A system and method for post-treatment of phosphoric acid extraction
By designing a post-treatment system for solvent-free extraction of phosphoric acid, including mixing, reaction, crystallization and concentration sections, the problems of high impurity content and low phosphoric acid concentration in phosphoric acid purification in the existing technology have been solved, and high-quality concentrated purified phosphoric acid production has been achieved, replacing The high energy consumption and high pollution thermal phosphoric acid is eliminated to achieve the purpose of energy saving and consumption reduction.
Patent Information
- Application Number
- CN202310344320.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-03
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2043-04-03
AI Technical Summary
The existing phosphoric acid purification treatment lacks an effective solvent-free extraction phosphoric acid post-treatment system, resulting in high impurity content and low phosphoric acid concentration, making it difficult to produce high-quality phosphates. In addition, thermal phosphoric acid consumes high energy and is highly polluting.
A system including a storage tank for solvent-free extracted phosphoric acid, a reaction tank, a crystallization tank, a filter and a purified phosphoric acid concentration device was designed. Through the mixing, reaction, crystallization, filtration and concentration sections, the impurities in the solvent-free extracted phosphoric acid were removed and improved. Phosphoric acid concentration.
It has realized the production of high-quality concentrated and purified phosphoric acid, with a concentration of 74.57% and an impurity content lower than the standard for high-quality industrial phosphoric acid. It can be processed into food-grade, pharmaceutical-grade and electronic-grade phosphoric acid, replacing high-energy-consuming and highly-polluting thermal phosphoric acid and saving energy. Reduce consumption.
Smart Images

Figure CN116477587B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of chemical industry, and in particular to a system and method for post-processing of extracted phosphoric acid, and in particular to a new process for further removing residual impurities in the solvent-free extracted phosphoric acid after extraction and solvent recovery by using some chemical substances, and then concentrating the solvent-free extracted phosphoric acid to obtain a pure target product, namely, concentrated purified phosphoric acid. Background Art
[0002] Phosphoric acid is an important intermediate chemical product. Its uses can be summarized into two aspects, namely fertilizer production and industrial phosphate production. Wet-process phosphoric acid produced by acid decomposition of phosphate rock is mainly used in fertilizer production due to its high impurity content. In addition to fertilizers, other industrial fields, wet-process phosphoric acid is difficult to be widely used. Thermal phosphoric acid is usually used in these occasions. Compared with wet-process phosphoric acid, thermal phosphoric acid is a high-energy consumption and high-pollution product. If wet-process phosphoric acid is used to produce high-quality phosphates to meet the requirements of food-grade, pharmaceutical-grade and electronic-grade products, the wet-process phosphoric acid must be purified to produce high-purity phosphoric acid.
[0003] The wet phosphoric acid purification production method is mainly divided into four parts: removal of organic impurities and concentration, extraction of phosphoric acid, recovery of extracted phosphoric acid solvent, and post-processing. Post-processing and concentration mainly include solvent-free extraction of phosphoric acid mixing and adding, mixed extraction of phosphoric acid reaction and crystallization, post-processing extraction of phosphoric acid filtration, and dilute purification of phosphoric acid concentration.
[0004] In the past, phosphoric acid purification did not include post-treatment and concentration. The impurity content of the purified phosphoric acid was high and the phosphoric acid concentration was low, which was not conducive to industrial use and difficult to produce high-quality phosphate. Therefore, it is urgent to provide a system and method for post-treatment of solvent-free phosphoric acid extraction with a simple process, low manufacturing cost, large production capacity and good treatment effect. Summary of the invention
[0005] The object of the present invention is to provide a system and method for post-processing of solvent-free extracted phosphoric acid, which system comprises a solvent-free extracted phosphoric acid storage tank, a No. 1 reaction tank, a No. 2 reaction tank, a crystallization tank, a filter, a purified phosphoric acid heat exchanger, a purified phosphoric acid concentration device, etc. The solvent-free extracted phosphoric acid from the phosphoric acid extraction solvent recovery system and the mixed solution from the mixing feed tank are mixed and reacted in the No. 1 reaction tank and the No. 2 reaction tank, and after the reaction, the solution is sent to the crystallization tank for crystallization and precipitation, and after the crystallization and precipitation, the solution is filtered, and the filtered solid material is sent to a phosphate fertilizer device to produce phosphate fertilizer, and the filtered filtrate is dilute purified phosphoric acid, and the dilute purified phosphoric acid is sent to a purified phosphoric acid concentration device to be concentrated into a target product, i.e., concentrated purified phosphoric acid.
[0006] By using the above system and method, the target product, concentrated purified phosphoric acid, which is free of solvents, has few impurities and good quality, is obtained to replace the high-energy consumption and high-pollution thermal phosphoric acid. The concentrated purified phosphoric acid is of better quality than industrial-grade phosphoric acid and can be further processed into food-grade, pharmaceutical-grade and electronic-grade phosphoric acid. This patent aims to save energy and reduce consumption, reduce carbon emissions of production equipment and reduce operation and maintenance costs.
[0007] The purpose of the present invention can be achieved through the following technical solutions:
[0008] A system for post-treatment of extracted phosphoric acid, the system comprising a solvent-free extracted phosphoric acid storage tank, a No. 1 reaction tank, a No. 2 reaction tank, a crystallization tank, a filter, a purified phosphoric acid heat exchanger and a purified phosphoric acid concentration device;
[0009] The solvent-free extracted phosphoric acid pipeline from the extracted phosphoric acid solvent recovery system is connected to the solvent-free extracted phosphoric acid storage tank, the outlet of the solvent-free extracted phosphoric acid storage tank is connected to the inlet of 1# reaction tank A, the bottom outlet of 1# reaction tank is connected to the inlet of the crystallization tank through the 2# reaction tank, the bottom outlet of the crystallization tank is connected to the feed end of the filter, and the liquid output end of the filter is connected to the inlet of the dilute purified phosphoric acid storage tank through a pipeline.
[0010] In the technical solution of the present invention: the ferrosilicon powder pipeline from the boundary zone is connected to the A inlet at the top of the mixing feeding tank, the calcium oxide chute from the boundary zone is connected to the B inlet at the top of the mixing feeding tank, the sodium sulfide chute from the boundary zone is connected to the C inlet at the top of the mixing feeding tank, the make-up water pipeline from the boundary zone is connected to the D inlet at the top of the mixing feeding tank, and the lower outlet of the mixing feeding tank is connected to the B inlet at the top of the 1# reaction tank through a pipeline.
[0011] In the technical solution of the present invention: the solid output end of the filter is connected to the feeding end of the solid material conveyor, and the discharge end of the solid material conveyor is provided with a boundary area phosphate fertilizer device.
[0012] In the technical scheme of the present invention, the bottom outlet of the dilute purified phosphoric acid storage tank is connected to the shell side inlet of the purified phosphoric acid heat exchanger through a dilute purified phosphoric acid pump, the shell side outlet of the purified phosphoric acid heat exchanger is connected to the inlet of the purified phosphoric acid concentration device through a pipeline, the outlet of the purified phosphoric acid concentration device is connected to the tube side inlet of the purified phosphoric acid heat exchanger through a pipeline, the tube side outlet of the purified phosphoric acid heat exchanger is connected to the top inlet of the concentrated purified phosphoric acid storage tank through a pipeline, and the lower outlet of the concentrated purified phosphoric acid storage tank is connected to the concentrated purified phosphoric acid pipeline, which is the target product of the delimited area, through a concentrated purified phosphoric acid pump.
[0013] In the technical solution of the present invention: the mixing feeding tank is provided with a mixing feeding tank stirrer, the No. 1 reaction tank is provided with a No. 1 reaction tank stirrer, the No. 2 reaction tank is provided with a No. 2 reaction tank stirrer, and the crystallization tank is provided with a crystallization tank rake.
[0014] A production method for post-treatment of phosphoric acid extraction using the above system comprises the following steps:
[0015] (1) Mixing and feeding section: the ferrosilicon powder from the boundary zone, the calcium oxide from the boundary zone, the sodium sulfide from the boundary zone and the supplementary water from the boundary zone enter the mixing feeding tank from the top of the mixing feeding tank, and the several substances are fully mixed into a uniform mixed liquid in the mixing feeding tank. The mixed liquid enters the No. 1 reaction tank through a pipeline from the lower outlet of the mixing feeding tank, and the solvent-free extracted phosphoric acid from the extraction phosphoric acid solvent recovery system enters the No. 1 reaction tank through the solvent-free extracted phosphoric acid storage tank. The mass ratio between the mixed liquid and the solvent-free extracted phosphoric acid is 1:600-700;
[0016] (2) Reaction and crystallization section: The mixed liquid from the lower outlet of the mixing and feeding tank and the solvent-free extracted phosphoric acid from the solvent-free extracted phosphoric acid storage tank are mixed and reacted in the No. 1 reaction tank at a reaction temperature of 62 to 67° C. and a residence time of ≥ 1 hour;
[0017] The mixed extracted phosphoric acid after the reaction enters the 2# reaction tank for mixing and reaction, the reaction temperature is 57-62°C, the residence time is ≥1 hour, and the mixed solution after the reaction enters the crystallization tank;
[0018] The mixed extracted phosphoric acid is crystallized and precipitated in a crystallization tank at a crystallization temperature of 53-57°C and a residence time of ≥1 hour;
[0019] (3) Filtration section: The post-processed extracted phosphoric acid from the crystallization tank is filtered at the feed end of the filter, and the filtered diluted purified phosphoric acid enters the diluted purified phosphoric acid storage tank; the filtered solid material enters the solid material conveyor, and the solid material is sent to the boundary area phosphate fertilizer device through the solid material conveyor;
[0020] (4) Concentration section: The dilute purified phosphoric acid from the dilute purified phosphoric acid storage tank is sent to the shell side inlet of the purified phosphoric acid heat exchanger, and heat exchange is carried out in the shell side of the purified phosphoric acid heat exchanger. After the heat exchange, the dilute purified phosphoric acid is sent from the shell side outlet of the purified phosphoric acid heat exchanger to the inlet of the purified phosphoric acid concentration device. In the purified phosphoric acid concentration device, the dilute purified phosphoric acid is concentrated into the target product, i.e., concentrated purified phosphoric acid. After concentration, the target product is sent from the outlet of the purified phosphoric acid concentration device to the tube side inlet of the purified phosphoric acid heat exchanger, and heat exchange is carried out in the tube side of the purified phosphoric acid heat exchanger. After the heat exchange, the concentrated purified phosphoric acid storage tank is sent. Beneficial effects of the present invention:
[0021] The present invention provides a system and method for post-treatment of solvent-free phosphoric acid extraction. The system and method can further remove impurities in the solvent-free phosphoric acid extracted from which the solvent has been removed, and the concentration of phosphoric acid can be further improved. When the concentration of the target product, concentrated purified phosphoric acid (H3PO4), reaches 74.57%, and the concentration of phosphorus pentoxide (P2O5) reaches 54.03%, the aluminum (Al) content in the acid is reduced by 15%, the iron (Fe) content is reduced by 71%, the magnesium (Mg) content is reduced by 49%, and the sulfate (SO4 2-) content is reduced by 75%, fluorine (F) content is reduced by 81%, and the impurity content is lower than the standard of superior industrial phosphoric acid. It can be processed into food grade, pharmaceutical grade and electronic grade purified phosphoric acid. The target product obtained after post-treatment of solvent-free extraction phosphoric acid - concentrated purified phosphoric acid can replace high-energy consumption and high-pollution thermal phosphoric acid. This patent aims to save energy and reduce consumption, reduce carbon emissions of production equipment and reduce operation and maintenance costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 This is the process flow diagram of this patent
[0023] Among them, there are a solvent-free extracted phosphoric acid storage tank 1, a solvent-free extracted phosphoric acid pump 2, a mixing and feeding tank 3, a mixing and feeding tank agitator 4, a No. 1 reaction tank 5, a No. 1 reaction tank agitator 6, a No. 2 reaction tank 7, a No. 2 reaction tank agitator 8, a crystallization tank 9, a crystallization tank rake 10, a post-processing extracted phosphoric acid pump 11, a filter 12, a dilute purified phosphoric acid storage tank 13, a dilute purified phosphoric acid pump 14, a purified phosphoric acid heat exchanger 15, a purified phosphoric acid concentration device 16, a concentrated purified phosphoric acid storage tank 17, a concentrated purified phosphoric acid pump 18, and a solid material conveyor 19. DETAILED DESCRIPTION
[0024] The present invention is further described below in conjunction with embodiments, but the protection scope of the present invention is not limited thereto:
[0025] like Figure 1 A system for post-processing extracted phosphoric acid, the system comprising a solvent-free extracted phosphoric acid storage tank 1, a No. 1 reaction tank 5, a No. 2 reaction tank 7, a crystallization tank 9, a filter 12, a purified phosphoric acid heat exchanger 15, a purified phosphoric acid concentration device 16, etc.; the solvent-free extracted phosphoric acid pipeline from the extracted phosphoric acid solvent recovery system is connected to the top inlet of the solvent-free extracted phosphoric acid storage tank 1, the lower outlet of the solvent-free extracted phosphoric acid storage tank 1 is connected to the top A inlet of the No. 1 reaction tank 5 through a solvent-free extracted phosphoric acid pump 2, the bottom outlet of the No. 1 reaction tank 5 is connected to the top inlet of the crystallization tank 9 through the No. 2 reaction tank 7, the bottom outlet of the crystallization tank 9 is connected to the feed end of the filter 12 through a post-processed extracted phosphoric acid pump 11, and the liquid output end of the filter 12 is connected to the top inlet of a diluted purified phosphoric acid storage tank 13 through a pipeline.
[0026] The ferrosilicon powder chute from the boundary zone is connected to the A inlet at the top of the mixing feeding tank 3, the calcium oxide chute from the boundary zone is connected to the B inlet at the top of the mixing feeding tank 3, the sodium sulfide chute from the boundary zone is connected to the C inlet at the top of the mixing feeding tank 3, the make-up water pipeline from the boundary zone is connected to the D inlet at the top of the mixing feeding tank 3, and the lower outlet of the mixing feeding tank 3 is connected to the B inlet at the top of the 1# reaction tank 5 through a pipeline.
[0027] The solid output end of the filter 12 is connected to the feed end of the solid material conveyor 19, and the discharge end of the solid material conveyor 19 is connected to the boundary area phosphate fertilizer device.
[0028] The bottom outlet of the dilute purified phosphoric acid storage tank 13 is connected to the shell side inlet of the purified phosphoric acid heat exchanger 15 through the dilute purified phosphoric acid pump 14, the shell side outlet of the purified phosphoric acid heat exchanger 15 is connected to the inlet of the purified phosphoric acid concentration device 16 through a pipeline, the outlet of the purified phosphoric acid concentration device 16 is connected to the tube side inlet of the purified phosphoric acid heat exchanger 15 through a pipeline, the tube side outlet of the purified phosphoric acid heat exchanger 15 is connected to the top inlet of the concentrated purified phosphoric acid storage tank 17 through a pipeline, and the lower outlet of the concentrated purified phosphoric acid storage tank 17 is connected to the concentrated purified phosphoric acid pipeline, which is the target product of the delimited area, through the concentrated purified phosphoric acid pump 18.
[0029] The mixing and feeding tank 3 is provided with a mixing and feeding tank agitator 4, the 1# reaction tank 5 is provided with a 1# reaction tank agitator 6, the 2# reaction tank 7 is provided with a 2# reaction tank agitator 8, and the crystallization tank 9 is provided with a crystallization tank rake 10.
[0030] A production method for post-treatment of phosphoric acid extraction using the above system includes the following steps. More than one mixed solution can be used. A mixed solution consisting of ferrosilicon powder, calcium oxide, sodium sulfide, and supplementary water is used as an example:
[0031] (1) Mixing and feeding section: the ferrosilicon powder (Si mass concentration 85%, Fe mass concentration 15%) from the boundary zone enters the mixing feeding tank 3 from the inlet A at the top of the mixing feeding tank 3, the calcium oxide from the boundary zone enters the mixing feeding tank 3 from the inlet B at the top of the mixing feeding tank 3, the sodium sulfide from the boundary zone enters the mixing feeding tank 3 from the inlet C at the top of the mixing feeding tank 3, and the make-up water from the boundary zone enters the mixing feeding tank 3 from the inlet D at the top of the mixing feeding tank 3. In the mixing feeding tank 3, the various substances are fully mixed into a uniform mixed liquid, and the mixed liquid is discharged from the mixing The lower outlet of the feeding tank 3 enters the 1# reaction tank 5 from the B inlet of the 1# reaction tank 5 through a pipeline. The solvent-free extracted phosphoric acid containing a P2O5 mass concentration of 23% from the extraction phosphoric acid solvent recovery system enters the solvent-free extracted phosphoric acid storage tank 1 from the top inlet of the solvent-free extracted phosphoric acid storage tank 1. The solvent-free extracted phosphoric acid has a temperature of 66-67° C. and enters the 1# reaction tank 5 from the A inlet of the 1# reaction tank 5 from the lower outlet of the solvent-free extracted phosphoric acid storage tank 1 through the solvent-free extracted phosphoric acid pump 2. The mass ratio between the mixed solution and the solvent-free extracted phosphoric acid is 1:647.
[0032] (2) Reaction and crystallization section: The mixed solution from the lower outlet of the mixing and feeding tank 3 and the solvent-free extracted phosphoric acid from the solvent-free extracted phosphoric acid storage tank 1 are mixed and reacted in the No. 1 reaction tank 5, the reaction temperature is 62-67° C., and the residence time is controlled to be 1 hour. The mixed extracted phosphoric acid after the reaction is discharged from the bottom outlet of the No. 1 reaction tank 5 and enters the No. 2 reaction tank 7 from the top inlet to mix and react. The reaction temperature is 57-62° C. and the residence time is controlled to be 1 hour. The mixed extracted phosphoric acid after the reaction is discharged from the bottom outlet of the No. 2 reaction tank 7 and enters the crystallization tank 9 from the top inlet to the crystallization tank 9. The mixed extracted phosphoric acid is crystallized and precipitated in the crystallization tank 9 at a crystallization temperature of 53-57° C. and the residence time is controlled to be 1 hour. The post-treated extracted phosphoric acid is discharged from the bottom outlet of the crystallization tank 9 to the post-treated extracted phosphoric acid pump 11.
[0033] (3) Filtration section: The post-processed extracted phosphoric acid from the crystallization tank 9 is filtered through the post-processed extracted phosphoric acid pump 11 to the feed end of the filter 12. The filtered diluted purified phosphoric acid exits the liquid output end of the filter 12 and contains a P2O5 mass concentration of 22-23% and a temperature of 49-50° C., and enters the diluted purified phosphoric acid storage tank 13 from the top inlet of the diluted purified phosphoric acid storage tank 13; the filtered solid material exits the solid output end of the filter 12 and enters the solid material conveyor 19 from the feed end of the solid material conveyor 19, and the solid material is conveyed to the boundary area phosphate fertilizer device through the solid material conveyor 19.
[0034] (4) Concentration section: The dilute purified phosphoric acid from the dilute purified phosphoric acid storage tank 13 is transported from the lower outlet of the storage tank 13 to the shell side inlet of the purified phosphoric acid heat exchanger 15 through the dilute purified phosphoric acid pump 14, and heat exchange is performed in the shell side of the purified phosphoric acid heat exchanger. After the heat exchange, the dilute purified phosphoric acid is transported from the shell side outlet of the purified phosphoric acid heat exchanger 15 to the inlet of the purified phosphoric acid concentrator 16. In the purified phosphoric acid concentrator 16, the dilute purified phosphoric acid is concentrated into a target product, i.e., concentrated purified phosphoric acid, having a P2O5 mass concentration of 54-55% (containing H3PO4 mass concentration of 74-76%). After the concentration, the target product, i.e., concentrated purified phosphoric acid, is transported from the outlet of the purified phosphoric acid concentrator 16 to the tube side inlet of the purified phosphoric acid heat exchanger 15, and heat exchange is performed in the tube side of the purified phosphoric acid heat exchanger 15. After the heat exchange, the target product, i.e., concentrated purified phosphoric acid, having a temperature of 54-55° C., is transported from the tube side outlet of the purified phosphoric acid heat exchanger 15 to the inlet of the concentrated purified phosphoric acid storage tank 17. The concentrated purified phosphoric acid in the concentrated purified phosphoric acid storage tank 17 is transported from the lower outlet of the concentrated purified phosphoric acid storage tank 17 to the boundary area through the concentrated purified phosphoric acid pump 18. The results of the operation of the present invention are shown in Table 1.
[0035] Table 1 Performance evaluation results of 60,000 tons / year solvent-free phosphoric acid post-treatment unit
[0036] Table 1 Performance evaluation results of 60,000 tons / year solvent-free phosphoric acid post-treatment unit
[0037]
[0038]
Claims
1. A production method for post-treatment of phosphoric acid extraction, characterized in that: The method comprises the following steps: (1) Mixing and feeding section: the ferrosilicon powder from the boundary zone, the calcium oxide from the boundary zone, the sodium sulfide from the boundary zone and the supplementary water from the boundary zone enter the mixing feeding tank (3) from the top of the mixing feeding tank (3), the several substances are fully mixed into a uniform mixed liquid in the mixing feeding tank (3), the mixed liquid enters the No. 1 reaction tank (5) through the pipeline from the lower outlet of the mixing feeding tank (3), the solvent-free extracted phosphoric acid from the extraction phosphoric acid solvent recovery system enters the No. 1 reaction tank (5) through the solvent-free extracted phosphoric acid storage tank (1), and the mass ratio between the mixed liquid and the solvent-free extracted phosphoric acid is 1:600-700; (2) Reaction and crystallization section: the mixed liquid from the lower outlet of the mixing and feeding tank (3) and the solvent-free extracted phosphoric acid from the solvent-free extracted phosphoric acid storage tank (1) are mixed and reacted in the No. 1 reaction tank (5), the reaction temperature is 62-67°C, and the residence time is ≥1 hour; The mixed extracted phosphoric acid after the reaction enters the 2# reaction tank (7) for mixing and reaction, the reaction temperature is 57~62°C, the residence time is ≥1 hour, and the mixed solution after the reaction enters the crystallization tank (9); The mixed extracted phosphoric acid is crystallized and precipitated in a crystallization tank (9) at a crystallization temperature of 53-57° C. and a residence time of ≥1 hour; (3) Filtration section: the post-processed extracted phosphoric acid from the crystallization tank (9) is filtered at the feed end of the filter (12), and the filtered diluted purified phosphoric acid enters the diluted purified phosphoric acid storage tank (13); the filtered solid material enters the solid material conveyor (19), and the solid material is conveyed to the boundary area phosphate fertilizer device through the solid material conveyor (19); (4) Concentration section: the dilute purified phosphoric acid from the dilute purified phosphoric acid storage tank (13) is transported to the shell side inlet of the purified phosphoric acid heat exchanger (15), and heat exchange is performed in the shell side of the purified phosphoric acid heat exchanger (15). After the heat exchange, the dilute purified phosphoric acid is transported from the shell side outlet of the purified phosphoric acid heat exchanger (15) to the inlet of the purified phosphoric acid concentration device (16). In the purified phosphoric acid concentration device (16), the dilute purified phosphoric acid is concentrated into a target product, i.e., concentrated purified phosphoric acid. After concentration, the target product is transported from the outlet of the purified phosphoric acid concentration device (16) to the tube side inlet of the purified phosphoric acid heat exchanger (15), and heat exchange is performed in the tube side of the purified phosphoric acid heat exchanger (15). After the heat exchange, the concentrated purified phosphoric acid is transported to the concentrated purified phosphoric acid storage tank (17); The system for implementing the above method comprises a solvent-free extraction phosphoric acid storage tank (1), a No. 1 reaction tank (5), a No. 2 reaction tank (7), a crystallization tank (9), a filter (12), a purified phosphoric acid heat exchanger (15) and a purified phosphoric acid concentration device (16); The solvent-free extracted phosphoric acid pipeline from the extracted phosphoric acid solvent recovery system is connected to the solvent-free extracted phosphoric acid storage tank (1), the outlet of the solvent-free extracted phosphoric acid storage tank (1) is connected to the inlet of the 1# reaction tank (5) A, the bottom outlet of the 1# reaction tank (5) is connected to the inlet of the crystallization tank (9) through the 2# reaction tank (7), the bottom outlet of the crystallization tank (9) is connected to the feed end of the filter (12), and the liquid output end of the filter (12) is connected to the inlet of the diluted purified phosphoric acid storage tank (13) through a pipeline.
2. The method for post-treatment of phosphoric acid extraction according to claim 1, characterized in that: The ferrosilicon powder pipeline from the boundary zone is connected to the A inlet at the top of the mixing and feeding tank (3), the calcium oxide chute from the boundary zone is connected to the B inlet at the top of the mixing and feeding tank (3), the sodium sulfide chute from the boundary zone is connected to the C inlet at the top of the mixing and feeding tank (3), the make-up water pipeline from the boundary zone is connected to the D inlet at the top of the mixing and feeding tank (3), and the lower outlet of the mixing and feeding tank (3) is connected to the B inlet at the top of the 1# reaction tank (5) through a pipeline.
3. The method for post-treatment of phosphoric acid extraction according to claim 1, characterized in that: The solid output end of the filter (12) is connected to the feed end of the solid material conveyor (19), and the discharge end of the solid material conveyor (19) is connected to the boundary area phosphate fertilizer device.
4. The method for post-treatment of phosphoric acid extraction according to claim 1, characterized in that: The bottom outlet of the dilute purified phosphoric acid storage tank (13) is connected to the shell side inlet of the purified phosphoric acid heat exchanger (15) through a dilute purified phosphoric acid pump (14), the shell side outlet of the purified phosphoric acid heat exchanger (15) is connected to the inlet of the purified phosphoric acid concentration device (16) through a pipeline, the outlet of the purified phosphoric acid concentration device (16) is connected to the tube side inlet of the purified phosphoric acid heat exchanger (15) through a pipeline, the tube side outlet of the purified phosphoric acid heat exchanger (15) is connected to the top inlet of the concentrated purified phosphoric acid storage tank (17) through a pipeline, and the lower outlet of the concentrated purified phosphoric acid storage tank (17) is connected to the concentrated purified phosphoric acid pipeline, which is the target product of the delimited area, through a concentrated purified phosphoric acid pump (18).
5. The method for post-treatment of phosphoric acid extraction according to claim 1, characterized in that: The mixing and feeding tank (3) is provided with a mixing and feeding tank agitator (4), the No. 1 reaction tank (5) is provided with a No. 1 reaction tank agitator (6), the No. 2 reaction tank (7) is provided with a No. 2 reaction tank agitator (8), and the crystallization tank (9) is provided with a crystallization tank rake (10).
Citation Information
Patent Citations
Washing method for wet-process phosphoric acid purification
CN109437144A
Wet method phosphoric acid purification method
CN1799996A
Phosphoric acid by wet process purification treatment production system
CN208166579U
Defluorination of wet process phosphoric acid
US4330517A