A precious metal sintering process

By setting up connection holes on the back of the hollow embossed pattern of T-shaped connecting nails and porcelain bottles on the back of the hollow embossed pattern, combining the tight fit of clay and outer glaze and the compression treatment of the pressing device, the unstable precious metal embossed pattern in the prior art is solved. The problem of this has achieved stable sintering and aesthetic improvement of hollow relief patterns.

CN115716762BActive Publication Date: 2024-11-22BEIJING HUAJIANG CULTURE DEV CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211438107.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-11-16
Publication Date
2024-11-22
Estimated Expiration
2042-11-16

AI Technical Summary

Technical Problem

The existing precious metal sintering process cannot firmly fix the hollow relief patterns of larger mass, larger areas and multiple enclaves on the porcelain bottle, and are prone to fall off or deform, affecting the aesthetics.

Method used

T-shaped connecting nails are set on the back of the hollow embossed pattern with preset precious metal content, and corresponding connecting holes are reserved for the porcelain bottle embossed body through high-temperature clay, and the outer glaze and the second clay are closely matched with the pressing device. Maintain the pressing state of the pattern during the drying process and perform glaze firing treatment at a preset temperature.

Benefits of technology

Effectively fix the hollow relief pattern on the porcelain bottle to prevent falling off and deform, improve the three-dimensional effect and aesthetics of the pattern, and ensure the stability of the pattern and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115716762B_ABST
    Figure CN115716762B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of precious metal sintering technology, and in particular to a precious metal sintering process, comprising step S1, selecting a precious metal with a preset precious metal content to make a hollow relief pattern, and a T-shaped connecting pin is preset on the back of the precious metal; step S2, selecting a first clay to make a porcelain bottle embryo, reserving a connecting hole corresponding to the connecting pin, and then performing a first bisque firing at high temperature to obtain a porcelain bottle embryo; step S3, applying an outer glaze to the porcelain bottle embryo, attaching a second clay to the connecting pin, covering the hollow relief pattern on the porcelain bottle bisque fired embryo, and obtaining a porcelain bottle glazed embryo after drying; step S4, performing a second glaze firing on the porcelain bottle glazed embryo according to the properties of the precious metal material, and obtaining a precious metal porcelain bottle after the glaze firing is completed; step S5, grinding and polishing the hollow relief pattern on the surface of the precious metal porcelain bottle. The present invention controls the material and temperature to stably sinter a large mass of enclave-type hollow precious metal relief pattern on the porcelain bottle.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of precious metal sintering, and in particular to a precious metal sintering process. Background Art

[0002] Porcelain is made of porcelain stone, kaolin, quartz stone, mullite, etc., and is covered with glass glaze or painted on the surface. With the development of society, the combination of precious metals and porcelain can better reflect the functionality and ornamental value of porcelain. Among the existing sintering processes of precious metals and porcelain, the commonly used methods are direct surface inlay method, sol-gel method and gold foil coating method. Among them, the direct surface inlay method is affected by later use and is easy to fall off under large temperature differences and repeated stress. The sol-gel method is affected by the material and will cause a certain degree of environmental damage. The existing sintering technology cannot make the precious metal patterns on the porcelain surface with large mass maintain a relief pattern with obvious layers, and the gold foil covering technology is easily affected by scratches and bumps, which causes the gold foil on the surface of the porcelain bottle to fall off and expose the porcelain embryo, seriously affecting the appearance. Therefore, when making large porcelain bottles, the precious metal patterns cannot be made clear and vivid. Therefore, there is an urgent need for a production process that can sinter the hollow precious metal relief pattern firmly on the porcelain bottle through a sintering process and can maintain the relief pattern of the precious metal.

[0003] Chinese patent publication number: CN107573103A, discloses a method for sintering a precious metal layer on the surface of ceramic or glass, which uses three kinds of slurries: base slurry, body slurry and surface slurry; firstly, the base slurry is applied to the surface of the ceramic or glass, dried and sintered; then the body slurry is applied, dried and sintered; then the surface slurry is applied, dried and sintered, and then the precious metal layer can be formed on the surface of the ceramic or glass; the weight proportions of the base slurry components are: 50-70 parts of precious metal powder, 3-5 parts of glass powder, and 1-2 parts of boron powder. 1-5 parts of sand, 1-5 parts of wetting agent, 10-20 parts of polyethylene glycol, 15-20 parts of water; the weight proportions of the body slurry components are: 70-80 parts of precious metal powder, 1-3 parts of glass powder, 1-5 parts of wetting agent, 5-10 parts of polyethylene glycol, 15-20 parts of water; the weight proportions of the surface slurry components are: 80-90 parts of precious metal powder, 0.5-1.5 parts of glass powder, 1-5 parts of wetting agent, 5-10 parts of polyethylene glycol, 2-20 parts of water. This method can make the precious metal layer firmly attached to the porcelain, with controllable and uniform thickness, and is environmentally friendly; it can be seen that the method uses a method similar to the silver paste method. Although an environmentally friendly slurry material is used, it still cannot make a large mass and large area of ​​hollow precious metal relief patterns firmly attached to the porcelain bottle. Summary of the invention

[0004] To this end, the present invention provides a precious metal sintering process to overcome the problem in the prior art that a large-mass, large-area, and multi-enclave hollow precious metal relief pattern cannot be stably sintered on a porcelain bottle.

[0005] To achieve the above object, the present invention provides a precious metal sintering process, comprising:

[0006] Step S1, selecting a precious metal material with a preset precious metal content to make a hollow relief pattern of a preset pattern, wherein a T-shaped connecting nail is preset on the back of the hollow relief pattern;

[0007] Step S2, selecting a first clay of a preset composition to prepare a porcelain bottle embryo, and at the same time reserving a connection hole corresponding to the T-shaped connection pin of the hollow relief pattern, and then performing a first bisque firing and a first glaze firing at a preset temperature on the porcelain bottle embryo to prepare a porcelain bottle embryo;

[0008] Step S3, applying glaze to the raw body of the porcelain bottle, and attaching a second clay with a preset composition to the T-shaped connecting nail on the back of the hollow relief pattern, and at the same time covering the hollow relief pattern on the unglazed body of the porcelain bottle obtained in step S2, wherein the T-shaped connecting nail attached with the second clay is tightly fitted with the connecting hole of step S2, and after drying, a glazed body of the porcelain bottle is obtained;

[0009] Step S4, subjecting the porcelain bottle glazing body obtained in step S3 to a second glaze firing at a preset temperature according to the properties of the precious metal material, and obtaining a precious metal porcelain bottle after the second glaze firing is completed;

[0010] Step S5, grinding and polishing the hollow relief pattern on the surface of the precious metal porcelain bottle obtained in step S4 to improve the smoothness of the hollow relief pattern.

[0011] In step S1, the precious metal includes gold, silver and platinum, the preset precious metal content includes precious metal contents of different purities, the hollow relief pattern includes an overall relief pattern and an enclave relief pattern, the background of the hollow relief pattern includes precious metal and colored glaze, and the backs of the overall relief pattern and the enclave relief pattern are both provided with T-shaped connecting nails, wherein the number of the T-shaped connecting nails on the backs of the overall relief pattern and the enclave relief pattern within the preset area is at least 2 respectively;

[0012] In step S2, the first clay is high-temperature clay, the depth of the connection hole reserved for the porcelain bottle embryo is half of the thickness of the embryo at the position of the connection hole of the porcelain bottle embryo, and corresponds to the T-shaped connection nail provided on the back of the hollow relief pattern, so that the T-shaped connection nail can be inserted into the connection hole reserved for the porcelain bottle embryo, and the porcelain bottle embryo is subjected to a high-temperature first bisque firing at a preset temperature, wherein the preset temperature is consistent with the sintering temperature of the first clay, so as to perform a high-temperature first bisque firing on the porcelain bottle embryo and form it to form a porcelain bottle embryo, and the high-temperature first bisque firing also includes firing the inner glaze of the porcelain bottle at a preset temperature, and the preset temperature of the inner glaze firing is consistent with the standard sintering temperature of the inner glaze applied;

[0013] In step S3, first, an outer glaze is applied to the raw porcelain bottle body, and the second clay attached to the T-shaped connecting pin is tightly fitted with the T-shaped connecting pin, and its shape is consistent with the shape of the connecting hole, so as to be inserted into the connecting hole reserved in the porcelain bottle body and tightly fit with the edge of the connecting hole, so as to make the sintered second clay tightly fit with the raw porcelain bottle body and fix the hollow relief pattern. After the hollow relief pattern is fitted to the raw porcelain bottle body, the edge of the hollow relief pattern is tightly covered with an outer glaze to prevent a gap from being generated between the hollow relief pattern and the raw porcelain bottle body, and then dried;

[0014] In step S3, the T-shaped connecting nail with the second clay is closely attached to the edge of the connecting hole. In order to make the T-shaped connecting nail with the second clay closely attached to the edge of the connecting hole, the volume of the T-shaped connecting nail with the second clay is limited, the volume of the connecting hole is preset as V1, the volume of the T-shaped connecting nail with the second clay is preset as V2, and V1<V2≤105%V1;

[0015] In step S3, the T-shaped connecting nail with the second clay is tightly fitted with the edge of the connecting hole, so as to make the sintered second clay tightly fit with the porcelain bottle embryo and fix the hollow relief pattern. In order to make the hollow relief pattern tightly fit with the porcelain bottle embryo, after the T-shaped connecting nail with the second clay is inserted into the connecting hole, the hollow relief pattern is pressed by a pressing device, and at the same time, it is dried for a preset time in the pressed state, wherein,

[0016] The pressing device includes a base, a fixing rod and a plurality of pressing units, wherein:

[0017] The base connects the fixing rod and the pressing unit and is used to support the fixing rod and the pressing unit.

[0018] The fixing rod includes a first trapezoidal screw mechanism, a second trapezoidal screw mechanism, a third trapezoidal screw mechanism and a first fixing device, wherein the first trapezoidal screw mechanism is connected to the second trapezoidal screw mechanism, the second trapezoidal screw mechanism is connected to the third trapezoidal screw mechanism, the first trapezoidal screw mechanism is used to adjust the height of the second trapezoidal screw mechanism, the second trapezoidal screw mechanism is used to adjust the horizontal position of the third trapezoidal screw mechanism, the third trapezoidal screw mechanism is wrapped with a soft rubber protective layer, the soft rubber protective layer is used to protect the porcelain bottle so as to reduce the damage caused by the accidental collision of the third trapezoidal screw mechanism to the porcelain bottle, the third trapezoidal screw mechanism is used to adjust its own height so that the end of the third trapezoidal screw mechanism is against the bottom of the porcelain bottle to fix the porcelain bottle at the current position, the first fixing device is respectively connected to the base and the first trapezoidal screw mechanism, so as to fix the first trapezoidal screw mechanism on the base,

[0019] The pressing unit includes a fourth trapezoidal screw mechanism, a fifth trapezoidal screw mechanism, a sixth trapezoidal screw mechanism, a display screen and a second fixing device, wherein:

[0020] The fourth trapezoidal screw mechanism is connected to the fifth trapezoidal screw mechanism, the fifth trapezoidal screw mechanism is connected to the sixth trapezoidal screw mechanism, the fourth trapezoidal screw mechanism is used to adjust the height of the fifth trapezoidal screw mechanism, and the fifth trapezoidal screw mechanism is used to adjust the horizontal position of the sixth trapezoidal screw mechanism.

[0021] A soft rubber pad is provided at the end of the sixth trapezoidal screw mechanism, and the soft rubber pad is used to press the hollow relief pattern. A pressure sensor is provided in the soft rubber pad to detect the pressing pressure of the soft rubber pad on the hollow relief pattern, and output the pressure value to the display screen to ensure that the current pressing pressure is always within the pressure standard range P required for the hollow relief pattern to fit tightly with the porcelain bottle embryo, wherein P includes P1 and P2, and P1<P2. The second fixing device connects the base and the fourth trapezoidal screw mechanism to fix the fourth trapezoidal screw mechanism on the base;

[0022] In step S3, the number of the pressing units is equal to the number of the T-shaped connecting pins provided on the back of the hollow relief pattern, and the pressing point of the soft rubber pad in the pressing unit is consistent with the setting position of the T-shaped connecting pin;

[0023] In step S4, the dried porcelain bottle glaze embryo is subjected to a second glaze firing at a preset temperature, where the preset temperature is the firing temperature of the outer glaze, wherein the outer glaze includes a low-temperature outer glaze and a high-temperature outer glaze;

[0024] In step S3, the glaze firing temperature and process sequence of step S3 and step S4 are determined according to the firing temperature of the glaze applied to the raw porcelain bottle and the precious metal material of the hollow relief pattern, wherein:

[0025] When the material of the hollow relief pattern includes silver, and the raw porcelain vase is glazed with a low-temperature outer glaze, in step S3, the glaze firing temperature is less than 950° C., and the second clay of the preset composition is low-temperature clay;

[0026] When the material of the hollow relief pattern includes silver, and the porcelain bottle embryo is glazed with high-temperature outer glaze, in step S3, the second glaze firing is performed after the outer glaze is applied to the porcelain bottle embryo, and the glaze firing temperature is the firing temperature of the high-temperature glaze. After the firing is completed and the porcelain bottle glazed embryo is cooled, a T-shaped connecting nail with the second clay is inserted into the connection hole reserved for the porcelain bottle glazed embryo, and dried when the pressing device presses the hollow relief, wherein the second clay with a preset composition is low-temperature clay, and the third sintering is performed after drying, and the sintering temperature is less than 950°C;

[0027] When the material of the hollow relief pattern includes gold, and the raw porcelain vase is glazed with a low-temperature outer glaze, in step S3, the glaze firing temperature is less than 1000° C., and the second clay of the preset composition is low-temperature clay;

[0028] When the material of the hollow relief pattern includes gold, and the porcelain bottle embryo is glazed at high temperature, then in step S3, the second glaze firing is performed after the porcelain bottle embryo is glazed, and the glaze firing temperature is the firing temperature of the high-temperature glaze. After the firing is completed and the porcelain bottle glazed embryo is cooled, a T-shaped connecting nail with the second clay is inserted into the connection hole reserved for the porcelain bottle glazed embryo, and dried while the pressing device presses the hollow relief, wherein the second clay with a preset composition is low-temperature clay, and the third sintering is performed after drying, and the sintering temperature is less than 1000°C;

[0029] When the material of the hollow relief pattern includes platinum, and the raw porcelain vase is coated with a low-temperature outer glaze, then in step S3, the glaze firing temperature is the firing temperature of the low-temperature outer glaze, and the second clay of the preset composition is low-temperature pottery clay;

[0030] When the material of the hollow relief pattern includes platinum, and the raw porcelain vase is glazed with high-temperature outer glaze, then in step S3, the glaze firing temperature is the firing temperature of the high-temperature outer glaze, and the second clay of the preset composition is the first clay;

[0031] According to the precious metal materials used in the hollow relief pattern, the glaze firing temperature and process sequence of the precious metal material with the lowest melting point included in the materials are selected as the glaze firing temperature and process sequence of step S3, wherein the materials used in the hollow relief pattern include gold, silver, and platinum. Specifically, the melting points of gold, silver, and platinum are arranged as the melting point of silver < the melting point of gold < the melting point of platinum.

[0032] Compared with the prior art, the invention has the beneficial effect that, by arranging a T-shaped connecting nail on the back of the hollow relief pattern, the hollow relief pattern can be better fixed on the surface of the porcelain bottle embryo, and is not easy to fall off or deform.

[0033] Furthermore, by providing at least two T-shaped connecting nails within a preset area on the back of the overall relief pattern and / or the enclave relief pattern, the porcelain glaze can be used as a base to better set off the distinctive style and artistic conception of the pattern, and ensure that the enclave relief pattern is not easy to shake;

[0034] Furthermore, by providing a connection hole on the porcelain bottle embryo that corresponds to the position of the T-shaped connection nail on the back of the hollow relief pattern, the hollow relief pattern can be vividly displayed on the porcelain bottle, highlighting the three-dimensional effect of the relief, making the pattern more vivid, spiritual, and full of artistic conception;

[0035] Furthermore, by attaching a second clay having a shape corresponding to the shape of the connecting hole to the T-shaped connecting nail, the second clay can be better bonded to the porcelain bottle body, and the T-shaped connecting nail is fixed at the same time to ensure that the hollow relief pattern can be closely attached to the porcelain bottle body;

[0036] Furthermore, during the drying process, after the T-shaped connecting pins on the back of the hollow relief pattern are inserted into the corresponding connecting holes in the porcelain vase body by the pressing device, the hollow relief pattern is always pressed tightly, so that the hollow relief pattern can be kept in close contact with the porcelain vase body during the drying process, and the hollow relief pattern can be prevented from falling off, loosening and shifting due to its own gravity, thereby ensuring the stability of the hollow relief pattern during the secondary glaze firing;

[0037] Furthermore, through the plurality of trapezoidal screw mechanisms provided in the pressing device, the pressing device can better fix and press porcelain bottles of various types and sizes and hollow relief patterns at different positions, and the current pressing force is detected by the pressure sensor and output to the display screen at the same time, so that the problem of inconsistent product quality caused by pressing based on experience in the past can be solved;

[0038] Furthermore, by determining the firing temperature of the glaze applied to the raw porcelain vase and the precious metal material of the hollow relief pattern, corresponding adjustments can be made to the current sintering process to better match the current material properties, reduce the scrap rate, increase the yield rate, and at the same time improve product quality and expand economic benefits. BRIEF DESCRIPTION OF THE DRAWINGS

[0039] The drawings described herein are used to provide a further understanding of the present invention and constitute a part of this application. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings:

[0040] Figure 1 This is a schematic structural diagram of a noble metal sintering process according to an embodiment of the present invention;

[0041] Figure 2 This is a schematic diagram of the structure of a pressing device for the precious metal sintering process according to an embodiment of the present invention;

[0042] Figure 3 This is a schematic diagram of the fixing rod structure of the pressing device of the precious metal sintering process according to an embodiment of the present invention;

[0043] Figure 4 A schematic diagram of the structure of a pressing unit of a pressing device for a precious metal sintering process according to an embodiment of the present invention;

[0044] In the figure: a base 1, a first trapezoidal screw mechanism 2, a second trapezoidal screw mechanism 3, a third trapezoidal screw mechanism 4, a fourth trapezoidal screw mechanism 5, a fifth trapezoidal screw mechanism 6, a sixth trapezoidal screw mechanism 7, a soft rubber pad 8, and a soft rubber protective layer 9. DETAILED DESCRIPTION

[0045] In order to make the objects and advantages of the present invention more clearly understood, the present invention is further described below in conjunction with embodiments; it should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0046] The preferred embodiments of the present invention are described below with reference to the accompanying drawings. It should be understood by those skilled in the art that these embodiments are only used to explain the technical principles of the present invention and are not intended to limit the protection scope of the present invention.

[0047] It should be noted that, in the description of the present invention, terms such as "up", "down", "left", "right", "inside" and "outside" indicating directions or positional relationships are based on the directions or positional relationships shown in the drawings. This is merely for the convenience of description and does not indicate or imply that the device or element must have a specific orientation, be constructed and operated in a specific orientation. Therefore, it cannot be understood as a limitation on the present invention.

[0048] In addition, it should be noted that in the description of the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For those skilled in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0049] See also Figure 1 As shown, it is a structural schematic diagram of the precious metal sintering process according to an embodiment of the present invention, and this embodiment includes:

[0050] Step S1, selecting a precious metal material with a preset precious metal content to make a hollow relief pattern of a preset pattern, wherein a T-shaped connecting nail is preset on the back of the hollow relief pattern;

[0051] Step S2, selecting a first clay of a preset composition to obtain a porcelain bottle embryo, and at the same time reserving a connection hole corresponding to the T-shaped connection pin of the hollow relief pattern, and then performing a first bisque firing at a preset temperature on the porcelain bottle embryo to obtain a porcelain bottle embryo;

[0052] Step S3, applying glaze to the raw body of the porcelain bottle, and attaching a second clay with a preset composition to the T-shaped connecting nail on the back of the hollow relief pattern, and at the same time covering the hollow relief pattern on the unglazed body of the porcelain bottle obtained in step S2, wherein the T-shaped connecting nail attached with the second clay is tightly fitted with the connecting hole of step S2, and after drying, a glazed body of the porcelain bottle is obtained;

[0053] Step S4, subjecting the porcelain bottle glazing body obtained in step S3 to a second glaze firing at a preset temperature according to the properties of the precious metal material, and obtaining a precious metal porcelain bottle after the second glaze firing is completed;

[0054] Step S5, grinding and polishing the hollow relief pattern on the surface of the precious metal porcelain bottle obtained in step S4 to improve the smoothness of the hollow relief pattern.

[0055] In step S1, the precious metal includes gold, silver and platinum, the preset precious metal content includes precious metal contents of different purities, the hollow relief pattern includes an overall relief pattern and an enclave relief pattern, the background of the hollow relief pattern includes precious metal and colored glaze, and the backs of the overall relief pattern and the enclave relief pattern are both provided with T-shaped connecting nails, wherein the number of the T-shaped connecting nails on the backs of the overall relief pattern and the enclave relief pattern within the preset area is at least 2 respectively;

[0056] In step S2, the first clay is high-temperature clay, the depth of the connection hole reserved for the porcelain bottle embryo is half of the thickness of the embryo at the position of the connection hole of the porcelain bottle embryo, and corresponds to the T-shaped connection nail provided on the back of the hollow relief pattern, so that the T-shaped connection nail can be inserted into the connection hole reserved for the porcelain bottle embryo, and the porcelain bottle embryo is subjected to a high-temperature first bisque firing at a preset temperature, wherein the preset temperature is consistent with the sintering temperature of the first clay, so as to perform a high-temperature first bisque firing on the porcelain bottle embryo and form it to form a porcelain bottle embryo, and the high-temperature first bisque firing also includes firing the inner glaze of the porcelain bottle at a preset temperature, and the preset temperature of the inner glaze firing is consistent with the standard sintering temperature of the inner glaze applied;

[0057] In step S3, first, an outer glaze is applied to the raw porcelain bottle body, and the second clay attached to the T-shaped connecting pin is tightly fitted with the T-shaped connecting pin, and its shape is consistent with the shape of the connecting hole, so as to be inserted into the connecting hole reserved in the porcelain bottle body and tightly fit with the edge of the connecting hole, so as to make the sintered second clay tightly fit with the raw porcelain bottle body and fix the hollow relief pattern. After the hollow relief pattern is fitted to the raw porcelain bottle body, the edge of the hollow relief pattern is tightly covered with an outer glaze to prevent a gap from being generated between the hollow relief pattern and the raw porcelain bottle body, and then dried;

[0058] In step S3, the T-shaped connecting nail with the second clay is closely attached to the edge of the connecting hole. In order to make the T-shaped connecting nail with the second clay closely attached to the edge of the connecting hole, the volume of the T-shaped connecting nail with the second clay is limited, the volume of the connecting hole is preset as V1, the volume of the T-shaped connecting nail with the second clay is preset as V2, and V1<V2≤105%V1;

[0059] Please continue reading Figure 2 As shown, it is a schematic diagram of the structure of the pressing device of the precious metal sintering process of the embodiment of the present invention. In step S3, the T-shaped connecting nail with the second clay is tightly fitted with the edge of the connecting hole, so as to make the sintered second clay tightly fit with the porcelain bottle embryo and fix the hollow relief pattern. In order to make the hollow relief pattern tightly fit with the porcelain bottle embryo, after the T-shaped connecting nail with the second clay is inserted into the connecting hole, the pressing device is used to press the hollow relief pattern, and at the same time, it is dried for a preset time in the pressed state, wherein,

[0060] The pressing device includes a base, a fixing rod and a plurality of pressing units, wherein:

[0061] The base 1 is connected to the fixing rod and the pressing unit, and is used to support the fixing rod and the pressing unit.

[0062] The fixing rod includes a first trapezoidal screw mechanism 2, a second trapezoidal screw mechanism 3, a third trapezoidal screw mechanism 4 and a first fixing device (not shown in the figure), wherein the first trapezoidal screw mechanism 2 is connected to the second trapezoidal screw mechanism 3, the second trapezoidal screw mechanism 3 is connected to the third trapezoidal screw mechanism 4, the first trapezoidal screw mechanism 2 is used to adjust the height of the second trapezoidal screw mechanism 3, the second trapezoidal screw mechanism 3 is used to adjust the horizontal position of the third trapezoidal screw mechanism 4, the third trapezoidal screw mechanism 4 is wrapped with a soft rubber protective layer 9, the soft rubber protective layer 9 is used to protect the porcelain bottle so as to reduce the damage caused by the accidental collision of the third trapezoidal screw mechanism 4 to the porcelain bottle, the third trapezoidal screw mechanism 4 is used to adjust its own height so that the end of the third trapezoidal screw mechanism 4 is against the bottom of the porcelain bottle to fix the porcelain bottle at the current position, the first fixing device is respectively connected to the base 1 and the first trapezoidal screw mechanism 2, and is used to fix the first trapezoidal screw mechanism 2 on the base 1,

[0063] The pressing unit includes a fourth trapezoidal screw mechanism 5, a fifth trapezoidal screw mechanism 6, a sixth trapezoidal screw mechanism 7, a display screen (not shown in the figure) and a second fixing device (not shown in the figure), wherein:

[0064] The fourth trapezoidal screw mechanism 5 is connected to the fifth trapezoidal screw mechanism 7, and the fifth trapezoidal screw mechanism 6 is connected to the sixth trapezoidal screw mechanism 7. The fourth trapezoidal screw mechanism 5 is used to adjust the height of the fifth trapezoidal screw mechanism 6, and the fifth trapezoidal screw mechanism 6 is used to adjust the horizontal position of the sixth trapezoidal screw mechanism 7.

[0065] A soft rubber pad 8 is provided at the end of the sixth trapezoidal screw mechanism 7. The soft rubber pad 8 is used to press the hollow relief pattern. A pressure sensor is provided in the soft rubber pad 8 to detect the pressing pressure of the soft rubber pad 8 on the hollow relief pattern, and output the pressure value to the display screen to ensure that the current pressing pressure is always within the pressure standard range P required for the hollow relief pattern to fit tightly with the porcelain vase embryo, wherein P includes P1 and P2, and P1<P2. The second fixing device connects the base 1 and the fourth trapezoidal screw mechanism 5 to fix the fourth trapezoidal screw mechanism 5 on the base 1;

[0066] In step S3, the number of the pressing units is equal to the number of the T-shaped connecting pins provided on the back of the hollow relief pattern, and the pressing point of the soft rubber pad 8 in the pressing unit is consistent with the setting position of the T-shaped connecting pin;

[0067] In step S4, the dried porcelain bottle glaze embryo is subjected to a second glaze firing at a preset temperature, where the preset temperature is the firing temperature of the outer glaze, wherein the outer glaze includes a low-temperature outer glaze and a high-temperature outer glaze;

[0068] In step S3, the glaze firing temperature and process sequence of step S3 and step S4 are determined according to the firing temperature of the glaze applied to the raw porcelain bottle and the precious metal material of the hollow relief pattern, wherein:

[0069] When the material of the hollow relief pattern includes silver, and the raw porcelain vase is glazed with a low-temperature outer glaze, in step S3, the glaze firing temperature is less than 950° C., and the second clay of the preset composition is low-temperature clay;

[0070] When the material of the hollow relief pattern includes silver, and the porcelain bottle embryo is glazed with high-temperature outer glaze, in step S3, the second glaze firing is performed after the outer glaze is applied to the porcelain bottle embryo, and the glaze firing temperature is the firing temperature of the high-temperature glaze. After the firing is completed and the porcelain bottle glazed embryo is cooled, a T-shaped connecting nail with the second clay is inserted into the connection hole reserved for the porcelain bottle glazed embryo, and dried when the pressing device presses the hollow relief, wherein the second clay with a preset composition is low-temperature clay, and the third sintering is performed after drying, and the sintering temperature is less than 950°C;

[0071] When the material of the hollow relief pattern includes gold, and the raw porcelain vase is glazed with a low-temperature outer glaze, in step S3, the glaze firing temperature is less than 1000° C., and the second clay of the preset composition is low-temperature clay;

[0072] When the material of the hollow relief pattern includes gold, and the porcelain bottle embryo is glazed at high temperature, then in step S3, the second glaze firing is performed after the porcelain bottle embryo is glazed, and the glaze firing temperature is the firing temperature of the high-temperature glaze. After the firing is completed and the porcelain bottle glazed embryo is cooled, a T-shaped connecting nail with the second clay is inserted into the connection hole reserved for the porcelain bottle glazed embryo, and dried while the pressing device presses the hollow relief, wherein the second clay with a preset composition is low-temperature clay, and the third sintering is performed after drying, and the sintering temperature is less than 1000°C;

[0073] When the material of the hollow relief pattern includes platinum, and the raw porcelain vase is coated with a low-temperature outer glaze, then in step S3, the glaze firing temperature is the firing temperature of the low-temperature outer glaze, and the second clay of the preset composition is low-temperature pottery clay;

[0074] When the material of the hollow relief pattern includes platinum, and the raw porcelain vase is glazed with high-temperature outer glaze, then in step S3, the glaze firing temperature is the firing temperature of the high-temperature outer glaze, and the second clay of the preset composition is the first clay;

[0075] According to the precious metal materials used in the hollow relief pattern, the glaze firing temperature and process sequence of the precious metal material with the lowest melting point included in the material are selected as the glaze firing temperature and process sequence of step S3, wherein the materials used in the hollow relief pattern include gold, silver, and platinum. Those skilled in the art can understand that the melting points of gold, silver, and platinum are arranged as the melting point of silver < the melting point of gold < the melting point of platinum.

[0076] So far, the technical solutions of the present invention have been described in conjunction with the preferred embodiments shown in the accompanying drawings. However, it is easy for those skilled in the art to understand that the protection scope of the present invention is obviously not limited to these specific embodiments. Without departing from the principle of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will fall within the protection scope of the present invention.

[0077] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A precious metal sintering process, It is characterized in that include: Step S1, selecting a precious metal material with a preset precious metal content to make a hollow relief pattern of a preset pattern, wherein a T-shaped connecting nail is provided on the back of the hollow relief pattern; Step S2, selecting a first clay of a preset composition to obtain a porcelain bottle blank, performing a first bisque firing and a first glaze firing at a preset temperature on the porcelain bottle blank to obtain a porcelain bottle blank, wherein the porcelain bottle blank is pre-reserved with a connection hole corresponding to the T-shaped connection pin of the hollow relief pattern; Step S3, applying outer glaze to the green body of the porcelain bottle, attaching a second clay of a preset composition to the T-shaped connecting nail, and covering the hollow relief pattern on the unglazed body of the porcelain bottle obtained in step S2, wherein the T-shaped connecting nail with the second clay attached is tightly fitted with the connecting hole of the porcelain bottle body, and after drying, a glazed body of the porcelain bottle is obtained; Step S4, performing a second glaze firing on the porcelain bottle glaze blank obtained in step S3 at a preset temperature according to the properties of the precious metal material, and obtaining a precious metal porcelain bottle after the second glaze firing is completed; Step S5, grinding and polishing the hollow relief pattern on the surface of the precious metal porcelain bottle obtained in step S4 to improve the smoothness of the hollow relief pattern.

2. The precious metal sintering process according to claim 1, It is characterized in that In the step S1, the preset precious metal content includes precious metal contents of different purities, the hollow relief pattern includes an overall relief pattern and an enclave relief pattern, the background of the hollow relief pattern includes precious metals and colored glaze, and the backs of the overall relief pattern and the enclave relief pattern are both provided with T-shaped connecting nails, wherein the number of T-shaped connecting nails on the backs of the overall relief pattern and the enclave relief pattern within the preset area is greater than or equal to 2.

3. The precious metal sintering process according to claim 2, It is characterized in that In step S2, the first clay is high-temperature clay, the depth of the connection hole reserved for the porcelain bottle blank is half of the thickness of the blank at the position of the connection hole of the porcelain bottle blank, and corresponds to the position of the T-shaped connecting nail, so that the T-shaped connecting nail can be inserted into the connection hole reserved for the porcelain bottle blank. In the high-temperature first bisque firing of the porcelain bottle blank at a preset temperature, the preset temperature is consistent with the sintering temperature of the first clay, so that the porcelain bottle blank is subjected to the first high-temperature bisque firing and formed to form a porcelain bottle green body. The high-temperature first bisque firing also includes firing the inner glaze of the porcelain bottle at a preset temperature, and the preset temperature of the inner glaze firing is consistent with the standard sintering temperature of the applied inner glaze.

4. The precious metal sintering process according to claim 3, It is characterized in that In step S3, the porcelain bottle blank is glazed with an outer glaze, and the second clay attached to the T-shaped connecting pin is tightly fitted with the T-shaped connecting pin. The shape of the second clay is consistent with the shape of the connecting hole, so that it is inserted into the connecting hole reserved in the porcelain bottle blank and tightly fits with the edge of the connecting hole, so that the sintered second clay is tightly fitted with the porcelain bottle blank and the hollow relief pattern is fixed. After the hollow relief pattern is fitted to the porcelain bottle blank, the edge of the hollow relief pattern is tightly covered with an outer glaze to prevent a gap from being generated between the hollow relief pattern and the porcelain bottle blank, and then dried.

5. The precious metal sintering process according to claim 4, It is characterized in that In step S3, the T-shaped connecting nail with the second clay is tightly fitted to the edge of the connecting hole, and the total volume of the T-shaped connecting nail with the second clay is limited, wherein the volume of the connecting hole is preset to be V1, the total volume of the T-shaped connecting nail with the second clay is preset to be V2, and V1<V2≤105%V1 is set.

6. The precious metal sintering process according to claim 5, It is characterized in that In step S3, the T-shaped connecting nail with the second clay is tightly fitted with the edge of the connecting hole, so as to make the sintered second clay tightly fit with the porcelain bottle green body and fix the hollow relief pattern, wherein, in order to make the hollow relief pattern tightly fit with the porcelain bottle green body, after the T-shaped connecting nail with the second clay is inserted into the connecting hole, a pressing device is used to press the hollow relief pattern, and at the same time, it is dried for a preset time in the pressed state, and the pressing device includes a base, a fixing rod and a plurality of pressing units, wherein the base connects the fixing rod and each of the pressing units, and is used to support the fixing rod. and a pressing unit, the fixing rod includes a first trapezoidal screw mechanism, a second trapezoidal screw mechanism, a third trapezoidal screw mechanism and a first fixing device, wherein the first trapezoidal screw mechanism is connected to the second trapezoidal screw mechanism, the second trapezoidal screw mechanism is connected to the third trapezoidal screw mechanism, the first trapezoidal screw mechanism is used to adjust the height of the second trapezoidal screw mechanism, the second trapezoidal screw mechanism is used to adjust the horizontal position of the third trapezoidal screw mechanism, the third trapezoidal screw mechanism is wrapped with a soft rubber protective layer, the soft rubber protective layer is used to protect the porcelain bottle so as to reduce the damage caused by the accidental collision of the third trapezoidal screw mechanism to the porcelain bottle, and the third The trapezoidal screw mechanism is used to adjust its own height so that the end of the third trapezoidal screw mechanism rests against the bottom of the porcelain bottle to fix the porcelain bottle at the current position. The first fixing device is respectively connected to the base and the first trapezoidal screw mechanism to fix the first trapezoidal screw mechanism on the base. The pressing unit includes a fourth trapezoidal screw mechanism, a fifth trapezoidal screw mechanism, a sixth trapezoidal screw mechanism, a display screen and a second fixing device, wherein the fourth trapezoidal screw mechanism is connected to the fifth trapezoidal screw mechanism, the fifth trapezoidal screw mechanism is connected to the sixth trapezoidal screw mechanism, and the fourth trapezoidal screw mechanism is used to adjust the fifth trapezoidal screw mechanism The fifth trapezoidal screw mechanism is used to adjust the horizontal position of the sixth trapezoidal screw mechanism; a soft rubber pad is provided at the end of the sixth trapezoidal screw mechanism, and the soft rubber pad is used to press the hollow relief pattern. A pressure sensor is provided in the soft rubber pad, and the pressure sensor is used to detect the pressing pressure of the soft rubber pad on the hollow relief pattern, and output the pressure value to the display screen to ensure that the current pressing pressure always meets the pressure standard P required for the hollow relief pattern to fit tightly with the porcelain bottle green body; the second fixing device is connected to the base and the fourth trapezoidal screw mechanism to fix the fourth trapezoidal screw mechanism on the base.

7. The noble metal sintering process according to claim 6, It is characterized in that In step S3, the number of the pressing units is equal to the number of the T-shaped connecting pins provided on the back of the hollow relief pattern, and the pressing point of the soft rubber pad in the pressing unit is consistent with the setting position of the T-shaped connecting pin.

8. The precious metal sintering process according to claim 7, It is characterized in that In the step S4, the dried porcelain bottle glazed body is subjected to a second glaze firing at a preset temperature, where the preset temperature is the firing temperature of the outer glaze, wherein the outer glaze includes a low-temperature outer glaze and a high-temperature outer glaze.

9. The noble metal sintering process according to claim 8, It is characterized in that In step S3, the glaze firing temperature and process sequence of step S4 are determined according to the firing temperature of the outer glaze applied to the green porcelain bottle and the precious metal material of the hollow relief pattern, wherein: When the material of the hollow relief pattern includes silver, and the porcelain bottle green body is glazed with a low-temperature outer glaze, in step S4, the glaze firing temperature is less than 950° C., and in step S3, the second clay of the preset composition is low-temperature clay; When the material of the hollow relief pattern includes silver, and the porcelain bottle green body is glazed with high-temperature outer glaze, then in the step S4, the porcelain bottle green body is glazed with outer glaze and then subjected to second glaze firing, the glaze firing temperature is the firing temperature of the high-temperature glaze, and after the firing is completed and the porcelain bottle glazed body is cooled, a T-shaped connecting nail with the second clay is inserted into the connection hole reserved for the porcelain bottle glazed body, and is dried while the pressing device presses the hollow relief, wherein in the step S3, the second clay of the preset composition is low-temperature clay, and after drying, a third sintering is performed, and the sintering temperature is less than 950°C; When the material of the hollow relief pattern includes gold, and the porcelain vase green body is glazed with a low-temperature outer glaze, in step S4, the glaze firing temperature is less than 1000° C., and in step S3, the second clay of the preset composition is low-temperature clay; When the material of the hollow relief pattern includes gold, and the porcelain bottle green body is glazed with high-temperature outer glaze, then in the step S4, the porcelain bottle green body is glazed with outer glaze and then subjected to second glaze firing, the glaze firing temperature is the firing temperature of the high-temperature glaze, and after the firing is completed and the porcelain bottle glazed body is cooled, a T-shaped connecting nail with the second clay is inserted into the connection hole reserved for the porcelain bottle glazed body, and is dried while the pressing device presses the hollow relief, wherein in the step S3, the second clay of the preset composition is low-temperature clay, and after drying, a third sintering is performed, and the sintering temperature is less than 1000°C; When the material of the hollow relief pattern includes platinum, and the porcelain bottle green body is applied with a low-temperature outer glaze, then in step S4, the glaze firing temperature is the firing temperature of the low-temperature outer glaze, and in step S3, the second clay of the preset composition is low-temperature pottery clay; When the material of the hollow relief pattern includes platinum, and the porcelain bottle green body is coated with high-temperature outer glaze, then in step S4, the glaze firing temperature is the firing temperature of the high-temperature outer glaze, and in step S3, the second clay with the preset composition is the first clay.

10. The precious metal sintering process according to claim 9, It is characterized in that In step S4, according to the different precious metal materials used in the hollow relief pattern, the glaze firing temperature and process sequence of the precious metal material with the lowest melting point included in the material are selected as the glaze firing temperature and process sequence of step S4, wherein the precious metal materials used in the hollow relief pattern include gold, silver, and platinum.