Article with a single-layer or multi-layer matrix having elastic properties, method for producing the article and use of aluminum hydroxide as reinforcing filler in rubber mixtures

By reducing the carbon black ratio in the rubber mixture and replacing carbon black with aluminum hydroxide, combined with chloroprene rubber, the problem of mechanical characteristics deterioration in the existing rubber mixture when improving fire resistance is solved, achieving higher durability and Vibration damping effect.

CN115244122BActive Publication Date: 2024-11-22GMT GUMMI METALL TECHNIK GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202080088811.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2019-12-20
Filing Date
2020-12-18
Publication Date
2024-11-22
Estimated Expiration
2040-12-18

AI Technical Summary

Technical Problem

While improving fire resistance, existing rubber mixtures lead to deterioration of tensile strength, elasticity, shrinkage behavior and fatigue resistance, and have poor durability under high mechanical loads, making it difficult to meet the elastic support and vibration damping requirements of vehicle structures.

Method used

By reducing the carbon black ratio in the rubber mixture to less than 5 phr and replacing the carbon black with aluminum hydroxide as a reinforcement filler, combining chloroprene rubber to form a multilayer matrix, the mechanical properties and fire resistance of the rubber mixture are optimized.

Benefits of technology

It achieves lower flammability and higher elongation of break, improves vibration damping characteristics and service life, and meets the durability requirements of high mechanical loads and improves the overall performance of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115244122B_ABST
    Figure CN115244122B_ABST
Patent Text Reader

Abstract

The invention relates to an article (100), in particular an air spring bellows (100), having a single-layer or multi-layer base body (8) with elastic properties, wherein at least one layer (3, 4, 5, 6, 9) of the base body (8) consists of a rubber mixture, wherein the carbon black proportion of at least one carbon black, in particular the total carbon black proportion of all carbon blacks in the rubber mixture, is less than 5 phr. The rubber mixture preferably comprises aluminum hydroxide as a reinforcing filler. The rubber mixture can have chloroprene rubber as a base polymer.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention relates to an article having a single-layer or multi-layer substrate having elastic properties.

[0002] Such articles can be configured, for example, as vibration dampers and / or metal-rubber elements. The articles can preferably be air spring bellows membranes and / or air spring bellows and / or damping elements of bearings and / or conical springs and / or laminated leaf springs.

[0003] Such products are known. Such products are known, for example, from DE 10 2017 223 538 A1.

[0004] The article with elastic properties disclosed in DE 10 2017 223 538 A1 has a base body with elastic properties, which is used for elastic support or vibration damping in vehicles, in particular in rail vehicles, and has at least one layer D composed of a rubber mixture, which contains a rubber mixture having a thickness of between 35 μm and 10 μm according to DIN-ISO 9277. 2 / g to 140m 2 At least one carbon black having a BET surface area of ​​1000 Å / g and an oil absorption number (OAN) of between 70 ml / 100 g and 140 ml / 100 g according to ISO 4656. The carbon black having the given physical properties has the function as reinforcing filler in the elastomer mixture.

[0005] Since in recent years the requirements placed on the products mentioned at the outset have been increasing with regard to the fire protection properties to be met (for example those arising from the fire protection standard EN 45545), increasingly halogen-free flame retardants in combination with carbon black of the type mentioned above have been admixed into rubber mixtures in order to be able to render the elastomers produced therefrom resistant to ignition.

[0006] Thus, it is known from DE 10 2017 223 538 A1 that the fire retardant behavior of rubber mixtures can be improved by directly mixing in a relatively large amount of flame retardant substances. However, this measure usually leads to a deterioration of the properties (such as tensile strength, elasticity, shrinkage behavior (Setzungsverhalten) and fatigue strength) related to use in dynamic applications in the mixture involved. In the products involved, this is particularly manifested as a significant deterioration of elastic support properties, shrinkage properties or vibration properties. In addition, such products have poor durability under high mechanical loads, so that their maximum service life is relatively short.

[0007] However, it has been shown that even technical embodiments of products of the type mentioned at the outset described in DE 10 2017 223 538 A1 always have unfavorable physical properties, which lead to relatively high wear and therefore also to insufficient elastic support properties, shrinkage properties or vibration properties after a certain period of use, in particular are not sufficient for the use of such products in vehicle construction.

[0008] It is therefore an object of the present invention to provide a product of the type mentioned at the outset which has improved usage properties compared to the solution from DE 10 2017 223 538 A1.

[0009] This object can be achieved by a product having the features according to independent claim 1 .

[0010] In order to achieve the above-mentioned purpose, the product of the type mentioned in the opening paragraph can be designed, so that the product is characterized in that at least one layer of the matrix is ​​composed of a rubber mixture, wherein the carbon black ratio of at least one carbon black in the rubber mixture is less than 5phr. The carbon black ratio is preferably based on the total carbon black ratio of all carbon blacks in the rubber mixture. The rubber mixture may not have carbon black, have one carbon black or have more than one carbon black. Reducing the carbon black ratio to less than 5phr has the following advantages: the flammability of the matrix is ​​improved relative to the matrix prepared based on the technical teaching of DE 10 2017 223 538 A1. Therefore, it is possible to achieve a reduction in the flammability of the at least one layer, because the carbon black ratio as the combustible part of the rubber mixture has been reduced relative to the known composition. In addition to lower flammability, reducing the carbon black ratio also unexpectedly leads to a higher elongation at break, that is, the material can be stretched to a greater extent. This has the following advantages in air springs (i.e., air spring airbags): improved damping properties and increased service life can be achieved.

[0011] DE 10 2017 223 538 A1 and the present invention both aim to ensure the best possible fire resistance for metal-rubber elements. However, the two take diametrically opposite approaches. DE 10 2017 223 538 seeks the solution described therein, namely to fix the carbon black as filler at a carbon black proportion of at least 5 phr and to find those carbon blacks with special flame retardant properties; whereas the present invention takes the approach of considering the carbon black as filler unnecessary by reducing the carbon black proportion to less than 5 phr and replacing the filler properties with aluminum hydroxide.

[0012] In the rubber chemical industry, the number of parts per hundred parts of rubber (phr) refers to the mass ratio of the individual mixture components in the elastomer mixture formulation. Here, these values ​​are respectively relative to 100 (mass) parts of a base polymer or multiple base polymers (in the case of polymer blends).

[0013] Advantageous embodiments of the invention will be described below, which, alone or in combination with features of other embodiments, can optionally be combined with the features from claim 1 .

[0014] It is particularly advantageous if the at least one layer covers at least the functional region or completely covers the layer located thereunder. The at least one layer can therefore be formed in particular to be continuous and / or non-porous.

[0015] The aluminum hydroxide may be present in the rubber mixture in a proportion of 50 to 150 phr, in particular 50 to 100 phr, in particular 100 to 150 phr, preferably 75 to 125 phr.

[0016] The total carbon black ratio can be greater than 0 phr or can also be 0 phr. The main difference between these two embodiments is that only in the former case, carbon black can play a dyeing effect, because in the latter case, the rubber mixture does not have any carbon black at all. Due to the very little carbon black ratio less than 5 phr, carbon black has no effect on the technical characteristics of the rubber mixture except dyeing. Therefore, this point is the same in these two embodiments.

[0017] It can be designed that at least one coloring agent is mixed into the rubber mixture. The coloring agent can be, for example, carbon black, iron oxide or titanium dioxide. Carbon black is dyed black, while iron oxide, for example Bayferrox 920, is usually dyed yellow. Titanium dioxide can be used to lighten the color. For dyeing red, for example, Colortherm red 520 can be used, and for dyeing blue, Oppasin blau 6900 can be used. Alternatively, it can be designed that the rubber mixture does not contain a coloring agent. In this case, no coloring agent is added to the rubber mixture at all.

[0018] According to an advantageous development, it can be provided that the at least one carbon black, preferably all carbon blacks used, in particular the carbon black admixed into the rubber mixture, has a relative humidity of 35 m / s according to DIN-ISO 9277. 2 / g to 140m 2 The BET surface area is outside the range of 35 m / g according to DIN-ISO9277. 2 / g to 140m 2Carbon black with a BET surface area of ​​35 m / g is added to the rubber mixture as a functional filler for reinforcement. A new alternative solution is to be developed to provide products of the type mentioned at the outset, wherein the use of such reinforcing carbon black fillers can be reduced or even completely omitted. 2 / g to 140m 2 In DE 10 2017 223 538 A1, the addition of such carbon black is considered a key feature of the technical teaching described therein. However, it is possible to mix other types of carbon black as a colorant in smaller amounts of less than 5 phr, i.e. carbon blacks having a BET surface area of ​​35 m / s according to DIN-ISO 9277. 2 / g to 140m 2 Carbon blacks having a BET surface area outside the range of 1.3 Å / g. Carbon blacks outside the range do not have any function as reinforcing fillers, but have particularly good coloring properties for coloring rubber mixtures black.

[0019] According to another advantageous embodiment, it can be provided that the at least one carbon black, preferably all the carbon blacks used, in particular the carbon black admixed into the rubber mixture, has an oil absorption number (OAN) outside the range of 70 ml / 100 g to 140 ml / 100 g according to ISO 4656. Similar to what has already been described in the above paragraphs with regard to the BET surface area, carbon blacks with an oil absorption number (OAN) of 70 ml / 100 g to 140 ml / 100 g according to ISO 4656 are also reinforcing carbon blacks. Since the proportion of such reinforcing carbon blacks can be reduced or even completely omitted in the composition of the rubber mixture of the at least one layer, the rubber mixture of the at least one layer contains carbon blacks with an oil absorption number (OAN) of 70 ml / 100 g to 140 ml / 100 g according to ISO 4656 only in a relatively small amount of less than 5 phr or does not contain such carbon blacks at all. The total carbon black proportion can thus be kept particularly low in order to improve the mechanical properties of the product.

[0020] The rubber mixture of at least one layer or all layers of the substrate may have only one carbon black type or may have at least two or more carbon black types. The total carbon black proportion may be less than 5 phr or have the above-mentioned properties, i.e. 35 m / s according to DIN-ISO 9277. 2 / g to 140m 2 The proportion of carbon black of a carbon black type having a BET surface area of ​​100 ml / 100 g and / or having at least one of an oil absorption number (OAN) of 70 ml / 100 g to 140 ml / 100 g may be less than 5 phr.

[0021] As described and claimed in this document, the structure of the article can be manifested in that the substrate has an inner elastomer layer, a central functional layer and an outer elastomer layer. The article usually has an air chamber, in which a positive pressure is generated in the use position. In order to be able to permanently form a positive pressure within the air chamber, the inner elastomer layer facing the air chamber is formed to be particularly airtight, especially airtight. The central functional layer is used for force transmission and, for example, influences the vibration damping properties of the article through its structure. The outer layer is used to protect the article from external influences, such as climate, oil resistance, temperature resistance, and fire protection. In particular, it can be designed that at least the outer elastomer layer and / or the inner elastomer layer have a carbon black ratio of less than five phr, preferably all layers of the substrate have a carbon black ratio of less than 5 phr. The described structure can achieve a particularly high mechanical load capacity and a particularly good vibration damping effect.

[0022] In order to further improve the mechanical load capacity, it can be designed according to another preferred embodiment that the central functional layer is formed as a capsule, in particular wherein the capsule comprises a cord fabric which is embedded in at least one sublayer of the elastomer matrix. The at least one layer mentioned above can also be understood as a sublayer as described above.

[0023] According to a particularly preferred embodiment, it can be provided that the at least one layer of the substrate or the rubber mixture has a carbon black content of a maximum of 4 phr, in particular a maximum of 3 phr, in particular a maximum of 2 phr. The carbon black content can also refer to the total carbon black content of all carbon blacks contained in the rubber mixture of the at least one layer. Such a low amount of carbon black does not affect the elasticity or mechanical properties of the substrate, but is well suited for dyeing the substrate of the article black.

[0024] In particular, it can be provided that the total carbon black proportion of the rubber mixture is so small that the elasticity and / or mechanical properties of the matrix are not influenced or are only influenced negligibly. Influence is negligible in particular when the relevant technical properties are influenced so little that they are considered irrelevant by a person skilled in the art since these properties are predetermined by the selection of the main components of the rubber mixture.

[0025] In order to form a layer with particularly low flammability, it can be provided that at least one layer of the substrate is formed by chloroprene rubber or a blend (Verschnitt) formed by chloroprene rubber and other rubbers, or includes chloroprene rubber or a blend formed by chloroprene rubber. Chloroprene rubber or the previously mentioned blend can in particular constitute the base polymer of the rubber mixture. The at least one layer can in particular be at least the outer elastomer layer. According to a particularly preferred embodiment, all layers of the substrate can be prepared from the same rubber mixture. Chloroprene rubber has particularly good combustion characteristics so that products that meet the requirements for fire protection can be formed.

[0026] In order to be able to improve the smoke toxicity in the event of a fire and at the same time also to improve the mechanical properties of the product, it has surprisingly proven to be advantageous that at least one layer of the substrate, in particular the rubber mixture, comprises aluminum hydroxide (also known as "aluminum trihydrate" and abbreviated to ATH; general formula: Al(OH)3) as a reinforcing filler and / or as a flame retardant. The aluminum hydroxide thus assumes a dual function, so that surprisingly, it is not necessary to use carbon black as a reinforcing filler in addition to ATH. The carbon black used as a reinforcing filler to date can therefore preferably be completely replaced by ATH. It is therefore not necessary to add ATH as a flame retardant and carbon black as a reinforcing filler to the rubber mixture, which improves the elastic properties of at least one layer of the substrate. In other words, a higher rubber ratio can be achieved compared to compositions in which it has not yet been recognized that ATH can also assume the function of a reinforcing filler in addition to its flame retardant effect. At the given quantitative ratios, the one or more base polymers are always set to 100 parts. In contrast, the proportion of ATH in the rubber mixture of the at least one layer can be 50 to 150 phr, in particular 50 to 100 phr, in particular 100 to 150 phr, preferably 75 to 125 phr.

[0027] The at least one layer can preferably comprise only aluminum hydroxide as reinforcing filler. The at least one layer can in particular be the outer elastomer layer or all layers of the base body.

[0028] According to a particularly advantageous embodiment, it can be provided that the article is a vibration damper and / or a metal-rubber element, preferably selected from the group consisting of an air spring bellows membrane, an air spring bellows, a damping element for a bearing, a conical spring and / or a laminated leaf spring. Particularly preferably, the article is an air spring bellows and / or an air spring bellows membrane.

[0029] Therefore, in order to achieve the above-mentioned objects, in particular, an article of the type mentioned at the outset can be provided, which is formed as an air spring bellows with a multilayer base body, which has elastic properties, wherein the base body has an inner elastomer layer, a central functional layer and an outer elastomer layer. It can be provided that the inner elastomer layer, the functional layer and the outer elastomer layer consist of the same rubber mixture, which contains aluminum hydroxide as a reinforcing filler and the total carbon black proportion of all carbon blacks in the rubber mixture is less than 5 phr. The rubber mixture preferably contains chloroprene rubber or a blend with chloroprene rubber.

[0030] In the case of air spring bellows, if present, the outer elastomer layer is used as a fireproof covering sublayer in any case, whereas the rubber matrix of the functional layer contains a special rubber mixture which does not ensure fire protection. The peculiarity of the above-described solution is that all three layers of the air spring bellows are implemented with the aid of the same mixture containing aluminum hydroxide, thereby achieving a continuous and homogeneous rubber matrix. It is known that the air spring bellows obtained surprisingly meet the highest level of fire protection requirements. The use of a homogeneous rubber matrix is ​​advantageous for a number of reasons. In addition to the economic advantages resulting from the simplified bellows production, there are also technical advantages, since, for example, the layers can be optimally crosslinked with one another.

[0031] The air spring bag usually has two flanges. The flanges enable connection to the connecting components. The flanges can be reinforced with flange cores respectively. The flanges can be connected via an air spring bag membrane. The air spring bag membrane usually consists of an inner elastomer layer (to ensure air tightness), an outer elastomer layer (to protect from environmental influences) and a functional layer. The functional layer generally comprises a cord fabric as a strength carrier and an elastomer matrix, which is used to embed the cord fabric and to cross-link the functional layer with the inner and outer layers. The air spring support function is basically achieved by an air chamber that is airtightly enclosed and works under positive pressure.

[0032] The above-mentioned object is also achieved by a method having the features of the parallel method claim.

[0033] To achieve the object, a method can be devised for producing an article having a single-layer or multi-layer matrix having elastic properties, the matrix being formed in particular from a rubber mixture as described and / or claimed herein, wherein aluminum hydroxide as a reinforcing filler and at least one carbon black as a colorant are admixed into the rubber mixture. It is thus possible to form an article having improved mechanical properties compared to the article from DE 10 2017 223 538 A1, which article also meets the fire protection requirements according to the fire protection standard EN 45545.

[0034] In order to achieve the above-mentioned object, a method can also be proposed to prepare an air spring bellows with a multilayer substrate, the substrate having elastic properties, wherein the substrate has an inner elastomer layer, a central functional layer and an outer elastomer layer. It can be provided that the inner elastomer layer, the functional layer and the outer elastomer layer are prepared from the same rubber mixture, aluminum hydroxide is mixed into the rubber mixture as a reinforcing filler and the total carbon black proportion of all carbon blacks in the rubber mixture is less than 5 phr. The air spring bellows is preferably formed in the manner described above and / or according to the claims for the air spring bellows. As described above, the total carbon black proportion can be 0 phr or greater than 0 phr.

[0035] Preferably, chloroprene rubber or a blend of chloroprene, in particular chloroprene rubber, is admixed to the rubber mixture as base polymer.

[0036] In addition, it is preferably designed that at least one colorant is mixed into the rubber mixture. The colorant can be formed, for example, as previously described. In particular, exactly one colorant, a plurality of colorants and / or a colorant mixture can be mixed. Alternatively, it can be designed that the rubber mixture does not contain a colorant. In this case, no colorant is mixed into the rubber mixture at all.

[0037] The objects mentioned above are also achieved by the use according to the parallel use claim.

[0038] To achieve this object, it can be proposed to use aluminum hydroxide as a reinforcing filler in a rubber mixture, in particular for forming at least one layer of a matrix, preferably a matrix of an article, as described and / or claimed herein. By using ATH instead of carbon black as a filler, the rubber proportion required for forming elastic properties can be higher than the solution from DE 10 2017223 538 A1.

[0039] It may also be provided that aluminum hydroxide is used as a reinforcing filler in a rubber mixture in order to form a base body of an air spring bellows, in particular wherein the air spring bellows is formed as described above or in accordance with one of the claims for an air spring bellows.

[0040] The invention will now be explained in more detail with reference to a number of embodiments, but the invention is not restricted to these embodiments. Further embodiments result from the combination of features of one or more claims with one another and / or with one or more features of the embodiments. Description of the drawings:

[0041] Figure 1 A longitudinal section through a possible embodiment variant of the article according to the invention, which is designed here as an air spring bellows, wherein the arrow points to a detailed view of the section through a layer of a base body of the air spring bellows membrane;

[0042] Figure 2 A perspective view of a possible embodiment variant of a product designed as an air spring bellows membrane is shown.

[0043] exist Figure 1 and Figure 2 1 and 2 , an article is shown which is designated as a whole by 100 , wherein the exemplary embodiment shown shows an air spring bellows 11 and an air spring bellows membrane 10 .

[0044] The article 100 has at least one base body 8 which is designed to be at least partially elastic and thus deformable.

[0045] An air chamber 12 is at least partially delimited by the base body 8 .

[0046] The article 100 may also have at least two reinforcing elements, in particular formed of metal, which may be formed, for example, as a metal core. The reinforcing elements may be adapted to connect the article to other components, in particular by bolting and / or clamping and / or inserting.

[0047] The article 100 has two flanges 2 which are each reinforced by a flange core 1. In this case, an air spring bellows membrane 10 extends between the two flanges 2 and forms an air chamber 12 on the inside.

[0048] The base body 8 is composed of a plurality of layers 3, 4, 5, 6, 9, which can be at least partially or completely cross-linked with one another to form a composite element. In particular, relative movements between the individual layers 3, 4, 5, 6, 9 can thus be prevented.

[0049] At least one layer 3, 4, 5, 6, 9 of the matrix 8 is formed by a rubber mixture, the carbon black ratio, especially the total carbon black ratio is less than 5 phr. It can be designed that all layers are formed by the rubber mixture. Since the layers are all formed by the same rubber mixture, they constitute a uniform rubber matrix.

[0050] This may be, for example, any carbon black or any carbon black having a carbon content of 35 m / s according to DIN-ISO 9277. 2 / g to 140m 2 / g and / or a carbon black having an oil absorption number (OAN) in accordance with ISO 4656 of 70 ml / 100 g to 140 ml / 100 g.

[0051] The addition of carbon black here only achieves the purpose of mixing carbon black as a colorant to dye the base body 8 black. If the product 100 is to obtain another color, the carbon black can be replaced by another colorant. If the color is to be removed, the carbon black or the colorant can be omitted. The elastic properties and mechanical properties of the rubber mixture are not changed.

[0052] The base body 8 comprises an inner elastomer layer 3, a central functional layer 4 and an outer elastomer layer 6. At least the outer elastomer layer 6 and / or the inner elastomer layer 3 can in particular have a carbon black content of less than 5 phr. All layers 3, 4, 5, 6, 9 of the base body 8 preferably each have a carbon black content of less than 5 phr.

[0053] The central functional layer 4 can be formed as a capsule 13. In the embodiment variant shown, the central functional layer 4 comprises at least one cord fabric 7, which is respectively embedded in a plurality of sub-layers 5 of an elastomeric matrix 9. The elastomeric matrix 9 can be formed from a plurality of sub-layers 5 of a rubber mixture as described above and further below.

[0054] The at least one layer 3, 4, 5, 6, 9 can have chloroprene rubber or a blend of chloroprene rubber and another rubber as the rubber component. The rubber component preferably consists exclusively of chloroprene rubber.

[0055] The rubber mixture of at least one layer 3, 4, 5, 6, 9 also includes aluminum hydroxide as a reinforcing filler, wherein the aluminum hydroxide also acts as a flame retardant. Here, the new situation is mainly the following unexpected discovery, that is, aluminum hydroxide can replace carbon black as a reinforcing filler. Therefore, aluminum hydroxide has a dual function as a flame retardant and a reinforcing filler. The rubber mixture can especially contain 50phr to 150phr, especially 60phr to 140phr, especially 70phr to 130phr of ATH.

[0056] The at least one layer 3 , 4 , 5 , 6 , 9 is preferably at least the outer elastomeric layer 6 .

[0057] In addition to this design, the article 100 can also be designed as an air spring bellows membrane 10 and / or an air spring bellows 11 and / or a vibration absorber and / or a metal-rubber element. The article 100 can preferably be configured as a damping element of a bearing and / or a conical spring and / or a laminated leaf spring.

[0058] In general, particle-filled polymers can be produced by means of reinforcing fillers, wherein, depending on the filler volume fraction, an increase in the elastic modulus is achieved. It is therefore necessary to use a certain amount of such fillers when producing elastomers in order to adjust the hardness, abrasion resistance and tearing behavior.

[0059] Reference numerals list

[0060] 100 Products

[0061] 1 Flange core

[0062] 2 Flange

[0063] 3 Inner elastomer layer

[0064] 4 Functional Layer

[0065] 5 Sublayer

[0066] 6 Outer elastomer layer

[0067] 7 Cord fabric

[0068] 8 Matrix

[0069] 9 Elastomer matrix

[0070] 10 Air spring bellows membrane

[0071] 11 Air spring airbag

[0072] 12 Air Chamber

[0073] 13. Cyst

Claims

1. An air spring bellows (100) having a multi-layer base body (8) with elastic properties, wherein the base body (8) has an inner elastomer layer (3), a central functional layer (4) and an outer elastomer layer (6), characterized in that: The inner elastomer layer (3), the functional layer (4) and the outer elastomer layer (6) consist of the same rubber mixture, the rubber mixture contains only aluminum hydroxide as a reinforcing filler and the total carbon black content in the rubber mixture is less than 5 phr, The central functional layer (4) is formed as a capsule (13), wherein the capsule (13) comprises a cord fabric (7) embedded in at least one sublayer (5) of an elastomeric matrix (9); And the aluminum hydroxide has a ratio of 50 phr to 150 phr in the rubber mixture, the rubber mixture includes chloroprene rubber or a blend formed of chloroprene rubber as a base polymer, and the air spring bellows (100) is a metal-rubber element.

2. The air spring bellows (100) according to claim 1, characterized in that: The aluminum hydroxide has a proportion of 50 to 100 phr in the rubber mixture.

3. The air spring airbag (100) according to claim 1, characterized in that: The aluminum hydroxide has a proportion of 100 to 150 phr in the rubber mixture.

4. The air spring airbag (100) according to claim 1, characterized in that: The aluminum hydroxide has a proportion of 75 phr to 125 phr in the rubber mixture.

5. The air spring bellows (100) according to any one of claims 1 to 4, characterized in that The total carbon black ratio is 0 phr.

6. The air spring bellows (100) according to any one of claims 1 to 4, characterized in that The total carbon black ratio is greater than 0 phr.

7. The air spring bellows (100) according to any one of claims 1 to 4, characterized in that At least one colorant is admixed into the rubber mixture.

8. The air spring bellows (100) according to claim 7, characterized in that: The at least one colorant is carbon black, iron oxide or titanium dioxide.

9. The air spring bellows (100) according to any one of claims 1 to 4, characterized in that The carbon black admixed into the rubber mixture has a carbon black content of 35 μm according to DIN-ISO 9277. 2 / g to 140m 2 / g, and / or The carbon black admixed into the rubber mixture has an oil absorption number (OAN) according to ISO 4656 outside the range of 70 ml / 100 g to 140 ml / 100 g.

10. The air spring bellows (100) according to any one of claims 1 to 4, characterized in that The total carbon black proportion of all carbon blacks in the rubber mixture is a maximum of 4 phr.

11. The air spring bellows (100) according to any one of claims 1 to 4, characterized in that The total carbon black proportion of all carbon blacks in the rubber mixture is a maximum of 3 phr.

12. The air spring bellows (100) according to any one of claims 1 to 4, characterized in that The total carbon black proportion of all carbon blacks in the rubber mixture is a maximum of 2 phr.

13. The air spring bellows (100) according to any one of claims 1 to 4, characterized in that The air spring bag (100) is a shock absorber, and / or the air spring bag (100) comprises an air spring bag membrane (10).

14. Method for producing an air spring bellows (100) according to claim 1 with a multi-layer base body (8) having elastic properties, wherein the base body (8) has an inner elastomer layer (3), a central functional layer (4) and an outer elastomer layer (6), characterized in that: The inner elastomer layer (3), the functional layer (4) and the outer elastomer layer (6) are produced from the same rubber mixture, aluminum hydroxide is mixed into the rubber mixture as a reinforcing filler so that the rubber mixture contains only aluminum hydroxide as a reinforcing filler and the total carbon black content in the rubber mixture is less than 5 phr; The aluminum hydroxide has a ratio of 50 to 150 phr in the rubber mixture, the rubber mixture is mixed with chloroprene rubber or a blend formed of chloroprene rubber as a base polymer, and the air spring bellows (100) is a metal-rubber element.

15. The method according to claim 14, characterized in that At least one colorant is admixed into the rubber mixture.

16. The method according to claim 15, characterized in that The at least one colorant is carbon black, iron oxide or titanium dioxide.

17. The method according to any one of claims 14 to 16, characterized in that No carbon black was admixed to the rubber mixture.

18. Use of aluminum hydroxide as a reinforcing filler in a rubber mixture for forming a base body (8) of an air spring bellows, wherein the air spring bellows is designed according to one of claims 1 to 13.