Amphoteric modified oligomeric polypropylene imine ethoxylates for improving detergency in laundry detergents

Through the ethoxylation, quaternization and transsulfation methods of amphoteric modified oligopropylene imine ethoxylate, alkoxylated oligopolymer and polyolefinimine in laundry applications in the prior art are solved. The deficiencies in cleaning performance and rheological impact have achieved efficient decontamination and low viscosity effects, and are suitable for low dose and high concentration products.

CN115397888BActive Publication Date: 2024-11-15BASF SE
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202180028702.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-05-29
Filing Date
2021-05-19
Publication Date
2024-11-15
Estimated Expiration
2041-05-19

AI Technical Summary

Technical Problem

In the prior art, alkoxylated oligomers and polyolefinimines have not fully utilized their potential for cleaning performance and rheology in laundry applications, especially in low doses of weight efficiency and viscosity management. Inadequate and complex preparation method, a variety of modifiers and auxiliary materials are required.

Method used

Using amphoteric modified oligopropylene imine ethoxylates through a combination of ethoxylation, quaternization and transsulfation, dialkyl sulfate as a single modifier, to prepare neutral or weak The internal zwitterionic polymer with net cationic charge simplifies the process and improves performance.

Benefits of technology

Significantly improves the detergent of clothing, while minimizing the negative impact of formulation viscosity at extremely low addition amounts, achieving high weight efficiency and high concentration products. It is suitable for upper door washing machines, and has a simple process and easy operate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0003890328060000041
    Figure BDA0003890328060000041
  • Figure BDA0003890328060000051
    Figure BDA0003890328060000051
  • Figure BDA0003890328060000081
    Figure BDA0003890328060000081
Patent Text Reader

Abstract

The present invention relates to amphiphilically modified ethoxylated oligoamines and their preparation and use.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention relates to certain amphiphilically modified ethoxylated oligoamines and their manufacture and use.

[0002] In the following, oligo / polypropyleneimine is also abbreviated as "PPI" and oligo / polyethyleneimine is also abbreviated as "PEI". Ethoxylated oligo / polypropyleneimine is referred to as "EPPI" (or "ePPI") and ethoxylated oligo / polyethyleneimine is referred to as "EPEI" (or "ePEI").

[0003] Furthermore, hereinafter, ethylene oxide is sometimes referred to as “EO”, and propylene oxide is sometimes referred to as “PO”.

[0004] Alkoxylated oligo- and polyalkyleneimines, especially alkoxylated oligo- and polyethyleneimines are well known as additives for various applications, such as laundry detergents (e.g. EP3301154, EP3167034 and EP112593), additives for cement-based binder systems (WO2016187085) or hard surface cleaners (EP2961819). In the case of laundry applications, benefits to primary and secondary cleaning performance have been mentioned, but no specific effects on rheology have been disclosed.

[0005] In addition, there are some reports on alkoxylated oligo- and poly-imines, especially on alkoxylated oligo- and polyethyleneimines, describing the effect on the viscosity of the formulation. US20180216037 and US20190024026 both describe polyethyleneimines (e.g., PEI-(EO)) reacted with ethylene oxide and propylene oxide. 10 (PO)5) as a viscosity modifier for anionic surfactant-containing formulations. PEI alkoxylates are used to reduce the viscosity of surfactant formulations. In contrast, no benefits on cleaning performance have been disclosed.

[0006] Furthermore, WO2020 / 030469 describes ethoxylated polyethyleneimines with a high molecular weight polyethyleneimine core, which are prepared by using a specific process (strong under-hydroxyethylation) to obtain additives for laundry applications having a good performance profile while showing a reduced negative impact on the viscosity of the detergent formulation.

[0007] In contrast, modified oligomeric and polyalkyleneimine alkoxylates are less common.

[0008] EP2662436 describes cationic alkoxylated polyethyleneimines in combination with bleach boosters for use in automatic dishwashing applications. In WO2004020563 hydrophobically modified and amphoteric modified polyalkyleneimines for use in detergent compositions are described.

[0009] For example, laundry compositions containing alkoxylated and optionally further cationically or amphoteric-modified polyalkyleneimines with at least 6 N atoms per molecule are described in EP 2961821. More specifically, modified and unmodified oligomeric and polypropyleneimines with at least 6 N atoms per molecule are disclosed which bring soil removal benefits and contribute to improved whiteness. Any effect on detergent rheology has not been mentioned.

[0010] Furthermore, EP3039109 and EP3039057 describe predominantly ethoxylated and optionally further amphiphilically modified oligo- and polyalkyleneimines with low melting points. Due to the incorporation of at least 1 mol of C3 to C5 alkylene oxide into the predominantly ethylene oxide-based polyalkoxylate chain, polymers with low melting points are obtained, which facilitates their preparation process. No mention has been made of any benefits in terms of application properties compared to the same polymers based solely on ethylene oxide and therefore having a higher melting point.

[0011] Furthermore, EP1198492 describes zwitterionic (i.e., amphoteric-modified) alkoxylated polyamines with improved thermal stability for use as additives for laundry detergents. Generally, the amphoteric modification of the material is obtained by a combination of separate quaternization and sulfation steps, wherein the sulfation is carried out with a sulfating agent such as chlorosulfonic acid. The zwitterionic polyamines have a net anionic charge, i.e., the number of cationic groups exceeds the number of anionic groups by at least 20%, preferably at least 50%. The benefits of improved cleaning performance and the positive effect on detergent viscosity have not been mentioned.

[0012] Processes for preparing alkoxylated and further amphiphilically modified oligo- and polyalkyleneimines are known in principle from the prior art.

[0013] As mentioned above, a process for making alkoxylated zwitterionic polyamines is described in EP 1 198 492, wherein the alkoxylate has been quaternized with a modifier (1) and sulfated using a different modifier (2) such as chlorosulfonic acid. The resulting structure has a net anionic charge.

[0014] WO2001029112 describes a process for sulfating alkoxylated quaternized polyamines using sulfur trioxide as the sulfating agent to achieve a high degree of sulfation. The structure also has a net anionic charge.

[0015] In EP 1309546, a method based on a combination of alkoxylation, quaternization and transsulfation starting from a tertiary amino alcohol is described. The method comprises the reaction of a tertiary amine with a sulfate precursor (e.g., dialkyl sulfate) to form a mixture comprising a quaternized amine and sulfate species. The hydroxy species is then sulfated under acidic conditions. More specifically, it has been disclosed to prepare alkoxylated, quaternized and fully sulfated oligomeric and polyimines by using auxiliary amines. The resulting polymer no longer contains any free hydroxyl groups, i.e., all groups have been converted into sulfate groups. Therefore, the net charge of the polymer is anionic.

[0016] Another method based on the combination of alkoxylation, quaternization and transsulfation without the use of auxiliary amines is described in WO200424858. The method comprises the reaction of the tertiary amine in the main chain of the alkoxylated oligo- or polyamine with a sulfate precursor (e.g. dialkyl sulfate) to form a mixture comprising quaternized polyamine alkoxylates and sulfates. The hydroxyl species is then sulfated under acidic conditions. Depending on the degree of conversion of the transsulfation process, a polymer exhibiting a neutral or weak net cationic charge can be obtained. In any case, the polyalkylene oxide block contains free terminal hydroxyl groups in addition to anionic sulfate groups. The same method for specific polyamine main chains and specific polyalkylene oxide side chains is also described in the above-mentioned patents EP2961821, EP3039109 and EP3039057.

[0017] Although several different unmodified and modified oligomeric and polyalkyleneimine alkoxylates and methods for their manufacture have been described in the prior art which show good cleaning performance in laundry applications and in some cases also do not have a significant negative impact on the rheology of the detergent formulations, there is still a need for better materials, especially with better performance at lower dosages (improved weight efficiency of the polymer). In addition, there is a need for polymers with good or even improved cleaning performance in laundry applications and a low or even no (negative) impact on the viscosity of the laundry formulations. In addition, there is a need for simple preparation methods, avoiding the use of more than one modifier for quaternization and sulfation and / or avoiding the use of auxiliary materials.

[0018] Unexpectedly, it has been found in the present invention that specific amphiphilic modified oligopropyleneimine ethoxylates can contribute to significantly improve the detergency of laundry detergents while minimizing the negative impact on the viscosity of the formulation. The improved performance of the materials of the present invention compared to prior art polymers is particularly evident at very low addition levels, which is an important prerequisite for use in top-loading washing machines. Their higher weight efficiency facilitates their use in the form of highly concentrated products, for example in a single unit dose. The amphiphilic modified oligopropyleneimine ethoxylates of the present invention can be easily obtained starting from the respective oligoamines by a combination of ethoxylation, quaternization and transsulfation, while the quaternization and transsulfation are carried out using dialkyl sulfate as a single modifier, i.e., no more than one modifier is required and / or no auxiliary materials are required. The amphiphilic modified oligopropyleneimine ethoxylates of the present invention have a neutral or weak net cationic charge, depending on the degree of conversion during the transsulfation step.

[0019] Therefore, one aspect of the present invention is an amphiphilically modified oligopropylene imine ethoxylate (A) of the general formula (I)

[0020]

[0021] in

[0022] R 1 are identical or different and are selected from C1-C4-alkyl, H and a free electron pair, wherein all R 1 At least 50%, preferably at least 80%, more preferably at least 90% of the

[0023] EO means -CH2-CH2-O,

[0024] Y is the same or different and is selected from SO3 - and H, wherein at least 30%, preferably at least 50%, of all Y are SO3 - ,

[0025] x is identical or different and is selected from 5 to 50, preferably 10 to 40, and n is selected from 1, 2 and 3.

[0026] The amphiphilically modified oligopropylene imine ethoxylate (A) of the present invention is an internal zwitterion. The counter ion of the quaternized nitrogen atom is SO3 - ion or alkyl sulfate ion (C1 to C4 monoalkyl sulfate).

[0027] After optional neutralization and optional dilution with water, further anions and cations are present in the mixture, but the polymer itself can still be regarded as an internal zwitterion.

[0028] In a preferred embodiment, all R 193% to 97% are C1-C4-alkyl.

[0029] In a preferred embodiment of the amphiphilically modified oligopropyleneimine ethoxylate (A) of the general formula (I) of the present invention, n is 2 or 3 and / or all R 1 At least 90% of the radicals are methyl groups.

[0030] In a further preferred embodiment of the amphiphilically modified oligopropyleneimine ethoxylate (A) of the general formula (I) according to the invention, n is 2 and / or all R 1 At least 90% of are methyl and / or x is in the range of 15 to 30.

[0031] In a further preferred embodiment of the polymer of the invention, n=1, 2 or 3, R 1 At least 80% of the 1 =C1-C4-alkyl and Y=SO3 - The ratio is an average of 1.0:1.0 to 1.0:0.8.

[0032] Further aspects of the invention include:

[0033] Compound mixture comprising at least one amphiphilically modified oligopropyleneimine ethoxylate (A) according to formula (I) in which n=2 and at least one isomeric compound according to formula (II)

[0034]

[0035] in

[0036] R 1 are identical or different and are selected from C1-C4-alkyl, H and a free electron pair, wherein all R 1 At least 50%, preferably at least 80%, more preferably at least 90% of the

[0037] EO means -CH2-CH2-O,

[0038] Y is the same or different and is selected from SO3 - and H, wherein at least 30%, preferably at least 50%, of all Y are SO3 - ,

[0039] x is the same or different and is selected from 5 to 50.

[0040] Preferred compound mixtures as described above comprise the amphiphilically modified oligopropyleneimine ethoxylate (A) according to formula (I) and the compound according to formula (II) in a total molar ratio of 10:1 or more.

[0041] In a preferred embodiment of the present invention, the inventive amphiphilically modified oligopropyleneimine ethoxylates (A) are obtained in a mixture which additionally comprises sulfates of alkali metals and / or amines.

[0042] In a further preferred embodiment of the compound mixture according to the invention, the mixture additionally comprises sulfates of amines, preferably sulfates of alkanolamines.

[0043] In another preferred embodiment of the present invention, the amphiphilic modified oligopropyleneimine ethoxylate (A) of the present invention and the mixture containing it are mixed with water in any ratio. Preferably, the mixture contains 1 to 80% by weight of water, more preferably 1 to 60% by weight of water, still more preferably 5 to 50% by weight of water, most preferably 10 to 40% by weight of water.

[0044] At least one antimicrobial agent can also be added to the aqueous solution of the amphiphilically modified oligopropyleneimine ethoxylate (A) and the mixture containing it according to the present invention. Preferably, 2-phenoxyethanol (CAS-no. 122-99-6, available for example from BASF PE) or 4,4'-dichloro-2-hydroxydiphenyl ether (CAS: 3380-30-1) and combinations thereof.

[0045] 4,4'-dichloro-2-hydroxydiphenyl ether can be used as a solution, for example a 30% by weight solution of 4,4'-dichloro-2-hydroxydiphenyl ether in 1,2-propylene glycol, such as is available from BASF as HP 100.

[0046] Methods for producing the compounds of the present invention

[0047] A further aspect of the present invention is also a method for producing the amphiphilically modified oligopropyleneimine ethoxylate (A) of the present invention, the method comprising the steps of:

[0048] (a) providing an amine selected from ammonia, 1,3-propylenediamine, bis-(3,3'-aminopropyl)amine and bis-(3,3'-aminopropyl)-1,3-propylenediamine or a mixture thereof,

[0049] (b) optionally, the amine is cyanoethylated with acrylonitrile in a ratio of 100:1 to 1:2.5, preferably 10:1 to 1:2.5, more preferably 3:1 to 1:2.1, followed by hydrogenation to obtain oligopropyleneimines having 2, 3 and 4 repeating units,

[0050] (c) optionally, purification of the oligopropylene imine from step (b),

[0051] (d) ethoxylation of the amine and / or oligopropyleneimine from step a, b or c, and

[0052] (e) At least partial quaternization and transsulfation with di-C1-C4-alkyl sulfates.

[0053] In a preferred embodiment of the process of the invention, purification step (c) is carried out to obtain oligopropyleneimines having 2, 3 and 4 repeating units or mixtures thereof in a purity of at least 80% by weight, preferably at least 90% by weight.

[0054] In a preferred embodiment of the above-described process according to the invention, the quaternization in step (e) is carried out with dimethyl sulfate.

[0055] In a further preferred embodiment of the above-described process according to the invention, the transsulfation in step (e) is carried out using sulfuric acid as catalyst.

[0056] In a further preferred embodiment of the process according to the invention, the transsulfation in step (e) is carried out quantitatively (>=80%) and a weakly cationic or net neutral polymer is obtained.

[0057] In a further preferred embodiment of the above-mentioned method of the present invention, the method further comprises a subsequent step of neutralizing the sulfuric acid with a base selected from alkali metal hydroxides and amines. Preferably, a base selected from amines, more preferably alkanolamines, or an aqueous solution thereof can be used.

[0058] In a preferred embodiment of the process according to the invention, the ethoxylation in step (d) is carried out in two substeps, namely (i) conversion with up to 1 mol of EO per NH function and subsequently (ii) conversion with more ethylene oxide under basic catalysis.

[0059] Also a further aspect of the present invention are the amphiphilically modified oligopropyleneimine ethoxylates (A) as defined above, obtainable by the process of the present invention as described above (and in more detail below).

[0060] The above-mentioned steps (a) to (c) of the method of the present invention can be carried out as follows.

[0061] Via Route A:

[0062] As previously described in CN107311891, 1 equivalent of acrylonitrile can be added dropwise to an excess of 1,3-propylenediamine, bis-(3,3'-aminopropyl)amine or bis-(3,3'-aminopropyl)-1,3-propylenediamine or a mixture thereof (up to 100 equivalents) optionally dissolved in a solvent in a reaction vessel at a temperature of 5°C to 80°C. After complete addition, the reaction can be stirred at the temperature indicated until the starting material is completely consumed and then cooled to room temperature. After optional purification (but preferably not purified), the crude mixture can be hydrogenated by [Cu], [Co], [Ni], [Pd], [Pt] or [Ru] catalysts in the presence or absence of solvents in a pressure reactor as previously described in DD238043 and / or JP08333308 and / or WO2018046393 under elevated hydrogen and optional ammonia pressure. During the hydrogenation, the temperature may be between 70°C and 200°C, preferably between 70°C and 150°C, and the hydrogen pressure may be between 1 and 250 bar, preferably between 50 and 250 bar. The catalyst may be removed, for example, by filtration, and the volatiles may be removed under reduced pressure. The mixture of desired oligomeric amino compounds obtained may then be separated in the next step by distillation under reduced pressure (<1 bar) to give the purified target compound bis-(3,3'-aminopropyl)amine, bis-(3,3'-aminopropyl)-1,3-propylenediamine or tris-(3,3',3"-aminopropyl)-1,3-propylenediamine. By route B:

[0063] As previously described in CN102941160 and / or WO9214709, acrylonitrile (up to 2.5 equivalents) can be added dropwise to 1 equivalent of ammonia, 1,3-propylenediamine, bis-(3,3'-aminopropyl)amine or bis-(3,3'-aminopropyl)-1,3-propylenediamine or a mixture thereof, optionally dissolved in a solvent, in a reaction vessel at a temperature of 5°C to 80°C. After the addition reaction is complete, the reaction can be stirred at the temperature indicated until the starting material is completely consumed and then cooled to room temperature. After optional purification (but preferably not purified), the crude mixture can be hydrogenated by [Cu], [Co], [Ni], [Pd], [Pt] or [Ru] catalysts in a pressure reactor in the presence or absence of a solvent under elevated hydrogen and optional ammonia pressure as previously described in DD238043 and / or JP08333308 and / or WO 2018046393. During the hydrogenation, the temperature may be between 70° C. and 200° C., preferably between 70° C. and 150° C., and the hydrogen pressure may be between 1 and 250 bar, preferably between 50 and 250 bar. The catalyst may be removed, for example, by filtration, and the volatiles may be removed under reduced pressure. The mixture of desired oligomeric amino compounds obtained may then be separated in the next step by distillation under reduced pressure (<1 bar) to give the purified target compound bis-(3,3′-aminopropyl)amine, bis-(3,3′-aminopropyl)-1,3-propylenediamine or tris-(3,3′,3″-aminopropyl)-1,3-propylenediamine.

[0064] The crude mixture according to route (A) or (B) contains mainly (>50 mol %) linear oligoamines, preferably more than 70 mol % linear oligoamines, more preferably more than 80 mol % linear oligoamines.

[0065] In a preferred embodiment of the present invention, the crude mixture according to route (A) or (B) is purified by distillation to remove any impurities from monomers, other oligomers or branched structures and branched isomers, respectively, to obtain a linear target compound bis-(3,3'-aminopropyl)amine, bis-(3,3'-aminopropyl)-1,3-propylenediamine or tris-(3,3',3"-aminopropyl)-1,3-propylenediamine or a mixture thereof in a purity of at least 80% by weight, more preferably at least 90% by weight, and even more preferably >95% by weight.

[0066] In one embodiment of the present invention, the purified bis-(3,3′-aminopropyl)-1,3-propylenediamine or a mixture containing the same may contain isomeric compounds (structure after alkoxylation / modification according to formula (II)) at a ratio of 10:1 mol % or more.

[0067]

[0068] in

[0069] R 1 are identical or different and are selected from C1-C4-alkyl, H and a free electron pair, wherein all R 1 At least 50%, preferably at least 80%, more preferably at least 90% of the

[0070] EO means -CH2-CH2-O,

[0071] Y is the same or different and is selected from SO3 - and H, wherein at least 30%, preferably at least 50%, of all Y are SO3 - ,

[0072] x is the same or different and is selected from 5 to 50.

[0073] Step (d) of the above-mentioned production method can be performed as follows.

[0074] The process step (d) of the present invention is characterized in that only ethylene oxide is used as alkoxylating agent. Other alkylene oxides, such as propylene oxide, are not useful for the process of the present invention and do not give the products of the present invention and their properties in laundry applications.

[0075] In a preferred embodiment of step (d) of the production process of the invention, the ethoxylation is carried out in two steps.

[0076] According to a preferred embodiment of the present invention, ethylene oxide is added in the first step (i) of process step (d) in an amount of 0.2 to 1.0 ethylene oxide units per NH group of the oligopropyleneimine (PPI), preferably 0.5 to 0.99, more preferably 0.6 to 0.95 ethylene oxide units per NH group of the oligopropyleneimine (PPI), still more preferably 0.70 to 0.95 ethylene oxide units per NH group of the oligopropyleneimine (PPI) (under-hydroxyethylation).

[0077] In a preferred embodiment of the process according to the invention, the minimum amount of ethylene oxide units per NH group added in step (i) is at least equal to the amount of basic catalyst C added later in step (ii) or higher, in order to prevent the formation of polyethylene glycol during step (ii) by direct reaction of catalyst C with ethylene oxide.

[0078] Preferably, the sum of the amounts of ethylene oxide EO added in steps (i) and (ii) is in the range of 5 to 50 ethylene oxide units per NH group of the oligopropyleneimine (PPI), more preferably 10 to 40 ethylene oxide units per NH group of the oligopropyleneimine (PPI), even more preferably 15 to 30 ethylene oxide units per NH group of the oligopropyleneimine (PPI).

[0079] Preferably, the first step (i) of process step (d) is carried out in the absence of a basic catalyst. Water can be added in the first step (i) of process step (d).

[0080] In one embodiment of the present invention, the second step (ii) of step (d) of the method of the present invention is carried out in the presence of a basic catalyst. Suitable bases are, for example, LiOH, NaOH, KOH, CsOH and mixtures thereof, sodium or potassium alcoholates, such as potassium methoxide (KOCH3), potassium tert-butoxide, sodium methoxide (NaOCH3), sodium n-hexoxide and sodium ethoxide. Further examples of catalysts are alkali metal hydrides and alkaline earth metal hydrides, such as sodium hydride and calcium hydride, and alkali metal carbonates, such as sodium carbonate and potassium carbonate. Preferred are alkali metal hydroxides, preferably potassium hydroxide and sodium hydroxide, and alkali metal alcoholates, preferably potassium methoxide (KOCH3) and sodium methoxide (NaOCH3). Particularly preferred are potassium hydroxide and potassium methoxide (KOCH3). The typical amount of base, such as KOH, is 0.02 to 10% by weight, in particular 0.05 to 1% by weight, relative to the ethoxylated oligopropyleneimine (EPPI).

[0081] In a preferred embodiment of the process according to the invention, the basic catalyst C is used only in the second step (ii) and is selected from alkaline earth metal-containing basic catalysts.

[0082] An especially preferred embodiment of the basic catalyst in the process of the invention is KOH; KOH can be used in the process of the invention as an aqueous solution.

[0083] In one embodiment of the process of the invention, the basic catalyst C is added in an amount of 0.05 to 0.3% by weight, preferably 0.15 to 0.25% by weight, relative to the ethoxylated oligopropyleneimine (EPPI).

[0084] In one embodiment, the temperature during the first step (i) of step (d) of the process of the invention is in the range of 90 to 160°C, preferably 100 to 150°C, more preferably 110 to 140°C.

[0085] In one embodiment, the temperature during the second step (ii) of step (d) of the process of the invention is in the range of 100 to 180°C, preferably 120 to 160°C, more preferably 120 to 145°C.

[0086] Higher temperatures than those specified above during the alkoxylation step are also possible, but not preferred, since they generally lead to (more) colored products.

[0087] In one embodiment of the present invention, the reaction during the first step (i) of step (d) of the process of the present invention can be carried out at a total pressure of up to 15 bar, preferably up to 10 bar, for example 1 to 6 bar. Preferred containers for carrying out the reaction are autoclaves and tubular reactors.

[0088] In one embodiment of the present invention, the reaction during the second step (ii) of step (d) of the process of the present invention can be carried out at a total pressure of up to 15 bar, preferably up to 10 bar, for example 2 to 10 bar. Preferred containers for carrying out the reaction are autoclaves and tubular reactors. The reaction during the second step (ii) of step (d) of the process of the present invention can be interrupted at different intermediates (i.e., the degree of alkoxylation) and can be continued with or without additional catalyst.

[0089] The product obtained after step (ii) of step (d) of the process of the present invention, ie ethoxylated oligopropyleneimine (EPPI), can be treated with a bleaching agent. The bleaching agent is preferably selected from borates, hypochlorites, borohydrides and hydrogen peroxide.

[0090] The abovementioned step (e) of the process according to the invention: (at least partial) quaternization and transsulfation with di-C1-C4-alkyl sulfate.

[0091] The quaternization and transsulfation step (e) is a combined process based on the quaternization of the amino groups in the backbone of the EPPI and the sulfation of the terminal hydroxyl moieties of the polyethylene oxide side chains. More generally, the quaternization and transsulfation step (e) comprises a sub-step (e1) of forming sulfate species (= quaternization) and a sub-step (e2) of providing controlled sulfation of one or more hydroxyl moieties (= transsulfation).

[0092] The first required sub-step (e1) of the method is carried out under alkaline or near pH neutral conditions. The second sub-step (e2) of the method is carried out under acidic conditions.

[0093] The method is described in detail below:

[0094] Sub-step (e1) (quaternization):In a preferred embodiment of the present invention, 0.5 to 1.0 equivalents of a sulfating agent, preferably 0.8 to 0.99 equivalents, most preferably 0.9 to 0.99 equivalents, are reacted with one tertiary amino group of the ethoxylated oligopropylene imine to form a quaternary ammonium ion in the backbone of the oligoamine and an equivalent amount of sulfate species. If desired, the process can be carried out in the presence of a solvent, preferably a non-reactive solvent such as toluene, glycol dimethyl ether or diglycol dimethyl ether can be used. The preferred sulfating agent according to the present invention is a dialkyl sulfate, preferably a di-C1-C4-alkyl sulfate, more preferably a di-C1-C2-alkyl sulfate, most preferably dimethyl sulfate. Substep (e1) of the process of the present invention is carried out under alkaline or near pH neutral conditions at a temperature of 0°C to 180°C, preferably 40°C to 100°C, and even more preferably 50°C to 90°C. The reaction can be controlled by any suitable means when exothermic, for example by cooling the reaction vessel or by providing a reflux condenser.

[0095] Sub-step (e2) (transsulfation): The formation of sulfated hydroxyl species is the second required step of the process of the present invention. One equivalent of sulfate species is required for each hydroxyl moiety to be sulfided. The number of sulfate species in the process of the present invention is equal to the number of quaternary ammonium ions in the oligoamine backbone. Depending on the degree of conversion during the transsulfation step, the product obtained after substep (e2) is an amphiphilically modified polymer (i) whose net charge is zero (= neutral polymer) if the sulfate species is completely (100%) converted during the transsulfation step, i.e. the number of quaternary ammonium ions and sulfated hydroxyl groups in the oligoamine backbone is equal; or (ii) whose net charge is positive (= weakly cationic polymer) if only partially (<100%) converted during the transsulfation step, i.e. the number of quaternary ammonium ions in the oligoamine backbone is slightly higher than the number of sulfated hydroxyl groups. In order to control the degree of conversion during the transsulfation step, the formulator can remove the alcohol formed as a by-product, preferably a C1-C4-alcohol, most preferably methanol (depending on the type of di-C1-C4-alkyl sulfate used in step (e1)). In practice, the relative amount of alcohol by-product removed can be used as a tool to control the degree of conversion of the transsulfation step. Any method convenient to the formulator can be used, such as distillation, absorption into molecular sieves, crystallization or precipitation, preferably distillation. In many cases, it is preferred to remove the by-product alcohol already during the reaction, preferably by distillation.

[0096] According to the invention, the degree of conversion during the transsulfation step is at least 50%, preferably at least 80%. 1 =C1-C4-alkyl and Y=SO3 - The preferred ratio is 1.0:1.0 to 1.0:0.8 on average.

[0097] The final product after substep (e2) is obtained as an internal zwitterion with a possible additional cationic charge in case of incomplete conversion (<100%) of the sulfated species during the transsulfation step. The counterion of the quaternized nitrogen atom is SO3 - ions so as to form an internal zwitterion and, in case of incomplete conversion during the transsulfation step, possibly additional alkyl sulfate ions (C1 to C4 monoalkyl sulfates), preferably methyl sulfate ions.

[0098] Substep (e2) must be carried out under acidic conditions. Suitable acids are especially sulfuric acid, hydrochloric acid, methanesulfonic acid or Lewis acids (e.g. boron trifluoride). In the process according to the invention, sulfuric acid is preferably used. The acid can be added in any amount sufficient to form the desired product, in any case, the process of the invention is carried out at a pH of less than about 6, preferably less than about 4, more preferably less than about 3, and most preferably at a pH of about 2. In practice, an acid content of about 0.01 to 1 molar ratio relative to ethoxylated oligopropyleneimine (EPPI) is preferred. The catalyst can be introduced in any manner convenient to the formulator, in any case, good mixing should be used. Alternatively, the acid can be generated in situ by adding an excess of a sulfating agent and reacting this excess with a limited proton source, especially water. Substep (e2) of the process of the invention is carried out at a temperature of 0°C to 200°C, preferably 40°C to 150°C, and more preferably 70°C to 120°C. The reaction can be controlled by any suitable means when exothermic, for example by cooling the reaction vessel or by providing a reflux condenser.

[0099] The use of sulfuric acid in a preferred embodiment of the invention can lead to an additional sulfation of the hydroxyl groups of the ethoxylated oligopropyleneimine as a side reaction, in addition to the conversion of the hydroxyl groups into sulfate groups by transsulfation (i.e. by means of the di-C1-C4-alkyl sulfate used).

[0100] The final product after sub-step (e2) can be further purified to remove volatile by-products and / or acidic catalysts, preferably sulfuric acid, or can be separated as a mixture. Volatile by-products, such as 1,4-dioxane, can be removed, for example, by distillation or stripping under vacuum. If the acidic catalyst is not removed from the final product after sub-step (e2), the mixture can be separated as is or the acidic catalyst can be neutralized. In a preferred embodiment of the present invention, the acidic catalyst is not removed, but neutralized. Any suitable base can be used to neutralize the acidic catalyst, especially ammonium hydroxide, lithium hydroxide, sodium hydroxide, potassium hydroxide, magnesium hydroxide, calcium hydroxide, barium hydroxide or amine. Lithium hydroxide, sodium hydroxide, potassium hydroxide or amine are preferably used, and sodium hydroxide, alkanolamine or its aqueous solution is more preferably used.

[0101] In one embodiment of the present invention, alkanolamine is used to neutralize the acidic catalyst. In the case where the acid used is sulfuric acid, the sulfate of the alkanolamine is formed, and if an aqueous base solution is used, the amphiphilic modified oligopropyleneimine ethoxylate (A) of the present invention is finally obtained in a mixture further comprising the sulfate of the alkanolamine and water.

[0102] The final product after substep (e2), if applicable, after removal or neutralization of the acidic catalyst, can be mixed with water in any ratio. Preferably, the final product after substep (e2) is mixed with 1 to 80% by weight of water, more preferably 1 to 60% by weight of water, even more preferably 5 to 50% by weight of water, most preferably 10 to 40% by weight of water, to reduce viscosity and improve handling.

[0103] The optional post-treatment step may also include adjusting the pH of the final product, especially if the product is obtained as an aqueous solution. Any suitable base or acid can be used to adjust the pH. Preferably, sodium hydroxide, potassium hydroxide or an amine is used as a base; sulfuric acid, hydrochloric acid or methanesulfonic acid is used as an acid. In one embodiment of the present invention, an alkanolamine is used to adjust the pH. A neutral to slightly alkaline pH of the aqueous solution of the polymer of the present invention is preferred to protect the sulfate groups from hydrolysis and cleavage into free hydroxyl groups. Therefore, the pH of the final product in water is preferably adjusted to a pH of 6 to 14, more preferably a pH of 6 to 11, and even more preferably a pH of 7 to 10.

[0104] Additionally, antimicrobial agents may be added to improve the preservation of aqueous solutions of the final product.

[0105] The following is a non-limiting example of a method according to the invention:

[0106] The alkoxylation product obtained from step (d) of the above-described process of the present invention can be heated to an elevated temperature, typically between 50° C. and 90° C., and charged into a reactor under a protective atmosphere, for example a nitrogen atmosphere. A molar excess of di-C1-C4-alkyl sulfate, for example dimethyl sulfate (DMS) relative to the ethoxylated oligopropyleneimine (EPPI) can be metered into the reactor preferably over a time span of 1 to 5 hours so that the temperature in the reactor does not exceed 90° C. The reaction can then be stirred at a temperature not exceeding 90° C. for a period of time, for example between 1 to 5 hours, to complete the reaction.

[0107] Then less than 1 equivalent of sulfuric acid relative to ethoxylated oligopropyleneimine (EPPI) can be added, and the temperature can be set to a value between 70° C. and 120° C. The reactor can be set under vacuum (e.g. 5 to 30 mbar) for 1 to 6 hours, optionally under inert gas stripping. After the reaction is complete, sodium hydroxide or triethanolamine (preferably in aqueous solution) and demineralized water can be added, and the pH can be adjusted to pH 7 to 10. The liquid product can then be removed from the reactor.

[0108] The transsulfation step (the second part of step (e) of the process of the present invention) can also be performed analogously to the process described in WO200424858A1 (Example 4).

[0109] The final polymer obtained according to the present invention has a weight average molecular weight of 1000 to 20000 g / mol, preferably 1500 to 15000 g / mol, more preferably 2000 to 10000 g / mol (determined by GPC, see experimental part). In a preferred embodiment of the present invention, the amphiphilic modified oligopropyleneimine ethoxylate (A) has a weight average molecular weight of 2500 to 8000 g / mol.

[0110] Laundry formulations containing the compounds of the invention

[0111] A further aspect of the present invention is also a laundry preparation comprising at least one of the amphiphilically modified oligopropyleneimine ethoxylates (A) according to the invention and / or the compound mixtures according to the invention as described above.

[0112] An aspect of the present invention is therefore also the use of the inventive amphiphilically modified oligopropyleneimine ethoxylates (A) as described above and / or the inventive compound mixtures in laundry applications.

[0113] Laundry formulations according to the present invention may be liquid, gel or solid compositions, solid embodiments including for example powders and tablets.Liquid compositions may be packaged as unit doses.

[0114] In one embodiment of the present invention, the amphoteric modified oligomeric polypropyleneimine ethoxylate (A) is a component of a laundry formulation (also referred to in this specification as laundry care composition) which additionally comprises at least one anionic surfactant (B).

[0115] Examples of suitable anionic surfactants (B) are C8-C 12 -Alkali metal and ammonium salts of alkyl sulfates, C 12 -C 18 -Alkali metal and ammonium salts of fatty alcohol ether sulfates, C 12 -C 18 -Alkali metal and ammonium salts of fatty alcohol polyether sulfates, ethoxylated C4-C 12 Alkali metal and ammonium salts of sulfuric acid half esters of -alkylphenols (ethoxylation: 3 to 50 mol ethylene oxide / mol), C 12 -C 18 -Alkali metal and ammonium salts of alkylsulfonic acids, C 12 -C 18 Sulfonic fatty acid alkyl esters, such as C 12 -C 18Alkali metal and ammonium salts of sulfonic fatty acid methyl esters, C 10 -C 18 -Alkyl aryl sulfonic acid, preferably nC 10 -C 18 -Alkali metal and ammonium salts of alkylbenzenesulfonic acids, C 10 -C 18 Alkali metal and ammonium salts of alkyl alkoxy carboxylates, and soaps, such as C8-C 24 - Alkali metal and ammonium salts of carboxylic acids. Preference is given to alkali metal salts of the above compounds, particularly preferably sodium salts.

[0116] In one embodiment of the present invention, the anionic surfactant (B) is selected from nC 10 -C 18 - alkylbenzenesulfonic acid and fatty alcohol polyether sulfate, which in the present invention is especially ethoxylated C 12 -C 18 -sulfuric acid half esters of alkanols (ethoxylation: 1 to 50 mol ethylene oxide / mol), preferably nC 12 -C 18 -Sulfate half esters of alkanols.

[0117] The composition according to the invention may comprise at least one builder (C). In the present invention, no distinction is made between builders and components referred to elsewhere as "co-builders". Examples of builders (C) are complexing agents (hereinafter also referred to as complexing agents (C)), ion exchange compounds and precipitants (C). The builders are selected from citrates, phosphates, silicates, carbonates, phosphonates, aminocarboxylates and polycarboxylates.

[0118] In the present invention, the term citrate includes monoalkali metal salts and dialkali metal salts of citric acid, in particular the monosodium salt and preferably the trisodium salt, ammonium salts or substituted ammonium salts of citric acid and citric acid. Citrate can be used as anhydrous compound or as hydrate, for example as sodium citrate dihydrate. The amount of citrate is calculated with reference to anhydrous trisodium citrate.

[0119] The term phosphate includes sodium metaphosphate, sodium orthophosphate, sodium hydrogenphosphate, sodium pyrophosphate and polyphosphates, such as sodium tripolyphosphate. Preferably, however, the composition according to the invention is free of phosphates and polyphosphates, including hydrogenphosphates, for example free of trisodium phosphate, pentasodium tripolyphosphate and hexasodium metaphosphate ("phosphate-free"). With regard to phosphates and polyphosphates, "free" is understood in the present invention to mean that the content of phosphates and polyphosphates totals from 10 ppm to 0.2% by weight of the respective composition, determined gravimetrically.

[0120] The term carbonate includes alkali metal carbonates and alkali metal bicarbonates, preferably the sodium salt. Particularly preferred is Na2CO3.

[0121] Examples of phosphonates are hydroxyalkanephosphonates and aminoalkanephosphonates. Among the hydroxyalkanephosphonates, 1-hydroxyethane-1,1-diphosphonate (HEDP) is particularly important as a builder. It is preferably used as a sodium salt, the disodium salt being neutral and the tetrasodium salt being alkaline (pH 9). Suitable aminoalkanephosphonates are preferably ethylenediaminetetramethylenephosphonate (EDTMP), diethylenetriaminepentamethylenephosphonate (DTPMP) and their higher homologues. They are preferably used in the form of neutral reacting sodium salts, for example as the hexasodium salt of EDTMP or as the heptasodium and octasodium salts of DTPMP.

[0122] Examples of aminocarboxylates and polycarboxylates are nitrilotriacetate, ethylenediaminetetraacetate, diethylenetriaminepentaacetate, triethylenetetraaminehexaacetate, propylenediaminetetraacetic acid, ethanol-diglycine, methylglycine diacetate and glutamine diacetate. The terms aminocarboxylates and polycarboxylates also include their respective unsubstituted or substituted ammonium and alkali metal salts, such as sodium salts, in particular the respective fully neutralized compounds.

[0123] Silicates in the context of the present invention include in particular sodium disilicate and sodium metasilicate, aluminosilicates, such as zeolites and phyllosilicates, in particular those of the formula α-Na2Si2O5, β-Na2Si2O5 and δ-Na2Si2O5.

[0124] The composition according to the invention may contain one or more builders selected from the materials not mentioned above. Examples of builders are alpha-hydroxypropionic acid and oxidized starch.

[0125] In one embodiment of the present invention, the builder (C) is selected from polycarboxylates. The term "polycarboxylates" includes non-polymeric polycarboxylates such as succinic acid, C2-C 16 -Alkyl disuccinate, C2-C 16 -alkenyl disuccinate, ethylenediamine N,N'-disuccinic acid, tartrate diacetate, alkali metal malonates, tartrate monoacetate, tricarballylic acid, butanetetracarboxylic acid and cyclopentanetetracarboxylic acid.

[0126] Oligomeric or polymeric polycarboxylates are, for example, the alkali metal salts of polyaspartic acid or, in particular, (meth)acrylic acid homopolymers or (meth)acrylic acid copolymers.

[0127] Suitable comonomers are monoethylenically unsaturated dicarboxylic acids, such as maleic acid, fumaric acid, maleic anhydride, itaconic acid and citraconic acid. Suitable polymers are in particular polyacrylic acids, which preferably have an average molecular weight M in the range of 2000 to 40 000 g / mol, preferably 2000 to 10 000 g / mol, in particular 3000 to 8000 g / mol. WFurther suitable copolymeric polycarboxylates are in particular copolymers of acrylic acid with methacrylic acid and copolymers of acrylic acid or methacrylic acid with maleic acid and / or fumaric acid.

[0128] It is also possible to use monoethylenically unsaturated C3-C 10 -monocarboxylic acid or C4-C 10 - Copolymers of at least one monomer of a dicarboxylic acid or anhydride thereof, such as maleic acid, maleic anhydride, acrylic acid, methacrylic acid, fumaric acid, itaconic acid and citraconic acid, with at least one hydrophilic or hydrophobic modifying comonomer as listed below.

[0129] Suitable hydrophobic comonomers are, for example, isobutylene, diisobutylene, butene, pentene, hexene and styrene, olefins having 10 or more carbon atoms or mixtures thereof, for example 1-decene, 1-dodecene, 1-tetradecene, 1-hexadecene, 1-octadecene, 1-eicosene, 1-docosahexadecene, 1-tetracosene and 1-hexacosene, C 22 -α-olefins, C 20 -C 24 - mixtures of α-olefins and polyisobutylenes having an average of 12 to 100 carbon atoms per molecule.

[0130] Suitable hydrophilic comonomers are monomers with sulfonate or phosphonate groups, and nonionic monomers with hydroxyl functions or alkylene oxide groups. For example, mention may be made of: allyl alcohol, prenyl alcohol, methoxypolyethylene glycol (meth) acrylate, methoxypolypropylene glycol (meth) acrylate, methoxypolybutylene glycol (meth) acrylate, methoxypoly(propylene oxide-co-ethylene oxide) (meth) acrylate, ethoxypolyethylene glycol (meth) acrylate, ethoxypolypropylene glycol (meth) acrylate, ethoxypolybutylene glycol (meth) acrylate and ethoxypoly(propylene oxide-co-ethylene oxide) (meth) acrylate. The polyalkylene glycols here may contain 3 to 50, in particular 5 to 40 and especially 10 to 30 alkylene oxide units per molecule.

[0131] Particularly preferred monomers containing sulfonic acid groups are 1-acrylamido-1-propanesulfonic acid, 2-acrylamido-2-propanesulfonic acid, 2-acrylamido-2-methylpropanesulfonic acid, 2-methacrylamido-2-methylpropanesulfonic acid, 3-methacrylamido-2-hydroxypropanesulfonic acid, allylsulfonic acid, methallylsulfonic acid, allyloxybenzenesulfonic acid, methallyloxybenzenesulfonic acid, 2-hydroxy-3-(2-propenyloxy)propanesulfonic acid, 2-methyl-2-propene-1-sulfonic acid, styrenesulfonic acid, vinylsulfonic acid, 3-sulfopropyl acrylate, 2-sulfoethyl methacrylate, 3-sulfopropyl methacrylate, sulfomethylacrylamide, sulfomethylmethacrylamide, and the salts of the acids, such as the sodium, potassium or ammonium salts thereof.

[0132] Particularly preferred monomers containing phosphonate groups are vinylphosphonic acid and its salts.

[0133] Furthermore, amphoteric polymers can also be used as builders.

[0134] The composition according to the invention may contain, for example, a total of 0.1 to 70% by weight, preferably 10 to 50% by weight, preferably up to 20% by weight of builder (C), especially in the case of solid preparations. Liquid preparations according to the invention preferably contain 0.1 to 8% by weight of builder (C).

[0135] The preparations according to the invention may contain one or more alkali carriers. If an alkaline pH is desired, the alkali carrier ensures, for example, a pH of at least 9. Suitable are, for example, the alkali metal carbonates, alkali metal hydrogencarbonates and alkali metal metasilicates mentioned above, and in addition, alkali metal hydroxides. Preferred alkali metals are in each case potassium, particularly preferably sodium.

[0136] In one embodiment of the present invention, the laundry preparations according to the invention additionally comprise at least one enzyme (D).

[0137] Useful enzymes are, for example, one or more of lipases, hydrolases, amylases, proteases, cellulases, hemicellulases, phospholipases, esterases, pectinases, lactases and peroxidases, and combinations of at least two of the above types.

[0138] Enzyme (D) can be incorporated in an amount sufficient to provide an effective cleaning amount. In the detergent composition according to the present invention, the preferred amount is in the range of 0.001 wt % to 5 wt % active enzyme. Enzyme stabilizer systems, such as calcium ions, boric acid, organic boronic acid, propylene glycol, short chain carboxylic acids and short chain carboxylic acids can also be used with the enzyme. In the present invention, the short chain carboxylic acid is selected from monocarboxylic acids having 1 to 3 carbon atoms per molecule and dicarboxylic acids having 2 to 6 carbon atoms per molecule. Preferred examples are formic acid, acetic acid, propionic acid, oxalic acid, succinic acid, HOOC(CH2)3COOH, adipic acid and a mixture of at least two of the above, and respective sodium and potassium salts.

[0139] The compositions according to the invention may comprise one or more bleaching agents (E).

[0140] Preferred bleaches (E) are selected from sodium perborate, anhydrous or, for example, as monohydrate or as tetrahydrate or so-called dihydrate, sodium percarbonate, anhydrous or, for example, as monohydrate, and sodium persulfate, the term "persulfate" in each case comprising the salts of the peracid H2SO5 as well as peroxodisulfates.

[0141] In this context, alkali metal salts may in each case also be alkali metal hydrogen carbonates, alkali metal hydrogen perborates and alkali metal hydrogen persulfates. However, dialkali metal salts are in each case preferred.

[0142] The preparations according to the invention may contain one or more bleach catalysts. The bleach catalysts may be selected from oxaziridinium-based bleach catalysts, bleach-enhancing transition metal salts or transition metal complexes, such as manganese-, iron-, cobalt-, ruthenium- or molybdenum-Salen complexes or carbonyl complexes. Complexes of manganese, iron, cobalt, ruthenium, molybdenum, titanium, vanadium and copper with nitrogen-containing tripodal ligands and cobalt-, iron-, copper- and ruthenium-amine complexes may also be used as bleach catalysts.

[0143] The preparations according to the invention may comprise one or more bleach activators, for example tetraacetylethylenediamine, tetraacetylmethylenediamine, tetraacetylglycoluril, tetraacetylhexanediamine, acylated phenolsulfonates, for example n-nonanoyl- or isononanoyloxybenzenesulfonate, N-methylmorpholinium-acetonitrile ("MMA salt"), trimethylammonium acetonitrile, N-acylimides, for example N-nonanoylsuccinimide, 1,5-diacetyl-2,2-dioxohexahydro-1,3,5-triazine ("DADHT") or nitrile quaternary ammonium compounds (trimethylammonium acetonitrile).

[0144] The formulations according to the invention may contain one or more corrosion inhibitors (F). In the present case, this is understood to include those compounds which inhibit metal corrosion. Examples of suitable corrosion inhibitors are triazoles, in particular benzotriazole, bisbenzotriazole, aminotriazole, alkylaminotriazole, and phenol derivatives, such as hydroquinone, catechol, hydroxyhydroquinone, gallic acid, phloroglucinol or pyrogallol.

[0145] In one embodiment of the invention, the preparations according to the invention comprise a total of 0.1 to 1.5% by weight of corrosion inhibitors.

[0146] The formulation according to the invention may also contain additional cleaning polymers (G) or soil release polymers (H). Additional cleaning polymers (G) may include, but are not limited to, polyfunctional polyethyleneimines (e.g. BASF's HP20) and / or polyfunctional diamines (e.g. BASF's HP96).

[0147] Laundry formulations comprising the amphiphilically modified oligopropyleneimine ethoxylates (A) of the present invention may also comprise at least one antimicrobial agent (I).

[0148] The antimicrobial agent may be selected from 2-phenoxyethanol (CAS-no. 122-99-6, available for example from BASF PE) or 4,4'-dichloro-2-hydroxydiphenyl ether (CAS: 3380-30-1) and combinations thereof.

[0149] 4,4'-dichloro-2-hydroxydiphenyl ether can be used as a solution, for example a 30% by weight solution of 4,4'-dichloro-2-hydroxydiphenyl ether in 1,2-propylene glycol, such as is available from BASF as HP 100.

[0150] The laundry formulations of the present invention may comprise at least one antimicrobial agent from the above list and / or combinations thereof and / or in combination with at least one other antimicrobial agent not listed here.

[0151] Antimicrobial agents may be added to the laundry formulations of the present invention at a concentration of 0.0001 to 10% relative to the total weight of polymer.

[0152] Preferably, the formulation contains 2-phenoxyethanol in a concentration of 0.01% to 5%, more preferably 0.1% to 2% and / or 4,4'-dichloro-2-hydroxydiphenyl ether in a concentration of 0.001% to 1%, more preferably 0.002% to 0.6% (in each case relative to the total weight of the polymer).

[0153] The preparations according to the invention may comprise at least one additional surfactant selected from nonionic surfactants and amphoteric surfactants.

[0154] Nonionic surfactants

[0155] Examples of (additional) surfactants are in particular nonionic surfactants. Preferred nonionic surfactants are alkoxylated alcohols and alkoxylated fatty alcohols, diblock and multiblock copolymers of ethylene oxide and propylene oxide, and reaction products of sorbitan with ethylene oxide or propylene oxide, and also alkylphenol ethoxylates, alkylglycosides, polyhydroxy fatty acid amides (glucamides) and so-called amine oxides.

[0156] Preferred examples of alkoxylated alcohols and alkoxylated fatty alcohols are compounds of the general formula (III)

[0157]

[0158] The variables are defined as follows:

[0159] R 1 Selected from straight chain C1-C 10 - alkyl, preferably ethyl, particularly preferably methyl,

[0160] R 2 Selected from C8-C 22 -alkyl, such as n-C8H 17 、nC 10 H 21 、nC 12 H 25 、nC14 H 29 、nC 16 H 33 or nC 18 H 37 ,

[0161] R 3 Selected from C1-C 10 -alkyl, methyl, ethyl, n-propyl, isopropyl, n-butyl, isobutyl, sec-butyl, tert-butyl, n-pentyl, isopentyl, sec-pentyl, neopentyl, 1,2-dimethylpropyl, isopentyl, n-hexyl, isohexyl, sec-hexyl, n-heptyl, n-octyl, 2-ethylhexyl, n-nonyl, n-decyl or isodecyl, m and n are in the range of 0 to 300, wherein the sum of n and m is at least 1. Preferably, m is in the range of 1 to 100 and n is in the range of 0 to 30.

[0162] Here, the compound of the general formula (III) may be a block copolymer or a random copolymer, and preferably a block copolymer.

[0163] Other preferred examples of alkoxylated alcohols and alkoxylated fatty alcohols are compounds of the general formula (IV)

[0164]

[0165] The variables are defined as follows:

[0166] R 1 are identical or different and are selected from straight-chain C1-C4-alkyl groups, preferably are identical in each case and are ethyl, particularly preferably methyl,

[0167] R 4 Selected from C6-C 20 -alkyl, especially n-C8H 17 、nC 10 H 21 、nC 12 H 25 、nC 14 H 29 、nC 16 H 33 、nC 18 H 37 ,

[0168] a is a number in the range of 0 to 6, preferably 1 to 6,

[0169] b is a number in the range of 0 to 20, preferably 4 to 20,

[0170] d is a number in the range of 4 to 25.

[0171] Preferably, at least one of a and b is greater than zero.

[0172] Here, the compound of the general formula (IV) may be a block copolymer or a random copolymer, and preferably a block copolymer.

[0173] Further suitable nonionic surfactants are selected from diblock and multiblock copolymers composed of ethylene oxide and propylene oxide. Further suitable nonionic surfactants are selected from ethoxylated or propoxylated sorbitan esters. Amine oxides, such as lauryl dimethylamine oxide ("laurylamine oxide") or alkylphenol ethoxylates or alkyl polyglycosides or polyhydroxy fatty acid amides (glucamides) are also suitable. An overview of suitable other nonionic surfactants can be found in EP-A 0 851 023 and DE-A 198 19 187.

[0174] Mixtures of two or more different nonionic surfactants may also be present.

[0175] Examples of amphoteric surfactants are C 12 -C 18 -Alkyl betaines and sulfobetaines.

[0176] The preparations according to the invention may also comprise water and additional organic solvents, such as ethanol or propylene glycol.

[0177] Additional optional ingredients may be, but are not limited to, viscosity modifiers, cationic surfactants, foam boosting or foam reducing agents, fragrances, dyes, optical brighteners and dye transfer inhibitors. Example

[0178] In the following paragraphs, several experimental examples are given to illustrate some aspects of the present invention. Synthesis of the embodiments of the present invention and comparative examples:

[0179] Synthesis of Oligoamines

[0180] Synthesis of Bis-(3,3'-aminopropyl)amine (Dipropylenetriamine, DPTA)

[0181] Acrylonitrile (7.8 kg, 0.15 kmol, 1.0 eq.) was introduced dropwise into an excess of 1,3-diaminopropane (27.0 kg, 0.36 kmol, 2.5 eq.) in a reaction vessel at 60° C. and maintained at 65° C. After the addition reaction was complete, the reaction was stirred at 60° C. for 2 hours and then cooled to room temperature. The crude mixture was then analyzed by GC chromatography and found to give a distribution of 45% (GC area-%) unreacted starting material, 47% (GC area-%) desired monocyanoethylated compound and 7% (GC area-%) dicyanoethylated compound (34.8 kg). Subsequently and without any further purification, the crude mixture was hydrogenated with ammonia (28-45 eq.) in a fixed bed pressure reactor catalyzed by a [Co]-catalyst at 90° C. and 200 bar hydrogen pressure. The crude oligoamine mixture was fractionally distilled under reduced pressure (140 to 20 mbar) and at elevated temperature (120-220° C. column temperature) to give DPTA as a colorless liquid (134° C.; 20 mbar; purity >99%).

[0182] GC analysis (30 m RTX5 Amin column; injection temperature at 60 °C, then heated to 280 °C at 10 °C / min): R t =11.39min (DPTA) and R t =17.25min(TPTA).

[0183] 1 H-NMR (500MHz,CDCl3):

[0184] 13 C-NMR (125MHz,CDCl3): Synthesis of Bis-(3,3'-aminopropyl)-1,3-propylenediamine (Tripropylenetetramine, TPTA)

[0185] Acrylonitrile (795 g, 15.0 mol, 2.05 eq.) was introduced dropwise into 1,3-diaminopropane (542 g, 7.3 mol, 1.0 eq.) in a reaction vessel at 13 ° C over 4 hours and kept below 15 ° C. After the addition reaction was complete, the reaction was stirred for another 2 hours at 15 ° C and then warmed to room temperature. Subsequently and without any further purification, the crude mixture was hydrogenated at 100 ° C and 200 bar hydrogen pressure in a batch pressure reactor catalyzed by Raney nickel catalyst (5 wt %) and stirred for 12 hours. After the reaction was complete, the reaction was quenched by purging the reaction vessel with nitrogen, the catalyst was removed by filtration and the volatiles were removed under reduced pressure. The desired target compound was obtained after distillation under reduced pressure (3 mbar) and at elevated temperature (170 ° C column temperature) and TPTA was obtained as a colorless liquid (130 ° C; 3 mbar; > 99% purity).

[0186] GC analysis (30 m RTX5 Amin column; injection temperature at 60 °C, then heated to 280 °C at 10 °C / min): R t =17.25min(TPTA).

[0187] 1 H-NMR (500MHz, MeOD):

[0188] 13 C-NMR (125 MHz, MeOD):

[0189] Synthesis of tris-(3,3',3"-aminopropyl)-1,3-propylenediamine (tetrapropylenepentamine, TPPA)

[0190] Acrylonitrile (339 g, 6.4 mol, 2.0 eq.) was introduced dropwise into a mixture of tripropylenetetramine (TPTA, 598 g, 3.2 mol, 1.0 eq.) in THF (750 mL) at 50 ° C in a reaction vessel over 3 hours. After the addition reaction was complete, the reaction was stirred at 50 ° C for another 2 hours and then cooled to room temperature. Subsequently and without any further purification, the crude mixture was hydrogenated in a batch pressure reactor catalyzed by Raney cobalt catalyst (5 wt. %) / THF at 120 ° C and 100 bar hydrogen pressure and stirred for 8 hours. After complete reaction, the reaction was quenched by purging the reaction vessel with nitrogen, the catalyst was removed by filtration and the solvent was removed under reduced pressure. The desired target compound was obtained after distillation under reduced pressure (2 mbar) and at elevated temperature (270 ° C column temperature) together with pentapropylenehexamine (PPHA) and TPPA was obtained as a yellow oil (147 ° C; 2 mbar; 93% purity).

[0191] GC analysis (30 m RTX5 Amin column; injection temperature at 80 °C, then heated to 280 °C at 15 °C / min): R t =20.23min(TPPA).

[0192] Polymer P1 (invention)

[0193] 96.03 g of dipropylenetriamine (DPTA, 0.83 mol, 1 eq.) and 10 g of water were loaded into a steel pressure reactor. The reactor was purged with nitrogen to remove air and a nitrogen pressure of 1 bar was set. The reactor was heated to 100° C. and 130 g of ethylene oxide (2.95 mol, 3.56 eq.) were metered into the reactor over 7 hours. Thereafter, the reaction mixture was kept at 100° C. for post-reaction. Volatile compounds were removed under vacuum and 221.5 g of a clear, highly viscous product were taken out of the reactor.

[0194] 39.8 g of the previously obtained product are charged into a steel pressure reactor and 2.4 g of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and a nitrogen pressure of 1 bar is set. The reactor is heated to 120° C. and 548 g of ethylene oxide (12.4 mol, 99.7 equivalents) are added over 6 hours. Volatile compounds are removed under vacuum and 589 g of a brown solid are obtained.

[0195] 200 g of the resulting ethoxylate (0.044 mol, 1 eq.) were heated to 60° C. and filled into a glass reactor under a nitrogen atmosphere. 16.2 g of dimethyl sulfate (0.13 mol, 2.9 eq.) were metered into the reactor in such a way that 1 ml of DMS was added per minute. During the addition, the temperature was increased to 70° C. After the addition was complete, the mixture was post-reacted at 70° C. for 2 hours. 3.6 g of sulfuric acid (0.036 mol, 0.9 eq.) was added to the reactor, the temperature was increased to 90° C. and the reactor was set under vacuum (15 mbar) for 3 hours. After the reaction was complete, 5.4 g of sodium hydroxide (50% aqueous solution) and 40 g of demineralized water were added and the orange liquid product was removed from the reactor.

[0196] Polymer P2 (invention)

[0197] 297.9 g of tripropylenetetramine (TPTA, 1.58 mol, 1 eq.) and 29.8 g of water were loaded into a steel pressure reactor. The reactor was purged with nitrogen to remove air and a nitrogen pressure of 2.5 bar was set. The reactor was heated to 100° C. and 335 g of ethylene oxide (7.61 mol, 4.81 eq.) were metered into the reactor over 10 hours. Thereafter, the reaction mixture was kept at 100° C. for 6 hours for post-reaction. Volatile compounds were removed under vacuum and 626.4 g of clear, highly viscous product were taken out of the reactor.

[0198] 100 g of the previously obtained product are charged into a steel pressure reactor and 5.5 g of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and a nitrogen pressure of 2 bar is set. The reactor is heated to 120° C. and 1270 g of ethylene oxide (28.8 mol, 115.2 equivalents) are added over 16 hours. Volatile compounds are removed under vacuum and 1374.2 g of a brown solid are obtained.

[0199] 705.1 g of the resulting ethoxylate (0.13 mol, 1 eq.) were heated to 60° C. and filled into a glass reactor under a nitrogen atmosphere. 62.1 g of dimethyl sulfate (0.49 mol, 3.8 eq.) were metered into the reactor in such a way that 1 ml of DMS was added per minute. During the addition, the temperature was increased to 70° C. After the addition was complete, the mixture was post-reacted at 70° C. for 2 hours. 8.0 g of sulfuric acid (0.08 mol, 0.6 eq.) was added to the reactor, the temperature was increased to 90° C. and the reactor was set under vacuum (15 mbar) for 3 hours. After the reaction was complete, 11.0 g of sodium hydroxide (50% aqueous solution) and 650 g of demineralized water were added and the orange liquid product was removed from the reactor.

[0200] Polymer P3 (present invention)

[0201] 138.9 g of tripropylenetetramine (TPTA, 0.74 mol, 1 eq.) and 13.9 g of water were loaded into a steel pressure reactor. The reactor was purged with nitrogen to remove air and a nitrogen pressure of 1 bar was set. The reactor was heated to 100° C. and 156 g of ethylene oxide (3.54 mol, 4.81 eq.) was metered into the reactor over 10 hours. Thereafter, the reaction mixture was kept at 100° C. for 5 hours for post-reaction. Volatile compounds were removed under vacuum and 290 g of clear, highly viscous product was taken out of the reactor.

[0202] 63 g of the previously obtained product are charged into a steel pressure reactor and 3.0 g of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and a nitrogen pressure of 1 bar is set. The reactor is heated to 120° C. and 696 g of ethylene oxide (15.8 mol, 100.3 eq.) are added over 10 hours. Volatile compounds are removed under vacuum and 754.8 g of a brown solid are obtained.

[0203] 556 g of the resulting ethoxylate (0.12 mol, 1 eq) were heated to 60° C. and filled into a glass reactor under a nitrogen atmosphere. 57.4 g of dimethyl sulfate (0.49 mol, 3.8 eq) were metered into the reactor in such a way that 1 ml of DMS was added per minute. During the addition, the temperature was increased to 70° C. After the addition was complete, the mixture was post-reacted at 70° C. for 2 hours. 7.0 g of sulfuric acid (0.07 mol, 0.6 eq) was added to the reactor, the temperature was increased to 90° C. and the reactor was set under vacuum (15 mbar) for 3 hours. After the reaction was complete, 10.0 g of sodium hydroxide (50% aqueous solution) and 500 g of demineralized water were added and the orange liquid product was removed from the reactor.

[0204] Polymer P4 (present invention)

[0205] 173.8 g of tripropylenetetramine (TPTA, 0.92 mol, 1 eq.) and 17.3 g of water were loaded into a steel pressure reactor. The reactor was purged with nitrogen to remove air and a nitrogen pressure of 2.5 bar was set. The reactor was heated to 100° C. and 195 g of ethylene oxide (4.43 mol, 4.81 eq.) was metered into the reactor over 10 hours. Thereafter, the reaction mixture was kept at 100° C. for 6 hours for post-reaction. Volatile compounds were removed under vacuum and 366.8 g of clear, highly viscous product was taken out of the reactor.

[0206] 60 g of the previously obtained product are charged into a steel pressure reactor and 4.9 g of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and a nitrogen pressure of 1 bar is set. The reactor is heated to 120° C. and 1159 g of ethylene oxide (26.2 mol, 174.6 eq.) are added over 15 hours. Volatile compounds are removed under vacuum and 1233 g of a brown solid are obtained.

[0207] 488.1 g of the resulting ethoxylate (0.06 mol, 1 eq) were heated to 60° C. and filled into a glass reactor under a nitrogen atmosphere. 29.3 g of dimethyl sulfate (0.23 mol, 3.87 eq) were metered into the reactor in such a way that 1 ml of DMS was added per minute. During the addition, the temperature was increased to 70° C. After the addition was complete, the mixture was post-reacted at 70° C. for 2 hours. 6.7 g of sulfuric acid (0.07 mol, 0.6 eq) were added to the reactor, the temperature was increased to 90° C. and the reactor was set under vacuum (15 mbar) for 3 hours. After the reaction was complete, 8.5 g of sodium hydroxide (50% aqueous solution) and 488.1 g of demineralized water were added and the orange liquid product was removed from the reactor.

[0208] Polymer P5 (present invention)

[0209] 83.3 grams of tripropylenetetramine (TPTA, 0.44 mole, 1 equivalent) and 8.3 grams of water are loaded into a steel pressure reactor. The reactor is purged with nitrogen to remove air and set a nitrogen pressure of 2.5 bar. The reactor is heated to 120°C and 93.5 grams of ethylene oxide (2.12 moles, 4.83 equivalents) are metered into the reactor in a manner that the internal pressure does not exceed 5.5 bar. Thereafter, the reaction mixture is maintained at 120°C for 6 hours for post-reaction. 9.1 grams of potassium hydroxide (50% aqueous solution) are added and water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and set a nitrogen pressure of 2.5 bar. The reactor is heated to 140°C and 844 grams of ethylene oxide (19.2 moles, 43.6 equivalents) are added in a manner that the internal pressure does not exceed 5.5 bar. The mixture is post-reacted for 6 hours. Volatile compounds are removed under vacuum and 952.2 grams of brown viscous liquid are obtained.

[0210] 494 g of the alkoxylate obtained previously were loaded into a steel pressure reactor, inerted with nitrogen and heated to 140° C. A nitrogen prepressure of 2.5 bar was set and 667.4 g of ethylene oxide (15.15 mol, 34.4 equivalents) were added to the reactor in such a way that the internal pressure remained below 5.5 bar. The mixture was post-reacted for 6 hours. The volatile compounds were removed in vacuo and 1060.8 g of a brown solid were obtained as product.

[0211] 326.3 g of the resulting ethoxylate (0.06 mol, 1 eq) were heated to 60°C and filled into a glass reactor under a nitrogen atmosphere. 29.9 g of dimethyl sulfate (0.24 mol, 3.9 eq) were metered into the reactor in such a way that 1 ml of DMS was added per minute. During the addition, the temperature was raised to 70°C. After the addition was complete, the mixture was post-reacted at 70°C for 2 hours. 4.0 g of sulfuric acid (0.04 mol, 0.68 eq) was added to the reactor, the temperature was raised to 90°C and the reactor was set under vacuum (15 mbar) for 3 hours. After the reaction was complete, 9.14 g of triethanolamine and 143.1 g of demineralized water were added and the orange liquid product was removed from the reactor.

[0212] Polymer P6 (present invention)

[0213] 62.9 grams of tetrapropylene pentamine (TPPA, 0.26 mole, 1 equivalent) and 6.3 grams of water are loaded into a steel pressure reactor. The reactor is purged with nitrogen to remove air and set a nitrogen pressure of 3.5 bar. The reactor is heated to 100°C and 60 grams of ethylene oxide (1.36 moles, 5.2 equivalents) are metered into the reactor within 7 hours. Thereafter, the reaction mixture is maintained at 100°C for post-reaction. Volatile compounds are removed under vacuum and 6.2 grams of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and set a nitrogen pressure of 1.5 bar. The reactor is heated to 120°C and 1435 grams of ethylene oxide (32.575 moles, 125 equivalents) are added within 12 hours. Volatile compounds are removed under vacuum and 1589.2 grams of brown solids are obtained.

[0214] 314.2 g of the resulting ethoxylate (0.05 mol, 1 eq) were heated to 60° C. and filled into a glass reactor under a nitrogen atmosphere. 31.4 g of dimethyl sulfate (0.25 mol, 4.9 eq) were metered into the reactor in such a way that 1 ml of DMS was added per minute. During the addition, the temperature was increased to 70° C. After the addition was complete, the mixture was post-reacted at 70° C. for 2 hours. 3.5 g of sulfuric acid (0.036 mol, 0.7 eq) was added to the reactor, the temperature was increased to 90° C. and the reactor was set under vacuum (15 mbar) for 3 hours. After the reaction was complete, 5.0 g of sodium hydroxide (50% aqueous solution) and 300 g of demineralized water were added and the orange liquid product was removed from the reactor.

[0215] Comparative Example:

[0216] Polymer CP1 (comparison)

[0217] 297.9 g of tripropylenetetramine (TPTA, 1.58 mol, 1 eq.) and 29.8 g of water were loaded into a steel pressure reactor. The reactor was purged with nitrogen to remove air and a nitrogen pressure of 2.5 bar was set. The reactor was heated to 100° C. and 335 g of ethylene oxide (7.61 mol, 4.81 eq.) were metered into the reactor over 10 hours. Thereafter, the reaction mixture was kept at 100° C. for 6 hours for post-reaction. Volatile compounds were removed under vacuum and 626.4 g of clear, highly viscous product were taken out of the reactor.

[0218] 100 g of the previously obtained product are charged into a steel pressure reactor and 5.5 g of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and a nitrogen pressure of 2 bar is set. The reactor is heated to 120° C. and 1270 g of ethylene oxide (28.8 mol, 115.2 equivalents) are added over 16 hours. Volatile compounds are removed under vacuum and 1374.2 g of a brown solid are obtained.

[0219] Polymer CP2 (Comparison)

[0220] 99.1 g of tripropylenetetramine (TPTA, 0.53 mol, 1 eq.) and 9.9 g of water were loaded into a steel pressure reactor. The reactor was purged with nitrogen to remove air and a nitrogen pressure of 1.0 bar was set. The reactor was heated to 100° C. and 112 g of ethylene oxide (2.54 mol, 4.83 eq.) was metered into the reactor over a period of 6 hours. Thereafter, the reaction mixture was kept at 100° C. for 6 hours for post-reaction. Volatile compounds were removed under vacuum and 210 g of clear, highly viscous product was taken out of the reactor.

[0221] 39.2 g of the previously obtained product are charged into a steel pressure reactor and 1.1 g of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and a nitrogen pressure of 1 bar is set. The reactor is heated to 120° C. and 498 g of ethylene oxide (11.3 mol, 115.2 equivalents) are added over 10 hours. Volatile compounds are removed under vacuum and 536 g of a brown solid are obtained.

[0222] 115 g of the resulting ethoxylate (0.02 mol, 1 eq) were heated to 60° C. and filled into a glass reactor under a nitrogen atmosphere. 10.3 g of dimethyl sulfate (0.08 mol, 3.9 eq) were metered into the reactor with 1 ml of DMS added per minute. During the addition, the temperature was raised to 70° C. After the addition was complete, the mixture was post-reacted at 70° C. for 2 hours. Sodium hydroxide (50% aqueous solution) was added to set the pH to 8.2. The product was obtained as a light brown solid.

[0223] Polymer CP3 (Comparison)

[0224] 500 g of polypropylene imine and 17 g of water were loaded into a steel pressure reactor. The reactor was purged with nitrogen to remove air and a nitrogen pressure of 2.5 bar was set. The reactor was heated to 120° C. and 348 g of ethylene oxide was metered into the reactor over 6 hours. Thereafter, the reaction mixture was kept at 120° C. for 6 hours for post-reaction. Volatile compounds were removed under vacuum and 825 g of yellow, highly viscous product was taken out of the reactor.

[0225] 90 g of the previously obtained product are charged into a steel pressure reactor and 3.5 g of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and a nitrogen pressure of 2 bar is set. The reactor is heated to 120° C. and 783 g of ethylene oxide (17.8 mol) are added over 16 hours. Volatile compounds are removed under vacuum and 875 g of a brown solid are obtained.

[0226] Polymer CP4 (Comparison)

[0227] 500 g of polypropylene imine and 17 g of water were loaded into a steel pressure reactor. The reactor was purged with nitrogen to remove air and a nitrogen pressure of 2.5 bar was set. The reactor was heated to 120° C. and 348 g of ethylene oxide was metered into the reactor over 6 hours. Thereafter, the reaction mixture was kept at 120° C. for 6 hours for post-reaction. Volatile compounds were removed under vacuum and 825 g of yellow, highly viscous product was taken out of the reactor.

[0228] 90 g of the previously obtained product are charged into a steel pressure reactor and 3.5 g of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and a nitrogen pressure of 2 bar is set. The reactor is heated to 120° C. and 783 g of ethylene oxide (17.8 mol) are added over 16 hours. Volatile compounds are removed under vacuum and 875 g of a brown solid are obtained.

[0229] 78.1 g of the resulting ethoxylate were heated to 60° C. and filled into a glass reactor under a nitrogen atmosphere. 6.6 g of dimethyl sulfate (0.05 mol) were metered into the reactor in such a way that 1 ml of DMS was added per minute. During the addition, the temperature was raised to 70° C. After the addition was complete, the mixture was post-reacted at 70° C. for 2 hours and neutralized with 5.4 g of sodium hydroxide (50% aqueous solution), yielding 82.2 g of a brown solid.

[0230] 33.0 g of brown solid were heated to 60°C and 1.2 g of sulfuric acid were added to the reactor, the temperature was increased to 90°C and the reactor was set under vacuum (15 mbar) for 3 hours. After the reaction was complete, 2.7 g of sodium hydroxide (50% aqueous solution) was added. The product was obtained as a brown solid.

[0231] Polymer CP5 (Comparison)

[0232] 98.9 g of 1,3-propylenediamine (1,3-PDA, 1.33 mol, 1 eq.) and 9.9 g of water were loaded into a steel pressure reactor. The reactor was purged with nitrogen to remove air and a nitrogen pressure of 1.0 bar was set. The reactor was heated to 100° C. and 189 g of ethylene oxide (4.29 mol, 3.23 eq.) was metered into the reactor over 6 hours. Thereafter, the reaction mixture was kept at 100° C. for 6 hours for post-reaction. Volatile compounds were removed under vacuum and 210 g of clear, highly viscous product was taken out of the reactor.

[0233] 50.05 g of the previously obtained product are charged into a steel pressure reactor and 3.3 g of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and a nitrogen pressure of 1 bar is set. The reactor is heated to 120° C. and 788 g of ethylene oxide (17.9 mol, 76.9 equivalents) are added over 10 hours. Volatile compounds are removed under vacuum and 838.1 g of a brown solid are obtained.

[0234] 200 g of the resulting ethoxylate (0.06 mol, 1 eq) were heated to 60° C. and filled into a glass reactor under a nitrogen atmosphere. 13.8 g of dimethyl sulfate (0.11 mol, 1.9 eq) were metered into the reactor in such a way that 1 ml of DMS was added per minute. During the addition, the temperature was increased to 70° C. After the addition was complete, the mixture was post-reacted at 70° C. for 2 hours. 3.6 g of sulfuric acid (0.04 mol, 0.6 eq) were added to the reactor, the temperature was increased to 90° C. and the reactor was set under vacuum (15 mbar) for 3 hours. After the reaction was complete, 5.0 g of sodium hydroxide (50% aqueous solution) and 40 g of demineralized water were added and the orange liquid product was removed from the reactor.

[0235] Polymer CP6 (Comparison)

[0236] 364 g of hexamethylenediamine (HMDA, 3.13 mol, 1 eq.) and 36.4 g of water were loaded into a steel pressure reactor. The reactor was purged with nitrogen to remove air and a nitrogen pressure of 2.0 bar was set. The reactor was heated to 100° C. and 442 g of ethylene oxide (10.0 mol, 3.19 eq.) was metered into the reactor over a period of 6 hours. Thereafter, the reaction mixture was maintained at 100° C. for 6 hours for post-reaction. Volatile compounds were removed under vacuum and 795.2 g of clear, highly viscous product was taken out of the reactor.

[0237] 80 g (0.43 mol, 1.0 eq.) of the previously obtained product are charged into a steel pressure reactor and 3.3 g of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and a nitrogen pressure of 1 bar is set. The reactor is heated to 130° C. and 1053 g of ethylene oxide (23.9 mol, 55.7 eq.) are added over 15 hours. Volatile compounds are removed under vacuum and 1149.4 g of a brown solid are obtained.

[0238] 364 g of the resulting ethoxylate (0.1 mol, 1 eq.) were heated to 60° C. and filled into a glass reactor under a nitrogen atmosphere. 24.8 g of dimethyl sulfate (0.20 mol, 1.9 eq.) were metered into the reactor in such a way that 1 ml of DMS was added per minute. During the addition, the temperature was increased to 70° C. After the addition was complete, the mixture was post-reacted at 70° C. for 2 hours. 3.4 g of sulfuric acid (0.03 mol, 0.3 eq.) was added to the reactor, the temperature was increased to 90° C. and the reactor was set under vacuum (15 mbar) for 3 hours. After the reaction was complete, 3.27 g of sodium hydroxide (50% aqueous solution) and 384 g of demineralized water were added and the liquid product was removed from the reactor.

[0239] Polymer CP7 (Comparison)

[0240] 97.9 g of ethylenediamine (EDA, 1.63 mol, 1 eq.) and 9.7 g of water were loaded into a steel pressure reactor. The reactor was purged with nitrogen to remove air and a nitrogen pressure of 1.0 bar was set. The reactor was heated to 100° C. and 230 g of ethylene oxide (5.22 mol, 3.2 eq.) was metered into the reactor over 6 hours. Thereafter, the reaction mixture was maintained at 100° C. for 6 hours for post-reaction. Volatile compounds were removed under vacuum and 327 g of clear, highly viscous product was taken out of the reactor.

[0241] 42.6 g (0.21 mol, 1.0 eq.) of the previously obtained product are charged into a steel pressure reactor and 3.0 g of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and a nitrogen pressure of 1 bar is set. The reactor is heated to 130° C. and 717 g of ethylene oxide (16.3 mol, 77.5 eq.) are added over 15 hours. Volatile compounds are removed under vacuum and 752.8 g of a brown solid are obtained.

[0242] 200 g of the resulting ethoxylate (0.06 mol, 1 eq) were heated to 60° C. and filled into a glass reactor under a nitrogen atmosphere. 13.9 g of dimethyl sulfate (0.11 mol, 1.9 eq) were metered into the reactor in such a way that 1 ml of DMS was added per minute. During the addition, the temperature was increased to 70° C. After the addition was complete, the mixture was post-reacted at 70° C. for 2 hours. 4.2 g of sulfuric acid (0.04 mol, 0.6 eq) were added to the reactor, the temperature was increased to 90° C. and the reactor was set under vacuum (15 mbar) for 3 hours. After the reaction was complete, 7.8 g of sodium hydroxide (50% aqueous solution) and 40 g of demineralized water were added and the orange liquid product was removed from the reactor.

[0243] Polymer CP8 (Comparison)

[0244] 96.7 g of diethylenediamine (DETA, 0.94 mol, 1 eq.) and 9.7 g of water were loaded into a steel pressure reactor. The reactor was purged with nitrogen to remove air and a nitrogen pressure of 1.0 bar was set. The reactor was heated to 100° C. and 136 g of ethylene oxide (3.08 mol, 3.3 eq.) were metered into the reactor over 6 hours. Thereafter, the reaction mixture was kept at 100° C. for 6 hours for post-reaction. Volatile compounds were removed under vacuum and 231 g of clear, highly viscous product were taken out of the reactor.

[0245] 45.9 g (0.16 mol, 1.0 eq.) of the previously obtained product are charged into a steel pressure reactor and 2.9 g of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and a nitrogen pressure of 1 bar is set. The reactor is heated to 130° C. and 696 g of ethylene oxide (15.8 mol, 98.8 eq.) are added over 15 hours. Volatile compounds are removed under vacuum and 732.7 g of a brown solid are obtained.

[0246] 200 g of the resulting ethoxylate (0.04 mol, 1 eq.) were heated to 60° C. and filled into a glass reactor under a nitrogen atmosphere. 16.5 g of dimethyl sulfate (0.13 mol, 2.9 eq.) were metered into the reactor in such a way that 1 ml of DMS was added per minute. During the addition, the temperature was increased to 70° C. After the addition was complete, the mixture was post-reacted at 70° C. for 2 hours. 3.9 g of sulfuric acid (0.04 mol, 0.8 eq.) was added to the reactor, the temperature was increased to 90° C. and the reactor was set under vacuum (15 mbar) for 3 hours. After the reaction was complete, 6.8 g of sodium hydroxide (50% aqueous solution) and 40 g of demineralized water were added and the orange liquid product was removed from the reactor.

[0247] Polymer CP9 (Comparison)

[0248] 233.6 g of triethylenetetramine (TETA, 1.60 mol, 1 eq.) and 23.3 g of water were loaded into a steel pressure reactor. The reactor was purged with nitrogen to remove air and a nitrogen pressure of 1.0 bar was set. The reactor was heated to 100° C. and 338 g of ethylene oxide (7.67 mol, 4.8 eq.) was metered into the reactor over a period of 6 hours. Thereafter, the reaction mixture was maintained at 100° C. for 6 hours for post-reaction. Volatile compounds were removed under vacuum and 571 g of clear, highly viscous product was taken out of the reactor.

[0249] 46.3 g (0.13 mol, 1.0 eq.) of the previously obtained product are charged into a steel pressure reactor and 2.8 g of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and a nitrogen pressure of 1 bar is set. The reactor is heated to 130° C. and 658 g of ethylene oxide (14.9 mol, 114.9 eq.) are added over 15 hours. Volatile compounds are removed under vacuum and 694 g of a brown solid are obtained.

[0250] 200 g of the resulting ethoxylate (0.04 mol, 1 eq.) are heated to 60° C. and filled into a glass reactor under a nitrogen atmosphere. 17.4 g of dimethyl sulfate (0.14 mol, 3.75 eq.) are metered into the reactor in such a way that 1 ml of DMS is added per minute. During the addition, the temperature is increased to 70° C. After the addition is complete, the mixture is post-reacted at 70° C. for 2 hours. 3.0 g of sulfuric acid (0.03 mol, 0.8 eq.) are added to the reactor, the temperature is increased to 90° C. and the reactor is set under vacuum (15 mbar) for 3 hours. After the reaction is complete, 7.6 g of sodium hydroxide (50% aqueous solution) and 40 g of demineralized water are added and the viscous liquid product is removed from the reactor.

[0251] Polymer CP10 (Comparison)

[0252] PEI600+20EO / NH, synthesized as described in WO9532272 or US9738754.

[0253] Polymer CP11 (Comparison)

[0254] 400 g of tripropylenetetramine (TPTA, 2.12 mol, 1 eq.) and 40 g of water were loaded into a steel pressure reactor. The reactor was purged with nitrogen to remove air and a nitrogen pressure of 2.5 bar was set. The reactor was heated to 100° C. and 450 g of ethylene oxide (10.22 mol, 4.8 eq.) was metered into the reactor over 10 hours. Thereafter, the reaction mixture was kept at 100° C. for 6 hours for post-reaction. Volatile compounds were removed under vacuum and 945 g of clear, highly viscous product was taken out of the reactor.

[0255] 50.0 g (0.13 mol, 1.0 eq.) of the previously obtained product are filled into a steel pressure reactor and 3.0 g of potassium hydroxide (50% aqueous solution) are added. Water is removed under reduced pressure. The reactor is purged with nitrogen to remove air and a nitrogen pressure of 2 bar is set. The reactor is heated to 130° C. and 337 g of ethylene oxide (7.65 mol, 61.1 eq.) are added within 6 hours. The mixture is post-reacted for 6 hours. Thereafter, 87 g of propylene oxide (1.50 mol, 12.0 eq.) are metered into the reactor within 2 hours. The mixture is post-reacted for 6 hours at 130° C. Subsequently, 264 g of ethylene oxide (5.99 mol, 48.0 eq.) are metered into the reactor at 130° C. and the mixture is post-reacted for 6 hours. Volatile compounds are removed under vacuum and 755 g of a yellow viscous liquid are obtained.

[0256] 451.6 g of the resulting ethoxylate (0.08 mol, 1 eq.) were heated to 60° C. and filled into a glass reactor under a nitrogen atmosphere. 39.1 g of dimethyl sulfate (0.31 mol, 3.9 eq.) were metered into the reactor in such a way that 1 ml of DMS was added per minute. During the addition, the temperature was increased to 70° C. After the addition was complete, the mixture was post-reacted at 70° C. for 2 hours. 5.80 g of sulfuric acid (0.06 mol, 0.7 eq.) was added to the reactor, the temperature was increased to 90° C. and the reactor was set under vacuum (15 mbar) for 3 hours. After the reaction was complete, 7.9 g of sodium hydroxide (50% aqueous solution) and 440 g of demineralized water were added and the orange liquid product was removed from the reactor.

[0257] Polymer CP12 (Comparison)

[0258] PEI2000+32.5EO / NH, synthesized as described in WO2020 / 030469 (polymer P.2):

[0259] According to the procedure described in US 2010 / 0216949, 508.5 grams of completely dehydrated and CO-free PEI2000 were loaded in a 2-liter autoclave. Then, PEI2000 was made into an 85% by weight aqueous solution by adding 89 grams of H2O. The container was purged 3 times with a nitrogen pressure of up to 5 bar, and finally the container was inertized with a 2-bar nitrogen cushion. The temperature was balanced at 100°C, and then 261 grams of ethylene oxide were metered in over 6 hours and allowed to react further for 1 hour. The product PEI2000+0.5EO / NH was then purged with nitrogen to strip any residual EO, emptied from the reactor, and water and any residual EO were stripped. 53.0 grams of this material were loaded into a clean, empty 2-liter autoclave. Then 4.8 grams of 50% by weight KOH aqueous solution were metered in and stirred with PEI2000+0.5EO / NH. Subsequently, water was stripped from the mixture at 120°C at 10 mbar for 2 hours. The temperature was then raised to 130° C., the vessel was inertized with a 2 bar nitrogen blanket, 1150 g of ethylene oxide were metered in over 12 hours at a total pressure of about 3.5 bar (initial pressure) to about 8 bar (pressure at the end of EO metering), and left to react for at least 6 hours. The sample was then purged with nitrogen to strip off any residual EO, evacuated from the reactor, and water and any residual EO were stripped off in vacuo (20 mbar, 90° C.). 1223 g of a light brown solid were obtained.

[0260] Characterization of polymers

[0261] Molecular weight was determined by gel permeation chromatography (GPC). The conditions used were hexafluoroisopropanol and 0.05% potassium trifluoroacetate as solvents. The column oven temperature was set to 35°C and the flow rate was 1 mL / min. 50 μL of sample was injected and the sample concentration was set to 1.5 mg / mL. The sample was filtered using a Millipore Millflex FG (0.2 μm) filter after the polymer was dissolved to avoid column clogging. The following columns were used: HFIP guard column (diameter: 8 mm, length 5 cm), PL HFIP gel column (separation material styrene-divinylbenzene, diameter: 7.5 mm, length: 30 cm) and PL HFIPGel column (separation material styrene-divinylbenzene, diameter: 7.5 mm, length: 30 cm, exclusion size: 100–100000 g / mol). The GPC system was calibrated using PMMA standards in the molecular weight range of 800 to 2200000 g / mol. The eluate was detected using a refractive index (RI) detector (DRI Agilent 1000).

[0262] The analytical data for the inventive and comparative polymers are summarized in Table 1.

[0263] Table 1. Composition and physicochemical characterization of the amphiphilically modified oligopropyleneimine ethoxylates of the present invention and comparative polymers

[0264]

[0265] *MALLS detector

[0266] CP.1 and CP.2: polymers similar to the polymers according to the invention (ie based on oligopropyleneimine) but without the amphiphilic modification.

[0267] CP.3 and CP.4: polymers described in EP2961821.

[0268] CP.6 (and similar polymers CP.5 and CP.7 based on different amines): described in WO200424858.

[0269] CP.8 and CP.9: polymers similar to the polymers of the present invention (ie based on oligopropyleneimine) but based on oligoethyleneimine.

[0270] CP.10: PEI ethoxylate as described in EP112593 (application), WO9532272 or US9738754 (synthesis).

[0271] CP.11: polymer containing mixed EO / PO alkoxylate chains, similar to the structures described in EP3039109 and EP3039057.

[0272] CP.12: PEI ethoxylate with high molecular weight, as described in WO2020 / 030469 (Polymer P.2).

[0273] Application Experiment

[0274] Initial cleaning performance

[0275] To determine the primary detergency, the cleaning performance on round red clay and yellow clay stains on polyester fabric (Warwick Equest, Consett, UK) was measured by measuring the color difference (ΔE) between the washed stain and the unstained white fabric using a reflectometer (Datacolor SF600 plus). Four round red clay stains and four yellow clay stains (i.e., 2 polyester test fabrics, each containing 2 round red clay stains and 2 yellow clay stains) were used in 1 experiment, and each experiment was repeated 3 times, so that a total of 12 washed stains were obtained for red clay and yellow clay under each test condition to calculate the average ΔE value. By using these ΔE values, the so-called "standardized cleaning performance" (ΔΔE) was calculated. "Standardized cleaning performance" (ΔΔE) is the performance difference between a laundry detergent comprising the corresponding amphiphilic modified oligopropyleneimine ethoxylate or comparative polymer vs. a laundry detergent not containing any amphiphilic modified oligopropyleneimine ethoxylate or comparative polymer.

[0276] Table 2 shows the composition of the laundry detergent. Table 3 shows the washing test conditions and Table 4 summarizes the resulting standardized cleaning performance. The standardized cleaning performance shown in Table 4 is the sum of the standardized cleaning performances for red and yellow clay. The greater the sum of the ΔΔE values, the greater the positive contribution of the corresponding amphiphilically modified oligopropyleneimine ethoxylate or comparative polymer to the cleaning performance.

[0277] Table 2. Composition of liquid laundry detergents

[0278]

[0279] *) All data are % active ingredient by weight, independent of the respective product form.

[0280] Table 3. Washing conditions used to evaluate primary detergency

[0281]

[0282] *) After the wash experiment, the test fabrics were rinsed with 12° fH water (2 times) and then dried overnight at ambient room temperature before being measured with the reflectometer.

[0283] Table 4. Results from the washing tests

[0284]

[0285] *) All data are % active ingredient by weight, independent of the respective product form.

[0286] **) The 95% confidence interval of the used method for ΔΔE sum is + / - 1.5.

[0287] Note: Comparative polymers CP.10 and CP.12 (both based on PEI core) show significantly worse performance than the polymers of the invention, even at three times higher concentration levels. At a lower concentration level of 0.83 wt%, no significant cleaning performance can be detected for CP.12 at all.

[0288] The results from the washing tests clearly demonstrate the superior performance of the polymers of the invention compared to the comparative polymers described in the prior art. All comparative polymers except CP.2 and CP.11 exhibit significantly inferior performance to the polymers of the invention. If the 95% confidence interval of the method used is taken into account, the comparative polymer CP.2 exhibits directionally inferior performance compared to the polymers of the invention.

[0289] Viscosity

[0290] In order to determine the influence of the polymer on the viscosity of liquid laundry formulations, 0.5% by weight or 1.45% by weight of the amphiphilically modified oligopropyleneimine ethoxylate or the comparative polymer were formulated in each case into a liquid detergent containing a fixed content of 0.85% by weight of a HASE thickening polymer (formulation F.1). The pH was adjusted to pH 7.5 with a 50% by weight aqueous NaOH solution. The formulation was stirred for 2 hours with a magnetic stirrer and subsequently stored for a further 24 hours without mechanical stirring. The viscosity of the samples was then measured at room temperature (23° C.) using a rotational rheometer Rheolab QC (Anton Paar, Ostfildern, Germany) with a spindle CC27. The measurements were carried out at shear rates of 0 to 1200 1 / s.

[0291] Table 5 shows the composition of the final formulations and Table 6 summarizes the viscosities obtained at a shear rate of 20 1 / s.

[0292] Table 5. Composition of liquid laundry formulations

[0293]

[0294] *) All data are % active ingredient by weight, independent of the respective product form.

[0295] Table 6. Viscosity of Liquid Laundry Formulations

[0296]

[0297] *) All data are % active ingredient by weight, independent of the respective product form.

[0298] **) The linearity standard deviation of the method used is + / - 10 mPa*s, obtained from measurements of 3 identical preparations.

[0299] Note: Similar to the washing tests (see Table 4), PEI ethoxylates CP.10 and CP.12 were used at 3 times higher concentration levels compared to all other polymers (polymers of the invention and comparative polymers).

[0300] The results from the viscosity measurements clearly demonstrate the superiority of the polymers according to the invention: compared to the comparative polymers investigated (except for comparative polymer CP.12, which, however, does not meet the target criteria for the polymers according to the invention due to its extremely poor cleaning performance (see Table 4)), in particular compared to comparative polymers CP.2 and CP.11, which already exhibit comparable cleaning performance (CP.11) or only slightly inferior cleaning performance (CP.2) (see Table 4), the polymers according to the invention result in significantly higher viscosities for liquid laundry detergents.

[0301] The combination of the results from Table 4 (cleaning performance) and Table 6 (viscosity of liquid laundry detergents) clearly demonstrates that only the polymers of the present invention bring about the desired target conditions of excellent cleaning performance (especially at low concentrations, preferably <1 wt % in liquid laundry detergents) and high viscosity of detergent formulations.

Claims

1. Amphoteric modified oligopropylene imine ethoxylate (A) of general formula (I) in R 1 are identical or different and are selected from C1-C4-alkyl, H and a free electron pair, wherein all R 1 at least 50% are C1-C4-alkyl, EO means -CH2-CH2-O, Y is the same or different and is selected from SO3 - and H, wherein at least 30% of all Y is SO3 - , x is the same or different and is selected from 5 to 50, and n is selected from 1, 2 and 3.

2. The amphiphilically modified oligopropylene imine ethoxylate (A) according to claim 1, wherein all R 1 80% are C1-C4-alkyl.

3. The amphiphilically modified oligopropylene imine ethoxylate (A) according to claim 1, wherein all R 1 At least 90% of the radicals are C1-C4-alkyl.

4. The amphiphilically modified oligopropyleneimine ethoxylate (A) according to claim 1, wherein at least 50% of all Y are SO3 - .

5. The amphiphilically modified oligopropyleneimine ethoxylate (A) according to claim 1, wherein x is selected from 10 to 40.

6. The amphiphilically modified oligopropylene imine ethoxylate (A) according to claim 1, wherein n=1, 2 or 3, R 1 At least 80% of the 1 =C1-C4-alkyl and Y=SO3 - The ratio is an average of 1.0:1.0 to 1.0:0.

8.

7. The amphiphilically modified oligopropylene imine ethoxylate (A) according to claim 6, wherein n=2 or 3, and all R 1 At least 90% of the radicals are methyl groups.

8. The amphiphilically modified oligopropylene imine ethoxylate (A) according to claim 6, wherein n=2, all R 1 At least 90% of the groups are methyl groups, and x=15-30.

9. A compound mixture comprising at least one amphiphilically modified oligopropyleneimine ethoxylate (A) according to any one of claims 1 to 8 with n=2 and at least one isomeric compound according to formula (II) in R 1 are identical or different and are selected from C1-C4-alkyl, H and a free electron pair, wherein all R 1 at least 50% are C1-C4-alkyl, EO means -CH2-CH2-O, Y is the same or different and is selected from SO3 - and H, wherein at least 30% of all Y is SO3 - , x is the same or different and is selected from 5 to 50.

10. A mixture according to claim 9, wherein all R 1 80% are C1-C4-alkyl.

11. A mixture according to claim 9, wherein all R 1 At least 90% of the radicals are C1-C4-alkyl.

12. A mixture according to claim 9, wherein at least 50% of all Y is SO3 - .

13. The mixture according to claim 9, comprising the amphiphilically modified oligopropyleneimine ethoxylate (A) according to formula (I) and the compound according to formula (II) in a total molar ratio of 10:1 or more.

14. Mixtures comprising the amphiphilically modified oligopropyleneimine ethoxylates (A) according to any of claims 1 to 8 or the compound mixtures according to any of claims 9 to 13, wherein the mixtures additionally comprise alkali metal and / or amine sulfates.

15. The mixture according to claim 14, wherein the mixture additionally comprises a sulfate salt of an alkanolamine.

16. A process for producing the amphiphilically modified oligopropyleneimine ethoxylate (A) according to any one of claims 1 to 8, comprising the steps of: (a) providing an amine selected from ammonia, 1,3-propylenediamine, bis-(3,3'-aminopropyl)amine and bis-(3,3'-aminopropyl)-1,3-propylenediamine or a mixture thereof, (b) optionally, cyanoethylation of the amine with acrylonitrile in a ratio of 100:1 to 1:2.5 followed by hydrogenation to obtain oligopropyleneimines having 2, 3 and 4 repeating units, (c) optionally, purification of the oligopropylene imine from step (b), (d) ethoxylation of the amine and / or oligopropyleneimine from step a, b or c, and (e) At least partial quaternization and transsulfation with di-C1-C4-alkyl sulfates.

17. The process according to claim 16, wherein the purification step (c) is carried out to obtain oligopropyleneimines having 2, 3 and 4 repeating units or mixtures thereof in a purity of at least 80% by weight.

18. The process according to claim 16 or 17, wherein the at least partial quaternization in step (e) is carried out with dimethyl sulfate.

19. The process according to claim 16 or 17, wherein the transsulfation in step (e) is carried out using sulfuric acid as catalyst.

20. The process according to claim 16 or 17, wherein the transsulfation in step (e) is carried out at a quantitative level of ≥ 80% and a weakly cationic or net neutral polymer is obtained.

21. The process according to claim 19, wherein the process comprises a subsequent step of neutralizing the sulfuric acid with a base selected from the group consisting of alkali metal hydroxides and amines.

22. A process according to claim 21, wherein the base used to neutralize the sulfuric acid is selected from alkanolamines.

23. The process according to claim 16 or 17, wherein the ethoxylation in step (d) is carried out in two sub-steps: (i) conversion with up to 1 mol of ethylene oxide per NH function, followed by (ii) Conversion with more ethylene oxide under basic catalysis.

24. The amphiphilically modified oligopropyleneimine ethoxylate (A) according to any one of claims 1 to 8, obtainable by a process according to any one of claims 16 to 23.

25. Use of the amphiphilically modified oligopropyleneimine ethoxylate (A) according to any one of claims 1 to 8 or the mixture according to any one of claims 9 to 15 in laundry applications.

26. Laundry preparation comprising at least one of the amphiphilically modified oligopropyleneimine ethoxylates (A) according to any one of claims 1 to 8 and / or the mixtures according to any one of claims 9 to 15.