A method for preparing an environmentally friendly, impurity-free carbon aerogel thermal insulation composite material

Through the combination of raw materials such as phenol organic monomer, aldehyde organic monomer and chitosan, combined with vacuum impregnation, hydrothermal and normal pressure drying processes, a high-strength and low thermal conductivity fiber-reinforced carbon aerogel composite is prepared to solve the problem of The problems of environmental pollution and poor mechanical properties are achieved, and environmentally friendly and low-cost preparation of thermal insulation materials are achieved.

CN116573949BActive Publication Date: 2024-11-22NAT UNIV OF DEFENSE TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310611242.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-05-28
Publication Date
2024-11-22
Estimated Expiration
2043-05-28

AI Technical Summary

Technical Problem

There are hidden dangers of environmental pollution and poor mechanical properties in the preparation of existing carbon aerogel thermal insulation materials, especially the environmental pollution caused by the use of organic solvents and the material brittleness cannot meet the needs of high-strength thermal insulation.

Method used

Using raw materials such as phenol organic monomers, aldehyde organic monomers, chitosan and acetic acid, fiber-reinforced carbon aerogel composite materials are prepared through vacuum impregnation, hydrothermal and atmospheric pressure drying processes, avoiding the use of organic solvents and forming high-quality Insulating material with strength and low thermal conductivity.

Benefits of technology

It has achieved green, environmentally friendly, low-cost, impurity-free carbon aerogel thermal insulation composite material preparation, the material's compressive strength is improved, the thermal conductivity is reduced, and the thermal insulation performance is significantly improved, making it suitable for industrial production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116573949B_ABST
    Figure CN116573949B_ABST
Patent Text Reader

Abstract

The present invention discloses a method for preparing an environmentally friendly, impurity-free carbon aerogel thermal insulation composite material, the purpose of which is to solve the problem that the current method for preparing impurity-free carbon aerogel thermal insulation material will cause environmental pollution and the carbon aerogel is brittle and fragile. The technical scheme is to first use phenol organic monomers, aldehyde organic monomers, chitosan, acetic acid and water to prepare an organic sol; then use a vacuum impregnation process to prepare an organic sol fiber preform composite; then use a hydrothermal process to prepare a fiber-reinforced organic gel composite; use a normal pressure drying process to prepare a fiber-reinforced organic aerogel composite; and finally use a carbonization cracking process to prepare a fiber-reinforced carbon aerogel composite material. The present invention is green and pollution-free, has a simple process, a short cycle, and low cost; the fiber-reinforced carbon aerogel composite material prepared by the present invention has no impurities, high compression strength, and good thermal insulation performance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of carbon aerogel preparation technology, and in particular relates to a method for preparing an environmentally friendly, impurity-free carbon aerogel thermal insulation composite material. Background Art

[0002] The continuous development of new high-speed aerospace vehicles has put forward an urgent demand for high-temperature resistant, lightweight and high-efficiency thermal insulation materials. Carbon aerogel, due to its nanoscale pores and particle chain structure, not only has the excellent properties of traditional aerogels such as low density, high porosity, high specific surface area and low thermal conductivity, but also has the advantages of ultra-high temperature resistance (inert atmosphere) and high infrared specific extinction coefficient, which makes it have significant advantages in being used as a thermal insulation material for thermal protection in ultra-high temperature areas.

[0003] Carbon aerogel is mainly prepared by carbonization of organic aerogel, among which sodium carbonate catalyzed resorcinol-formaldehyde is the most commonly used raw material system. The preparation of carbon aerogel generally includes five steps: sol preparation, gel aging, solvent replacement, supercritical drying and carbonization. However, the alkali metal catalyst used in the sol preparation process will bring metal impurities, thereby accelerating the high-temperature oxidation of carbon aerogel insulation materials; the solvent replacement cycle is relatively long, generally 5 to 7 days, and a large amount of organic waste liquid will be generated; the supercritical drying process has problems such as high cost, limited product size and safety. In addition, carbon aerogel is brittle and fragile, with poor strength and toughness, and it is difficult to directly use it as an insulation material for thermal protection systems. Therefore, how to achieve green, environmentally friendly and low-cost preparation of impurity-free carbon aerogel insulation materials with high mechanical strength remains an important challenge.

[0004] By using an acidic catalyst or an organic alkaline catalyst hexamethylenetetramine, metal impurities can be eliminated; by using atmospheric pressure drying, the production process can be effectively simplified and the cost can be reduced. [Acetic-acid-catalyzed and atmospheric pressure dried carbon aerogels with a nanometer-sized structure and a wide density range, Acetic-acid-catalyzed and subcritically dried carbon aerogels with a nanometer-sized structure and a wide density range. Journal of Non-Crystalline Solids, 2004, 350: 131-135] Organic acetic acid is used to catalyze resorcinol and formaldehyde, and then atmospheric pressure drying is used to prepare impurity-free carbon aerogels. However, this method has a narrow process window, and requires organic solvent replacement, and there is organic waste liquid. [Strong and machinable carbon aerogel monoliths with low thermal conductivity prepared via ambient pressure drying. Carbon, 2016, 108: 551-560] Carbon aerogel is prepared by using thermoplastic phenolic resin as carbon source and hexamethylenetetramine as curing agent. Although this method can avoid metal impurities and realize the preparation of carbon aerogel by atmospheric pressure drying, it requires the use of organic solvents, which will produce organic waste liquid and bring environmental pollution risks. There are similar patents [CN110482525B], [CN1199854C], [CN112341234A], [CN110951103A], which all need to use organic solvents in the preparation process, which will cause environmental pollution problems. Patent [CN1583555A] discloses a method for preparing carbon aerogel, which uses resorcinol and formaldehyde as reaction monomers, organic surfactants (e.g., hexadecyltrimethylammonium bromide, sodium dodecylsulfonate) as emulsifiers and catalysts, water as solvent, and atmospheric pressure drying to prepare carbon aerogel. This method is low in cost, but the organic surfactants used in the preparation process will cause environmental pollution. The mechanical strength of carbon aerogel can be effectively improved by using reinforcing fibers. For this purpose, carbon fiber reinforcement is now widely used at home and abroad.[Determination of the Anisotropic Thermal Conductivity of a Carbon Aerogel-Fiber Composite by a Non-contact Thermographic Technique. International Journal of Thermophysics, 2007, 28: 1542-1562.] Carbon fiber reinforced carbon aerogel composites were prepared by normal pressure drying. The carbon fiber hardly shrinks during the carbonization process, but the aerogel shrinks by 20-30% during the carbonization process. Therefore, the two will produce internal stress during the carbonization process due to inconsistent shrinkage, resulting in cracks in the obtained material, which in turn affects the thermal insulation performance of the material, making its room temperature thermal conductivity as high as 0.34W / m·K. In addition, cracks will also weaken the mechanical strength of the material.

[0005] In summary, the current low-cost preparation of environmentally friendly, impurity-free aerogel insulation materials still has the following problems: organic solutions bring hidden dangers of environmental pollution; carbon aerogel has poor mechanical properties. Therefore, the green, environmentally friendly and low-cost preparation of impurity-free carbon aerogel insulation materials with high strength is still an urgent problem to be solved in this field, which is also the key to the industrial preparation and application of carbon aerogel insulation materials. Summary of the invention

[0006] The technical problem to be solved by the present invention is to provide an environmentally friendly, low-cost, impurity-free carbon aerogel thermal insulation composite material preparation method in view of the problems that the use of organic solvents in the preparation process of the current preparation of low-cost impurity-free carbon aerogel thermal insulation material will cause environmental pollution and the carbon aerogel is brittle and fragile. The method is simple, efficient, green and environmentally friendly, low-cost, and the prepared material has high compression strength and good thermal insulation performance.

[0007] To achieve the above object, the technical solution of the present invention is as follows:

[0008] The first step is to prepare an organosol by:

[0009] Phenol organic monomer, aldehyde organic monomer, chitosan, acetic acid and water are mixed and stirred evenly to obtain an organic sol, wherein the phenol organic monomer and aldehyde organic monomer are used as carbon precursors; chitosan (containing amino group) is used as a soft template, which can react with the aldehyde organic monomer to generate a compound containing an imine group, and the chitosans can be cross-linked to form a three-dimensional network structure; water is used as a solvent, acetic acid is used as a catalyst, and the phenol organic monomer generates a hydroxymethyl derivative under acid catalysis; chitosan and the hydroxymethyl derivative undergo a polymerization reaction, which can effectively improve the reaction network cross-linking density and network skeleton strength of the gel. In this organic sol, the molar ratio of phenol organic monomer, aldehyde organic monomer, acetic acid and water is 1:2:0.03~3.3:10~250; based on the determined content of phenol organic monomer, the mass ratio of phenol organic monomer and chitosan is 100~610;

[0010] The phenolic organic monomer is one of phenol or resorcinol;

[0011] The aldehyde organic monomer is one of formaldehyde or furfural;

[0012] In the second step, the organosol fiber preform composite is prepared by vacuum impregnation process, the method is:

[0013] According to the volume size of the carbon precursor fiber preform and the apparent density of the carbon precursor fiber preform, the required mass of the carbon precursor fiber is calculated by mass = density × volume, the required mass of the carbon precursor fiber is weighed, the weighed carbon precursor fiber is clamped and fixed by a mold, and the fiber arrangement direction is perpendicular to the heat flow direction when used for thermal insulation, to obtain the carbon precursor fiber preform, the carbon precursor fiber preform is placed in a sealed container, and the fiber preform is vacuum impregnated with the organic sol obtained in the first step by a vacuum impregnation process to obtain an organic sol fiber preform composite;

[0014] The carbon precursor fiber is any one of polyacrylonitrile-based fiber, viscose-based fiber, phenolic-based fiber or asphalt-based fiber;

[0015] The apparent density of the carbon precursor fiber preform is required to be 0.08-0.30 g / cm 3 ;

[0016] In the third step, a fiber-reinforced organogel composite is prepared by a hydrothermal process, wherein:

[0017] The organosol fiber preform composite is placed in a sealed box, and then placed in a water bath at a constant temperature for a certain period of time, and taken out after cooling to room temperature to obtain a fiber-reinforced organogel composite;

[0018] The constant temperature refers to the external heating temperature being controlled at 60-90°C;

[0019] The insulation time is 5 to 72 hours;

[0020] The fourth step is to prepare a fiber-reinforced organic aerogel composite by a normal pressure drying process, the method being:

[0021] The fiber-reinforced organic gel composite obtained in the third step is placed in an oven for normal pressure (0.1 MPa) drying, gradually heated according to the first heating program, and taken out after cooling to room temperature to obtain a fiber-reinforced organic aerogel composite;

[0022] The first temperature rise program is 40°C to 60°C to 80°C to 110°C, with each temperature node being kept at a temperature for 2 to 8 hours, and a heating rate between temperature nodes being 0.1 to 5°C / min;

[0023] The fifth step is to prepare a fiber-reinforced carbon aerogel composite material by a carbonization pyrolysis process, the method being:

[0024] The fiber-reinforced organic aerogel composite is placed in a pyrolysis furnace, evacuated, and after the vacuum degree is less than 100 Pa, heated according to a second heating program for carbonization and pyrolysis, and taken out after cooling to room temperature to obtain a fiber-reinforced carbon aerogel composite material;

[0025] The second temperature rising program is from room temperature to the highest temperature of carbonization and cracking (700-2000°C), requiring a heating rate of 0.5-10°C / min, and a holding time of 1-10h at the highest temperature of carbonization and cracking.

[0026] Compared with the prior art, the present invention has the following beneficial effects:

[0027] (1) The process of the present invention is green and environmentally friendly. In the first step of the present invention, chitosan is used as a soft template and water is used as a solvent; in the third step, the fiber-reinforced organic aerogel complex is obtained by drying the fiber-reinforced organic gel complex at normal pressure. The present invention uses non-toxic, harmless, biodegradable chitosan as a soft template and water as a solvent, which is green and pollution-free; the normal pressure drying process is used, and no organic solvent replacement is required, thereby avoiding the environmental pollution risks caused by organic waste liquid.

[0028] (2) The process of the present invention is simple, the cycle is short, and the cost is low. In the first step of the present invention, phenol organic monomer and aldehyde organic monomer are used as carbon precursors, acetic acid is used as a catalyst, chitosan is used as a soft template, and water is used as a solvent. The raw materials are directly mixed and uniformly prepared into an organic sol; the second step is to use the organic sol to vacuum pressurize and impregnate a carbon precursor fiber preform made of polyacrylonitrile-based fiber, viscose-based fiber, phenolic-based fiber or asphalt-based fiber; the third step is to obtain a fiber-reinforced organic gel composite through a hydrothermal process; the fourth step is to obtain a fiber-reinforced organic aerogel composite by drying the fiber-reinforced organic gel composite under normal pressure; the fifth step is to directly prepare a fiber-reinforced carbon aerogel composite by carbonizing and pyrolyzing the fiber-reinforced organic aerogel composite. The raw materials used in the present invention can all be obtained industrially at a low price; the atmospheric pressure drying process is adopted, thereby avoiding the traditional supercritical drying process, and the equipment is simple, which further reduces the cost; the main process steps in the entire process flow are the third step, the fourth step, and the fifth step, namely the hydrothermal process, the atmospheric pressure drying process, and the carbonization and cracking process, and the process time is only about 1 to 2 days, and the entire process flow only takes 3 to 6 days, the process cycle is short, and it is suitable for industrial production.

[0029] (3) The fiber-reinforced carbon aerogel composite material prepared by the present invention is free of impurities. In the first step of the present invention, acetic acid is used as a catalyst and chitosan is used as a soft template to avoid the introduction of metal impurities and obtain a carbon aerogel free of impurities.

[0030] (4) The fiber-reinforced carbon aerogel composite material prepared by the present invention has high compression strength and good thermal insulation performance. Its compression strength can reach 0.72-38.96MPa, while its thermal conductivity is only 0.04305-0.12255W / m·k. In the first step of the present invention, chitosan is used as a soft template, which reacts with aldehyde organic monomers to generate compounds containing imine groups; phenol organic monomers can generate hydroxymethyl derivatives under acid catalysis. Chitosan containing imine groups can cross-link with each other to form a three-dimensional network structure, and undergo polymerization reaction with hydroxymethyl derivatives, which can effectively improve the cross-linking density and network skeleton strength of the gel reaction network. In addition, in the second step of the present invention, an organic sol is used to vacuum-pressurize a carbon precursor fiber preform made of polyacrylonitrile-based fiber, viscose-based fiber, phenolic-based fiber or asphalt-based fiber, and a fiber-reinforced organic gel composite is obtained after a third step of hydrothermal process. By introducing fiber reinforcement, the mechanical strength of carbon aerogel can be effectively improved. At the same time, the use of carbon precursor fibers can effectively solve the problem of shrinkage mismatch between the reinforcement and the carbon aerogel matrix and reduce the brittleness and shrinkage of the carbon aerogel caused by pyrolysis, thereby avoiding a significant increase in the thermal conductivity of the carbon aerogel and effectively improving its mechanical strength. Finally, a carbon aerogel thermal insulation composite material with both high mechanical strength and excellent thermal insulation performance can be obtained. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Figure 1 It is the overall flow chart of the present invention;

[0032] Figure 2 The compressive strength curve of the environmentally friendly, impurity-free carbon aerogel thermal insulation composite material (Example 1) prepared by the present invention;

[0033] Figure 3 This is an optical photograph of the environmentally friendly, impurity-free carbon aerogel thermal insulation composite material (Example 1) prepared by the present invention. DETAILED DESCRIPTION

[0034] The present invention is further described below in conjunction with the accompanying drawings and embodiments. In the embodiments, the thermal conductivity and compressive strength of the carbon aerogel thermal insulation composite material are mainly characterized. Among them, the thermal conductivity of the carbon aerogel thermal insulation composite material in the embodiments is tested using FOX, and the compressive strength is tested using a universal testing machine.

[0035] In the preparation process of carbon aerogel thermal insulation composite materials, the type of phenol organic monomer, the type of aldehyde organic monomer, the chitosan content, the water content, the acetic acid content and the fiber preform density have an important influence on the thermal conductivity and compressive strength of the carbon aerogel thermal insulation composite materials. Other indicators only affect the length of the process cycle or the process cost, and have no effect on the thermal conductivity and compressive strength of the final carbon aerogel. The following discusses the influence of the six key parameters of the type of phenol organic monomer, the type of aldehyde organic monomer, the chitosan content, the water content, the acetic acid content and the fiber preform density on the thermal conductivity and compressive strength of the carbon aerogel composite materials, and further explains the present invention through examples. The protection scope of the present invention should not be interpreted as being limited to these examples.

[0036] Example 1

[0037] The operation process of preparing Example 1 is as follows Figure 1 As shown, the following steps are included:

[0038] The first step is to prepare an organosol by:

[0039] Resorcinol, formaldehyde, chitosan, acetic acid and water are mixed and stirred to obtain an organosol. The molar ratio of resorcinol, formaldehyde, acetic acid and water is 1:2:0.4:64; the mass ratio of resorcinol and chitosan is 100;

[0040] In the second step, the organosol fiber preform composite is prepared by vacuum impregnation process, the method is:

[0041] According to the volume size of the phenolic fiber preform and the apparent density of the phenolic fiber preform (0.13 g / cm 3), using mass = density × volume to calculate the required mass of phenolic fiber, weighing the required mass of phenolic fiber, clamping and fixing the weighed phenolic fiber with a mold, and making the fiber arrangement direction perpendicular to the heat flow direction when used for thermal insulation, to obtain a phenolic fiber preform, placing the fiber preform in a sealed container, and using a vacuum impregnation process to vacuum impregnate the phenolic fiber preform with the organosol obtained in the first step to obtain an organosol fiber preform composite;

[0042] In the third step, a fiber-reinforced organogel composite is prepared by a hydrothermal process, wherein:

[0043] The organosol fiber preform composite is placed in a sealed box, and then placed in a water bath at 80°C for 36 hours, and taken out after cooling to room temperature to obtain a fiber-reinforced organogel composite;

[0044] The fourth step is to prepare a fiber-reinforced organic aerogel composite by a normal pressure drying process, the method being:

[0045] The fiber-reinforced organic gel composite obtained in the third step is placed in an oven for normal pressure (0.1 MPa) drying, and is kept at each temperature node for 6 hours according to the set temperature of 40°C to 60°C to 80°C to 110°C, and the temperature is gradually increased at a heating rate of 1°C / min between the temperature nodes, and is taken out after cooling to room temperature to obtain a fiber-reinforced organic aerogel composite;

[0046] The fifth step is to prepare a fiber-reinforced carbon aerogel composite material by a carbonization pyrolysis process, the method being:

[0047] The fiber-reinforced organic aerogel composite is placed in a pyrolysis furnace and evacuated to meet the vacuum degree of <100Pa. The heating rate from room temperature to the maximum temperature of carbonization pyrolysis is 5°C / min, the maximum temperature of carbonization pyrolysis is 1000°C, and the maximum temperature of carbonization pyrolysis is kept at 1h. The temperature is heated for carbonization pyrolysis, and the mixture is taken out after being cooled to room temperature to obtain a fiber-reinforced carbon aerogel composite material.

[0048] Figure 2 The compression strength curve of the environmentally friendly, low-cost, impurity-free carbon aerogel thermal insulation composite material (Example 1) prepared by the present invention is shown in the figure. The horizontal axis is the compression deformation of the carbon aerogel thermal insulation composite material, and the vertical axis is the compression pressure of the carbon aerogel thermal insulation composite material. It can be seen that when the carbon aerogel thermal insulation composite material is compressed by more than 50%, the compression strength still does not decrease, that is, the carbon aerogel thermal insulation composite material does not break. In addition, the carbon aerogel thermal insulation composite material still has a high compression strength of 2.88MPa under a compression deformation of 10%.

[0049] Figure 3This is an optical photograph of the environmentally friendly, low-cost, impurity-free carbon aerogel thermal insulation composite material (Example 1) prepared by the present invention. It can be seen that the surface of the carbon aerogel thermal insulation composite material is smooth and free of cracks.

[0050] When the organic sol fiber preform composite is prepared by the second step vacuum impregnation process, the polyacrylonitrile-based fiber, viscose-based fiber, phenolic-based fiber or asphalt-based fiber used are all carbon precursor fibers, which will be carbonized and cracked to form carbon fibers in the fifth step carbonization and cracking process. Different types of carbon precursor fibers only have certain differences in composition, which only affect the process cost, and have little effect on the thermal conductivity and compressive strength of the finally prepared fiber-reinforced carbon aerogel composite material. Therefore, in order to save space, only some embodiments 325 to 336 of different fiber types are listed, among which the fiber types of embodiments 325 to 328 are polyacrylonitrile-based fibers, the fiber types of embodiments 329 to 332 are viscose-based fibers, and the fiber types of embodiments 333 to 336 are asphalt-based fibers; when the fiber-reinforced organic gel composite is prepared by the third step hydrothermal process, for the constant The temperature is kept in a water bath of a certain time, and the temperature and time are determined by the type of raw materials used. The reactivity of different raw materials is different. As long as the gel reaction is fully and completely within the set temperature and time, the properties of the prepared fiber-reinforced carbon aerogel composite material are little affected; in the fourth step of the atmospheric pressure drying process to prepare the fiber-reinforced organic aerogel composite, the oven used ensures that the atmospheric pressure drying is fully and thoroughly to completely volatilize the solvent, and the first heating program gradually increases the temperature in steps to prevent the excessive surface tension during the rapid heating process from causing the material to shrink and crack; in the fifth step of the carbonization and cracking process to prepare the fiber-reinforced carbon aerogel composite, the carbonization and cracking temperature and time determine the carbonization and cracking degree of the carbon precursor fiber preform and the organic aerogel matrix, as long as the carbon precursor fiber preform and the organic aerogel matrix are completely carbonized and cracked into carbon materials and carbon aerogels. The above conditions have no effect on the compressive strength and thermal conductivity of the fiber-reinforced carbon aerogel thermal insulation composite material, so the process parameters used in Examples 2 to 336 are shown in Table 1, and the experimental process parameters not listed in the table are the same as those in Example 1.

[0051] The above embodiments are only preferred embodiments of the present invention and are not intended to limit the scope of protection of the present invention. Any changes made by adopting the design principle of the present invention and by non-creative labor on this basis shall fall within the scope of protection of the present invention. In the present organosol, the molar ratio of phenol organic monomer, aldehyde organic monomer, acetic acid and water is 1:2:0.03-3.3:10-250; based on the content of phenol organic monomer, the mass ratio of phenol organic monomer to chitosan is 100-610.

[0052] Table 1 Preparation process parameters and material performance parameters of fiber reinforced carbon aerogel thermal insulation composites

[0053]

[0054]

[0055]

[0056]

[0057]

[0058]

[0059]

[0060]

[0061]

[0062]

[0063]

[0064]

[0065]

[0066]

[0067]

Claims

1. A method for preparing an environmentally friendly, impurity-free carbon aerogel thermal insulation composite material, characterized in that The following steps are involved: The first step is to prepare an organosol by: Phenol organic monomer, aldehyde organic monomer, chitosan, acetic acid and water are mixed and stirred to obtain an organic sol, wherein the phenol organic monomer and the aldehyde organic monomer are used as carbon precursors; chitosan is used as a soft template to react with the aldehyde organic monomer to generate a compound containing an imine group, and the chitosans are cross-linked to form a three-dimensional network structure; water is used as a solvent, acetic acid is used as a catalyst, and the phenol organic monomer generates a hydroxymethyl derivative under acid catalysis; chitosan and the hydroxymethyl derivative undergo a polymerization reaction to increase the reaction network crosslinking density and network skeleton strength of the gel; the molar ratio of the phenol organic monomer, the aldehyde organic monomer, the acetic acid and the water is 1:2:0.03-3.3:10-250; based on the determined content of the phenol organic monomer, the mass ratio of the phenol organic monomer to the chitosan is 100-610; In the second step, the organosol fiber preform composite is prepared by vacuum impregnation process, the method is: According to the volume size of the carbon precursor fiber preform and the apparent density of the carbon precursor fiber preform, the required mass of the carbon precursor fiber is calculated by mass = density × volume, the required mass of the carbon precursor fiber is weighed, the weighed carbon precursor fiber is clamped and fixed by a mold, and the fiber arrangement direction is perpendicular to the heat flow direction when used for thermal insulation, to obtain the carbon precursor fiber preform, the carbon precursor fiber preform is placed in a sealed container, and the fiber preform is vacuum impregnated with the organic sol obtained in the first step by a vacuum impregnation process to obtain an organic sol fiber preform composite; In the third step, a fiber-reinforced organogel composite is prepared by a hydrothermal process, wherein: The organosol fiber preform composite is placed in a sealed box, and then placed in a water bath at a constant temperature for heat preservation, and taken out after cooling to room temperature to obtain a fiber-reinforced organogel composite; The fourth step is to prepare a fiber-reinforced organic aerogel composite by a normal pressure drying process, the method being: The fiber-reinforced organic gel composite obtained in the third step is placed in an oven for normal pressure drying, gradually heated according to the first heating program, and taken out after cooling to room temperature to obtain a fiber-reinforced organic aerogel composite; The first temperature rising program is 40°C to 60°C to 80°C to 110°C; The fifth step is to prepare a fiber-reinforced carbon aerogel composite material by a carbonization pyrolysis process, the method being: The fiber-reinforced organic aerogel composite is placed in a pyrolysis furnace, evacuated, and after the vacuum degree is less than 100 Pa, heated according to a second heating program for carbonization and pyrolysis, and taken out after cooling to room temperature to obtain a fiber-reinforced carbon aerogel composite material; The second temperature rising program is from room temperature to the highest temperature of carbonization and cracking.

2. The method for preparing an environmentally friendly, impurity-free carbon aerogel thermal insulation composite material as claimed in claim 1, characterized in that In the first step, the phenol organic monomer is one of phenol or resorcinol; and the aldehyde organic monomer is one of formaldehyde or furfural.

3. The method for preparing an environmentally friendly, impurity-free carbon aerogel thermal insulation composite material according to claim 1, characterized in that In the second step, the carbon precursor fiber is any one of polyacrylonitrile-based fiber, viscose-based fiber, phenolic-based fiber or asphalt-based fiber; the apparent density of the carbon precursor fiber preform is required to be 0.08-0.30 g / cm 3 .

4. The method for preparing an environmentally friendly, impurity-free carbon aerogel thermal insulation composite material as claimed in claim 1, characterized in that The constant temperature during the heat preservation in the water bath in the third step refers to the external heating temperature being controlled at 60 to 90° C.; the heat preservation time is 5 to 72 hours.

5. The method for preparing an environmentally friendly, impurity-free carbon aerogel thermal insulation composite material as claimed in claim 1, characterized in that The normal pressure in the fourth step refers to 0.1 MPa; the first heating program requires that each temperature node be kept warm for 2 to 8 hours, and the heating rate between temperature nodes is 0.1 to 5°C / min.

6. The method for preparing an environmentally friendly, impurity-free carbon aerogel thermal insulation composite material according to claim 1, characterized in that The second heating program in step 5 requires a heating rate of 0.5 to 10°C / min, a holding time of 1 to 10 hours at the highest carbonization and pyrolysis temperature, and the highest carbonization and pyrolysis temperature is 700 to 2000°C.