Additive manufacturing system and additive manufacturing method

Through the additive manufacturing system, the fiber preform is guided and pretreated on the substrate, heat-cured resin is applied and localized heating is performed, and combined with pressure curing, the complexity and cost of traditional composite materials are solved, achieving efficient and rapid Composite material formation.

CN115139520BActive Publication Date: 2024-11-12CARBONFORM INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110334786.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-03-29
Publication Date
2024-11-12
Estimated Expiration
2041-03-29

AI Technical Summary

Technical Problem

Traditional composite materials are complex and expensive to manufacture, making it difficult to meet the processing needs of high-precision, high-complexity and special-shaped components, especially in aerospace, automobiles and other fields.

Method used

Using an additive manufacturing system, a first material is provided on the substrate through a guide device, a second material is applied after pretreatment, and a heating device is used to achieve local heating to form a composite material, and a movable module and a pressure curing device are used to achieve rapid curing.

Benefits of technology

The curing speed and curing degree of printing materials are improved, the target shape formation process of composite materials is simplified, the development cycle and cost are reduced, and the printing efficiency is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115139520B_ABST
    Figure CN115139520B_ABST
Patent Text Reader

Abstract

Embodiments of the present disclosure provide an additive manufacturing system and an additive manufacturing method. The additive manufacturing system includes: a guiding device, which guides a first material and sets the first material on a substrate, so that the first material is formed on the substrate to have a target shape; a pretreatment device, which performs surface pretreatment on the first material; an application device, which is configured to apply a second material to the surface of the first material that has been surface pretreated; and a heating device, which locally heats the first material to solidify the second material to form a composite material of the first material and the second material. The additive manufacturing system and the additive manufacturing method do not need to set up additional steps to make the composite material have a target shape, and can apply the second material on the surface of the first material that has a target shape and has been surface activated and additionally functionalized. The composite material is directly formed to have a target shape, thereby improving printing efficiency and achieving rapid additive manufacturing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] Embodiments of the present invention relate to an additive manufacturing system and an additive manufacturing method. Background Art

[0002] With the rapid development of industry and manufacturing, traditional manufacturing processing technology can no longer meet the processing requirements of many high-precision, high-complexity, and special-shaped parts. Under the impetus of various high-demand and high-standard processing needs, a new rapid prototyping method has emerged: three-dimensional (3D) printing, also known as additive manufacturing. With its many advantages, 3D printing technology has become one of the most popular and vital technologies in the new manufacturing field. Unlike ordinary printers that can only move in two dimensions, the basic principle of 3D printing is to control the machine to stack the printing materials layer by layer to produce three-dimensional objects. This manufacturing method not only shortens the development cycle but also reduces the R&D cost when producing complex parts.

[0003] Continuous fiber reinforced composite materials have the advantages of low density and high strength. They are widely used engineering structural materials, specifically in aerospace, automobiles, ships, oceans, petroleum, construction, medical treatment, high-performance sports goods, consumer electronics, etc. However, the traditional composite material manufacturing process is complex and costly. The use of 3D printing to produce continuous carbon fiber reinforced composite materials can achieve more flexible designs and help save resources and time, which has attracted widespread attention. Summary of the invention

[0004] In a first aspect, an embodiment of the present disclosure provides an additive manufacturing system, comprising: a guiding device, guiding a first material and arranging the first material on a substrate so that the first material is formed on the substrate to have a target shape; a pretreatment device, performing surface pretreatment on the first material; an applying device, configured to apply a second material to the surface of the first material that has been surface pretreated; and a heating device, locally heating the first material to solidify the second material to form a composite material of the first material and the second material.

[0005] For example, the additive manufacturing system also includes: a movable module, which is configured to move according to the target shape, the guiding device, the pretreatment device, the applying device and the heating device are accommodated in the movable module and move along with the movement of the movable module, and the guiding device guides the first material while the movable module moves.

[0006] For example, the movable module further includes: a pressure curing device configured to apply pressure and provide heat to the composite material to fix the composite material to the substrate, and the movable module moves in a direction away from the fixed composite material.

[0007] For example, the additive manufacturing system further includes: a supply device configured to provide the first material with controllable tension to the movable module; and a storage device configured to store the first material and provide the first material to the supply device.

[0008] For example, the first material is a fiber preform, and the storage device is a roll wound with the fiber preform.

[0009] For example, the additive manufacturing system further includes: a cutting device, which is disposed between the supply device and the guide device, configured to guide the first material to the guide device, and configured to cut off the first material.

[0010] For example, the substrate includes a building table or a composite material of the first material and the second material fixed on the building table in a previous process.

[0011] For example, the additive manufacturing system further includes: a chamber configured to accommodate the movable module and the building platform, and the chamber is also provided with a temperature control device and a pressure control device.

[0012] For example, the application device includes a nozzle and is configured to apply the second material in liquid form to the first material.

[0013] For example, the second material is a thermosetting resin.

[0014] For example, the additive manufacturing system further includes: a driving device configured to drive the movable module to move within the chamber, and the driving device is disposed outside the chamber.

[0015] For example, the moving direction of the movable module is parallel to the fiber direction of the fiber preform, and the applying device, the heating device and the pressure curing device are arranged in sequence along the direction opposite to the moving direction of the movable module and in the fiber direction.

[0016] In a second aspect, an embodiment of the present disclosure further provides an additive manufacturing method, using any additive manufacturing system described in the first aspect, the method comprising: using the guiding device to guide the first material and setting the first material on a substrate according to a target shape; using the pretreatment device to perform surface pretreatment on the first material; using the applying device to apply a second material on the first material; using the heating device to locally heat the first material to solidify the second material to form a composite material of the first material and the second material.

[0017] For example, the additive manufacturing method further includes: processing the composite material so that the composite material is further solidified and fixed on the processing table.

[0018] For example, the additive manufacturing system includes: a movable module configured to move according to the target shape,

[0019] The guiding device, the pretreatment device, the applying device and the heating device are accommodated in the movable module and move along with the movement of the movable module. The additive manufacturing method further includes: while guiding the first material by the guiding device and arranging the first material on the substrate according to the target shape, moving the movable module in a direction away from the fixed composite material.

[0020] For example, the processing of the composite material includes: applying pressure and temperature to the composite material using a pressure curing device, so that the composite material is completely cured and fixed on the processing table.

[0021] For example, the substrate includes a building table or a composite material of the first material and the second material fixed on the building table in a previous process.

[0022] For example, applying the second material on the first material includes: spraying the second material in liquid form on the first material by using a supply device.

[0023] For example, the surface pretreatment of the first material using the pretreatment device includes: performing surface activation and / or additional functionalization treatment on the surface of the first material.

[0024] For example, performing surface activation on the surface of the first material includes: applying an adhesive coating, performing functional group implantation, plasma etching, plasma implantation, ozone cleaning treatment, surface energy activation, or spraying a sizing agent on the surface of the first material.

[0025] For example, performing additional functionalization treatment on the surface of the first material includes: spraying or depositing functional powder or particle material on the surface of the first material.

[0026] For example, the additive manufacturing method further includes: using a supply device to provide the first material with controllable tension to the movable module; using a storage device to store the first material and providing the first material to the supply device through the storage device.

[0027] For example, the first material is a fiber preform, the moving direction of the movable module is parallel to the fiber direction of the fiber preform, and the applying device and the heating device are arranged in sequence along the direction opposite to the moving direction of the movable module and in the fiber direction.

[0028] Embodiments of the present disclosure provide an additive manufacturing system and an additive manufacturing method, wherein the additive manufacturing system includes: a guiding device, which guides a first material and arranges the first material on a substrate so that the first material is formed on the substrate to have a target shape; a pretreatment device, which performs surface pretreatment on the first material; an applying device, which is configured to apply a second material to the surface of the first material that has been surface pretreated; and a heating device, which locally heats the first material to solidify the second material to form a composite material of the first material and the second material. In the additive manufacturing system, the first material is guided to have a target shape on the substrate by the movement of the guiding system, for example, the shape of each stacked layer of the three-dimensional shape to be manufactured in the end, and the first material is further locally heated by using a heating device, and a temperature gradient is formed between the area where the second material is applied and the area of ​​the first material being heated, so that the viscosity of the applied liquid second material decreases from low temperature to high temperature, and the second material flows to the locally heated area due to capillary action, and the higher temperature in the heated area causes the liquid second material to solidify, and forms a composite material with the first material, thereby achieving rapid solidification of the composite material; in this way, since the first material has been set to have a target shape, the second material applied to the first material and solidified forms a composite material with the first material together with the first material, and the final three-dimensional shape is located at the target shape of the layer. By repeating the above printing process, the desired three-dimensional shape is finally formed. Such an additive printing system uses a local heating method, which can improve the curing speed and degree of the printed material, and achieve fast and convenient additive manufacturing. Moreover, before the composite material is solidified, the first material is guided to have a target shape by utilizing the movement of the guide system, so there is no need to set up additional steps to make the composite material have the target shape, thereby improving printing efficiency and realizing rapid additive manufacturing. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings of the embodiments will be briefly introduced below. Obviously, the drawings in the following description only relate to some embodiments of the present invention, but are not intended to limit the present invention.

[0030] Figure 1 is a schematic diagram of an additive manufacturing system according to an embodiment of the present disclosure;

[0031] Figure 2 is another schematic diagram of an additive manufacturing system according to an embodiment of the present disclosure;

[0032] Figure 3 is another schematic diagram of an additive manufacturing system according to an embodiment of the present disclosure; and

[0033] Figure 4 is a schematic flow chart of an additive manufacturing method according to an embodiment of the present disclosure. DETAILED DESCRIPTION

[0034] In order to make the purpose, technical solution and advantages of the embodiment of the present invention clearer, the technical solution of the embodiment of the present invention will be clearly and completely described below in conjunction with the drawings of the embodiment of the present invention. Obviously, the described embodiment is a part of the embodiment of the present invention, not all of the embodiments. Based on the described embodiment of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0035] Unless otherwise defined, the technical terms or scientific terms used herein should be understood by people with ordinary skills in the field to which the present invention belongs. "First", "second" and similar words used in this disclosure do not indicate any order, quantity or importance, but are only used to distinguish different components. Similarly, "one", "one" or "the" and other similar words do not indicate quantity restrictions, but indicate that there is at least one. "Including" or "including" and other similar words mean that the elements or objects appearing in front of the word cover the elements or objects listed after the word and their equivalents, without excluding other elements or objects. "Connect" or "connected" and other similar words are not limited to physical or mechanical connections, but can include electrical connections, whether direct or indirect. "Up", "down", "left", "right" and the like are only used to indicate relative positional relationships. When the absolute position of the described object changes, the relative positional relationship may also change accordingly.

[0036] Embodiments of the present disclosure provide an additive manufacturing system and an additive manufacturing method, wherein the additive manufacturing system includes: a guiding device, which guides a first material and arranges the first material on a substrate so that the first material is formed on the substrate to have a target shape; a pretreatment device, which performs surface pretreatment on the first material; an applying device, which is configured to apply a second material to the surface of the first material that has been surface pretreated; and a heating device, which locally heats the first material to solidify the second material to form a composite material of the first material and the second material. In the additive manufacturing system, the first material is guided to have a target shape on the substrate by the movement of the guiding system, for example, the shape of each stacked layer of the three-dimensional shape to be manufactured in the end, and the first material is further locally heated by using a heating device, and a temperature gradient is formed between the area where the second material is applied and the area of ​​the first material being heated, so that the viscosity of the applied liquid second material decreases from low temperature to high temperature, and the second material flows to the locally heated area due to capillary action, and the higher temperature in the heated area causes the liquid second material to solidify, and forms a composite material with the first material, thereby achieving rapid solidification of the composite material; in this way, since the first material has been set to have a target shape, the second material applied to the first material and solidified forms a composite material with the first material together with the first material, and the final three-dimensional shape is located at the target shape of the layer. By repeating the above printing process, the desired three-dimensional shape is finally formed. Such an additive printing system uses a local heating method, which can improve the curing speed and degree of the printed material, and achieve fast and convenient additive manufacturing. Moreover, before the composite material is solidified, the first material is guided to have a target shape by utilizing the movement of the guide system, so there is no need to set up additional steps to make the composite material have the target shape, thereby improving printing efficiency and realizing rapid additive manufacturing.

[0037] The additive manufacturing system and additive manufacturing direction of the embodiments of the present disclosure will be exemplarily described below in conjunction with the accompanying drawings.

[0038] Figure 1 A schematic diagram of an additive manufacturing system according to an embodiment of the present disclosure is shown. Figure 1 As shown, the additive manufacturing system 1000 includes: a guiding device 15, guiding the first material 101 and arranging the first material on a substrate so that the first material is formed on the substrate to have a target shape; a pretreatment device 11, performing surface pretreatment on the first material; an applying device 12, configured to apply a second material 102 to the surface of the first material that has been surface pretreated; and a heating device 13, locally heating the first material to solidify the second material 102 to form a composite material of the first material and the second material.

[0039] For example, the guiding device may include a guiding roller, and the first material may be arranged on the substrate into a predetermined target shape under the guidance of the guiding roller, and then, the first material and the second material are formed into a composite material having a target shape by applying the second material and curing the second material.

[0040] For example, by using a heating device to locally heat the first material, a temperature gradient is generated between the place where the second material is applied and the heating area of ​​the first material. Under this temperature gradient, since the viscosity of the second material decreases at a higher temperature, the second material will flow to the heating area and solidify there due to the higher temperature, thereby forming a composite material.

[0041] For example, the heating device can provide laser, infrared light, microwave or plasma to the local area of ​​the first material to achieve heating of the local area. For example, the heating device can be a laser emitter, infrared light emitter, microwave emitter or plasma heater.

[0042] For example, the pretreatment device can clean and activate the surface of the first material to improve wettability and interface properties. For example, a binder coating can be applied to the surface of the first material, such as binder spraying, functional groups, such as -COOH, -OH, transplantation, plasma etching, plasma surface grafting, ozone cleaning treatment, surface energy activation, spraying sizing agent, such as spraying silane and urethane, etc.; and / or the surface of the first material can be functionalized, such as applying, such as spraying functional powder or particles on the surface to make it adhere to the surface of the first material. The functional powder or particles can include polymer particles, thermosetting polymer powders and thermoplastic powders, metals (e.g., Al, Fe) and metal oxides (e.g., Al 2 O 3 , Fe 2 O 3 , Fe 3 O 4 ) powders and wires, ceramics (such as SiC, SiO 2 ) powders and wires, nanomaterials (e.g., carbon black, carbon nanotubes, graphene, graphite, boron nitride, Mexene).

[0043] For example, the additive manufacturing system may also include: a movable module 100, which is configured to move according to the target shape, wherein the guiding device 15, the pretreatment device 11, the applying device 12 and the heating device 13 can be accommodated in the movable module 100 and move with the movement of the movable module, and the guiding device guides the first material while the movable module moves, so that the first material 101 is formed on the substrate with a predetermined target shape.

[0044] For example, the movable module 100 may further include: a pressure curing device 14, which is configured to apply pressure and heat to the composite material to fix the composite material to the substrate, wherein the movable module moves in a direction away from the fixed composite material. The pressure curing device 14 may include a pressure applying member, a heating member, and a pressure roller, wherein the pressure roller is pressed against the composite material by the pressure applying member and applies a certain pressure to the composite material, and the pressure roller is heated by the heating member to heat the composite material, so that the layer thickness can be controlled by providing pressure, thereby making the composite material more dense and having a lower porosity, and the curing rate of more than 95% can be achieved by heating.

[0045] For example, Figure 1 As shown, the pressure curing device 14 is on the left side. Under the action of the pressure curing device 14, the composite material of the first material and the second material is completely cured and fixed on the substrate, and the movable module 100 moves in a direction away from the fixed composite material, that is, moves to the right along the direction of arrow A. As the movable module moves to the right, the first material is continuously provided and guided by the guide device to be set on the substrate in a predetermined target shape, and the second material is gradually applied to the first material in a direction from left to right to form a composite material with a target shape. As the movable module continues to move to the right, the first material is continuously supplied to the substrate below the movable module, thereby achieving continuous additive manufacturing.

[0046] For example, by moving the movable module, the guiding device continuously guides the first material, the second material is applied to the second material and is solidified and fixed on the substrate, and this step is continuously repeated, so that a plurality of layers having a target shape are stacked, and finally a three-dimensional object to be printed is obtained.

[0047] For example, in the embodiment of the present disclosure, the substrate can be the building platform 16 or the printed material formed on the building platform 16 in the previous step, that is, the composite material of the fixed first material and the second material. The building platform 16 can be a rigid material platform with a flat surface or a surface with a specific morphology, such as a stainless steel platform; or a plastic material platform with a flat surface or a surface with a specific morphology, such as a silicone platform, etc. The building platform can also be provided with a heating system to heat the three-dimensional printing material located thereon.

[0048] For example, Figure 3 As shown, build table 16 may be supported by support columns 161 .

[0049] For example, the additive manufacturing system 1000 may further include: a supply device 18, configured to provide the first material 101 with controllable tension to the movable module 100; and a storage device 19, configured to store the first material and provide the first material to the supply device.

[0050] For example, the supply device includes a tensioning system to draw the first material out of the storage device and control the tension of the first material according to the type of the first material, for example Figure 2 As shown, the tensioning system may include guide roller sets 181 and 182, and a tension control device 183.

[0051] Alternatively, the supply device and the storage device may be disposed inside or outside the movable module, and the embodiments of the present disclosure are not limited thereto.

[0052] For example, the first material may be a fiber preform, and the storage device may be a roll wound with the fiber preform.

[0053] For example, the fiber preform can be carbon fiber, aramid fiber, glass fiber, natural fiber, steel fiber, silver fiber, copper fiber or multi-component fiber, and any combination thereof. The fiber preform can be in the form of fiber bundle (untwisted), yarn (twisted), woven, non-woven, braided, knitted, two-dimensional and three-dimensional fabrics, pre-impregnated fabrics, thermoplastic or thermosetting coated fibers or fabrics or mixed yarns and fabrics.

[0054] For example, the application device 12 may be a spraying member with a nozzle or a coating member on which the second material is coated. The second material may be in a liquid state, so that it can be sprayed onto the first material through a nozzle, or the second material may be in a viscous state, so that it can be spin-coated onto the first material through a coating member, such as a coating roller. The embodiments of the present disclosure are not limited to this, as long as the second material can be applied to the surface of the first material.

[0055] For example, the second material can be a resin, for example, a thermosetting resin, for example, polyester, epoxy, phenolic, vinyl ester, thermosetting polyurethane, silicone resin, polyimide, polybismaleimide, polycarbosilane, etc., a UV curable resin, for example, acrylic epoxy resin, acrylic polyester, acrylic polyurethane, etc. Stabilizers can also be added to the resin, mainly including: UV absorbers, antioxidants, quenchers, lubricants, plasticizers, flame retardants, for example, lubricants can include fatty alcohols, acids and esters or hydrocarbons, plasticizers can include phthalates, adipic acid esters or polychlorinated hydrocarbons, and flame retardants can include halogenated, non-halogenated, etc.

[0056] For example, the additive manufacturing system may further include: a cutting device 17, which is disposed between the supply device and the guide device, and is configured to guide the first material to the guide device, and cut the first material when it is necessary to cut the first material. The cutting device may be a fiber preform cutting machine, such as a laser cutting machine or a mechanical scissors.

[0057] Alternatively, the cutting device may be disposed inside or outside the movable module. If disposed inside the movable module, the cutting device may move with the movable module, thereby facilitating cutting of the first material, better controlling the shape of the 3D printed object, and improving the 3D printing accuracy.

[0058] For example, a guide roller 20 may be further provided between the cutting device and the supply device to guide the first material to the cutting device.

[0059] Alternatively, the guide roller may be located inside or outside the movable module, which is not limited in the embodiments of the present disclosure.

[0060] For example, the additive manufacturing system according to the embodiment of the present disclosure may further include: a chamber 200 configured to accommodate the movable module 100 and the building platform 16, and the chamber is also provided with a temperature control device and a pressure control device.

[0061] For example, the additive manufacturing system according to the embodiment of the present disclosure may further include: a driving device, configured to drive the movable module to move within the chamber, and the driving device is disposed outside the chamber.

[0062] For example, the driving device may be a robotic arm control system, which is fixedly connected to the movable module through a manipulator to control the movement of the movable module. The robotic arm control system may be a six-axis control system, that is, the robotic arm may be a six-axis robotic arm, so that three-dimensional objects of complex shapes can be printed, thereby improving printing applicability. Alternatively, the robotic arm control system may also be an elevated XYZ frame, so that the movable module can be controlled to move in three directions: X, Y, and Z.

[0063] Alternatively, the supply device and the storage device can be arranged inside the chamber or outside the chamber. Arranging them outside the chamber can save space, provide more moving space for the movable module, and improve the three-dimensional printing accuracy, but the embodiments of the present disclosure are not limited to this.

[0064] For example, when the first material is a fiber preform, the moving direction of the movable module is parallel to the fiber direction of the fiber preform, and the applying device, the heating device and the pressure curing device are arranged in sequence along the direction opposite to the moving direction of the movable module and in the fiber direction. Figure 2 The movable module moves in the direction of arrow A, which is parallel to the fiber direction, and the setting directions of the applying device 12, the heating device 13 and the pressure curing device 14 are also parallel to the fiber direction and are sequentially arranged in the movable module in the direction opposite to the moving direction of the movable module.

[0065] It should be noted here that the accompanying drawings show the phase positions of the applying device 12, the heating device 13 and the pressure curing device 14, the cutting device, and the supply device. However, the applying device 12, the heating device 13 and the pressure curing device 14 only need to be arranged in parallel to the fiber direction, and the phase positions of the three can also be appropriately adjusted in the movable module. For the cutting device, it only needs to be set in the direction of supply of the first material. For the supply device, it can be set in the movable module or in the chamber. For the convenience of implementation, technicians in this field can set it as needed, and the embodiments of the present disclosure are not limited to this.

[0066] The additive manufacturing system of the embodiment of the present disclosure locally heats the first material, for example, the fiber preform, by a heating device, and forms a temperature gradient distribution along the fiber direction, so that the second material, for example, the liquid thermosetting resin, has a reduced viscosity from the low temperature to the high temperature area on the fiber, and the reduced viscosity causes it to flow into the adjacent fibers due to the capillary force, and the higher temperature causes the liquid resin to solidify, thereby achieving rapid and synchronous infusion and solidification, and the composite material can be solidified into any three-dimensional shape. This local heating method can achieve a faster solidification speed and a higher degree of solidification of the printed material. The second material, for example, the liquid resin, can even overcome gravity under the capillary action and move vertically upward between the fibers. The composite material is densified due to the capillary action of the liquid resin between the fibers, thereby achieving a higher fiber volume fraction, which helps to improve the material performance. Moreover, before the composite material is solidified, the first material is guided to have a target shape by utilizing the movement of the guide system, so that no additional steps are required to make the composite material have a target shape, thereby improving the printing efficiency and achieving rapid additive manufacturing. Furthermore, by using a pressure curing device, it is possible to heat while applying pressure, making the composite material denser and having a lower porosity, and making the composite material reach a curing rate of more than 95%. Furthermore, by setting a pretreatment device, the surface of the first material can be activated and / or additionally functionalized before the second material is applied, so that the second material is easier to combine with the first material, and the two form a more stable composite material, and additional functionalization of the first material can make the three-dimensional printing material more stable and the product performance better.

[0067] The embodiments of the present disclosure also provide an additive manufacturing method, which uses any of the additive manufacturing systems described above, such as Figure 4 As shown, the method includes: using the guiding device to guide the first material and setting the first material on the substrate according to the target shape; using the pretreatment device to perform surface pretreatment on the first material; using the applying device to apply the second material on the first material; and using the heating device to locally heat the first material to solidify the second material to form a composite material of the first material and the second material.

[0068] Furthermore, the additive manufacturing method may also include: processing the composite material so that the composite material is further solidified and fixed on the processing table.

[0069] For example, the processing of the composite material includes applying pressure and temperature to the composite material using a pressure curing device, so that the composite material is completely cured and fixed on the processing table. By using the pressure curing device in the above embodiment to pressurize and heat the composite material, the layer thickness of the composite material is controlled, so that the three-dimensional printing material is denser and has a low void ratio, and by providing heating, the composite material can reach a curing rate of more than 95%.

[0070] For example, the additive manufacturing system may include: a movable module configured to move according to the target shape, the guiding device, the pretreatment device, the application device, and the heating device being accommodated in the movable module and moving with the movement of the movable module. Accordingly, the additive manufacturing method may also include: while guiding the first material by the guiding device and placing the first material on the substrate according to the target shape, moving the movable module in a direction away from the fixed composite material.

[0071] For example, the substrate includes a building table or a composite material of the first material and the second material fixed on the building table in the previous process. The substrate can be the building table 16 or a printed material formed on the building table 16 in the previous step, that is, a composite material of the fixed first material and the second material. The building table 16 can be a rigid material table with a flat surface or a surface with a specific morphology, such as a stainless steel table; or a plastic material table with a flat surface or a surface with a specific morphology, such as a silicone table, etc. The building table can also be provided with a heating system to heat the three-dimensional printing material located thereon.

[0072] For example, in the additive manufacturing method according to an embodiment of the present disclosure, applying the second material on the first material includes: spraying the second material in liquid form on the first material by using a supply device.

[0073] Alternatively, applying the second material on the first material includes: coating the second material to the first material by a coating member. For example, the second material may be viscous so that it can be spin-coated onto the first material by a coating member, such as a coating roller. The embodiments of the present disclosure are not limited to this, as long as the second material can be applied to the surface of the first material.

[0074] For example, the second material can be a resin, for example, a thermosetting resin, for example, polyester, epoxy, phenolic, vinyl ester, thermosetting polyurethane, silicon, polyimide, polybismaleimide, ultraviolet curing resin, polycarbosilane, etc. Stabilizers can also be added to the resin, mainly including: ultraviolet absorbers, primary antioxidants, secondary antioxidants, quenchers, lubricants, plasticizers, flame retardants, for example, lubricants can include fatty alcohols, acids and esters or hydrocarbons, plasticizers can include phthalates, adipates or polychlorinated hydrocarbons, and flame retardants can include halogenated, non-halogenated, etc.

[0075] For example, in the additive manufacturing method of the embodiment of the present disclosure, locally heating the first material using the heating device may include: providing laser, infrared light, microwave or plasma to a local area of ​​the first material to achieve heating of the local area. For example, the heating device may be a laser emitter, an infrared light emitter, a microwave emitter or a plasma heater.

[0076] For example, in the additive manufacturing method according to an embodiment of the present disclosure, the performing surface pretreatment on the first material by using the pretreatment device may include:

[0077] The surface of the first material is subjected to surface activation and / or additional functionalization treatment.

[0078] For example, activation of the surface of the first material can be a cleaning and activation treatment to improve wettability and interface properties. For example, an adhesive coating can be applied to the surface of the first material, such as adhesive spraying, functional groups, such as -COOH, -OH, transplantation, plasma etching, plasma transplantation, ozone cleaning treatment, surface energy activation, spraying sizing agent, etc.

[0079] For example, performing additional functionalization on the surface of the first material may include, for example, applying, for example, spraying, functional powder or particles on the surface to attach them to the surface of the first material. The functional powder or particles may include polymer particles, thermosetting polymer powders and thermoplastic powders, metals (e.g., Al, Fe) and metal oxides (e.g., Al 2 O 3 , Fe 2 O 3 , Fe 3 O 4 ) powders and wires, ceramics (such as SiC, SiO 2 ) powders and wires, nanomaterials (e.g., carbon black, carbon nanotubes, graphene, graphite, boron nitride, Mexene).

[0080] For example, the additive manufacturing method according to the embodiment of the present disclosure may further include: using a supply device to provide the first material with controllable tension to the movable module; using a storage device to store the first material and providing the first material to the supply device through the storage device.

[0081] For example, Figure 2 As shown, the supply device includes a tensioning system to draw the first material from the storage device and guide it out and control the tension of the first material according to the type of the first material, for example, Figure 2 As shown, the tensioning system may include guide roller sets 181 and 182, and a tension control device 183.

[0082] For example, the additive manufacturing method according to the embodiment of the present disclosure may further include: cutting the first material, wherein the cutting is performed as follows: Figure 2 The cutting device 17 shown is arranged between the supply device and the guide device, and is configured to guide the first material to the guide device and cut the first material when the first material needs to be cut. The cutting device can be a fiber preform cutting machine, such as a laser cutting machine or a mechanical scissors.

[0083] Alternatively, the cutting device may be disposed inside or outside the movable module. If disposed inside the movable module, the cutting device may move with the movable module, thereby facilitating cutting of the first material, better controlling the shape of the 3D printed object, and improving the 3D printing accuracy.

[0084] For example, the first material may be a fiber preform, and the storage device may be a roll wound with the fiber preform.

[0085] For example, the fiber preform can be carbon fiber, aramid fiber, glass fiber, natural fiber, steel fiber, silver fiber, copper fiber or multi-component fiber, and any combination thereof. The fiber preform can be in the form of fiber bundle (untwisted), yarn (twisted), woven, non-woven, braided, knitted, 2D and 3D fabrics, pre-impregnated fabrics, thermoplastic or thermosetting coated fibers or fabrics or mixed yarns and fabrics.

[0086] For example, in the additive manufacturing method of the embodiment of the present disclosure, when the first material is a fiber preform, the moving direction of the movable module is parallel to the fiber direction of the fiber preform, and the applying device and the heating device are arranged in sequence along the direction opposite to the moving direction of the movable module and in the fiber direction. Figure 2The movable module moves in the direction of arrow A, which is parallel to the fiber direction, and the setting directions of the applying device 12, the heating device 13 and the pressure curing device 14 are also parallel to the fiber direction and are sequentially arranged in the movable module in the direction opposite to the moving direction of the movable module.

[0087] For example, in the additive manufacturing method, the movable module and the building platform can be arranged in a chamber, and the chamber is also provided with a temperature control device and a pressure control device. The additive manufacturing method can also include: measuring the temperature of the chamber, controlling the temperature in the chamber according to the temperature measurement result, for example, cooling or heating the chamber according to different three-dimensional printing materials and / or controlling the pressure in the chamber, etc., to further improve the quality of the three-dimensional printed product.

[0088] For example, the additive manufacturing method of the embodiment of the present disclosure may further include controlling the movement of the movable module using a control device, for example, the driving device is disposed outside the chamber.

[0089] For example, the driving device may be a robotic arm control system, which is fixedly connected to the movable module through a manipulator to control the movement of the movable module, and the robotic arm control system may be a six-axis control system, that is, the robotic arm may be a six-axis robotic arm, so that it can print three-dimensional objects of complex shapes and improve printing applicability. Alternatively, the robotic arm control system may also be an elevated XYZ frame, so that the movable module can be controlled to move in the three directions of X, Y|, and Z. Exemplarily, the movable module may be fixed on the frame of the elevated XYZ frame, for example, on a frame extending in a certain direction, the frame may be driven by a motor to move in the X direction and the Z direction, and the movable module may be driven by a motor to move along the frame in the Y direction, thereby realizing the movement of the movable module in the X, Y, and Z directions; or the frame may move in the Y direction and the Z direction, and the movable module may be driven by a motor to move along the frame in the X direction, so as to realize the movement of the movable module in the X, Y, and Z directions.

[0090] Below, the complete process flow of the additive manufacturing method according to the embodiment of the present disclosure is described exemplarily by taking the first material as a fiber preform and the second material as a liquid resin as an example: the fiber preform wound on the roller is pulled by the supply device and the tension of the first material is controlled according to the type of the first material, and then the fiber preform is sent to the movable module through the guide roller, and is laid on the construction platform through the cutting device and the guiding device in the movable module. With the rightward movement of the print head and the continuous supply of the fiber preform, the fiber preform moves to the left relative to the print head, and first passes through the pretreatment device for surface performance and functional preparation. Then, the liquid resin is sprayed on the surface of the application device, and then passes through the heating device. Under the action of the heat source, the resin impregnates the fiber preform and begins to solidify to form a composite material. The impregnated and nearly solidified composite material is pressed to a certain height by the pressure curing device, the holes are removed, and a high degree of solidification is achieved and bonded to the construction platform or the previous layer of printed material. In the above process flow, when the first material needs to be cut after the printing of a layer of material is completed, the first material is cut by the cutting device arranged between the supply device and the guiding device. If the movable module is mounted on a 6-axis robot arm, the movable module can move in three-dimensional space according to the shape of the printed part to perform three-dimensional stacking of materials.

[0091] In the additive manufacturing method of the embodiment of the present disclosure, the first material, for example, the fiber preform is locally heated by a heating device, and a temperature gradient distribution is formed along the fiber direction, so that the second material, for example, the liquid thermosetting resin has a reduced viscosity from the low temperature to the high temperature area on the fiber, and the reduced viscosity causes it to flow into the adjacent fibers due to the capillary force, and the higher temperature causes the liquid resin to solidify, so as to achieve rapid and synchronous infusion and solidification, and the composite material can be solidified into any three-dimensional shape. This local heating method can achieve a faster solidification speed and a higher degree of solidification of the printed material. The second material, for example, the liquid resin, can even overcome gravity under the capillary action and move vertically upward between the fibers. The composite material is densified due to the capillary action of the liquid resin between the fibers, thereby achieving a higher fiber volume fraction, which helps to improve the material performance. Moreover, before the composite material is solidified, the first material is guided to have a target shape by utilizing the movement of the guide system, so that no additional steps are required to make the composite material have a target shape, thereby improving the printing efficiency and achieving rapid additive manufacturing. Furthermore, by using a pressure curing device, it is possible to heat while applying pressure, making the composite material denser and having a lower porosity, and making the composite material reach a curing rate of more than 95%. Furthermore, by setting a pretreatment device, the surface of the first material can be activated and / or additionally functionalized before the second material is applied, so that the second material is easier to combine with the first material, and the two form a more stable composite material, and additional functionalization of the first material can make the three-dimensional printing material more stable and the product performance better.

[0092] There are a few points to note:

[0093] (1) The drawings of the embodiments of the present disclosure only relate to the structures related to the embodiments of the present disclosure, and other structures may refer to the general design.

[0094] (2) For the sake of clarity, in the drawings used to describe the embodiments of the present disclosure, the thickness of layers or regions is exaggerated or reduced, that is, these drawings are not drawn according to the actual scale. It is understood that when an element such as a layer, film, region or substrate is referred to as being "on" or "under" another element, the element may be "directly" "on" or "under" the other element or there may be intermediate elements.

[0095] (3) In the absence of conflict, the embodiments of the present disclosure and the features therein may be combined with each other to obtain new embodiments.

[0096] The above is only a specific implementation of the present disclosure, but the protection scope of the present disclosure is not limited thereto. Any person skilled in the art who is familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed in the present disclosure, which should be included in the protection scope of the present disclosure. Therefore, the protection scope of the present disclosure should be based on the protection scope of the claims.

Claims

1. An additive manufacturing system comprising: a guiding device for guiding a first material and arranging the first material on a substrate so that the first material is formed on the substrate to have a target shape; a pretreatment device for performing surface pretreatment on the first material; an applying device configured to apply a liquid second material to the surface of the pre-treated first material; A heating device locally heats the first material to solidify the second material and make the second material flow toward the heated area to form a composite material of the first and second materials. The additive manufacturing system further comprises: a movable module configured to move according to the target shape, The guiding device, the pre-treatment device, the applying device, and the heating device are housed in the movable module and move along with the movement of the movable module. The guiding device guides the first material while the movable module moves, and simultaneously applies the second material to the first material in the same direction as the moving direction of the movable module, and solidifies the second material to form the composite material having the target shape. The applying device and the heating device are sequentially arranged along a direction opposite to a moving direction of the movable module.

2. The additive manufacturing system according to claim 1, wherein the movable module further comprises: a pressure curing device configured to apply pressure and heat to the composite material to fix the composite material to the substrate, The movable module moves in a direction away from the fixed composite material.

3. The additive manufacturing system according to claim 2, further comprising: a supply device configured to supply the first material with controllable tension to the movable module; A storage device is configured to store the first material and provide the first material to the supply device. 4 . The additive manufacturing system according to claim 3 , wherein the first material is a fiber preform, and the storage device is a roller wound with the fiber preform.

5. The additive manufacturing system according to claim 2, further comprising: The cutting device is provided between the supply device and the guide device, and is configured to guide the first material to the guide device and to cut the first material. 6 . The additive manufacturing system according to claim 1 , wherein the substrate comprises a build table or a composite material of the first material and the second material fixed on the build table in a previous process.

7. The additive manufacturing system according to claim 6, further comprising: The chamber is configured to accommodate the movable module and the construction platform, and is further provided with a temperature control device and a pressure control device. 8 . The additive manufacturing system according to claim 2 , wherein the application device comprises a nozzle and is configured to apply the second material in liquid form to the first material.

9. The additive manufacturing system of claim 2, wherein the second material is a thermosetting resin.

10. The additive manufacturing system according to claim 7, further comprising: A driving device is configured to drive the movable module to move within the chamber, and the driving device is disposed outside the chamber.

11. The additive manufacturing system according to claim 4, wherein the moving direction of the movable module is parallel to the fiber direction of the fiber preform, and the applying device, the heating device and the pressure curing device are arranged in sequence along a direction opposite to the moving direction of the movable module and in the fiber direction.

12. An additive manufacturing method, using the additive manufacturing system according to claim 1, the method comprising: using the guiding device to guide the first material and arrange the first material on the substrate according to a target shape; Simultaneously, the surface of the first material is pretreated by the pretreatment device; Simultaneously, applying a liquid second material on the first material using the applying device; At the same time, the first material is locally heated by the heating device to solidify the second material and make the second material flow toward the heated area to form a composite material of the first material and the second material. The additive manufacturing system comprises: a movable module configured to move according to the target shape, The guiding device, the pre-processing device, the applying device and the heating device are accommodated in the movable module and move along with the movement of the movable module. The additive manufacturing method further comprises: while guiding the first material with the guide device and placing the first material on the substrate in a target shape, moving the movable module in a direction away from the fixed composite material, The applying device and the heating device are sequentially arranged along a direction opposite to a moving direction of the movable module.

13. The additive manufacturing method according to claim 12, further comprising: The composite material is processed so that the composite material is further solidified and fixed on a processing table.

14. The additive manufacturing method according to claim 13, wherein processing the composite material comprises: A pressure curing device is used to apply pressure and temperature to the composite material so that the composite material is completely cured and fixed on the processing table. 15 . The additive manufacturing method according to claim 13 , wherein the substrate comprises a build table or a composite material of the first material and the second material fixed on the build table in a previous process.

16. The additive manufacturing method of claim 12, wherein applying a second material on the first material comprises: The second material in liquid state is sprayed on the first material by using a supply device.

17. The additive manufacturing method according to claim 12, wherein the step of performing surface pretreatment on the first material using the pretreatment device comprises: The surface of the first material is subjected to surface activation and / or additional functionalization treatment.

18. The additive manufacturing method according to claim 17, wherein performing surface activation on the surface of the first material comprises: The surface of the first material is subjected to adhesive coating application, functional group implantation, plasma etching, plasma implantation, ozone cleaning treatment, surface energy activation or spraying of sizing agent.

19. The additive manufacturing method according to claim 17, wherein performing additional functionalization on the surface of the first material comprises: Functional powder or particle material is sprayed or deposited on the surface of the first material.

20. The additive manufacturing method according to claim 12, further comprising: Using a supply device to provide the first material with controllable tension to the movable module; The first material is stored in a storage device and is provided to the supply device through the storage device.

21. The additive manufacturing method according to claim 20, wherein the first material is a fiber preform, The moving direction of the movable module is parallel to the fiber direction of the fiber preform, and the applying device and the heating device are arranged in sequence along a direction opposite to the moving direction of the movable module and in the fiber direction.