A printing process for diversified book surfaces

By combining modified ketone-aldehyde resin and ink in a specific ratio, along with light drying technology and engraving treatment, the problems of ink unevenness and low printing efficiency are solved, achieving fast drying, high stability printing effect and beautiful pattern display.

CN115709607BActive Publication Date: 2024-10-15JIANGSU PHOENIX YANCHENG PRINTING
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211373351.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-11-04
Publication Date
2024-10-15
Estimated Expiration
2042-11-04

AI Technical Summary

Technical Problem

In existing technologies, the ink has poor uniformity and stability, which easily leads to bubbles and unevenness during the printing process, resulting in low printing efficiency, unattractive and poorly formed patterns.

Method used

The ink, composed of modified ketone-aldehyde resin and raw materials in a specific ratio, is combined with light drying technology. First, it is engraved and recessed on the prominent display area of ​​the book cover. Then, it is mounted, inked, and printed on the printing press. Finally, it is sprayed with wax to improve the printing effect and aesthetics.

Benefits of technology

It enables rapid drying and curing of ink, improves printing efficiency and effect, ensures the stability and aesthetics of printed patterns, and enhances the waterproof and stain-resistant properties of book covers.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention relates to the technical field of book printing technology, and in particular to a printing process with diversified book surfaces. The following technical scheme is proposed: comprising the following steps: S1, arranging the designed book covers neatly and orderly, keeping the book covers clean and dry; S2, imprinting the prominently displayed parts of the book covers, so that the prominently displayed parts are recessed to a certain depth; S3, installing plates, applying ink materials, and testing the embossing on a printing machine; S4, conveying, formally embossing, and drying the book covers; the ink in step S3 is composed of the following parts by weight: 40-60 parts of waterborne polyurethane resin, 10-20 parts of modified ketone-aldehyde resin, 15-25 parts of water-based pigment, 5-10 parts of 1,2-propylene glycol, 4-12 parts of acryloyl morpholine, 3-9 parts of water-soluble titanate coupling agents, and 4-8 parts of curing agents. The raw materials obtained by the ratio of the present invention have the performance of fast printing, and the stability of the printing ink is high, which ensures the effect of printing, and the printing process is simple and efficient.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of book printing technology, and in particular to a printing technology for diversified book surfaces. Background Art

[0002] Books are a medium that records information in the form of text or images. They are usually bound together with many pages and protected by covers. In order to display the key content of the book, key pictures or key texts are printed on the cover of the book. The diversified display makes the book easy to classify and convenient for people to find. Printing is an indispensable process in book processing. With the progress of society, printing technology has also been vigorously developed. Ink is used in the printing process. Due to the large printing volume, the demand for ink is also very large.

[0003] In the prior art, the uniformity and stability of ink are not good enough. After the ink is stored for a certain period of time, it is necessary to mix the ink to make the raw materials inside the ink fully and evenly distributed. However, bubbles will be generated inside the ink during the mixing process, and the surface of the ink will foam, which will directly affect the printing effect and quality; the printing volume is large, and it cannot be dried quickly after printing, and the efficiency is low;

[0004] When designing a printed pattern, in order to highlight the display content, sometimes some pictures or texts are printed emphatically, so that the pattern or text will protrude from the cover. Although this solves the problem of the prominent display effect, the complete protrusion appears unsightly and uneven, and the molding stability is poor. In view of the above defects, we propose a printing process for diversified book surfaces. Summary of the invention

[0005] The purpose of the present invention is to propose a printing process for diversified book surfaces in view of the problems existing in the background technology.

[0006] The technical solution of the present invention is a printing process for diversified book surfaces, comprising the following steps:

[0007] S1. Arrange the designed book covers neatly and orderly, and keep the book covers clean and dry;

[0008] S2. Carve a mark on the protruding portion of the book cover so that the protruding portion is recessed to a certain depth;

[0009] S3, install the plate, apply ink and test the printing on the printing machine;

[0010] S4, transport, formally stamp and dry the book cover;

[0011] S5. Spray wax on the printed book cover and then seal it with film.

[0012] The ink in step S3 is composed of the following raw materials in parts by weight: 40-60 parts of aqueous polyurethane resin, 10-20 parts of modified ketone-aldehyde resin, 15-25 parts of aqueous pigment, 5-10 parts of 1,2-propylene glycol, 4-12 parts of acryloylmorpholine, 3-9 parts of water-soluble titanate coupling agent, 4-8 parts of curing agent, 3-7 parts of antioxidant, 4-10 parts of acrylate leveling agent, 3-7 parts of solvent, and 20-30 parts of purified water.

[0013] Preferably, the preparation of modified ketone-aldehyde resin:

[0014] Step a: adding polyetheretherketone powder into a reaction container, and then adding a mixture of chlorosulfonic acid and sulfur trioxide into the container, wherein the volume ratio of chlorosulfonic acid to sulfur trioxide is 2:1;

[0015] Step b: Stir thoroughly and react at a constant temperature for 16 hours, then let stand for 10 hours and filter the precipitate;

[0016] Step c: washing the liquid obtained in step b with distilled water until the liquid is neutral, and then drying;

[0017] Step d: Add the ketone-aldehyde resin powder into the container of step c and add a certain ratio of solvent, heat and stir until the raw materials are completely dissolved to obtain a modified ketone-aldehyde resin.

[0018] Preferably, the ink is composed of the following raw materials in parts by weight:

[0019] 45-55 parts of water-based polyurethane resin, 12-18 parts of modified ketone-aldehyde resin, 18-22 parts of water-based pigment, 6-8 parts of 1,2-propylene glycol, 6-10 parts of acryloylmorpholine, 4-8 parts of water-soluble titanate coupling agent, 5-7 parts of curing agent, 4-6 parts of antioxidant, 5-8 parts of acrylate leveling agent, 4-6.5 parts of solvent, and 22-28 parts of purified water.

[0020] Preferably, the ink is composed of the following raw materials in parts by weight: 60 parts of water-based polyurethane resin, 20 parts of modified ketone-aldehyde resin, 25 parts of water-based pigment, 10 parts of 1,2-propylene glycol, 12 parts of acryloylmorpholine, 9 parts of water-soluble titanate coupling agent, 8 parts of curing agent, 7 parts of antioxidant, 10 parts of acrylate leveling agent, 7 parts of solvent, and 30 parts of purified water.

[0021] Preferably, the color of the water-based pigment is one or more combinations of white pigment, black pigment, yellow pigment, orange pigment, blue pigment, green pigment, red pigment and purple pigment.

[0022] Preferably, the curing agent is vinyltriamine curing agent.

[0023] Preferably, the antioxidant is a mixture of tert-butylhydroquinone and tea polyphenols.

[0024] Preferably, the solvent is toluene, dichloromethane, ethyl acetate or a mixture of two or more thereof.

[0025] Preferably, the preparation of the ink comprises the following steps:

[0026] Step 1: Add waterborne polyurethane resin and modified ketone-aldehyde resin into a container, then add a certain amount of pure water and solvent, stir well, and heat the container to completely melt the raw materials inside;

[0027] Step 2: Add water-based pigments of corresponding colors to the melted and evenly stirred raw materials, and stir them again;

[0028] Step 3: Add the well-proportioned 1,2-propylene glycol, acryloyl morpholine, water-soluble titanate coupling agent, curing agent, antioxidant, and acrylate leveling agent into another container, mix well, and set aside;

[0029] Step 4: Add the additives mixed evenly in step 3 into the container of step 2 in multiple times, stir for 10-20 minutes each time adding the additives, finally make the additives completely mixed in the raw materials, grind and filter to obtain ink.

[0030] Compared with the prior art, the present invention has the following beneficial technical effects:

[0031] 1. The present invention modifies the ketone-aldehyde resin and then adds the modified ketone-aldehyde resin into the raw material according to the ratio, so that the printed ink can be quickly dried and solidified under the light environment, thereby shortening the drying and setting time and improving the printing efficiency;

[0032] Second, the present invention adds 1,2-propylene glycol, acryloyl morpholine and water-soluble titanate coupling agent to the raw materials. The combination of the three greatly improves the miscibility of the ink material. The stability after mixing is high, and there will be no stratification or precipitation due to long-term storage, thereby improving the printing efficiency and ensuring the printing effect;

[0033] Third, the present invention performs engraving on the prominent display part of the book cover before printing, so that the prominent display part is sunken to a certain depth, thereby improving the beauty of the prominent printing and making the printed line contour more distinct;

[0034] Fourth, the present invention sprays wax on the book cover after printing, so that the surface color of the book is brighter and brighter and does not fade, the pattern and handwriting are prominent, which can give readers a three-dimensional sense of vision, and is waterproof and anti-fouling for long-term preservation. DETAILED DESCRIPTION

[0035] The technical solution of the present invention is further described below.

[0036] Embodiment 1

[0037] The present invention provides a printing process for diversified book surfaces, comprising the following steps:

[0038] S1. Arrange the designed book covers neatly and orderly, and keep the book covers clean and dry;

[0039] S2. Carve the highlighted part of the book cover to make the highlighted part concave to a certain depth, so that the ink has a better adhesion effect during printing and achieve a better printing effect;

[0040] S3, install the plate, apply ink and test the printing on the printing machine;

[0041] S4. Transporting, formally stamping and drying the book cover. The drying method is light drying. The greater the light intensity, the faster the drying speed.

[0042] S5. Spray wax on the printed book cover and then seal it with film; spray wax makes the surface color of the book brighter and brighter and does not fade, and the pattern and handwriting stand out, which can give readers a three-dimensional sense of vision. It is waterproof and anti-fouling for long-term preservation, and can make the book cover harder and have a better texture.

[0043] The ink in step S3 is composed of the following raw materials in parts by weight: 40 parts of water-based polyurethane resin, 10 parts of modified ketone-aldehyde resin, 15 parts of water-based pigment, 5 parts of 1,2-propylene glycol, 4 parts of acryloylmorpholine, 3 parts of water-soluble titanate coupling agent, 4 parts of curing agent, 3 parts of antioxidant, 4 parts of acrylate leveling agent, 3 parts of solvent, and 20 parts of purified water; wherein the color of the water-based pigment is one or more combinations of white pigment, black pigment, yellow pigment, orange pigment, blue pigment, green pigment, red pigment, and purple pigment; the curing agent is ethylenetriamine curing agent; the antioxidant is a mixture of tert-butylhydroquinone and tea polyphenols; the solvent is toluene or dichloromethane or ethyl acetate, or a mixture of toluene and dichloromethane, or a mixture of toluene and ethyl acetate, or a mixture of dichloromethane and ethyl acetate, or a mixture of toluene, dichloromethane and ethyl acetate.

[0044] Preparation of modified ketone-aldehyde resin:

[0045] Step a: Add polyetheretherketone powder into a reaction container, and then add a mixed solution of chlorosulfonic acid and sulfur trioxide into the container, wherein the volume ratio of chlorosulfonic acid to sulfur trioxide is 2:1.

[0046] Step b: Stir thoroughly and react at a constant temperature for 16 hours, then let stand for 10 hours and filter the precipitate;

[0047] Step c: washing the liquid obtained in step b with distilled water until the liquid is neutral, and then drying;

[0048] Step d: Add the ketone-aldehyde resin powder into the container of step c and add a certain ratio of solvent, heat and stir until the raw materials are completely dissolved to obtain a modified ketone-aldehyde resin, which can make the printed ink dry and solidify quickly under light, shortening the drying and setting time.

[0049] The preparation of the above ink comprises the following steps:

[0050] Step 1: Add waterborne polyurethane resin and modified ketone-aldehyde resin into a container, then add a certain amount of pure water and solvent, stir well, and heat the container to completely melt the raw materials inside;

[0051] Step 2: Add water-based pigments of corresponding colors to the melted and evenly stirred raw materials, and stir them again;

[0052] Step 3: Add the well-proportioned 1,2-propylene glycol, acryloyl morpholine, water-soluble titanate coupling agent, curing agent, antioxidant, and acrylate leveling agent into another container, mix well, and set aside;

[0053] Step 4: Add the additives mixed evenly in step 3 into the container of step 2 in multiple times, stir for 10 minutes each time adding the additives, finally make the additives completely mixed in the raw materials, grind and filter to obtain ink.

[0054] In the above embodiment, the printed book surface has a good sense of contour, and the key printing area is prominent and not abrupt; the ink material composed of the above-mentioned raw material ratio by weight has good stability. The ink material is stored at room temperature for three months without stratification or bottom precipitation. It can be directly inked and printed, ensuring the efficiency and uniformity of printing. The drying speed is also faster than that of traditional inks, and it can be completely dried in 20 seconds under light at 40°C.

[0055] Embodiment 2

[0056] The present invention provides a printing process for diversified book surfaces, comprising the following steps:

[0057] S1. Arrange the designed book covers neatly and orderly, and keep the book covers clean and dry;

[0058] S2. Carve the highlighted part of the book cover to make the highlighted part concave to a certain depth, so that the ink has a better adhesion effect during printing and achieve a better printing effect;

[0059] S3, install the plate, apply ink and test the printing on the printing machine;

[0060] S4. Transporting, formally stamping and drying the book cover. The drying method is light drying. The greater the light intensity, the faster the drying speed.

[0061] S5. Spray wax on the printed book cover and then seal it with film; spray wax makes the surface color of the book brighter and brighter and does not fade, and the pattern and handwriting stand out, which can give readers a three-dimensional sense of vision, and is waterproof and anti-fouling for long-term preservation.

[0062] The ink in step S3 is composed of the following raw materials in parts by weight: 45-55 parts of waterborne polyurethane resin, 12-18 parts of modified ketone-aldehyde resin, 18-22 parts of waterborne pigment, 6-8 parts of 1,2-propylene glycol, 6-10 parts of acryloylmorpholine, 4-8 parts of water-soluble titanate coupling agent, 5-7 parts of curing agent, 4-6 parts of antioxidant, 5-8 parts of acrylate leveling agent, 4-6.5 parts of solvent, and 22-28 parts of purified water;

[0063] The colors of the water-based pigment are: one or more combinations of white pigment, black pigment, yellow pigment, orange pigment, blue pigment, green pigment, red pigment, and purple pigment; the curing agent is vinyltriamine curing agent; the antioxidant is a mixture of tert-butylhydroquinone and tea polyphenols; the solvent is toluene or dichloromethane or ethyl acetate, or a mixture of toluene and dichloromethane, or a mixture of toluene and ethyl acetate, or a mixture of dichloromethane and ethyl acetate, or a mixture of toluene, dichloromethane and ethyl acetate.

[0064] Preparation of modified ketone-aldehyde resin:

[0065] Step a: adding polyetheretherketone powder into a reaction container, and then adding a mixture of chlorosulfonic acid and sulfur trioxide into the container, wherein the volume ratio of chlorosulfonic acid to sulfur trioxide is 2:1;

[0066] Step b: Stir thoroughly and react at a constant temperature for 16 hours, then let stand for 10 hours and filter the precipitate;

[0067] Step c: washing the liquid obtained in step b with distilled water until the liquid is neutral, and then drying;

[0068] Step d: adding the ketone-aldehyde resin powder into the container of step c and adding a certain ratio of solvent, heating and stirring until the raw materials are completely dissolved to obtain a modified ketone-aldehyde resin; the printed ink can be quickly dried and solidified under light, thus shortening the drying and setting time.

[0069] The preparation of the above ink comprises the following steps:

[0070] Step 1: Add waterborne polyurethane resin and modified ketone-aldehyde resin into a container, then add a certain amount of pure water and solvent, stir well, and heat the container to completely melt the raw materials inside;

[0071] Step 2: Add water-based pigments of corresponding colors to the melted and evenly stirred raw materials, and stir them again;

[0072] Step 3: Add the well-proportioned 1,2-propylene glycol, acryloyl morpholine, water-soluble titanate coupling agent, curing agent, antioxidant, and acrylate leveling agent into another container, mix well, and set aside;

[0073] Step 4: Add the additives mixed evenly in step 3 into the container of step 2 in multiple times, stir for 13-18 minutes each time the additives are added, and finally the additives are completely mixed in the raw materials, and then ground and filtered to obtain ink.

[0074] In the above embodiment, the highlighted part of the book cover is engraved before printing, so that the highlighted part is sunken to a certain depth, and then printed to make the key printing area stand out clearly and not appear abrupt; the ink material composed of the above-mentioned raw material ratios has higher stability, and the ink material can be stored at room temperature for 4-8 months without stratification or bottom precipitation, and can be directly inked and printed, thereby ensuring the efficiency and uniformity of printing; the drying speed is faster, and it can be completely dried in 12-16 seconds under light at 40°C, thereby improving the efficiency of printing.

[0075] Embodiment 3

[0076] The present invention provides a printing process for diversified book surfaces, comprising the following steps:

[0077] S1. Arrange the designed book covers neatly and orderly, and keep the book covers clean and dry;

[0078] S2. Carve the highlighted part of the book cover to make the highlighted part concave to a certain depth, so that the ink has a better adhesion effect during printing and achieve a better printing effect;

[0079] S3, install the plate, apply ink and test the printing on the printing machine;

[0080] S4. Transporting, formally stamping and drying the book cover. The drying method is light drying. The greater the light intensity, the faster the drying speed.

[0081] S5. Spray wax on the printed book cover and then seal it with film; spray wax makes the surface color of the book brighter and brighter and does not fade, and the pattern and handwriting stand out, which can give readers a three-dimensional sense of vision, and is waterproof and anti-fouling for long-term preservation.

[0082] The ink in step S3 is composed of the following raw materials in parts by weight: 60 parts of waterborne polyurethane resin, 20 parts of modified ketone-aldehyde resin, 25 parts of waterborne pigment, 10 parts of 1,2-propylene glycol, 12 parts of acryloylmorpholine, 9 parts of water-soluble titanate coupling agent, 8 parts of curing agent, 7 parts of antioxidant, 10 parts of acrylate leveling agent, 7 parts of solvent, and 30 parts of purified water;

[0083] The colors of the water-based pigment are: one or more combinations of white pigment, black pigment, yellow pigment, orange pigment, blue pigment, green pigment, red pigment, and purple pigment; the curing agent is vinyltriamine curing agent; the antioxidant is a mixture of tert-butylhydroquinone and tea polyphenols; the solvent is toluene or dichloromethane or ethyl acetate, or a mixture of toluene and dichloromethane, or a mixture of toluene and ethyl acetate, or a mixture of dichloromethane and ethyl acetate, or a mixture of toluene, dichloromethane and ethyl acetate.

[0084] Preparation of modified ketone-aldehyde resin:

[0085] Step a: adding polyetheretherketone powder into a reaction container, and then adding a mixture of chlorosulfonic acid and sulfur trioxide into the container, wherein the volume ratio of chlorosulfonic acid to sulfur trioxide is 2:1;

[0086] Step b: Stir thoroughly and react at a constant temperature for 16 hours, then let stand for 10 hours and filter the precipitate;

[0087] Step c: washing the liquid obtained in step b with distilled water until the liquid is neutral, and then drying;

[0088] Step d: adding the ketone-aldehyde resin powder into the container of step c and adding a certain ratio of solvent, heating and stirring until the raw materials are completely dissolved to obtain a modified ketone-aldehyde resin; the printed ink can be quickly dried and solidified under light, thus shortening the drying and setting time.

[0089] The preparation of the above ink comprises the following steps:

[0090] Step 1: Add waterborne polyurethane resin and modified ketone-aldehyde resin into a container, then add a certain amount of pure water and solvent, stir well, and heat the container to completely melt the raw materials inside;

[0091] Step 2: Add water-based pigments of corresponding colors to the melted and evenly stirred raw materials, and stir them again;

[0092] Step 3: Add the well-proportioned 1,2-propylene glycol, acryloyl morpholine, water-soluble titanate coupling agent, curing agent, antioxidant, and acrylate leveling agent into another container, mix well and set aside;

[0093] Step 4: Add the additives mixed evenly in step 3 into the container of step 2 in multiple times, stir for 20 minutes each time adding the additives, finally make the additives completely mixed in the raw materials, grind and filter to obtain ink.

[0094] In this embodiment, the ink material formed by the above-mentioned raw material ratio by weight has a very high stability. The ink material can be stored at room temperature for 12 months without stratification or bottom precipitation, and can maintain good uniformity. It can be directly inked and printed without shaking when used. The uniformity during printing is very good, the color is bright, and it has a good sense of outline, giving readers a very good reading experience; it dries quickly and can be completely dried in 8 seconds under light at 40°C. It can be printed quickly in large quantities, greatly improving the printing efficiency.

[0095] The above-mentioned specific embodiments are only several preferred embodiments of the present invention. Based on the technical solutions of the present invention and the relevant inspirations of the above-mentioned embodiments, those skilled in the art can make various alternative improvements and combinations to the above-mentioned specific embodiments.

Claims

1. A printing process for diversified book surfaces, characterized in that: The following steps are involved: S1. Arrange the designed book covers neatly and orderly, and keep the book covers clean and dry; S2. Carve a mark on the protruding portion of the book cover so that the protruding portion is recessed to a certain depth; S3, install the plate, apply ink and test the printing on the printing machine; S4, transport, formally stamp and dry the book cover; S5, spraying wax on the printed book cover, and then sealing the cover with film; The ink in step S3 is composed of the following raw materials in parts by weight: 40-60 parts of waterborne polyurethane resin, 10-20 parts of modified ketone-aldehyde resin, 15-25 parts of waterborne pigment, 5-10 parts of 1,2-propylene glycol, 4-12 parts of acryloylmorpholine, 3-9 parts of water-soluble titanate coupling agent, 4-8 parts of curing agent, 3-7 parts of antioxidant, 4-10 parts of acrylate leveling agent, 3-7 parts of solvent, and 20-30 parts of purified water; Preparation of modified ketone-aldehyde resin: Step a: adding polyetheretherketone powder into a reaction container, and then adding a mixture of chlorosulfonic acid and sulfur trioxide into the container, wherein the volume ratio of chlorosulfonic acid to sulfur trioxide is 2:1; Step b: Stir thoroughly and react at a constant temperature for 16 hours, then let stand for 10 hours and filter the precipitate; Step c: washing the liquid obtained in step b with distilled water until the liquid is neutral, and then drying; Step d: Add the ketone-aldehyde resin powder into the container of step c and add a certain ratio of solvent, heat and stir until the raw materials are completely dissolved to obtain a modified ketone-aldehyde resin.

2. A printing process for diversified book surfaces according to claim 1, characterized in that: The ink is composed of the following raw materials in parts by weight: 45-55 parts of water-based polyurethane resin, 12-18 parts of modified ketone-aldehyde resin, 18-22 parts of water-based pigment, 6-8 parts of 1,2-propylene glycol, 6-10 parts of acryloylmorpholine, 4-8 parts of water-soluble titanate coupling agent, 5-7 parts of curing agent, 4-6 parts of antioxidant, 5-8 parts of acrylate leveling agent, 4-6.5 parts of solvent, and 22-28 parts of purified water.

3. A printing process for diversified book surfaces according to claim 1, characterized in that: The ink is composed of the following raw materials in parts by weight: 60 parts of water-based polyurethane resin, 20 parts of modified ketone-aldehyde resin, 25 parts of water-based pigment, 10 parts of 1,2-propylene glycol, 12 parts of acryloylmorpholine, 9 parts of water-soluble titanate coupling agent, 8 parts of curing agent, 7 parts of antioxidant, 10 parts of acrylate leveling agent, 7 parts of solvent, and 30 parts of purified water.

4. A printing process for diversified book surfaces according to claim 3, characterized in that: The colors of water-based pigments are: one or more combinations of white pigment, black pigment, yellow pigment, orange pigment, blue pigment, green pigment, red pigment, and purple pigment.

5. A printing process for diversified book surfaces according to claim 1, characterized in that: The curing agent is vinyltriamine curing agent.

6. A printing process for diversified book surfaces according to claim 1, characterized in that: The antioxidant is a mixture of tert-butylhydroquinone and tea polyphenols.

7. A printing process for diversified book surfaces according to claim 1, characterized in that: The solvent is toluene, dichloromethane, ethyl acetate or a mixture of two or more thereof.

8. A printing process for diversified book surfaces according to any one of claims 1 to 7, characterized in that: The preparation of ink comprises the following steps: Step 1: Add waterborne polyurethane resin and modified ketone-aldehyde resin into a container, then add a certain amount of pure water and solvent, stir well, and heat the container to completely melt the raw materials inside; Step 2: Add water-based pigments of corresponding colors to the melted and evenly stirred raw materials, and stir them again; Step 3: Add the well-proportioned 1,2-propylene glycol, acryloyl morpholine, water-soluble titanate coupling agent, curing agent, antioxidant, and acrylate leveling agent into another container, mix well, and set aside; Step 4: Add the additives mixed evenly in step 3 into the container of step 2 in multiple times, stir for 10-20 minutes each time adding the additives, finally make the additives completely mixed in the raw materials, grind and filter to obtain ink.