Polyolefin elastomers in multi-pack carriers
By using polymer compositions, including recycled plastics and elastomeric ethylene copolymers in flexible plastic container carriers, the problem of extended elastic recovery time is solved, rapid and stable container installation is achieved, and effective fixation of containers is ensured and Subsequent use.
Patent Information
- Application Number
- CN202180007885.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2021-01-07
- Filing Date
- 2021-01-08
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2041-01-08
AI Technical Summary
The elastic recovery time of existing flexible plastic container carriers is extended when stretched, which affects the container installation efficiency and may cause the container to fall spontaneously.
The polymer composition is used to form a flexible sheet, including recycled low-density polyethylene and linear low-density polyethylene, combined with elastomeric ethylene copolymer, designed to provide rapid elastic recovery after the container is installed, preventing the container from deformation and shedding.
It realizes rapid elastic recovery of the container installation process while using a large amount of recycled plastic, ensures that the container is fixed and not easy to fall off, and improves the efficiency of the container carrier.
Smart Images

Figure CN114901562B_ABST
Abstract
Description
[0001] Related Applications
[0002] This application claims priority to U.S. Patent Application Serial No. 17 / 143,884, filed on January 7, 2021; U.S. Patent Application Serial No. 16 / 741,149, filed on January 13, 2020; and U.S. Provisional Application Serial No. 63 / 052,868, filed on July 16, 2020. Each of the foregoing applications is incorporated herein by reference. Technical Field
[0003] The present invention relates to a multi-pack container carrier, which includes a polyolefin elastomer for improving its elastic recovery. Background Art
[0004] Conventional container carriers are often used to package multiple similarly sized containers (e.g., cans, bottles, jars, and boxes) and / or similar containers that need to be packaged together. A flexible plastic ring carrier is one such conventional container carrier. A flexible plastic ring carrier having a plurality of container receiving apertures that each engage with a corresponding container can be used to package four, six, eight, twelve, or other suitable groups of containers together into convenient multi-packs, and these container receiving apertures are generally oval, circular, or rectangular in configuration.
[0005] Pending U.S. patent application Ser. No. 16 / 741,149, filed Jan. 13, 2020 and published as US2002 / 0223608, describes a flexible container carrier formed using a polymer blend including a low density polyethylene, a post-consumer recycled plastic blend of low density polyethylene and linear low density polyethylene, and one or more additives for improved manufacturing characteristics and / or post-consumer characteristics such as reduced degradation. Post-consumer recycled plastic (“PCRP”) is derived from end products such as plastic containers, flexible container carriers, plastic bags, and other plastic products that have completed their initial life cycle as a consumer product and can be recycled rather than discarded.
[0006] Although the increased use of PCRP in multi-piece packaging carriers is environmentally friendly, it results in a loss of elastic recovery when these carriers are stretched to enable the container to be inserted into the orifice. The extended stretching time of these carriers is detrimental to the manufacturing process because it slows down the container installation process and, in some cases, causes the container to spontaneously fall out after installation. Maintaining a relatively short recovery time is critical to effectively secure the container in the carrier and restart the installation process for the next subsequent carrier.
[0007] Therefore, there is a need or desire for a flexible plastic container carrier that is capable of including a large amount of PCRP while maintaining a standard, relatively short and effective elastic recovery time during installation of the container. Summary of the invention
[0008] The present invention relates to a flexible carrier for packaging containers, which meets the need for improved elastic recovery after the container is installed in the aperture. The flexible container carrier includes a flexible sheet and a plurality of main apertures formed in the sheet for receiving portions of the container. The flexible sheet defines an arrangement of container receiving apertures configured to allow placement on the container and to allow a uniform package of containers to be carried.
[0009] The flexible sheet is formed using a polymer composition designed to promote and optimize the use of post-consumer recycled plastics ("PRCP") while providing enhanced elastic recovery of the sheet after a container is inserted into the aperture. The flexible sheet and the container receiving aperture are designed to allow the aperture to be opened to receive the container by generally evenly distributed stretching of the container carrier. The flexible sheet may include a generally oval, circular, rectangular, or triangular container receiving aperture.
[0010] In one embodiment, the present invention relates to a flexible carrier for carrying a plurality of containers, the flexible carrier comprising a flexible sheet and a plurality of main apertures formed in the sheet for receiving portions of the containers. The flexible sheet is formed using a polymer composition comprising the following components:
[0011] from about 10% to about 95% by weight of a PCRP comprising recycled branched low density polyethylene and recycled linear low density polyethylene polymer;
[0012] Zero to about 90% by weight of a branched low density polyethylene polymer having a molecular weight of about 0.910 to about 0.950 g / cm 3 (grams / cm 3 ) density; and
[0013] From greater than zero to about 65% by weight of an elastomeric ethylene copolymer comprising from about 60% by weight to less than 100% by weight ethylene and from greater than zero to about 40% by weight of a vinyl acetate comonomer.
[0014] In another embodiment, the present invention is directed to a flexible carrier for carrying a plurality of containers, the flexible carrier comprising a flexible sheet and a plurality of main apertures formed in the sheet for receiving portions of the containers. The flexible sheet is formed using a polymer composition comprising the following components:
[0015] from about 10% to about 95% by weight of a PCRP comprising recycled branched low density polyethylene and recycled linear low density polyethylene polymer;
[0016] from about 5% to about 90% by weight of an ethylene-carbon monoxide copolymer comprising a branched low density polyethylene polymer formed using a high pressure polymerization process and a carbon monoxide comonomer; and
[0017] From greater than zero to about 65% by weight of an elastomeric ethylene copolymer comprising from about 60% by weight to less than 100% by weight ethylene and from greater than zero to about 40% by weight of a vinyl acetate comonomer.
[0018] In another embodiment, the present invention is directed to a flexible carrier for carrying a plurality of containers, the flexible carrier comprising a flexible sheet and a plurality of main apertures formed in the sheet for receiving portions of the containers. The flexible sheet is formed using a polymer composition comprising the following components:
[0019] about 40% to about 90% by weight of a PCRP comprising recycled branched low density polyethylene and recycled linear low density polyethylene polymer;
[0020] From about 10% to about 60% of an elastomeric ethylene copolymer or blend thereof with a branched low density polyethylene polymer, wherein the elastomeric ethylene copolymer or blend thereof has a combined vinyl acetate content of from about 2% to about 10% by weight.
[0021] The polymer composition used to prepare the flexible sheet may also include additives such as slip agents and other processing aids for enhancing extrusion and / or die cutting. Additives may include compounds for improving or aiding degradation (including photodegradation and / or biodegradation), such as polyolefins including up to about 20% by weight of carbon monoxide comonomers, with or without additional photodegradants or bioactive degradation agents.
[0022] In view of the foregoing, it is a feature and advantage of the present invention to provide a flexible container carrier that accommodates large amounts of PCRP and still provides excellent elastic recovery.
[0023] It is also a feature and advantage of the present invention to provide a flexible container carrier that accommodates a large number of PCRPs without slowing down the process of securing the containers in the flexible carrier.
[0024] It is also a feature and advantage of the present invention to provide a flexible container carrier that accommodates a large amount of PCRP while preventing deformation and falling off of the container due to slow elastic recovery.
[0025] The foregoing and other features and advantages of the present invention will become more apparent from the following detailed description of the invention when read in conjunction with the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 is a side elevation view of a container carrier according to an exemplary embodiment of the present invention. DETAILED DESCRIPTION
[0027] Figure 1 A flexible carrier 10 is shown for unitizing a plurality of containers into a resulting unitized package. Figure 1 A carrier having six container receiving apertures 25 is shown, but this illustration is exemplary, and the present invention is not limited to the flexible carrier shown for six containers. For example, the flexible carrier 10 may be configured and used to uniformly package four, eight, ten, twelve, or any other desired number of containers.
[0028] These containers may be cans or bottles, however, any other commonly found unitized packaging containers may be used with the flexible carrier 10 according to the invention. The containers within a single flexible carrier are preferably, but not necessarily, of the same size.
[0029] Each flexible carrier 10 may include a single layer of flexible sheet material 20 having a width and a length defining a plurality of container receiving apertures 25 therein, each of which is configured to receive a container. The plurality of container receiving apertures may be arranged in two longitudinal rows and a plurality of longitudinal columns to form an array of container receiving apertures, such as for example Figure 1 The six-container multipack shown in FIG. 1 is an array of two rows by three columns. The container receiving apertures 25 are preferably slightly elongated generally in the longitudinal direction of the flexible carrier 10. The container receiving apertures 25 and the intermediate (smaller) apertures are suitably formed into a geometry that allows the carrier to be evenly applied to the containers.
[0030] A representative package resulting from a flexible carrier includes a plurality of uniformly packaged containers. The flexible carrier 10 is typically applied to a container by stretching a portion of the flexible sheet material surrounding the container receiving opening of the container and allowing the stretched carrier to recover to provide a tight fit with the container. Effective elastic recovery of the stretched carrier is important so that the resulting container assembly can be removed from the processing machine and stored to make way for subsequent batches of containers to be installed in the flexible carrier.
[0031] like Figure 1As shown in , the flexible carrier 10 is manufactured as a generally continuous carrier strip, wherein the carriers are stamped or otherwise formed longitudinally adjacent to other carriers. In this way, a generally continuous carrier strip is formed, which can be rolled onto a reel or folded into a box shape for subsequent unwinding and application to a container. The carrier is then cut into individual carriers and packages. The container to be inserted into the container receiving aperture 25 can have varying shapes and diameters. See Figure 1 Each flexible carrier 10 is mounted on a container, for example, by stretching the carrier receiving portion 30 in a transverse direction in an opposing manner. The subsequent recovery of the carrier receiving portion 30 provides a snug fit around the rid, chime, or outer surface of the container, the strength of which is affected in part by the modulus and elastic recovery of the flexible sheet 20 used to construct the flexible carrier 10. The plan view dimensions of the flexible carrier 10 and its components vary depending on the end use. Specific end uses include, but are not limited to, soft drink and beverage cans and bottles of various sizes and shapes.
[0032] The flexible sheet material 20 used to form the flexible container carrier 10 is desirably a plastic film that can be formed by an extrusion process and then cut to form a flexible carrier. The thickness of the flexible sheet material 20 provides sufficient structural integrity to carry a desired number of containers. For example, each flexible carrier 10 can be designed to carry multiple containers of desired products with a specific weight, volume, shape, and size. For most applications, the flexible sheet material 20 can have a thickness of about 3-50 mils, suitably about 5-30 mils, and typically about 10-20 mils.
[0033] The flexible sheet 20 used to form the flexible carrier 10 is formed using a polymer composition that provides the carrier 10 with desired recovery after stretching and suitable elongation at break and strength at break. The elongation at break and strength at break are measured using the stress-strain test described in ASTM D882-91, which is incorporated by reference. Recovery after stretching can be measured using various standard and proprietary procedures.
[0034] The polymer composition for forming the flexible carrier may include PCRP, which includes recycled branched low density polyethylene and / or recycled linear low density polyethylene polymer. The polymer composition may include about 10% to about 95% PCRP by weight, suitably about 25% to about 90% PCRP by weight, or about 40% to about 90% PCRP by weight, or about 40% to about 70% PCRP by weight.
[0035] The polymer composition for forming the flexible carrier can also include branched low-density polyethylene polymers that are not recycled. The polymer composition can include zero to about 90% branched low-density polyethylene polymers by weight, or about 5% to about 90% branched low-density polyethylene polymers by weight, suitably about 10% to about 75% by weight, or about 10% to about 60% by weight, or about 30% to about 60% branched low-density polyethylene polymers by weight. The branched low-density polyethylene polymer can have a molecular weight of about 0.910 to about 0.950 g / cm 3 , or from about 0.915 to about 0.940 g / cm 3 , or about 0.920 to about 0.935 g / cm 3 density.
[0036] The polymer composition used to form the flexible carrier may also include an elastomeric ethylene copolymer. The elastomeric ethylene copolymer improves the elastic recovery of the flexible container carrier after the flexible container carrier 10 is stretched and the container is installed in the orifice 25, so that the flexible container carrier 10 and its container can fit more quickly and more tightly. The polymer composition may include an elastomeric ethylene copolymer of greater than zero to about 65% by weight, or about 2% to about 50% by weight, or about 2% to about 25% by weight, or about 2% to about 20% by weight, or about 3% to about 15% by weight, or about 3% to about 10% by weight.
[0037] The elastomeric ethylene copolymer can be ethylene-vinyl acetate and can include from about 60% by weight to less than 100% by weight ethylene and from greater than zero to about 40% by weight vinyl acetate comonomer. The elastomeric ethylene copolymer can include from about 60% to about 98% by weight, or from about 65% to about 97% by weight, or from about 70% to about 96% by weight, or from about 75% to about 95% by weight, or from about 80% to about 95% by weight ethylene. In these embodiments, the elastomeric ethylene copolymer can include from about 2% to about 40% by weight, or from about 3% to about 35% by weight, or from about 4% to about 30% by weight, or from about 5% to about 25% by weight, or from about 5% to about 20% by weight vinyl acetate. Suitable ethylene-vinyl acetate copolymers include, but are not limited to, those known by the names Those ethylene-vinyl acetate copolymers available from Dow Chemical Co.
[0038] The recycled branched low density polyethylene in the PCRP may be a high pressure polyethylene homopolymer or an ethylene-alpha olefin copolymer, and is suitably a homopolymer. Its density may be from about 0.910 to about 0.950 g / cm 3, suitably about 0.920 to about 0.935 g / cm 3 When the branched low density polyethylene is a copolymer, its density will vary depending on the amount and type of ethylene-alpha olefin comonomer. The comonomer can be C3 to C 12 alpha-olefins, suitably C4 to C8 alpha-olefins, and may constitute from zero to 20% by weight, suitably zero to 10% by weight of recycled branched low density polyethylene polymer.
[0039] The recycled linear low density polyethylene in the PCRP may have a molecular weight of from about 0.910 to about 0.950 g / cm 3 , suitably about 0.920 to about 0.935 g / cm 3 The density of the low-pressure ethylene-alpha olefin copolymer will vary depending on the amount and type of the ethylene-alpha olefin comonomer. The comonomer can be C3 to C 12 alpha-olefins, suitably C4 to C8 alpha-olefins, and may constitute from about 2 to 20% by weight, suitably about 3 to 10% by weight of the branched low density polymer.
[0040] The PCRP may include any amount (zero to 100% by weight) of recycled branched low density polyethylene and any amount (zero to 100% by weight) of recycled linear low density polyethylene, and may suitably include from about 10% to about 90% by weight of each, or from about 25% to about 75% by weight of each, or from about 40% to about 60% by weight of each.
[0041] The branched low density polyethylene that is not recycled can be a high pressure polyethylene homopolymer, or an ethylene-alpha olefin copolymer, or a copolymer of any of the foregoing items and carbon monoxide. The branched low density polyethylene is suitably a polyethylene homopolymer or a copolymer of ethylene and carbon monoxide. When the branched low density polyethylene is an ethylene-alpha olefin copolymer, its density will vary depending on the amount and type of the ethylene-alpha olefin comonomer. The comonomer can be C3 to C 12 α-olefins, suitably C4 to C8 α-olefins, and can constitute from zero to 20% by weight, suitably zero to 10% by weight of branched low density polymers. When carbon monoxide is included in the branched low density polyethylene as the only comonomer or an additional comonomer, carbon monoxide makes the carrier susceptible to degradation in the presence of ultraviolet light. When carbon monoxide is included, it can be present in about 0.1% to 20% by weight of the branched low density polymer, suitably about 1% to 10% by weight.
[0042] To ensure smooth processing, stretching and recovery, both the PCRP and the branched low density polyethylene that has not been recycled should have a melt index of about 0.2 to 3.0 grams / 10 min., suitably about 0.3 to 1.5 grams / 10 min., or about 0.4 to 0.7 grams / 10 min., measured at 190° C. using ASTM D1238. If either of the components does not have a melt index within the desired range, the combination of the PCRP and the branched low density polyethylene together, and especially the entire polymer composition, should be modified to have a melt index within the desired range.
[0043] The elastomeric ethylene copolymer may have a weight of about 0.900 to about 0.940 g / cm 3 , suitably about 0.910 to about 0.930 g / cm 3 or about 0.915 to about 0.925 g / cm 3 The elastomeric ethylene copolymer may have a melt index of about 0.2 to about 20 g / 10 min, suitably about 0.2 to 3.0 g / 10 min, or about 0.3 to 1.5 g / 10 min, or about 0.4 to 0.7 g / 10 min, measured at 190°C using ASTM D1238.
[0044] The amount of the branched low-density polyethylene of elastomeric copolymer and unrecycled can be changed to reach the vinyl acetate content of about 2% to about 12% by weight or about 3% and about 10% by weight or about 4% to about 8% by weight based on the combination of these two ingredients. For example, the higher the vinyl acetate content of the elastomeric copolymer, the less the required copolymer of the vinyl acetate reaching this level in combination. In one embodiment, the branched low-density polyethylene can be omitted to facilitate the use of the elastomeric copolymer of the vinyl acetate content of about 2% to about 12% by weight or about 3% to about 10% by weight or about 4% to about 8% by weight itself. The commercially available blend of elastomeric copolymer and branched low-density polyethylene can also be used, provided that the blend has the total vinyl acetate content in the desired range. In one example, the polymer composition can include about 40% to about 90% by weight of a PCRP comprising recycled branched low density polyethylene and recycled linear low density polyethylene polymers, and about 10% to about 60% of an elastomeric ethylene copolymer or a blend thereof with a branched low density polyethylene polymer, wherein the elastomeric ethylene copolymer or the blend thereof has a combined vinyl acetate content of about 2% to about 12% by weight, or about 3% to about 10% by weight, or about 4% to about 8% by weight.
[0045] In an alternative embodiment, the elastomeric ethylene copolymer can be an ethylene-vinyl acetate-carbon monoxide terpolymer. The terpolymer can include about 60% to about 98% by weight, or about 60% to about 90% by weight, or about 60% to about 80% by weight of ethylene. The terpolymer can include about 1% to about 20% by weight, or about 5% to about 20% by weight, or about 10% to about 20% by weight of vinyl acetate. The terpolymer can include about 1% to about 20% by weight, or about 5% to about 20% by weight, or about 10% to about 20% by weight of carbon monoxide. The presence of the carbon monoxide comonomer further contributes to the biodegradability (especially photodegradability) of the flexible carrier 10 in the presence of sunlight.
[0046] The polymer composition may include additional amounts of known and / or identifiable additives. For example, it will be appreciated that a commercially available PCRP blend based primarily on recycled branched low density polyethylene and recycled linear low density polyethylene may also include small amounts (typically less than 10% by weight, suitably less than 5% by weight) of other plastic materials. Table 1 below shows a component analysis of three batches of a suitable PCRP blend based on recycled branched low density polyethylene and recycled linear low density polyethylene. Although hexene and butene are common comonomers contained in linear low density polyethylene, propylene and styrene are typically present in separate polymers.
[0047] Table 1: Component analysis of a PCRP
[0048]
[0049] The polymer composition may also contain from about 0.1% to about 10% by weight of the composition of other optional additives to act as processing aids for enhancing or optimizing the elastic recovery of the carrier and / or prodegradants for improving the biodegradability of the carrier. Suitable prodegradants include photodegradants and bioreactive degradants, which, when used, may be present at 0.1%-10% by weight, or 0.1%-5% by weight of the composition. Examples include, but are not limited to, ATTACH® available from Colortech, Inc. in Morristown, Tennessee. 10365-16 and Symphony Environmental Technologies, Inc., United Kingdom D2w. In one embodiment, a single-site catalyzed ethylene-alpha olefin copolymer plastomer may be included, suitably at about 1% to about 10% by weight of the polymer composition, to improve the recovery and modulus properties of the flexible carrier 10. The plastomer may have a modulus of about 0.850-0.905 g / cm 3Examples of suitable single-site catalyzed ethylene-alpha olefin copolymer plastomers are available from Exxon-Mobil Chemical Co. under the tradename EXACT and from The Dow Chemical Company under the tradenames AFFINITY and ENGAGE.
[0050] Other additives that may constitute 0.1%-10% of the polymer composition include slip agents and other processing aids for enhancing extrusion and / or die cutting. Other additives may include anti-blocking agents, antioxidants and slip agents to adjust the composition to suit the stretch and recovery characteristics required for the finished container carrier.
[0051] Examples
[0052] The following materials were used in these examples:
[0053] PCRP Blend—As described in Table 1 above.
[0054] Branched LDPE - Dow 4581 (proprietary ethylene-carbon monoxide copolymer).
[0055] Ethylene Vinyl Acetate - Lyondell-Basell LB362 (a commercial blend of branched LDPE and EVA containing 6.6% total EVA).
[0056] Processing aid-KYNAR FLEX 5300.
[0057] Other additives: lubricant, antioxidant, anti-caking agent.
[0058] A polymer composition containing 55% by weight PCRP, 44% by weight Dow 4581 branched low density polyethylene, 0.25% by weight processing aids and 0.75% by weight other additives was used to form a flexible container carrier. A conventional polymer composition that does not contain PCRP and includes 99% by weight Dow 4581 as well as processing aids and other additives was used to form a similar flexible container carrier. In order to compare the elastic recovery of the two materials, the elastic recovery and modulus of the two polymer compositions were evaluated according to ASTM D882-91. It was found that the recovery time of the polymer composition containing PCRP was three to four times longer than the recovery time of the conventional polymer composition. This significant difference will slow down the time required to install the container in the carrier using PCRP.
[0059] Next, the aforementioned polymer composition containing PCRP was modified by replacing the conventional branched LDPE with LyondellBasell LB362 containing 6.6% by weight of total vinyl acetate as described above. The resulting modified polymer composition was formed into a container carrier. The elastic recovery and modulus of the modified polymer composition were evaluated according to ASTM D882-91. It was found that the modified polymer composition had an elastic recovery time that was only 10%-15% longer than that of the conventional polymer composition without PCRP, making it suitable for use in a container carrier.
[0060] The results of these evaluations are shown in Table 2 below.
[0061] Table 2: Elastic modulus and elastic recovery
[0062] Polymer composition Elastic modulus Elastic recovery LDPE+Additives 18,000±2000psi <2 seconds PRCP+LDPE+additives 18,000±2000psi 8 seconds PCRP+LDPE / EVA blend+additives 14,500psi 2 seconds
[0063] Although the present invention has been described in the foregoing specification with respect to certain preferred embodiments thereof, and many details have been set forth for purposes of illustration, it will be apparent to those skilled in the art that the flexible carrier 10 is susceptible to additional embodiments and that certain details described herein may be varied considerably without departing from the basic principles of the present invention.
Claims
1. A flexible carrier for carrying a plurality of containers, the flexible carrier comprising a flexible sheet and a plurality of main apertures formed in the sheet for receiving portions of the containers, the flexible sheet comprising a polymer composition, the polymer composition comprising: 10% to 95% by weight of PCRP comprising recycled branched low density polyethylene and recycled linear low density polyethylene polymers; Zero to 90% by weight of non-recycled branched low density polyethylene polymer having a molecular weight of 0.910 to 0.950 g / cm 3 density; and Greater than zero to 65% by weight of an elastomeric ethylene copolymer comprising 60% by weight to less than 100% by weight ethylene and greater than zero to 40% by weight of a vinyl acetate comonomer.
2. The flexible carrier according to claim 1, wherein: The recycled branched low-density polyethylene and the recycled linear low-density polyethylene polymer each have a molecular weight of 0.910 to 0.950 g / cm 3 density.
3. The flexible carrier according to claim 1, wherein: The branched low density polyethylene is present in 5 to 90% by weight of the polymer composition and comprises an ethylene homopolymer.
4. The flexible carrier according to claim 1, wherein: The branched low density polyethylene is present in 5 to 90% by weight of the polymer composition and comprises an ethylene-alpha olefin copolymer.
5. The flexible carrier according to claim 1, wherein: The elastomeric ethylene copolymer comprises 70 to 96% by weight of ethylene and 4 to 30% by weight of vinyl acetate comonomer.
6. The flexible carrier according to claim 1, wherein: The elastomeric ethylene copolymer comprises 80 to 95% by weight of ethylene and 5 to 20% by weight of vinyl acetate comonomer.
7. The flexible carrier according to claim 1, wherein: The elastomeric ethylene copolymers include ethylene-vinyl acetate-carbon monoxide terpolymers.
8. The flexible carrier according to claim 7, wherein: The ethylene-vinyl acetate-carbon monoxide terpolymer includes 60 to 90% by weight of ethylene, 5 to 20% by weight of vinyl acetate and 5 to 20% by weight of carbon monoxide.
9. The flexible carrier according to claim 1, wherein: The PCRP is present at 40% to 90% by weight of the polymer composition.
10. The flexible carrier according to claim 9, wherein: The branched low density polyethylene polymer is present at 10% to 60% by weight of the polymer composition.
11. The flexible carrier according to claim 1, wherein: The elastomeric ethylene copolymer is present in 2 to 20% by weight of the polymer composition.
12. The flexible carrier according to claim 1, wherein: The elastomeric ethylene copolymer is present at 3 to 10% by weight of the polymer composition.
13. The flexible carrier according to claim 1, wherein: The polymer composition further comprises 0.1 to 10% by weight of a photodegradant.
14. The flexible carrier according to claim 1, wherein: The polymer composition further comprises 0.1% to 10% by weight of a bioreactive degradation agent.
15. A flexible carrier for carrying a plurality of containers, the flexible carrier comprising a flexible sheet and a plurality of main apertures formed in the sheet for receiving portions of the containers, the flexible sheet comprising a polymer composition comprising: 10% to 95% by weight of PCRP comprising recycled branched low density polyethylene and recycled linear low density polyethylene polymers; 5% to 90% by weight of an ethylene-carbon monoxide copolymer comprising a branched low density polyethylene polymer formed using a high pressure polymerization process and a carbon monoxide comonomer; and Greater than zero to 65% by weight of an elastomeric ethylene copolymer comprising 60% by weight to less than 100% by weight ethylene and greater than zero to 40% by weight of a vinyl acetate comonomer.
16. The flexible carrier according to claim 15, wherein: The elastomeric ethylene copolymer comprises 70 to 96% by weight of ethylene and 4 to 30% by weight of vinyl acetate comonomer.
17. The flexible carrier according to claim 15, wherein: The elastomeric ethylene copolymers include ethylene-vinyl acetate-carbon monoxide terpolymers.
18. The flexible carrier according to claim 17, wherein: The ethylene-vinyl acetate-carbon monoxide terpolymer includes 60 to 90% by weight of ethylene, 5 to 20% by weight of vinyl acetate and 5 to 20% by weight of carbon monoxide.
19. The flexible carrier according to claim 15, wherein: The PCRP is present at 40% to 90% by weight of the polymer composition.
20. The flexible carrier according to claim 19, wherein: The ethylene-carbon monoxide copolymer is present in 10 to 60% by weight of the polymer composition.
21. The flexible carrier according to claim 15, wherein: The polymer composition further comprises 0.1 to 10% by weight of a photodegradant.
22. The flexible carrier according to claim 15, wherein: The polymer composition further comprises 0.1% to 10% by weight of a bioreactive degradation agent.
23. The flexible carrier according to claim 15, wherein: The elastomeric ethylene copolymer is present at 3 to 15% by weight of the polymer composition.
24. A flexible carrier for carrying a plurality of containers, the flexible carrier comprising a flexible sheet and a plurality of main apertures formed in the sheet for receiving portions of the containers, the flexible sheet comprising a polymer composition comprising: 40% to 90% by weight of PCRP comprising recycled branched low density polyethylene and recycled linear low density polyethylene polymers; 10% to 60% of an elastomeric ethylene copolymer or blend thereof with a branched low density polyethylene polymer, wherein the elastomeric ethylene copolymer or blend thereof has a combined vinyl acetate content of 2% to 12% by weight.
Citation Information
Patent Citations
Display element
US20030099027A1
Container carrier
US20200223608A1
Polyolefin Elastomer In Multi-Packaging Carrier
US20210214537A1
A machine and system for applying container carriers to containers
CN103221309A
Container carrier
CN104395200A