A method for synthesizing a phosphorus-containing extreme pressure antiwear agent

By adding dropwise alcohol, catalyst and propylene oxide to the phosphorus pentasulfide solution, and adding phosphorus pentoxide and primary amine, a phosphorus-containing extreme pressure antiwear agent was successfully produced, which solved the problem of insufficient synthesis methods in the existing technology and improved improve product stability and performance.

CN116606681BActive Publication Date: 2024-10-22HENAN RUNYANG CHEMICAL NEW MATERIALS CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202310596907.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-05-18
Publication Date
2024-10-22
Estimated Expiration
2043-05-18

AI Technical Summary

Technical Problem

The existing technology lacks effective methods to synthesize phosphorus-containing extreme pressure antiwear agents to improve the tribological properties of lubricating oil and extend the service life of mechanical equipment.

Method used

Phosphorus-containing extreme pressure antiwear agent is prepared by adding an excess amount of alcohol to the phosphorus pentasulfide solution for sulfur phosphating reaction, then adding catalyst and propylene oxide for double esterification, and finally adding primary amine for amination reaction.

Benefits of technology

Through this method, the production of phosphorus-containing extreme pressure anti-wear agent is realized, the reaction temperature and addition ratio are controlled, the stability of the product is improved, the proportion of side reactions is reduced, and the performance of the product is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116606681B_ABST
    Figure CN116606681B_ABST
Patent Text Reader

Abstract

The present invention relates to the technical field of phosphorus-containing extreme pressure anti-wear agents, and in particular to a method for synthesizing a phosphorus-containing extreme pressure anti-wear agent, which comprises the following steps: step S101, dripping an excess alcohol in a phosphorus pentasulfide solution, and performing a sulfurization reaction after heating; step S102, cooling, adding a catalyst, and then slowly dripping propylene oxide; step S103, heating, uniformly adding phosphorus pentoxide for complex esterification; step S104, heating, adding a primary amine for amination reaction, and obtaining a phosphorus-containing extreme pressure anti-wear agent. The invention has the beneficial effects of: through steps S101-S104, the production and manufacture of the phosphorus-containing extreme pressure anti-wear agent is realized, and by continuously and uniformly adding phosphorus pentoxide, under the condition of reaction temperature control, the proportion of the main reaction is increased, while the proportion of the side reaction is reduced, which is beneficial to improving the stability of the product.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of phosphorus-containing extreme pressure anti-wear agents, and in particular to a method for synthesizing a phosphorus-containing extreme pressure anti-wear agent. Background Art

[0002] Extreme pressure anti-wear agents are usually added to lubricating oils to improve the tribological properties of base oils, reduce friction resistance, reduce wear and abrasion, and ultimately achieve the purpose of improving the load-bearing capacity of lubricating oils. The normal operation of mechanical equipment is inseparable from lubricating oils. Lubricating oils with excellent performance can reduce friction and wear, reduce energy consumption, improve mechanical efficiency and extend the service life of mechanical equipment; therefore, the use of extreme pressure anti-wear agents to improve the performance of lubricating oils to reduce friction, wear and prevent sintering is of great significance to production;

[0003] Therefore, a method for synthesizing a phosphorus-containing extreme pressure anti-wear agent is needed to produce the phosphorus-containing extreme pressure anti-wear agent. Summary of the invention

[0004] In order to solve the above problems, the present invention provides a method for synthesizing a phosphorus-containing extreme pressure anti-wear agent, which achieves the purpose of solving the problems raised in the background technology.

[0005] In order to achieve the above object, the present invention specifically adopts the following technical scheme: a method for synthesizing a phosphorus-containing extreme pressure antiwear agent, comprising the following steps:

[0006] Step S101, adding excess alcohol to a phosphorus pentasulfide solution, and heating the solution to perform a sulfurization reaction;

[0007] Step S102, cooling, adding a catalyst, and then slowly dropping propylene oxide;

[0008] Step S103, heating, and adding phosphorus pentoxide at a uniform rate to perform re-esterification;

[0009] Step S104, raising the temperature, adding primary amine to carry out an amination reaction, and obtaining a phosphorus-containing extreme pressure antiwear agent.

[0010] As a further improvement of the above technical solution:

[0011] Step S101 is specifically as follows: adding excess alcohol to the phosphorus pentasulfide solution for 1-2 hours, heating to maintain the temperature at 70-80° C., and then performing sulfurization reaction for 2-4 hours.

[0012] In step S101, the molecular formula of the alcohol is ROH, wherein R is any fatty alcohol from C8H17 to C12H25 or a combination thereof.

[0013] In step S101, the molar ratio of alcohol to phosphorus pentasulfide is 6-8:1.

[0014] Step S102 is specifically as follows: after the sulfur phosphating reaction is completed, the temperature is lowered to 10-30°C, a catalyst is added, and then propylene oxide is slowly added dropwise for 1-2 hours, and the temperature during the addition process is kept below 30°C.

[0015] In step S102, the molar ratio of propylene oxide to phosphorus pentasulfide is 0.4-0.6:1.

[0016] In step S102, the catalyst includes one or both of ammonia water and hydrogen peroxide, and the mass ratio of the catalyst to phosphorus pentasulfide is 1:500-1000.

[0017] Step S103 is specifically as follows: heating to 70-80°C, adding phosphorus pentoxide at a constant speed for 1-2 hours to perform re-esterification;

[0018] The molar ratio of phosphorus pentoxide to phosphorus pentasulfide is 0.9-1.1:1.

[0019] Step S104 is specifically as follows: heating to 80-85° C., adding primary amine to carry out amination reaction for 2-4 hours, and obtaining a phosphorus-containing extreme pressure anti-wear agent.

[0020] In step S104, the primary amine is one or a mixture of the following substances: octadecylamine, soybean oil primary amine, hydrogenated tallow primary amine; the mass ratio of the primary amine to phosphorus pentasulfide is 1:200-500.

[0021] The beneficial effects of the present invention are:

[0022] Through steps S101-S104, the production of phosphorus-containing extreme pressure anti-wear agent is realized, and by continuously and evenly adding phosphorus pentoxide, under the condition of controlling the reaction temperature, the proportion of the main reaction is increased, while the proportion of the side reaction is reduced, which is beneficial to improving the stability of the product. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a schematic diagram of the process of the present invention. DETAILED DESCRIPTION

[0024] The preferred embodiments of the present invention are described below with reference to the accompanying drawings. It should be understood by those skilled in the art that these embodiments are only used to explain the technical principles of the present invention and are not intended to limit the protection scope of the present invention.

[0025] See also Figure 1 The present invention discloses a method for synthesizing a phosphorus-containing extreme pressure antiwear agent, comprising the following steps:

[0026] Step S101, adding excess alcohol to a phosphorus pentasulfide solution, and heating the solution to perform a sulfurization reaction;

[0027] Step S102, cooling, adding a catalyst, and then slowly dropping propylene oxide;

[0028] Step S103, heating, and adding phosphorus pentoxide at a uniform rate to perform re-esterification;

[0029] Step S104, raising the temperature, adding primary amine to carry out an amination reaction, and obtaining a phosphorus-containing extreme pressure antiwear agent.

[0030] Through steps S101-S104, the production of phosphorus-containing extreme pressure anti-wear agent is realized, and by continuously and evenly adding phosphorus pentoxide, under the condition of controlling the reaction temperature, the proportion of the main reaction is increased, while the proportion of the side reaction is reduced, which is beneficial to improving the stability of the product.

[0031] Step S101 is specifically as follows: adding excess alcohol to the phosphorus pentasulfide solution for 1-2 hours, heating to maintain the temperature at 70-80° C., and then performing sulfurization reaction for 2-4 hours.

[0032] In step S101, the molecular formula of the alcohol is ROH, wherein R is any fatty alcohol from C8H17 to C12H25 or a combination thereof.

[0033] In step S101, the molar ratio of alcohol to phosphorus pentasulfide is 6-8:1; preferably, the alcohol is isooctyl alcohol or dodecanol, and the molar ratio of alcohol to phosphorus pentasulfide is 6.5:1; preferably, the temperature of adding alcohol is maintained at 75°C for 2 hours, and the reaction is carried out for 4 hours after the addition is completed.

[0034] Step S102 is specifically as follows: after the sulfurization reaction is completed, the temperature is lowered to 10-30°C, a catalyst is added, and then propylene oxide is slowly added dropwise for 1-2 hours, and the temperature during the addition process is kept below 30°C; preferably, the temperature is lowered to 20°C, and the molar ratio of propylene oxide to phosphorus pentasulfide is 0.6:1.

[0035] In step S102, the molar ratio of propylene oxide to phosphorus pentasulfide is 0.4-0.6:1.

[0036] In step S102, the catalyst includes one or both of ammonia water or hydrogen peroxide, and the mass ratio of the catalyst to phosphorus pentasulfide is 1:500-1000; preferably, the catalyst is 20% ammonia water, and the mass ratio of the catalyst to phosphorus pentasulfide is 1:500.

[0037] Step S103 is specifically as follows: heating to 70-80°C, adding phosphorus pentoxide at a constant speed for 1-2 hours to perform re-esterification;

[0038] The molar ratio of phosphorus pentoxide to phosphorus pentasulfide is 0.9-1.1:1; preferably, the molar ratio of phosphorus pentoxide to phosphorus pentasulfide is 1:1, and the addition time is 1 hour.

[0039] Step S104 is specifically as follows: heating to 80-85° C., adding primary amine to carry out amination reaction for 2-4 hours, and obtaining a phosphorus-containing extreme pressure anti-wear agent.

[0040] In step S104, the primary amine is one or a mixture of the following substances: octadecylamine, soybean oil primary amine, hydrogenated tallow primary amine; the mass ratio of the primary amine to phosphorus pentasulfide is 1:200-500; preferably, the primary amine is octadecylamine, and the mass ratio to phosphorus pentasulfide is 1:200, and the reaction time after addition is 2.0h.

[0041] Embodiment 1:

[0042] Add 100.0 g of solid phosphorus pentasulfide into a four-necked flask equipped with a stirrer, a condenser, a thermometer and a constant pressure dropping funnel, add 450 g of isooctyl alcohol into the constant pressure dropping funnel, connect a tail gas absorption device, add isooctyl alcohol dropwise into the four-necked flask, keep the temperature below 70-80°C during the dropping process, keep the temperature for 4 hours after the addition is completed, cool to 25°C, add 0.1 g of 20% ammonia water, keep the temperature below 30°C, add 100.0 g of propylene oxide dropwise for 1.0 hour, raise the temperature to 75°C after the addition is completed, evenly add 65.0 g of phosphorus pentoxide for 1.0 hour, raise the temperature to 85°C, add 0.5 g of octadecylamine, react for 4.0 hours to obtain a phosphorus-containing extreme pressure anti-wear agent, recorded as product 1.

[0043] Embodiment 2:

[0044] Add 100.0 g of solid phosphorus pentasulfide into a four-necked flask equipped with a stirrer, a condenser, a thermometer and a constant pressure dropping funnel, add 450 g of isooctyl alcohol into the constant pressure dropping funnel, connect a tail gas absorption device, add isooctyl alcohol dropwise into the four-necked flask, keep the temperature below 70-80°C during the dropping process, keep the temperature warm for 4 hours after the addition is completed, cool to 25°C, add 0.1 g of 20% ammonia water, keep the temperature below 30°C, add 100.0 g of propylene oxide dropwise for 2.0 hours, raise the temperature to 75°C after the addition is completed, evenly add 65.0 g of phosphorus pentoxide over 1.0 hour, raise the temperature to 85°C, add 0.5 g of octadecylamine, and react for 4.0 hours to obtain a phosphorus-containing extreme pressure anti-wear agent, recorded as Product 2.

[0045] Embodiment three:

[0046] In a four-necked flask equipped with a stirrer, a condenser, a thermometer and a constant pressure dropping funnel, 100.0 g of solid phosphorus pentasulfide was added, and 450 g of isooctyl alcohol was added to the constant pressure dropping funnel. A tail gas absorption device was connected, and isooctyl alcohol was added dropwise into the four-necked flask. The temperature of the dropping process was kept below 70-80°C. After the dropping was completed, the temperature was kept warm for 4 hours. After the reaction was completed, the temperature was lowered to 25°C, 0.1 g of 20% ammonia water was added, and the temperature was kept below 30°C. 100.0 g of propylene oxide was added dropwise for 2.0 hours. After the dropping was completed, the temperature was raised to 75°C. 65.0 g of phosphorus pentoxide was evenly added after 1.0 hour. The temperature was raised to 85°C, 0.5 g of octadecylamine was added, and the reaction was carried out for 2.0 hours to obtain a phosphorus-containing extreme pressure anti-wear agent, which was recorded as product 3.

[0047] Embodiment 4:

[0048] Add 100.0 g of solid phosphorus pentasulfide into a four-necked flask equipped with a stirrer, a condenser, a thermometer and a constant pressure dropping funnel, add 600 g of lauryl alcohol into the constant pressure dropping funnel, connect a tail gas absorption device, add isooctyl alcohol dropwise into the four-necked flask, keep the temperature below 70-80°C during the dropping process, keep the temperature warm for 4 hours after the addition is completed, cool to 25°C, add 0.1 g of 20% ammonia water, keep the temperature below 30°C, add 100.0 g of propylene oxide dropwise for 2.0 hours, raise the temperature to 75°C after the addition is completed, evenly add 65.0 g of phosphorus pentoxide over 1.0 hour, raise the temperature to 85°C, add 0.4 g of octadecylamine, and react for 2.0 hours to obtain a phosphorus-containing extreme pressure anti-wear agent, recorded as product 4.

[0049] Embodiment five:

[0050] In a four-necked flask equipped with a stirrer, a condenser, a thermometer and a constant pressure dropping funnel, 100.0 g of solid phosphorus pentasulfide was added, and 600 g of lauryl alcohol was added to the constant pressure dropping funnel. A tail gas absorption device was connected, and isooctyl alcohol was added dropwise into the four-necked flask. The temperature of the addition process was kept below 70-80°C. After the addition was completed, the temperature was kept warm for 4 hours. After the reaction was completed, the temperature was lowered to 25°C, 0.1 g of 20% ammonia water was added, and the temperature was kept below 30°C. 100.0 g of propylene oxide was added dropwise for 2.0 hours. After the addition was completed, the temperature was raised to 75°C. 65.0 g of phosphorus pentoxide was evenly added within 1.0 hour. The temperature was raised to 85°C, 0.5 g of soybean oil primary amine was added, and the reaction was carried out for 2.0 hours to obtain a phosphorus-containing extreme pressure antiwear agent, which was recorded as product 5.

[0051] The following table shows the main parameters of the products 1-5 obtained by using the above-mentioned embodiments 1 to 5:

[0052]

[0053] It should be noted that in the description of the present invention, the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer" and the like indicating directions or positional relationships are based on the directions or positional relationships shown in the drawings, which are only for the convenience of description, and do not indicate or imply that the device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.

[0054] In addition, it should be noted that in the description of the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For those skilled in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0055] The term "comprise" or any other similar term is intended to cover a non-exclusive inclusion, such that a process, article, or apparatus / device that includes a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such process, article, or apparatus / device.

[0056] So far, the technical solutions of the present invention have been described in conjunction with the preferred embodiments shown in the accompanying drawings. However, it is easy for those skilled in the art to understand that the protection scope of the present invention is obviously not limited to these specific embodiments. Without departing from the principle of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will fall within the protection scope of the present invention.

Claims

1. A method for synthesizing a phosphorus-containing extreme pressure antiwear agent, characterized in that: The following steps are involved: Step S101, add excess alcohol to the phosphorus pentasulfide solution for 1-2 hours, heat to maintain the temperature at 70-80°C, and then perform sulfurization reaction for 2-4 hours; wherein the molecular formula of the alcohol is ROH; wherein R is C8H 17 ~C 12 H 25 Any fatty alcohol or a combination thereof, wherein the molar ratio of the alcohol to phosphorus pentasulfide is 6-8:1; Step S102, cooling, the sulfurization reaction is finished, the catalyst is added after the temperature is cooled to 10-30°C, and then propylene oxide is slowly added dropwise for 1-2 hours, and the temperature during the addition process is kept below 30°C, wherein the molar ratio of propylene oxide to phosphorus pentasulfide is 0.4-0.6:1; wherein the catalyst is ammonia water, and the mass ratio of ammonia water to phosphorus pentasulfide is 1:1000; Step S103, raising the temperature to 70-80°C, adding phosphorus pentoxide at a constant speed for 1-2 hours for re-esterification; wherein the molar ratio of phosphorus pentoxide to phosphorus pentasulfide is 0.9-1.1:1; Step S104, heating to 80-85°C, adding primary amine for amination reaction, and obtaining a phosphorus-containing extreme pressure anti-wear agent; wherein the primary amine is one or a mixture of the following substances: octadecylamine, soybean oil primary amine, hydrogenated tallow primary amine; the mass ratio of primary amine to phosphorus pentasulfide is 1:200-500.

Citation Information

Patent Citations

  • Preparation method of nitrogen-containing thiophosphoric acid derivative

    CN113512059A

  • Oil-soluble additive containing phosphorus and nitrogen atoms

    JP1997235578A

  • Reaction products of olefins, sulfur, aliphatic amine, alkylene oxide, phosphorus pentasulfide, and phosphorus pentoxide and lubricant compositions thereof