A method for etching single-sided graphics of flexible glass
By pasting and cutting the anti-acid film layer on the flexible glass substrate, combined with the protection measures of anti-acid ink, it is divided into initial and repeated etching steps, which solves the problems of operation difficulties and easy fall off in the prior art, and realizes the problem of anti-acid film Complete exposure and efficient etching of the graphics area reduce the risk of loss and improve the apparent yield.
Patent Information
- Application Number
- CN202211642683.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-12-20
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2042-12-20
AI Technical Summary
In the single-sided pattern etching process of flexible glass substrates, the operation is difficult, the cutting is difficult, and the acid-proof film is prone to fall off, resulting in risks such as oozing and breaking, and the complete bareness and efficient etching of the pattern area cannot be achieved.
Use a transparent anti-acid film layer to paste on the edge of the graphics area for cutting, retaining the protective anti-acid film layer, applying anti-acid ink to protect the graphics area, which is divided into primary etching and secondary etching steps to ensure complete bareness and low risk of the graphics area. Etching.
It realizes simple and fast glass etching treatment, ensuring the intact graphic area, reducing the risk of product damage, and improving apparent yield.
Smart Images

Figure CN115947543B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of flexible glass, and more specifically, relates to a method for etching a single-sided pattern of flexible glass. Background Art
[0002] With the development of modern science and technology, the production process and equipment level of glass have been further improved. Flexible glass substrates with special graphic depressions on one side have great development space in the future fields of new energy, energy conservation and environmental protection, electronic information industry, construction industry, automobile industry, etc. The existing process is to use a conventional acid-proof film to stick on the graphic surface, cut the acid-proof film in the graphic area and directly put it into etching, which has major defects: Disadvantage 1: It is difficult to operate with conventional acid-proof films, and the graphic area cannot be completely exposed; Disadvantage 2: It is difficult to cut the acid-proof film; Disadvantage 3: The acid-proof film is easy to fall off from the glass substrate during etching, resulting in risks such as leakage and fragmentation. In the prior art, there is a technology named "Manufacturing method of flexible glass substrate and flexible glass substrate" and publication number "CN102131743A", which includes the following steps: temporarily bonding a support body on one side surface of the glass substrate; etching the other side surface of the glass substrate to make the glass substrate thinner; bonding a film substrate on the other side surface after the etching treatment; peeling off the support body temporarily bonded to one side surface of the glass substrate. This technology cannot solve the technical problem of this application. Summary of the invention
[0003] The technical problem to be solved by the present invention is: in view of the shortcomings of the prior art, a method for etching a single-sided pattern of flexible glass is provided which has simple steps, is convenient and quick to implement glass etching processing, ensures that the pattern area of the glass is completely concave, has a low risk of product damage, and has a high apparent yield.
[0004] To solve the above-mentioned technical problems, the technical solution adopted by the present invention is:
[0005] The present invention is a method for etching a single-sided pattern of flexible glass. The etching steps of the method for etching a single-sided pattern of flexible glass are as follows:
[0006] S1. preparing a flexible glass substrate to be etched, wherein the surface of the flexible glass substrate has a pattern area;
[0007] S2. Paste a transparent acid-proof film layer on one side of the flexible glass substrate with a graphic area, cut the acid-proof film layer along the edge of the graphic area, the acid-proof film layer in the graphic area is a protective acid-proof film layer, and tear off the excess acid-proof film layer other than the protective acid-proof film layer;
[0008] S3. Acid-proof ink is applied to the surface of the flexible glass substrate of the flexible glass substrate to protect the acid-proof film layer on one side thereof, to form an acid-proof ink layer;
[0009] S4. Tear off the protective acid-proof film layer in the graphic area to expose the graphic area;
[0010] S5. Place the flexible glass substrate in a hydrofluoric acid solution for initial etching, etch the pattern area, perform initial etching, and then perform secondary etching on the flexible glass substrate after the initial etching.
[0011] After the initial etching is completed, the flexible glass substrate is cleaned, and then the flexible glass substrate is placed in an acid-resistant ink remover to clean the acid-resistant ink layer.
[0012] After the flexible glass substrate is placed in an acid-proof ink remover to clean the acid-proof ink layer, the flexible glass substrate is placed in a hydrofluoric acid solution for secondary etching. The graphic area of the flexible glass substrate reaches the etching target thickness after the secondary etching, and the thickness of the secondary etching is greater than the thickness of the initial etching.
[0013] After the secondary etching is completed, the flexible glass substrate is cleaned to obtain a finished flexible glass substrate with a concave pattern area on one side.
[0014] The acid-proof film layer is a polytetrafluoroethylene film, a polyethylene film or a polypropylene film.
[0015] When cutting the acid-proof film layer along the edge of the graphic area, use a knife to cut.
[0016] The total etching thickness of the graphic area is controlled within a range of 40um-60um.
[0017] The technical solution of the present invention is adopted, and the working principle and beneficial effects are as follows:
[0018] The etching method of the single-sided pattern of the flexible glass described in the present invention, when etching the single-sided pattern of the flexible glass, first, paste the acid-proof film layer to one side of the flexible glass substrate with the pattern area, the acid-proof film layer covers the surface of the flexible glass, cut the acid-proof film layer, retain the acid-proof film layer covering the pattern area, the part is the protective acid-proof film layer, the acid-proof film layer outside the pattern area, that is, the redundant acid-proof film layer is removed, and the acid-proof ink is applied. Due to the existence of the protective acid-proof film layer, the acid-proof ink will not be applied to the pattern area, but will only be applied to the position where the redundant acid-proof film layer is removed from the flexible glass, and the acid-proof ink protects the part where the acid-proof ink is applied, tear off the protective acid-proof film layer in the pattern area, expose the pattern area, and then perform the initial etching on the flexible glass substrate. Since the acid-proof ink protects the part where the acid-proof ink is applied, the pattern area is exposed, and what needs to be etched is the pattern area, and the pattern area can be initially etched in a hydrofluoric acid solution, while the part where the acid-proof ink is applied will not be etched, and is reliably protected. In this way, according to the size of the pattern area on different flexible glasses, the size of the protective acid-proof film layer is set to meet the needs. The graphic area to be etched is completely exposed, which improves the etching effect and efficiency. The acid-proof film layer has been torn off during etching, so there is no risk of the acid-proof film layer falling off the glass substrate and causing the hydrofluoric acid solution to penetrate into the substrate and cause fragmentation. At the same time, the etching of the graphic area in this application is divided into primary etching and secondary etching. The primary etching with a smaller etching amount is performed first, and then the step with a larger etching amount is performed to reduce the risk of product damage. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] The following is a brief description of the contents and symbols in the drawings of this specification:
[0020] Figure 1 This is a schematic diagram of the structure of the flexible glass of the present invention after the acid-proof film layer is attached;
[0021] Figure 2 This is a schematic diagram of the structure of the flexible glass of the present invention after the redundant acid-proof film layer is cut off;
[0022] Figure 3 This is a schematic structural diagram of the flexible glass of the present invention when an acid-proof ink layer is formed;
[0023] Figure 4 This is a schematic diagram of the structure of the flexible glass before secondary etching according to the present invention;
[0024] The markings in the attached drawings are: 1. flexible glass substrate; 2. acid-proof ink layer; 3. acid-proof film layer; 4. graphic area; 5. protective acid-proof film layer; 6. redundant acid-proof film layer. DETAILED DESCRIPTION
[0025] The following is a further detailed description of the specific implementation of the present invention, such as the shape, structure, mutual position and connection relationship between the various components involved, the function and working principle of each part, etc., through the description of the embodiments with reference to the accompanying drawings:
[0026] As attached Figure 1 -Attached Figure 4 As shown, the present invention is a method for etching a single-sided pattern of flexible glass, and the etching steps of the method for etching a single-sided pattern of flexible glass are as follows:
[0027] S1. Prepare a flexible glass substrate 1 to be etched, and the surface of the flexible glass substrate 1 has a graphic area 4; S2. Paste a transparent acid-proof film layer 3 on one side of the flexible glass substrate 1 with the graphic area 4, cut the acid-proof film layer 3 along the edge of the graphic area 4, and the acid-proof film layer 3 of the graphic area 4 is a protective acid-proof film layer 5, and tear off the excess acid-proof film layer 6 other than the protective acid-proof film layer 5; S3. Apply acid-proof ink to the surface of the flexible glass substrate 1 on the side of the flexible glass substrate 1 pasted with the protective acid-proof film layer 5 to form an acid-proof ink layer 2; S4. Tear off the protective acid-proof film layer 5 of the graphic area 4 to expose the graphic area 4; S5. Put the flexible glass substrate 1 into a hydrofluoric acid solution for initial etching, etch the graphic area 4, perform initial etching, and then etch the flexible glass substrate 1 for a second time after the initial etching. The above steps propose an improved technical solution for the deficiencies in the prior art. When single-sided pattern etching of flexible glass is performed, first, an acid-proof film layer 3 is pasted to one side of a flexible glass substrate 1 having a pattern area 4, the acid-proof film layer 3 covers the surface of the flexible glass, and then the acid-proof film layer 3 is cut to retain the acid-proof film layer covering the pattern area, which is the protective acid-proof film layer 5, and the acid-proof film layer outside the pattern area, that is, the excess acid-proof film layer 6 is removed, and then acid-proof ink is applied. Due to the presence of the protective acid-proof film layer 5, the acid-proof ink will not be applied to the pattern area, but will only be applied to the position where the excess acid-proof film layer is removed from the flexible glass, and the acid-proof ink protects the area where the acid-proof ink is applied, and then the protective acid-proof film layer 5 of the pattern area 4 is torn off to expose the pattern area 4, and then the flexible glass substrate is initially etched. Since the acid-proof ink protects the substrate area where the acid-proof ink is applied, and the pattern area is exposed, and it is the pattern area 4 that needs to be etched, in this way, the pattern area 4 can complete the initial etching in the hydrofluoric acid solution, and the substrate area where the acid-proof ink is applied will not be etched, thereby obtaining reliable protection. In this way, according to the size of the graphic area 4 on different flexible glasses, the size of the protective acid-proof film layer 5 is set to meet the needs. The graphic area that needs to be etched is completely exposed to improve the etching effect and efficiency, and the acid-proof film layer has been torn off during etching, so there will be no acid-proof film layer falling off from the glass substrate during etching, causing the hydrofluoric acid solution to penetrate into the substrate and causing the risk of fragmentation. At the same time, the etching of the graphic area in the present application is divided into primary etching and secondary etching, first performing the primary etching with a smaller etching amount, and then performing the step with a larger etching amount to reduce the risk of product damage. The etching method of the single-sided graphic of the flexible glass described in the present invention has simple steps, conveniently and quickly realizes glass etching processing, ensures that the graphic area of the glass is concave and complete, has a low risk of product damage, and has a high apparent yield.
[0028] After the initial etching is completed, the flexible glass substrate 1 is cleaned, and then the flexible glass substrate 1 is placed in an acid-resistant ink remover to clean the acid-resistant ink layer 2. In the above steps, after the initial etching is completed, the substrate is cleaned, and then the acid-resistant ink layer 2 is cleaned to complete the initial etching operation of the glass.
[0029] After the flexible glass substrate 1 is placed in an acid-proof ink remover to clean the acid-proof ink layer 2, the flexible glass substrate 1 is placed in a hydrofluoric acid solution for secondary etching. The graphic area 4 of the flexible glass substrate 1 reaches the etching target thickness after the secondary etching, and the thickness of the secondary etching is greater than the thickness of the initial etching. In the above steps, the secondary etching is performed on the entire substrate surface. The thickness of the secondary etching is the same, and the graphic area is in a concave state as a whole after the initial etching.
[0030] After the secondary etching is completed, the flexible glass substrate 1 is cleaned to obtain a finished flexible glass substrate with a concave pattern area on one side. After the above steps, the finished substrate is obtained after the secondary etching.
[0031] The acid-proof film layer 3 is a polytetrafluoroethylene film or a polyethylene film or a polypropylene film. The acid-proof film layer 3 is cut along the edge of the graphic area 4 with a cutter. The total etching thickness of the graphic area 4 is controlled to be 40um-60um. The above structure controls the total etching thickness of the graphic area, and the thickness of the initial etching is less than the thickness of the secondary etching, ensuring that the initial etching with a smaller etching amount is performed first, and then the step with a larger etching amount is performed, effectively reducing the risk of product damage.
[0032] The etching method of the single-sided pattern of the flexible glass described in the present invention, when etching the single-sided pattern of the flexible glass, first, paste the acid-proof film layer to one side of the flexible glass substrate with the pattern area, the acid-proof film layer covers the surface of the flexible glass, cut the acid-proof film layer, retain the acid-proof film layer covering the pattern area, the part is the protective acid-proof film layer, the acid-proof film layer outside the pattern area, that is, the redundant acid-proof film layer is removed, and the acid-proof ink is applied. Due to the existence of the protective acid-proof film layer, the acid-proof ink will not be applied to the pattern area, but will only be applied to the position where the redundant acid-proof film layer is removed from the flexible glass, and the acid-proof ink protects the part where the acid-proof ink is applied, tear off the protective acid-proof film layer in the pattern area, expose the pattern area, and then perform the initial etching on the flexible glass substrate. Since the acid-proof ink protects the part where the acid-proof ink is applied, the pattern area is exposed, and what needs to be etched is the pattern area, and the pattern area can be initially etched in a hydrofluoric acid solution, while the part where the acid-proof ink is applied will not be etched, and is reliably protected. In this way, according to the size of the pattern area on different flexible glasses, the size of the protective acid-proof film layer is set to meet the needs. The graphic area to be etched is completely exposed, which improves the etching effect and efficiency. The acid-proof film layer has been torn off during etching, so there is no risk of the acid-proof film layer falling off the glass substrate and causing the hydrofluoric acid solution to penetrate into the substrate and cause fragmentation. At the same time, the etching of the graphic area in this application is divided into primary etching and secondary etching. The primary etching with a smaller etching amount is performed first, and then the step with a larger etching amount is performed to reduce the risk of product damage.
[0033] The present invention is described above by way of example in conjunction with the accompanying drawings. It is obvious that the specific implementation of the present invention is not limited to the above-mentioned method. As long as various improvements are made using the method concept and technical solution of the present invention, or the concept and technical solution of the present invention are directly applied to other occasions without improvement, they are all within the protection scope of the present invention.
Claims
1. A method for etching a single-sided pattern of flexible glass, characterized in that: The etching steps of the method for etching a single-sided pattern of flexible glass are as follows: S1. preparing a flexible glass substrate (1) to be etched, wherein the surface of the flexible glass substrate (1) has a patterned area (4); S2. Paste a transparent acid-proof film layer (3) on one side of the flexible glass substrate (1) having a graphic region (4), cut the acid-proof film layer (3) along the edge of the graphic region (4), the acid-proof film layer (3) of the graphic region (4) is a protective acid-proof film layer (5), and tear off the excess acid-proof film layer (6) other than the protective acid-proof film layer (5); S3. Applying acid-proof ink to the surface of the flexible glass substrate (1) to which the protective acid-proof film layer (5) is attached to form an acid-proof ink layer (2); S4. Tear off the protective acid-proof film layer (5) of the graphic area (4), exposing the graphic area (4); S5. placing the flexible glass substrate (1) in a hydrofluoric acid solution for primary etching, performing primary etching on the etching pattern area (4), and performing secondary etching on the flexible glass substrate (1) after the primary etching; When single-sided pattern etching of flexible glass is performed, an acid-proof film layer (3) is pasted to one side of a flexible glass substrate (1) having a pattern area (4), the acid-proof film layer (3) covers the surface of the flexible glass, and then the acid-proof film layer (3) is cut to retain the acid-proof film layer covering the pattern area, the acid-proof film layer covering the pattern area is the protective acid-proof film layer (5), and the acid-proof film layer outside the pattern area, that is, the excess acid-proof film layer (6) is removed, and acid-proof ink is applied. Due to the presence of the protective acid-proof film layer (5), the acid-proof ink will not be applied to the pattern area, but will only be applied to the position of the flexible glass where the excess acid-proof film layer is removed, and the acid-proof ink protects the portion where the acid-proof ink is applied, and then the protective layer of the pattern area (4) is torn off. The acid-proof film layer (5) is protected, the graphic area (4) is exposed, and then the flexible glass substrate is initially etched. Since the acid-proof ink protects the substrate portion coated with the acid-proof ink, and the graphic area is exposed, and it is the graphic area (4) that needs to be etched, the graphic area (4) can be initially etched in the hydrofluoric acid solution, while the substrate portion coated with the acid-proof ink will not be etched and protected. The size of the protective acid-proof film layer (5) is set according to the size of the graphic area (4) on different flexible glasses. The acid-proof film layer is torn off during etching, so there is no risk of the acid-proof film layer falling off from the glass substrate causing the hydrofluoric acid solution to penetrate into the substrate and cause fragmentation during etching.
2. The method for etching a single-sided pattern of flexible glass according to claim 1, characterized in that: After the initial etching is completed, the flexible glass substrate (1) is cleaned.
3. The method for etching a single-sided pattern of flexible glass according to claim 2, characterized in that: The flexible glass substrate (1) is cleaned, and then the flexible glass substrate (1) is placed in an acid-resistant ink remover to clean the acid-resistant ink layer (2).
4. The method for etching a single-sided pattern of flexible glass according to claim 3, characterized in that: After the flexible glass substrate (1) is placed in an acid-resistant ink remover to clean the acid-resistant ink layer (2), the flexible glass substrate (1) is placed in a hydrofluoric acid solution for secondary etching.
5. The method for etching a single-sided pattern of flexible glass according to claim 4, characterized in that: The graphic area (4) of the flexible glass substrate (1) reaches the etching target thickness after secondary etching, and the thickness of the secondary etching is greater than the thickness of the initial etching.
6. The method for etching a single-sided pattern of flexible glass according to claim 4, characterized in that: After the secondary etching is completed, the flexible glass substrate (1) is cleaned to obtain a finished flexible glass substrate with a recessed pattern area on one side.
7. The method for etching a single-sided pattern of flexible glass according to claim 1 or 2, characterized in that: The acid-proof film layer (3) is a polytetrafluoroethylene film, a polyethylene film or a polypropylene film.
8. The method for etching a single-sided pattern of flexible glass according to claim 1 or 2, characterized in that: When cutting the acid-proof film layer (3) along the edge of the graphic area (4), a cutter is used for cutting.
9. The method for etching a single-sided pattern of flexible glass according to claim 1, characterized in that: The total etching thickness of the graphic area (4) is controlled within a range of 40um-60um.
Citation Information
Patent Citations
Process for producing flexible glass substrate, and flexible glass substrate
CN102131743A
Conductive ink, and preparation method and application method thereof
CN102675961A
Plate glass separation and perforation method and device
CN102849933A
Stainless steel tray etching method
CN105506630A
One-chip OGS (One Glass Solution) touch screen and manufacture method thereof
CN105630255A