A ferromagnetic pipeline flaw detection device based on pulsed eddy current and internal and external detection method

By analyzing the intersection time between the pulse eddy current tangential magnetic field signals, combined with TMR magnetic sensor detection, the problem of distinguishing defects inside and outside the ferromagnetic pipeline is solved, and efficient detection of ferromagnetic material pipelines is achieved, and data processing is simplified.

CN114965680BActive Publication Date: 2024-11-15HUBEI UNIV OF TECH +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202210515305.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-05-11
Publication Date
2024-11-15
Estimated Expiration
2042-05-11

AI Technical Summary

Technical Problem

The prior art is difficult to effectively distinguish and quantify the internal and external defects of ferromagnetic pipelines, especially in pulse eddy current detection technology, the ferromagnetic materials have a large magnetic permeability and obvious skin effect, resulting in detection problems.

Method used

The method is adopted to distinguish and quantify internal and external defects based on the time of the intersection between the pulse eddy current tangential magnetic field signals. A pair of coils parallel to the axis generates a uniform tangential magnetic field, and detects signal changes through the TMR magnetic sensor, and combines data analysis to distinguish and Quantitative defects.

Benefits of technology

It has achieved simple distinction and quantification of internal and external defects of ferromagnetic material pipelines, enriched the research on the relationship between magnetic field signals and defects in the tangential direction of pulse eddy current detection technology, and has the advantages of simple distinction methods and easy data processing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114965680B_ABST
    Figure CN114965680B_ABST
Patent Text Reader

Abstract

The present invention discloses a ferromagnetic pipeline flaw detection device based on pulse eddy current and an internal and external flaw detection method, including: based on a pair of coils with parallel axes as excitation coils, pulse excitations in opposite directions are introduced into the pair of excitation coils, and a uniform tangential magnetic field is formed between the two excitation coils. When the lift-off height between the probe and the test piece remains unchanged, the lift-off height of the TMR magnetic sensor is adjusted, and the reference signal of the low lift-off height and the detection signal of the high lift-off height obtained will produce an intersection, and the relationship between the intersection information and the internal and external defects is analyzed. Compared with the traditional method of distinguishing and quantifying the internal and external flaws of metal materials, the present invention has the advantages of simple distinguishing methods and easy data processing, and at the same time enriches the research on the influence of pulse eddy current detection technology on the relationship between tangential magnetic field signals and defects.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of electromagnetic nondestructive testing, and in particular to a ferromagnetic pipeline flaw detection device based on pulse eddy current and an internal and external detection method. Background Art

[0002] Pipelines are one of the most commonly used transportation methods for oil and natural gas. Fatigue and corrosion defects will occur during long-term use. If they are not discovered in time, serious energy leakage will occur, which will not only cause serious damage to the environment and bring great economic losses, but also oil and gas are flammable and explosive, which can easily cause serious safety accidents. Therefore, non-destructive testing and structural health monitoring of pipelines, timely detection and treatment of defects are of great significance to ensure industrial production and the safety of people's lives and property.

[0003] Pulsed eddy current testing technology is a new technology developed on the basis of eddy current testing technology in recent years. The excitation source used is a pulsed square wave, which has a rich frequency and can reflect multiple defect information of different depths at the same time in one test. As the working conditions of oil and gas pipelines become more and more complex, the ordinary presence or absence of defects and the quantification of surface defects can no longer meet the needs of industrial production. Classification of oil and gas pipeline defects has always been a difficult problem. With the continuous in-depth research and development of pulsed eddy current technology, its potential in classifying different defects is attracting the attention of many scholars.

[0004] Pulse eddy current testing technology mainly focuses on the detection of defects in metal plates. The progress and achievements in distinguishing internal and external defects of metal materials are mainly concentrated in non-metallic materials. The characteristic quantities commonly used in quantifying metal defects in non-ferromagnetic materials are: peak value, peak time, zero-crossing time, etc. of the transient response signal. Since ferromagnetic materials have a large magnetic permeability, obvious skin effect, and limited penetration depth, it is necessary to prepare specific high-power current source equipment when detecting internal defects. In addition, the response characteristics are greatly different from those of non-ferromagnetic metal materials, mainly concentrated in the late signal period. At present, pulse eddy current testing technology is mainly used in the thinning of thick walls of pipelines under the coating layer. Therefore, further strengthening the research on pulse eddy current testing in the detection of internal and external defects of ferromagnetic metals is of great significance to solving the problem of distinguishing internal and external defects of oil and gas pipelines. Summary of the invention

[0005] In order to solve the technical problem that it is difficult to distinguish and quantify the internal and external defects of ferromagnetic pipes mentioned above, the present invention provides a method for distinguishing and quantifying internal and external defects based on analyzing the time of the intersection between the pulse eddy current tangential magnetic field signals. A pair of coils with parallel axes are used as excitation coils, and pulse currents in opposite directions are passed through the pair of excitation coils. At this time, a uniform tangential magnetic field is formed between the two excitation coils. Keeping the probe lift-off height unchanged, adjusting the magnetic sensor lift-off height to obtain a reference signal at a low lift-off height and a detection signal at a high lift-off height will produce an intersection, and the relationship between the intersection information and the internal and external defects is analyzed. Compared with traditional methods for distinguishing and quantifying internal and external defects of metal materials, the present invention has the advantages of simple distinction methods and easy data processing, and at the same time enriches the research on the influence of pulse eddy current detection technology on the relationship between tangential magnetic field signals and defects.

[0006] In order to achieve the above object, the present invention adopts the following specific scheme:

[0007] A pair of excitation coils and a TMR magnetic sensor; the inner diameters of the two excitation coils are both larger than the spacing between the excitation coils, the two excitation coils are at the same horizontal height and are parallel to the surface of the test piece; a signal generator is connected to the two excitation coils, and pulse excitation signals with opposite current directions are input to the two excitation coils; the TMR magnetic sensor is located in the middle of the two excitation coils, and the height during detection can be freely adjusted according to the actual detection situation. The sensitive direction is the tangential magnetic field direction, and the change in the tangential magnetic field intensity is converted into a voltage signal, which is output to a computer for analysis through a data acquisition card.

[0008] Preferably, the excitation coil is a racetrack ring, the vertical cross section of the coil is rectangular, and the horizontal cross section is in the shape of a racetrack. When the two excitation coils are subjected to reverse excitation, the tested piece generates uniform tangential eddy currents in the area directly below the two coils. Compared with the cylindrical coil, the tangential eddy currents generated by the racetrack coil on the tested piece are stronger and wider in range.

[0009] Preferably, the pulse excitation signal is a square wave pulse signal with a frequency of 20 to 200 Hz.

[0010] The working principle of the probe is:

[0011] A reverse pulse excitation is introduced into the double-track coil to generate a primary magnetic field. The primary magnetic field induces transient eddy currents on the test piece, and the transient eddy currents induce a secondary magnetic field (induced magnetic field); when the two excitation coils work at the same time, the main magnetic flux directions are opposite, and the middle area of ​​the excitation coil will generate a tangential magnetic field parallel to the surface of the test piece. A TMR magnetic sensor with a sensitive direction in the tangential direction is selected and placed in the middle position of the two excitation coils to measure the change in the superimposed magnetic field strength of the primary magnetic field and the secondary magnetic field and output it as a voltage signal. When there are defects in the test piece, the induced magnetic field strength will change compared to that of the defect-free one, causing the detection signal output by the magnetic sensor to change. By analyzing the relevant characteristics of the detection signal, information about the size and type of the defect can be obtained. The probe is always kept at a certain height from the test piece, and the TMR magnetic sensor is placed at the upper limit of the lift-off height to obtain detection signals of surface defects and internal defects of different depths in standard test pieces with only surface defects or only internal defects. Then replace the defect-free standard specimen of the same material and size, gradually lower the lift-off height of the TMR magnetic sensor from the upper limit of the lift-off height, and obtain multiple sets of reference signals. The detection signals of the standard specimen with only surface defects or only internal defects are merged with the multiple sets of reference signals obtained into the same coordinate system. It can be found that as the lift-off height of the TMR magnetic sensor decreases, the reference signal will gradually increase and produce intersections with the detection signals of defects of different depths. Since the diffusion process of the induced eddy current from the surface to the inside of the test piece has a certain time sequence, the change of the induced voltage signal caused by the surface defect is earlier than that of the internal defect. When there is a surface defect, the time of the intersection is in the first half of the cycle and increases with the increase of the defect depth; when there is an internal defect, the time of the intersection is in the second half of the cycle and increases with the increase of the defect burial depth. The internal and external defects can be distinguished and quantified through the intersection information.

[0012] The method for distinguishing internal and external damage of ferromagnetic materials based on the intersection information of pulse eddy current tangential magnetic field signal:

[0013] S1. Place the pair of excitation coils above a defect-free test piece, adjust the TMR magnetic sensor to the upper limit of the reference signal lift-off height, use a pulse power supply to provide a pulse excitation signal to the two excitation coils, measure the tangential response magnetic field intensity through the TMR magnetic sensor to obtain a reference signal, gradually reduce the TMR magnetic sensor lift-off height, and obtain multiple groups of reference signals corresponding to different TMR magnetic sensor lift-off heights;

[0014] S2, replacing the defect-free specimen with a standard specimen having only surface defects or only internal defects, and gradually deepening the defect depth, adjusting the TMR magnetic sensor to a position higher than the upper limit of the reference signal lift-off height, measuring the tangential response magnetic field intensity by the TMR magnetic sensor to obtain a detection signal, merging the detection signal of the standard specimen having only surface defects or only internal defects and the multiple groups of reference signals obtained in step S1 into the same coordinate system, taking a group of reference signals that have intersections with all the detection signal curves as the optimal reference signal, wherein the optimal reference signal intersects with the detection signal of the standard specimen having surface defects in the first half period, and intersects with the detection signal of the standard specimen having internal defects in the second half period;

[0015] S3, for the data from the reference test piece with only surface defects, the peak value data of the first half cycle of the detection signal and the corresponding surface defect depth data are fitted to obtain a peak value-depth relationship curve, and the peak time data of the first half cycle of the detection signal and the corresponding surface defect depth data are fitted to obtain a peak time-depth relationship curve;

[0016] For the data from the reference test piece with only internal defects, the intersection time-burial depth relationship curve is obtained by fitting the relationship curve between the intersection time data of the detection signal and the optimal reference signal and the corresponding internal buried depth defect depth data, and the intersection magnetic field intensity-burial depth relationship curve is obtained by fitting the relationship curve between the intersection tangential magnetic field intensity data of the detection signal and the optimal reference signal and the corresponding internal buried depth defect depth data;

[0017] S4, replacing the reference test piece with the test piece to be tested, keeping the lift-off height of the TMR magnetic sensor the same as the lift-off height in step S2, measuring the tangential response magnetic field intensity by the TMR magnetic sensor to obtain a detection signal, and merging it with the optimal reference signal into the same coordinate system;

[0018] S5, judging whether the detection signal obtained in step S4 has an intersection with the optimal reference signal. If there is no intersection, it means that the test piece to be detected has neither surface defects nor internal defects; if the detection signal and the optimal reference signal have an intersection in the first half cycle, it means that the test piece to be detected has a surface defect; if the detection signal and the optimal reference signal have an intersection in the second half cycle, it means that the test piece to be detected has an internal defect;

[0019] S6. If it is determined that there is a surface defect, the surface defect depth of the test piece corresponding to the peak value and peak time is quantified according to the peak value and peak time of the first half cycle of the detection signal and compared with the peak value-depth relationship curve and the peak time-depth relationship curve;

[0020] If it is determined that there is an internal defect, the internal defect depth of the test piece corresponding to the intersection time and intersection magnetic field is quantified based on the intersection time of the test signal and the reference signal and the tangential magnetic field strength at the intersection, and compared with the intersection time-depth relationship curve and the intersection magnetic field-deep burial relationship curve.

[0021] Compared with the prior art, the present invention has the following advantages:

[0022] At present, most of the research on pulsed eddy current detection signals focuses on normal magnetic field signals, and less research is done on tangential magnetic field signals. The present invention proposes a ferromagnetic material pipeline flaw detection device and an internal and external flaw detection method by studying and analyzing pulsed eddy current tangential magnetic field signals. Compared with the prior art, the present invention has the advantages of simple differentiation method and easy data processing. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the present invention and, together with the description, are used to explain the principles of the present invention;

[0024] Figure 1 It is a schematic diagram of double-track probe detection based on tangential magnetic field signals of the present invention;

[0025] Figure 2 It is a flow chart of the double-track probe detection used in the present invention;

[0026] Figure 3 It is a schematic diagram of the double-track type probe used in the present invention to detect the magnetic field;

[0027] Figure 4 is a schematic diagram of a detection signal / reference signal of the present invention;

[0028] Figure 5 It is a schematic diagram of the intersection of the surface defect detection signal of the present invention and different lift-off reference signals;

[0029] Figure 6 It is a schematic diagram of the intersection of the internal defect detection signal of the present invention and different lift-off reference signals;

[0030] Figure 7 It is a schematic diagram showing that the surface defect depth is positively correlated with the peak value and peak time of the detection signal before the detection signal;

[0031] Figure 8 It is a schematic diagram showing that the buried depth of internal defects in the present invention is positively correlated with the magnitude of the magnetic field intensity corresponding to the intersection point and time. Specific implementation methods

[0032] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0033] Embodiment 1:

[0034] The present invention is based on the double-track probe detection of tangential magnetic field signals, such as Figure 1 As shown, the probe includes a left runway type excitation coil 1, a right runway type excitation coil 2 and a TMR magnetic sensor, and the inner diameter of the two excitation coils is greater than the spacing between the excitation coils. The TMR magnetic sensor is located in the middle of the two excitation coils, and the height during detection is freely adjusted according to the actual detection situation. The sensitive direction is the tangential magnetic field direction, and the change in the tangential magnetic field intensity is converted into a voltage signal. The induced voltage signal of multiple cycles is continuously collected by the data acquisition card and output to the computer for analysis.

[0035] The excitation coil is a runway coil, the vertical cross section of the coil is rectangular, the horizontal cross section is in the shape of a runway, the number of turns is 200, the coil is 80mm long, 30mm wide and 12mm high. It is made of enameled wire with a diameter of 0.03m to 0.1mm and is tightly wound in a space spiral. The TMR magnetic sensor uses a high-sensitivity, low-noise TMR linear sensor produced by Multidimensional Technology. The TMR magnetic sensor is located at the geometric center of the lower surface of the left runway-type excitation coil 1 and the right runway-type excitation coil 2. The sensitive axis direction is parallel to the surface of the test piece and points to the positive direction of the X-axis. When the two excitation coils are subjected to reverse excitation, the test piece generates uniform tangential eddy currents in the area directly below the two coils. Compared with the cylindrical coil, the runway coil generates a wider range of tangential eddy currents on the test piece, and the generated induced magnetic field is correspondingly wider and easier to detect.

[0036] like Figure 1 As shown, the detection schematic diagram also includes: a detection signal extraction height position 3, a reference signal extraction height position 4, a test piece 5, a surface defect 6 and an internal defect 7.

[0037] The dual-track probe based on measuring the tangential magnetic field signal is placed at a height of 2mm above the test piece and remains unchanged. The upper limit of the lift-off height of the TMR magnetic sensor is set to 2mm (the lift-off height of the probe remains unchanged during the detection process, and the TMR magnetic sensor can be adjusted downward from the upper limit of the lift-off height). A pulse power supply is used to provide a square wave pulse excitation signal with a frequency of 100Hz to the two excitation coils. The steel pipe of the test piece is magnetized, and the coils are superimposed to generate a stable and uniform tangential magnetic field.

[0038] The signal output by the TMR magnetic sensor is measured by the tangential response magnetic field strength, such as Figure 4 As shown (7 and 8 in the figure are the first half cycle and the second half cycle of the signal curve respectively).

[0039] On a defect-free standard specimen, the lift-off height of the TMR magnetic sensor is gradually reduced from the upper limit of the lift-off height of 2 mm to obtain multiple reference signal curves at different lift-off heights.

[0040] Adjust the TMR magnetic sensor back to the upper limit of the lift-off height of 2 mm, replace the test piece with surface defects of different depths, and measure the tangential response magnetic field intensity with the TMR magnetic sensor to obtain the detection signal of defects of different depths.

[0041] Keep the TMR magnetic sensor at the upper limit of the lift-off height of 2mm, replace the test piece with internal defects of different buried depths, and measure the tangential response magnetic field intensity with the TMR magnetic sensor to obtain the detection signal of defects with different buried depths.

[0042] After merging the multiple reference signal curves at different lift-off heights and the multiple groups of surface defect or internal defect detection signals into the same coordinate system, it is found that: when the TMR magnetic sensor is reduced from the lift-off height to 0.5mm, the reference signal obtained and the detection signals of all surface defects of different depths and all internal defects of different buried depths all produce intersections, so the reference signal (optimal reference signal) obtained by the TMR magnetic sensor at a lift-off height of 0.5mm is selected. A pattern can be found: when the test piece under inspection has surface defects, the intersection time of the reference signal and the detection signal is in the first half of the cycle, and increases with the increase of the defect depth; when the test piece under inspection has internal defects, the intersection time of the reference signal and the detection signal is in the second half of the cycle, and increases with the increase of the defect burial depth. The reference signal obtained by the TMR magnetic sensor at a lift-off height of 0.5mm and the multiple groups of surface defect or internal defect detection signals are merged into the same coordinate system to obtain the intersection information of the reference signal and the detection signal.

[0043] When the tested piece has no defects, there is no intersection between the reference signal and the detection signal;

[0044] When the tested piece has a surface defect, the reference signal and the test signal intersect, and the intersection time is in the first half cycle. The peak value and peak time of the first half cycle of the test signal have a strong linear relationship with the depth of the surface defect. Figure 7 The peak-depth relationship curve and the peak-time-depth relationship curve quantify the surface defect depth of the test piece corresponding to the peak value and the peak time;

[0045] When there is an internal defect in the tested piece, the reference signal and the test signal have an intersection, and the intersection time is in the second half of the cycle. The intersection time increases with the increase of the internal defect burial depth; the tangential magnetic field strength at the intersection decreases with the increase of the internal defect burial depth. According to the intersection time of the test signal and the reference signal and the tangential magnetic field strength at the intersection, Figure 8 The intersection time-embedded depth relationship curve and the intersection magnetic field strength-embedded depth relationship curve quantify the internal defect embedded depth of the test piece corresponding to the intersection time and the intersection magnetic field strength.

Claims

1. A method for detecting internal and external flaws of a ferromagnetic pipeline flaw detector based on pulsed eddy current, characterized in that: The flaw detection device comprises: a pair of excitation coils and a TMR magnetic sensor; the inner diameters of the two excitation coils are both larger than the spacing between the excitation coils, the two excitation coils are at the same horizontal height and are parallel to the surface of the tested piece; a signal generator is connected to the two excitation coils, and inputs pulse excitation signals with opposite current directions to the two excitation coils; the TMR magnetic sensor is located in the middle of the two excitation coils, and the height during detection is freely adjusted according to the actual detection situation, and the sensitive direction is the tangential magnetic field direction, and the change of the tangential magnetic field intensity is converted into a voltage signal, which is output to a computer for analysis through a data acquisition card; The detection method comprises the following steps: S1. Place the pair of excitation coils above a defect-free test piece, adjust the TMR magnetic sensor to the upper limit of the reference signal lift-off height, use a pulse power supply to provide a pulse excitation signal to the two excitation coils, measure the tangential response magnetic field intensity through the TMR magnetic sensor to obtain a reference signal, gradually reduce the TMR magnetic sensor lift-off height, and obtain multiple groups of reference signals corresponding to different TMR magnetic sensor lift-off heights; S2, replacing the defect-free specimen with a standard specimen having only surface defects or only internal defects, and gradually deepening the defect depth, adjusting the TMR magnetic sensor to a position higher than the upper limit of the reference signal lift-off height, measuring the tangential response magnetic field intensity by the TMR magnetic sensor to obtain a detection signal, merging the detection signal of the standard specimen having only surface defects or only internal defects and the multiple groups of reference signals obtained in step S1 into the same coordinate system, taking a group of reference signals that have intersections with all the detection signal curves as the optimal reference signal, wherein the optimal reference signal intersects with the detection signal of the standard specimen having surface defects in the first half period, and intersects with the detection signal of the standard specimen having internal defects in the second half period; S3, for the data from the reference test piece with only surface defects, the peak value data of the first half cycle of the detection signal and the corresponding surface defect depth data are fitted to obtain a peak value-depth relationship curve, and the peak time data of the first half cycle of the detection signal and the corresponding surface defect depth data are fitted to obtain a peak time-depth relationship curve; For the data from the reference test piece with only internal defects, the intersection time-embedded depth relationship curve is obtained by fitting the relationship curve between the intersection time data of the detection signal and the optimal reference signal and the corresponding internal defect depth data, and the intersection magnetic field intensity-embedded depth relationship curve is obtained by fitting the relationship curve between the intersection tangential magnetic field intensity data of the detection signal and the optimal reference signal and the corresponding internal defect depth data; S4, replacing the reference test piece with the test piece to be tested, keeping the lift-off height of the TMR magnetic sensor the same as the lift-off height in step S2, measuring the tangential response magnetic field intensity by the TMR magnetic sensor to obtain a detection signal, and merging it with the optimal reference signal into the same coordinate system; S5, judging whether the detection signal obtained in step S4 has an intersection with the optimal reference signal. If there is no intersection, it means that the test piece to be detected has neither surface defects nor internal defects; if the detection signal and the optimal reference signal have an intersection in the first half cycle, it means that the test piece to be detected has a surface defect; if the detection signal and the optimal reference signal have an intersection in the second half cycle, it means that the test piece to be detected has an internal defect; S6. If it is determined that there is a surface defect, the surface defect depth of the test piece corresponding to the peak value and peak time is quantified according to the peak value and peak time of the first half cycle of the detection signal and compared with the peak value-depth relationship curve and the peak time-depth relationship curve; If it is determined that there is an internal defect, the internal defect burial depth of the test piece corresponding to the intersection time and intersection magnetic field strength is quantified based on the intersection time of the test signal and the reference signal and the tangential magnetic field strength at the intersection, and compared with the intersection time-burial depth relationship curve and the intersection magnetic field strength-burial depth relationship curve.

Citation Information

Patent Citations

  • Flexible magnetic saturation pulse eddy current test probe and test method

    CN107505388A

  • Flexible spiral transient eddy current shimming excitation probe and defect detection method

    CN114034766A

  • Rotary eddy current integrated damage detection device

    CN210322898U

  • Super sensitive eddy-current electromagnetic probe system and method for inspecting anomalies in conducting plates