Anti-counterfeiting elements and products

By combining a microlens array layer and a micrographic array layer in an anti-counterfeiting element, as well as a metal coating and an interference optically variable layer, the problem of poor anti-counterfeiting performance of existing anti-counterfeiting elements is solved, diversified optical effects and color changes are achieved, and enhanced Improve the anti-counterfeiting capabilities and reliability of the product.

CN116118382BActive Publication Date: 2024-10-11ZHONGCHAO SPECIAL SECURITY TECH +1
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202111350993.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-11-15
Publication Date
2024-10-11
Estimated Expiration
2041-11-15

AI Technical Summary

Technical Problem

The anti-counterfeiting performance of existing anti-counterfeiting components is poor, and it is difficult to meet the needs of some product designs for thicker lines and diverse appearances, and a single technology results in a relatively single appearance.

Method used

An anti-counterfeiting element design including a base material, a microlens array layer, a micrographic array layer, a first color layer and a second color layer is adopted, and the micrographic array layer is sampled and synthesized through the microlens array layer to form an enlarged image, and Combined with metal coating and interference optical change layer, the dynamic effect and color contrast are enhanced.

Benefits of technology

It improves the anti-counterfeiting capability and reliability of anti-counterfeiting components, can present diverse optical effects and color changes when the viewing angle changes, and enhances product recognition and security.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116118382B_ABST
    Figure CN116118382B_ABST
Patent Text Reader

Abstract

The present invention provides an anti-counterfeiting element and an anti-counterfeiting product. The anti-counterfeiting element includes: a substrate, the substrate includes a first surface and a second surface opposite to each other; a microlens array layer, the microlens array layer is located on the first surface of the substrate; a micro-image array layer, the micro-image array layer is located on the second surface of the substrate, and the surface of the micro-image array layer away from the substrate includes at least a micro-image area and a micro-image background area, and both the micro-image area and the micro-image background area are multiple and alternately arranged; a second color layer, the second color layer is located on the surface of the micro-image array layer away from the substrate; a first color layer, the first color layer is located between the micro-image array layer and the second color layer, there are multiple first color layers, and the multiple first color layers are arranged one-to-one with the multiple micro-image areas; wherein, one of the first color layer and the second color layer is a metal plating layer, and the other is an interference light variable layer. The present invention solves the problem of poor anti-counterfeiting performance of anti-counterfeiting elements in the prior art.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of anti-counterfeiting technology, and in particular to an anti-counterfeiting element and an anti-counterfeiting product. Background Art

[0002] In order to prevent the production or counterfeiting of various high-security or high-value-added printed materials such as banknotes, cards and product packaging by means of scanning and copying, security lines, stickers or logos are widely used in them. Optical anti-counterfeiting elements use a variety of anti-counterfeiting technologies. Among them, holographic anti-counterfeiting technology is currently the most common anti-counterfeiting technology, for example, the window security line of the fifth set of RMB 2005 version of China, except for the 1 yuan note, and important documents such as my country's identity card, driver's license, passport, etc.

[0003] With the development of technology, interference optical variable technology has attracted more and more attention because of its specific optical color change effect under different observation angles. Interference optical variable technology generally uses vapor deposition to form a multi-layer interference coating. The classic multi-layer interference coating generally includes a reflective layer, a dielectric layer and an absorption layer. The reflective layer is generally made of high-brightness metal materials, the dielectric layer is generally made of transparent inorganic or organic materials, and the absorption layer is also called a semi-transparent layer, which is generally made of thinner metal materials with good absorption. The fifth set of 2015 version of the 100 yuan RMB security line uses multi-layer interference optical variable technology, which is magenta when viewed from the front and green when viewed from an angle. In addition, in recent years, optically variable ink (OVI) based on the principle of interference optical variable technology has also been valued by banknotes and other high-end commercial anti-counterfeiting industries because it is easy to integrate with the traditional printing industry. For example, the front denomination numbers of the fifth set of 2015 version of 100 yuan RMB, the 2019 version of 50, 20, 10 yuan RMB, and the 2020 version of 5 yuan RMB all use optically variable ink.

[0004] On the other hand, with the adoption of Motion security thread in the new version of US dollar banknotes, the anti-counterfeiting industry has developed a strong interest in this new type of microlens array technology. It is an anti-counterfeiting technology with dynamic characteristics or depth of field effect based on the moiré magnification effect of the microlens array on the micro-image array, that is, the microlens array can sample and synthesize the micro-image array to form an image. The image presents a dramatic motion effect as the observation angle changes. This technology requires that the micro-image array and its background need to have sufficient color or brightness contrast. Patent document CN200680062431.9 discloses a method for making micro-images by scraping ink, that is, first forming an undulating structure layer with an icon concave structure, then coating the whole with a certain thickness of radiation-curable ink, and then scraping off the ink outside the concave structure with a scraper, and finally curing the radiation-curable ink in the concave structure with a certain dose of radiation source. The lines of the micro-images of this method can only be very thin, for example, it is difficult to achieve lines with a width greater than 5um. This is strict for product design, because some product designs require that the lines are relatively rough or even macroscopic. In addition, the color of the image and text obtained by this method is the color of the ink itself, so the appearance is relatively simple.

[0005] Single holographic technology, interferometric optical variable technology and even microlens array technology are increasingly being used in general market products, such as decorative products. Therefore, it is highly necessary to enhance the comprehensive anti-counterfeiting capabilities of these technologies.

[0006] That is to say, the anti-counterfeiting elements in the prior art have the problem of poor anti-counterfeiting performance. Summary of the invention

[0007] The main purpose of the present invention is to provide an anti-counterfeiting element and an anti-counterfeiting product to solve the problem of poor anti-counterfeiting performance of the anti-counterfeiting element in the prior art.

[0008] In order to achieve the above-mentioned purpose, according to one aspect of the present invention, there is provided an anti-counterfeiting element, which includes: a substrate, the substrate includes a first surface and a second surface opposite to each other; a microlens array layer, the microlens array layer is located on the first surface of the substrate; a micro-image array layer, the micro-image array layer is located on the second surface of the substrate, and the side surface of the micro-image array layer away from the substrate includes at least a micro-image area and a micro-image background area, and both the micro-image area and the micro-image background area are multiple and alternately arranged; a second color layer, the second color layer is located on the side surface of the micro-image array layer away from the substrate; a first color layer, the first color layer is located between the micro-image array layer and the second color layer, there are multiple first color layers, and the multiple first color layers are arranged in a one-to-one correspondence with the multiple micro-image areas; wherein, one of the first color layer and the second color layer is a metal plating layer, and the other is an interference light variable layer.

[0009] Furthermore, the depth-to-width ratio of the micro-image area on the micro-image array layer is smaller than the depth-to-width ratio of the micro-image background area on the micro-image array layer; and / or the specific volume of the micro-image area on the micro-image array layer is smaller than the specific volume of the micro-image background area on the micro-image array layer.

[0010] Furthermore, the depth-to-width ratio of the micro-image area on the micro-image array layer is less than 0.3; and / or the depth-to-width ratio of the micro-image background area on the micro-image array layer is greater than 0.3.

[0011] Furthermore, the specific volume of the micro-image area on the micro-image array layer is greater than or equal to 0um. 3 / um 2 And less than 0.5um 3 / um 2 ; and / or the specific volume of the micro-graphic background area on the micro-graphic array layer is greater than 0.4um 3 / um 2 And less than 2um 3 / um 2 .

[0012] Furthermore, the micro-image and text area includes multiple lines, the width of some of the multiple lines is less than 5um, and the width of another part of the lines is greater than 5um; and / or the micro-image and text background area includes multiple lines, the width of some of the multiple lines is less than 5um, and the width of another part of the lines is greater than 5um.

[0013] Further, the metal plating layer includes one of aluminum, silver, copper, tin, chromium, nickel and titanium.

[0014] Furthermore, the interference optical variable layer includes an absorption layer, a dielectric layer and a reflective layer stacked in sequence, the absorption layer is arranged closer to the micro-image array layer than the reflective layer, the absorption layer includes one of aluminum, nickel, chromium, silver, copper, tin and titanium; and / or the dielectric layer includes one of MgF2, SiO2, ZnS, TiN, TiO2, TiO, Ti2O3, Ti3O5, Ta2O5, Nb2O5, CeO2, Bi2O3, Cr2O3, Fe2O3, HfO2 and ZnO; and / or the reflective layer includes one of aluminum, silver, copper, tin, chromium, nickel and titanium.

[0015] Furthermore, the interference light-variable layer is composed of optically color-variable ink.

[0016] Furthermore, the anti-counterfeiting element further includes a microstructure relaxation layer, and the microstructure relaxation layer is located between the first color layer and the second color layer.

[0017] Furthermore, a surface of the microstructure mitigation layer facing the second color layer is flat.

[0018] According to another aspect of the present invention, there is provided an anti-counterfeiting product comprising the anti-counterfeiting element described above.

[0019] Further, the anti-counterfeiting product includes a label, a hot stamping strip, a sticker and a security thread.

[0020] Applying the technical solution of the present invention, the anti-counterfeiting element includes a substrate, a microlens array layer, a micro-image array layer, a second color layer and a first color layer, the substrate includes a first surface and a second surface opposite to each other; the microlens array layer is located on the first surface of the substrate; the micro-image array layer is located on the second surface of the substrate, and the surface of the micro-image array layer on the side away from the substrate at least includes a micro-image area and a micro-image background area, and both the micro-image area and the micro-image background area are multiple and alternately arranged; the second color layer is located on the surface of the micro-image array layer on the side away from the substrate; the first color layer is located between the micro-image array layer and the second color layer, there are multiple first color layers, and the multiple first color layers are arranged in a one-to-one correspondence with the multiple micro-image areas; wherein, one of the first color layer and the second color layer is a metal plating layer, and the other is an interference light variable layer.

[0021] By setting a microlens array layer and a micro-image array layer, the microlens array layer samples and synthesizes the micro-image array layer to form an enlarged image. Since the micro-image area of ​​the micro-image array layer corresponds to the first color layer, and the micro-image background area corresponds to the second color layer, after the moiré magnification of the microlens array layer, as the observation angle changes, the micro-image area not only presents a dynamic effect formed by the moiré magnification effect, but also presents a specific optical effect, such as hologram, relief, etc., and the micro-image area and the micro-image background area have different color effects. When the first color layer is a metal plating layer and the second color layer is an interference light variable layer, after imaging, the micro-image area has the display characteristics of the metal plating layer, and the micro-image background area has a color change characteristic that changes with the observation angle, which further enhances the anti-counterfeiting ability of the anti-counterfeiting element and ensures the reliability of the use of the anti-counterfeiting element. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] The drawings constituting a part of the present application are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings:

[0023] Figure 1 A schematic structural diagram of an anti-counterfeiting element according to an optional embodiment of the present invention is shown;

[0024] Figure 2 A schematic structural diagram of an anti-counterfeiting element according to another optional embodiment of the present invention is shown;

[0025] Figure 3 A schematic structural diagram of an anti-counterfeiting element according to another optional embodiment of the present invention is shown.

[0026] The above drawings include the following reference numerals:

[0027] 1. Substrate; 2. Microlens array layer; 3. Micro-image array layer; A. Micro-image area; B. Micro-image background area; 4. First color layer; 5. Microstructure relaxation layer; 6. Second color layer; 61. Absorption layer; 62. Dielectric layer; 63. Reflection layer; 7. Hot melt adhesive layer. DETAILED DESCRIPTION

[0028] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The present invention will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.

[0029] It should be noted that, unless otherwise specified, all technical and scientific terms used in this application have the same meanings as commonly understood by ordinary technicians in the technical field to which this application belongs.

[0030] In the present invention, unless otherwise specified, the directional words used, such as "up, down, top, bottom", usually refer to the directions shown in the drawings, or to the components themselves in the vertical, perpendicular or gravity directions; similarly, for ease of understanding and description, "inside and outside" refer to the inside and outside relative to the outline of each component itself, but the above-mentioned directional words are not used to limit the present invention.

[0031] In order to solve the problem of poor anti-counterfeiting performance of anti-counterfeiting elements in the prior art, the present invention provides an anti-counterfeiting element and an anti-counterfeiting product.

[0032] like Figures 1 to 3 As shown, the anti-counterfeiting element includes a substrate 1, a microlens array layer 2, a micro-image array layer 3, a second color layer 6 and a first color layer 4, the substrate 1 includes a first surface and a second surface opposite to each other; the microlens array layer 2 is located on the first surface of the substrate 1; the micro-image array layer 3 is located on the second surface of the substrate 1, and the side surface of the micro-image array layer 3 away from the substrate 1 at least includes a micro-image area A and a micro-image background area B, and both the micro-image area A and the micro-image background area B are multiple and alternately arranged; the second color layer 6 is located on the side surface of the micro-image array layer 3 away from the substrate 1; the first color layer 4 is located between the micro-image array layer 3 and the second color layer 6, there are multiple first color layers 4, and the multiple first color layers 4 are arranged one-to-one with the multiple micro-image areas A; wherein, one of the first color layer 4 and the second color layer 6 is a metal plating layer, and the other is an interference light variable layer.

[0033] By setting the microlens array layer 2 and the micro-image array layer 3, the microlens array layer 2 samples and synthesizes the micro-image array layer 3 to form an enlarged image. Since the micro-image area A of the micro-image array layer 3 corresponds to the first color layer 4, and the micro-image background area B corresponds to the second color layer 6, after the moiré magnification of the microlens array layer 2, as the observation angle changes, the micro-image area A not only presents the dynamic effect formed by the moiré magnification effect, but also presents a specific optical effect, such as hologram, relief, etc., and the micro-image area A and the micro-image background area B have different color effects. When the first color layer 4 is a metal plating layer and the second color layer 6 is an interference light variable layer, after imaging, the micro-image area A has the display characteristics of the metal plating layer, and the micro-image background area B has the color change characteristics that change with the observation angle, which further enhances the anti-counterfeiting ability of the anti-counterfeiting element and ensures the reliability of the use of the anti-counterfeiting element.

[0034] The invention relates to an anti-counterfeiting element suitable for various high-security or high-value-added products such as banknotes, cards and product packaging, and to products with the anti-counterfeiting element.

[0035] It should be noted that the micro-graphics area A and the micro-graphics background area B are artificial divisions for the sake of simplicity and are not absolute. For example, an Arabic numeral can be considered as the micro-graphics area A and the rest of the area as the micro-graphics background area B, or the numeral itself can be considered as the micro-graphics background area B and the rest of the area as the micro-graphics area A.

[0036] It should be noted that, in the present application, the first color layer 4 is a metal plating layer, and the second color layer 6 is an interference light variable layer. Of course, they can also be selected according to actual conditions.

[0037] Observing from the side of the substrate 1 with the microlens array layer 2, the microlens array layer 2 of the anti-counterfeiting element can sample and synthesize the micro-image array layer 3 to form an enlarged image, and the imaged micro-image area A has the characteristics of being combined with the first color layer 4, and the micro-image background area B has the characteristics of the second color layer 6. Although the micro-image area A and the micro-image background area B are both provided with the second color layer 6, that is, the interference light-variable layer, the metal plating layer is sandwiched between the micro-image array layer 3 and the interference light-variable layer. Therefore, when observing from the side of the microlens array layer 2, the interference light-variable layer corresponding to the micro-image area A is not visible.

[0038] Preferably, the microlens array layer 2 is a columnar microlens array. When the observation angle is perpendicular to the stretching direction of the columnar microlens, it can be seen that the micro-image area A has obvious dynamic features formed by the moiré principle, such as movement, scaling, distortion, etc., while the color change feature is not obvious; when the observation angle changes along the stretching direction of the columnar microlens, it can be seen that the micro-image background area B has obvious color change features, while the micro-image area A does not have obvious dynamic features formed by the moiré principle. Such a visual effect effectively increases the recognizability of the anti-counterfeiting element.

[0039] In order to facilitate application on the protected product, the anti-counterfeiting element should not be too thick. Thus, the focal length of the microlens array layer 2 is generally required to be 10um to 100um. Accordingly, the period of the microlens array layer 2 and the micro-image array layer 3 are both 10um to 100um. With the anti-counterfeiting element of the present invention, there is no restriction on the line size of the micro-image area A and the micro-image background area B. It can contain ultra-fine lines, such as lines with a width of less than 8um, and can also contain relatively macroscopic lines, such as lines with a width of more than 20um, and can also contain ultra-fine lines and macroscopic lines at the same time.

[0040] Specifically, the micro-graphic area A includes multiple lines, the width of some of the multiple lines is less than 5um, and the width of another part of the lines is greater than 5um; the micro-graphic background area B includes multiple lines, the width of some of the multiple lines is less than 5um, and the width of another part of the lines is greater than 5um, which can be set according to actual conditions.

[0041] In order to achieve the production of high-precision lines in the micro-image area A and the micro-image background area B, that is, to achieve the precise removal of the metal coating in the micro-image background area B, a unique non-traditional metal layer hollowing technology must be used, which is generally referred to as precise hollowing technology. The line fineness achieved by traditional printing hollowing technology is generally greater than 100um, which is difficult to meet the integration with microlens array technology. Patent documents CN200680006666.1 and CN201510954137.5 disclose methods for realizing precise hollowing technology based on different technical principles. The former uses the difference in the depth-to-width ratio of the microstructure to achieve precise hollowing, and the latter uses the difference in the specific volume of the microstructure to achieve precise hollowing. The depth-to-width ratio of the microstructure mentioned here refers to the ratio of the depth of the microstructure to the width along the periodic direction. The specific volume of the microstructure refers to the ratio of the volume of liquid that is assumed to completely cover the surface of the microstructure when the microstructure layer is placed in a horizontal state to the projection area of ​​the microstructure on the horizontal plane. According to this definition, the depth-to-width ratio is a dimensionless physical quantity, and the dimension of the specific volume is um. 3 / um 2According to this definition, a flat structure is considered to have an aspect ratio of zero and a specific volume of zero. Aspect ratio and specific volume are two physical quantities that have no direct relationship in terms of quantity. For example, if the C structure is a one-dimensional sawtooth grating with a depth of 1um and a period of 1um, its aspect ratio is 1 and its specific volume is 0.5um. 3 / um 2 ; The D structure is a one-dimensional sawtooth grating with a depth of 2um and a period of 4um, so its aspect ratio is 0.5 and its specific volume is 1um 3 / um 2 . If the depth-to-width ratio of the microstructure of the micro-image area A is smaller than the depth-to-width ratio of the microstructure of the micro-image background area B, the metal plating of the micro-image background area B can be precisely removed according to the method disclosed in patent CN200680006666.1; if the specific volume of the microstructure of the micro-image area A is smaller than the specific volume of the microstructure of the micro-image background area B, the metal plating of the micro-image background area B can be precisely removed according to the method disclosed in patent CN201510954137.5; if the depth-to-width ratio of the microstructure of the micro-image area A is smaller than the depth-to-width ratio of the microstructure of the micro-image background area B, and at the same time, the specific volume of the microstructure of the micro-image area A is smaller than the specific volume of the microstructure of the micro-image background area B, the metal plating of the micro-image background area B can be precisely removed according to both the method disclosed in patent CN200680006666.1 and the method disclosed in CN201510954137.5.

[0042] Specifically, the depth-to-width ratio of the micro-image area A on the micro-image array layer 3 is smaller than the depth-to-width ratio of the micro-image background area B on the micro-image array layer 3; the specific volume of the micro-image area A on the micro-image array layer 3 is smaller than the specific volume of the micro-image background area B on the micro-image array layer 3. The depth-to-width ratio of the micro-image area A on the micro-image array layer 3 can be understood as the depth-to-width ratio of the microstructure of the above-mentioned micro-image area A, the depth-to-width ratio of the micro-image background area B on the micro-image array layer 3 can be understood as the depth-to-width ratio of the microstructure of the above-mentioned micro-image background area B, the specific volume of the micro-image area A on the micro-image array layer 3 can be understood as the specific volume of the microstructure of the above-mentioned micro-image area A, and the specific volume of the micro-image background area B on the micro-image array layer 3 can be understood as the specific volume of the microstructure of the above-mentioned micro-image background area B.

[0043] Specifically, the micro-graphic area A of the present application needs to be provided with a high-brightness metal coating, so the depth-to-width ratio of the micro-graphic area A should be smaller to ensure the reflectivity of the metal coating. The depth-to-width ratio of the micro-graphic area A on the micro-graphic array layer 3 is less than 0.3; the depth-to-width ratio of the micro-graphic background area B on the micro-graphic array layer 3 is greater than 0.3. Preferably, the microstructure of the micro-graphic area A is a grating structure with a depth less than 200nm and a width greater than 800nm. The microstructure of the micro-graphic area A can provide special optical effects for the metal coating, such as holography, relief, etc., and the parameters are set according to the specific product requirements. The specific volume of the micro-graphic area A on the micro-graphic array layer 3 is greater than or equal to 0um. 3 / um 2 And less than 0.5um 3 / um 2 The specific volume of the micro-graphic background area B on the micro-graphic array layer 3 is greater than 0.4um 3 / um 2 And less than 2um 3 / um 2 .

[0044] Specifically, the metal coating includes one of aluminum, silver, copper, tin, chromium, nickel and titanium. Of course, the metal coating can also be an alloy of aluminum, silver, copper, tin, chromium, nickel and titanium. Due to the high brightness and low cost of aluminum, the material of the metal coating is preferably aluminum.

[0045] Specifically, the interference optical variable layer has definite and obviously different color characteristics when viewed from the front and when viewed from an angle, respectively, and has a high anti-counterfeiting effect. The interference optical variable layer includes an absorption layer 61, a dielectric layer 62, and a reflective layer 63 stacked in sequence, the absorption layer 61 is arranged closer to the micro-image array layer 3 than the reflective layer 63, the absorption layer 61 includes one of aluminum, nickel, chromium, silver, copper, tin and titanium, or an alloy thereof; the dielectric layer 62 includes one of MgF2, SiO2, ZnS, TiN, TiO2, TiO, Ti2O3, Ti3O5, Ta2O5, Nb2O5, CeO2, Bi2O3, Cr2O3, Fe2O3, HfO2 and ZnO; the reflective layer 63 includes one of aluminum, silver, copper, tin, chromium, nickel and titanium, or an alloy thereof.

[0046] If the arrangement of the microstructure of the micro-image background area B can form a specific optical effect, such as dynamic, zooming, etc., then the micro-image background area B after moiré magnification has an optical effect that combines the specific optical effect and the interference light-changing effect.

[0047] like Figure 2In another embodiment shown, the anti-counterfeiting element further includes a microstructure relaxation layer 5, which is located between the first color layer 4 and the second color layer 6. Due to the need for hollowing out, the depth of the microstructure of the micro-graphic background area B is usually large, and the brightness of the interference light variable layer directly formed may be poor. Preferably, a microstructure relaxation layer 5 of a certain thickness is first applied, and then the interference light variable layer is formed. After applying the microstructure relaxation layer 5, the microstructure of the micro-graphic background area B becomes appropriately lighter, the color of the interference light variable layer becomes brighter, and the specific optical effect presented by the microstructure is not affected. It is also possible to choose to apply a thicker microstructure relaxation layer 5 to fill the microstructure and turn it into a flat structure. In this way, although the micro-graphic background area B no longer presents a specific optical effect, the interference light variable layer on the flat structure has the highest interference efficiency and the highest color saturation. The surface of the microstructure relaxation layer 5 facing the second color layer 6 is a plane.

[0048] like Figure 3 In another embodiment shown, the interference light variable layer is composed of optically variable ink (OVI). The pigment of the optically variable ink is a crushed interference light variable coating layer. Generally, the pigment flakes of the optically variable ink are large and will completely cover the microstructure of the micro-image background area B, so that the specific optical effect of the microstructure will not be presented. After the ink film is formed and dried, the pigment flakes are basically arranged along the plane of the interference light variable layer, forming a color change effect similar to that of the interference light variable layer.

[0049] like Figures 1 to 3 As shown, in order to achieve the functions of bonding the anti-counterfeiting element to the protected product, the anti-counterfeiting element further includes a hot melt adhesive layer 7, which is connected to the surface of the second color layer 6 away from the substrate 1. Of course, the hot melt adhesive layer 7 can also be a coating with other functions.

[0050] The present application provides an anti-counterfeiting product, including the above-mentioned anti-counterfeiting element. Specifically, the anti-counterfeiting product includes a label, a hot stamping strip, a sticker and a security thread.

[0051] Figures 1 to 3 Three implementations of the anti-counterfeiting element of the present application are shown respectively:

[0052] like Figure 1, is a cross-sectional view of an exemplary anti-counterfeiting element according to an embodiment of the present invention. The substrate 1 is composed of a biaxially oriented polypropylene (BOPP) film with a thickness of 70um. A microlens array layer 2 formed of a plurality of columnar microlenses is formed on the first surface of the substrate 1. The microlens array layer 2 is formed by UV resin cured by UV light irradiation. The period of the microlens array layer 2 is 50um and the height is 10um. The second surface of the substrate 1 has a micro-image array layer 3. The micro-image array layer 3 is formed by UV resin cured by UV light irradiation. The period is 50.2um and the thickness is 5um. The surface of the micro-graphic array layer 3 on one side away from the substrate 1 is divided into a micro-graphic area A and a micro-graphic background area B according to the different specific volumes of the microstructures on the surface, wherein the microstructure of the micro-graphic area A is a Fresnel grating structure with a depth of 0.1-0.2um, a period of 0.8-10um, and a three-dimensional relief effect, and the microstructure of the micro-graphic background area B is a micro-mirror grating structure with a depth of 1um, a period of 4um, and a horizontal arrangement that can form a scroll bar feature. The micro-graphic area A of the micro-graphic array layer 3 is provided with a first color layer 4, that is, a metal coating, and the metal coating is an aluminum layer with a thickness of 30nm, and the micro-graphic background area B is not provided with a metal coating. The micro-graphic area A and the micro-graphic background area B are provided with a second color layer 6, that is, an interference light variable layer as a whole. The aluminum layer is sandwiched between the micro-graphic array layer 3 and the interference light variable layer. The interference optical variable layer is composed of an absorption layer 61, a dielectric layer 62 and a reflection layer 63, the materials of which are Ni, SiO2 and Al, and the thicknesses are 5nm, 380nm and 50nm respectively. The anti-counterfeiting element also has a hot melt adhesive layer 7 for bonding with the protected product.

[0053] When observing from one side of the microlens array layer 2, the observation angle changes along the stretching direction of the columnar microlenses, and it can be seen that the micro-image background area B is golden when viewed straight on and green when observed at an angle, and has the characteristics of a scroll bar; when the observation angle changes perpendicular to the stretching direction of the columnar microlenses, it can be seen that the three-dimensional relief image has obvious dynamic characteristics (such as movement, scaling, distortion, etc.) formed by the Moore principle.

[0054] like Figure 2As shown, it is a cross-sectional view of another exemplary anti-counterfeiting element according to an embodiment of the present invention. The substrate 1 is composed of a polyethylene terephthalate (PET) film with a thickness of 15um. The first surface of the substrate 1 has a microlens array layer 2 composed of a plurality of columnar microlenses, which is formed by UV resin being cured by UV light irradiation, and the period of the microlens array layer 2 is 25um and the height is 5um. The second surface of the substrate 1 is formed with a micro-image array layer 3, which is formed by UV resin being cured by UV light irradiation, with a period of 25.1um and a thickness of 5um. The surface of the micro-image array layer 3 on one side away from the substrate 1 is divided into a micro-image area A and a micro-image background area B according to the different depth-to-width ratios of the microstructure of the surface, wherein the depth of the microstructure of the micro-image area A is 0.1-0.15um, the period is 0.8-1.2um, and the cross section is a cosine grating, and the depth of the microstructure of the micro-image background area B is 0.3um, the period is 1um, and the cross section is a cosine grating. The micro-image area A of the micro-image array layer 3 is provided with a first color layer 4, that is, a metal coating, and the metal coating is an aluminum layer with a thickness of 30nm. The micro-image background area B is not provided with an aluminum layer. The micro-image area A and the micro-image background area B are provided with a microstructure relaxation layer 5 as a whole, with a thickness of 4um. The aluminum layer is sandwiched between the micro-image array layer 3 and the interference light variable layer. Because the material refractive index of the micro-image array layer 3 and the material refractive index of the microstructure relaxation layer 5 are basically the same, the micro-image background area B is basically invisible at the interface of the micro-image array layer 3. The side of the microstructure relaxation layer 5 away from the substrate 1 is a flat structure. The microstructure relaxation layer 5 is provided with an interference light variable layer as a whole, and the interference light variable layer is composed of an absorption layer 61, a dielectric layer 62, and a reflection layer 63. The materials are Ni, SiO2 and Al, respectively, and the thicknesses are 5nm, 380nm, and 50nm, respectively. The absorption layer 61 is connected to the microstructure relaxation layer 5. The anti-counterfeiting element also has a hot-melt adhesive layer 7 for bonding with the protected product.

[0055] Observing from one side of the microlens array layer 2, the observation angle changes along the stretching direction of the columnar microlenses, and it can be seen that the micro-image background area B is highly saturated gold when viewed straight on, and is highly saturated green when observed at an angle; the observation angle changes perpendicular to the stretching direction of the columnar microlenses, and it can be seen that the micro-image area A with rainbow holographic features has obvious dynamic features (such as movement, scaling, distortion, etc.) formed by the Moore principle.

[0056] like Figure 3, is a cross-sectional view of another exemplary anti-counterfeiting element according to an embodiment of the present invention. The substrate 1 is composed of a polyethylene terephthalate (PET) film with a thickness of 15um. The first surface of the substrate 1 has a microlens array layer 2 composed of a plurality of columnar microlenses, which is formed by UV resin being cured by UV light irradiation, and the period of the microlens array layer 2 is 25um and the height is 5um. The second surface of the substrate 1 is formed with a micro-image array layer 3, which is formed by UV resin being cured by UV light irradiation, with a period of 25.1um and a thickness of 5um. The surface of the micro-image array layer 3 on one side away from the substrate 1 is divided into a micro-image area A and a micro-image background area B according to the different depth-to-width ratios of the microstructure of the surface, wherein the depth of the microstructure of the micro-image area A is 0.1um-0.15um, the period is 0.8-1.2um, and the cross section is a cosine grating, and the depth of the microstructure of the micro-image background area B is 0.3um, the period is 1um, and the cross section is a cosine grating. The micro-image area A of the micro-image array layer 3 is provided with a first color layer 4, that is, a metal plating layer, which is an aluminum layer with a thickness of 30nm, and the micro-image background area B is not provided with an aluminum layer. The micro-image area A and the micro-image background area B are provided with a second color layer 6 as a whole. In this embodiment, the second color layer 6 is an interference light variable layer, and the interference light variable layer is composed of optical color variable ink (OVI). The aluminum layer is sandwiched between the micro-image array layer 3 and the interference light variable layer. Because the material refractive index of the micro-image array layer 3 and the material refractive index of the binder in the optical color variable ink are basically the same, the micro-image background area B is basically invisible at the interface of the micro-image array layer 3. The pigment of the optical color variable ink is a crushed interference light variable plating layer sheet, for example, it can be Ni, SiO2, Al, SiO2 and Ni, with thicknesses of 5nm, 380nm, 50nm, 380nm, 5nm, respectively, and the typical diameter of the interference light variable plating layer sheet is 40um. The pigment flakes of the optically chromic ink have a much larger period than the microstructure of the micro-image background area B, and thus completely cover the microstructure. After the optically chromic ink forms a film and dries, the pigment flakes are basically arranged along the plane of the micro-image array layer 3. The anti-counterfeiting element also has a hot melt adhesive layer 7 that acts as a bond with the protected product.

[0057] Observing from one side of the microlens array layer 2, the observation angle changes along the stretching direction of the columnar microlenses, and it can be seen that the micro-image background area B is golden when viewed straight on and green when observed at an angle; the observation angle changes perpendicular to the stretching direction of the columnar microlenses, and it can be seen that the image with rainbow holographic characteristics has obvious dynamic features (such as movement, scaling, distortion, etc.) formed by the Moore principle.

[0058] compared to Figure 2 The security element shown, Figure 3The color saturation and brightness of the micro-image background area B of the anti-counterfeiting element shown are slightly poor, but the advantage is that the optically variable ink OVI can be locally set through the printing process to form a pattern of a specific shape.

[0059] Obviously, the above-described embodiments are only a part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.

[0060] It should be noted that the terms used herein are only for describing specific embodiments and are not intended to limit the exemplary embodiments according to the present application. As used herein, unless the context clearly indicates otherwise, the singular form is also intended to include the plural form. In addition, it should be understood that when the terms "comprise" and / or "include" are used in this specification, it indicates the presence of features, steps, operations, devices, components and / or combinations thereof.

[0061] It should be noted that the terms "first", "second", etc. in the specification and claims of the present application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the numbers used in this way can be interchanged where appropriate, so that the embodiments of the present application described herein can be implemented in an order other than those illustrated or described herein.

[0062] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. An anti-counterfeiting element, It is characterized in that The anti-counterfeiting element comprises: A substrate (1), the substrate (1) comprising a first surface and a second surface opposite to each other; A microlens array layer (2), the microlens array layer (2) being located on the first surface of the substrate (1); A micro-image array layer (3), the micro-image array layer (3) being located on the second surface of the substrate (1), the surface of the micro-image array layer (3) being away from the substrate (1) comprising at least a micro-image area (A) and a micro-image background area (B), the micro-image area (A) and the micro-image background area (B) being multiple and arranged alternately; A second color layer (6), the second color layer (6) being located on a surface of the micro-image array layer (3) that is away from the substrate (1); a first color layer (4), the first color layer (4) being located between the micro-image array layer (3) and the second color layer (6), the first color layer (4) being multiple, and the multiple first color layers (4) being arranged in a one-to-one correspondence with the multiple micro-image areas (A); The first color layer (4) is a metal plating layer, and the second color layer (6) is an interference light-variable layer; when observed from the side of the substrate (1) having the microlens array layer (2), the microlens array layer (2) of the anti-counterfeiting element samples and synthesizes the micro-image array layer (3) to form an enlarged image, and the imaged micro-image area (A) has the characteristics of the micro-image area and the first color layer (4), the micro-image background area (B) has the characteristics of the second color layer (6), and the interference light-variable layer is not visible in the micro-image area (A).

2. The anti-counterfeiting element according to claim 1, It is characterized in that The aspect ratio of the micro-image area (A) on the micro-image array layer (3) is smaller than the aspect ratio of the micro-image background area (B) on the micro-image array layer (3); and / or The specific volume of the micro-image and text area (A) on the micro-image and text array layer (3) is smaller than the specific volume of the micro-image and text background area (B) on the micro-image and text array layer (3).

3. The anti-counterfeiting element according to claim 1, It is characterized in that The aspect ratio of the micro-image area (A) on the micro-image array layer (3) is less than 0.3; and / or The aspect ratio of the micro-image background area (B) on the micro-image array layer (3) is greater than 0.

3.

4. The anti-counterfeiting element according to claim 1, It is characterized in that The specific volume of the micro-image area (A) on the micro-image array layer (3) is greater than or equal to 0 um. 3 / um 2 And less than 0.5um 3 / um 2 ; and / or The specific volume of the micro-image background area (B) on the micro-image array layer (3) is greater than 0.4 μm. 3 / um 2 And less than 2um 3 / um 2 .

5. The anti-counterfeiting element according to claim 1, It is characterized in that The micro-image area (A) includes a plurality of lines, some of which have a width less than 5 um, and another portion of which has a width greater than 5 um; and / or The micro-image background area (B) includes a plurality of lines, some of which have a width less than 5 um, and another portion of which has a width greater than 5 um.

6. The anti-counterfeiting element according to claim 1, It is characterized in that The metal plating layer includes one of aluminum, silver, copper, tin, chromium, nickel and titanium.

7. The anti-counterfeiting element according to claim 1, It is characterized in that The interference optical variable layer comprises an absorption layer (61), a dielectric layer (62) and a reflection layer (63) stacked in sequence, wherein the absorption layer (61) is arranged closer to the micro-image array layer (3) than the reflection layer (63). The absorption layer (61) comprises one of aluminum, nickel, chromium, silver, copper, tin and titanium; and / or The dielectric layer (62) includes MgF 2 、SiO 2 、ZnS、TiN、TiO 2 、TiO、Ti 2 O 3 、Ti 3 O 5 、 2 O 5 , Nb 2 O 5 、CeO 2 、Bi 2 O 3 Cr 2 O 3 , Fe 2 O 3 , HfO 2 and ZnO; and / or The reflective layer (63) comprises one of aluminum, silver, copper, tin, chromium, nickel and titanium.

8. The anti-counterfeiting element according to claim 1, It is characterized in that The interference light-variable layer is made of optical color-variable ink.

9. The anti-counterfeiting element according to claim 1, It is characterized in that The anti-counterfeiting element further comprises a microstructure relaxation layer (5), wherein the microstructure relaxation layer (5) is located between the first color layer (4) and the second color layer (6).

10. The anti-counterfeiting element according to claim 9, It is characterized in that The surface of the microstructure relaxation layer (5) facing the second color layer (6) is a plane. 11.An anti-counterfeiting product, It is characterized in that The anti-counterfeiting element comprises the anti-counterfeiting element according to any one of claims 1 to 10.

12. The anti-counterfeiting product according to claim 11, It is characterized in that The anti-counterfeiting product includes a label, a hot stamping strip, a sticker and a security thread.

Citation Information

Patent Citations

  • Method for producing a multilayer body and corresponding multilayer body

    CN101166633A

  • Optical anti-counterfeiting member and preparation method thereof

    CN106891637A

  • Optical anti-fake component and products using the same and preparation method of optical anti-fake component

    CN102975568A

  • Optical anti-counterfeiting element and optical anti-counterfeiting product using optical anti-counterfeiting element

    CN105479974A

  • Optical anti-counterfeiting element, preparation method thereof and optical anti-counterfeiting product