A fast DLP 3D printing control parameter optimization method combining continuous and layered molding
The liquid-liquid interface printing scene was simulated by VoF method, combined with Posuo leaf flow and Lambert-Bill's law, and optimized the control parameters of DLP 3D printing, solving the problem of insufficient printing speed and model adaptability in DLP 3D printing technology, realizing the Fast and efficient printing results.
Patent Information
- Application Number
- CN202210540382.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-05-13
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2042-05-13
AI Technical Summary
The existing DLP 3D printing technology has limitations in improving the printing speed and model adaptation range, especially due to the leveling speed of the photosensitive resin and the loss of lubricant fluid, resulting in low printing efficiency and limited model adaptation.
The fluid volume (VoF) method is used to simulate the liquid-liquid interface printing scene, combining Posuo leaf flow and Lambert-Bill's law to optimize the control parameters of continuous and layered printing, including resin curing time, maximum fillable distance and printing platform enhancement speed , to achieve fast DLP 3D printing.
By optimizing control parameters, rapid printing of any model is achieved, printing efficiency and model adaptability are improved, and it is suitable for most DLP 3D printing scenarios, improving printing speed and scope of application.
Smart Images

Figure CN115230163B_ABST
Abstract
Description
Technical Field
[0001] The present invention involves computational fluid dynamics, intelligent control and image processing technology. By simulating the flow behavior of resin and adopting relevant laws of computational fluid dynamics to express key control parameters of digital light processing (DLP) 3D, the fast DLP 3D printing control is optimized and the printing efficiency and model adaptation range are improved. Background Art
[0002] 3D printing technology refers to a device that uses 3D printing technology to produce real three-dimensional models. Its basic principle is to use special consumables (glue, resin or powder, etc.) according to the three-dimensional model pre-designed by the computer, and to bond each layer of powder into shape through the deposition of adhesive, and finally print out a 3D entity. At present, there are many different 3D printing processes, such as stereolithography (SLA), laminated object manufacturing (LOM), fused deposition modeling (FDM), selected laser sintering (SLS), three-dimensional printing (3DP), DLP 3D printing, etc. However, at present, FDM has poor accuracy, and it is necessary to continuously melt the material filament and wait for the material to solidify, and the overall molding speed is slow. Digital Light Processing (DLP) 3D printing technology uses DLP light machine or projector as the light source, and adopts a layered printing method. The printing platform rises and then falls, leaving a slice layer thickness with the resin tank, and can complete layer-by-layer exposure. Compared with other printing methods, it has quickly improved the printing speed.
[0003] As the demand for DLP 3D printing technology production continues to increase, the layered molding method can no longer meet the market's requirements for printing speed. In recent years, a series of continuous molding technologies for DLP 3D printing have emerged, including the continuous interface production technology (Continuous Liquid Interface Production, CLIP) invented by the University of North Carolina in the United States in 2015 based on DLP 3D printing. In 2018, Song Yanlin's team at the Institute of Chemistry, Chinese Academy of Sciences, was inspired by the smoothness of the surface of pitcher plants and invented an ultra-low adhesion manufacturing interface. In 2019, Walker DA and others from Northwestern University in the United States invented a large-scale rapid DLP 3D printing method based on liquid-liquid interface. The above methods can increase the speed of DLP 3D printing, but are limited by the leveling speed of photosensitive resins and have a limited range of applicable models.
[0004] In 2021, Liu et al. combined layering with continuous printing based on the ultra-low adhesion interface designed by Song Yanlin, and proposed the key parameter of the maximum resin filling distance during continuous printing, which increased the model adaptation range. However, the loss of lubricating fluid limited the height of the printed model. In 2022, Li YD et al. proposed a model-guided layered and continuous 3D printing method based on Walker DA's liquid-liquid interface printing method. On the basis of the method of Liu et al., they proposed the optimal lifting height for layered printing to reduce the layered printing time, and the method proposed by Li YD et al. can adapt to most models, but the parameters are determined by experiments, which is inefficient, greatly affected by the environment, and the parameters that can be optimized are limited. These have seriously affected the application of DLP 3D printing technology. Summary of the invention
[0005] The present invention provides a fast DLP 3D printing control parameter optimization method combining continuous and layered molding, simulating the liquid-liquid interface printing scene through the volume of fluid (VoF) method, and recording the flow behavior of the resin between the printed object and the fluorinated oil after printing a layer of slices, and then based on Poiseuille flow, Jacobs working curve and Lambert-Beer law, it is used to express the resin curing time of continuous and layered printing, the maximum filling distance of continuous printing, the best lifting distance of layered printing and the lifting speed of the printing platform corresponding to the two methods. The proposed fast DLP 3D printing control parameter optimization method combining continuous and layered molding can achieve fast printing of any model by obtaining the optimal control parameters.
[0006] To solve the above technical problems, the embodiments of the present invention adopt the following technical solutions:
[0007] A method for optimizing control parameters of fast DLP 3D printing combining continuous and layered molding comprises the following steps:
[0008] Step 100: Slice the 3D model to be printed to obtain the number of slices i, determine the printable area of each slice, and calculate the maximum value D of the shortest distances from all points in the printable area of each slice to its boundary points. MAX [i];
[0009] Step 200, based on the standard solver of the open source computational fluid dynamics (CFD) software OpenFOAM, according to the liquid-liquid two-phase flow printing scenario of resin-fluorinated oil, a numerical simulation model is established using the VoF model;
[0010] Step 300: Establish a Cartesian coordinate system according to the printing scene, based on the D obtained in step 100.MAX [i] and the numerical simulation model established in step 200, using Poiseuille flow characteristics analysis to obtain the printing mode of each slice;
[0011] Step 400, according to the slice printing mode obtained in step 300, take the slices printed in a continuous manner, calculate the rising speed of the continuous molding printing platform according to the Lambert-Beer law, and write it into the printing configuration file;
[0012] Step 500: According to the slice printing mode obtained in step 300, take the slice printed in a layered manner, calculate the relationship between its resin leveling time and other control parameters, and obtain the expression of the layered resin curing time according to the Jacobs working curing curve, and write the obtained control parameters into the printing configuration file;
[0013] Step 600: Before printing begins, the printing origin is determined by camera monitoring, and then printing is completed according to the printing configuration file.
[0014] The 3D model to be printed is sliced to obtain the number of slices i, the printable area of each slice is determined, and the maximum value D of the shortest distances from all points in the printable area of each slice to its boundary points is calculated. MAX [i] Step 100 includes:
[0015] Slice the 3D model to be printed. At this time, only the pixels with a grayscale value of 255 are the pixels to be exposed. Take the area with a grayscale value of 255 as the printable area of the slice.
[0016] Detect the printable areas of different slices, determine the four points of the upper left corner, lower left corner, upper right corner and lower right corner, connect them into a closed area S, and obtain the pixel point closest to the center point of the printable area among the non-edge points, record these distance values and compare them to obtain the maximum value D of the minimum distance corresponding to different slices i MAX [i].
[0017] Among them, based on the standard solver of the open source computational fluid dynamics (CFD) software OpenFOAM, according to the liquid-liquid two-phase flow printing scene of resin-fluorinated oil, the VoF model is adopted to establish the numerical simulation model step 200, which includes:
[0018] According to the standard solver of the open source CFD software OpenFOAM, and using the VoF model, a liquid-liquid two-phase flow printing scenario including the resin tank, printing platform, printing object, resin and fluorinated oil is established;
[0019] At the same time, the resin tank, printing platform and printing object are set as rigid materials, the boundary where the resin tank contacts the fluorinated oil and resin is set as a solid wall boundary, the surface where the printing platform and printing object contact the resin and fluorinated oil is set as a linear sliding boundary, and the boundary between the resin and the fluorinated oil is a no-slip boundary.
[0020] Wherein, a Cartesian coordinate system is established according to the printing scene, and the D MAX [i] and the numerical simulation model established in step 200, further adopting Poiseuille flow characteristic analysis to obtain the printing mode of each slice, step 300 includes:
[0021] The resin has the same flow characteristics in any direction in the printed model and the gap between the fluorinated oil, and a Cartesian coordinate system is established according to the printing scene;
[0022] The Reynolds number of the resin flowing in the gap between the printed model and the fluorinated oil is less than 1, which conforms to the laminar flow between the plates and the Poiseuille flow, and has the NS equation:
[0023]
[0024] The origin of y is the interface between the fluorinated oil and the resin, indicating the distance from this interface. The origin of x is the interface between the fluorinated oil and the resin perpendicular to the edge of the printed object, indicating the distance of the resin filling. There are boundary conditions:
[0025]
[0026] Where u is the maximum speed of the resin moving in the x-axis direction, u s is the slip velocity, H s is the height of the printing platform, dp / dx is the pressure gradient, μ1 is the viscosity of the resin, and the integral of formula (1) is:
[0027]
[0028] Here C1 and C2 are constants. Substituting the boundary condition (3) into (1), we can obtain:
[0029]
[0030] C2=0#(5)
[0031]
[0032] According to the linear sliding setting of the scene, we can get:
[0033]
[0034] Where D sis the slip length. According to equations (1), (4) and (7), we can obtain:
[0035]
[0036]
[0037] According to formula (9), the volume flow Q between the printed model with a width of W and the fluorinated oil can be obtained as:
[0038]
[0039] The average flow rate of photosensitive resin is:
[0040]
[0041] During the time t1 when the platform rises, the resin fills the distance L in one direction. r Relationship with time variable t:
[0042]
[0043] v m is the speed of the printing platform during the rising process, t1 is the filling distance L r The resin filling time is the time for continuous printing.
[0044] The boundary between continuous printing and layered printing needs to determine the maximum filling distance of the resin for continuous printing, which must be less than D MAX [i], then the time required for single frame playback is 1 / f n The gap left after the printing platform rises is completely filled, and at the same time, the resin filling the gap can be completely cured before the next frame of the image is played. In the continuous printing, the rising speed of the printing platform is slow. Combined with formula (12), we have:
[0045]
[0046] The maximum filling distance of continuous printing resin can be obtained, and the corresponding D MAX [i]′:
[0047]
[0048] Therefore, if the slice D MAX [i]>D MAX [i]′ then this slice is printed using layered molding. If the slice D MAX [i]≤D MAX [i]′ uses continuous molding printing.
[0049] According to the slice printing mode obtained in step 300, the slices printed in a continuous manner are taken, and the rising speed of the continuous molding printing platform is calculated according to the Lambert-Beer law, and the rising speed is written into the printing configuration file. Step 400 includes:
[0050] Take the slice of the continuous molding print obtained in step 300, according to the Lambert-Beer law:
[0051]
[0052] Where P(z) is the optical power at a depth z away from the printing interface. The unit of depth z is μm and the unit of optical power is mW / cm 2 , P o is the power at the curing interface, which is the interface between the resin and the fluorinated oil. Therefore, the critical curing energy E of the slice at z is c have:
[0053]
[0054] Under the premise of ensuring curability, the printing platform rise speed v of continuous printing m The relationship with the maximum curable layer thickness z is:
[0055]
[0056] The thickness of the slice to be printed is determined according to the user's printing needs, and the rising speed of the continuous printing platform is calculated according to formula (17). The rising speed of the continuous printing platform and its corresponding slice layer number are written into the printing configuration file.
[0057] According to the slice printing mode obtained in step 300, the slice printed in a layered manner is taken, the relationship between the resin leveling time and other control parameters is calculated, and the expression of the layered resin curing time is obtained according to the Jacobs working curing curve, and the obtained control parameters are written into the printing configuration file. Step 500 includes:
[0058] Take the slice of the layered molding print obtained in step 300, and the resin is r Flow to D MAX The time of [i] is recorded as t2, and according to formula (12):
[0059]
[0060] The time T for resin filling in layered printing is recorded as:
[0061]
[0062] According to formula (19), the slip length D s Much smaller than the printing platform lifting height Hs , so it is believed that (H s -D s ) / (H s -4D s ) is a constant C3 greater than 1, then the relationship between the optimal lifting height of the printing platform and the resin filling time T when the resin filling time of layered printing is the minimum is:
[0063]
[0064] At this time, the obtained H s Optimal lifting height for layered printing;
[0065] The resin curing time model was established based on the Jacobs working curing curve:
[0066]
[0067] Among them C d is the curing depth, D p is the penetration depth, E o is the accumulated illumination energy of the DLP light source at the curing interface, E c It is the critical exposure for resin curing under UV light. The unit of curing depth and transmission depth is μm, and the unit of light energy is mw / cm 2 The unit of critical exposure is mw / cm 2 Therefore, for slices with different layer thicknesses printed in layers, the curing time t3 can be expressed as:
[0068]
[0069] The thickness of the slice to be printed is determined according to the user's printing needs. The optimal lifting height of the layered molding printing platform is calculated according to formula (20). The rising speed of the printing platform can also be obtained based on this. The resin curing time of the layered molding is determined according to formula (22). The optimal lifting height of the printing platform, the rising speed of the printing platform, the resin curing time and the corresponding slice layer number are written into the printing configuration file.
[0070] Furthermore, before printing starts, the printing origin is determined by camera monitoring, and then according to the printing configuration file, the printing step 600 includes:
[0071] Before printing, add fluorinated oil into the printing resin tank, pour photosensitive resin on top, and place the light source under the resin tank. Because fluorinated oil is a colorless liquid and photosensitive resin is a colored liquid, a camera can be used to monitor the printing origin from the side before printing begins to ensure that the printing platform is lowered to a place one slice layer thickness away from the fluorinated oil interface;
[0072] The printing configuration files obtained in steps 400 and 500 are loaded, and the model printing is started.
[0073] A fast DLP 3D printing control parameter optimization method combining continuous and layered molding according to an embodiment of the present invention has the following advantages:
[0074] 1) Using the proposed method, a set of optimal control parameters can be quickly designed for different models by combining continuous and layered molding methods for DLP 3D printing based on liquid-liquid interface;
[0075] 2) Portability. The method of this patent can simulate the motion characteristics of the interface between resin and fluorinated oil. By setting different parameters, the real printing process can be approached as close as possible to obtain simulation results such as resin filling time. At the same time, this method is not only applicable to liquid-liquid printing scenarios, but also can be applied to other DLP 3D printing scenarios by modifying the material represented by the fluorinated oil and the boundary conditions of the contact surface with the resin;
[0076] 3) Printability: The method of combining layered printing with continuous printing can be applied to most models. Therefore, the present invention has high theoretical significance and application value. BRIEF DESCRIPTION OF THE DRAWINGS
[0077] Figure 1 The device composition principle according to the embodiment of the present invention
[0078] Figure 2 It is a flow chart of a method for optimizing control parameters of fast DLP 3D printing combining continuous and layered molding according to an embodiment of the present invention.
[0079] Figure 3 It is a schematic diagram of a liquid-liquid two-phase flow printing scenario according to an embodiment of the present invention.
[0080] Figure 4 Schematic diagram of resin flow according to an embodiment of the present invention.
[0081] Figure 5 Schematic diagram showing the layers and continuous areas of the tower model. DETAILED DESCRIPTION
[0082] The embodiments of the present invention will be described in detail below in conjunction with the accompanying drawings. It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other arbitrarily.
[0083] The present invention provides a method for optimizing control parameters of fast DLP 3D printing combined with continuous and layered molding, simulating the liquid-liquid interface printing scene through the VoF method, and recording the flow behavior of the resin between the printed object and the fluorinated oil after printing a layer of slices, and then based on Poiseuille flow, Jacobs working curve and Lambert-Beer law, it is used to express the control parameters of the resin curing time of continuous and layered printing, the maximum filling distance of continuous printing, the optimal lifting distance of layered printing and the lifting speed of the printing platform corresponding to the two methods. The proposed method for optimizing control parameters of fast DLP 3D printing combined with continuous and layered molding can achieve fast printing of any model by obtaining the optimal control parameters.
[0084] DLP technology is considered to have the production efficiency that matches that of traditional manufacturing due to its fast printing speed. With the further increase in the demand for DLP 3D printing technology, the layered printing method can no longer meet the market's requirements for printing speed. In recent years, a series of continuous molding technologies for DLP 3D printing have emerged. However, limited by the leveling speed of photosensitive resins, the above methods are mostly used to print hollow models, and are difficult to apply to models with many large-sized solid slices. The method of the embodiment of the present invention addresses the problem of continuous printing. While ensuring model adaptation, a fast DLP 3D printing control parameter optimization method combining continuous and layered molding is proposed to improve printing efficiency and adaptability to slices of models of any size. Figure 1 The schematic diagram of the device composition of the example of the present invention is shown, which includes a DLP light source 1010, a resin tank 1060, a printing platform 1050 and a lead screw 1070, wherein the resin tank 1060 is located directly above the DLP light source 1010, and the DLP light source and the lead screw 1070 are respectively connected to the control host computer. Before printing begins, the resin tank contains fluorinated oil 1020 and resin 1030, and the DLP light source 1010 projects a two-dimensional slice of the model to be printed onto the interface between the fluorinated oil 1020 and the resin 1030 in the resin tank 1060, and the resin is induced to change from liquid to solid by ultraviolet light, solidified into a printed object 1040 and bonded to the printing platform 1050, and the lead screw 1070 drives the printing platform to move, and the resin flows into the gap between the solidified layer and the fluorinated oil, and then the aforementioned steps are repeated until the curing of the printed model is finally completed.
[0085] Figure 2 The flowchart of a method for optimizing control parameters of fast DLP 3D printing combining continuous and layered molding according to an embodiment of the present invention.
[0086] The embodiment of the present invention provides a method for optimizing control parameters of fast DLP 3D printing combining continuous and layered molding, comprising:
[0087] Step 100: Slice the 3D model to be printed to obtain the number of slices i, determine the printable area of each slice, and calculate the maximum value D of the shortest distances from all points in the printable area of each slice to its boundary points. MAX [i];
[0088] Step 200, based on the standard solver of the open source computational fluid dynamics (CFD) software OpenFOAM, according to the liquid-liquid two-phase flow printing scenario of resin-fluorinated oil, a numerical simulation model is established using the VoF model;
[0089] Step 300: Establish a Cartesian coordinate system according to the printing scene, based on the D obtained in step 100. MAX [i] and the numerical simulation model established in step 200, further using Poiseuille flow characteristics analysis to obtain the printing mode of each slice;
[0090] Step 400, according to the slice printing mode obtained in step 300, take the slices printed in a continuous manner, calculate the rising speed of the continuous molding printing platform according to the Lambert-Beer law, and write it into the printing configuration file;
[0091] Step 500: According to the slice printing mode obtained in step 300, take the slice printed in a layered manner, calculate the relationship between its resin leveling time and other control parameters, and obtain the expression of the layered resin curing time according to the Jacobs working curing curve, and write the obtained control parameters into the printing configuration file;
[0092] Step 600: Before printing begins, the printing origin is determined by camera monitoring, and then printing is completed according to the printing configuration file.
[0093] The processing step 100 includes:
[0094] Sub-step 110, slicing the 3D model to be printed, at which point only pixels with a grayscale of 255 are pixels to be exposed, and an area with a pixel grayscale value of 255 is taken as the printable area of the slice;
[0095] Sub-step 120: Detect the printable areas of different slices, determine the four points of the upper left corner, lower left corner, upper right corner and lower right corner, connect them into a closed area S, and obtain the pixel point closest to the center point of the printable area among the non-edge points, record these distance values and compare them to obtain the maximum value D of the minimum distance corresponding to different slices i MAX [i].
[0096] Further, step 200 includes:
[0097] Sub-step 210: Based on the standard solver of the open source CFD software OpenFOAM and the VoF model, establish Figure 3 The liquid-liquid two-phase flow printing scene shown includes a liquid-liquid two-phase flow printing scene including fluorinated oil 1010 , resin 1020 , a printing object 1030 , a printing platform 1040 and a resin tank 1050 .
[0098] Sub-step 220, setting the resin tank, printing platform and printing object as rigid materials, setting the contact boundary between the resin tank and the fluorinated oil and resin as a solid wall boundary, setting the contact surface between the printing platform and the printing object and the resin and fluorinated oil as a linear sliding boundary, and setting the boundary between the resin and the fluorinated oil as a no-slip boundary.
[0099] Further, step 300 includes:
[0100] Sub-step 310: The resin has the same flow characteristics in any direction in the printing model and the gap between the fluorinated oil. Figure 3 The Cartesian coordinate system of resin flow shown is used to analyze the resin moving in the x-axis direction;
[0101] Sub-step 310: The resin has the same flow characteristics in any direction in the printing model and the gap between the fluorinated oil. Figure 4 The resin flow Cartesian coordinate system shown, 3010 is fluorinated oil, 3020 is resin, and 3030 is the printed object.
[0102] Sub-step 320, the resin flows in the gap between the printed model and the fluorinated oil, and its Reynolds number is less than 1, which conforms to the laminar flow between the plates and the Poiseuille flow, and has the NS equation:
[0103]
[0104] The origin of y is the interface between the fluorinated oil and the resin, indicating the distance from this interface. The origin of x is the interface between the fluorinated oil and the resin perpendicular to the edge of the printed object, indicating the distance of the resin filling. There are boundary conditions:
[0105]
[0106] Where u is the maximum speed of the resin moving in the x-axis direction, u s is the slip velocity, H s is the height of the printing platform, dp / dx is the pressure gradient, μ1 is the viscosity of the resin, and the integral of formula (1) is:
[0107]
[0108] Here C1 and C2 are constants. Substituting the boundary condition (3) into (1), we can obtain:
[0109]
[0110] C2=0#(5)
[0111]
[0112] According to the linear sliding setting of the scene, we can get:
[0113]
[0114] Where D s is the slip length, according to equations (1)(4)(7):
[0115]
[0116]
[0117] According to formula (9), the volume flow Q between the printed model with a width of W and the fluorinated oil can be obtained as:
[0118]
[0119] The average flow rate of photosensitive resin is:
[0120]
[0121] During the time t1 when the platform rises, the resin fills the distance L in one direction. r Relationship with time variable t:
[0122]
[0123] v m is the speed of the printing platform during the rising process, t1 is the filling distance L r The resin filling time is the time for continuous printing.
[0124] Sub-step 330: The boundary between continuous printing and layered printing needs to determine the maximum filling distance of the resin for continuous printing, which must be less than D MAX [i], then the time required for single frame playback is 1 / f n The gap left after the printing platform rises is completely filled, and at the same time, the resin filling the gap can be completely cured before the next frame of the image is played. In the continuous printing, the rising speed of the printing platform is slow. Combined with formula (12), we have:
[0125]
[0126] The maximum filling distance of continuous printing resin can be obtained, and the corresponding D MAX [i]′:
[0127]
[0128] Therefore, if the slice D MAX [i]>D MAX [i]′ then this slice is printed using layered molding. If the slice D MAX [i]≤D MAX [i]′ then adopts continuous molding printing, such as Figure 4 It is the layered and continuous confirmation result of the tower model, where 3010 is the continuous molding and printing slice layer, and 3020 is the layered molding and printing slice layer.
[0129] The definitions of continuous molding and layered molding are as follows:
[0130] Continuous molding, i.e. surface exposure, the printer continuously rises and does not stop or fall, and it takes a short time to print one layer, which is suitable for D MAX [i] Smaller slice layer; layered molding means that after printing a layer of image with a grayscale of 0, the printing platform rises and then falls. At this time, the photosensitive resin has been fully leveled and is suitable for D MAX [i] Larger slice layers.
[0131] The step 400 includes:
[0132] Sub-step 410, taking the slices of the continuous molding print obtained in step 300, according to the Lambert-Beer law:
[0133]
[0134] Where P(z) is the optical power at a depth z away from the printing interface. The unit of depth z is μm and the unit of optical power is mW / cm 2 , Po is the power at the curing interface, which is the interface between the resin and the fluorinated oil. Therefore, the critical curing energy E of the slice at z is c have:
[0135]
[0136] Under the premise of ensuring curability, the printing platform rise speed v of continuous printing m The relationship with the maximum curable layer thickness z is:
[0137]
[0138] Sub-step 420: Determine the thickness of the slice layer to be printed according to the user's printing needs, calculate the rising speed of the continuous printing platform according to formula (17), and write the rising speed of the continuous printing platform and its corresponding slice layer number into the printing configuration file.
[0139] The step 500 includes:
[0140] Sub-step 510: Take the slices of the layered molding print obtained in step 300, and the resin is r Flow to D MAX The time of [i] is recorded as t2, and according to formula (12):
[0141]
[0142] The time T for resin filling in layered printing is recorded as:
[0143]
[0144] According to formula (19), the slip length D s Much smaller than the printing platform lifting height H s , so it is believed that (H s -D s ) / (H s -4D s ) is a constant C3 greater than 1, then the relationship between the optimal lifting height of the printing platform and the resin filling time T when the resin filling time of layered printing is the minimum is:
[0145]
[0146] At this time, the obtained H s Optimal lifting height for layered printing;
[0147] Sub-step 520: Establishing a resin curing time model based on Jacobs working curing curve:
[0148]
[0149] Among them C d is the curing depth, D p is the penetration depth, E o is the accumulated illumination energy of the DLP light source at the curing interface, E c It is the critical exposure for resin curing under UV light. The unit of curing depth and transmission depth is μm, and the unit of light energy is mw / cm 2 The unit of critical exposure is mw / cm 2 Therefore, for slices with different layer thicknesses printed in layers, the curing time t3 can be expressed as:
[0150]
[0151] Sub-step 530, determine the thickness of the slice layer to be printed according to the user's printing needs, calculate the optimal lifting height of the layered molding printing platform according to formula (20), and the rising speed of the printing platform can also be obtained based on this. Determine the layered molding resin curing time according to formula (22), and write the optimal lifting height of the printing platform, the rising speed of the printing platform, the resin curing time and the corresponding slice layer number into the printing configuration file.
[0152] The step 600 includes:
[0153] Sub-step 610: before printing, add fluorinated oil into the printing resin tank, pour photosensitive resin on top, and place the light source under the resin tank. Because fluorinated oil is a colorless liquid and photosensitive resin is a colored liquid, a camera can be used to monitor the printing origin from the side before printing starts to ensure that the printing platform is lowered to a place one slice layer thickness away from the fluorinated oil interface;
[0154] Sub-step 620, loading the printing configuration file obtained in step 400 and step 500, and starting model printing.
[0155] A fast DLP 3D printing control parameter optimization method combining continuous and layered molding according to an embodiment of the present invention has the following advantages:
[0156] 1) Using the proposed method, a set of optimal control parameters can be quickly designed for different models by combining continuous and layered molding methods for DLP 3D printing based on liquid-liquid interface;
[0157] 2) Portability. The method of this patent can simulate the motion characteristics of the interface between resin and fluorinated oil. By setting different parameters, the real printing process can be approached as close as possible to obtain simulation results such as resin filling time. At the same time, this method is not only applicable to liquid-liquid printing scenarios, but also can be applied to other DLP 3D printing scenarios by modifying the material represented by the fluorinated oil and the boundary conditions of the contact surface with the resin;
[0158] 3) Printability: The method of combining layered printing with continuous printing can be applied to most models. Therefore, the present invention has high theoretical significance and application value.
Claims
1. A method for optimizing control parameters of fast DLP 3D printing combining continuous and layered molding, characterized in that: The following steps are involved: Step 100: Slice the 3D model to be printed to obtain the number of slices i, determine the printable area of each slice, and calculate the maximum value D of the shortest distances from all points in the printable area of each slice to its boundary points. MAX [i]; Step 200, based on the standard solver of the open source computational fluid dynamics (CFD) software OpenFOAM, according to the liquid-liquid two-phase flow printing scenario of resin-fluorinated oil, a fluid volume VoF model is used to establish a numerical simulation model; Step 300: Establish a Cartesian coordinate system according to the printing scene, based on the D obtained in step 100. MAX [i] and the numerical simulation model established in step 200, using Poiseuille flow characteristics analysis to obtain the printing mode of each slice; Step 400, according to the slice printing mode obtained in step 300, take the slices printed in a continuous manner, calculate the rising speed of the continuous molding printing platform according to the Lambert-Beer law, and write it into the printing configuration file; Step 500: According to the slice printing mode obtained in step 300, take the slice printed in a layered manner, calculate the relationship between its resin leveling time and other control parameters, and obtain the expression of the layered resin curing time according to the Jacobs working curing curve, and write the obtained control parameters into the printing configuration file; Step 600: Before printing begins, the printing origin is determined by camera monitoring, and then printing is completed according to the printing configuration file; Step 300 is specifically as follows: The resin has the same flow characteristics in any direction in the printed model and the gap between the fluorinated oil, and a Cartesian coordinate system is established according to the printing scene; The Reynolds number of the resin flowing in the gap between the printed model and the fluorinated oil is less than 1, which conforms to the laminar flow between the plates and the Poiseuille flow, and has the NS equation: The origin of y is the interface between the fluorinated oil and the resin, indicating the distance from this interface. The origin of x is the interface between the fluorinated oil and the resin perpendicular to the edge of the printed object, indicating the distance of the resin filling. There are boundary conditions: Where u is the maximum speed of the resin moving in the x-axis direction, u s is the slip velocity, H s is the height of the printing platform, dp / dx is the pressure gradient, μ1 is the viscosity of the resin, and the integral of formula (1) is: Here C1 and C2 are constants. Substituting the boundary condition (3) into (1), we get: C2=0#(5) According to the linear sliding setting of the scene, we get: Where D s is the slip length, according to equations (1)(4)(7): According to formula (9), the volume flow Q between the printed model with a width of W and the fluorinated oil is: The average flow rate of photosensitive resin is: During the time t1 when the platform rises, the resin fills the distance L in one direction. r Relationship with time variable t: v m is the speed of the printing platform during the rising process, t1 is the filling distance L r The resin filling time is the time for continuous printing. The boundary between continuous printing and layered printing needs to determine the maximum filling distance of the resin for continuous printing, which must be less than D MAX [i], then the time required for single frame playback is 1 / f n The gap left after the printing platform rises is completely filled, and at the same time, the resin filling the gap can be completely cured before the next frame of the image is played. In the continuous printing, the rising speed of the printing platform is slow. Combined with formula (12), we have: Get the maximum filling distance of continuous printing resin, corresponding to D MAX [i]′: Therefore, if the slice D MAX [i]>D MAX [i]′ then this slice is printed using layered molding. If the slice D MAX [i]≤D MAX [i]′ uses continuous molding printing.
2. The method of claim 1, wherein: Step 100 is specifically as follows: Slice the 3D model to be printed. At this time, only the pixels with a grayscale value of 255 are the pixels to be exposed. Take the area with a grayscale value of 255 as the printable area of the slice. Detect the printable areas of different slices, determine the four points of the upper left corner, lower left corner, upper right corner and lower right corner, connect them into a closed area S, and obtain the pixel point closest to the center point of the printable area among the non-edge points, record these distance values and compare them to obtain the maximum value D of the minimum distance corresponding to different slices i MAX [i].
3. The method of claim 1, wherein: Step 200 is specifically as follows: According to the standard solver of the open source CFD software OpenFOAM, and using the VoF model, a liquid-liquid two-phase flow printing scenario including the resin tank, printing platform, printing object, resin and fluorinated oil is established; At the same time, the resin tank, printing platform and printing object are set as rigid materials, the boundary where the resin tank contacts the fluorinated oil and resin is set as a solid wall boundary, the surface where the printing platform and printing object contact the resin and fluorinated oil is set as a linear sliding boundary, and the boundary between the resin and the fluorinated oil is a no-slip boundary.
4. The method of claim 1, wherein: Step 400 is specifically as follows: Take the slice of the continuous molding print obtained in step 300, according to the Lambert-Beer law: Where P(z) is the optical power at a depth z away from the printing interface. The unit of depth z is μm and the unit of optical power is mW / cm 2 , P o is the power at the curing interface, which is the interface between the resin and the fluorinated oil. Therefore, the critical curing energy E of the slice at z is c have: Under the premise of ensuring curability, the printing platform rise speed v of continuous printing m The relationship with the maximum curable layer thickness z is: The thickness of the slice to be printed is determined according to the user's printing needs, and the rising speed of the continuous printing platform is calculated according to formula (17). The rising speed of the continuous printing platform and its corresponding slice layer number are written into the printing configuration file.
5. The method of claim 1, wherein: Step 500 is specifically as follows: Take the slice of the layered molding print obtained in step 300, and the resin is r Flow to D MAX The time of [i] is recorded as t2, and according to formula (12): The time T for resin filling in layered printing is recorded as: According to formula (19), the slip length D s Much smaller than the printing platform lifting height H s , so it is believed that (H s -D s ) / (H s -4D s ) is a constant C3 greater than 1, then the relationship between the optimal lifting height of the printing platform and the resin filling time T when the resin filling time of layered printing is the minimum is: At this time, the obtained H s Optimal lifting height for layered printing; The resin curing time model was established based on the Jacobs working curing curve: Among them C d is the curing depth, D p is the penetration depth, E o is the accumulated illumination energy of the DLP light source at the curing interface, E c It is the critical exposure for resin curing under UV light. The unit of curing depth and transmission depth is μm, and the unit of light energy is mw / cm 2 The unit of critical exposure is mw / cm 2 Therefore, for slices with different layer thicknesses printed in layers, the curing time t3 is expressed as: The thickness of the slice to be printed is determined according to the user's printing needs. The optimal lifting height of the layered molding printing platform is calculated according to formula (20). The rising speed of the printing platform can also be obtained based on this. The resin curing time of the layered molding is determined according to formula (22). The optimal lifting height of the printing platform, the rising speed of the printing platform, the resin curing time and the corresponding slice layer number are written into the printing configuration file.
6. The method of claim 1, wherein: Step 600 is specifically as follows: Before printing, add fluorinated oil into the printing resin tank, pour photosensitive resin on top, and place the light source under the resin tank. Because fluorinated oil is a colorless liquid and photosensitive resin is a colored liquid, a camera is used to monitor the printing origin from the side before printing begins to ensure that the printing platform is lowered to a place one slice layer thickness away from the fluorinated oil interface; The printing configuration files obtained in steps 400 and 500 are loaded, and the model printing is started.
Citation Information
Patent Citations
Mechanical movement system and method for surface exposure rapid prototyping
CN108501362A
Model-adaptive rapid surface exposure 3D printing method
CN114290682A
Multi-resolution photocuring 3D printing system and edge optimization printing method
CN114407349A
Method of dynamically adjusting lifting parameter
US20200081351A1