A method for preparing hexene and co-producing octene and decene by oligomerization

By changing the catalyst components and introducing butene in the ethylene oligomerization process, the problem that it is difficult to produce hexene, octene and decene in high yields simultaneously with the existing technology has been solved, and high-selectivity co-production and proportion control have been achieved, meeting the needs of demand for high value-added products.

CN115246759BActive Publication Date: 2024-10-29PETROCHINA CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202110463473.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-04-27
Publication Date
2024-10-29
Estimated Expiration
2041-04-27

AI Technical Summary

Technical Problem

The existing ethylene oligomerization process is difficult to produce high value-added hexene, octene and decene products at high yields at the same time.

Method used

Based on the process of ethylene oligomerization to produce hexene catalyzed by chromium-based catalysts, some catalyst components are changed, butene is introduced as raw material, and the ratio of hexene, octene and decene in the product is controlled by adjusting the raw material ratio to achieve Highly selective cogeneration.

Benefits of technology

It achieves the oligomerization of ethylene to produce hexene while co-producing octene and decene with high selectivity. The proportion of products can be controlled by adjusting the catalyst components and process conditions to meet the demand for high value-added products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0003041696080000081
    Figure BDA0003041696080000081
Patent Text Reader

Abstract

The present invention relates to a method for preparing hexene by oligomerization and co-producing octene and decene, which comprises the following steps: ethylene and butene undergo oligomerization reaction under the action of a catalyst to obtain hexene, octene and decene products, the catalyst comprising: a chromium source, a ligand and an organic aluminum compound, the molar ratio of the three being 1:1-20:1-500; the ligand is selected from heterocyclic compounds, the general formula of which is XRn, wherein X is a five-membered heterocycle, R is selected from substituted or unsubstituted straight-chain alkanes, substituted or unsubstituted branched alkanes, substituted or unsubstituted cycloalkanes, substituted or unsubstituted aromatics, and n is 1-5. The method of the present invention is based on the process of producing hexene by ethylene oligomerization catalyzed by a chromium-based catalyst, and without changing the process flow of producing hexene by ethylene oligomerization, by changing part of the catalyst components and introducing butene as a raw material, the purpose of producing hexene by ethylene oligomerization and co-producing octene and decene with high selectivity can be achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of petrochemical technology, and in particular to a method for producing hexene and octene by polymerization of ethylene. Background Art

[0002] Hexene, octene and decene are very useful organic chemical raw materials with wide applications. Hexene-1 is the main comonomer for synthesizing high value-added, high-performance linear low-density polyethylene (LLDPE) and high-density polyethylene (HDPE). Hexene-1 copolymer products have the advantages of high tensile strength, strong impact resistance and tear resistance. At present, 66% of octenes on the market are used as comonomers of LLDPE, and more than 33% of octenes are used to produce high-quality plasticizers, detergents and lubricants. Decene is the main raw material for synthesizing poly-alpha-olefin lubricants (PAO). According to statistics, more than 85% of the PAO base oils currently on the market use decene as raw materials. Compared with traditional mineral lubricant base oils (Class I, II and III base oils), this type of lubricant base oil has good stability and can be used as internal combustion engine oil, gear oil, refrigeration oil, high-viscosity aviation lubricant, long-life lubricant, metalworking fluid, etc. in cold and extremely cold regions. It is not only widely used in civil industries such as automobiles and industry, but also the main source of high-grade lubricant base oils used in aviation, aerospace, military and other industries.

[0003] Since Union Carbide reported the method of synthesizing hexene by catalyzing the polymerization of ethylene with chromium-based catalysts, many patents at home and abroad have reported the method of preparing hexene with chromium-based catalysts. Among them, the hexene production technologies developed by Philips and China Petroleum and Chemical Research Institute have been successfully industrialized. Their process flow is comprehensive and the technology is advanced, and they can produce high-quality hexene products that meet the requirements of polyethylene comonomers.

[0004] CN105228973A discloses an ethylene oligomerization method, wherein ethylene is mainly oligomerized into hexene or octene, or a mixture of hexene and octene. The catalyst is a chromium source, a diphosphorus coordination compound and an optional activator, and catalyzes the ethylene oligomerization under appropriate reaction conditions.

[0005] In the ethylene polymerization process of WO2004 / 05647, the ligand is changed so that the octene content reaches 69% and the hexene content is 10-20%.

[0006] EP 0608447A reports a chromium-based catalytic system as a catalyst for ethylene polymerization, which contains a chromium-containing compound, a pyrrole compound, an aluminum-containing co-catalyst, and a halogen-containing compound as a promoter. The catalyst has a high selectivity for hexene-1 and produces 3% decene.

[0007] However, the above disclosed production methods are unable to simultaneously produce high value-added hexene, octene and decene products in high yield. Summary of the invention

[0008] Based on the above, the purpose of the present invention is to provide a method for preparing hexene by polymerization of ethylene and butene and co-producing octene and decene. The method of the present invention is based on the process of producing hexene by polymerization of ethylene catalyzed by chromium-based catalysts. Without changing the process flow of producing hexene by polymerization of ethylene, the method changes part of the catalyst components and introduces butene as a raw material, so that the purpose of producing hexene by polymerization of ethylene and co-producing octene and decene with high selectivity can be achieved. At the same time, the ratio of hexene: octene: decene in the product can be controlled by adjusting the raw material ratio.

[0009] To this end, the present invention provides a method for preparing hexene by polymerization and producing octene and decene, comprising the following steps: ethylene and butene undergo polymerization reaction under the action of a catalyst to obtain hexene, octene and decene products, the catalyst comprising: a chromium source, a ligand and an organic aluminum compound, the molar ratio of the three being 1:1-20:1-500, preferably, the amount of the catalyst used is 0.02mmol / L-0.50mmol / L in terms of chromium element concentration;

[0010] The ligand is selected from heterocyclic compounds, and its general formula is XRn, wherein X is a five-membered heterocycle, R is selected from substituted or unsubstituted straight-chain alkanes, substituted or unsubstituted branched alkanes, substituted or unsubstituted cycloalkanes, substituted or unsubstituted aromatics, and n is 1-5.

[0011] Specifically, in the method provided by the present invention, within the ratio range of each component of the catalyst, raw materials ethylene and butene undergo oligomerization reaction under the action of the catalyst, and the reaction product is mainly hexene, while octene and decene are co-produced.

[0012] In the method for preparing hexene by oligomerization and co-producing octene and decene of the present invention, it is preferred that n is 1-2.

[0013] In the method for preparing hexene and co-producing octene and decene by oligomerization of the present invention, it is preferred that the molar ratio of the chromium source, the ligand and the organoaluminum compound is 1:1-5:100-200.

[0014] In the method for preparing hexene by oligomerization and co-producing octene and decene described in the present invention, it is preferred that the chromium source is selected from at least one of tetrahydrofuran chromium trichloride, chromium octoate, chromium trichloride, chromium acetylacetonate, chromium 2-ethylhexanoate and chromium acetate.

[0015] In the method for preparing hexene by oligomerization and co-producing octene and decene of the present invention, it is preferred that the chromium source is at least one selected from tetrahydrofuran chromium trichloride, chromium 2-ethylhexanoate, and chromium acetylacetonate.

[0016] In the method for preparing hexene by oligomerization and co-producing octene and decene of the present invention, it is preferred that X is furan, thiophene or pyrrole.

[0017] In the method for preparing hexene by oligomerization and co-producing octene and decene described in the present invention, it is preferred that R is a branched alkane.

[0018] In the method for preparing hexene by oligomerization and co-producing octene and decene described in the present invention, it is preferred that R is methyl, ethyl or tert-butyl.

[0019] In the method for preparing hexene by polymerization and co-producing octene and decene described in the present invention, it is preferred that the organic aluminum compound is selected from at least one of trimethyl aluminum, triethyl aluminum, triisobutyl aluminum, tri-n-hexyl aluminum, diethyl aluminum monochloride and ethyl aluminum dichloride.

[0020] In the method for preparing hexene by oligomerization and co-producing octene and decene described in the present invention, it is preferred that the organic aluminum compound is selected from at least one of triethylaluminum, diethylaluminum monochloride and ethylaluminum dichloride.

[0021] In the method for preparing hexene by polymerization and co-producing octene and decene of the present invention, it is preferred that the organoaluminum compound is a composition of non-halogen alkyl aluminum and halogen-containing alkyl aluminum, wherein the molar ratio of halogen-containing alkyl aluminum to non-halogen alkyl aluminum is 1:1-50.

[0022] In the method for preparing hexene by oligomerization and co-producing octene and decene of the present invention, preferably, the molar ratio of ethylene to butene is 1:1-20.

[0023] The method for preparing hexene by oligomerization and co-producing octene and decene of the present invention is preferably carried out in an inert solvent, and the inert solvent is an alkane, an aromatic hydrocarbon, a halogenated hydrocarbon or an olefin.

[0024] In the method for preparing hexene and co-producing octene and decene by polymerization of the present invention, preferably, the alkane is n-hexane, methylcyclohexane, cyclohexane, heptane or decane; the aromatic hydrocarbon is benzene, toluene, xylene or isopropylbenzene; and the olefin is butene-1, hexene-1 or octene-1.

[0025] The method for preparing hexene and co-producing octene and decene by oligomerization of the present invention specifically comprises the following steps:

[0026] Add inert solvent and catalyst into the reactor, introduce butene as the second reaction monomer, the molar ratio of ethylene to butene is 1:1-20, when the temperature rises to the reaction temperature of 50-150°C, introduce ethylene to 3-5MPa, the reaction time is 0.5-5h, collect the product and calculate the selectivity of each component. The amount of catalyst is calculated as chromium element, and the concentration range is 0.02mmol / L-0.5mmol / L.

[0027] The method of the present invention is based on the process of producing hexene by ethylene polymerization catalyzed by chromium-based catalysts. Under the premise of not changing the process flow of producing hexene by ethylene polymerization, some catalyst components are changed and butene is introduced as a raw material, so that the purpose of producing hexene by ethylene polymerization and simultaneously co-producing octene and decene with high selectivity can be achieved. At the same time, the ratio of hexene: octene: decene in the product can be controlled by adjusting the raw material ratio. DETAILED DESCRIPTION

[0028] The following is a detailed description of the embodiments of the present invention: This embodiment is implemented on the premise of the technical solution of the present invention, and a detailed implementation method and process are given, but the protection scope of the present invention is not limited to the following embodiments. The experimental methods in the following embodiments without specifying specific conditions are usually carried out under conventional conditions.

[0029] The method for preparing hexene and co-producing octene and decene by oligomerization provided by the present invention comprises the following steps: ethylene and butene undergo oligomerization reaction under the action of a catalyst to obtain hexene, octene and decene products, wherein the catalyst comprises: a chromium source, a ligand and an organic aluminum compound, the molar ratio of the three being 1:1-20:1-500, and preferably, the amount of the catalyst used is 0.02 mmol / L-0.50 mmol / L in terms of the concentration of the chromium element;

[0030] The ligand is selected from heterocyclic compounds, and its general formula is XRn, wherein X is a five-membered heterocycle, R is selected from substituted or unsubstituted straight-chain alkanes, substituted or unsubstituted branched alkanes, substituted or unsubstituted cycloalkanes, substituted or unsubstituted aromatics, and n is 1-5.

[0031] Specifically, in the method provided by the present invention, within the ratio range of each component of the catalyst, raw materials ethylene and butene undergo oligomerization reaction under the action of the catalyst, and the reaction product is mainly hexene, while octene and decene are co-produced.

[0032] In some embodiments, n is 1-2.

[0033] In some embodiments, the molar ratio of the chromium source, the ligand and the organoaluminum compound is 1:1-5:100-200.

[0034] In some embodiments, the chromium source is selected from at least one of tetrahydrofuran chromium trichloride, chromium octoate, chromium trichloride, chromium acetylacetonate, chromium 2-ethylhexanoate, and chromium acetate.

[0035] In some embodiments, the chromium source is selected from at least one of tetrahydrofuran chromium trichloride, chromium 2-ethylhexanoate, and chromium acetylacetonate.

[0036] In some embodiments, X is furan, thiophene, or pyrrole.

[0037] In some embodiments, R is a branched alkane.

[0038] In some embodiments, said R is methyl, ethyl or tert-butyl.

[0039] In some embodiments, the organoaluminum compound is selected from at least one of trimethylaluminum, triethylaluminum, triisobutylaluminum, tri-n-hexylaluminum, diethylaluminum monochloride, and ethylaluminum dichloride.

[0040] In some embodiments, the organoaluminum compound is selected from at least one of triethylaluminum, diethylaluminum monochloride, and ethylaluminum dichloride.

[0041] In some embodiments, the organoaluminum compound is a composition of a non-halogen alkyl aluminum and a haloalkyl aluminum, wherein the molar ratio of the haloalkyl aluminum to the non-halogen alkyl aluminum is 1:1-50.

[0042] In some embodiments, the molar ratio of ethylene to butene is 1:1-20.

[0043] In some embodiments, the method is performed in an inert solvent, which is an alkane, an aromatic hydrocarbon, a halogenated hydrocarbon, or an alkene.

[0044] In some embodiments, the alkane is n-hexane, methylcyclohexane, cyclohexane, heptane or decane; the aromatic hydrocarbon is benzene, toluene, xylene or isopropylbenzene; the olefin is butene-1, hexene-1 or octene-1.

[0045] Example 1

[0046] A 1L high-pressure reactor was evacuated at 120°C for 1h, replaced with hydrogen three times, and after cooling, 200mL of hexane solvent was added under hydrogen protection, triethylaluminum was added to the reactor, stirring was started for 3min, stirring was stopped, and the hexane solution of chromium octanoate and 2,5-di-tert-butylpyrrole prepared in advance was added. The amount of the catalyst system was 0.05mmol / L in terms of chromium element concentration, and the molar ratio of the three components of the added catalyst (chromium octanoate, 2,5-di-tert-butylpyrrole, triethylaluminum in sequence) was 1:4: 150, after stirring for 1min, 224g of butene was added to the kettle, the reaction temperature was raised to 100℃, ethylene was introduced to 3MPa, the reaction temperature was controlled at 100℃, the reaction was continued for 1h, the internal cooling was turned on after the reaction, the hot water was removed to cool down, and when the temperature dropped to 35℃, the gas phase and liquid phase compositions were measured respectively. The product contained hexene, octene and decene components. According to the weight gain of the product, the catalytic activity was calculated to be 132kg product / gCr.h, of which the hexene selectivity was 47%, the octene selectivity was 36%, and the decene selectivity was 12%. The specific data are shown in Table 1.

[0047] Example 2

[0048] A 1L high-pressure reactor was evacuated at 120°C for 1h, replaced with hydrogen three times, and after cooling, 100mL of hexane solvent was added under hydrogen protection, diethylaluminum chloride was added to the reactor, stirring was started for 3min, stirring was stopped, and the pre-prepared hexane solutions of chromium acetylacetonate and 1,3-dimethylpyrrole were added. The amount of the catalyst system was 0.05mmol / L in terms of chromium concentration, and the molar ratio of the three catalyst components (chromium acetylacetonate, 1,3-dimethylpyrrole, diethylaluminum chloride, in turn) was: 1:4:120, after stirring for 1 min, add 280g of butene to the kettle, raise the reaction temperature to 100℃, introduce ethylene to 3MPa, control the reaction temperature at 100℃, react for 1h, open the internal cooling after the reaction is completed, remove the hot water to cool down, wait for the temperature to drop to 35℃, measure the gas phase and liquid phase composition respectively, the product contains hexene, octene and decene components, according to the weight gain of the product, the catalytic activity is calculated to be 219kg product / gCr.h, of which the hexene selectivity is 48%, the octene selectivity is 46%, and the decene selectivity is 5%. Specific data are shown in Table 1.

[0049] Example 3

[0050] A 1L high-pressure reactor was evacuated at 120°C for 1h, replaced with hydrogen three times, and after cooling, 200mL of hexane solvent was added under hydrogen protection, diethylaluminum chloride was added to the reactor, and stirring was started for 3min. Stirring was stopped, and then the pre-prepared hexane solutions of chromium isooctanoate and 2,5-dimethylpyrrole were added. The amount of the catalyst system was 0.05mmol / L in terms of chromium element concentration, and the molar ratio of the three catalyst components (chromium isooctanoate, 2,5-dimethylpyrrole, and diethylaluminum chloride, in turn) was 1:1. :4:150, after stirring for 1 min, 224 g of butene was added to the kettle, the reaction temperature was raised to 100 ° C, ethylene was introduced to 2 MPa, the reaction temperature was controlled at 100 ° C, and the reaction was carried out for 1 h. After the reaction was completed, the internal cooling was turned on to remove the hot water to cool down. When the temperature dropped to 35 ° C, the gas phase and liquid phase compositions were measured respectively. The product contained hexene, octene and decene components. According to the weight gain of the product, the catalytic activity was calculated to be 87 kg product / gCr.h, of which the hexene selectivity was 28%, the octene selectivity was 31%, and the decene selectivity was 40%. Specific data are shown in Table 1.

[0051] Example 4

[0052] A 1L high-pressure reactor was evacuated at 120°C for 1h, replaced with hydrogen three times, and after cooling, 200mL of hexane solvent was added under hydrogen protection, triethylaluminum was added to the reactor, stirring was started for 3min, stirring was stopped, and the pre-prepared hexane solutions of chromium isooctanoate and 2,5-dimethylpyrrole were added. The amount of the catalyst system was 0.05mmol / L in terms of the concentration of chromium element, and the molar ratio of the three catalyst components added (chromium isooctanoate, 2,5-dimethylpyrrole, triethylaluminum) was 1:4:2 00, after stirring for 1 min, 168 g of butene was added to the kettle, the reaction temperature was raised to 110 ° C, ethylene was introduced to 4.5 MPa, the reaction temperature was controlled at 110 ° C, and the reaction was continued for 1 h. After the reaction was completed, the internal cooling was turned on to remove the hot water to cool down. When the temperature dropped to 35 ° C, the gas phase and liquid phase compositions were measured respectively. The product contained hexene, octene and decene components. According to the weight gain of the product, the catalytic activity was calculated to be 459 kg product / gCr.h, of which the hexene selectivity was 67%, the octene selectivity was 21%, and the decene selectivity was 11%. Specific data are shown in Table 1.

[0053] Table 1

[0054]

[0055] As shown in Table 1, the method provided by the present invention can control the selectivity of hexene, octene and decene by adjusting the catalyst components and the ratio between the components and the polymerization process conditions. The method provided by the present invention has a wide range of application prospects.

[0056] In summary, the method of the present invention is based on the process of producing hexene by ethylene polymerization catalyzed by chromium-based catalysts. Under the premise of not changing the process flow of producing hexene by ethylene polymerization, by changing some catalyst components and introducing butene as a raw material, the purpose of producing hexene by ethylene polymerization and simultaneously co-producing octene and decene with high selectivity can be achieved. At the same time, the ratio of hexene: octene: decene in the product can be controlled by adjusting the raw material ratio.

[0057] Of course, the present invention may have many other embodiments. Without departing from the spirit and essence of the present invention, technicians familiar with the field may make various corresponding changes and deformations based on the present invention, but these corresponding changes and deformations should all fall within the scope of protection of the present invention.

Claims

1. A method for preparing hexene by oligomerization and co-producing octene and decene, characterized in that: The following steps are involved: Ethylene and butene undergo oligomerization reaction under the action of a catalyst to obtain hexene, octene and decene products, wherein the catalyst comprises: a chromium source, a ligand and an organic aluminum compound, the molar ratio of the three being 1:1-20:1-500, and the amount of the catalyst used being 0.02 mmol / L-0.50 mmol / L in terms of the concentration of the chromium element; The ligand is a heterocyclic compound with the general formula XRn, wherein X is pyrrole and R is methyl, ethyl or tert-butyl; The chromium source is selected from at least one of chromium 2-ethylhexanoate and chromium acetylacetonate; The molar ratio of ethylene to butene is 1:1-20; The molar ratio of the chromium source, the ligand and the organoaluminum compound is 1:1-5:100-200; The organoaluminum compound is at least one selected from trimethylaluminum, triethylaluminum, triisobutylaluminum, tri-n-hexylaluminum, diethylaluminum monochloride, and ethylaluminum dichloride; The method is carried out in an inert solvent, wherein the inert solvent is an alkane, an aromatic hydrocarbon, a halogenated hydrocarbon or an olefin; the alkane is n-hexane, methylcyclohexane, cyclohexane, heptane or decane; the aromatic hydrocarbon is benzene, toluene, xylene or isopropylbenzene; and the olefin is hexene-1 or octene-1.

2. The method for preparing hexene by oligomerization and co-producing octene and decene according to claim 1, characterized in that: The organoaluminum compound is at least one selected from triethylaluminum, diethylaluminum monochloride and ethylaluminum dichloride.

Citation Information

Patent Citations

  • Oligomerisation of ethylene to mixtures of 1-hexene and 1-octene

    CN105228973A

  • Process for the preparation of a catalyst for olefin polymerization

    EP0608447A1

  • Method for producing 1-hexene and coproducing heptene and octene

    CN104447168A