A fine circuit board based on a semi-additive process, its fabrication method, surface treatment method, and applications.
By modifying the substrate with hydrophilicity and treating it with mercaptosilane, the bonding force between the substrate and metal ions is enhanced, solving the problem of poor adhesion of the seed layer and achieving high bonding force and efficient production of fine circuits.
Patent Information
- Application Number
- CN202211369939.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-11-03
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2042-11-03
AI Technical Summary
In existing semi-additive processes, the seed layer of fine circuits has poor adhesion to the substrate, leading to sidewall corrosion and circuit detachment, which affects system yield and production efficiency.
Hydrophilic modification of the substrate creates a hydroxylated surface, and mercaptosilane is selectively deposited in the fine circuit region to enhance the chelation between the substrate and metal ions, forming a seed layer with strong interfacial adhesion. Fine circuits are then formed using chemical deposition technology.
It improves the adhesion between the substrate and the fine circuitry, reduces sidewall corrosion and circuit detachment, enables the processing of ultra-fine line widths and spacings, and improves system yield and production efficiency.
Smart Images

Figure CN115767927B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of chip packaging technology, specifically relating to a fine circuit board based on a semi-additive process, its preparation method, surface treatment method, and application. Background Technology
[0002] The semi-additive process is a mature manufacturing method used for producing fine-line circuitry in high-density IC substrates. The main steps are: first, applying a copper seed layer onto the substrate dielectric material; second, patterning and electroplating the fine lines; and finally, removing unnecessary copper and the seed layer. Currently, fine-line circuitry fabricated using the semi-additive process is widely used in high-density interconnect circuit boards with linewidths and spacings less than 50 micrometers.
[0003] Semi-additive process circuit boards offer advantages such as ultra-fine linewidth and spacing, and low metal trace roughness. However, when creating the seed layer using chemical copper plating, problems such as poor adhesion between the seed layer and the substrate, and the resulting sidewall corrosion, still persist. If the adhesion of the seed layer beneath the fine traces can be locally improved through patterning, the problems of sidewall corrosion and trace detachment can be effectively reduced, thereby significantly improving system yield and production efficiency. Summary of the Invention
[0004] In order to overcome the shortcomings of the prior art, one of the objectives of this invention is to provide a surface treatment method for fine circuit substrates, which can effectively improve the substrate's adsorption performance of metal ions and enhance the adhesion between the substrate and fine circuits.
[0005] The second objective of this invention is to provide an application of a surface treatment method for fine circuit boards.
[0006] The third objective of this invention is to provide a method for preparing a fine circuit board based on a semi-additive process, which improves the interfacial bonding between the fine circuit and the substrate, allows for controllable thickness of the fine circuit, and mitigates the problems of sidewall corrosion and circuit detachment in the fine circuit board.
[0007] The fourth objective of this invention is to provide a fine circuit board based on a semi-additive process, which has small line width and spacing, and the fine lines are not easily detached.
[0008] One of the objectives of this invention is achieved through the following technical solution:
[0009] A surface treatment method for a fine circuit board includes the following steps:
[0010] 1) The surface of the substrate is hydrophilically modified to form a hydroxylated surface, thus obtaining a hydrophilic substrate;
[0011] 2) A photoresist dry film is laminated onto the hydrophilic substrate, exposed and developed to form a fine circuit pattern, thus obtaining a substrate with a pattern;
[0012] 3) After treating the patterned substrate with mercaptosilane, the photoresist dry film is removed to obtain a substrate with surface modification of fine circuit area.
[0013] Further, in step 1), the hydrophilic modification treatment method is at least one of plasma treatment, ultraviolet treatment, and ozone treatment.
[0014] Furthermore, the substrate is made of any one or a combination of two or more of the following materials: glass, ceramic, silicon wafer, epoxy resin, BT resin, and PI resin.
[0015] Further, in step 3), the mercaptolation process involves selectively depositing vapor-phase mercaptosilane onto the fine circuit pattern area of the substrate.
[0016] Furthermore, the mercaptosilane is at least one selected from 3-mercaptopropyltrimethoxysilane, 3-mercaptopropyltriethoxysilane, and mercaptopropylmethyldimethoxysilane.
[0017] The second objective of this invention is achieved by the following technical solution:
[0018] An application of a surface treatment method for a fine circuit board, and the application of the surface treatment method for the fine circuit board in the production of fine circuit boards.
[0019] The third objective of this invention is achieved by the following technical solution:
[0020] A method for fabricating a fine circuit board based on a semi-additive process includes the following steps:
[0021] S1, the surface treatment method of the fine circuit substrate is used to treat the substrate to obtain a surface-treated substrate.
[0022] S2, perform chemical deposition of copper on the surface of the surface-treated substrate to form a seed layer;
[0023] S3, a second photoresist film is applied to the seed layer in step S2, followed by exposure, development, and electroplating to form fine lines.
[0024] S4. After removing the photoresist dry film from the substrate containing fine circuits in step S3, the seed layer is etched away to obtain the fine circuit board.
[0025] Furthermore, in step S3, the metal material of the fine circuit is any one or a combination of two or more of copper, gold, and silver.
[0026] Furthermore, in step S4, the linewidth of the fine lines in the fine circuit board is 1-200μm, and the line spacing is 1-200μm.
[0027] The fourth objective of this invention is achieved by the following technical solution:
[0028] A fine circuit board based on a semi-additive process is prepared by the aforementioned method for preparing a fine circuit board based on a semi-additive process.
[0029] Compared with the prior art, the beneficial effects of the present invention are as follows:
[0030] The present invention discloses a surface treatment method for a fine circuit substrate. First, the surface of the substrate is hydrophilically modified to expose hydroxyl groups. Then, mercaptosilane is selectively deposited in the corresponding fine circuit areas to coat the substrate with mercapto groups. The strong chelation between mercapto groups and metal ions can effectively adsorb metal ions. After reduction, a seed layer with strong interfacial bonding force with the substrate material is formed, thereby significantly improving the bonding force between the seed layer and the substrate.
[0031] This invention discloses a method for preparing a fine circuit board based on a semi-additive process. After selectively coating the substrate with thiol groups using the aforementioned surface treatment method, a copper seed layer is chemically deposited. This results in extremely high interfacial adhesion between the exposed areas corresponding to the fine circuits and the strong chelation between the thiol groups and copper ions. Simultaneously, the adhesion between the copper seed layer and the substrate in the non-exposed areas is weak, making it easy to etch and remove the copper seed layer. Further electroplating of the seed layer using a semi-additive process to form the fine circuits achieves the effect of ultra-fine linewidth and spacing, while simultaneously improving the problems of sidewall corrosion and line detachment in the fine circuits.
[0032] The present invention provides a fine circuit board based on a semi-additive process, which has small line width and line spacing, controllable thickness, low roughness of metal lines, and fine lines that are not easily detached. Attached Figure Description
[0033] Figure 1 This is a process flow diagram of a surface treatment method for a fine circuit board according to the present invention.
[0034] Figure 2 This is a schematic diagram of the chemically deposited seed layer in a method for preparing a fine circuit board based on a semi-additive process according to the present invention.
[0035] Figure 3 This is a process flow diagram of a method for fabricating a fine circuit board based on a semi-additive process according to the present invention.
[0036] Figure 4 This is a physical image of the fine circuit board obtained in Embodiment 4 of the present invention.
[0037] Among them, 1. substrate; 2. seed layer; 3. photoresist dry film; 4. fine circuitry. Detailed Implementation
[0038] The present invention will now be further described in conjunction with specific embodiments. It should be noted that, without conflict, the various embodiments or technical features described below can be arbitrarily combined to form new embodiments.
[0039] Example 1
[0040] A surface treatment method for a fine circuit board, referring to Figure 1 This includes the following steps:
[0041] 1) The surface of the substrate is subjected to hydrophilic modification treatment to form a hydroxylated surface, thereby obtaining a hydrophilic substrate; the material of the substrate is epoxy resin; the hydrophilic modification treatment method includes, but is not limited to, plasma treatment, ultraviolet treatment and ozone treatment. Preferably, the hydrophilic modification treatment method in this embodiment is plasma treatment, with a treatment power of 10-100W and a treatment time of 10s-10min.
[0042] 2) A photoresist dry film is laminated onto the hydrophilic substrate, exposed and developed to form a fine circuit pattern, thus obtaining a substrate with a pattern;
[0043] 3) After treating the patterned substrate with mercaptosilane, the photoresist dry film is removed to obtain a substrate with mercaptomodified surface in the fine circuit area.
[0044] Further, the mercaptosilane is 3-mercaptopropyltrimethoxysilane; the specific operation of the mercapto treatment in this embodiment is as follows: the substrate to be treated is placed in a vacuum chamber with a volume of 1-100L; then 1-100ml of 3-mercaptopropyltrimethoxysilane liquid is dropped into the chamber, and then a vacuum is drawn to maintain a vacuum degree of less than 0.1 atmospheres; after standing in vacuum for 30 minutes, the mercapto surface modification is completed.
[0045] Example 2
[0046] A surface treatment method for a fine circuit board, referring to Figure 1 This includes the following steps:
[0047] 1) The surface of the substrate is subjected to hydrophilic modification treatment to form a hydroxylated surface, thereby obtaining a hydrophilic substrate; the material of the substrate is BT resin; the hydrophilic modification treatment method is ultraviolet treatment.
[0048] 2) A photoresist dry film is laminated onto the hydrophilic substrate, exposed and developed to form a fine circuit pattern, thus obtaining a substrate with a pattern;
[0049] 3) After treating the patterned substrate with mercaptosilane, the photoresist dry film is removed to obtain a substrate with mercaptomodified surface in the fine circuit area.
[0050] Furthermore, the mercaptolation process involves selectively depositing a gaseous mercaptosilane onto the fine circuit pattern area of the substrate; the mercaptosilane is 3-mercaptopropyltriethoxysilane.
[0051] Example 3
[0052] A surface treatment method for a fine circuit board, referring to Figure 1 This includes the following steps:
[0053] 1) The surface of the substrate is subjected to hydrophilic modification treatment to form a hydroxylated surface, thereby obtaining a hydrophilic substrate; the material of the substrate is PI resin; the hydrophilic modification treatment method is ozone treatment.
[0054] 2) A photoresist dry film is laminated onto the hydrophilic substrate, exposed and developed to form a fine circuit pattern, thus obtaining a substrate with a pattern;
[0055] 3) After treating the patterned substrate with mercaptosilane, the photoresist dry film is removed to obtain a substrate with mercaptomodified surface in the fine circuit area.
[0056] Furthermore, the mercaptolation process involves selectively depositing a gaseous mercaptosilane onto the fine circuit pattern area of the substrate; the mercaptosilane is mercaptopropylmethyldimethoxysilane.
[0057] Example 4
[0058] A method for fabricating a fine circuit board based on a semi-additive process, referring to... Figure 2-3 This includes the following steps:
[0059] S1, the surface treatment method of fine circuit substrate described in Example 1 is used to treat the surface of substrate 1, and then copper is chemically deposited on the surface of the surface-treated substrate 1 to form a seed layer 2.
[0060] S2, apply a second photoresist dry film 3 to the seed layer 2 in step S1, expose and develop to determine the area of fine lines.
[0061] S3, the substrate obtained in step S2 is electroplated with copper to form fine lines 4.
[0062] S4, the blank board with fine lines obtained in step S3 is subjected to photoresist dry film 3 removal treatment to expose seed layer 2.
[0063] S5, the exposed seed layer 2 is removed by etching the blank obtained in step S4 to obtain a fine circuit board; the line width of the fine circuits in the fine circuit board is 1-10μm and the line spacing is 1-50μm.
[0064] Reference Figure 4 The method for fabricating fine circuit boards in this embodiment can form fine circuits with line width and line spacing within 10μm, and the high-density circuit structure is intact, without obvious sidewall corrosion or line detachment problems.
[0065] Example 5
[0066] A method for fabricating a fine circuit board based on a semi-additive process, referring to... Figure 2-3 This includes the following steps:
[0067] S1, the surface treatment method of fine circuit substrate described in Example 2 is used to treat the surface of substrate 1, and then copper is chemically deposited on the surface of the surface-treated substrate 1 to form a seed layer 2.
[0068] S2, apply a second photoresist dry film 3 to the seed layer 2 in step S1, expose and develop to determine the area of fine lines.
[0069] S3, the substrate obtained in step S2 is electroplated with gold to form fine lines 4.
[0070] S4, the blank board with fine lines obtained in step S3 is subjected to photoresist dry film 3 removal treatment to expose seed layer 2.
[0071] S5, the exposed seed layer 2 is removed by etching the blank obtained in step S4 to obtain a fine circuit board; the line width of the fine circuits in the fine circuit board is 10-30μm and the line spacing is 10-100μm.
[0072] Example 6
[0073] A method for fabricating a fine circuit board based on a semi-additive process, referring to... Figure 2-3 This includes the following steps:
[0074] S1, the surface treatment method of fine circuit substrate described in Example 3 is used to treat the surface of substrate 1, and then copper is chemically deposited on the surface of the surface-treated substrate 1 to form a seed layer 2.
[0075] S2, apply a second photoresist dry film 3 to the seed layer 2 in step S1, expose and develop to determine the area of fine lines.
[0076] S3, the substrate obtained in step S2 is electroplated with silver to form fine lines 4.
[0077] S4, the blank board with fine lines obtained in step S3 is subjected to photoresist dry film 3 removal treatment to expose seed layer 2.
[0078] S5, the exposed seed layer 2 is removed by etching the blank obtained in step S4 to obtain a fine circuit board; the line width of the fine circuits in the fine circuit board is 100-200μm and the line spacing is 50-200μm.
[0079] This invention discloses a method for preparing a fine circuit board based on a semi-additive process. After selectively coating the substrate with thiol groups using a surface treatment method, a copper seed layer is chemically deposited. This results in extremely high interfacial adhesion between the exposed areas corresponding to the fine circuits and the strong chelation between the thiol groups and copper ions. Simultaneously, the adhesion between the copper seed layer and the substrate in the non-exposed areas is weak, making it easy to etch and remove the copper seed layer. Further electroplating of the seed layer using a semi-additive process to form the fine circuits achieves the effect of ultra-fine linewidth and spacing, while also improving the problems of sidewall corrosion and line detachment in the fine circuits.
[0080] The above embodiments are merely preferred embodiments of the present invention and should not be construed as limiting the scope of protection of the present invention. Any non-substantial changes and substitutions made by those skilled in the art based on the present invention shall fall within the scope of protection claimed by the present invention.
Claims
1. A method for fabricating a fine circuit board based on a semi-additive process, characterized in that, Includes the following steps: S1, Perform surface treatment on the substrate to obtain a surface-treated substrate; S2, perform chemical deposition of copper on the surface of the surface-treated substrate to form a seed layer; S3, a second photoresist film is applied to the seed layer in step S2, followed by exposure, development, and electroplating to form fine lines. S4. After removing the photoresist dry film from the substrate containing fine circuits in step S3, the seed layer is etched away to obtain the fine circuit board. The surface treatment of the substrate includes the following steps: 1) The surface of the substrate is hydrophilically modified to form a hydroxylated surface, thus obtaining a hydrophilic substrate; 2) A photoresist dry film is laminated onto the hydrophilic substrate, exposed and developed to form a fine circuit pattern, thus obtaining a substrate with a pattern; 3) After treating the patterned substrate with mercaptosilane, the photoresist dry film is removed to obtain a substrate with surface modification of fine circuit area. In step 3), the mercaptolation process involves selectively depositing vapor-phase mercaptosilane onto the fine circuit pattern area of the substrate. The mercaptosilane is at least one of 3-mercaptopropyltrimethoxysilane, 3-mercaptopropyltriethoxysilane, and mercaptopropylmethyldimethoxysilane.
2. The preparation method according to claim 1, characterized in that: In step 1), the hydrophilic modification treatment method is at least one of plasma treatment, ultraviolet treatment, and ozone treatment.
3. The preparation method according to claim 1, characterized in that: The substrate is made of any one or a combination of two or more of the following materials: glass, ceramic, silicon wafer, epoxy resin, BT resin, and PI resin.
4. An application of a surface treatment method for a fine circuit board, characterized in that, The application of the surface treatment method for the substrate in the preparation method according to any one of claims 1-3 in the production of fine circuit boards.
5. The preparation method according to claim 1, characterized in that: In step S3, the metal material of the fine circuit is any one or a combination of two or more of copper, gold and silver.
6. The preparation method according to claim 1, characterized in that: In step S4, the line width of the fine lines in the fine circuit board is 1-200μm, and the line spacing is 1-200μm.
7. A fine circuit board based on a semi-additive process, characterized in that: It is prepared by any one of the preparation methods described in claims 1-3 and 5-6.
Citation Information
Patent Citations
Site-selective metal plating onto a package dielectric
US20190202845A1