A continuous crystallization method for D-pantolactone
By controlling the temperature and stirring conditions in multiple crystallization kettles, continuous crystallization of D-panolactone is achieved, and the problems of unstable cooling rate, too low crystallization temperature and long process time in the prior art are solved, and high Purity and high particle size D-panolactone crystals reduce production costs.
Patent Information
- Application Number
- CN202310365629.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-07
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2043-04-07
AI Technical Summary
The existing crystallization process of D-panolactone has problems such as unstable cooling rate, low crystallization temperature, impurity inclusion, and long process time, resulting in small product particle size and unqualified purity.
By using the continuous crystallization method, the temperature and stirring conditions are controlled in multiple crystal kettles, the crystals are uniformly dispersed and stable growth are achieved, the residue of washing solvents is reduced, and the filtration performance and product purity are improved.
D-panolactone lactone crystals with low impurity content, large particle size and high purity are realized, which shortens the crystallization time, reduces production costs, and improves the fluidity and stability of the product.
Smart Images

Figure CN116589437B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of crystallization technology and relates to a continuous crystallization method of D-pantolactone. Background Art
[0002] D-(-)-PANTOLACTONE, also known as dihydro-3-hydroxy-4,4-dimethyl-2(3H)furanone, has a CAS number of 599-04-2. D-Pantolactone is a very important pharmaceutical intermediate, mainly used in the synthesis of vitamin B5 drugs, D-panthenol and D-calcium pantothenate, and is the main product of pantothenic acid in the liver. D-Pantolactone is a hygroscopic crystal (benzene / petroleum ether, or sublimation), easily soluble in water, soluble in ethanol, ether, chloroform, carbon disulfide, and benzene.
[0003] Crystallization is one of the most effective methods for producing pure solids. During crystallization, the solutes in the solution are separated due to their different solubility from the solubility of the impurities. The crystallization process also directly affects the crystal form and purity of the product. The traditional crystallization process of D-pantoic acid lactone is similar to the ordinary crystallization process, which can be basically divided into three processes: nucleation, crystal growth, and crystal cultivation. The current crystallization process is that the mother liquor from the upstream distillation tower kettle enters the first crystallization kettle, cools down and maintains for 24 hours, and discharges crude D-pantoic acid lactone. The remaining slurry is transferred to the secondary crystallization kettle; in the secondary crystallization kettle, recrystallization is carried out, and the temperature is controlled to -10℃ by ethylene glycol and maintained for 24 hours. Then the product is washed once in water and activated carbon, and centrifuged to obtain mono-fine D-pantoic acid lactone; then it is washed twice with water and activated carbon again, and centrifuged to obtain di-fine D-pantoic acid lactone.
[0004] At present, the crystallization process of D-pantoic acid lactone is mainly cooling crystallization. In the actual operation process, there are mainly the following problems: (1) Cooling rate: The cooling rate is fast at first and then slow, resulting in severe nucleation during the crystallization process and a small particle size of the final product; (2) Crystallization temperature: The final crystallization temperature is -10°C, resulting in impurities being mixed in the product, resulting in unqualified purity; (3) Crystallization time: The entire process time is 60-80 hours, which is relatively long.
[0005] Based on the above technical status, the inventors believe that it is imperative to develop a reasonable and scientific continuous crystallization technology for D-pantolactone based on the existing industrial crystallization production equipment, and to seek a D-pantolactone continuous crystallization technology with low impurity content, large particle size, low energy consumption, high efficiency, stable product quality, simple process and low production cost. Summary of the invention
[0006] In order to solve the deficiencies of the prior art, the object of the present invention is to provide a D-pantoic acid lactone continuous crystallization method, which realizes continuous crystallization, improves the purity of the crystal product, increases the particle size, improves the filtration performance, and reduces the crystallization process time. The washing method in the crystallization process is reduced to reduce the solvent residue of the left ester product, while ensuring the fluidity of the final D-pantoic acid lactone product and reducing the impurities entrained in the product.
[0007] In order to solve the above technical problems, the present invention adopts the following technical solutions:
[0008] In order to achieve the purpose of the invention, the present invention adopts the following technical solutions:
[0009] One of the objects of the present invention is to provide a continuous crystallization method for D-pantolactone, the continuous crystallization method comprising the following steps:
[0010] (1) Under stirring, D-pantolactone mother liquor with a concentration of 80-85 wt% is introduced into the first-stage crystallization kettle, heated to 60-75° C. and kept warm for 20-40 min, then cooled to 45-60° C., the slurry is discharged from the first-stage crystallization kettle and enters the second-stage crystallization kettle, wherein during the heating and cooling process, the liquid level change is maintained within 10% above or below the equilibrium liquid level;
[0011] (2) controlling the temperature of the second-stage crystallization kettle to be 30-45° C., adding D-pantolactone seed crystals under stirring conditions so that the seed crystals are uniformly dispersed in the second-stage crystallization kettle, and when the volume of the slurry reaches more than 80% of the volume of the second-stage crystallization kettle, the slurry is discharged from the second-stage crystallization kettle and enters the third-stage crystallization kettle;
[0012] (3) controlling the temperature of the third-stage crystallization kettle to 5-20° C., and allowing the D-pantolactone crystals to grow stably under stirring conditions, and the crystal slurry is discharged from the third-stage crystallization kettle and enters the solid-liquid separation system, wherein during the stable growth of the crystals, the liquid level change is maintained within 10% above or below the equilibrium liquid level;
[0013] (4) In the solid-liquid separation system, the separated solid is discharged from the solid-liquid separation system and the mother liquid is recycled.
[0014] Preferably, the D-pantolactone mother liquor in step (1) is a D-pantolactone upstream mother liquor;
[0015] Preferably, the content of pantoic acid impurities in the D-pantoic acid lactone mother liquor in step (1) is 0.5-1wt%, the content of the largest single impurity (the impurity with the largest mass fraction of a single impurity in the mother liquor) is 2-3wt%, and the content of total impurities (all impurities in the mother liquor) is 8-9wt%.
[0016] Preferably, the stirring rate in step (1) is 100-350 rpm;
[0017] Preferably, the added volume of the D-pantoic acid lactone mother liquor in step (1) is 50-70% of the volume of the first-stage crystallization kettle.
[0018] Preferably, the particle size of the seed crystal in step (2) is 0.45-0.65 mm;
[0019] Preferably, based on the addition amount of D-pantoic acid lactone mother liquor being 90-110 g, the addition amount of the seed crystals in step (2) is 2-5 g.
[0020] Preferably, the uniform dispersion time in step (2) is 4-7 hours;
[0021] Preferably, the stirring rate in step (2) is 100-350 rpm.
[0022] Preferably, the stirring rate in step (3) is 50-200 rpm;
[0023] Preferably, the stable growth time of the crystal in step (3) is 6-10 hours.
[0024] Preferably, the mother liquor in step (4) is separated by evaporation and then circulated in the first-stage crystallization kettle to perform a multi-stage continuous crystallization process together with the continuously replenished D-pantolactone mother liquor;
[0025] Preferably, the solid-liquid separation in step (4) is carried out by centrifugation;
[0026] Preferably, the step (4) further comprises washing and drying the solid obtained after solid-liquid separation in sequence.
[0027] Preferably, the preparation method further comprises post-processing the solid obtained by solid-liquid separation;
[0028] Preferably, the post-treatment comprises: adding a saturated aqueous solution of D-pantolactone to the solid obtained after solid-liquid separation for soaking and washing;
[0029] Preferably, based on the addition amount of 60 g of the dry solid obtained after solid-liquid separation, the addition amount of the saturated D-pantoic acid lactone saturated aqueous solution is 45-60 g.
[0030] The second object of the present invention is to provide a continuous crystallization method as described in the first object to crystallize D-pantoic acid lactone.
[0031] Preferably, in the D-pantoic acid lactone, the pantoic acid content is less than ≤0.2%, the maximum single impurity is ≤0.1%, the total impurities are ≤0.5%, the L-pantoic acid lactone is ≤1.0%, and the product purity is greater than 99%.
[0032] Preferably, the average particle size of the D-pantolactone is 0.7-0.9 mm.
[0033] The third object of the present invention is to provide a use of the D-pantoic acid lactone as described in the second object in the preparation of a pharmaceutical intermediate.
[0034] Compared with the prior art, the present invention has the following beneficial effects:
[0035] The method of the invention provides a process for continuously and stably producing D-pantoic acid lactone crystals with high purity, low impurity content, large particle size and easy filtration.
[0036] The method of the invention clarifies the cooling rate, the final crystallization temperature, the temperature, the particle size and the weight of the seed crystals added in the cooling crystallization, and improves the purity of the product so that the pantoic acid content in the D-pantoic acid lactone related substances is less than or equal to 0.2%, the maximum single impurity is less than or equal to 0.1%, the total impurities are less than or equal to 0.5%, and the L-pantoic acid lactone is less than or equal to 1.0%, and the product purity is greater than 99%.
[0037] The method of the invention clarifies the post-treatment method of the crystal product, so that the yield of D-pantoic acid lactone after washing is greater than 90%. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] Figure 1 This is a scanning electron microscope image of the D-pantolactone crystal product produced by the conventional batch crystallization process, with a scale of 1000 μm;
[0039] Figure 2 This is a scanning electron microscope image of the D-pantoic acid lactone crystal product obtained by continuous crystallization in Example 1, with a scale of 1000 μm. DETAILED DESCRIPTION
[0040] It should be noted that the following detailed descriptions are all exemplary and are intended to provide further explanation of the present invention. Unless otherwise specified, all technical and scientific terms used herein have the same meanings as those generally understood by those of ordinary skill in the art to which the present invention belongs. The technical scheme of the present invention is further illustrated below by specific embodiments. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention.
[0041] Example 1
[0042] This embodiment provides a continuous crystallization method of D-pantolactone, comprising the following steps:
[0043] (1) Under the action of a stirring rate of 100 rpm, a D-pantolactone mother liquor with a concentration of 80 wt% (50% by volume of the first-stage crystallization kettle) was introduced into the first-stage crystallization kettle, heated to 60° C. and kept warm for 30 min, and then cooled to 45° C., and the slurry was discharged from the first-stage crystallization kettle and entered into the second-stage crystallization kettle, wherein during the heating and cooling process, the liquid level change was maintained within 10% above and below the equilibrium liquid level;
[0044] (2) controlling the temperature of the second-stage crystallization kettle to 30° C., adding D-pantolactone seed crystals with a particle size of 0.45-0.65 mm (based on the addition amount of D-pantolactone mother liquor being 100 g, the addition amount of seed crystals is 2 g) at a stirring rate of 100 rpm, so that the seed crystals are uniformly dispersed in the second-stage crystallization kettle for 4 h, and when the volume of the slurry reaches more than 80% of the volume of the second-stage crystallization kettle, the slurry is discharged from the second-stage crystallization kettle and enters the third-stage crystallization kettle;
[0045] (3) controlling the temperature of the third-stage crystallization kettle to 5° C. and stirring at a rate of 50 rpm to allow D-pantolactone crystals to grow stably for 6 hours, and the slurry is discharged from the third-stage crystallization kettle and enters the solid-liquid separation system, wherein during the stable growth of the crystals, the liquid level change is maintained within 10% above or below the equilibrium liquid level;
[0046] (4) In the centrifugal system, the separated solid is discharged from the centrifugal system and added with saturated D-pantoic acid lactone mother liquor for washing (the amount of the dry solid added after centrifugal separation is 60 g, and the amount of the saturated D-pantoic acid lactone saturated aqueous solution added is 50 g). After evaporation and separation, it enters the first-stage crystallization kettle for circulation, and undergoes a multi-stage continuous crystallization process together with the continuously replenished D-pantoic acid lactone mother liquor.
[0047] The product obtained in Example 1 was tested as follows:
[0048] (1) Particle size test (test equipment: Malvern Laser Particle Sizer Mastersizer 3000): Figure 2 The scanning electron microscope image of the product was obtained for this example. Figure 2 It can be seen that the average particle size of the product is 0.97 mm;
[0049] (2) Optical rotation test (test equipment: digital automatic polarimeter SGW-2): The optical rotation of the obtained product is -2.4697;
[0050] (3) Purity test (HPLC): It can be seen that the maximum single impurity of the product is 0.03%, and the total impurity is 0.04%.
[0051] In the preparation method of the present application, the overall process takes 13.5 hours, and the problem of explosive nucleation does not occur during the preparation process.
[0052] Example 2
[0053] This embodiment provides a continuous crystallization method of D-pantolactone, comprising the following steps:
[0054] (1) Under the action of a stirring rate of 250 rpm, a D-pantolactone mother liquor with a concentration of 82 wt% (60% by volume of the first-stage crystallization kettle) was introduced into the first-stage crystallization kettle, heated to 70° C. and kept warm for 30 min, and then cooled to 55° C., and the slurry was discharged from the first-stage crystallization kettle and entered into the second-stage crystallization kettle, wherein during the heating and cooling process, the liquid level change was maintained within 10% above and below the equilibrium liquid level;
[0055] (2) controlling the temperature of the second-stage crystallization kettle to 40° C., adding D-pantolactone seed crystals with a particle size of 0.45-0.65 mm (the amount of seed crystals added is 3 g based on the amount of D-pantolactone mother liquor added is 100 g) at a stirring rate of 250 rpm, so that the seed crystals are uniformly dispersed in the second-stage crystallization kettle for 5 h, and when the volume of the slurry reaches more than 80% of the volume of the second-stage crystallization kettle, the slurry is discharged from the second-stage crystallization kettle and enters the third-stage crystallization kettle;
[0056] (3) controlling the temperature of the third-stage crystallization kettle to be 15° C. and stirring at a rate of 150 rpm to allow D-pantolactone crystals to grow stably for 8 h, and the slurry is discharged from the third-stage crystallization kettle and enters the solid-liquid separation system, wherein during the stable growth of the crystals, the liquid level change is maintained within 10% above or below the equilibrium liquid level;
[0057] (4) In the centrifugal system, the separated solid is discharged from the centrifugal system and added with saturated D-pantoic acid lactone mother liquor for washing (the amount of the dry solid added after centrifugal separation is 60 g, and the amount of the saturated D-pantoic acid lactone saturated aqueous solution added is 50 g). After evaporation and separation, it enters the first-stage crystallization kettle for circulation, and undergoes a multi-stage continuous crystallization process together with the continuously replenished D-pantoic acid lactone mother liquor.
[0058] The product obtained in this example was tested by the same testing method as in Example 1. It was found that the average particle size of the product was 0.97 mm, the optical rotation of the product was -2.3874, the maximum single impurity of the product was 0.04%, and the total impurity was 0.08%.
[0059] In the preparation method of the present application, the overall process takes 16.5 hours, and the problem of explosive nucleation does not occur during the preparation process.
[0060] Example 3
[0061] This embodiment provides a continuous crystallization method of D-pantolactone, comprising the following steps:
[0062] (1) Under the action of a stirring rate of 350 rpm, a D-pantolactone mother liquor with a concentration of 85 wt% (70% by volume of the first-stage crystallization kettle) was introduced into the first-stage crystallization kettle, heated to 75° C. and kept warm for 30 min, and then cooled to 60° C., and the slurry was discharged from the first-stage crystallization kettle and entered into the second-stage crystallization kettle, wherein during the heating and cooling process, the liquid level change was maintained within 10% above and below the equilibrium liquid level;
[0063] (2) controlling the temperature of the second-stage crystallization kettle to be 45° C., adding D-pantolactone seed crystals with a particle size of 0.45-0.65 mm (the amount of seed crystals added is 5 g based on the amount of D-pantolactone mother liquor added being 100 g) at a stirring rate of 350 rpm, so that the seed crystals are uniformly dispersed in the second-stage crystallization kettle for 7 h, and when the volume of the slurry reaches more than 80% of the volume of the second-stage crystallization kettle, the slurry is discharged from the second-stage crystallization kettle and enters the third-stage crystallization kettle;
[0064] (3) controlling the temperature of the third-stage crystallization kettle to 20° C. and stirring at a rate of 200 rpm to allow D-pantolactone crystals to grow stably for 10 h, and the slurry is discharged from the third-stage crystallization kettle and enters the solid-liquid separation system, wherein during the stable growth of the crystals, the liquid level change is maintained within 10% above or below the equilibrium liquid level;
[0065] (4) In the centrifugal system, the separated solid is discharged from the centrifugal system and added with saturated D-pantoic acid lactone mother liquor for washing (the amount of the dry solid added after centrifugal separation is 60 g, and the amount of the saturated D-pantoic acid lactone saturated aqueous solution added is 50 g). After evaporation and separation, it enters the first-stage crystallization kettle for circulation, and undergoes a multi-stage continuous crystallization process together with the continuously replenished D-pantoic acid lactone mother liquor.
[0066] The product obtained in this example was tested by the same testing method as in Example 1. It was found that the average particle size of the product was 0.95 mm, the optical rotation of the product was -2.5928, the maximum single impurity of the product was 0.03%, and the total impurity was 0.05%.
[0067] In the preparation method of the present application, the overall process takes 20.5 hours, and the problem of explosive nucleation does not occur during the preparation process.
[0068] Comparative Example 1
[0069] One-step cooling crystallization is adopted, a conventional batch process, without adding seed crystals.
[0070] The first-stage crystallization kettle is fed with a D-pantoic acid lactone mother liquor with a concentration of 85wt% at a temperature of 70-90°C. The crystallization kettle contains low-temperature brine, which is cooled to 20°C within 12 hours and kept warm for 24 hours. It is then transferred to the second crystallization kettle for recrystallization in ethylene glycol, cooled to -10°C within 12 hours, and kept for 24 hours. The product is then washed twice in activated carbon to obtain the final product. The entire process takes 72 hours, which is a long time. The mother liquor has severe nucleation explosion, and impurities are hidden inside the crystals. The final crystal product has a small particle size and a high impurity content. The pantoic acid content is >0.2%, the maximum single impurity is >0.1%, the total impurities are >0.5%, and the L-pantoic acid lactone is >1.0%. The product purity is less than 95%.
[0071] The particle size, optical rotation and impurities of the D-pantoic acid lactone product in Example 1 and Comparative Example 1 are shown in the table below.
[0072] Table 1D-Pantolactone Crystallization Process Comparison
[0073]
[0074] Figure 1 This is a scanning electron microscope image of the D-pantolactone crystal product obtained by conventional intermittent crystallization process in Comparative Example 1. Figure 2 This is a scanning electron microscope image of the D-pantolactone crystal product obtained by continuous crystallization in Example 1. Figure 1 and Figure 2 By comparison, it can be seen that the average particle size of D-pantolactone crystals produced by the traditional intermittent crystallization process is reduced by 30%, and explosive nucleation occurs, impurities are hidden inside the crystals, and the total impurities increase to 0.17%.
[0075] Comparative Example 2
[0076] A two-step crystallization method is adopted, with a first-stage crystallization kettle and a second-stage crystallization kettle, but no third-stage crystallization kettle, to simulate a two-stage continuous crystallization process.
[0077] (1) Under the action of a stirring rate of 250 rpm, a D-pantolactone mother liquor with a concentration of 85 wt% (60% by volume of the first-stage crystallization kettle) was introduced into the first-stage crystallization kettle, heated to 70° C. and kept warm for 30 min, and then cooled to 55° C., and the slurry was discharged from the first-stage crystallization kettle and entered into the second-stage crystallization kettle, wherein during the heating and cooling process, the liquid level change was maintained within 10% above and below the equilibrium liquid level;
[0078] (2) The temperature of the second-stage crystallization kettle was controlled at 40°C, and D-pantoic acid lactone seed crystals with a particle size of 0.45-0.65 mm were added at a stirring rate of 250 rpm (the amount of seed crystals added was 3 g based on the amount of D-pantoic acid lactone mother liquor added was 100 g), so that the D-pantoic acid lactone crystals grew stably for 8 hours.
[0079] (4) In the centrifugal system, the separated solid is discharged from the centrifugal system and added with saturated D-pantoic acid lactone mother liquor for washing (the amount of the dry solid added after centrifugal separation is 60 g, and the amount of the saturated D-pantoic acid lactone saturated aqueous solution added is 50 g). After evaporation and separation, it enters the first-stage crystallization kettle for circulation, and undergoes a multi-stage continuous crystallization process together with the continuously replenished D-pantoic acid lactone mother liquor.
[0080] The product obtained in this comparative example was tested by the same testing method as in Example 1. It was found that the average particle size of the product was 0.67 mm, the optical rotation of the product was -2.4775, the maximum single impurity of the product was 0.04%, and the total impurity was 0.09%.
[0081] In the preparation method of the present application, the overall process takes 11.5 hours, and the problem of explosive nucleation occurs during the preparation process.
[0082] By comparing Comparative Example 2 with Example 1, it can be seen that the stable growth time of crystals without the third-stage crystallization kettle is reduced, and after adding the seed crystal, the supersaturation cannot be used for crystal growth, and explosive nucleation occurs, the average particle size is reduced to 0.67 mm, and the total impurities are increased to 0.09%.
[0083] Comparative Example 3
[0084] A two-step crystallization method is adopted, with a first-stage crystallization kettle and a third-stage crystallization kettle, but no second-stage crystallization kettle, to simulate a two-stage continuous crystallization process.
[0085] (1) Under the action of a stirring rate of 250 rpm, a D-pantolactone mother liquor with a concentration of 85 wt% (60% by volume of the first-stage crystallization kettle) was introduced into the first-stage crystallization kettle, heated to 70° C. and kept warm for 30 min, and then cooled to 55° C., and the slurry was discharged from the first-stage crystallization kettle and entered into the second-stage crystallization kettle, wherein during the heating and cooling process, the liquid level change was maintained within 10% above and below the equilibrium liquid level;
[0086] (2) The temperature of the second-stage crystallization kettle was controlled at 15°C, and D-pantoic acid lactone seed crystals with a particle size of 0.45-0.65 mm were added at a stirring rate of 250 rpm (the amount of seed crystals added was 3 g based on the amount of D-pantoic acid lactone mother liquor added was 100 g), so that the D-pantoic acid lactone crystals grew stably for 8 hours.
[0087] (4) In the centrifugal system, the separated solid is discharged from the centrifugal system and added with saturated D-pantoic acid lactone mother liquor for washing (the amount of the dry solid added after centrifugal separation is 60 g, and the amount of the saturated D-pantoic acid lactone saturated aqueous solution added is 50 g). After evaporation and separation, it enters the first-stage crystallization kettle for circulation, and undergoes a multi-stage continuous crystallization process together with the continuously replenished D-pantoic acid lactone mother liquor.
[0088] The product obtained in this comparative example was tested by the same testing method as in Example 1. It was found that the average particle size of the product was 0.58 mm, the optical rotation of the product was -2.4793, the maximum single impurity of the product was 0.07, and the total impurity was 0.12%.
[0089] In the preparation method of the present application, the overall process takes 11.5 hours, and the problem of explosive nucleation occurs during the preparation process.
[0090] By comparing Comparative Example 3 with Example 1, it can be seen that without the second-stage crystallization kettle, the temperature for adding the seed crystals is too low, and explosive nucleation occurs before the seed crystals are added, resulting in impurities being hidden inside the product. The average particle size of the product is 0.58 mm, and the total impurities increase to 0.12%.
[0091] Comparative Example 4
[0092] A two-step crystallization method is adopted, with a second-stage crystallization kettle and a third-stage crystallization kettle, but without a first-stage crystallization kettle, to simulate a two-stage continuous crystallization process.
[0093] (1) Under the action of a stirring rate of 250 rpm, a D-pantolactone mother liquor with a concentration of 85 wt% (60% by volume of the first-stage crystallization kettle) was introduced into the first-stage crystallization kettle, heated to 70° C. and kept warm for 30 min, and then cooled to 40° C., and the slurry was discharged from the first-stage crystallization kettle and entered into the second-stage crystallization kettle, wherein during the heating and cooling process, the liquid level change was maintained within 10% above and below the equilibrium liquid level;
[0094] (2) The temperature of the second-stage crystallization kettle was controlled at 15°C, and D-pantoic acid lactone seed crystals with a particle size of 0.45-0.65 mm were added at a stirring rate of 250 rpm (the amount of seed crystals added was 3 g based on the amount of D-pantoic acid lactone mother liquor added was 100 g), so that the D-pantoic acid lactone crystals grew stably for 8 hours.
[0095] (4) In the centrifugal system, the separated solid is discharged from the centrifugal system and added with saturated D-pantoic acid lactone mother liquor for washing (the amount of the dry solid added after centrifugal separation is 60 g, and the amount of the saturated D-pantoic acid lactone saturated aqueous solution added is 50 g). After evaporation and separation, it enters the first-stage crystallization kettle for circulation, and undergoes a multi-stage continuous crystallization process together with the continuously replenished D-pantoic acid lactone mother liquor.
[0096] The results show that there is no first-stage crystallization kettle in the crystallization process, the temperature drops too quickly, the explosive nucleation phenomenon is serious, and a large number of fine crystals appear. D-pantoic acid lactone crystals with a particle size of >90mm account for 3.28% of the total crystals, and the average particle size is 0.56mm.
[0097] The product obtained in this comparative example was tested by the same testing method as in Example 1. It was found that the average particle size of the product was 0.56 mm, the optical rotation of the product was -2.4674, the maximum single impurity of the product was 0.04%, and the total impurity was 0.13%.
[0098] In the preparation method of the present application, the overall process takes 11.5 hours, and the problem of explosive nucleation occurs during the preparation process.
[0099] By comparing Comparative Example 4 with Example 1, it can be seen that without the first-stage crystallization kettle, the temperature drops too quickly, the explosive nucleation phenomenon is serious, and a large number of fine crystals appear with an average particle size of 0.56 mm and a total impurity of 0.10%.
[0100] Comparative Example 5
[0101] The only difference from Example 1 is that D-pantolactone seed crystals smaller than 0.45 mm obtained by recrystallization are added, and the rest of the preparation method is the same as that of Example 1.
[0102] The product obtained in this comparative example was tested by the same testing method as in Example 1. It was found that the average particle size of the product was in the range of 0.50-0.70 mm, the optical rotation of the product was -2.4778, the maximum single impurity of the product was 0.04%, and the total impurity was 0.10%.
[0103] In the preparation method of the present application, the overall process takes 13.5 hours, and the problem of explosive nucleation occurs during the preparation process.
[0104] By comparing Comparative Example 5 with Example 1, it can be seen that after adding D-pantoic acid lactone seed crystals less than 0.45 mm obtained by recrystallization, the mother liquor explodes into nuclei to produce a large number of small-sized crystal nuclei, and finally a small product with a particle size of 0.50-0.70 mm is obtained. Impurities are easily hidden in the crystals, resulting in a maximum single impurity of 0.04% and a total impurity of 0.10%.
[0105] Comparative Example 6
[0106] The only difference from Example 2 is that activated carbon is added and the crystal product is eluted with pure water. The rest of the preparation method is the same as Example 2.
[0107] The washing yields of the D-pantoic acid lactone products in Example 2 and Comparative Example 6 and the maximum single impurity are shown in the table below.
[0108]
[0109] Actual yield = (actual crystal mass / g) / (crystal mass in solution / g) × 100%
[0110] Washing yield = (mass of washed product / g) / (mass of wet product / g) × 100%
[0111] By comparing Example 2 and Comparative Example 6, it can be known that the saturated aqueous solution washing D-pantoic acid lactone crystals reduces the washing solvent consumption by 30% compared to pure water washing, and the solubility of D-pantoic acid lactone in water is very large. Using water washing will dissolve the large particle size product into a small particle size, and the particle size is reduced by 30%. The crystal will not dissolve in the washing solvent, and the occurrence of recrystallization phenomenon is avoided. In addition, there is residual activated carbon in the product, which becomes a new impurity and the total impurity increases. After washing with saturated solution, the actual yield is increased to 58.53%, the washing yield is increased to 90%, there is no pantoic acid impurity, the maximum single impurity is 0.03%, the total impurity is 0.09%, and the L-pantoic acid lactone content is 0.36%.
[0112] The applicant declares that the above is only a specific implementation mode of the present invention, but the protection scope of the present invention is not limited thereto. Those skilled in the art should understand that any changes or substitutions that can be easily thought of by those skilled in the art within the technical scope disclosed by the present invention shall fall within the protection scope and disclosure scope of the present invention.
Claims
1. A continuous crystallization method for D-pantolactone, characterized in that: The continuous crystallization method comprises the following steps: (1) Under stirring, D-pantolactone mother liquor with a concentration of 80-85 wt% is introduced into the first-stage crystallization kettle, heated to 60-75° C. and kept warm for 20-40 min, then cooled to 45-60° C., the slurry is discharged from the first-stage crystallization kettle and enters the second-stage crystallization kettle, wherein during the heating and cooling process, the liquid level change is maintained within 10% above or below the equilibrium liquid level; (2) controlling the temperature of the second-stage crystallization kettle to be 30-45° C., adding D-pantolactone seed crystals under stirring conditions so that the seed crystals are uniformly dispersed in the second-stage crystallization kettle, and when the volume of the slurry reaches more than 80% of the volume of the second-stage crystallization kettle, the slurry is discharged from the second-stage crystallization kettle and enters the third-stage crystallization kettle; The particle size of the seed crystal in step (2) is 0.45-0.65 mm; Based on the addition amount of D-pantoic acid lactone mother liquor being 90-110 g, the addition amount of the seed crystals in step (2) is 2-5 g; The uniform dispersion time in step (2) is 4-7 hours; (3) controlling the temperature of the third-stage crystallization kettle to 5-20° C., and allowing the D-pantolactone crystals to grow stably under stirring conditions, and the crystal slurry is discharged from the third-stage crystallization kettle and enters the solid-liquid separation system, wherein during the stable growth of the crystals, the liquid level change is maintained within 10% above or below the equilibrium liquid level; The crystal growth time in step (3) is 6-10 hours; (4) In the solid-liquid separation system, the separated solid is discharged from the solid-liquid separation system, and the mother liquid is recycled; The method further comprises post-processing the solid obtained from the solid-liquid separation; The post-treatment comprises: adding a saturated D-pantolactone saturated aqueous solution to the solid obtained after solid-liquid separation for soaking and washing.
2. The continuous crystallization method according to claim 1, characterized in that The D-pantolactone mother liquor in step (1) is a D-pantolactone upstream mother liquor.
3. The continuous crystallization method according to claim 1, characterized in that The content of pantoic acid impurities in the D-pantoic acid lactone mother liquor in step (1) is 0.5-1wt%, the content of the maximum single impurity is 2-3wt%, and the content of total impurities is 8-9wt%.
4. The continuous crystallization method according to claim 1, characterized in that The stirring rate in step (1) is 100-350 rpm.
5. The continuous crystallization method according to claim 1, characterized in that The added volume of the D-pantoic acid lactone mother liquor in step (1) is 50-70% of the volume of the first-stage crystallization kettle.
6. The continuous crystallization method according to claim 1, characterized in that The stirring rate in step (2) is 100-350 rpm.
7. The continuous crystallization method according to claim 1, characterized in that The stirring rate in step (3) is 50-200 rpm.
8. The continuous crystallization method according to claim 1, characterized in that The mother liquor in step (4) is separated by evaporation and then circulated in the first-stage crystallization kettle to undergo a multi-stage continuous crystallization process together with the continuously replenished D-pantoic acid lactone mother liquor.
9. The continuous crystallization method according to claim 1, characterized in that The solid-liquid separation method in step (4) is centrifugation.
10. The continuous crystallization method according to claim 1, characterized in that Based on the addition amount of 60 g of the dried solid obtained after solid-liquid separation, the addition amount of the saturated aqueous solution of D-pantolactone is 45-60 g.
Citation Information
Patent Citations
Method for preparing D-(-)- or L-(+)-pantoic acid lactone by splitting pantoic acid lactone
CN102229584A
Preparation method of D-calcium pantothenate
CN108129345A
Aqueous solution crystallization method of D-panolactone
CN110734415A
Refining method of D-pantolactone
CN110862362A
Preparation method of Dexpanthenol
CN112047851A