Ceramic panel for making refrigerator door, refrigerator door and manufacturing method
By adding reinforcement fibers to the ceramic stone panel of the refrigerator door and forming a layer of touch and pattern, the problem of insufficient strength of the stone parts is solved, and the service life and aesthetic effect of the refrigerator door are improved.
Patent Information
- Application Number
- CN202210843791.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-07-18
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2042-07-18
AI Technical Summary
Due to insufficient strength and hardness, the stone parts of existing refrigerator doors are prone to cracking and falling off, and cannot meet the requirements of home appliances.
The substrate layer is made of ceramic stone and reinforced fibers, and then coated with ink layer on one side, forming a touch-sensitive layer and pattern layer, increasing the strength and gloss effect of the ceramic panel while on the uncoated ink layer Add protective layer on one side to prevent damage.
It improves the strength and hardness of the ceramic panel, solves the problems of cracking and falling off stone parts during use, extends the service life of refrigerator doors, and improves its tactile and gloss effect.
Smart Images

Figure CN115127287B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of household electrical appliances, and in particular to a ceramic panel for making a refrigerator door, a refrigerator door and a manufacturing method thereof. Background Art
[0002] With the improvement of people's living standards, refrigerators have entered thousands of households and become a necessity in people's daily lives. As a container that can keep food or other items in a constant low-temperature state, refrigerators have become one of the indispensable household appliances in modern families.
[0003] At present, the door panels commonly used in the home appliance industry are steel plates and glass. However, both steel plates and glass have certain limitations due to their own material properties. Steel plates have poor corrosion resistance and poor plasticity. After being subjected to destructive forces exceeding their yield strength, they cannot recover to normal use. Glass has an amorphous structure, which has limitations on its shaping and surface touch.
[0004] With the deepening of the stone industry, compared with steel plates and glass, the material has a soft touch and high-end visual effects, so it is loved by consumers. However, the strength of stone itself is not high, so multiple processes are required to process the stone to ensure its strength, which leads to many processes and complicated processes when making stone parts. In addition, for the home appliance industry, stone parts will crack and fall off during use due to insufficient strength and hardness. The impact strength and hardness of stone still do not meet the requirements of home appliance products. Summary of the invention
[0005] In order to solve the problems of stone cracking and falling off due to insufficient strength and hardness of stone parts in the home appliance industry during use, in the first aspect, the present application provides a ceramic panel, including: a substrate layer, the substrate layer is made of ceramic stone and reinforcing fiber; one side of the substrate layer is installed with the refrigerator door; the other side is covered by a touch layer and a pattern layer in sequence; wherein the preparation method of the touch layer and the pattern layer is:
[0006] Applying an ink layer on one side of the substrate layer;
[0007] The substrate layer coated with the ink layer is fired to obtain a tactile layer and a pattern layer after the ink layer is separated; wherein the tactile layer is formed by the portion where the ink layer and the substrate layer are in direct contact, and the pattern layer is a solid layer formed by the remaining ink in the ink layer, wherein the firing temperature is 800°C-1200°C, and the firing time is between 10 seconds and 30 seconds.
[0008] Optionally, the ceramic stone is made of one or more of kaolinite, silicon carbonate, albite, calcium carbonate, and clay;
[0009] The reinforcing fiber is one or more of aluminum sulfate fiber, glass fiber, non-woven fiber or plant fiber;
[0010] The ink used to make the pattern layer is one or more of water-based paint, real stone paint, sand wall paint, and fluorocarbon paint.
[0011] Optionally, the ceramic panel further comprises a protective layer covering a side of the substrate layer not coated with the ink layer; the protective layer is any one of a non-metallic protective layer, a metal protective layer or a chemical protective layer.
[0012] Optionally, the content ratio of the ceramic stone to the reinforcing fiber in the substrate layer is in a range of 10:1 to 50:1.
[0013] In a second aspect, the present application provides a refrigerator door, comprising: the ceramic panel according to any one of the first aspects, a refrigerator door lining and a refrigerator door frame;
[0014] Wherein, one side of the refrigerator door frame is spliced and installed with the refrigerator door lining, a gap is formed between the refrigerator door lining and the refrigerator door frame, and the gap is filled with an elastic filler;
[0015] The ceramic panel is fitted and installed on the other side of the refrigerator door frame.
[0016] In a third aspect, the present application provides a method for manufacturing a refrigerator door, the method comprising:
[0017] The ceramic stone and the reinforcing fiber are crushed to obtain ceramic powder; the ratio of the ceramic stone to the reinforcing fiber is in a range of 10:1 to 50:1;
[0018] The ceramic powder is subjected to stamping treatment to obtain a base material layer for making a ceramic panel;
[0019] Coating an ink layer on one side of the substrate layer;
[0020] The substrate layer coated with the ink layer is fired to obtain the ceramic panel, wherein the ceramic panel includes a touch layer and a pattern layer separated from the ink layer; wherein the touch layer is formed by the portion where the ink layer is in direct contact with the substrate layer, and the pattern layer is a solid layer formed by the remaining ink in the ink layer; wherein the firing temperature is 800° C.-1200° C., and the firing time is between 10 seconds and 30 seconds;
[0021] The ceramic panel is assembled with a refrigerator door component to obtain a refrigerator door; the refrigerator door component includes a refrigerator door lining and a refrigerator door frame.
[0022] Optionally, after the step of crushing the ceramic stone and the reinforcing fiber to obtain ceramic powder, the method further comprises:
[0023] Analyzing the metal element content in the ceramic stone;
[0024] According to the content of the metal element, a corresponding densifying additive is added to the ceramic powder.
[0025] Optionally, the step of stamping the ceramic powder further includes:
[0026] Punching the ceramic powder to obtain a blank for processing the substrate layer;
[0027] The blank is cut according to a preset size, and the cut blank is subjected to edge grinding, cleaning and surface frosting in sequence to obtain the substrate layer.
[0028] Optionally, after the step of firing the substrate layer coated with the ink layer to obtain the ceramic panel, the method further includes: depositing a protective layer on the side of the substrate layer not coated with the ink layer; the protective layer is any one of a non-metallic protective layer, a metal protective layer or a chemical protective layer.
[0029] Optionally, the step of assembling the ceramic panel with a refrigerator door component to obtain a refrigerator door includes:
[0030] Splicing one side of the refrigerator door frame with the refrigerator door lining, forming a gap between the refrigerator door lining and the refrigerator door frame, and filling the gap with an elastic filler;
[0031] The ceramic panel is fitted and installed on the other side of the refrigerator door frame.
[0032] It can be seen from the above scheme that the present application provides a ceramic panel for making a refrigerator door, a refrigerator door and a manufacturing method. By coating a layer of ink on one side of a substrate layer made of ceramic stone and reinforcing fiber, and firing it for a predetermined time under a certain temperature environment, the portion of the ink layer that is in direct contact with the substrate layer forms a tactile layer attached to the substrate layer, thereby improving the tactile effect of the ceramic panel. The remaining ink in the ink layer forms a pattern layer to improve the gloss effect of the ceramic panel. The present application improves the strength of the ceramic panel by adding reinforcing fibers to the ceramic stone, thereby solving the problems of stone cracking and falling off due to insufficient strength and hardness of components made of stone in the home appliance industry during use, thereby improving the strength and hardness of components made of stone. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] In order to more clearly illustrate the technical solution of the present application, the drawings required for use in the embodiments are briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without any creative work.
[0034] Figure 1 A schematic diagram of the structure of a ceramic panel provided for this application;
[0035] Figure 2 A schematic diagram of the structure of a refrigerator door provided in this application;
[0036] Figure 3 A flowchart of a refrigerator door manufacturing method provided in this application.
[0037] Illustration: Ceramic panel-1, refrigerator door lining-2, refrigerator door frame-3, pattern layer-11, touch layer-12, base material layer-13, protective layer-14. DETAILED DESCRIPTION
[0038] In order to enable those skilled in the art to better understand the technical solutions in the present application, the technical solutions in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without creative work should fall within the scope of protection of the present application.
[0039] At present, the door panels commonly used in the home appliance industry are steel plates and glass. However, both steel plates and glass have certain limitations due to their own material properties. Steel plates have poor corrosion resistance and poor plasticity. After being subjected to destructive forces exceeding their yield strength, they cannot be restored to normal use. Glass has an amorphous structure, which has limitations on its shaping and surface touch. With the deepening of the stone industry, its material has a soft touch and high-end visual effects compared with steel plates and glass, so it is loved by consumers. However, the strength of stone itself is not high at present, so multiple processes are required to process the stone to ensure its strength, which leads to many processes and cumbersome processes when making stone parts. In addition, for the home appliance industry, stone parts will also crack and fall off due to insufficient strength and hardness during use. The impact strength and hardness of stone still do not meet the use of home appliance products.
[0040] In order to solve the problems of stone cracking and falling off caused by insufficient strength and hardness in the process of using stone parts in the home appliance industry, firstly, see Figure 1The present application provides a ceramic panel, including a substrate layer 13, wherein the substrate layer 13 is made of ceramic stone and reinforcing fiber. The substrate layer 13 is the main structure of the ceramic panel 1, and the subsequent process steps for preparing the ceramic panel 1 are all based on further processing on the substrate layer 13.
[0041] In some embodiments, the ratio of the content of ceramic stone and reinforcing fiber used in preparing the substrate layer 13 ranges from 10:1 to 50:1. Ceramic stone is the main material for preparing the substrate layer 13, and the ceramic stone is made of one or more of kaolinite, silicon carbonate, sodium feldspar, calcium carbonate, and clay. The purpose of adding reinforcing fiber to the ceramic stone is to improve the strength of the prepared substrate layer 13 by reinforcing the physical properties of high temperature resistance, friction resistance, heat conduction and corrosion resistance, so that the substrate layer 13 can have a strength that meets the requirements of household appliances. The reinforcing fiber is one or more of aluminum sulfate fiber, glass fiber, non-woven fiber or plant fiber.
[0042] The greater the proportion of reinforcing fibers in the material of the prepared substrate layer 13, the higher the strength of the prepared substrate layer 13. However, in the home appliance industry, the substrate layer 1 will be too strong, so that the prepared ceramic panel 1 cannot be adapted to most home appliances. Therefore, the optimum ratio range of the ceramic stone material and reinforcing fibers used to prepare the substrate layer 13 is between 10:1 and 50:1.
[0043] One side of the base material layer 13 is installed with the refrigerator door; the other side is covered by the touch layer 12 and the pattern layer 11 in sequence; the touch layer 12 is directly covered on the base material layer 13, which can improve the touch effect of the ceramic panel 1, and the pattern layer 11 is covered on the touch layer 12, which further improves the gloss effect of the surface of the ceramic panel 1.
[0044] Wherein, the preparation method of the touch layer 12 and the pattern layer 11 is:
[0045] First, a layer of ink is coated on one side of the substrate layer 13; the ink in the ink layer is one or more of water-based paint, real stone paint, sand wall paint, and fluorocarbon paint.
[0046] Secondly, the substrate layer 13 coated with the ink layer is fired, wherein the firing temperature is 800°C-1200°C, and the firing time is between 10 seconds and 30 seconds, to obtain the tactile layer 12 and the pattern layer 11 after the ink layer is separated; wherein the tactile layer 12 is formed by the portion where the ink layer is in direct contact with the substrate layer 13, and the pattern layer 11 is a solid layer formed by the remaining ink in the ink layer, and the raw material of the pattern layer 11 is the ink in the coated ink layer.
[0047] During the firing process, the ink layer portion in direct contact with the substrate layer 13 will be converted into the touch layer 12 under the action of high temperature, and the remaining ink that has not been converted into the touch layer 12 will slowly dry in a natural state to form the pattern layer 11 and adhere to the touch layer 12. The touch layer 12 and the pattern layer 11 can simultaneously protect the side of the substrate layer 13 coated with the ink layer, preventing the substrate layer 13 from being directly exposed to the air and oxidized by the oxygen in the air, causing the ceramic panel 1 to change color or reduce strength. In addition, the touch layer 12 and the pattern layer 11 can further protect the substrate layer 13 from being left with scratches and other marks by external collisions, which affects the beauty of the ceramic panel 1.
[0048] In some embodiments, Figure 1 , the ceramic panel 1 also includes a protective layer 14 covering the side of the substrate layer 13 that is not coated with the ink layer; the protective layer 14 is any one of a non-metallic protective layer, a metal protective layer or a chemical protective layer. The protective layer 14 can further protect the other side of the substrate layer 13 (the side that is not coated with the ink layer). Prevent the other side of the substrate layer 13 from being scratched, impacted, and leaving scratches and scrapes when installed on the refrigerator door. When recycling the ceramic panel 1 on the discarded refrigerator door, the recycling personnel can directly peel the ceramic panel 1 from the refrigerator door from the substrate layer 13 and the protective layer 14 to ensure the integrity of the substrate layer 13 for subsequent secondary use.
[0049] Second, see Figure 2 , Figure 2 A schematic structural diagram of a refrigerator door provided in this application.
[0050] like Figure 2 As shown, the present application provides a refrigerator door, comprising: a ceramic panel 1 as described in any one of the first aspects, a refrigerator door lining 2 and a refrigerator door frame 3.
[0051] Among them, one side of the refrigerator door frame 3 is spliced and installed with the refrigerator door lining 2 to form the frame of the refrigerator door, and after the refrigerator door frame 3 and the refrigerator door lining 2 are installed, the upper end and the lower end of the refrigerator door frame 3 and the refrigerator door lining 2 need to be fixed respectively. The fixing method can be strong glue bonding, bolt connection or welding, etc. This embodiment does not specifically limit the fixing method of the refrigerator door frame 3 and the refrigerator door lining 2.
[0052] A gap is formed between the refrigerator door lining 2 and the refrigerator door frame 3, and the gap is filled with an elastic filler; the elastic filler may be polyurethane foam plastic, glass wool or a filler made of plastic, etc. On the one hand, the elastic filler can prevent the hot air outside the refrigerator from entering the refrigerator and affecting the refrigeration environment inside the refrigerator. On the other hand, the elastic filler can buffer the refrigerator door when the user closes the refrigerator door, thereby reducing the damage to the refrigerator door caused by the user applying too much force when closing the refrigerator door.
[0053] The ceramic panel 1 is mounted on the other side of the refrigerator door frame 3 .
[0054] Thirdly, see Figure 3 , Figure 3 A flowchart of a refrigerator door manufacturing method provided in this application.
[0055] like Figure 3 As shown, the present application provides a method for manufacturing a refrigerator door, the method comprising:
[0056] S100: Crush the ceramic stone and the reinforcing fiber to obtain ceramic powder; the ceramic stone is made of one or more of kaolinite, silicon carbonate, albite, calcium carbonate, and clay; the reinforcing fiber is one or more of aluminum sulfate fiber, glass fiber, non-woven fiber or plant fiber; the content ratio of the ceramic stone to the reinforcing fiber is between 10:1 and 50:1. Adding the reinforcing fiber as a reinforcing material to the material of the substrate layer 13 for preparing the ceramic panel 1 can enhance the strength of the substrate layer 13, so that it has a strength that can adapt to the normal use of the refrigerator door, avoid the ceramic panel 1 from cracking, falling off, etc. during use, and improve the service life of the refrigerator door to which the ceramic panel 1 is applied.
[0057] Taking glass fiber as an example, glass fiber is an inorganic non-metallic material with excellent performance, good insulation, strong heat resistance, good corrosion resistance, and high mechanical strength. By making the glass fiber into powder and mixing it with the powder made of ceramic stone, the strength and toughness of the substrate layer 13 can be improved by the properties of the glass fiber such as good corrosion resistance and high mechanical strength.
[0058] In some embodiments, the density of the substrate layer 13 may be increased by adding some densifying additives to the ceramic powder. Therefore, after step S100, the method further includes:
[0059] Analyzing the metal element content in the ceramic stone;
[0060] Generally, the main elements of ceramics are silicon, aluminum, and oxygen, and clay is the main raw material. Before firing, some dense additives can be added to the ceramic powder to prevent the grains inside the substrate layer 13 from becoming coarse during firing, thereby causing pores to form inside the substrate layer 13 and reducing the strength of the substrate layer 13. Taking kaolinite as an example, the chemical composition of kaolinite is Al4[Si4O 10 ]·(OH)8. Its main elements are aluminum and silicon.
[0061] According to the content of the metal element, a corresponding densifying additive is added to the ceramic powder.
[0062] In the above embodiment, when aluminum and silicon are used as metal elements, after kaolinite is made into powder, a trace amount of magnesium oxide or zirconium oxide powder can be added to improve the density of the manufactured substrate layer 13 .
[0063] S200: stamping the ceramic powder to obtain the substrate layer 13 for making the ceramic panel 1; in step 200, in order to improve the compactness of the substrate layer 13, a larger tonnage press is required to stamp the ceramic powder. The tonnage of the press usually used is 15,000 tons to 35,000 tons.
[0064] In some embodiments, step S200 may also be evolved into:
[0065] S201: stamping the ceramic powder to obtain a blank for processing the substrate layer 13.
[0066] S202: cutting the blank into a preset size, and sequentially performing edge grinding, cleaning and surface frosting on the cut blank to obtain the substrate layer 13.
[0067] In this embodiment, after the stamping process, a whole blank for preparing the substrate layer 13 is obtained. After obtaining the blank, first, the blank needs to be cut according to the size of the substrate layer 13, wherein the size of the substrate layer 13 is determined according to the specific size of the refrigerator door. For refrigerator doors with some special door bodies, such as double-door refrigerators, three-door refrigerators or side-by-side refrigerators, it is also necessary to cut multiple substrate layers 13 of different sizes.
[0068] Secondly, the edges of the substrate layer 13 are polished to remove the burrs generated during the cutting process to prevent the burrs from scratching the preparation personnel during the handling process. Finally, the polished blank is cleaned and the surface is frosted to obtain the substrate layer 13. The cleaning and surface frosting can make the substrate layer 13 smoother and improve the visual texture of the substrate layer 13.
[0069] S300: coating a layer of ink on one side of the substrate layer 13; the ink used to make the ink layer may be one or more of water-based paint, real stone paint, sand wall paint, and fluorocarbon paint. In the home appliance industry, the ink layer is also required to have a certain conductivity, so the ink used to make the ink layer may also be conductive ink.
[0070] S400: The substrate layer 13 coated with the ink layer is fired to obtain the ceramic panel 1, wherein the ceramic panel 1 includes a tactile layer 12 and a pattern layer 11 after the ink layer is separated; wherein the tactile layer 12 is formed by the portion where the ink layer is in direct contact with the substrate layer 13, and the pattern layer 11 is a solid layer formed by the remaining ink in the ink layer; wherein the firing temperature is 800°C-1200°C, and the firing time is between 10 seconds and 30 seconds.
[0071] During the firing process, since the heat absorbed by the solid is higher than that absorbed by the liquid, the heat absorbed by the substrate layer 13 can be further released to the ink layer. Therefore, the part of the ink layer directly contacted by the substrate layer 13 will form the touch layer 12 under the combined effect of the high temperature of the firing heating and the high temperature of the substrate layer 13. After firing for 10 to 30 seconds, the remaining ink in the ink layer will slowly dry by the residual heat of the firing to form the pattern layer 11, and the prepared ceramic panel 1 is obtained.
[0072] In some embodiments, in order to prevent the refrigerator door component from colliding with the ceramic panel 1 and thus damaging the ceramic panel 1 during the installation of the ceramic panel 1, after step S400, the method further includes: depositing a protective layer 14 on the side of the substrate layer 13 that is not coated with the ink layer; the protective layer 14 is any one of a non-metallic protective layer, a metal protective layer or a chemical protective layer. Among them, the non-metallic protective layer can be an organic mixture and an inorganic mixture, such as plastic, paint, rubber, asphalt, enamel, enamel, acid-resistant material, rust-proof oil, etc. The metal protective layer can use a metal or alloy with stable chemical properties as the protective layer 14 in the form of a coating. The metal protective layer is usually coated with a metal protective film, wherein the metal includes zinc, tin, tin, nickel, chromium, copper, cadmium, lead, gold, silver, palladium, rhodium, etc. and alloys. The chemical protective layer is formed by an electrochemical or chemical method on the side of the substrate layer 13 that is not coated with the ink layer.
[0073] S500: Assembling the ceramic panel 1 with a refrigerator door component to obtain a refrigerator door; the refrigerator door component includes a refrigerator door lining 2 and a refrigerator door frame 3.
[0074] In step S500, the ceramic panel 1 is assembled with the refrigerator door lining 2 and the refrigerator door frame 3 according to the structure of the refrigerator door described in the second aspect.
[0075] The specific operation is to splice one side of the refrigerator door frame 3 with the refrigerator door lining 2, and a gap is formed between the refrigerator door lining 2 and the refrigerator door frame 3, and the gap is filled with an elastic filler.
[0076] During the installation process, the installed refrigerator door lining 2 needs to be fixed to the refrigerator door frame 3 first, and usually the upper and lower ends of the refrigerator door frame 3 and the refrigerator door lining 2 need to be fixed respectively. The fixing method can be super glue bonding, bolt connection or welding, etc. This embodiment does not specifically limit the fixing method of the refrigerator door frame 3 and the refrigerator door lining 2.
[0077] The refrigerator door can be obtained by fitting the ceramic panel 1 to the other side of the refrigerator door frame 3. The ceramic panel 1 is installed on the outer side of the door body of the refrigerator door. When the user uses the refrigerator door, the ceramic panel 1 will not crack or fall off due to insufficient strength and hardness of the ceramic panel 1, thereby improving the application strength and service life of the refrigerator door.
[0078] It can be seen from the above scheme that the present application provides a ceramic panel for making a refrigerator door, a refrigerator door and a manufacturing method. By coating a layer of ink on one side of a substrate layer 13 made of ceramic stone and reinforcing fiber, and firing it for a predetermined time under a certain temperature environment, the portion of the ink layer that is in direct contact with the substrate layer 13 forms a tactile layer 12 attached to the substrate layer 13, thereby improving the tactile effect of the ceramic panel 1. The remaining ink in the ink layer forms a pattern layer 11, thereby improving the gloss effect of the ceramic panel 1. The present application improves the strength of the ceramic panel 1 by adding reinforcing fibers to the ceramic stone 1, thereby solving the problems of cracking and falling off of stone due to insufficient strength and hardness of components made of stone in the home appliance industry during use, thereby improving the strength and hardness of components made of stone.
[0079] For the convenience of explanation, the above description has been made in conjunction with specific embodiments. However, the above exemplary discussion is not intended to be exhaustive or limit the embodiments to the specific forms disclosed above. Based on the above teachings, various modifications and variations can be obtained. The selection and description of the above embodiments are to better explain the principles and practical applications, so that those skilled in the art can better use the embodiments and various different variations of the embodiments suitable for specific use considerations.
Claims
1. A ceramic panel, characterized in that: include: A substrate layer (13), wherein the substrate layer (13) is made of ceramic stone and reinforcing fibers; one side of the substrate layer (13) is covered by the touch layer (12) and the pattern layer (11) in sequence, and the other side is mounted on the refrigerator door; the ceramic stone is made of one or more of kaolinite, silicon carbonate, sodium feldspar, calcium carbonate, and clay; the reinforcing fibers are one or more of aluminum sulfate fibers, glass fibers, non-woven fibers, or plant fibers; the ink used to make the pattern layer (11) is one or more of water-based paint, real stone paint, sand wall paint, and fluorocarbon paint; The method for preparing the ceramic panel comprises: The ceramic stone and the reinforcing fiber are crushed to obtain ceramic powder; the ratio of the ceramic stone to the reinforcing fiber is in a range of 10:1 to 50:1; Performing a stamping process on the ceramic powder to obtain the substrate layer (13); Coating an ink layer on one side of the substrate layer (13); The substrate layer (13) coated with the ink layer is fired to obtain a tactile layer (12) and a pattern layer (11) after the ink layer is separated; wherein the tactile layer (12) is formed by the portion of the ink layer directly contacting the substrate layer (13), and the pattern layer (11) is a solid layer formed by the remaining ink in the ink layer, wherein the firing temperature is 800° C.-1200° C., and the firing time is between 10 seconds and 30 seconds; and the pattern layer (11) is formed by drying the remaining ink in the ink layer through residual heat from firing.
2. The ceramic panel according to claim 1, characterized in that: It also includes a protective layer (14) covering a side of the substrate layer (13) that is not coated with the ink layer; the protective layer (14) is a non-metallic protective layer, a metallic protective layer, or a chemical protective layer.
3. A refrigerator door, characterized in that: include: The ceramic panel (1), refrigerator door lining (2) and refrigerator door frame (3) according to any one of claims 1 to 2; Wherein, one side of the refrigerator door frame (3) is spliced and installed with the refrigerator door lining (2), a gap is formed between the refrigerator door lining (2) and the refrigerator door frame (3), and the gap is filled with an elastic filler; The ceramic panel (1) is fitted and mounted on the other side of the refrigerator door frame (3).
4. A method for manufacturing a refrigerator door, characterized in that: The method comprises: The ceramic stone and the reinforcing fiber are crushed to obtain ceramic powder; the ratio of the ceramic stone to the reinforcing fiber is in a range of 10:1 to 50:1; Performing a stamping process on the ceramic powder to obtain a base material layer (13) for making a ceramic panel (1); Coating an ink layer on one side of the substrate layer (13); The base material layer (13) coated with the ink layer is subjected to a firing treatment to obtain the ceramic panel (1), wherein the ceramic panel (1) comprises a touch layer (12) and a pattern layer (11) separated from the ink layer; wherein the touch layer (12) is formed by the portion of the ink layer directly contacting the base material layer (13), and the pattern layer (11) is a solid layer formed by the remaining ink in the ink layer; wherein the firing temperature is 800° C. to 1200° C., and the firing time is between 10 seconds and 30 seconds; and the pattern layer (11) is formed by drying the remaining ink in the ink layer by residual heat from firing; The ceramic panel (1) is assembled with a refrigerator door component to obtain a refrigerator door; the refrigerator door component comprises a refrigerator door lining (2) and a refrigerator door frame (3).
5. The method for manufacturing a refrigerator door according to claim 4, characterized in that: After the step of crushing the ceramic stone and the reinforcing fiber to obtain ceramic powder, the method further comprises: Analyzing the metal element content in the ceramic stone; According to the content of the metal element, a corresponding densifying additive is added to the ceramic powder.
6. The method for manufacturing a refrigerator door according to claim 4, characterized in that: The step of stamping the ceramic powder further includes: Performing a stamping process on the ceramic powder to obtain a blank for processing the substrate layer (13); The blank is cut into a preset size, and the cut blank is subjected to edge grinding, cleaning and surface frosting in sequence to obtain the substrate layer (13).
7. The method for manufacturing a refrigerator door according to claim 4, characterized in that: After the step of firing the base material layer (13) coated with the ink layer to obtain the ceramic panel (1), the method further comprises: depositing a protective layer (14) on the side of the base material layer (13) not coated with the ink layer; the protective layer (14) is a non-metallic protective layer, a metallic protective layer or a chemical protective layer.
8. The method for manufacturing a refrigerator door according to claim 4, characterized in that: The steps of assembling the ceramic panel (1) with the refrigerator door component to obtain the refrigerator door include: One side of the refrigerator door frame (3) is spliced with the refrigerator door lining (2), so that a gap is formed between the refrigerator door lining (2) and the refrigerator door frame (3), and the gap is filled with an elastic filler; The ceramic panel (1) is fitted onto the other side of the refrigerator door frame (3).