film assembly has good strength to meet the needs of practical applications; secondly, it is resistant to high temperatures, and both materials can withstand high temperatures of 280°C; finally, the chemical properties are stable. For example, the polytetrafluoroethylene film is resistant to acid and alkali, and has stable performance.
[0045] The dustproof film assembly provided by the present invention needs to perform audio testing on the MEMS on the PCB board. Preferably, the sound barrier of the dustproof film assembly is less than 1dB@1kHz, and the air permeability of the dustproof film assembly is 5000-150000ml / (min*cm 2 )@7KPa, which makes the dustproof membrane assembly have better sound permeability and air permeability when MEMS is used for audio testing.
[0046] When sound passes through an object, a certain amount of loss will occur; this loss actually refers to the sound blocking amount of the object. The greater the sound blocking amount of the object, the greater the sound loss, and the smaller the sound blocking amount of the object, the smaller the sound loss. The test method for the sound blocking amount of the object is: punch the object to be tested into a disc with a diameter of 5.0mm, then stack the punched material to be tested and a ring-shaped double-sided tape with an outer diameter of 5.0mm and an inner diameter of 1.7mm concentrically, and the thickness of the double-sided tape is 0.15mm. Finally, the double-sided tape is attached to a microphone test board with a sound outlet hole of 1mm diameter and 0.8mm depth. The analog microphone is Knowles SPA1687LR5H. An artificial mouth is set 2cm away from the microphone tooling. Both the analog microphone and the artificial mouth are connected to the Audio Precision x525 audio analyzer. The audio test software provided by Audio Precision is used to make the artificial mouth emit a sound with a frequency of 20Hz-20000Hz and a sound pressure level of 94dBSPL. The response signals of the microphone end with and without the test component mounted on the surface of the microphone tooling are collected and subtracted to finally obtain the sound blocking amount of the corresponding object.
[0047] The thickness of the dustproof film assembly cannot be too large. The preferred thickness of the dustproof film assembly is 24-215 μm, so that the adhesive can be easily peeled off from the PCB board. The dustproof film assembly can be completely peeled off from the PCB board, which can better avoid the occurrence of stratification. At the same time, the appropriate thickness ensures that the dustproof and sound-transmitting membrane assembly not only has high mechanical strength, but also has high sound transmission performance, with very little sound loss.
[0048] The present invention also provides a method for using the dustproof film assembly, comprising the following steps:
[0049] The dustproof film assembly is attached to the sound hole of the PCB board during the silicon microphone board making process, wherein the silicon microphone board making process includes processes such as reflow soldering, sound permeability inspection and board separation process; the dustproof film assembly is torn off before the silicon microphone is packaged or used as a dustproof and sound-permeable film assembly built into the silicon microphone; this method of use effectively prevents the silicon microphone from being contaminated by dust and flux during the board making process, and the dustproof film in the dustproof film assembly is used for protection during the board making process.
[0050] Compared with the prior art, the present invention has the following beneficial effects:
[0051] The dustproof film assembly provided in the above technical solution has a small volume, and the adhesive and the dustproof film form a two-layer structure. Compared with the four-layer structure in the prior art, the overall thickness of the dustproof film assembly is greatly reduced; the adhesive is easy to peel off from the PCB board, and the dustproof film assembly can be completely peeled off from the PCB board, which can better avoid the stratification phenomenon; and, using an adhesive with a glue layer on one side, the adhesive is bonded to the dustproof film through the glue layer. At the same time, since the PCB board is not sticky, there is no bonding relationship between the PCB board and the dustproof film, that is, there is no situation where the stickiness on both sides of the dustproof film is different, which can effectively avoid the stratification phenomenon inside the dustproof film assembly; after tearing off the dustproof film assembly, there is no residual glue on the PCB board, so that the MEMS arranged on the PCB board has good sound permeability and air permeability. The use method of the dustproof film assembly provided in the above technical solution effectively prevents the silicon wheat board from being contaminated by dust and flux during the board making process, and the dustproof film in the dustproof film assembly is used as protection during the board making process. BRIEF DESCRIPTION OF THE DRAWINGS
[0052] Figure 1 This is a schematic structural diagram of a dustproof film assembly in one embodiment of the present invention;
[0053] Figure 2 for Figure 1 An exploded schematic diagram of the dust-proof membrane assembly shown;
[0054] Figure 3 for Figure 1 A schematic diagram of a dust-proof film assembly from one viewing angle is shown;
[0055] Figure 4 for Figure 1 A schematic top view of the dustproof membrane assembly shown;
[0056] Figure 5 for Figure 4 A cross-sectional schematic diagram of the dust-proof membrane assembly shown;
[0057] Figure 6 Schematic diagram of a dustproof film assembly in Embodiment 6 and Embodiment 7 of the present invention;
[0058] Figure 7 for Figure 6 A cross-sectional schematic diagram of the dust-proof membrane assembly shown;
[0059] Figure 8 Schematic diagram of a test device for the amount of glue overflow at high temperature in an embodiment of the present invention;
[0060] Fig. 9 A schematic cross-sectional view of a pair of proportional dust-proof membrane assemblies of the present invention;
[0061] Fig.10This is a schematic diagram of the structure of a dustproof film assembly and a PCB board in one embodiment of the present invention;
[0062] Fig.11 The present invention is a schematic structural diagram of an adhesive component in a dustproof film assembly.
[0063] Description of the accompanying symbols:
[0064] 1. Adhesive part; 11. Opening; 12. Protrusion; 13. Adhesive area; 14. Mucous membrane area; 15. Base material layer; 16. Glue layer; 2. Dust-proof film; 3. Handle; 4. Protective film; 51. First double-sided adhesive layer; 52. Second double-sided adhesive layer; 61. Weight; 62. Glue; 63. Rack; 7. PCB board. DETAILED DESCRIPTION
[0065] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0066] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0067] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0068] See also Figure 1-Figure 11 In an embodiment of the present invention, a dustproof film assembly is provided, wherein the area where the edge of the adhesive member 1 is bonded to the PCB board 7 is a bonding area 13, the bonding area 13 is annular, and the maximum width of the bonding area 13 is equal to or unequal to the minimum width of the bonding area 13. It is defined that: the minimum width of the bonding area 13 is a, and the maximum width of the bonding area 13 is b. Figure 3-5 As shown, when a and b are equal, they are equal to the average width, which is convenient for operation and easy assembly; Figure 6-7 As shown, when a and b are not equal, it is suitable for certain special fields, and the average width of the bonding area 13 is the average value of the sum of a and b.
[0069] like Figure 6-7 As shown, the center of the dustproof film 2 is offset from the center of the adhesive 1, and the center of the dustproof film 2 is located on the side of the center of the adhesive 1 away from the handle 3; the width of the adhesive area 13 close to the handle 3 is greater than the width of the adhesive area 13 away from the handle 3, that is, b>a.
[0070] like Fig.10 As shown, since both the protrusion 12 and the handle 3 have a certain thickness, the adhesive area 13 near the handle 3 will first move downward and then upward, and the actual contact area between the PCB board 7 and the adhesive area 13 near the protrusion 12 is reduced. Figure 4 As shown, the contact area is the area around point b, which makes the bonding weak. Therefore, Figure 6-7 As shown, in the embodiment of the present invention, the center of the dustproof film 2 is offset from the center of the adhesive member 1 so that the width (b) of the adhesive area 13 close to the handle 3 is greater than the width (a) of the adhesive area 13 away from the handle 3, thereby obtaining an appropriate size of the adhesive area 13, so that the adhesive member 1 and the PCB board 7 have a more suitable contact area.
[0071] like Fig.11 As shown, the adhesive member 1 is a single-sided adhesive, and the adhesive member includes a base material layer 15 and a glue layer 16 arranged along the thickness direction thereof.
[0072] Example 1
[0073] In this embodiment, a dustproof film assembly is provided for protecting the silicon microphone during the patch assembly process, comprising a single-sided adhesive member 1 and a dustproof and breathable dustproof film 2. The thickness of the dustproof film assembly is 200um, the sound barrier of the dustproof film assembly is 0.9dB@1kHz, and the air permeability of the dustproof film assembly is 5000ml / (min*cm 2 )@7KPa.
[0074] The adhesive member 1 is an annular structure, and an opening 11 is formed through the adhesive member 1 along its thickness direction, wherein a sticky protrusion 12 is provided on the side of the adhesive member 1, and the protrusion 12 is bonded to the handle 3, and the handle 3 is polyimide; the thickness of the adhesive member 1 is 180μm, the outer diameter of the adhesive member 1 is 2mm, the inner diameter is 0.6mm, the tensile strength of the adhesive member 1 is 100N / 25mm, and the shear strength of the adhesive member 1 is 150kPa.
[0075] The adhesive member 1 comprises a substrate layer 15 and a glue layer 16 arranged along the thickness direction thereof, the elastic modulus of the substrate layer 15 is 50 MPa, the elastic limit deformation of the substrate layer 15 is 0.5%, the ratio of the thickness of the substrate layer 15 to the thickness of the glue layer 16 is 4:1, and the substrate layer 15 is polyimide; the thickness of the glue layer 16 is 36 um, the bonding strength of the glue layer 16 is 5 N / 25 mm, the high temperature overflow of the glue layer 16 is 50 μm @ 280 ° C · 3 min, and the test method is: Figure 8 As shown, first, cut two pieces of 8cm*1cm glue 62, and stick them on the upper weight 61, with a sticking area of 1cm*1cm each, and the sticking positions of the two glues 62 should be 180° apart as much as possible; secondly, put the weight 61 on the shelf 63, stick the lower weight 61, with a sticking area of 1cm*1cm, 180° apart, and mark the positions of the upper and lower four sticking positions; finally, put the entire shelf 63 into a high-temperature oven, with the lower weight 61 suspended in the air, keep it at 280℃ for 3 minutes, then take it out and observe the displacement of the glue 62.
[0076] The edge area of the adhesive member 1 is bonded to the PCB board 7 through the glue layer 16, and the remaining area is bonded to the dust-proof film 2 through the glue layer 16; the area where the edge of the adhesive member 1 is bonded to the PCB board 7 is the bonding area 13, the bonding area 13 is annular, the average width of the bonding area 13 is 0.2mm, and the ratio of the average width of the bonding area 13 to the outer diameter of the adhesive member 1 is 0.1:1; the area where the adhesive member 1 is bonded to the dust-proof film 2 is the mucosal area 14, the mucosal area 14 is annular, the average width of the mucosal area 14 is 0.3mm, and the ratio of the average width of the mucosal area 14 to the diameter of the dust-proof film 2 is 0.3:1.
[0077] The diameter of the dustproof film 2 is larger than the inner diameter of the adhesive member 1; the dustproof film 2 covers the opening 11, and the dustproof film 2 covers the PCB board 7, the surface energy of the dustproof film 2 is 15mN / m, and the pore size of the dustproof film 2 is 0.02μm; the diameter of the dustproof film 2 is 1mm, the thickness of the dustproof film 2 is 20μm, the ratio of the thickness of the dustproof film 2 to the thickness of the adhesive member 1 is 1:9, and the dustproof film 2 is a polytetrafluoroethylene film.
[0078] The method for using the dustproof film assembly comprises the following steps:
[0079] The dustproof film assembly is attached to the sound hole of the PCB board 7 during the silicon microphone board making process, wherein the silicon microphone board making process includes processes such as reflow soldering, sound permeability inspection and board separation process; the dustproof film assembly is torn off before the silicon microphone is packaged or is used as a dustproof and sound-permeable film assembly built into the silicon microphone.
[0080] Example 2
[0081] In this embodiment, a dustproof film assembly is provided for process protection of silicon microphones during patch assembly, comprising an adhesive member 1 with single-sided bonding and a dustproof film 2 for dustproof and breathable performance. The thickness of the dustproof film assembly is 24um, the sound blocking value of the dustproof film assembly is 0.4dB@1kHz, and the air permeability of the dustproof film assembly is 150000ml / (min*cm2)@7KPa.
[0082] The adhesive member 1 is an annular structure, and an opening 11 is formed through the adhesive member 1 along its thickness direction, wherein a sticky protrusion 12 is provided on the side of the adhesive member 1, and the protrusion 12 is bonded to the handle 3, and the handle 3 is polyimide; the thickness of the adhesive member 1 is 20 μm, the outer diameter of the adhesive member 1 is 4 mm, the inner diameter is 2 mm, the tensile strength of the adhesive member 1 is 300 N / 25 mm, and the shear strength of the adhesive member 1 is 350 kPa.
[0083] The adhesive member 1 includes a substrate layer 15 and a glue layer 16 arranged along its thickness direction, the glue layer 16 has a thickness of 5um, a bonding strength of the glue layer 16 of 5N / 25mm, and a high-temperature overflow of the glue layer 16 of 40μm@280℃·3min; the elastic modulus of the substrate layer 15 is 50MPa, the elastic limit deformation of the substrate layer 15 is 5%, the ratio of the thickness of the substrate layer 15 to the thickness of the glue layer 16 is 3:1, and the substrate layer 15 is polyimide.
[0084] The edge area of the adhesive member 1 is bonded to the PCB board 7 through the glue layer 16, and the remaining area is bonded to the dust-proof film 2 through the glue layer 16; the area where the edge of the adhesive member 1 is bonded to the PCB board 7 is the bonding area 13, the bonding area 13 is annular, the average width of the bonding area 13 is 0.24mm, and the ratio of the average width of the bonding area 13 to the outer diameter of the adhesive member 1 is 0.06:1; the area where the adhesive member 1 is bonded to the dust-proof film 2 is the mucosal area 14, the mucosal area 14 is annular, the average width of the mucosal area 14 is 0.6mm, and the ratio of the average width of the mucosal area 14 to the diameter of the dust-proof film 2 is 0.2:1.
[0085] The diameter of the dustproof film 2 is larger than the inner diameter of the adhesive member 1; the dustproof film 2 covers the opening 11, and the dustproof film 2 covers the PCB board 7, the surface energy of the dustproof film 2 is 30mN / m, and the pore size of the dustproof film 2 is 2μm; the diameter of the dustproof film 2 is 3mm, the thickness of the dustproof film 2 is 4μm, the ratio of the thickness of the dustproof film 2 to the thickness of the adhesive member 1 is 1:5, and the dustproof film 2 is a polytetrafluoroethylene film.
[0086] The method for using the dustproof film assembly comprises the following steps:
[0087] The dustproof film assembly is attached to the sound hole of the PCB board 7 during the silicon microphone board making process, wherein the silicon microphone board making process includes processes such as reflow soldering, sound permeability inspection and board separation process; the dustproof film assembly is torn off before the silicon microphone is packaged or is used as a dustproof and sound-permeable film assembly built into the silicon microphone.
[0088] Example 3
[0089] In this embodiment, a dustproof film assembly is provided for process protection of silicon microphones during patch assembly, comprising an adhesive member 1 with single-sided bonding and a dustproof film 2 for dustproof and breathable performance. The thickness of the dustproof film assembly is 160um, the sound blocking value of the dustproof film assembly is 0.6dB@1kHz, and the air permeability of the dustproof film assembly is 100000ml / (min*cm2)@7KPa.
[0090] The adhesive member 1 is an annular structure, and an opening 11 is formed through the adhesive member 1 along its thickness direction, wherein a sticky protrusion 12 is provided on the side of the adhesive member 1, and the protrusion 12 is bonded to the handle 3, and the handle 3 is polyimide; the thickness of the adhesive member 1 is 140μm, the outer diameter of the adhesive member 1 is 3mm, the inner diameter is 1mm, the tensile strength of the adhesive member 1 is 150N / 25mm, and the shear strength of the adhesive member 1 is 300kPa.
[0091] The adhesive member 1 includes a substrate layer 15 and a glue layer 16 arranged along its thickness direction, the glue layer 16 has a thickness of 70um, a bonding strength of the glue layer 16 of 25N / 25mm, and a high-temperature overflow of the glue layer 16 of 45μm@280℃·3min; the elastic modulus of the substrate layer 15 is 150MPa, the elastic limit deformation of the substrate layer 15 is 3.5%, the ratio of the thickness of the substrate layer 15 to the thickness of the glue layer 16 is 1:1, and the substrate layer 15 is polyimide.
[0092] The edge area of the adhesive member 1 is bonded to the PCB board 7 through the glue layer 16, and the remaining area is bonded to the dust-proof film 2 through the glue layer 16; the area where the edge of the adhesive member 1 is bonded to the PCB board 7 is the bonding area 13, the bonding area 13 is annular, the average width of the bonding area 13 is 0.6mm, and the ratio of the average width of the bonding area 13 to the outer diameter of the adhesive member 1 is 0.2:1; the area where the adhesive member 1 is bonded to the dust-proof film 2 is the mucosal area 14, the mucosal area 14 is annular, the average width of the mucosal area 14 is 0.8mm, and the ratio of the average width of the mucosal area 14 to the diameter of the dust-proof film 2 is 0.4:1.
[0093] The diameter of the dustproof film 2 is larger than the inner diameter of the adhesive member 1; the dustproof film 2 covers the opening 11, and the dustproof film 2 covers the PCB board 7, the surface energy of the dustproof film 2 is 25mN / m, and the pore size of the dustproof film 2 is 1μm; the diameter of the dustproof film 2 is 2mm, the thickness of the dustproof film 2 is 20μm, the ratio of the thickness of the dustproof film 2 to the thickness of the adhesive member 1 is 1:7, and the dustproof film 2 is a polytetrafluoroethylene film.
[0094] The method for using the dustproof film assembly comprises the following steps:
[0095] The dustproof film assembly is attached to the sound hole of the PCB board 7 during the silicon microphone board making process, wherein the silicon microphone board making process includes processes such as reflow soldering, sound permeability inspection and board separation process; the dustproof film assembly is torn off before the silicon microphone is packaged or is used as a dustproof and sound-permeable film assembly built into the silicon microphone.
[0096] Example 4
[0097] In this embodiment, a dustproof film assembly is provided for process protection of silicon microphones during patch assembly, comprising an adhesive member 1 with single-sided bonding and a dustproof film 2 for dustproof and breathable performance. The thickness of the dustproof film assembly is 105um, the sound blocking value of the dustproof film assembly is 0.5dB@1kHz, and the air permeability of the dustproof film assembly is 130000ml / (min*cm2)@7KPa.
[0098] The adhesive member 1 is an annular structure, and an opening 11 is formed through the adhesive member 1 along its thickness direction, wherein a sticky protrusion 12 is provided on the side of the adhesive member 1, and the protrusion 12 is bonded to the handle 3, and the handle 3 is polyimide; the thickness of the adhesive member 1 is 95μm, the outer diameter of the adhesive member 1 is 2.5mm, the inner diameter is 1mm, the tensile strength of the adhesive member 1 is 160N / 25mm, and the shear strength of the adhesive member 1 is 280kPa.
[0099] The adhesive member 1 includes a substrate layer 15 and a glue layer 16 arranged along its thickness direction, the glue layer 16 has a thickness of 25um, a bonding strength of the glue layer 16 of 20N / 25mm, and a high-temperature overflow of the glue layer 16 of 43μm@280℃·3min; the elastic modulus of the substrate layer 15 is 250MPa, the elastic limit deformation of the substrate layer 15 is 4%, the ratio of the thickness of the substrate layer 15 to the thickness of the glue layer 16 is 2.8:1, and the substrate layer 15 is polyimide.
[0100] The edge area of the adhesive member 1 is bonded to the PCB board 7 through the glue layer 16, and the remaining area is bonded to the dust-proof film 2 through the glue layer 16; the area where the edge of the adhesive member 1 is bonded to the PCB board 7 is the bonding area 13, the bonding area 13 is annular, the average width of the bonding area 13 is 0.4mm, and the ratio of the average width of the bonding area 13 to the outer diameter of the adhesive member 1 is 0.16:1; the area where the adhesive member 1 is bonded to the dust-proof film 2 is the mucosal area 14, the mucosal area 14 is annular, the average width of the mucosal area 14 is 0.3mm, and the ratio of the average width of the mucosal area 14 to the diameter of the dust-proof film 2 is 0.2:1.
[0101] The diameter of the dustproof film 2 is larger than the inner diameter of the adhesive member 1; the dustproof film 2 covers the opening 11, and the dustproof film 2 covers the PCB board 7, the surface energy of the dustproof film 2 is 25mN / m, and the pore size of the dustproof film 2 is 1.5μm; the diameter of the dustproof film 2 is 1.5mm, the thickness of the dustproof film 2 is 10μm, the ratio of the thickness of the dustproof film 2 to the thickness of the adhesive member 1 is 1:9.5, and the dustproof film 2 is a polytetrafluoroethylene film.
[0102] The method for using the dustproof film assembly comprises the following steps:
[0103] The dustproof film assembly is attached to the sound hole of the PCB board 7 during the silicon microphone board making process, wherein the silicon microphone board making process includes processes such as reflow soldering, sound permeability inspection and board separation process; the dustproof film assembly is torn off before the silicon microphone is packaged or is used as a dustproof and sound-permeable film assembly built into the silicon microphone.
[0104] Example 5
[0105] In this embodiment, a dustproof film assembly is provided for protecting the silicon microphone during the patch assembly process, comprising an adhesive member 1 with single-side bonding and a dustproof film 2 for dustproof and breathable use. The thickness of the dustproof film assembly is 180um, the sound barrier of the dustproof film assembly is 0.8dB@1kHz, and the air permeability of the dustproof film assembly is 7000ml / (min*cm 2 )@7KPa.
[0106] The adhesive member 1 is an annular structure, and an opening 11 is formed through the adhesive member 1 along its thickness direction, wherein a sticky protrusion 12 is provided on the side of the adhesive member 1, and the protrusion 12 is bonded to the handle 3, and the handle 3 is polyimide; the thickness of the adhesive member 1 is 160μm, the outer diameter of the adhesive member 1 is 2.5mm, the inner diameter is 1.5mm, the tensile strength of the adhesive member 1 is 180N / 25mm, and the shear strength of the adhesive member 1 is 200kPa.
[0107] The adhesive member 1 includes a substrate layer 15 and a glue layer 16 arranged along its thickness direction, the glue layer 16 has a thickness of 80um, a bonding strength of the glue layer 16 of 20N / 25mm, and a high-temperature overflow of the glue layer 16 of 35μm@280℃·3min; the elastic modulus of the substrate layer 15 is 100MPa, the elastic limit deformation of the substrate layer 15 is 4%, the ratio of the thickness of the substrate layer 15 to the thickness of the glue layer 16 is 1:1, and the substrate layer 15 is polyimide.
[0108] The edge area of the adhesive member 1 is bonded to the PCB board 7 through the glue layer 16, and the remaining area is bonded to the dust-proof film 2 through the glue layer 16; the area where the edge of the adhesive member 1 is bonded to the PCB board 7 is the bonding area 13, the bonding area 13 is annular, the average width of the bonding area 13 is 0.25mm, and the ratio of the average width of the bonding area 13 to the outer diameter of the adhesive member 1 is 0.1:1; the area where the adhesive member 1 is bonded to the dust-proof film 2 is the mucosal area 14, the mucosal area 14 is annular, the average width of the mucosal area 14 is 0.4mm, and the ratio of the average width of the mucosal area 14 to the diameter of the dust-proof film 2 is 0.4:1.
[0109] The diameter of the dustproof film 2 is larger than the inner diameter of the adhesive member 1; the dustproof film 2 covers the opening 11, and the dustproof film 2 covers the PCB board 7, the surface energy of the dustproof film 2 is 25mN / m, and the pore size of the dustproof film 2 is 0.5μm; the diameter of the dustproof film 2 is 1mm, the thickness of the dustproof film 2 is 20μm, the ratio of the thickness of the dustproof film 2 to the thickness of the adhesive member 1 is 1:8, and the dustproof film 2 is a polytetrafluoroethylene film.
[0110] The method for using the dustproof film assembly comprises the following steps:
[0111] The dustproof film assembly is attached to the sound hole of the PCB board 7 during the silicon microphone board making process, wherein the silicon microphone board making process includes processes such as reflow soldering, sound permeability inspection and board separation process; the dustproof film assembly is torn off before the silicon microphone is packaged or is used as a dustproof and sound-permeable film assembly built into the silicon microphone.
[0112] Example 6
[0113] In this embodiment, a dustproof film assembly is provided for process protection of silicon microphones during patch assembly, including an adhesive part 1 with single-sided bonding and a dustproof film 2 for dustproof and breathable performance. The thickness of the dustproof film assembly is 200um, the sound blocking amount of the dustproof film assembly is 0.9dB@1kHz, and the air permeability of the dustproof film assembly is 5000ml / (min*cm2)@7KPa.
[0114] The adhesive member 1 is an annular structure, and an opening 11 is formed through the adhesive member 1 along its thickness direction, wherein a sticky protrusion 12 is provided on the side of the adhesive member 1, and the protrusion 12 is bonded to the handle 3, and the handle 3 is polyimide; the thickness of the adhesive member 1 is 180μm, the outer diameter of the adhesive member 1 is 2mm, the inner diameter is 0.6mm, the tensile strength of the adhesive member 1 is 100N / 25mm, and the shear strength of the adhesive member 1 is 150kPa.
[0115] The adhesive member 1 includes a substrate layer 15 and a glue layer 16 arranged along its thickness direction, the glue layer 16 has a thickness of 36um, a bonding strength of the glue layer 16 of 5N / 25mm, and a high-temperature overflow of the glue layer 16 of 50μm@280℃·3min; the elastic modulus of the substrate layer 15 is 50MPa, the elastic limit deformation of the substrate layer 15 is 0.5%, the ratio of the thickness of the substrate layer 15 to the thickness of the glue layer 16 is 4:1, and the substrate layer 15 is polyimide.
[0116] The edge area of the adhesive member 1 is bonded to the PCB board 7 through the glue layer 16, and the remaining area is bonded to the dustproof film 2 through the glue layer 16; the area where the edge of the adhesive member 1 is bonded to the PCB board 7 is the bonding area 13, the bonding area 13 is annular, and the average width of the bonding area 13 is 0.2mm, the center of the dustproof film 2 is misaligned with the center of the adhesive member 1, and the center of the dustproof film 2 is located on the side of the center of the adhesive member 1 away from the handle 3, and the width of the bonding area 13 close to the handle 3 is greater than the width of the bonding area 13 away from the handle 3 The width of the side, the width of the bonding area 13 close to the handle 3 is 0.3mm, the width of the bonding area 13 away from the handle 3 is 0.1mm, the ratio of the width of the bonding area 13 away from the handle 3 to the outer diameter of the adhesive 1 is 5%, and the ratio of the average width of the bonding area 13 to the outer diameter of the adhesive 1 is 0.1:1; the area where the adhesive 1 is bonded to the dust-proof film 2 is the mucosal area 14, the mucosal area 14 is annular, the average width of the mucosal area 14 is 0.3mm, and the ratio of the average width of the mucosal area 14 to the diameter of the dust-proof film 2 is 0.3:1.
[0117] The diameter of the dustproof film 2 is larger than the inner diameter of the adhesive member 1; the dustproof film 2 covers the opening 11, and the dustproof film 2 covers the PCB board 7, the surface energy of the dustproof film 2 is 15mN / m, and the pore size of the dustproof film 2 is 0.02μm; the diameter of the dustproof film 2 is 1mm, the thickness of the dustproof film 2 is 20μm, the ratio of the thickness of the dustproof film 2 to the thickness of the adhesive member 1 is 1:9, and the dustproof film 2 is a polytetrafluoroethylene film.
[0118] The method for using the dustproof film assembly comprises the following steps:
[0119] The dustproof film assembly is attached to the sound hole of the PCB board 7 during the silicon microphone board making process, wherein the silicon microphone board making process includes processes such as reflow soldering, sound permeability inspection and board separation process; the dustproof film assembly is torn off before the silicon microphone is packaged or is used as a dustproof and sound-permeable film assembly built into the silicon microphone.
[0120] Example 7
[0121] In this embodiment, a dustproof film assembly is provided for process protection of silicon microphones during patch assembly, comprising an adhesive member 1 with single-sided bonding and a dustproof film 2 for dustproof and breathable performance. The thickness of the dustproof film assembly is 200um, the sound blocking amount of the dustproof film assembly is 0.4dB@1kHz, and the air permeability of the dustproof film assembly is 150000ml / (min*cm2)@7KPa.
[0122] The adhesive member 1 is an annular structure, and an opening 11 is formed through the adhesive member 1 along its thickness direction, wherein a sticky protrusion 12 is provided on the side of the adhesive member 1, and the protrusion 12 is bonded to the handle 3, and the handle 3 is polyimide; the thickness of the adhesive member 1 is 180 μm, the outer diameter of the adhesive member 1 is 2 mm, the inner diameter is 0.6 mm, the tensile strength of the adhesive member 1 is 200 N / 25 mm, and the shear strength of the adhesive member 1 is 200 kPa.
[0123] The adhesive member 1 includes a substrate layer 15 and a glue layer 16 arranged along its thickness direction, the glue layer 16 has a thickness of 36um, a bonding strength of the glue layer 16 of 5N / 25mm, and a high-temperature overflow of the glue layer 16 of 50μm@280℃·3min; the elastic modulus of the substrate layer 15 is 200MPa, the elastic limit deformation of the substrate layer 15 is 3.5%, the ratio of the thickness of the substrate layer 15 to the thickness of the glue layer 16 is 4:1, and the substrate layer 15 is polyimide.
[0124] The edge area of the adhesive member 1 is bonded to the PCB board 7 through the glue layer 16, and the remaining area is bonded to the dustproof film 2 through the glue layer 16; the area where the edge of the adhesive member 1 is bonded to the PCB board 7 is the bonding area 13, the bonding area 13 is annular, and the average width of the bonding area 13 is 0.2mm, the center of the dustproof film 2 is misaligned with the center of the adhesive member 1, and the center of the dustproof film 2 is located on the side of the center of the adhesive member 1 away from the handle 3, and the width of the bonding area 13 close to the handle 3 is greater than the width of the bonding area 13 away from the handle 3 The width of the side, the width of the bonding area 13 close to the handle 3 is 0.8mm, the width of the bonding area 13 away from the handle 3 is 0.5mm, the ratio of the width of the bonding area 13 away from the handle 3 to the outer diameter of the adhesive 1 is 25%, and the ratio of the average width of the bonding area 13 to the outer diameter of the adhesive 1 is 0.1:1; the area where the adhesive 1 is bonded to the dust-proof film 2 is the mucosal area 14, the mucosal area 14 is annular, the average width of the mucosal area 14 is 0.3mm, and the ratio of the average width of the mucosal area 14 to the diameter of the dust-proof film 2 is 0.3:1.
[0125] The diameter of the dustproof film 2 is larger than the inner diameter of the adhesive member 1; the dustproof film 2 covers the opening 11, and the dustproof film 2 covers the PCB board 7, the surface energy of the dustproof film 2 is 20mN / m, and the pore size of the dustproof film 2 is 2μm; the diameter of the dustproof film 2 is 1mm, the thickness of the dustproof film 2 is 20μm, the ratio of the thickness of the dustproof film 2 to the thickness of the adhesive member 1 is 1:9, and the dustproof film 2 is a polytetrafluoroethylene film.
[0126] The method for using the dustproof film assembly comprises the following steps:
[0127] The dustproof film assembly is attached to the sound hole of the PCB board 7 during the silicon microphone board making process, wherein the silicon microphone board making process includes processes such as reflow soldering, sound permeability inspection and board separation process; the dustproof film assembly is torn off before the silicon microphone is packaged or is used as a dustproof and sound-permeable film assembly built into the silicon microphone.
[0128] Comparative Example 1
[0129] In this comparative example, a dustproof film assembly is provided for the process protection of silicon microphones in patch assembly, comprising an adhesive part 1 with single-sided bonding and a dustproof film 2 for dustproof and breathable performance. The thickness of the dustproof film assembly is 200um, the sound blocking amount of the dustproof film assembly is 0.7dB@1kHz, and the air permeability of the dustproof film assembly is 50000ml / (min*cm2)@7KPa.
[0130] The adhesive member 1 is an annular structure, and an opening 11 is formed through the adhesive member 1 along its thickness direction, wherein a sticky protrusion 12 is provided on the side of the adhesive member 1, and the protrusion 12 is bonded to the handle 3, and the handle 3 is polyimide; the thickness of the adhesive member 1 is 180μm, the outer diameter of the adhesive member 1 is 2.5mm, the inner diameter is 0.6mm, the tensile strength of the adhesive member 1 is 200N / 25mm, and the shear strength of the adhesive member 1 is 350kPa.
[0131] The adhesive member 1 includes a substrate layer 15 and a glue layer 16 arranged along its thickness direction, the glue layer 16 has a thickness of 90um, a bonding strength of the glue layer 16 of 20N / 25mm, and a high-temperature overflow of the glue layer 16 of 80μm@280℃·3min; the elastic modulus of the substrate layer 15 is 200MPa, the elastic limit deformation of the substrate layer 15 is 3%, the ratio of the thickness of the substrate layer 15 to the thickness of the glue layer 16 is 1:1, and the substrate layer 15 is polyimide.
[0132] The edge area of the adhesive member 1 is bonded to the PCB board 7 through the glue layer 16, and the remaining area is bonded to the dust-proof film 2 through the glue layer 16; the area where the edge of the adhesive member 1 is bonded to the PCB board 7 is the bonding area 13, the bonding area 13 is annular, the average width of the bonding area 13 is 0.4mm, and the ratio of the average width of the bonding area 13 to the outer diameter of the adhesive member 1 is 0.16:1; the area where the adhesive member 1 is bonded to the dust-proof film 2 is the mucosal area 14, the mucosal area 14 is annular, the average width of the mucosal area 14 is 0.3mm, and the ratio of the average width of the mucosal area 14 to the diameter of the dust-proof film 2 is 0.2:1.
[0133] The diameter of the dustproof film 2 is larger than the inner diameter of the adhesive member 1; the dustproof film 2 covers the opening 11, and the dustproof film 2 covers the PCB board 7, the surface energy of the dustproof film 2 is 45mN / m, and the pore size of the dustproof film 2 is 0.8μm; the diameter of the dustproof film 2 is 1.5mm, the thickness of the dustproof film 2 is 20μm, the ratio of the thickness of the dustproof film 2 to the thickness of the adhesive member 1 is 1:9, and the dustproof film 2 is a polytetrafluoroethylene film.
[0134] The method for using the dustproof film assembly comprises the following steps:
[0135] The dustproof film assembly is attached to the sound hole of the PCB board 7 during the silicon microphone board making process, wherein the silicon microphone board making process includes processes such as reflow soldering, sound permeability inspection and board separation process; the dustproof film assembly is torn off before the silicon microphone is packaged or is used as a dustproof and sound-permeable film assembly built into the silicon microphone.
[0136] Comparative Example 2
[0137] like Fig. 9 As shown, a dustproof film assembly is provided in this comparative example, including a protective film 4, a first double-sided adhesive layer 51, a second double-sided adhesive layer 52 and a dustproof film 2. The bottom surface of the protective film 4 is bonded to the upper surface of the first double-sided adhesive layer 51, the bottom surface of the first double-sided adhesive layer 51 is bonded to the upper surface of the dustproof film 2, the bottom surface of the dustproof film 2 is bonded to the upper surface of the second double-sided adhesive layer 52, and the bottom surface of the second double-sided adhesive layer 52 is bonded to the PCB board 7. The first double-sided adhesive layer 51 and the second double-sided adhesive layer 52 can be the same, and the structure, performance parameters, etc. of the second double-sided adhesive layer 52 will not be repeated below.
[0138] The thickness of the dustproof film assembly is 350um, the thickness of the protective film 4 is 130μm, the sound barrier of the dustproof film assembly is 2dB@1kHz, and the air permeability of the dustproof film assembly is 200000ml / (min*cm 2 )@7KPa.
[0139] The first double-sided adhesive layer 51 is an annular structure, and the first double-sided adhesive layer 51 is penetrated along the thickness direction thereof to form an opening 11; the first double-sided adhesive layer 51 is 100 μm thick, the outer diameter of the first double-sided adhesive layer 51 is 3 mm, the inner diameter is 1 mm, the tensile strength of the first double-sided adhesive layer 51 is 200 N / 25 mm, and the shear strength of the first double-sided adhesive layer 51 is 200 kPa; the first double-sided adhesive layer 51 includes a substrate layer 15 and a The glue layer 16 is arranged on both sides of the substrate layer 15, the thickness of the glue layer 16 is 25um, the bonding strength of the glue layer 16 is 20N / 25mm, and the high-temperature overflow of the glue layer 16 is 45μm@280℃·3min; the elastic modulus of the substrate layer 15 is 200MPa, the elastic limit deformation of the substrate layer 15 is 3%, the ratio of the thickness of the substrate layer 15 to the thickness of the glue layer 16 is 2:1, and the substrate layer 15 is polyimide.
[0140] The bottom surface of the second double-sided adhesive layer 52 is bonded to the PCB board 7 through the glue layer 16, and the upper surface thereof is bonded to the bottom surface of the dust-proof film 2 through the glue layer 16; the area where the second double-sided adhesive layer 52 is bonded to the PCB board 7 is the bonding area 13, the bonding area 13 is annular, the width of the bonding area 13 is 1 mm, and the ratio of the width of the bonding area 13 to the outer diameter of the second double-sided adhesive layer 52 is 1:3; the area where the second double-sided adhesive layer 52 is bonded to the dust-proof film 2 is the mucosal area 14, the mucosal area 14 is annular, the width of the mucosal area 14 is 1 mm, and the ratio of the width of the mucosal area 14 to the diameter of the dust-proof film 2 is 1:3.
[0141] The diameter of the dustproof film 2 is larger than the inner diameter of the second double-sided adhesive layer 52; the dustproof film 2 covers the opening 11, and the dustproof film 2 covers the PCB board 7, the surface energy of the film surface of the dustproof film 2 is 20mN / m, and the pore size of the dustproof film 2 is 0.05μm; the diameter of the dustproof film 2 is 3mm, the thickness of the dustproof film 2 is 20μm, the ratio of the thickness of the dustproof film 2 to the thickness of the second double-sided adhesive layer 52 is 1:5, and the dustproof film 2 is a polytetrafluoroethylene film.
[0142] The method for using the dustproof film assembly comprises the following steps:
[0143] The dustproof film assembly is attached to the sound hole of the PCB board 7 during the silicon microphone board making process, wherein the silicon microphone board making process includes processes such as reflow soldering, sound permeability inspection and board separation process; the dustproof film assembly is torn off before the silicon microphone is packaged or is used as a dustproof and sound-permeable film assembly built into the silicon microphone.
[0144] The performance tests were performed on the dustproof film assemblies in the above-mentioned Examples 1 to 7 and Comparative Examples 1 to 2, and the test results are shown in the following table:
[0145]
[0146] It can be seen from the above test results that, whether compared with the dustproof film assembly (Comparative Example 1) with a large amount of high-temperature overflow (strong high-temperature fluidity), a thicker glue layer 16, and a higher surface energy of the dustproof film 2 (poor oleophobicity), or compared with the dustproof film assembly with a four-layer structure (Comparative Example 2), the dustproof film assembly provided in the above embodiments 1 to 7 of the present application will not have stratification, will not produce residual glue, and will also have good sound permeability and air permeability; especially embodiments 6 and 7, the problem of reduced contact area between the bonding area 13 and the PCB board 7 on the side close to the handle 3 is solved, and the center of the dustproof film 2 is staggered with the center of the adhesive 1, so that the width of the bonding area 13 on the side close to the handle 3 is greater than the width of the bonding area 13 away from the handle 3, so that the adhesive 1 and the PCB board 7 have a more suitable contact area, so that the bonding area 13 on the side close to the handle 3 is more firmly bonded to the PCB board 7.
[0147] The above-mentioned embodiments are only preferred embodiments of the present invention and cannot be used to limit the scope of protection of the present invention. Any non-substantial changes and substitutions made by technicians in this field on the basis of the present invention shall fall within the scope of protection required by the present invention.
Claims
1. A dustproof film assembly, used for protecting silicon microphones during patch assembly, characterized in that: The invention comprises an adhesive member with single-side bonding and a dust-proof membrane for preventing dust and being breathable; The adhesive member is an annular structure, and an opening is formed through the adhesive member along the thickness direction thereof; The adhesive member includes a substrate layer and a glue layer arranged along the thickness direction thereof, and the edge area of the adhesive member is bonded to the PCB board through the glue layer; the remaining area is bonded to the dustproof film through the glue layer; The diameter of the dustproof film is greater than the inner diameter of the adhesive member; the dustproof film covers the opening, and the dustproof film covers the PCB board.
2. The dustproof film assembly according to claim 1, characterized in that: The side of the adhesive piece is provided with an adhesive protrusion, and the dustproof film assembly further comprises a handle bonded to the protrusion.
3. The dustproof film assembly according to claim 2, characterized in that: The area where the edge of the adhesive piece is bonded to the PCB board is the bonding area, the bonding area is annular, the average width of the bonding area is 0.2mm-0.6mm, and the thickness of the dustproof film is 2-20μm.
4. The dustproof film assembly according to claim 3, characterized in that: The center of the dustproof film is offset from the center of the adhesive member, and the center of the dustproof film is located on the side of the adhesive member away from the handle; the width of the adhesive area close to the handle is greater than the width of the adhesive area away from the handle.
5. The dustproof film assembly according to claim 4, characterized in that: The width of the adhesive zone near the handle is 0.3-0.8 mm, and the width of the adhesive zone away from the handle is 0.1-0.5 mm; The ratio of the width of the bonding area away from the handle to the outer diameter of the bonding piece is not less than 4%.
6. The dustproof film assembly according to claim 3, characterized in that: The ratio of the average width of the bonding area to the outer diameter of the bonding piece is 0.06-0.2:
1.
7. The dustproof film assembly according to claim 1, characterized in that: The thickness of the glue layer is 5-80um, and the bonding strength of the glue layer is 5N / 25mm-30N / 25mm; The high-temperature overflow of the glue layer is no more than 50 μm @ 280°C·3min; The surface energy of the dustproof film is 15-30 mN / m.
8. The dustproof film assembly according to claim 1, characterized in that: The area where the adhesive member is bonded to the dustproof film is a mucosal area, the mucosal area is annular, and the average width of the mucosal area is 0.3-0.8 mm.
9. The dustproof film assembly according to claim 8, characterized in that: The ratio of the average width of the mucosal area to the diameter of the dust-proof film is 0.2-0.4:
1.
10. The dustproof film assembly according to claim 1, characterized in that: The thickness of the adhesive member is 20-200 μm, the outer diameter of the adhesive member is 2 mm-4 mm, and the inner diameter is 0.6-2 mm.
11. The dustproof film assembly according to claim 1, characterized in that: The elastic modulus of the substrate layer is 50-300 MPa, and the elastic limit deformation of the substrate layer is 0.5%-5%; the tensile strength of the adhesive is 100N / 25mm-300N / 25mm; The shear strength of the adhesive is 150-350 kPa; The ratio of the thickness of the substrate layer to the thickness of the glue layer is 1-4:
1.
12. The dustproof film assembly according to claim 1, characterized in that: The pore size of the dust-proof film is 0.02-2 μm; the diameter of the dust-proof film is 1 mm-3 mm; The ratio of the thickness of the dustproof film to the thickness of the adhesive member is 1:2-1:
12.
13. The dustproof film assembly according to claim 2, characterized in that: The dustproof film is a polytetrafluoroethylene film; The handle is made of polyimide; the substrate layer is made of polyimide; The thickness of the dustproof film assembly is 24-215um; The sound barrier of the dustproof film assembly is less than 1dB@1kHz. The air permeability of the dustproof membrane assembly is 5000-150000 ml / (min*cm 2 )@7KPa.
14. A method for using the dustproof film assembly according to any one of claims 1 to 13, characterized in that: The steps include: The dustproof film assembly is attached to the sound hole of the PCB board during the silicon microphone board making process, wherein the silicon microphone board making process includes reflow soldering, sound permeability inspection and board separation process; the dustproof film assembly is torn off before the silicon microphone is packaged or is used as a dustproof and sound-permeable film assembly built into the silicon microphone.
Citation Information
Patent Citations
A matrix type structure of a dustproof, waterproof and sound-transmitting film of a micro electro mechanical sensor
CN111601222A
Dustproof protection film
CN205193412U