Chip-on-film and compensation method thereof, and display device

By setting the opening and division of the insulating film layer on the crystal-covered film, combined with multiple compensation steps, the problem of low binding accuracy of large-size flexible display panels is solved, and the binding accuracy and comprehensive performance of the display panel are improved.

CN114845464BActive Publication Date: 2024-11-22GUANGZHOU CHINA STAR OPTOELECTRONICS SEMICON DISPLAY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210554668.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-05-20
Publication Date
2024-11-22
Estimated Expiration
2042-05-20

AI Technical Summary

Technical Problem

Large-size flexible display panels are prone to expansion or contraction during the binding process of crystal-covered thin film, resulting in reduced binding accuracy and binding failure, affecting the quality and reliable performance of the display panel.

Method used

A crystal-covered film is designed, which includes a substrate, a binding portion and an insulating film layer. The insulating film layer is provided with an opening in the binding region. The extension direction of the opening is perpendicular to the side of the binding portion and passes through the first and second The partition is divided into sections, multiple interval binding terminals and alignment marks are set, and multiple compensations are performed to adjust the offset and deflection angle.

Benefits of technology

It effectively reduces the low accuracy and deformation problems of the crystal-covered film during the binding process, and improves the binding accuracy and comprehensive performance of the display panel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114845464B_ABST
    Figure CN114845464B_ABST
Patent Text Reader

Abstract

The embodiment of the present invention provides a chip-on-chip film and a compensation method and a display device thereof. The chip-on-chip film includes a substrate, a binding portion, and an insulating film layer. The binding portion is arranged in a binding area of ​​the substrate, and the insulating film layer also includes an opening, which is at least correspondingly arranged in the binding area, and the extension direction of the opening is perpendicular to the side of the substrate and one side of the binding portion. By setting an opening on the chip-on-chip film in the binding area, the chip-on-chip film is divided into at least two parts. When the chip-on-chip film is bound, the chip-on-chip films on both sides of the opening are compensated respectively, thereby effectively reducing the quality problems such as low precision and binding deformation that are prone to occur in the binding process of large-size chip-on-chip films.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of display panel manufacturing, and in particular to a chip-on-chip film and a compensation method thereof, and a display device. Background Art

[0002] With the development of display panel manufacturing technology, people have put forward higher requirements on the display effect and comprehensive performance of display panels and display devices.

[0003] During the preparation process, the display panel needs to go through multiple process treatments, such as cleaning, lighting, evaporation, etching, and corresponding binding processes. The existing binding process is mainly a chip on film (COF) binding process. For large-sized flexible display panels, when the COF process is used for binding, the binding stability of the flexible binding part has always been one of the difficulties of the flexible bonding process. Among them, when binding the chip on film, the binding area of ​​the corresponding chip on film on the large-sized flexible panel is also large. Therefore, the larger film layer is prone to large expansion or contraction and other shape variations after binding, which in turn causes the deformation of the originally precisely fitted film layer, thereby reducing the binding accuracy and binding effect of the display panel and affecting the working performance of the display panel.

[0004] In summary, when binding the chip-on-chip film of a large-sized flexible display panel, the larger-sized chip-on-chip film is prone to shape variations such as expansion and contraction, thereby reducing the binding accuracy, causing binding failure, and affecting the quality and reliability of the display panel. Summary of the invention

[0005] The embodiment of the present invention provides a COF and a compensation method thereof, and a display device, which can effectively improve the quality problem that a large-sized COF is prone to expansion and deformation when binding a display panel, thereby reducing the binding accuracy and causing binding failure.

[0006] In order to solve the above technical problems, the present invention provides a flip chip film, comprising:

[0007] substrate;

[0008] a binding portion, the binding portion being disposed in a binding region of the substrate; and

[0009] An insulating film layer, the insulating film layer being disposed on the substrate and the binding portion;

[0010] Wherein, the insulating film layer includes an opening, the opening is at least arranged in the binding area, and an angle is formed between an extending direction of the opening and a side edge of a side to which the binding portion is bound.

[0011] According to an embodiment of the present invention, the angle is set to be a right angle.

[0012] According to an embodiment of the present invention, the insulating film layer includes a first dividing portion and a second dividing portion, and the first dividing portion and the second dividing portion are respectively arranged on both sides of the opening.

[0013] According to an embodiment of the present invention, the binding portion of the chip-on-film includes a plurality of binding terminals arranged at intervals;

[0014] The first dividing portion and the second dividing portion are patterned in a region corresponding to the binding terminal, and a surface of the binding terminal is exposed to the insulating film layer.

[0015] According to an embodiment of the present invention, the first dividing portion and the second dividing portion are symmetrically arranged relative to the opening, and positioning marks are also arranged on the first dividing portion and the second dividing portion.

[0016] According to an embodiment of the present invention, the corresponding widths at different positions of the opening are the same.

[0017] According to an embodiment of the present invention, the width of the opening at a location close to the binding terminal of the binding portion is greater than the width of the opening at a location far from the binding terminal.

[0018] According to an embodiment of the present invention, the width of the opening is 60um-150um.

[0019] According to a second aspect of an embodiment of the present invention, there is further provided a display device, including:

[0020] display panel; and

[0021] A chip-on-chip film, wherein the chip-on-chip film is bound to the display panel;

[0022] The chip-on-film comprises a binding portion and an insulating film layer, a connecting terminal is provided on one side of the display panel, the binding portion is bound to the connecting terminal, and the chip-on-film is the chip-on-film provided in the embodiment of the present application.

[0023] According to a third aspect of an embodiment of the present invention, a compensation method for a chip-on-film is also provided, comprising the following steps:

[0024] A substrate and a chip-on-chip film are provided, wherein a connection terminal is provided on one side of the display panel, and the chip-on-chip film is the chip-on-chip film provided in the embodiment of the present application;

[0025] Binding the chip-on-film to the connecting terminal, wherein during the binding process, a first alignment mark on the chip-on-film is made to correspond to a second alignment mark on the substrate, and after the alignment is completed, the offset and deflection angle of the chip-on-film relative to the substrate in the horizontal and vertical directions are measured, and a first correction is performed;

[0026] The offset between the chip-on-film and the second alignment mark on both sides of the opening in the horizontal direction is measured, and the chip-on-film is corrected for the second time according to the offset.

[0027] Beneficial effects of the embodiments of the present invention: Compared with the prior art, the embodiments of the present invention provide a chip-on-chip film and a compensation method thereof, and a display device. The chip-on-chip film includes a substrate, a binding portion, and an insulating film layer. The binding portion is arranged in a binding area of ​​the substrate, and the insulating film layer also includes an opening, which is at least correspondingly arranged in the binding area, and the extension direction of the opening is perpendicular to the side of the substrate and the binding portion. In the embodiment of the present application, an opening is provided on the chip-on-chip film in the binding area, thereby dividing the chip-on-chip film into at least two different parts. When the chip-on-chip film is bound, the chip-on-chip films on both sides of the opening are compensated respectively, thereby effectively reducing the quality problems such as low precision and binding deformation that are prone to occur in the binding process of large-size chip-on-chip films, thereby improving the overall performance of the display panel. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] In order to more clearly illustrate the technical solutions in the embodiments or the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0029] Figure 1 A schematic diagram of the structure of a chip-on-chip film corresponding to a display device provided by the prior art;

[0030] Figure 2 A schematic diagram of the structure of each film layer of the flip chip film provided in an embodiment of the present application;

[0031] Figure 3 A schematic diagram of the binding structure of the display device provided in an embodiment of the present application;

[0032] Figure 4 A schematic diagram of a compensation method flow chart provided in an embodiment of the present application;

[0033] Figure 5 A binding diagram provided for an embodiment of the present application. DETAILED DESCRIPTION

[0034] In conjunction with the accompanying drawings in the embodiments of the present invention, the following disclosure provides different implementation methods or examples to implement different structures of the present invention. In order to simplify the present invention, the components and settings of specific examples are described below. In addition, the examples of various specific processes and materials provided by the present invention are examples that ordinary technicians in the field can recognize the application of other processes. All other embodiments obtained by those skilled in the art without making creative work are within the scope of protection of the present invention.

[0035] In the description of the present invention, it is to be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features.

[0036] With the continuous development of display panel manufacturing technology, people have put forward higher requirements on the performance and display effect of display panels and display devices.

[0037] like Figure 1 As shown, Figure 1 A schematic diagram of the structure of a chip-on-chip film corresponding to a display device provided by the prior art. When preparing and forming the chip-on-chip film structure, a plurality of terminals 101 are usually set in the edge area of ​​the chip-on-chip film, and the plurality of terminals 101 can be directly set on the corresponding substrate 100, and then an insulating film layer 103 is set on the substrate 100. When binding, the terminals 101 on the chip-on-chip film are electrically connected to the conductive terminals on the display panel. However, for a large-size display panel, the corresponding binding area 102 is also larger. Therefore, after the insulating film layer 103 is set and bound, there is a large expansion or deformation force inside the larger film layer. When marking and measuring are performed through the positioning mark 104, there is a large deformation between the insulating film layer and the terminal and the substrate, which leads to a reduction in the accuracy of its binding process.

[0038] The embodiments of the present application provide a COF and a compensation method thereof, and a display device, so as to effectively improve the quality problem in the existing binding process that the COF is prone to expansion or deformation, resulting in reduced accuracy of the binding process.

[0039] like Figure 2 As shown, Figure 2 Schematic diagram of the film structure of each film layer of the flip chip film provided in the embodiment of the present application. In the embodiment of the present application, the flip chip film is only described by taking the corresponding structure in the binding area as an example. Specifically, the flip chip film includes a substrate 104 and a binding portion 208. When the flip chip film is formed, the binding portion 208 is correspondingly attached to the binding area of ​​the substrate 104.

[0040] At the same time, a plurality of binding terminals 1011 are arranged in the binding area corresponding to the substrate 104, and are electrically connected to the display panel or flexible circuit board to be bound through the binding terminals. In the embodiment of the present application, the plurality of binding terminals 1011 are arranged at intervals in the binding area.

[0041] Preferably, the distance between two adjacent binding terminals 1011 may be the same, wherein the number and distance value of the binding terminals 1011 on the substrate 104 may be determined according to the size and requirements of the actual product, thereby ensuring the binding effect of the display panel.

[0042] Furthermore, Figure 2 The chip-on-chip film 207 in the figure is only a partial structural schematic diagram, and the chip-on-chip film 207 can continue to extend to other areas to form a large-sized structure.

[0043] In the embodiment of the present application, the COF 207 further includes an insulating film layer 103, and the insulating film layer 103 is at least arranged in the binding area corresponding to the substrate 104. At the same time, the insulating film layer 103 is patterned in the binding area. Specifically, it can be hollowed out in the binding area, and its hollowed-out pattern can correspond to the structure of the binding terminal 1011 on the display panel.

[0044] Preferably, the insulating film layer 103 is hollowed out in the binding area to form a plurality of corresponding hollowed-out strips 209. The plurality of hollowed-out strips 209 are arranged at intervals, and a hollowed-out distance is set between two adjacent hollowed-out strips 209. In the embodiment of the present application, when binding is performed, the hollowed-out strips are correspondingly bound and attached to the display panel, and each hollowed-out strip 209 is arranged between two adjacent binding terminals 1011, thereby preventing the problem of short circuit between two adjacent binding terminals 1011.

[0045] In the embodiment of the present application, when the insulating film layer 103 is provided, the insulating film layer 103 further includes an opening 220. The opening 220 may be provided correspondingly in the area where the binding terminal 1011 is not provided. Therefore, after the COF 207 is bound to the display panel, the opening 220 will not affect the connection between the binding terminals 1011.

[0046] Further, in the embodiment of the present application, the insulating film layer 103 is described by taking the first dividing portion 201 and the second dividing portion 202 as an example. The first dividing portion 201 and the second dividing portion 202 are respectively arranged in the two side areas of the opening 220. Preferably, the first dividing portion 201 and the second dividing portion 202 can be symmetrically arranged relative to the opening 220, thereby simplifying the preparation process of the flip chip film. At the same time, the opening 220 also divides the flip chip film 207 into two left and right parts.

[0047] In the embodiment of the present application, the first dividing portion 201 and the second dividing portion 202 are both attached to the corresponding substrate, and in the binding area, the first dividing portion 201 and the second dividing portion 202 are at least partially separated due to the effect of the opening.

[0048] Meanwhile, in the embodiment of the present application, the binding terminals 1011 on the substrate 104 are exposed to the insulating film layer. Preferably, when the binding terminals 1011 on the substrate 104 are arranged, in the middle area of ​​the binding area, the distance between two adjacent binding terminals 1011 is greater than the distance between the remaining binding terminals 1011.

[0049] Preferably, in the embodiment of the present application, the extending direction of the opening 220 may have an angle β with the side edge of the side where the binding portion 208 is bound to the substrate 104. That is, the extending direction of the opening 220 may be the same as the direction of the corresponding hollow strip 209. In the embodiment of the present application, the angle is preferably a right angle. At the same time, at the edge of the opening 220 and the side edge, the first dividing portion 201 and the second dividing portion 202 are not separated.

[0050] Further, when the above-mentioned opening 220 is set, the opening width of the opening 220 in different areas can be set to be the same, or set according to actual conditions. Preferably, when the opening widths of the opening 220 in different areas are set to the same width, the opening width is set to 60um-150um, and preferably, the opening width is set to 100um.

[0051] When the opening widths of the opening 220 in different regions are not completely the same, the opening width on the side close to the binding terminal 1011 may be greater than the opening width on the side away from the binding terminal 1011. At this time, within the plane formed by the flip chip film, the width of the opening near the edge is greater than the width of the opening in the central region. Preferably, the width of the opening can be smoothly transitioned, and the width of the opening can be set to 60um-150um.

[0052] Furthermore, the flip chip film also includes a plurality of first alignment marks. In the embodiment of the present application, a first alignment mark 203, a first alignment mark 204, a first alignment mark 205, and a first alignment mark 206 are arranged in the first segmentation portion 201 and the second segmentation portion 202 corresponding to the binding area. The first alignment mark 203 and the first alignment mark 204 are respectively arranged near the two side edges of the binding area, and the first alignment mark 205 and the first alignment mark 206 are correspondingly arranged in the middle area of ​​the binding area.

[0053] In the embodiment of the present application, the plurality of first alignment marks can be set to be alignment marks of different sizes, for example, the first alignment marks 203 and the first alignment marks 204 on both sides are larger than the alignment marks in the middle area.

[0054] At the same time, in an embodiment of the present application, a plurality of second alignment marks 142 are correspondingly arranged on the substrate 104. When the insulating film layer 103 is bonded to the substrate 104, the first alignment mark is made to correspond to the second alignment mark, and then bonding and compensation are performed. In an embodiment of the present application, the setting method of the second alignment mark 142 can be set with reference to the shape and structure of the first alignment mark. And the second alignment mark and the first alignment mark are both set to at least two marks at the middle 230 position of the binding area. In the above embodiments, the shapes of the first alignment mark and the second alignment mark can be set to a circle, or to other shapes.

[0055] Furthermore, on the insulating film layer 103, the first alignment mark 205 and the first alignment mark 206 are respectively arranged on the second dividing portion 202 and the first dividing portion 201. In the embodiment of the present application, when the insulating film layer 103 needs to be compensated, the offset between the first alignment marks 203 and 205 and the marks corresponding to the substrate is measured respectively, and at the same time, the offset between the first alignment marks 204 and 206 and the marks corresponding to the substrate is measured, and then according to the above different offsets, compensation is performed in the horizontal direction corresponding to the insulating film layer 103, so as to ensure the accuracy of the flip chip film after binding.

[0056] like Figure 3 As shown, Figure 3A schematic diagram of the binding structure of the display device provided in an embodiment of the present application. The two ends of the chip-on-chip film 207 are bound and electrically connected to the display panel 302 and the flexible circuit board 301. At the same time, a plurality of connection terminals 340 are provided on the binding side of the display panel 302, and the connection terminals 340 are electrically connected to the binding terminals on the chip-on-chip film. A driver chip 306 is also provided on the chip-on-chip film 207, and the driver chip 306 is correspondingly arranged in the middle of the chip-on-chip film 207. In the embodiment of the present application, the driver chip 306 is electrically connected to the terminals on both sides through the connecting wires arranged inside the chip-on-chip film 207.

[0057] The opening 220 may extend from the bottom of at least one side of the insulating film layer 103 to the vicinity of the driver chip 306. At the same time, the opening 220 may be symmetrically arranged along the central axis of the COF 207, so that the insulating film layer 103 is divided into two identical parts. When the above-mentioned opening 220 is arranged, the opening 220 may be arranged only on one side of the driver chip 306, or the opening may be arranged on both sides of the driver chip 306. In the embodiment of the present application, the insulating film layer may be a polyimide film layer.

[0058] Furthermore, in an embodiment of the present application, a compensation method for a chip-on-chip film is also provided. Figure 4 As shown, Figure 4 A flow chart of a compensation method provided in an embodiment of the present application. Specifically, the compensation method includes the following steps:

[0059] S100: providing a substrate and a chip-on-cover film, wherein a connection terminal is disposed on one side of the substrate, and the chip-on-cover film is the chip-on-cover film provided in an embodiment of the present application;

[0060] S101: Binding the COF to the connection terminals, wherein during the binding process, first alignment marks on both sides of the COF are made to correspond to second alignment marks on both sides of the substrate, and after the alignment is completed, the offset and deflection angle of the COF relative to the substrate in the horizontal and vertical directions are measured, and a first correction is performed;

[0061] S102: measuring the offset in the horizontal direction between the first alignment mark and the corresponding second alignment mark in the middle area of ​​the chip on film, and performing a second correction on the chip on film according to the offset.

[0062] Specifically, Figure 5 As shown, Figure 5A binding schematic diagram provided for an embodiment of the present application. Specifically, when binding, the chip-on-chip film 207 is aligned and bonded to the substrate 510. Alignment marks are provided on both the chip-on-chip film 207 and the substrate 510, such as a plurality of first alignment marks 204 are provided on the chip-on-chip film 207, and a plurality of second alignment marks 142 are provided on the substrate 510. The first alignment marks 204 and the second alignment marks 142 correspond to each other.

[0063] When laminating, firstly, the first alignment mark 204 on both sides is aligned with the second alignment mark 142. After laminating, there is a certain alignment deviation and deflection angle between the COF 207 and the substrate 510 in the horizontal direction X and the vertical direction Y. In the embodiment of the present application, when laminating, the insulating film layer of the COF 207 is laminated on the substrate 510.

[0064] At this time, the first locator 51 and the second locator 52 can be used to measure respectively, and the deviation values ​​and deflection angles in the horizontal direction X and the vertical direction Y can be obtained. Then, according to the above measurement results, the flip chip film can be adjusted in the X, Y directions and its deflection angle to perform the first compensation.

[0065] In the embodiment of the present application, the horizontal direction X may be the lateral direction of the COF, and the vertical direction Y may be the longitudinal direction of the COF. In the first compensation, the alignment marks on both sides of the COF are mainly aligned accurately, such as the alignment marks in the first edge region 501 and the second edge region 502 on both sides.

[0066] After the first compensation is completed, the third locator 53 is turned on. In the embodiment of the present application, the third locator 53 is located in the middle area 503 of the flip chip film, and the third locator 53 can locate the alignment mark in the middle area 503. The distance value X1 between the first alignment mark in the middle area 503 and the alignment mark on the left side of the flip chip film 207, and the distance value X2 between the first alignment mark in the middle area 503 and the alignment mark on the right side are measured and obtained by the third locator 53, the second locator 52 and the first locator 51. And the distance values ​​X3 and X4 between the second alignment marks corresponding to the two sides of X1 and X2 on the substrate 510 are respectively measured.

[0067] After measuring the above distance values ​​X1, X2, X3, and X4, the differences between X1 and X3, and X3 and X4 are compared respectively, and then the chip-on-chip film is compensated for the second time according to the corresponding difference values. In the embodiment of the present application, when performing the second compensation, compensation is only performed in the horizontal direction X. Specifically, if the value of X1 is less than the value of X3, it indicates that the chip-on-chip film 207 has a certain amount of inward shrinkage. In order to ensure its binding accuracy, the first segmentation portion in the chip-on-chip film 207 needs to be stretched to both sides in the horizontal direction to ensure that it is the same as the distance value X3 on the substrate.

[0068] If the value of X1 is greater than the value of X3, it indicates that the chip-on-chip film 207 has expanded. In order to ensure its binding accuracy, the first segmented portion corresponding to the chip-on-chip film needs to be compressed so that the distance value X1 is the same as the distance value X3. Correspondingly, the chip-on-chip film of the second segmented portion is also compensated for the second time in the above manner. Therefore, in the embodiment of the present application, the chip-on-chip film with a large area is compensated in multiple segments, thereby effectively improving its binding accuracy. In the embodiment of the present application, the substrate can be a display panel or other substrate.

[0069] Specifically, when the total width of the chip-on-cover film is 42mm, if the chip-on-cover film is a conventional structure of a whole piece, an expansion deformation of 20um will occur during its binding process. When the chip-on-cover film is set to the structure provided in the embodiment of the present application, and the deformation of different divisions is measured after the binding is completed. Among them, after measurement, in the embodiment of the present application, the deformation of the first division and the second division is 10um. At the same time, in the embodiment of the present application, only one driver chip is still required in each chip-on-cover film. Therefore, in the embodiment of the present application, the deformation of the chip-on-cover film during binding can be effectively reduced, thereby effectively improving the binding accuracy of the chip-on-cover film.

[0070] In summary, the above is a detailed introduction to a flip chip film and its compensation method and display device provided by an embodiment of the present invention. Specific examples are used in this article to illustrate the principles and implementation methods of the present invention. The description of the above embodiments is only used to help understand the technical solution and core ideas of the present invention. Although the present invention is disclosed as above in the preferred embodiments, the above preferred embodiments are not used to limit the present invention. Ordinary technicians in this field can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention is based on the scope defined by the claims.

Claims

1. A chip-on-film, It is characterized in that include: substrate; a binding portion, the binding portion being arranged in a binding region of the substrate; as well as, An insulating film layer, the insulating film layer being disposed on the substrate and the binding portion; Wherein, the insulating film layer comprises an opening, the opening is at least arranged in the binding area, and an angle is formed between an extending direction of the opening and a side edge of a side to which the binding portion is bound; The insulating film layer further includes a first dividing portion and a second dividing portion respectively arranged at both sides of the opening, and the first dividing portion and the second dividing portion are symmetrically arranged relative to the opening, and the first dividing portion and the second dividing portion are not separated.

2. The chip-on-film according to claim 1, It is characterized in that The angle is set to be a right angle.

3. The chip-on-film according to claim 1, It is characterized in that The binding portion of the chip-on-film includes a plurality of binding terminals arranged at intervals; The first dividing portion and the second dividing portion are patterned in a region corresponding to the binding terminal, and a surface of the binding terminal is exposed to the insulating film layer.

4. The chip-on-film according to claim 1, It is characterized in that Positioning marks are also arranged on the first dividing portion and the second dividing portion.

5. The chip-on-film according to claim 1, It is characterized in that The corresponding widths at different positions of the opening are the same.

6. The chip-on-film according to claim 1, It is characterized in that The width of the opening at a location close to the binding terminal of the binding portion is greater than the width of the opening at a location far from the binding terminal.

7. The chip-on-film according to claim 6, It is characterized in that The width of the opening is 60um-150um.

8. A display device, It is characterized in that include: Display panel; as well as, A chip-on-chip film, the chip-on-chip film being bound to the display panel; The chip-on-film comprises a binding portion and an insulating film layer, a connecting terminal is provided on one side of the display panel, the binding portion is bound to the connecting terminal, and the chip-on-film is the chip-on-film as claimed in any one of claims 1-7.

9. A compensation method for flip chip film, It is characterized in that The steps include: A substrate and a chip-on-film are provided, wherein a connection terminal is provided on one side of the substrate, and the chip-on-film is the chip-on-film according to any one of claims 1 to 7; Binding the chip-on-film to the connection terminals, wherein during the binding process, first alignment marks on both sides of the chip-on-film are made to correspond to second alignment marks on both sides of the substrate, and after the alignment is completed, the offset and deflection angle of the chip-on-film relative to the substrate in the horizontal and vertical directions are measured, and a first correction is performed; The offset between the first alignment mark and the corresponding second alignment mark in the middle area of ​​the chip on film in the horizontal direction is measured, and the chip on film is corrected for the second time according to the offset.