A method for trimming the curved working surface of lens polishing and trimming mold

By using emery aqueous solution and pure water of different particle sizes in stages to trim the polishing mold, the problem of edge collapse of the polishing mold is solved, the surface accuracy of the lens product is improved, and a high-precision polishing mold trimming effect is achieved.

CN114932458BActive Publication Date: 2024-10-29MLOPTIC CORP
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202210598569.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-05-30
Publication Date
2024-10-29
Estimated Expiration
2042-05-30

AI Technical Summary

Technical Problem

During the cold processing of the lens, the edge of the polished mold is prone to collapse, which affects the surface accuracy of the processed lens product. It is difficult to effectively prevent this problem with existing machine trimming methods.

Method used

Adopt a staged dressing method, first use 80 mesh emery aqueous solution for rough processing, then use W5.5 mesh emery aqueous solution for fine processing, and finally use pure water for lubrication and finishing, through a combination of emery aqueous solutions and pure water with different particle sizes Use it to ensure the radius and high-precision surface shape of the polished mold.

Benefits of technology

It effectively prevents the edge of the polishing mold from sagging, improves the accuracy of the working surface of the polishing mold, and ensures that the radius and surface shape of the polishing mold reach high precision, with a height difference of up to 0.1um.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114932458B_ABST
    Figure CN114932458B_ABST
Patent Text Reader

Abstract

The invention discloses a method for trimming the surface of a lens polishing and mold-making arc-shaped working surface. The method first uses a corundum aqueous solution as a first mold-making liquid for mold-making, and the corundum particle size in the first mold-making liquid is 80 meshes; then uses a corundum aqueous solution as a second mold-making liquid for mold-making, and the corundum particle size in the second mold-making liquid is w5.5, and finally uses pure water as a third mold-making liquid for mold-making. The method of the invention trims the polishing and mold-making in stages, and uses corundum aqueous solutions containing different particle sizes during the trimming process, first with coarse sand, then with fine sand, and finally with water, and finally reaches a polishing and mold-making with a certain radius and a high-precision surface shape. The method ensures the high precision of the radius and surface shape of the polishing and mold-making arc-shaped working surface by machine fixed trimming of the polishing and mold-making and using corundum with corresponding particle sizes in different trimming stages during trimming. When the machine is started, the corundum aqueous solution will be sprayed through a conduit to the arc-shaped contact surface between the polishing and mold-making and the polishing and mold-making. The method of the invention ensures the radius and high-precision surface shape of the polishing and mold-making, and further ensures the radius and high-precision surface shape of the polishing mold.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for trimming the surface of a lens polishing and trimming arc-shaped working surface. Background Art

[0002] During the lens cold machining process, the required polishing die radius and high-precision surface shape require trimming with a polishing die with a specific radius and high-precision surface shape. Currently, the trimming of the polishing die radius and high-precision surface shape is done manually. Most importantly, when using a machine to trim the polishing die, a liquid containing corundum is sprayed between the polishing die and the polishing counter die. When using existing corundum trimming liquid to trim the polishing die, it is easy to cause the edge of the polishing die to collapse (collapse means that too much of the edge is removed, resulting in a collapse). This in turn causes the edge of the trimmed polishing die to collapse, which in turn affects the surface accuracy of the processed lens product. Summary of the Invention

[0003] Purpose of the invention: The purpose of the present invention is to provide a method for trimming the curved working surface of a lens polishing mold, which can effectively prevent the problem of edge collapse at the polishing mold edge, thereby improving the working surface shape of the polishing mold.

[0004] Technical solution: The method for trimming the curved working surface of a lens polishing mold according to the present invention first uses a corundum aqueous solution as a first mold repair liquid for mold repair, and the corundum particle size in the first mold repair liquid is 80 mesh; then uses a corundum aqueous solution as a second mold repair liquid for mold repair, and the corundum particle size in the second mold repair liquid is w5.5; finally, pure water is used as a third mold repair liquid for mold repair.

[0005] Wherein, the mass concentration of the corundum in the first mold repairing liquid and the second mold repairing liquid is 1-10%.

[0006] Among them, when the first mold repairing liquid, the second mold repairing liquid and the third mold repairing liquid are used for mold repairing, the rotation speed of each stage is 200-300 rpm, the pressure is 1.5-2 kg; the mold repairing time of each stage is 30-60 minutes.

[0007] Among them, the dressing device adopted in the method includes a polishing die, and the polishing die includes a handle and an arc-shaped groove fixed on the upper end of the handle; the handle of the polishing die is fixed to the main shaft of the machine through a jig; the arc-shaped working surface of the polishing die is placed on the arc-shaped groove of the polishing die, and a diamond layer is provided on the arc-shaped working surface of the polishing die; the polishing die is placed on the polishing die through the iron pen head, one end of the iron pen head is pressed on the polishing die, and the other end of the iron pen head is fixedly connected to the movable shaft of the external machine, and the polishing die rotates relative to the polishing die under the drive of the machine; during the process of the polishing die driving the polishing die to rotate synchronously, a die repairing liquid is sprayed between the two, and the diamond layer on the arc-shaped working surface of the polishing die is cut by the die repairing liquid.

[0008] Among them, the fixture is a metal cylindrical relay with an external thread at one end. The fixture is fixedly connected to the machine spindle through the internal and external threads. A groove structure is provided at one end. The polishing and die repairing handle is embedded in the groove structure and fixed in the groove structure by a fastening screw.

[0009] The stylus tip is a pointed stylus tip, and the end of the polishing and film repairing handle is provided with an inward groove, which facilitates the insertion of the tip of the stylus tip, and the stylus tip is aligned and pressed into the groove of the polishing and film repairing handle.

[0010] Wherein, the polishing counter-mold and the polishing repair mold are both made of metal.

[0011] The particle size of the corundum in the first mold repair liquid is 80 mesh. When 80 mesh corundum is selected, due to the large particle size of the sand, when the mold repair curved surface moves against each other, the coarse sand between them will produce faster cutting on the two curved surfaces, so that the two curved surfaces can be quickly matched. Since the linear speed is faster at the edge, the edge of the mold repair curved surface will be removed more than the center, which is what we call a larger collapsed edge. However, a large amount of cutting is required to quickly match the two curved surfaces, and a large collapsed edge phenomenon is inevitable. This collapsed edge phenomenon will be discussed later. It is gradually eliminated during processing; for the same reason, the use of W5.5 corundum, which has a smaller particle size, will lead to less edge collapse. At this time, a smaller amount of cutting is required to quickly obtain a further match between the two curved surfaces. At this time, the surface accuracy achieved will be higher, and the edge collapse will be better. Similarly, when water is used, water will not have a cutting effect, but only a lubricating effect. At this time, when the two curved surfaces of the mold repair and the counter-mold move against each other, their two curved surfaces will have a slight cutting effect on each other, and there will be no difference in the amount of removal between the edge and the center. At this time, higher surface accuracy can be obtained and the edge collapse phenomenon can be eliminated.

[0012] Beneficial effect: The method of the present invention performs trimming on the polishing mold in stages, and uses an aqueous solution of corundum containing different particle sizes during the trimming process, first with coarse sand, then with fine sand, and finally with water, to finally achieve a polishing mold with a certain radius and high-precision surface shape. The method is through machine customization (meaning that the pressure, speed, and time are constant and the relative positions of the components remain unchanged. Only when all parameters are unchanged can one of the parameters be adjusted as needed to achieve a high-precision effect more quickly) to trim the polishing mold and use corundum of corresponding particle sizes in different trimming stages to ensure the high-precision radius and surface shape of the arc working surface of the polishing mold. When the machine is started, the corundum aqueous solution will be sprayed through the conduit to the arc contact surface between the polishing mold and the polishing counter mold. The method of the present invention ensures the radius and high-precision surface shape of the polishing mold, and thus ensures the radius and high-precision surface shape of the polishing mold. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 It is a schematic diagram of the connection between the polishing pair repair mold and the polishing repair mold;

[0014] Figure 2 This is a schematic diagram of the connection between the polishing die and the polishing die;

[0015] Figure 3 Schematic diagram of the connection between the polishing and die repairing handle and the jig. DETAILED DESCRIPTION

[0016] The method for trimming the curved working surface of a lens by polishing and trimming the mold of the present invention is specifically as follows:

[0017] First, fix the handle 11 of the polishing die 1 to the main shaft of the machine through the fixture 5, place the arc-shaped working surface 23 of the polishing die 2 into the arc-shaped groove 12 of the polishing die 1, and press the stylus head 3 connected to the movable main shaft of the machine into the groove 21 of the handle of the polishing die 2. Adjust the machine parameters (speed of 300 rpm, pressure of 2 kg), and prepare an aqueous solution containing 80# corundum as the first die-cutting liquid. Start the machine and start polishing the diamond layer on the arc-shaped working surface 23 of the polishing die 2. The first stage of rough machining, which takes 30 minutes, is designed to quickly obtain a certain radius and shape for the polishing die arc working surface. This stage involves the high-speed rotation of the polishing die 1 driven by the machine spindle and the passive rotation of the polishing die 2 arc working surface 23. Under the pressure of the stylus 3, the diamond layer on the arc working surface 23 is cut by the diamond grains in the arc-shaped contact portion between the polishing die 2 and the polishing die 1, thereby obtaining the initial radius and shape of the arc working surface of the polishing die 2.

[0018] Then, the prepared fine corundum aqueous solution is used as the second die-dressing liquid. The second die-dressing liquid adopts a corundum aqueous solution with a w5.5 concentration, and the second stage of fine processing of the polishing die 2 is started. The processing time is 30 minutes. This stage is mainly to further adjust the radius of the arc-shaped working surface 23 of the polishing die 2 and obtain a higher precision surface shape. By the high-speed rotation of the polishing die 1 driven by the machine spindle and the passive rotation of the arc-shaped working surface 23 of the polishing die 2, and under the pressure of the stylus 3, the arc-shaped contact part of the polishing die 2 and the polishing die 1 produces a cutting effect on the diamond layer on the arc-shaped working surface 23 due to the presence of corundum, thereby obtaining the arc-shaped working surface 23 of the polishing die 2 with the corresponding radius and surface shape.

[0019] Finally, pure water is used as the third die repairing liquid. At this time, water only plays a lubricating role. The most important thing is to perform the third stage of fine processing on the metal curved working surface of the polishing die 1 and the curved working surface 23 of the polishing die 2. The processing time is 45 to 60 minutes. This stage is to obtain the final radius and surface shape of the curved working surface 23 of the polishing die 2. The polishing die 1 is driven by the machine spindle to rotate at high speed and the curved working surface 23 of the polishing die 2 is passively rotated. Under the pressure of the stylus 3, the curved contact parts of the polishing die 2 and the polishing die 1 produce a cutting effect on each other due to the existence of pressure, so that the diamond layers on the curved working surfaces 23 of the polishing die 1 and the polishing die 2 produce a slight cutting on each other, thereby producing a smooth surface with a high degree of consistency between the two. At this time, the surface accuracy of the diamond layer on the curved working surface 23 of the polishing die 2 is the highest, thereby obtaining the final radius and surface shape of the curved working surface 23 of the polishing die 2.

[0020] Precision refers to the regularity of the surface shape of the polished and molded arc surface. Generally speaking, the regularity of the polished and molded surface shape in the lens processing industry is determined by the height difference. A height difference of 1 to 2 μm is considered high precision. The height difference of the polished and molded surface obtained by the method of the present invention can reach 0.1 μm.

[0021] like Figure 1As shown, the dressing device used in the method of the present invention includes a polishing die 1, which includes a handle 11 and an arc-shaped groove 12 fixed to the upper end of the handle 11; the handle 11 of the polishing die 1 is fixed to the main shaft of the machine through a jig 5; the arc-shaped working surface 23 of the polishing die 2 is placed on the arc-shaped groove 12 of the polishing die 1, and a diamond layer is provided on the arc-shaped working surface 23 of the polishing die 2; the polishing die 2 is supported on the polishing die 1 by a stylus head 3, one end of the stylus head 3 is pressed on the polishing die 2, and the other end of the stylus head 3 is fixedly connected to the movable shaft of the external machine, and the position of the polishing die 2 on the polishing die 1 is adjusted by the movable shaft; the polishing die 1 rotates relative to the polishing die 2 under the drive of the machine; in the process of the polishing die 1 driving the polishing die 2 to rotate synchronously, a die-dressing liquid is sprayed between the two, and the diamond layer on the arc-shaped working surface 23 of the polishing die 2 is cut by the die-dressing liquid. The jig 5 is a metal cylindrical relay with an external thread 7 at one end. The jig 5 is fixedly connected to the machine spindle via these threads. One end has a groove structure, into which the handle 11 of the polishing die 1 is inserted and secured by a set screw 6. The stylus 3 is a pointed stylus. The end of the handle 22 of the polishing die 2 has an indented groove 21, which facilitates the insertion of the tip of the stylus 3. The stylus 3 is then pressed into the groove 21 of the handle of the polishing die 2. Both the polishing die 1 and the polishing die 2 are made of metal.

[0022] like Figures 2-3 As shown, the handle 22 of the trimmed polishing die 2 is fixed to the main shaft of the machine through the fixture 5, and then the arc groove 41 of the polishing die 4 is placed on the arc protrusion 23 of the polishing die 2. The stylus head 3 connected to the movable main shaft of the machine is pressed into the groove 42 of the handle 43 of the polishing die 4. A layer of polishing material is loaded on the metal arc groove 41. The polishing material is polyurethane, bakelite or polishing sheet; adjust the rotation time and speed of the main shaft of the machine, as well as the pressure, the relative position of the polishing die 2 and the polishing die 4 (adjusting the position of the stylus head 3 to adjust the relative position of the polishing die 4 and the polishing die 4) 2, where the curved surfaces of the polishing die 4 contact each other). When the machine is started, the conduit automatically sprays water onto the working surfaces of the two molds. As the polishing die 2 rotates at high speed driven by the machine's main shaft, the curved working surface of the polishing die 4 passively rotates. Under the pressure of the stylus 3, the curved surfaces where the polishing die 2 and the polishing die 4 contact each other produce a cutting action, thereby obtaining the corresponding radius and surface shape of the curved groove 41 of the polishing die 4. By changing the machine's rotation time, speed, the position of the curved contact surface between the polishing die 2 and the polishing die 4, and the pressure, the curved groove 41 of the polishing die 4 with different radii and surface shapes can be obtained. Under the same rotation time, pressure, speed, and relative position, the surface accuracy of the resulting polishing die is consistent.

Claims

1. A method for trimming the curved working surface of a lens polishing mold, characterized in that: Specifically: First, the handle (11) of the polishing die (1) is fixed to the main shaft of the machine through the jig (5), the arc-shaped working surface (23) of the polishing die (2) is placed in the arc-shaped groove (12) of the polishing die (1), and the stylus head (3) connected to the movable main shaft of the machine is pressed into the groove (21) of the handle of the polishing die (2), and the machine parameters are adjusted to 300 rpm and 2 kg of pressure. At the same time, an aqueous solution containing 80# corundum is prepared as the first die-repairing liquid, and the machine is started to start polishing the die. (2) The diamond layer on the arc-shaped working surface (23) is subjected to the first stage rough machining, the machining time is 30 minutes, by which the polishing die (1) is driven by the main shaft of the machine to rotate at high speed and the arc-shaped working surface (23) of the polishing die (2) is passively rotated, and under the pressure of the stylus (3), the arc-shaped contact part between the polishing die (2) and the polishing die (1) produces a cutting effect on the diamond layer on the arc-shaped working surface (23) due to the presence of diamond sand, thereby obtaining the radius and surface shape of the initial arc-shaped working surface of the polishing die (2); Then, the prepared fine corundum aqueous solution is used as the second die repairing liquid, and the second die repairing liquid adopts a corundum aqueous solution with a w5.5, and the polishing die (2) is subjected to the second stage of fine processing, and the processing time is 30 minutes. The polishing die (1) is driven by the main shaft of the machine to rotate at a high speed and the arc-shaped working surface (23) of the polishing die (2) is passively rotated, and under the pressure of the stylus (3), the arc-shaped contact part between the polishing die (2) and the polishing die (1) produces a cutting effect on the diamond layer on the arc-shaped working surface (23) due to the presence of corundum, thereby obtaining the arc-shaped working surface (23) of the polishing die (2) with the corresponding radius and surface shape; Finally, pure water is used as the third mold repairing liquid. At this time, water only plays a lubricating role. The most important thing is to perform the third stage of finishing by polishing the metal arc-shaped working surface of the mold repairing (1) and the arc-shaped working surface (23) of the polishing mold repairing (2). The processing time is 45 to 60 minutes. In this stage, the radius and surface shape of the final arc-shaped working surface (23) of the polishing mold repairing (2) are obtained. The mold repairing (1) is driven by the machine spindle to rotate at a high speed and the arc-shaped working surface (23) of the polishing mold repairing (2) is passively rotated, and Under the pressure of the stylus tip (3), the arc-shaped contact parts of the polishing die (2) and the polishing die (1) produce a cutting effect on each other due to the existence of pressure, so that the diamond layers on the arc-shaped working surfaces (23) of the polishing die (1) and the polishing die (2) produce a slight amount of cutting on each other, thereby producing a smooth surface that is highly consistent between the two. At this time, the surface accuracy of the diamond layer on the arc-shaped working surface (23) of the polishing die (2) is the highest, thereby obtaining the final radius and surface shape of the arc-shaped working surface (23) of the polishing die (2); The polished and trimmed arc surface obtained by the above method has high surface accuracy and the height loss difference reaches 0.1um.

2. The method for trimming the curved working surface of a lens polishing mold according to claim 1, characterized in that: The finishing device used in the above method comprises a polishing die (1), wherein the polishing die (1) comprises a handle (11) and an arc-shaped groove (12) fixed to the upper end of the handle (11); the handle (11) of the polishing die (1) is fixed to the main shaft of the machine through a fixture (5); the arc-shaped working surface (33) of the polishing die (2) is placed on the arc-shaped groove (12) of the polishing die (1), and a diamond layer is provided on the arc-shaped working surface (23) of the polishing die (2); 2) The stylus head (3) is pressed against the polishing die (1), one end of the stylus head (3) is pressed against the polishing die (2), and the other end of the stylus head (3) is fixedly connected to a movable shaft of an external machine, and the polishing die (1) is driven by the machine to rotate relative to the polishing die (2); when the polishing die (1) drives the polishing die (2) to rotate synchronously, a die repairing liquid is sprayed between the two, and the diamond layer on the arc-shaped working surface (23) of the polishing die (2) is cut by the die repairing liquid.

3. The method for trimming the curved working surface of a lens polishing mold according to claim 2, characterized in that: The jig (5) is a metal cylindrical relay with an external thread (7) at one end. The jig (5) is fixedly connected to the machine spindle via the internal and external threads. A groove structure is provided at one end. The handle (11) of the polishing and repairing mold (1) is embedded in the groove structure and fixed in the groove structure via a fastening screw (6).

4. The method for trimming the curved working surface of a lens polishing mold according to claim 2, characterized in that: The stylus tip (3) is a pointed stylus tip, and a recessed groove (21) is provided at the end of the handle (22) of the polishing and film repairing device (2). The groove (21) facilitates the tip of the stylus tip (3) to be embedded, and the stylus tip (3) is aligned and pressed into the groove (21) of the handle of the polishing and film repairing device (2).

5. The method for trimming the curved working surface of a lens polishing mold according to claim 2, characterized in that: The polishing die (1) and the polishing die (2) are both made of metal.

Citation Information

Patent Citations

  • Workpiece polishing method and method of dressing polishing pad

    CN106944929A

  • Sharpening method of circular arc diamond grinding wheel

    CN110293482A

  • Surface machining device for high-precision hemispherical lens

    CN203292977U

  • Anchor clamps of optics cold working control lens center thickness

    CN208246476U

  • Method for polishing optical lenses and polishing apparatus with multiple spindles and tools for carrying out the method