A Raman detection method based on in-situ formation of a coating layer on the surface of gold nanoparticles induced by a coagulation agent
By forming a coating layer on the surface of gold nanoparticles and using the reaction of agglomerating agent and precipitating agent to immobilize the molecules to be measured, the problem of difficulty in fixing the molecules to be measured under the gold nanoparticle-enhanced substrate is solved, and the stability and stability of the detection signal are significantly improved. Sensitivity, achieving efficient detection capabilities.
Patent Information
- Application Number
- CN202210797179.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-07-08
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2042-07-08
AI Technical Summary
When using gold nanoparticles as enhanced substrates for SERS detection, it is difficult to achieve high-sensitivity and stable signals. This is mainly due to the poor fixation and capture effects of the molecules to be measured on the surface of the nanoparticles, which makes it difficult to fix and stabilize the detection signal at lower concentrations. .
By forming a coating layer in situ on the surface of gold nanoparticles, using the reaction of different coagulants and precipitants to generate insoluble or poorly soluble compounds, the molecules to be measured are fixed at hot spots, thereby improving the detection signal.
The stability and sensitivity of the detection signal are improved. Compared with samples without adding precipitant, the detection capability is improved by 3-4 orders of magnitude. It is simple to operate, has high repeatability and high flexibility.
Smart Images

Figure CN115184335B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of Raman spectroscopy detection, and in particular relates to a Raman detection method based on in-situ formation of a coating layer on the surface of nano-gold particles induced by a coagulation agent. Background Art
[0002] Using gold and silver nanoparticle sols as an enhanced substrate to detect molecules to be tested is a convenient and fast method, which is very suitable for the detection of liquid samples. The synthesis method of gold nanoparticles is simple and they are more stable than silver particles. However, in actual detection, it is difficult to achieve highly sensitive SERS detection using gold nanoparticles as an enhanced substrate. In the sol system, molecules diffuse in and out of hot spots due to Brownian motion. In addition, molecules are adsorbed and desorbed on the surface of nanoparticles, making it difficult for molecules to be fixed at hot spots on the particle surface. This makes it difficult to detect highly sensitive stable signals using gold nanocolloids as an enhanced substrate at lower concentrations.
[0003] The fixation and capture of the molecules to be tested on the surface of nanoparticles is conducive to improving the detection performance of the molecules. The existing research on Raman detection by sol method mainly focuses on the optimization of the type and amount of coagulation agent, and the generation of hot spots by the aggregation of nanoparticles. However, there is relatively little research on how to further fix the molecules to be tested at the hot spots of nanoparticles to improve the detection sensitivity. Therefore, the development of new methods in the system of gold nanoparticle sol as an enhancement agent by adding coagulation agents has important research significance and application prospects for improving the detection ability of molecules. Summary of the invention
[0004] The purpose of the present invention is to provide a Raman detection method based on the in-situ formation of a coating layer on the surface of nano-gold particles induced by a coagulant, by using gold nano-particle sol as an enhanced substrate and adding different coagulants and precipitants to form a coating layer on the surface of the gold particles in situ, thereby improving the detection ability of the molecules to be detected.
[0005] To achieve the above object, the technical solution of the present invention is as follows:
[0006] Step 1, preparation of gold nanoparticles:
[0007] Add 100 mL of ultrapure water to a conical flask, stir and heat to 130°C, then add 3-5 mL of a 1-2% sodium citrate aqueous solution and mix well, then add 0.25-0.35 mL of a 10-25 mmol / L chloroauric acid solution, and continue the reaction to obtain a nano-gold seed solution;
[0008] Second step of growth of nano-gold: add 160 mL of ultrapure water and 40 mL of nano-gold seed solution into a conical flask, stir and heat to 130°C, add 3-5 mL of 1-2% sodium citrate aqueous solution and mix well, then add 10-25 mmol / L chloroauric acid solution, add 0.4 mL each time, add 10 times in total, each time with an interval of 8 minutes, and continue to react for 15 minutes after the last addition of chloroauric acid to obtain the nano-gold solution grown in the second step;
[0009] The third step of growth: add 160 mL of ultrapure water and 40 mL of the nanogold solution obtained in the second step into a conical flask, stir and heat to 130°C, add 3-5 mL of a 1-2% sodium citrate aqueous solution, mix well, and then add a 10-25 mmol / L chloroauric acid solution, add 0.4 mL each time, add 10 times in total, each time at an interval of 8 minutes, and continue to react for 15 minutes after the last addition of chloroauric acid to obtain the final gold nanoparticle sol;
[0010] Step 2: Prepare standard solutions of different concentrations of the molecule to be tested
[0011] Take 250-500uL of gold nanoparticle sol and add it to the sample detection pool, then add 1-2mL of the standard solution of the dye molecule to be tested and mix well, then add 10-250uL of a precipitant with a concentration of 1-2mol / L and mix well, then add 2-250uL of a precipitant with a concentration of 10mmol / L-1.5mol / L, and after mixing, use a portable Raman spectrometer to detect the sample.
[0012] The coagulation agent is sodium chloride, sodium bromide, sodium iodide, calcium chloride or magnesium sulfate.
[0013] The precipitant is silver nitrate, magnesium sulfate or sodium carbonate.
[0014] The coagulating agent and the precipitating agent react to generate insoluble or poorly soluble compounds. When the coagulating agent is sodium chloride, sodium bromide or sodium iodide, the precipitating agent is silver nitrate; when the coagulating agent is calcium chloride, the precipitating agent is silver nitrate, magnesium sulfate or sodium carbonate; when the coagulating agent is magnesium sulfate, the precipitating agent is silver nitrate.
[0015] The dye molecules in the dye molecule standard solution include: crystal violet, rhodamine 6G, diquat, methylene blue or malachite green.
[0016] The volume of the gold nanoparticle sol in step 2 is 250uL.
[0017] The volume of the standard solution of the dye molecule to be tested in step 2 is 1 mL.
[0018] The concentration of the coagulant in step 2 is 1.5 mol / L.
[0019] Compared with the prior art, the present invention has the following beneficial effects:
[0020] 1. The present invention adds gold nanoparticle sol, a dye molecule solution to be tested, and a coagulation agent to a sample detection pool and mixes them evenly, then adds a precipitant that can react with the coagulation agent to produce an insoluble precipitate, and the precipitant covers the surface of the gold nanoparticles to form a coating layer. The coating layer fixes the molecules to be tested at the hot spot, thereby improving the detection signal.
[0021] 2. The present invention generates a coating layer on the surface of gold nanoparticles through the reaction between the coagulation agent and the precipitant. The reaction is fast and the response signal of the molecule to be tested can be quickly generated. In addition, the invention has a variety of coagulation agents and precipitants to choose from and has high flexibility.
[0022] 3. After the coagulation agent and the precipitant are added, a coating layer is formed on the surface of the gold particles, which improves the detection sensitivity of the molecules to be tested. Compared with the sample without the precipitant, the detection capability is improved by 3-4 orders of magnitude. The method is simple to operate and has high repeatability, which improves the detection sensitivity and application prospects of gold nanoparticle sol as an enhanced substrate. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 This is a transmission electron micrograph of the gold nanoparticle sol after sodium chloride coagulation agent was added;
[0024] Figure 2 Transmission electron microscopy image of gold nanoparticle sol after adding sodium chloride coagulation agent and silver nitrate precipitation agent;
[0025] Figure 3 Sodium chloride coagulation agent was added to the gold nanoparticle sol to detect the Raman spectra of crystal violet samples with different concentrations;
[0026] Figure 4 Sodium chloride coagulation agent and silver nitrate precipitant were added to the gold nanoparticle sol to detect the Raman spectra of crystal violet samples with different concentrations;
[0027] Figure 5 Sodium chloride coagulation agent and silver nitrate precipitant were added to the gold nanoparticle sol to detect the Raman spectra of rhodamine 6G samples with different concentrations;
[0028] Figure 6 Sodium chloride coagulation agent and silver nitrate precipitant were added to the gold nanoparticle sol to detect the Raman spectra of diquat at different concentrations;
[0029] Figure 7 Calcium chloride coagulation agent and magnesium sulfate precipitant were added to the gold nanoparticle sol to detect the Raman spectra of crystal violet samples with different concentrations;
[0030] Figure 8Magnesium sulfate precipitant and silver nitrate precipitant were added to the gold nanoparticle sol to detect the Raman spectra of crystal violet samples with different concentrations. DETAILED DESCRIPTION
[0031] The present invention is further described in detail below in conjunction with the accompanying drawings.
[0032] Embodiment 1:
[0033] Step 1, preparation of gold nanoparticles:
[0034] Add 100 mL of ultrapure water to a conical flask, stir and heat to 130°C, then add 4 mL of 1% sodium citrate aqueous solution and mix well, then add 0.3 mL of 10 mmol / L chloroauric acid solution, and continue the reaction to obtain a nano-gold seed solution;
[0035] Second step of growth of nano-gold: add 160 mL of ultrapure water and 40 mL of nano-gold seed solution into a conical flask, stir and heat to 130°C, add 4 mL of 1% sodium citrate aqueous solution and mix well, then add 10 mmol / L chloroauric acid solution, add 0.4 mL each time, add 10 times in total, each time with an interval of 8 minutes, and continue to react for 15 minutes after the last addition of chloroauric acid to obtain the nano-gold solution grown in the second step;
[0036] The third step of growth: add 160 mL of ultrapure water and 40 mL of the nanogold solution obtained in the second step into a conical flask, stir and heat to 130°C, add 4 mL of a 1% sodium citrate aqueous solution, mix well, and then add a 10 mmol / L chloroauric acid solution, 0.4 mL each time, for a total of 10 times, with an interval of 8 minutes each time. After the last addition of chloroauric acid, continue to react for 15 minutes to obtain the final gold nanoparticle sol;
[0037] Step 2: Prepare standard solutions of different concentrations of the molecule to be tested
[0038] Prepare a 0.01 mol / L crystal violet standard solution and dilute the solution to obtain 10 -8 mol / L-10 -14 mol / L standard test solution. Take 250uL of gold nanoparticle sol and add it to the sample detection pool, then add 1mL of crystal violet standard solution of the dye molecule to be tested and mix well, then add 250uL of 1.5mol / L sodium chloride coagulant and mix well to make the nanoparticles aggregate. The sample was detected using a portable Raman spectrometer with a power of 300mW, a laser wavelength of 785nm, and an integration time of 20s.
[0039] Then, 10 uL of 10 mmol / L silver nitrate precipitant was added and mixed, and the sample was detected again using a portable Raman spectrometer with a power of 300 mW, a laser wavelength of 785 nm, and an integration time of 20 s.
[0040] from Figure 1 It can be seen that the nanoparticles without precipitant aggregated and the dispersed nanoparticles were close together. Figure 2 It can be seen that after adding the precipitant, a precipitation layer is formed on the surface of the particles, and the adjacent nanoparticles are connected by the precipitation layer and are no longer dispersed single particles.
[0041] In Example 1, the Raman spectra of the crystal violet samples with different concentrations after adding sodium chloride coagulation agent for detection are as follows: Figure 3 As shown, a concentration of 10 -8 mol / L crystal violet signal, when the concentration of the test solution is 10 -9 mol / L, no detection signal can be obtained.
[0042] In Example 1, the Raman spectra of the crystal violet samples with different concentrations after adding sodium chloride coagulation agent and silver nitrate precipitation agent are as follows: Figure 4 As shown, a concentration of 10 -12 The crystal violet signal was 1.34 mol / L, and the detection sensitivity was improved by 4 orders of magnitude compared with the sample without adding the precipitant in Example 1.
[0043] Embodiment 2:
[0044] Step 1, preparation of gold nanoparticles:
[0045] Add 100 mL of ultrapure water to a conical flask, stir and heat to 130°C, then add 3 mL of 1.3% sodium citrate aqueous solution and mix well, then add 0.32 mL of 18 mmol / L chloroauric acid solution, and continue the reaction to obtain a nano-gold seed solution;
[0046] Second step of gold nanoparticle growth: 160 mL of ultrapure water and 40 mL of gold nanoparticle seed solution were added to a conical flask, stirred and heated to 130°C, 3 mL of 1.3% sodium citrate aqueous solution was added and mixed evenly, and then 18 mmol / L chloroauric acid solution was added, 0.4 mL each time, for a total of 10 times, with an interval of 8 minutes each time. After the last addition of chloroauric acid, the reaction was continued for 15 minutes to obtain the gold nanoparticle solution grown in the second step;
[0047] The third step of growth: add 160 mL of ultrapure water and 40 mL of the nanogold solution obtained in the second step into a conical flask, stir and heat to 130°C, add 3 mL of 1.3% sodium citrate aqueous solution, mix well, and then add 18 mmol / L chloroauric acid solution, add 0.4 mL each time, add 10 times in total, each time with an interval of 8 minutes, and continue to react for 15 minutes after the last addition of chloroauric acid to obtain the final gold nanoparticle sol;
[0048] Step 2: Prepare standard solutions of different concentrations of the molecule to be tested
[0049] Prepare 0.01 mol / L Rhodamine 6G standard solution, dilute the solution to obtain 10 -8 mol / L-10 -13 mol / L standard test solution. Take 300uL of gold nanoparticle sol and add it to the sample detection pool, then add 1.5mL of the test dye molecule Rhodamine 6G standard solution and mix well, then add 200uL of 1.2mol / L sodium chloride coagulation agent and mix well to make the nanoparticles aggregate. The sample was detected using a portable Raman spectrometer with a power of 300mW, a laser wavelength of 785nm, and an integration time of 20s.
[0050] Then, 100 uL of 100 mmol / L silver nitrate precipitant was added and mixed, and the sample was detected again using a portable Raman spectrometer with a power of 300 mW, a laser wavelength of 785 nm, and an integration time of 20 s.
[0051] In Example 2, the Raman spectra of rhodamine 6G samples with different concentrations after adding sodium chloride coagulation agent and silver nitrate precipitation agent for detection are as follows: Figure 5 Without the addition of silver nitrate precipitant, 10 -9 mol / L Raman signal of rhodamine 6G; after adding silver nitrate precipitant, the minimum detectable -12 mol / L.
[0052] Embodiment 3:
[0053] Step 1, preparation of gold nanoparticles:
[0054] Add 100 mL of ultrapure water to a conical flask, stir and heat to 130°C, then add 5 mL of 1.8% sodium citrate aqueous solution and mix well, then add 0.28 mL of 25 mmol / L chloroauric acid solution, and continue the reaction to obtain a nano-gold seed solution;
[0055] Second step of gold nanoparticle growth: 160 mL of ultrapure water and 40 mL of gold nanoparticle seed solution were added to a conical flask, stirred and heated to 130°C, 5 mL of 2% sodium citrate aqueous solution was added and mixed evenly, and then 13 mmol / L chloroauric acid solution was added, 0.4 mL each time, for a total of 10 times, with an interval of 8 minutes each time. After the last addition of chloroauric acid, the reaction was continued for 15 minutes to obtain the gold nanoparticle solution for the second step of growth;
[0056] The third step of growth: add 160 mL of ultrapure water and 40 mL of the nanogold solution obtained in the second step into a conical flask, stir and heat to 130°C, add 5 mL of a 2% sodium citrate aqueous solution, mix well, and then add a 25 mmol / L chloroauric acid solution, 0.4 mL each time, for a total of 10 times, with an interval of 8 minutes each time. After the last addition of chloroauric acid, continue to react for 15 minutes to obtain the final gold nanoparticle sol;
[0057] Step 2: Prepare standard solutions of different concentrations of the molecule to be tested
[0058] Prepare a 0.01 mol / L diquat standard solution and dilute the solution to obtain 10 -7 mol / L-10 -10 mol / L standard test solution. Take 400uL of gold nanoparticle sol and add it to the sample detection pool, then add 1.8mL of the test dye molecule diquat standard solution and mix well, then add 100uL of 1mol / L sodium chloride coagulant and mix well to make the nanoparticles aggregate. The sample was detected using a portable Raman spectrometer with a power of 300mW, a laser wavelength of 785nm, and an integration time of 20s.
[0059] Subsequently, 2 uL of a silver nitrate precipitant with a concentration of 500 mmol / L was added and mixed, and the sample was detected again using a portable Raman spectrometer with a power of 300 mW, a laser wavelength of 785 nm, and an integration time of 20 s.
[0060] In Example 3, the Raman spectra of the samples with different concentrations of diquat after adding sodium chloride coagulation agent and silver nitrate precipitation agent for detection are as follows: Figure 6 Without the addition of silver nitrate precipitant, 10 -8 mol / L Diquat Raman signal; after adding silver nitrate precipitant, the minimum detectable -9 mol / L.
[0061] Embodiment 4:
[0062] Step 1, preparation of gold nanoparticles:
[0063] Add 100 mL of ultrapure water to a conical flask, stir and heat to 130°C, then add 3.5 mL of 2% sodium citrate aqueous solution and mix well, then add 0.35 mL of 13 mmol / L chloroauric acid solution, and continue the reaction to obtain a nano-gold seed solution;
[0064] Second step of gold nanoparticle growth: 160 mL of ultrapure water and 40 mL of gold nanoparticle seed solution were added to a conical flask, stirred and heated to 130°C, 4.5 mL of 1.5% sodium citrate aqueous solution was added and mixed evenly, and then 20 mmol / L chloroauric acid solution was added, 0.4 mL each time, for a total of 10 times, with an interval of 8 minutes each time. After the last addition of chloroauric acid, the reaction was continued for 15 minutes to obtain the gold nanoparticle solution for the second step of growth;
[0065] The third step of growth: add 160 mL of ultrapure water and 40 mL of the nanogold solution obtained in the second step into a conical flask, stir and heat to 130°C, add 4.5 mL of a 1.5% sodium citrate aqueous solution, mix well, and then add a 13 mmol / L chloroauric acid solution, 0.4 mL each time, for a total of 10 times, with an interval of 8 minutes each time. After the last addition of chloroauric acid, continue to react for 15 minutes to obtain the final gold nanoparticle sol;
[0066] Step 2: Prepare standard solutions of different concentrations of the molecule to be tested
[0067] Prepare a 0.01 mol / L crystal violet standard solution and dilute the solution to obtain 10 -8 mol / L-10 -13 mol / L standard test solution. Take 500uL of gold nanoparticle sol and add it to the sample detection pool, then add 1.5mL of the crystal violet standard solution of the dye molecule to be tested and mix well, then add 50uL of 2mol / L calcium chloride coagulant and mix well to make the nanoparticles aggregate. The sample was detected using a portable Raman spectrometer with a power of 300mW, a laser wavelength of 785nm, and an integration time of 20s.
[0068] Subsequently, 200 uL of 1 mol / L magnesium sulfate precipitant was added and mixed, and the sample was detected again using a portable Raman spectrometer with a power of 300 mW, a laser wavelength of 785 nm, and an integration time of 20 s.
[0069] In Example 4, the Raman spectra of crystal violet samples with different concentrations after adding calcium chloride coagulation agent and magnesium sulfate precipitation agent for detection are as follows: Figure 7 When magnesium sulfate precipitant is not added, 10 -9 mol / L crystal violet Raman signal; after adding magnesium sulfate precipitant, the minimum detectable-11 mol / L.
[0070] Embodiment 5:
[0071] Step 1, preparation of gold nanoparticles:
[0072] Add 100 mL of ultrapure water to a conical flask, stir and heat to 130°C, then add 4.5 mL of 1.5% sodium citrate aqueous solution and mix well, then add 0.25 mL of 20 mmol / L chloroauric acid solution, and continue the reaction to obtain a nano-gold seed solution;
[0073] Second step of gold nanoparticle growth: 160 mL of ultrapure water and 40 mL of gold nanoparticle seed solution were added to a conical flask, stirred and heated to 130°C, 3.5 mL of 1.8% sodium citrate aqueous solution was added and mixed evenly, and then 25 mmol / L chloroauric acid solution was added, 0.4 mL each time, for a total of 10 times, with an interval of 8 minutes each time. After the last addition of chloroauric acid, the reaction was continued for 15 minutes to obtain the gold nanoparticle solution grown in the second step;
[0074] The third step of growth: add 160 mL of ultrapure water and 40 mL of the nanogold solution obtained in the second step into a conical flask, stir and heat to 130°C, add 3.5 mL of a 1.8% sodium citrate aqueous solution, mix well, and then add a 20 mmol / L chloroauric acid solution, 0.4 mL each time, for a total of 10 times, with an interval of 8 minutes each time. After the last addition of chloroauric acid, continue to react for 15 minutes to obtain the final gold nanoparticle sol;
[0075] Step 2: Prepare standard solutions of different concentrations of the molecule to be tested
[0076] Prepare a 0.01 mol / L crystal violet standard solution and dilute the solution to obtain 10 -8 mol / L-10 -13 mol / L standard test solution. Take 450uL of gold nanoparticle sol and add it to the sample detection pool, then add 2mL of crystal violet standard solution of the dye molecule to be tested and mix well, then add 10uL of magnesium sulfate coagulation agent with a concentration of 1.8mol / L and mix well to make the nanoparticles aggregate. The sample was detected using a portable Raman spectrometer with a power of 300mW, a laser wavelength of 785nm, and an integration time of 20s.
[0077] Subsequently, 250 uL of 1.5 mol / L silver nitrate precipitant was added and mixed, and the sample was detected again using a portable Raman spectrometer with a power of 300 mW, a laser wavelength of 785 nm, and an integration time of 20 s.
[0078] In Example 5, the Raman spectra of crystal violet samples with different concentrations after adding magnesium sulfate coagulation agent and silver nitrate precipitant for detection are as follows: Figure 8 Without the addition of silver nitrate precipitant, 10 -9 mol / L crystal violet Raman signal; after adding silver nitrate precipitant, the minimum detectable -11 mol / L.
Claims
1. A Raman detection method based on the in-situ formation of a coating layer on the surface of gold nanoparticles induced by a coagulation agent, characterized in that: The following steps are involved: Step 1, preparation of gold nanoparticles: Add 100 mL of ultrapure water to a conical flask, stir and heat to 130°C, then add 3-5 mL of a 1-2% sodium citrate aqueous solution and mix well, then add 0.25-0.35 mL of a 10-25 mmol / L chloroauric acid solution, and continue the reaction to obtain a nano-gold seed solution; Second step of growth of nano-gold: add 160 mL of ultrapure water and 40 mL of nano-gold seed solution into a conical flask, stir and heat to 130°C, add 3-5 mL of 1-2% sodium citrate aqueous solution and mix well, then add 10-25 mmol / L chloroauric acid solution, add 0.4 mL each time, add 10 times in total, each time with an interval of 8 minutes, and continue to react for 15 minutes after the last addition of chloroauric acid to obtain the nano-gold solution grown in the second step; The third step of growth: add 160 mL of ultrapure water and 40 mL of the nanogold solution obtained in the second step into a conical flask, stir and heat to 130°C, add 3-5 mL of a 1-2% sodium citrate aqueous solution, mix well, and then add a 10-25 mmol / L chloroauric acid solution, add 0.4 mL each time, add 10 times in total, each time at an interval of 8 minutes, and continue to react for 15 minutes after the last addition of chloroauric acid to obtain the final gold nanoparticle sol; Step 2: Prepare standard solutions of different concentrations of the molecule to be tested Take 250-500uL of gold nanoparticle sol and add it to the sample detection pool, then add 1-2mL of the standard solution of the dye molecule to be tested and mix well, then add 10-250uL of a precipitant with a concentration of 1-2mol / L and mix well, then add 2-250uL of a precipitant with a concentration of 10mmol / L-1.5mol / L, and after mixing, use a portable Raman spectrometer to detect the sample.
2. The method for Raman detection based on the in-situ formation of a coating layer on the surface of gold nanoparticles induced by a coagulation agent according to claim 1, characterized in that: The coagulation agent is sodium chloride, sodium bromide, sodium iodide, calcium chloride or magnesium sulfate.
3. The method for Raman detection based on the in-situ formation of a coating layer on the surface of gold nanoparticles induced by a coagulation agent according to claim 1, characterized in that: The precipitant is silver nitrate, magnesium sulfate, or sodium carbonate.
4. The method for Raman detection based on the in-situ formation of a coating layer on the surface of gold nanoparticles induced by a coagulation agent according to claims 2 and 3, characterized in that: The coagulating agent and the precipitating agent react to generate insoluble or poorly soluble compounds. When the coagulating agent is sodium chloride, sodium bromide or sodium iodide, the precipitating agent is silver nitrate; when the coagulating agent is calcium chloride, the precipitating agent is silver nitrate, magnesium sulfate or sodium carbonate; when the coagulating agent is magnesium sulfate, the precipitating agent is silver nitrate.
5. The method for Raman detection based on in-situ formation of a coating layer on the surface of gold nanoparticles induced by a coagulation agent according to claim 1, characterized in that: The dye molecules in the dye molecule standard solution include: crystal violet, rhodamine 6G, diquat, methylene blue or malachite green.
6. The method for Raman detection based on the in-situ formation of a coating layer on the surface of gold nanoparticles induced by a coagulation agent according to claim 1, characterized in that: The volume of the gold nanoparticle sol in step 2 is 250uL.
7. The method for Raman detection based on in-situ formation of a coating layer on the surface of gold nanoparticles induced by a coagulation agent according to claim 1, characterized in that: The volume of the standard solution of the dye molecule to be tested in step 2 is 1 mL.
8. The method for Raman detection based on the in-situ formation of a coating layer on the surface of gold nanoparticles induced by a coagulation agent according to claim 1, characterized in that: The concentration of the coagulant in step 2 is 1.5 mol / L.