An improved hot-dip galvanizing horizontal continuous annealing furnace hot strip threading method
By designing the "working" thermal threading needle and steel ball iron chain anti-tangle method of 0Cr18Ni9Ti material, the failure and interruption of the hot-wiring belt of the horizontal continuous annealing furnace is solved, and an efficient and reliable thermal-wiring process is achieved, which significantly Improves success rate and saves energy and material consumption.
Patent Information
- Application Number
- CN202310160210.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-02-24
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2043-02-24
AI Technical Summary
In the prior art, the horizontal continuous annealing furnace hot-through belt has problems in the selection and appearance design of needle threading materials, resulting in failure and interruption of the hot-through belt process, and lack of reliable operating methods, which affects the unit's operating efficiency and energy consumption.
Design a "working"-shaped heat threading needle made of 0Cr18Ni9Ti material, and adopts the anti-tangle method of steel ball iron chain to ensure that the strip steel passes through the inlet of the horizontal continuous annealing furnace to the 4# thermal tension roller steering chamber to prevent steel The belt is tangled to achieve disposable heat-wrapping belt.
Improve the success rate of thermal strap penetration to 100%, shorten the thermal strap penetration time, reduce from 3.0 hours to 1.0 hours, save energy consumption and material consumption, reduce the loss of shutdown materials and secondary strap penetration, and save 931,500 yuan in annual savings Yuan.
Smart Images

Figure CN116162783B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to an improved hot-dip galvanizing horizontal continuous annealing furnace hot strip threading method. Background Art
[0002] Hot threading of galvanized horizontal continuous annealing furnace is the key process technology of hot-dip galvanizing unit, which directly affects the success rate of annealing furnace threading and the operation efficiency of the unit. Since the hot threading of horizontal continuous annealing furnace uses a new type of needle to thread from the annealing furnace entrance to the 4# hot tension roller turning chamber and uses 2# steel ball iron chain with the help of steel ball iron chain anti-entanglement method to thread from the 4# hot tension roller 1# roller in the turning chamber and the 2# roller out of the reasonable connection, the hot threading is ensured to be successful; otherwise, it will cause the hot threading failure and the hot threading of the annealing furnace will be interrupted. The hot threading of continuous annealing furnace has many influencing factors and complex environmental conditions. Therefore, the research on the hot threading of annealing furnace has become the focus of attention of manufacturers. Different manufacturers have reported on the hot threading of continuous annealing furnace.
[0003] The literature search revealed: (1) Li Jiuling's "Continuous Hot-dip Galvanizing of Strip Steel" 2012 3rd Edition P204-207 "First Threading of New Production" and "Threading of Broken Strip Accident" of Horizontal Furnaces, introduced the cold and hot threading methods of horizontal annealing furnaces without 4# hot tension rollers in the furnace, and solved the technical problems of cold threading of the furnace or recovery from broken strips in the furnace to normal production. (2) Li Weiqiang, Ma Changlong, etc. in "Research and Improvement Methods of Threading Methods of Horizontal Annealing Furnaces" in "Industrial Furnaces" Vol. 44, No. 3, 2022 P36-38 systematically analyzed the selection and improvement methods of threading methods in horizontal annealing furnaces during production, conducted in-depth research on the changes in the threading process, found out the problems in the threading process, and took measures to eliminate them, thereby improving the success rate of threading in the annealing furnace and the operating efficiency of the unit.
[0004] From the above information, it can be known that hot-dip galvanizing horizontal continuous annealing furnace hot-dip galvanizing is a common process technology problem in the hot-dip galvanizing process of metallurgical enterprises. It is necessary for hot-dip galvanizing startup, or for the recovery of normal production of the unit due to belt breakage in the continuous annealing furnace. However, there are problems with the selection of needle materials and the design of external dimensions for hot-dip galvanizing of the continuous annealing furnace, and unreasonable and non-standard hot-dip galvanizing operation may cause the hot-dip galvanizing process of the annealing furnace to fail and be interrupted. At present, there is no specific, reliable and operable method for hot-dip galvanizing of the continuous annealing furnace that has been verified in actual production. Summary of the invention
[0005] The object of the present invention is to provide an improved hot-dip galvanizing horizontal continuous annealing furnace hot strip threading method, which can improve the unit operation rate, product yield rate and reduce energy consumption.
[0006] The object of the present invention is achieved by: An improved hot-dip galvanizing horizontal continuous annealing furnace hot strip threading method, first prepare the tool according to the following steps:
[0007] 1) Design and manufacture a hot-threading needle, which is made of 0Cr18Ni9Ti, has an "I"-shaped cross-section, a height of 60mm, and a needle length of 9200mm;
[0008] 2) The steel strip is hot threaded at the 4# hot tension roller group in the turning chamber of the annealing furnace using the steel ball iron chain anti-entanglement method. The steel ball iron chain is designed and manufactured. The iron chain is a 2# oblong chain link iron chain, and one end of the iron chain is connected to a steel ball. The specific steps are as follows:
[0009] A. Open the 1# gate valve hole on the top of the annealing furnace turning room at the 4# hot tension roller group. The operator places one end of the 2# oblong chain ring iron chain with a steel ball at the front end of the 2# roller of the 4# hot tension roller group through the 1# gate valve hole, and places the front end chain of the 2# oblong chain ring iron chain at the working side WS of the 2# roller, and the rear end chain of the 2# oblong chain ring iron chain at the transmission side DS of the 2# roller. Open the 2# and 3# gate valves in the annealing furnace turning room to the maximum, so that the 3# gate valve and the production operator at the 2# gate valve on the platform can coordinate and cooperate. With the help of a flashlight and a long-arm iron hook, the front end of the 2# oblong chain ring iron chain and its rear end are staggered, and the horizontal spacing S>300mm. Then, with the help of a flashlight, manually use a long-arm iron hook to pull the steel ball at the front end of the 2# oblong chain ring iron chain out of the turning room to the valve hole of the 2# gate valve, and fix the iron chain steel ball to the working side WS of the 2# gate valve handle.
[0010] B. The tail of the threading needle in step 1) is also connected to a chain, which is a 1# rectangular chain link iron chain. The end of the chain is connected to the steel strip through a triangular ring. The steel strip is pulled into the annealing furnace by the threading needle. With the completion of the first stage of hot threading, the threading needle and the head of the 1# iron chain pass through the 3# gate valve hole of the annealing furnace. The 5-ton crane above the zinc pot area is started to lift the threading needle away, and then the front chain of the 1# iron chain is fixed to the transmission side DS of the valve handle of the 3# gate valve, and then the chain ring of the rear end chain of the 2# iron chain is hooked out from the steering chamber and connected to the chain ring of the front chain of the 1# iron chain with a lock buckle;
[0011] The production staff at C, 2# and 3# gate valves coordinated and cooperated, and used flashlights and long-arm iron hooks to hook the steel ball out from between the 1# and 2# iron chains, and then followed steps A and B. After checking that everything was correct, the steel ball was thrown into the bottom of the turning chamber furnace from the valve hole of the 2# valve plate with the help of a long-arm iron hook. After coordination by the staff at 2# and 3# gate valves, the steel ball was guided into the wedge groove under the annealing furnace and submerged in the zinc pot. The steel ball was manually fished out from the front end of the sinking roller as required. At the same time, the 1#, 2# and 3# gate valves were closed to complete the hot threading of the annealing furnace.
[0012] The present invention: 1. A new type of hot strip threading tool is used, and the strip can be stably, reliably and quickly threaded from the entrance of the horizontal continuous annealing furnace to the turning chamber of the 4# hot tension roller with the help of its traction; 2. By adopting the steel ball and iron chain method, the strip can be continuously and stably threaded from the 1# roller of the 4# hot tension roller in the turning chamber and the 2# roller out, and because the 4# hot tension roller in the turning chamber adopts a method to prevent the entanglement of the steel ball and iron chain for hot strip threading, the steel strip can be stably and reliably threaded on the 4# hot tension roller, which is the key to the 100% success rate of hot strip threading on the 4# hot tension roller; 3. During the hot strip threading process when the hot-dip galvanizing machine is started, or the unit is restored to normal production due to a broken strip in the annealing furnace, the problem of high energy consumption and material consumption indicators is solved. The method is simple, efficient, and highly operable, and the success rate of hot strip threading is 100%; the use of this method for hot strip threading can prevent the steel strip from overflowing between the furnace rollers in large amounts and the high temperature at the overlap, which may cause secondary strip breakage;
[0013] Beneficial effects of the present invention:
[0014] The heat-threading time is shortened from 3.0h to 1.0h, which produces benefits.
[0015] 1.1 The benefits of production loss: hourly output is about 25 tons, and the benefit per ton of steel = 200 yuan; benefit = 25*2*24*200 = 24 (10,000 yuan);
[0016] 1.2 years of saving N2 and mixed gas consumption to generate benefits: During hot belt threading, N2 consumption is about 300m3 per hour, and the unit price of N2 is 2 yuan / m3; mixed gas consumption is about 32.5GJ per hour, and the unit price of mixed gas is about 25.6 yuan / GJ; benefit = (300*2*2+32.5*25.6*2)*24=68,500 yuan;
[0017] 1.3 Reducing the waste of downtime materials will generate benefits: each time the waste of downtime materials is reduced by about 5 tons, and the annual reduction of waste of downtime materials is about: 24*5=120 tons; benefit = 120*(5500-2000)=42 (million yuan);
[0018] The use of a new hot needle threading and iron chain anti-entanglement method for hot threading in the annealing furnace avoids the loss caused by secondary threading and produces benefits:
[0019] 2.1 The benefit generated by the loss of production = 25*4*4*200 = 8 (ten thousand yuan);
[0020] 2.2 Benefits generated by the consumption of N2 and mixed gas produced by secondary belt threading: Benefit = (300*2*4+32.5*25.6*4)*4=23,000 yuan;
[0021] 2.3 Loss of downtime materials and consumables caused by secondary belt breakage in the furnace due to secondary belt threading: Benefit = 5*4*(5500-2000)+2.5*4*(5000-2000)=10 (million yuan); Subtotal: 24+68,500+42+8+23,000+10=931,500 yuan; i.e., a reduction of 931,500 yuan in losses each year. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a schematic diagram of the workflow of the present invention. Implementation
[0023] An improved hot-dip galvanizing horizontal continuous annealing furnace hot strip threading method, such as Figure 1 As shown, first prepare the tools as follows:
[0024] 1) Design and manufacture a hot strip threading needle 3 to solve the problem of continuous, stable and one-time hot strip threading of strip steel from the entrance of the horizontal continuous annealing furnace to the 4# hot tension roller; the hot strip threading needle 3 is made of 0Cr18Ni9Ti, which can prevent the threading needle from deforming in a closed furnace with a temperature of 550-650℃ and a length of ~135m; its cross-sectional structure is in the shape of an "I" to ensure its strength and resistance to bending deformation; the height is 60mm to ensure a low center of gravity and stable operation; the threading needle length is designed to meet the "three rollers in one line and the shortest length principle" at any position in the furnace, that is, the threading needle is always in contact with the three furnace rollers in the furnace and has the shortest length. See the attached picture for the threading needle 3 Figure 1 , the length of needle 3 is L=350+3*3000-150=9200mm, in order to avoid the needle from deflecting and falling off during operation in the furnace. A new type of hot strip threading needle is the key to the fast, stable and one-time hot threading of the steel strip from the annealing furnace entrance to the 4# hot tension roller;
[0025] 2) The steel strip 1 is hot-threaded by the 4# hot tension roller group in the turning chamber 6 of the annealing furnace 4 using a steel ball iron chain anti-entanglement method, which is the key to achieving stable, reliable, and one-time hot threading of the steel strip between the 1# roller and the 2# roller of the 4# hot tension roller group; the steel ball iron chain is designed and manufactured, and the iron chain is a 2# oblong chain ring iron chain 10, and the chain connected to the tail of the threading needle to complete the first stage of hot threading is a 1# rectangular chain ring iron chain 2. In order to prevent the steel strip from being entangled with the front end of the traction steel strip during the threading process after the 2# iron chain is connected to the 1# iron chain during the hot threading of the 4# hot tension roller, the steel ball iron chain anti-entanglement method is adopted, and the specific steps are as follows:
[0026] A. Open the valve hole of 1# gate valve 16 on the top of 4# hot tension roller steering chamber 6 to the maximum. The operator presses Figure 1Place one end of the 2# iron chain 10 with the steel ball 11 at the front end of the 2# roller 15 of the 4# hot tension roller group, and place the front end chain of the 2# iron chain on the working side (WS) of the 2# roller 15, and the rear end chain of the 2# iron chain on the transmission side (DS) of the 2# roller 15. Open the 2# and 3# gate valves 7 and 8 to the maximum, so that the 3# gate valve 8 and the production operators at the 2# gate valve 7 on the platform can coordinate with each other. With the help of a flashlight and a long-arm iron hook, the front end of the 2# iron chain 10 and its rear end are staggered, and the lateral spacing S>300mm, and the larger the spacing, the better. Then, with the help of a flashlight, manually use the long-arm iron hook to pull the steel ball at the front end of the 2# iron chain 10 out of the steering chamber 6 to the valve hole of the 2# gate valve 7, and fix the iron chain steel ball 11 to the working side of the valve handle of the 2# gate valve 7 (WS).
[0027] B. The tail of the threading needle 3 in step 1) is also connected to a chain, which is a 1# rectangular chain link iron chain 2. The end of the chain is connected to the steel strip 1 through a triangular ring. The steel strip 1 is pulled into the annealing furnace 4 by the threading needle 3. With the completion of the first stage of hot threading, the threading needle 3 and the head of the 1# iron chain 2 pass through the hole of the 3# gate valve 8. The 5-ton crane above the zinc pot area is started to lift the threading needle 3. After that, the front chain of the 1# iron chain is fixed to the transmission side (DS) of the valve handle of the 3# gate valve 8, and then the chain ring of the rear end chain of the 2# iron chain 10 is hooked out from the steering chamber 6 and connected with the chain ring of the front chain of the 1# iron chain 2 with a lock buckle;
[0028] The production staff at C, 2#, 3# gate valves 7 and 8 coordinated and used flashlights and long-arm iron hooks to hook the steel ball 11 out from between the 1# and 2# iron chains, and then followed steps A and B. After checking that everything was correct, the steel ball 11 was thrown into the bottom of the steering chamber 6 from the valve hole of the 2# valve plate valve 7 with the help of a long-arm iron hook. After coordination by the staff at the 2# gate valve and 3# gate valves, the steel ball 11 was introduced into the lower wedge groove 9 of the annealing furnace and submerged in the zinc pot 12. The steel ball was manually fished out from the front end of the sinking roller as required, and at the same time, the 1#, 2#, 3# gate valves 16, 7, 8 were closed to complete the hot threading of the annealing furnace. This method is simple, efficient, and highly operational, with a 100% success rate for hot threading.
[0029] Take a company's 150,000-ton hot-dip galvanizing unit as an example:
[0030] The continuous annealing furnace is replaced with N2 to replace the air in the furnace. At the same time, the radiation tube is ignited and heated to a furnace temperature of 550-650℃. The furnace rollers are started to run. The new hot-threading needle is hung on the roller table 13 in front of the annealing furnace. Figure 1Connect the threading needle, chain, triangular ring and traction strip steel as shown in the figure, manually start the furnace door to rise to 60-70mm, place the threading needle head at the threading hole in the center of the bottom of the annealing furnace door, and make the threading center coincide with the center line of the continuous annealing furnace before entering the furnace, then start the 3# tension roller at the ground station at the entrance of the annealing furnace, so that there is always about 5m of steel strip overflow between the threading needle tail and the 3# tension roller, manually send the threading needle and the 3# tension roller strip steel overflow into the furnace, and wait until the threading needle completely enters the annealing furnace entrance, and then manually close it. Close the furnace door, then the ground station operator coordinates with the process operator to hot thread the strip 1 to the 4# hot tension roller group in the turning chamber 6, and then the threading needle 3 comes out from the 3# valve hole 8 in the turning chamber, and the threading needle is taken away above the zinc pot with the help of a 5t electric single-beam crane. At the same time, the hot threading of the hot-dip galvanizing horizontal continuous annealing furnace is carried out using the steps in the steel ball and iron chain anti-entanglement method for hot threading with 4# hot tension rollers. Manually close the 1#, 2#, and 3# gate valves to complete the hot threading of the annealing furnace, and then pass H2 into the furnace to raise the temperature to the normal production furnace temperature.
Claims
1. An improved hot-dip galvanizing horizontal continuous annealing furnace hot strip threading method, characterized in that First prepare the tools as follows: 1) Design and manufacture a hot-threading needle, which is made of 0Cr18Ni9Ti, with a cross-sectional structure of "I" shape, a height of 60mm, and a needle length of 9200mm; 2) The steel strip is hot threaded at the 4# hot tension roller group in the turning chamber of the annealing furnace using the steel ball iron chain anti-entanglement method. The steel ball iron chain is designed and manufactured. The iron chain is a 2# oblong chain link iron chain, and one end of the iron chain is connected to a steel ball. The specific steps are as follows: A. Open the 1# gate valve hole on the top of the annealing furnace turning room at the 4# hot tension roller group. The operator places one end of the 2# oblong chain ring iron chain with a steel ball at the front end of the 2# roller of the 4# hot tension roller group through the 1# gate valve hole, and places the front end chain of the 2# oblong chain ring iron chain at the working side WS of the 2# roller, and the rear end chain of the 2# oblong chain ring iron chain at the transmission side DS of the 2# roller. Open the 2# and 3# gate valves in the annealing furnace turning room to the maximum, so that the 3# gate valve and the production operator at the 2# gate valve on the platform can coordinate and cooperate. With the help of a flashlight and a long-arm iron hook, the front end of the 2# oblong chain ring iron chain and its rear end are staggered, and the horizontal spacing S>300mm. Then, with the help of a flashlight, manually use a long-arm iron hook to pull the steel ball at the front end of the 2# oblong chain ring iron chain out of the turning room to the valve hole of the 2# gate valve, and fix the iron chain steel ball to the working side WS of the 2# gate valve handle. B. The tail of the threading needle in step 1) is also connected to a chain, which is a 1# rectangular chain link iron chain. The end of the chain is connected to the steel strip through a triangular ring. The steel strip is pulled into the annealing furnace by the threading needle. With the completion of the first stage of hot threading, the threading needle and the head of the 1# iron chain pass through the 3# gate valve hole of the annealing furnace. The 5-ton crane above the zinc pot area is started to lift the threading needle away, and then the front chain of the 1# iron chain is fixed to the transmission side DS of the valve handle of the 3# gate valve, and then the chain ring of the rear end chain of the 2# iron chain is hooked out from the steering chamber and connected to the chain ring of the front chain of the 1# iron chain with a lock buckle; The production staff at C, 2# and 3# gate valves coordinated and cooperated, and used flashlights and long-arm iron hooks to hook the steel ball out from between the 1# and 2# iron chains, and then followed steps A and B. After checking that everything was correct, the steel ball was thrown into the bottom of the turning chamber furnace from the valve hole of the 2# valve plate with the help of a long-arm iron hook. After coordination by the staff at 2# and 3# gate valves, the steel ball was guided into the wedge groove under the annealing furnace and submerged in the zinc pot. The steel ball was manually fished out from the front end of the sinking roller as required. At the same time, the 1#, 2# and 3# gate valves were closed to complete the hot threading of the annealing furnace.