A three-dimensional 1S1C memory based on ring capacitor and preparation method thereof

By adopting the separation design of the ring capacitor and gate tube functional layer in the three-dimensional 1S1C memory, the capacitor preparation process is simplified, and the problems of complexity and low yield of capacitor preparation in the prior art are solved, thus achieving higher consistency and goodness Rate.

CN116322032BActive Publication Date: 2024-11-26HUAZHONG UNIV OF SCI & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211686527.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-12-27
Publication Date
2024-11-26
Estimated Expiration
2042-12-27

AI Technical Summary

Technical Problem

The 3D-1S1C memory capacitor preparation process with the existing 3D-NAND structure is complex, resulting in a decrease in yield and becoming a bottleneck that restricts the technical route.

Method used

Using a three-dimensional 1S1C memory design based on annular capacitors, the capacitor preparation process is simplified by forming annular grooves in the peripheral electrode layer and filling the capacitor dielectric layer. The capacitor preparation process is simplified. The capacitor unit preparation is completed in just one longitudinal etching, and through gate The separation design of the functional layer of the tube and the capacitance dielectric layer improves the consistency and yield of the preparation.

Benefits of technology

The number of etching times of capacitor preparation is reduced, the yield and consistency of capacitor preparation is improved, the process flow is simplified, and the performance of the memory is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116322032B_ABST
    Figure CN116322032B_ABST
Patent Text Reader

Abstract

The present invention discloses a three-dimensional 1S1C memory based on an annular capacitor and a preparation method thereof, wherein the memory comprises: a horizontal peripheral electrode layer, a vertical functional layer and a capacitor dielectric layer: the peripheral electrode layer comprises a first dielectric layer and a first metal electrode layer alternately stacked and grown on a substrate, a plurality of grooves penetrating in a vertical direction are arranged in the peripheral electrode layer, a plurality of holes penetrating in a vertical direction are arranged, an annular groove is arranged outside each hole, the annular groove surrounds the hole and vertically cuts off the peripheral electrode layer, the annular groove is uniformly filled with a capacitor dielectric layer, the top of the second metal electrode layer extends to the surface of the topmost first dielectric layer to form a bit line electrode and is connected to the bit line, and the area directly facing the second metal electrode layer and the first metal electrode layer constitutes a storage unit. The present invention reduces the number of etching times when preparing the capacitor, and only requires one etching and one deposition of the capacitor dielectric layer to complete the preparation of all capacitor units, thereby improving the yield of capacitor preparation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of memory technology, and more specifically, relates to a three-dimensional 1S1C memory based on a ring capacitor and a preparation method thereof. Background Art

[0002] The difficulty in achieving three-dimensional stacking of DRAM to improve storage density is one of the bottlenecks of modern computer performance. Currently, there is a related technology that uses two-terminal selection devices to replace MOS control to charge and discharge capacitors, thereby realizing data storage functions (1S1C memory) without significantly reducing the memory operating speed, and has the potential for three-dimensional stacking.

[0003] There are two main 1S1C memory three-dimensional stacking schemes proposed in the relevant technology: (1) forming a crossbar structure, setting a memory cell at the intersection of the word line and the bit line. This three-dimensional integration method requires the production of a gate tube unit and a capacitor unit when preparing each layer of memory cells. The process steps are very complicated and require high lithography accuracy. When preparing multi-layer memory cells, the process flow is too long. (2) using a structure similar to the floating gate 3D-NAND. This structure is easier to achieve multi-layer memory stacking and only requires the deposition of the gate tube film once. However, the preparation process of its capacitor is more complicated. In order to prepare multiple independent horizontal capacitors in the deep hole, it is necessary to go through multiple etching processes, resulting in a reduced yield, which has become one of the bottlenecks restricting this technical route. Summary of the invention

[0004] In view of the defects of the prior art, the purpose of the present invention is to propose a three-dimensional 1S1C memory based on a ring capacitor and a preparation method, aiming to solve the problem of complex preparation process of 3D-1S1C memory capacitor with a 3D-NAND-like structure.

[0005] The present invention provides a three-dimensional 1S1C memory based on a ring capacitor, comprising: a horizontal peripheral electrode layer, a vertical functional layer and a capacitor dielectric layer: the peripheral electrode layer comprises a first dielectric layer and a first metal electrode layer alternately stacked and grown on a substrate, the top layer being the first dielectric layer; the peripheral electrode layer is provided with a plurality of grooves penetrating in a vertical direction, the grooves are parallel to each other, and the bottom of the grooves is located in the substrate, the first metal electrode layer in each layer is divided into a plurality of independent strip electrodes by the grooves, and the strip electrodes are word lines of the memory; the peripheral electrode layer is provided with a plurality of holes penetrating in a vertical direction, the holes are arranged in an array according to a certain rule, and the bottom of the holes at least extends to the first electrode layer of the bottom layer; The dielectric layer; the inner wall of the hole is evenly covered with a gate tube functional layer, a second metal electrode layer is formed on the surface of the gate tube functional layer, the thickness of the second metal electrode layer and the bottom of the gate tube functional layer in the vertical direction is lower than the first metal electrode layer at the bottom layer, an annular groove is arranged outside each hole, the hole is located at the center of the annular groove, the annular groove surrounds the hole and vertically cuts off the peripheral electrode layer, the bottom of the annular groove extends to at least the first dielectric layer at the bottom layer, the annular groove is evenly filled with the capacitor dielectric layer, the top of the second metal electrode layer extends to the surface of the first dielectric layer at the top layer to form a bit line electrode and is connected to the bit line, and the area directly facing the second metal electrode layer and the first metal electrode layer constitutes a storage unit.

[0006] Furthermore, the first dielectric layers and the first metal electrode layers alternately stacked with each other are periodically repeated in the vertical direction as needed, and the number of repetitions is the same as the number of memory cell layers required by the three-dimensional 1S1C memory.

[0007] Furthermore, all memory cells in the same vertical direction share the same bit line electrode, and all memory cells in the same strip electrode share the same word line electrode.

[0008] Furthermore, the thickness of the first metal electrode layer and the size of the hole satisfy the following relationship: h*w<1um 2 , where h is the thickness of the first metal electrode layer and w is the circumference of the hole.

[0009] Furthermore, the holes are arranged in a rectangular arrangement or a parallelogram arrangement.

[0010] Furthermore, the area where the gate tube functional layer contacts the first metal electrode layer constitutes a gate tube unit, wherein the second metal electrode layer is the upper electrode of the gate tube unit, and the area where the first metal electrode layer contacts the gate tube functional layer constitutes the lower electrode of the gate tube unit. The first metal electrode layer is vertically cut by the annular groove, leaving two electrodes opposite to each other in the horizontal direction, which form a capacitor with the filled capacitor dielectric layer, and the electrode sandwiched between the hole and the annular groove is the lower electrode of the gate tube unit and the upper electrode of the capacitor, which are used to connect the gate tube unit and the capacitor to form a storage unit.

[0011] Furthermore, the width of the annular groove and the dielectric constant of the capacitor dielectric layer jointly determine the capacitance of the capacitor, and the width of the groove is designed according to the capacitance required by the storage unit.

[0012] The present invention also provides a method for preparing the three-dimensional 1S1C memory, comprising the following steps:

[0013] S1 forming a peripheral electrode layer on the substrate of the memory cell region, including alternately growing a first dielectric layer and a first metal electrode layer, wherein the number of layers of the first metal electrode layer grown is the same as the number of layers of the memory cell required by the three-dimensional 1S1C memory;

[0014] S2 is etching to form a plurality of annular grooves penetrating in the vertical direction, the bottom of the annular grooves at least extending to the bottom first dielectric layer, and the annular grooves are filled with the capacitor dielectric layer, and the annular grooves are arranged in an array according to a certain rule;

[0015] S3. Etching a hole in the area surrounded by each annular groove to form a hole penetrating in the vertical direction, wherein the hole is located at the center of the annular groove, and the bottom of the hole extends to at least the bottom first dielectric layer;

[0016] S4: forming a gate tube layer and a second metal electrode layer on the sidewall and bottom of the hole in sequence, wherein the second metal electrode layer extends to the surface of the topmost first dielectric layer to form a bit line electrode and is connected to the bit line;

[0017] S5 is etching to form a plurality of grooves penetrating in a vertical direction, wherein the grooves are parallel to each other and the bottom of the grooves is located in the substrate, and the grooves divide the peripheral electrode layer into a plurality of independent strip-shaped parts.

[0018] Furthermore, the material of the capacitor dielectric layer includes SiO2 or high-k material.

[0019] Furthermore, the high-k material includes nitride, metal oxide, oxynitride or perovskite phase oxide; the nitride is SiN, AlN, TiN; the metal oxide is oxide of subgroup and lanthanide metal elements, such as MgO, Al2O3, Ta2O5, TiO2, ZnO, ZrO2, HfO2, CeO2, Y2O3, La2O3; the oxynitride is SiON or HfSiON; the perovskite phase oxide is PbZrxTi1-xO3 (PZT) or BaxSr1-xTiO3 (BST).

[0020] Compared with the prior art, the above technical solutions conceived by the present invention have the following beneficial effects:

[0021] (1) In the present invention, the gate layer and the capacitor are separated for preparation, and a ring capacitor is introduced, which is sleeved outside the hole-shaped groove of the gate layer to form a 1S1C memory, wherein the capacitor preparation process only requires one longitudinal etching of the ring groove, which can be completed by conventional physical etching means, reducing the number of etching times, and the etching process is also relatively simple. Since the number of etching times when preparing the capacitor is reduced, only one etching and one deposition of the capacitor dielectric layer are required to complete the preparation of all capacitor units, thereby improving the yield of capacitor preparation.

[0022] (2) The upper and lower plate areas of all capacitor units in the present invention are the surface areas of the annular groove in contact with the word line electrode layer, and the thickness of the capacitor dielectric layer is the width of the annular groove, so the prepared capacitors have good consistency. Since the capacitance of the capacitor is mainly determined by the area of ​​the facing plates, the distance between the plates and the dielectric layer; the structure proposed by the present invention makes the area of ​​the facing plates and the distance between the plates of all capacitor units equal, so the memory finally prepared has good consistency.

[0023] (3) When the three-dimensional 1S1C memory needs to prepare capacitor units with different capacitance values ​​(when the capacitance value of the capacitor unit needs to be changed), the distance between the electrodes can be changed by adjusting the width of the annular groove, thereby achieving the purpose of regulating the capacitance value; therefore, capacitors with different capacitance values ​​can be prepared simply by changing the width of the annular groove. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 1 is a schematic diagram of the structure of a three-dimensional 1S1C memory based on a ring capacitor provided in an embodiment of the present invention;

[0025] Figure 2 It is a process flow chart of a method for preparing a three-dimensional 1S1C memory based on a ring capacitor provided by an embodiment of the present invention;

[0026] Figure 3It is a flow chart of the implementation of the method for preparing a three-dimensional 1S1C memory based on a ring capacitor provided in an embodiment of the present invention.

[0027] Among them, 1 is the first metal electrode layer, 2 is the first dielectric layer, 3 is the annular groove filled with the capacitor dielectric layer, 4 is the gate tube functional layer, and 5 is the second metal electrode layer. DETAILED DESCRIPTION

[0028] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.

[0029] In the 3D-1S1C memory structure similar to the 3D-NAND structure, the storage cells are all arranged in the horizontal direction, that is, the layers of thin films that make up a single storage cell are vertical in shape and contact each other in the horizontal direction. In order to separate the capacitors between the various storage cells, the horizontal electrode layer needs to be etched inward laterally and the capacitor is formed in the annular groove formed by the lateral etching. The preparation process is extremely complicated and the yield is reduced. The present invention innovatively prepares the capacitor and the selection layer independently, and the capacitor is formed in one step. The preparation process is simple, the process tolerance is high, and the yield is greatly improved.

[0030] The present invention provides a three-dimensional 1S1C memory based on vertical electrodes, the three-dimensional 1S1C memory comprising: a horizontal peripheral electrode layer, a vertical functional layer and a capacitor dielectric layer:

[0031] The peripheral electrode layer includes a bottom silicon dioxide substrate, a metal electrode layer and a silicon dioxide insulating layer stacked alternately from bottom to top, and a top silicon dioxide top layer;

[0032] The functional layers are, from inside to outside, a bit line electrode layer and a gate material functional layer;

[0033] The capacitor dielectric layer surrounds the vertical functional layer and cuts off the peripheral electrode layer, and the metal electrode between the vertical functional layer and the capacitor dielectric layer is the top electrode of the storage unit capacitor;

[0034] The vertical functional layer and the capacitor dielectric layer in the functional layer are perpendicular to the peripheral electrode layer and extend to the surface of the three-dimensional 1S1C memory structure.

[0035] The alternately stacked bottom-up metal electrodes and silicon dioxide insulating layers are repeated periodically in the vertical direction as needed, and the number of repetitions is the same as the number of storage unit layers required by the three-dimensional 1S1C memory. The periodic repetition is determined by the structure and function. To realize multi-layer storage, this structure requires repeated metal electrodes and silicon dioxide insulating layers; the number of times the layer needs to be repeated is the number of times the number of memory layers required.

[0036] Among them, all memory cells in the same vertical direction share the same bit line electrode, and all memory cells in the same horizontal direction in the same layer share the same word line electrode. Different rows in the three-dimensional 1S1C memory are separated, and the bit line electrodes in the same column extend to the surface and are connected together by column bit lines. The word line electrode of each memory cell is arranged in the horizontal direction, and the capacitor layer in each memory cell is an annular area, and the gate tube layer in each memory cell is the functional layer part corresponding to the capacitor layer.

[0037] The present invention also provides a method for preparing the three-dimensional 1S1C memory, comprising the following steps:

[0038] (1) Using magnetron sputtering to alternately grow metal electrode materials and SiO2 insulating layers on a silicon substrate until the required number of layers is reached;

[0039] (2) etching to form a plurality of annular through holes until the bottom metal electrode is completely etched and a capacitor dielectric layer is grown in the through holes;

[0040] In an embodiment of the present invention, a capacitor is prepared by etching an annular groove and filling a dielectric layer in the groove, which improves the capacitor preparation process and makes the capacitor preparation process simpler. In addition, since the plate spacing of each capacitor unit prepared by etching is relatively consistent, the capacitance uniformity of each capacitor unit is better guaranteed.

[0041] (3) etching a through hole of the vertical functional layer at the center of the annular area until the bottom metal electrode is completely etched, and a gate material functional layer and a bit line electrode layer are sequentially grown in the through hole;

[0042] In the embodiment of the present invention, a vertical functional layer through hole is overetched at the center of the annular region so that the gate tube unit is completely wrapped by the annular capacitor unit to form a 1S1C storage unit.

[0043] (4) growing column bit line electrodes;

[0044] (5) Etch out steps to expose all word line electrodes.

[0045] The columnar pore structure is a square pore structure or a circular pore structure. The sidewalls formed by the circular pores or the square pore structure are relatively smooth, and it is easy for a thin film to be deposited on the sidewalls.

[0046] Further preferably, the capacitor dielectric layer is a circular ring or a square ring.

[0047] When magnetron sputtering is used to deposit the gate layer and the bit line electrode layer, in order to prevent the photoresist from being damaged by excessive energy, it is necessary to start and stop for a period of time. Sputtering for too long will cause the photoresist to denature and cannot be stripped off, resulting in sample preparation failure.

[0048] In order to further illustrate the three-dimensional 1S1C memory based on the ring capacitor and the preparation method provided by the embodiment of the present invention, the following is described in detail with reference to the accompanying drawings and in combination with specific examples:

[0049] Figure 1 A three-dimensional 1S1C memory structure diagram based on an annular capacitor provided in an embodiment of the present invention, the bottom layer is a silicon dioxide layer, on the silicon dioxide bottom layer are metal word line electrode layers and silicon dioxide insulating layers grown alternately, and the three-dimensional 1S1C memory needs as many layers of storage cells as it needs, and it needs to be grown repeatedly as many times. There are multiple storage cells in each word line electrode layer, and these storage cells are composed of storage capacitors and gate tube functional layers, wherein the storage capacitor is composed of a word line metal electrode as a capacitor bottom electrode, a dielectric layer filled in an annular groove as a capacitor dielectric layer, and a word line metal electrode inside the annular groove as a metal top electrode; wherein the gate tube functional layer is composed of a gate tube functional layer material and a bit line electrode layer material in a vertical through hole. Storage cells of different layers are separated by a horizontal silicon dioxide insulating layer. The bit line electrode extends to the surface of the device, and the bit lines of storage cells in the same column are connected together by column bit lines.

[0050] like Figure 2 and Figure 3 As shown, a method for preparing a three-dimensional 1S1C memory based on a ring capacitor provided by an embodiment of the present invention specifically includes the following steps:

[0051] like Figure 2As shown in (a), a metal electrode material is first grown on a substrate, and then an insulating layer is grown on the prepared metal electrode, and then the alternating growth of the metal electrode material and the insulating layer is repeated until the desired number of layers is grown. The deposition process includes, for example, LPCVD, PECVD, HDPCVD, UHVCVD, MOCVD, MBE, ALD, evaporation, sputtering, etc. In order to be compatible with the existing IC manufacturing process, the substrate is preferably a substrate containing silicon, such as Si, SiO2, etc. The material of the insulating layer stacking structure includes at least one of the following insulating media, such as silicon oxide, silicon nitride, silicon oxynitride, amorphous carbon, diamond-like amorphous carbon (DLC), germanium oxide, aluminum oxide, etc. and combinations thereof. In order to be compatible with the existing IC manufacturing process, SiO2 is preferably selected as the medium of the insulating layer.

[0052] Then, a ring-shaped hole structure is etched on the prepared wafer by ultraviolet light to etch a through hole. Etching requires the selection of an anisotropic etching process, such as plasma dry etching or RIE using a carbon fluoride-based (CxHyFz constitutes a fluorinated hydrocarbon) etching gas, to vertically etch the alternating insulating layers and metal layers downward until the bottom insulating dielectric layer is reached. Figure 2 As shown in (b), the next step is to grow a dielectric layer material on the prepared wafer as the dielectric layer of the capacitor. Since the through hole is deep, LPCVD, PECVD, HDPCVD, UHVCVD, MOCVD and other processes can be used for deposition. Metal oxides, oxynitrides, perovskite oxides and the like can be used as dielectric layer materials, and SiO2 can be selected as the dielectric of the insulating layer in order to be compatible with the existing IC manufacturing process. After the deposition is completed, the photoresist is stripped off.

[0053] like Figure 2 As shown in (c), a columnar hole structure is then etched out in the center of the ring structure of the prepared wafer using a purple coat, and a through hole is etched. When etching, an anisotropic etching process is also selected and the etching is performed to the bottom insulating dielectric layer, and then the photoresist is stripped off. A purple coat is then etched on the columnar hole structure, and only the photoresist is developed, and the photoresist is not stripped off for the time being. Figure 2 As shown in (d), a gate material layer and a bit line electrode layer are sequentially deposited in the through hole. The functional layer is grown by magnetron sputtering, and the functional layer needs to use a material with gate performance, such as OTS, CBTS, MIT gate material, etc. Figure 2 As shown in (e), the bit line electrode is also deposited in the through hole by magnetron sputtering, and the prepared electrode needs to be extended to the device surface.

[0054] After the functional layer is prepared, the spin-coated photoresist is stripped off; then, ultraviolet lithography is performed to carve out the bit line electrode structure of the same column, only the photoresist is developed, and the bit line electrode metal layer is deposited by magnetron sputtering, and then the spin-coated photoresist is stripped off; and the structure is prepared as follows Figure 1 The column bit line electrodes in.

[0055] Finally, ultraviolet lithography is performed to etch grooves to expose the top word line electrode metal; then this step is repeated, and the number of repetitions is the same as the number of repetitions of the word line electrode layer and SiO2, each etching depth is deeper than the previous time, and the groove position is closer to the edge of the upper electrode than the previous time, and all the bottom electrode metals are exposed in turn; the preparation is as follows Figure 1 The stepped word line electrode in the embodiment.

[0056] In the prior art of the three-dimensional 1S1C memory preparation process, each time a layer of storage cells is prepared, a hole structure needs to be overlaid and etched out and a functional layer (storage capacitor unit and gate tube unit) needs to be filled in the hole structure. In the 1S1C memory preparation method provided by the present invention, it is only necessary to deposit all the word line electrode layers and isolation layers, then photolithograph and etch a ring structure once and fill the capacitor dielectric layer in the ring structure, then overlay and etch a vertical functional layer through hole in the center of the ring structure, and fill the gate tube functional layer material and the bit line electrode layer material in the through hole, which greatly simplifies the complexity of the preparation process and improves the yield of the three-dimensional 1S1C memory preparation.

[0057] After the above steps, the three-layer three-dimensional 1S1C memory based on vertical electrodes can be prepared, which has the potential to achieve higher storage density and avoids the problems of inaccurate precision and high cost caused by multiple overlays.

[0058] The three-dimensional 1S1C memory structure obtained by the above-mentioned preparation method only needs to deposit the storage capacitor unit and the gate tube material once, which reduces the process complexity of the three-dimensional 1S1C memory. At the same time, the number of storage unit layers of the three-dimensional 1S1C memory can be increased by simply increasing the number of word line electrode layers and isolation layers.

[0059] It will be easily understood by those skilled in the art that the above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A three-dimensional 1S1C memory based on a ring capacitor, characterized in that: include: Horizontal peripheral electrode layer, vertical functional layer and capacitor dielectric layer: The peripheral electrode layer includes a first dielectric layer and a first metal electrode layer alternately stacked and grown on the substrate, and the topmost layer is the first dielectric layer; The peripheral electrode layer is provided with a plurality of grooves penetrating in a vertical direction, each groove is parallel to each other, and the bottom of the groove is located in the substrate, and the first metal electrode layer in each layer is divided into a plurality of independent strip electrodes by the grooves, and the strip electrodes are word lines of the memory; The peripheral electrode layer is provided with a plurality of holes penetrating in the vertical direction, the holes are arranged in an array according to a certain rule, and the bottom of the holes at least extends to the bottom first dielectric layer; The inner wall of the hole is evenly covered with a gate tube functional layer, a second metal electrode layer is formed on the surface of the gate tube functional layer, the thickness of the second metal electrode layer and the bottom of the gate tube functional layer in the vertical direction is lower than that of the bottom first metal electrode layer, an annular groove is arranged outside each hole, the hole is located at the center of the annular groove, the annular groove surrounds the hole and vertically cuts off the peripheral electrode layer, the bottom of the annular groove extends to at least the bottom first dielectric layer, the annular groove is evenly filled with the capacitor dielectric layer, the top of the second metal electrode layer extends to the surface of the top first dielectric layer to form a bit line electrode and is connected to the bit line, and the area directly facing the second metal electrode layer and the first metal electrode layer constitutes a storage unit.

2. The three-dimensional 1S1C memory according to claim 1, characterized in that: The first dielectric layers and the first metal electrode layers alternately stacked with each other are periodically repeated in the vertical direction as required, and the number of repetitions is the same as the number of memory cell layers required by the three-dimensional 1S1C memory.

3. The three-dimensional 1S1C memory according to claim 1, characterized in that: All memory cells in the same vertical direction share the same bit line electrode, and all memory cells in the same strip electrode share the same word line electrode.

4. The three-dimensional 1S1C memory according to claim 1, characterized in that: The thickness of the first metal electrode layer and the size of the hole satisfy the following relationship: h*w<1um 2 , where h is the thickness of the first metal electrode layer and w is the circumference of the hole.

5. The three-dimensional 1S1C memory according to claim 1, characterized in that: The holes are arranged in a rectangular or parallelogram arrangement.

6. The three-dimensional 1S1C memory according to claim 1, characterized in that: The area where the gate tube functional layer contacts the first metal electrode layer constitutes a gate tube unit, wherein the second metal electrode layer is the upper electrode of the gate tube unit, and the area where the first metal electrode layer contacts the gate tube functional layer constitutes the lower electrode of the gate tube unit. The first metal electrode layer is vertically cut by the annular groove, leaving two electrodes opposite to each other in the horizontal direction, which form a capacitor with the filled capacitor dielectric layer, and the electrode sandwiched between the hole and the annular groove is the lower electrode of the gate tube unit and the upper electrode of the capacitor, which are used to connect the gate tube unit and the capacitor to form a storage unit.

7. The three-dimensional 1S1C memory according to claim 1, characterized in that: The width of the annular groove and the dielectric constant of the capacitor dielectric layer jointly determine the capacitance of the capacitor, and the width of the groove is designed according to the capacitance required by the storage unit.

8. A method for preparing a three-dimensional 1S1C memory according to any one of claims 1 to 7, characterized in that: The following steps are involved: S1 forming a peripheral electrode layer on the substrate of the memory cell region, including alternately growing a first dielectric layer and a first metal electrode layer, wherein the number of layers of the first metal electrode layer grown is the same as the number of layers of the memory cell required by the three-dimensional 1S1C memory; S2 is etching to form a plurality of annular grooves penetrating in the vertical direction, the bottom of the annular grooves at least extending to the bottom first dielectric layer, and the annular grooves are filled with the capacitor dielectric layer, and the annular grooves are arranged in an array according to a certain rule; S3. Etching a hole in the area surrounded by each annular groove to form a hole penetrating in the vertical direction, wherein the hole is located at the center of the annular groove, and the bottom of the hole extends to at least the bottom first dielectric layer; S4: forming a gate tube layer and a second metal electrode layer on the sidewall and bottom of the hole in sequence, wherein the second metal electrode layer extends to the surface of the topmost first dielectric layer to form a bit line electrode and is connected to the bit line; S5 is etching to form a plurality of grooves penetrating in a vertical direction, wherein the grooves are parallel to each other and the bottom of the grooves is located in the substrate, and the grooves divide the peripheral electrode layer into a plurality of independent strip-shaped parts.

9. The preparation method according to claim 8, characterized in that: The material of the capacitor dielectric layer includes SiO2 or high-k material.

10. The preparation method according to claim 9, characterized in that: The high-k material includes nitride, metal oxide, oxynitride or perovskite phase oxide; The nitride is SiN, AlN, or TiN; The metal oxide is a subgroup and lanthanide metal element oxide; The oxynitride is SiON or HfSiON; The perovskite phase oxide is PbZrxTi1-xO3 (PZT) or BaxSr1-xTiO3 (BST).

11. The preparation method according to claim 10, characterized in that: The metal oxides are MgO, Al2O3, Ta2O5, TiO2, ZnO, ZrO2, HfO2, CeO2, Y2O3 and La2O3.