Method for generating a conductive pattern on a substrate
Through electromagnetic radiation heating and pressing technology, the substrate heat absorption problem caused by hot melt heating is solved, and the conductive pattern formation with low energy consumption and environmental protection is achieved, which is suitable for various cellulose and polymer materials.
Patent Information
- Application Number
- CN202080088746.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-12-20
- Filing Date
- 2020-12-17
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2040-12-17
AI Technical Summary
Prior art When forming a conductive pattern on a substrate, hot melt heating causes the substrate to absorb heat, which may cause dimensional changes, drying or combustion, and high energy consumption.
Electromagnetic radiation heating is used, with a wavelength in the range of 600-1400nm, so that the temperature of the conductive solid particles exceeds the melting point, and then press it in the pressure zone to form a conductive pattern to reduce the heat absorption of the substrate.
It reduces substrate heat absorption, reduces energy consumption, and avoids substrate damage. It is suitable for thermally sensitive and environmentally friendly materials.
Abstract
Description
Technical Field
[0001] The present invention relates to a method for producing a conductive pattern on a substrate and a method for producing an RFID tag. Background Art
[0002] Prior Art - Problem
[0003] It is known to form a conductive pattern on a substrate, wherein solid conductive particles are formed into a predetermined pattern on the substrate. The solid particles are then heated, usually by thermal heating, in an oven, where they reach a temperature above their characteristic melting point. The particles are then pressed into a nip so that they are flattened, wherein the particles are electrically connected to each other and thereby form a conductive pattern.
[0004] One disadvantage of this method is that during the heating process not only the solid particles absorb heat, but also the substrate. This can cause problems, for example, that the fiber substrate dries out when heated. This will lead to unwanted dimensional changes in the substrate. In addition, if heated to too high a temperature, the fibers will start to turn brown or even burn. In addition, the energy consumption of hot melt heating is relatively high. Summary of the invention
[0005] Purpose of the Invention
[0006] It is an object of the present invention to provide a method for generating a conductive pattern on a substrate which at least partially solves the above-mentioned problems.
[0007] The present invention is a method for generating a conductive pattern on a substrate, wherein the method comprises the following steps:
[0008] - forming an adhesive layer of a predetermined pattern on a substrate made of at least one of a cellulose material and a polymer material,
[0009] - adding conductive solid particles to the adhesive layer, wherein the particles adhere to the adhesive,
[0010] - heating the solid particles by electromagnetic radiation, wherein the wavelength of the electromagnetic spectrum is in the range of 600-1400 nm, preferably in the range of 700-1200 nm, so that the temperature of the particles exceeds their characteristic melting point, and
[0011] - Pressing the heated particles into a nip of the substrate, where the particles are flattened, so that the particles are electrically connected to each other and thereby form the conductive pattern.
[0012] Furthermore, the present invention is a method for generating an RFID tag, wherein the method comprises the following steps:
[0013] - forming an adhesive layer of a predetermined pattern on a substrate made of at least one of a cellulose material and a polymer material,
[0014] - adding conductive solid particles to the adhesive layer, wherein the particles adhere to the adhesive,
[0015] - heating the solid particles by electromagnetic radiation, wherein the wavelength of the electromagnetic spectrum is in the range of 600-1400 nm, preferably in the range of 700-1200 nm, so that the temperature of the particles exceeds their characteristic melting point, and
[0016] - pressing the heated particles into a nip of the substrate, where they are flattened so that they are electrically connected to one another and thereby form an antenna, and
[0017] - attaching an integrated circuit (IC) to the antenna such that an electrical connection is established between the IC and the antenna, wherein the antenna and the IC form the RFID tag. DETAILED DESCRIPTION
[0018] The method for generating a conductive pattern on a substrate according to the present invention will be described in more detail below with reference to some preferred embodiments.
[0019] The method comprises the following steps: forming a predetermined pattern of adhesive layers on the substrate. The adhesive pattern can be applied by the method for applying the adhesive pattern to any suitable nip on the substrate, such as inkjet, flexographic printing, relief printing, gravure printing, screen printing, spraying, web coating, wheel coating, brushing, or comprising any other method that can deposit the adhesive pattern on the substrate. The adhesive can be any suitable adhesive for this purpose. A preferred adhesive is an acrylic acid-based adhesive, such as styrene / acrylate, styrene / butadiene or PVAc emulsion. The adhesive can also be a starch-based adhesive, such as modified starch.
[0020] The substrate can be a paper or paperboard material, because these cellulose materials have very good adhesion properties to the conductive pattern. In addition, paper and paperboard are environmentally friendly because they are biodegradable and recyclable. A preferred substrate is a cellulose substrate with a particle size of 30 to 200 gsm. In addition, the substrate can be a single or multiple substrates. Another suitable cellulose substrate is a substrate made of microfibrillated cellulose (micro fibrillated cellulose, MFC) or a film made of microfibrillated cellulose.
[0021] However, it will be appreciated by those skilled in the art that other non-conductive substrates are possible, such as polyester taffeta or nylon. The above polymer substrates are particularly suitable if the product (e.g. a care label on a garment containing washing instructions) is to be used in a humid environment. These polymers are highly sensitive to heat, so the present invention is also very suitable for these materials. It will also be appreciated by those skilled in the art that the substrate may be made of a combination of cellulosic and polymeric materials.
[0022] The method further comprises the step of adding conductive solid particles to the adhesive layer pattern, wherein the particles adhere to the adhesive. The solid particles can be added in a variety of different ways, and the invention is not limited to a particular method of addition. For example, the adding step can be blowing the solid particles onto the adhesive, dipping the substrate into a particle bed, wherein the particles adhere to the adhesive pattern, or by electrostatic transfer.
[0023] The conductive solid particles are preferably made of a solder material of a non-eutectic alloy. However, most preferred are alloys containing tin and bismuth or alloys containing only tin. Tin and bismuth are lead-free and therefore more environmentally friendly. Moreover, they have a relatively low melting temperature and relatively good electrical conductivity.
[0024] The method further comprises at least one heating step. The heating is performed by heating the solid particles by electromagnetic radiation, wherein the wavelength of the electromagnetic spectrum is in the range of 600-1400 nm, preferably in the range of 700-1200 nm, so that the temperature of the particles exceeds their characteristic melting point.
[0025] The energy of electromagnetic radiation is 1.5-2.8MW / μm m 2 within the range.
[0026] Tests have shown that electromagnetic radiation at these short wavelengths is well suited for heating / melting solid solder particles of non-eutectic alloys. In this range, the radiation excites a combination of molecular vibrations and harmonics. This means that the molar absorptivity is generally small in this part of the electromagnetic spectrum, with the result that many polymer compounds do not have a strong absorptivity and are therefore not easily heated when irradiated with such a short wavelength of electromagnetic radiation. Electromagnetic radiation with these short wavelengths has the potential to selectively heat materials with strong absorptivity in this part of the spectrum, and the inherent energy density of the electromagnetic radiation will enable it to achieve a high speed, while the underlying substrate will enable the radiation to penetrate the substrate, thereby avoiding damage. Electromagnetic radiation with such a short wavelength is also referred to as near infrared (Near Infrared) or NIR. Electromagnetic radiation can be applied directly to the front side of the substrate facing the solid particles, or to the back side of the substrate away from the solid particles, or to both sides of the substrate at the same time.
[0027] As a result, paper, fiber-based substrates and most common plastic packaging do not absorb radiation significantly at these short wavelengths. This means that unnecessary heating of the substrate, which can indirectly have a negative impact on substrates made of paper, cardboard, polyester and nylon, is greatly reduced.
[0028] The method further comprises the following steps: pressing the heated particles onto a substrate. The pressing is performed in a nip zone, the surface temperature of which is lower than the characteristic melting temperature of the particles. Pressing the nip zone will flatten the particles, so that the particles are electrically connected to each other and thus form a conductive pattern.
[0029] The pressing is preferably applied as soon as possible after the radiant heating, wherein the particles still remain in an almost molten state. Thus, the previously molten material solidifies in the form of a substantially continuous conductive pattern.
[0030] The nip may be a non-heated nip. Preferably, however, the surface of the nip is heated to a temperature slightly below the characteristic melting temperature (such as 30-60° C.). This ensures, for example, that the melt does not solidify prematurely before being pressed onto the substrate. The nip will cause the previously melted material of the initially solid conductive particles to solidify again, but this time not in the form of separate particles, but in the form of a substantially continuous conductive layer arranged in a predetermined pattern.
[0031] The method may also involve one or more additional heating steps. These additional heating steps may be provided before and / or after the short-wavelength electromagnetic radiation step.
[0032] The additional heating step may be infrared radiation (IR) heating with a wavelength of 1500 nm and above. The IR source is preferably 2×2 kW IR lamps or 4×2 kW IR lamps. A preferred embodiment is to perform IR heating with a wavelength of 1500 nm and above after the electromagnetic radiation step with a wavelength range of 600-1400 nm.
[0033] The additional heating step may also be hot melt heating in an oven, wherein the temperature of the oven is below 200°C.
[0034] Additional heating steps may be advantageous because the conductors may be geometries of various shapes and sizes. Combinations of different heating steps may heat different geometries differently. For example, one heating method may heat the narrow shapes or edges of a solid pattern first, while another heating method may heat the center of the solid pattern first. Therefore, it may be beneficial to accompany the electromagnetic radiation heating step (wavelength 600-1400nm) of the present invention with IR and / or hot melt heating to achieve a balanced and uniform heating profile for a variety of geometries.
[0035] In a preferred embodiment of the present invention, the formed conductive pattern is an antenna, preferably an antenna for an RFID tag.
[0036] In another embodiment, the present invention includes a method for producing an RFID tag. This embodiment is the same as the above embodiment, and further includes the following steps: attaching an integrated circuit (IC) or a microchip to the conductive pattern, i.e., the antenna, so as to establish an electrical connection between the IC and the antenna, wherein the antenna and the IC form an RFID tag.
[0037] The attachment of the IC to the antenna can be achieved in various ways. In a first embodiment, the IC is attached to the antenna by applying an adhesive between the IC and the antenna pad area and pressing the IC onto the RFID antenna. In a second embodiment, the IC is attached by soldering.
[0038] Compared with the prior art, some advantages of the method according to the present invention are:
[0039] The substrate will absorb less heat, which means less risk of substrate damage.
[0040] · Since heat is directed to where it is needed, energy consumption will be reduced.
[0041] Due to the heating step of the present invention, energy consumption will be reduced even if additional heating is used.
[0042] • The method of the invention allows the use of heat-sensitive substrates.
[0043] Substrates made of cellulose and / or polymers do not significantly absorb radiation at these short wavelengths. This means that unnecessary heating of the substrate is greatly reduced, as heating and cooling of the substrate has been shown to increase stresses in the substrate, which can lead to cracks, etc.
[0044] In the foregoing, the invention has been described based on some preferred embodiments. However, those skilled in the art will appreciate that additional embodiments and variations are possible within the scope of the appended claims.
[0045] For example, the present invention is not only applicable to the production of antennas for RFID tags. Those skilled in the art will appreciate that the method of the present invention can be used to produce other conductive patterns, such as printed wiring, conductors for flexible batteries, displays, sensors, heaters or the like.
Claims
1. A method for generating a conductive pattern on a substrate, in, The method comprises the following steps: - forming an adhesive layer of a predetermined pattern on a substrate made of at least one of a cellulose material and a polymer material, - adding conductive solid particles to the adhesive layer, wherein the conductive solid particles adhere to the adhesive layer, - heating the conductive solid particles by electromagnetic radiation, wherein the wavelength of the electromagnetic spectrum is in the range of 600-1400 nm, so that the temperature of the conductive solid particles exceeds their characteristic melting point, and - pressing the heated conductive solid particles into a nip of the substrate, where the conductive solid particles are flattened, so that the conductive solid particles are electrically connected to each other and thereby form the conductive pattern, and - at least one additional heating step, in which the conductive solid particles are heated to a temperature below the characteristic melting point, wherein the additional heating step is performed by infrared radiation heating, wherein the wavelength of the IR source is 1500nm and above.
2. The method according to claim 1, in, The additional heating step is hot melt heating in an oven, wherein the temperature of the oven is lower than 200°C.
3. The method according to claim 1 or 2, in, The energy radiation of the electromagnetic radiation is 1.5-2.8 MW / μmm 2 within the range.
4. The method according to claim 1 or 2, in, The conductive solid particles are made of a eutectic alloy.
5. The method according to claim 4, in, The eutectic alloy includes tin.
6. The method according to claim 1 or 2, in, The substrate is made of paper or paperboard material.
7. The method according to claim 1 or 2, in, The substrate is made of polyester fiber or nylon.
8. The method according to claim 1 or 2, in, The conductive pattern is an antenna.
9. The method according to claim 8, in, The method further includes the step of attaching an integrated circuit to the antenna, thereby establishing an electrical connection between the integrated circuit and the antenna, wherein the antenna and the integrated circuit form an RFID tag.
10. The method according to claim 1, in, The wavelengths of the electromagnetic spectrum are in the range of 700-1200nm.
11. The method according to claim 5, in, The eutectic alloy includes tin and bismuth.
12. A method for generating an RFID tag, in, The method comprises the following steps: - forming an adhesive layer of a predetermined pattern on a substrate made of at least one of a cellulose material and a polymer material, - adding conductive solid particles to the adhesive layer, wherein the conductive solid particles adhere to the adhesive layer, - heating the conductive solid particles by electromagnetic radiation, wherein the wavelength of the electromagnetic spectrum is in the range of 600-1400 nm, so that the temperature of the conductive solid particles exceeds their characteristic melting point, and - pressing the heated conductive solid particles into a nip of the substrate, where the conductive solid particles are flattened, so that the conductive solid particles are electrically connected to each other and thereby form an antenna, and - attaching an integrated circuit to the antenna such that an electrical connection is established between the integrated circuit and the antenna, wherein the antenna and the integrated circuit form the RFID tag, and - at least one additional heating step, in which the conductive solid particles are heated to a temperature below the characteristic melting point, wherein the additional heating step is performed by infrared radiation heating, wherein the wavelength of the IR source is 1500nm and above.
13. The method according to claim 12, in, The integrated circuit is attached to the antenna by bonding and pressing the integrated circuit onto the antenna.
14. The method according to claim 12, in, The integrated circuit is attached by soldering.
15. The method according to claim 12, in, The wavelengths of the electromagnetic spectrum are in the range of 700-1200nm.