Additive Manufacturing Mechanical Property Defect Prediction Method Based on Non-Contact Displacement Sensing

By establishing a model database that linearly correlates sintered necks with mechanical properties, and combining it with real-time detection using non-contact displacement sensors, the problem of online prediction of mechanical properties in additive manufacturing was solved. This enabled real-time non-destructive quantitative observation and defect detection of internal microstructures, shortening the inspection cycle and reducing waste consumption.

CN116702482BActive Publication Date: 2026-11-17CHONGQING INST OF GREEN & INTELLIGENT TECH CHINESE ACAD OF SCI
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310694216.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-06-13
Publication Date
2026-11-17
Estimated Expiration
2043-06-13

AI Technical Summary

Technical Problem

Existing technologies are insufficient to meet the online prediction requirements of the mechanical properties of additively manufactured parts. They can only observe surface morphology and internal macroscopic defects, and cannot achieve real-time non-destructive quantitative observation of internal microstructure.

Method used

By establishing a model database that linearly correlates sintering necks with mechanical properties, and combining it with non-contact displacement sensors to monitor the additive manufacturing process in real time, surface contour features are collected layer by layer, the radius of the sintering neck is calculated, and a threshold is set to judge mechanical property defects, thus achieving online prediction.

Benefits of technology

It enables real-time, non-destructive, quantitative observation of mechanical properties during additive manufacturing, timely detection of critical defects, shortening of inspection cycles, and reduction of manpower and material consumption caused by scrap parts.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116702482B_ABST
    Figure CN116702482B_ABST
Patent Text Reader

Abstract

This invention provides a method for predicting mechanical property defects in additive manufacturing based on non-contact displacement sensing. By establishing a model database that linearly correlates sintering necks with mechanical properties, and combining this with a method for setting a sintering neck radius threshold and grading, the invention achieves online prediction of mechanical property defects in additive manufacturing. This not only allows for the timely detection of fatal mechanical defects to terminate manufacturing, but also records the distribution of mechanical properties at each joint of the formed part throughout the entire process, effectively reflecting whether there are other secondary weaknesses in the overall formed part, facilitating product classification and use. The online calculation of the sintering neck radius using non-contact displacement sensing, compared to conventional online detection of quality defects in additive manufacturing which can only observe surface morphology defects or internal macroscopic defects, enables real-time, non-destructive quantitative observation of the internal microstructure. Furthermore, it can cover every formed part, helping to shorten the product inspection cycle and reduce manpower and material consumption caused by scrap.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of additive manufacturing technology, and more specifically to a method for predicting mechanical property defects in additive manufacturing based on non-contact displacement sensing. Background Technology

[0002] Additive manufacturing is a manufacturing technology that uses digital models as a basis to stack materials layer by layer to form a three-dimensional structural entity. Compared with traditional subtractive manufacturing (such as machining) and equal-material manufacturing (such as casting, forging, and welding), additive manufacturing technology has irreplaceable advantages in the production of complex structural parts and has been widely used in various fields of industrial production.

[0003] With the further development and application of this technology, online prediction technology for additive manufacturing quality defects has also gradually developed. The quality assessment of additively manufactured parts includes both morphological accuracy and mechanical properties. The quality of mechanical properties is crucial to the use of the manufactured parts. For example, in the additive manufacturing of large-size precision structural parts, insufficient mechanical properties will cause rapid failure of the parts, resulting in a large waste of time and material costs.

[0004] However, existing technologies can only observe surface morphology defects in additively manufactured parts. For example, using visual inspection technologies such as industrial cameras combined with image processing, macroscopic defects such as surface collapse and deformation of additively manufactured parts can be identified; or by using thermal image information of the outer surface of the part with low spatiotemporal resolution, coarse defects such as sidewall holes and top depressions can be predicted.

[0005] Therefore, current testing methods are insufficient to meet the requirements for online prediction of the mechanical properties of additively manufactured parts. Summary of the Invention

[0006] To address the shortcomings of existing technologies, this invention provides a method for predicting mechanical property defects in additive manufacturing based on non-contact displacement sensing, thereby solving the technical problem that current detection methods are unable to meet the online prediction requirements of the mechanical properties of additively manufactured parts.

[0007] This invention provides a method for predicting mechanical property defects in additive manufacturing based on non-contact displacement sensing, comprising:

[0008] S1. Set the process parameters for additive manufacturing so that the sintering neck radius X of the formed part changes linearly, measure the mechanical properties of the formed part, and establish a model database that shows a linear relationship between the sintering neck and the mechanical properties.

[0009] S2. Based on the specific requirements for the mechanical properties of qualified parts in the formed parts, the minimum mechanical property value is obtained, the model database is queried, and the sintering neck radius Xmin corresponding to the minimum value is determined as the constraint threshold.

[0010] S3. A non-contact displacement sensor is used to detect the entire additive manufacturing process of the test part in the formed part in real time, and the surface contour features of the newly formed part of the test part are collected layer by layer;

[0011] S4. Based on the surface contour features of the transition from wave crest to wave trough in the collected information, extract the distance L between the wave crest and wave trough, and calculate the sintering neck radius X of the test piece in real time.

[0012] S5. Determine the sign of the sintering neck radius X of the test piece. If X≤0, it is determined that the sintering neck of the test piece has not been formed, and the forming process is terminated. If X>0, proceed to S6.

[0013] S6. Based on the constraint threshold, determine the mechanical property defects. If the sintering neck radius X of the test piece is less than the constraint threshold Xmin, it is determined that the mechanical properties of the corresponding area have defects, and the forming is terminated. If the sintering neck radius X of the test piece is greater than or equal to the constraint threshold Xmin, proceed to S7.

[0014] S7. Query the model database to obtain and record the mechanical property value corresponding to the sintering neck radius X of the test piece;

[0015] S8. Check the end time. If the end time has not arrived, repeat steps S4-S7. Otherwise, determine that the forming is completed normally.

[0016] Optionally, the real-time calculation of the sintering neck radius X of the test piece includes:

[0017] The calculation of the sintering neck radius X is expressed as follows:

[0018] X = floor height / 2 - L.

[0019] Optionally, setting the additive manufacturing process parameters includes:

[0020] The process parameters include at least nozzle temperature, layer height, channel spacing, filament output speed, fill rate, and printing speed.

[0021] Optionally, the step of making the sintering neck radius X of the same molded part change linearly includes:

[0022] The linear change of the sintering neck radius X needs to cover the maximum and minimum values ​​of the sintering neck radius under the process window.

[0023] Optionally, the measurement of the mechanical properties of the molded part includes:

[0024] The mechanical properties include at least tensile properties, bending properties, compressive properties, impact properties, tear properties, torsional properties, shear properties, hardness properties, notch strength and toughness impact, fracture toughness, fatigue properties, high temperature mechanical properties, corrosion brittle fracture properties, corrosion fatigue properties, wear resistance and friction properties.

[0025] Optionally, the non-contact displacement sensor includes:

[0026] The non-contact displacement sensor shown includes at least a laser sensor, a dispersive confocal sensor, a white light interferometer sensor, an ultrasonic sensor, and an eddy current sensor.

[0027] Optionally, the real-time detection of the entire additive manufacturing process of the test part in the formed part using a non-contact displacement sensor includes:

[0028] The non-contact displacement sensor is used to integrate with the additive manufacturing device to achieve synchronous scanning and detection during the additive manufacturing process.

[0029] Optionally, the non-contact displacement sensor is used for integration with the additive manufacturing apparatus, including:

[0030] The non-contact sensor is used to be directly integrated with the printhead of the additive manufacturing device; or it can be first installed on a separate single-axis or multi-axis motion mechanism, and then integrated with the additive manufacturing device along with the single-axis or multi-axis motion mechanism.

[0031] Optionally, the step of acquiring the surface contour features of the newly formed portion of the test part layer by layer includes:

[0032] The surface contour features are either two-dimensional planar features or three-dimensional solid features.

[0033] Compared with the prior art, the present invention has the following beneficial effects:

[0034] 1. By using non-contact displacement sensing to calculate the sintering neck radius online, compared with conventional additive manufacturing quality defect online detection which can only observe surface morphology defects or internal macroscopic defects, it can realize real-time non-destructive quantitative observation of internal microstructure.

[0035] 2. By establishing a model database that linearly correlates sintering neck with mechanical properties, and combining it with a method for setting a sintering neck radius threshold and a grading judgment, online prediction of mechanical property defects in additive manufacturing is realized. This not only allows for the timely detection of fatal mechanical defects so that manufacturing can be terminated, but also records the distribution of mechanical properties at each joint of the formed part throughout the entire process, effectively reflecting whether there are other secondary weaknesses in the overall formed part, which facilitates the classification and use of the product.

[0036] 3. The online non-contact non-destructive prediction method proposed in this invention can cover each molded part, which helps to shorten the product inspection cycle and reduce the manpower and material consumption caused by defective parts. Attached Figure Description

[0037] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with the invention and, together with the description, serve to explain the principles of the invention.

[0038] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, for those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0039] Figure 1 This is a schematic diagram of the method flow of the present invention;

[0040] Figure 2 This is a flowchart illustrating another embodiment of the present invention;

[0041] Figure 3 This is a schematic diagram illustrating the calculation of the sintering neck radius X using surface profile features in this invention. Detailed Implementation

[0042] To make the objectives, technical solutions, and advantages of the embodiments of this application clearer, the technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, not all embodiments. Based on the embodiments of this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application. Functional units with the same reference numerals in the examples of this invention have the same and similar structures and functions.

[0043] See Figure 1 This invention provides a method for predicting mechanical property defects in additive manufacturing based on non-contact displacement sensing, comprising:

[0044] S1. Set the process parameters for additive manufacturing so that the sintering neck radius X of the formed part changes linearly, measure the mechanical properties of the formed part, and establish a model database that shows a linear relationship between the sintering neck and the mechanical properties.

[0045] S2. Based on the specific requirements for the mechanical properties of qualified parts in the formed parts, the minimum mechanical property value is obtained, the model database is queried, and the sintering neck radius Xmin corresponding to the minimum value is determined as the constraint threshold.

[0046] S3. A non-contact displacement sensor is used to detect the entire additive manufacturing process of the test part in the formed part in real time, and the surface contour features of the newly formed part of the test part are collected layer by layer;

[0047] S4. Based on the surface contour features of the transition from wave crest to wave trough in the collected information, extract the distance L between the wave crest and wave trough, and calculate the sintering neck radius X of the test piece in real time.

[0048] S5. Determine the sign of the sintering neck radius X of the test piece. If X≤0, it is determined that the sintering neck of the test piece has not been formed, and the forming process is terminated. If X>0, proceed to S6.

[0049] S6. Based on the constraint threshold, determine the mechanical property defects. If the sintering neck radius X of the test piece is less than the constraint threshold Xmin, it is determined that the mechanical properties of the corresponding area have defects, and the forming is terminated. If the sintering neck radius X of the test piece is greater than or equal to the constraint threshold Xmin, proceed to S7.

[0050] S7. Query the model database to obtain and record the mechanical property value corresponding to the sintering neck radius X of the test piece;

[0051] S8. Check the end time. If the end time has not arrived, repeat steps S4-S7. Otherwise, determine that the forming is completed normally.

[0052] In this embodiment, the present invention establishes a model database that linearly correlates sintering neck with mechanical properties, sets a threshold for sintering neck radius and a method for grading, and performs online calculation of sintering neck radius through non-contact displacement sensing. Compared with conventional online detection of quality defects in additive manufacturing, which can only observe surface morphology defects or internal macroscopic defects, this invention can achieve real-time non-destructive quantitative observation of internal microstructure.

[0053] The present invention is specifically described as follows:

[0054] S1. Set the process parameters for additive manufacturing so that the sintering neck radius X of the formed part changes linearly, measure the mechanical properties of the formed part, and establish a model database that shows a linear relationship between the sintering neck and the mechanical properties.

[0055] First, based on the additive manufacturing process parameters, a model database is constructed to linearly correlate the sintered neck with mechanical properties. This model database serves as the basis for subsequent judgments. The additive manufacturing process parameters include at least nozzle temperature, layer height, runner spacing, filament output speed, fill rate, and printing speed. The linear variation of the sintered neck radius needs to cover the maximum and minimum values ​​of the sintered neck radius within the process window. The mechanical properties include at least tensile properties, bending properties, compressive properties, impact properties, tear properties, torsional properties, shear properties, hardness properties, notch strength and toughness impact, fracture toughness, fatigue properties, high-temperature mechanical properties, corrosion brittle fracture properties, corrosion fatigue properties, wear resistance, and friction properties.

[0056] S2. Based on the specific requirements of the mechanical properties of qualified parts, the minimum mechanical property value is obtained, and the model database is queried to determine the sintering neck radius Xmin corresponding to the minimum value as the constraint threshold.

[0057] The constraint threshold is used as a criterion for determining whether a fatal mechanical defect has occurred.

[0058] S3. A non-contact displacement sensor is used to detect the entire additive manufacturing process of the workpiece in real time, and the surface contour features of the newly formed part of the workpiece are collected layer by layer.

[0059] The contact displacement sensors used in this invention include at least laser sensors, dispersive confocal sensors, white light interferometers, ultrasonic sensors, and eddy current sensors; and the non-contact sensors are used to be directly integrated with the printhead of the additive manufacturing device; or first installed on a separate single-axis or multi-axis motion mechanism, and then integrated with the additive manufacturing device along with the single-axis or multi-axis motion mechanism; at the same time, the surface contour features collected by the non-contact displacement sensors can be two-dimensional planar features or three-dimensional features.

[0060] S4. Based on the surface contour features of the transition from wave crest to wave trough in the collected information, extract the distance L between the wave crest and wave trough, and calculate the sintering neck radius X of the test piece in real time.

[0061] S5. Determine the sign of the sintering neck radius X of the test piece. If X≤0, it is determined that the sintering neck of the test piece has not been formed, and the forming process is terminated. If X>0, proceed to S6.

[0062] S6. Based on the constraint threshold, determine the mechanical property defects. If the sintering neck radius X of the test piece is less than the constraint threshold Xmin, it is determined that the mechanical properties of the corresponding area have defects, and the forming is terminated. If the sintering neck radius X of the test piece is greater than or equal to the constraint threshold Xmin, proceed to S7.

[0063] S7. Query the model database to obtain and record the mechanical property value corresponding to the sintering neck radius X of the test piece.

[0064] S8. Check the end time. If the end time has not arrived, repeat steps S4-S7. Otherwise, determine that the forming is completed normally.

[0065] This invention establishes a model database that linearly correlates sintering necks with mechanical properties. By combining this with a method of setting a threshold for the radius of sintering necks and a grading judgment, it enables online prediction of mechanical property defects in additive manufacturing. This not only allows for the timely detection of fatal mechanical defects so that manufacturing can be terminated, but also records the distribution of mechanical properties at each joint of the formed part throughout the entire process. This effectively reflects whether there are other secondary weaknesses in the overall formed part, facilitating the classification and use of the product.

[0066] Furthermore, by using a non-contact displacement sensing method to calculate the sintering neck radius online, compared with conventional additive manufacturing quality defect online detection which can only observe surface morphology defects or internal macroscopic defects, it can achieve real-time non-destructive quantitative observation of the internal microstructure.

[0067] Meanwhile, the prediction method of the present invention can cover each molded part, which helps to shorten the product inspection cycle and reduce the manpower and material consumption caused by defective parts.

[0068] See Figure 2 In another embodiment, the present invention is described in detail, wherein the non-contact displacement sensor used in the present invention is a laser displacement sensor with a maximum measurement frequency of 1.5 kHz, a resolution of 0.03 μm, a linearity of < ±0.6 μm, and a light source of a semiconductor laser <1 mW, 670 nm (red light). This laser displacement sensor is integrated with the printhead and completes the scanning as the printhead moves. The additively manufactured part is a thin-walled long tube, and the mechanical properties involved are bending strength, specifically including the following steps:

[0069] S1. Change the channel spacing to a variation of 10μm, while keeping other process parameters fixed; according to the process window, make the sintering neck radius X of the thin-walled long tube decrease linearly from 90μm to 40μm; measure the corresponding bending strength of this batch of thin-walled long tubes to be 3.5MPa to 1MPa, that is, when X = 90μm, the bending strength is 3.5MPa, and when X = 40μm, the bending strength is 1MPa, and establish a model database of linear correlation between the sintering neck and mechanical properties.

[0070] S2. Based on the actual usage requirements of the thin-walled long tube to be tested, the minimum bending strength is known to be 2MPa; query the S1 model database to determine the sintering neck radius constraint threshold corresponding to this minimum bending strength as Xmin=60μm; once the measured sintering neck radius X is less than this constraint threshold, it is considered that there is a defect in the bending strength at that location.

[0071] S3. Conduct online prediction: throughout the additive manufacturing process of the part to be inspected, use a non-contact laser displacement sensor to collect the surface contour features of the newly formed part layer by layer online.

[0072] S4. Based on the surface contour features of the transition from wave crest to wave trough in the online information collected in S3, extract the distance L between wave crest and wave trough, and automatically calculate the sintering neck radius X = layer height / 2-L in real time.

[0073] S5. Determine the sign of the sintering neck radius X. If X≤0, it is determined that the sintering neck has not been formed, and the forming process is terminated; if X>0, proceed to S6.

[0074] S6. Based on the constraint threshold of the sintering neck radius in S2, determine the mechanical property defects: if the sintering neck radius X < 60 μm, it is determined that the mechanical properties of the corresponding area have defects, and the forming is terminated; if the sintering neck radius X ≥ 60 μm, proceed to S7.

[0075] S7. Query the model database in S1 to obtain the bending strength value corresponding to the sintering neck radius and record its value; for example, when the 4th layer is formed and the sintering neck radius X = 70μm, query S1 to find that the corresponding bending strength is 2.8MPa.

[0076] S8. Query the end time: If the end time has not arrived, return to S4; if the end time has arrived, the forming process is completed normally.

[0077] See Figure 3 Taking fused wire additive manufacturing as an example, when the layer height is 0.35mm, the distance between the peaks and valleys L = 90μm is extracted in real time based on the surface contour features of the adjacent filament bonding area collected by non-contact displacement sensing. According to the sintering radius calculation formula, the sintering radius X = 350 / 2 - 90 = 85μm can be obtained.

[0078] It should be noted that, in this document, relational terms such as "first" and "second" are used merely to distinguish one entity or operation from another, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Furthermore, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Without further limitations, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes said element.

[0079] The above description is merely a specific embodiment of the present invention, enabling those skilled in the art to understand or implement the invention. Various modifications to these embodiments will be readily apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the invention. Therefore, the present invention is not to be limited to the embodiments shown herein, but is to be accorded the widest scope consistent with the principles and novel features claimed herein.

Claims

1. A method for predicting mechanical property defects in additive manufacturing based on non-contact displacement sensing, characterized in that, include: S1. Set the process parameters for additive manufacturing, including at least nozzle temperature, layer height, runner spacing, filament output speed, fill rate, and printing speed, so that the sintering neck radius X of the formed part changes linearly. The linear change of the sintering neck radius X needs to cover the maximum and minimum values ​​of the sintering neck radius under the process window. Measure the mechanical properties of the formed part and establish a model database of linear correlation between the sintering neck and mechanical properties. S2. Based on the specific requirements for the mechanical properties of qualified parts in the formed parts, the minimum mechanical property value is obtained, the model database is queried, and the sintering neck radius Xmin corresponding to the minimum value is determined as the constraint threshold. S3. A non-contact displacement sensor is used to detect the entire additive manufacturing process of the test part in the formed part in real time, and the surface contour features of the newly formed part of the test part are collected layer by layer; S4. Based on the surface contour features of the transition from wave crest to wave trough in the collected information, the distance L between the wave crest and wave trough is extracted, and the sintering neck radius X of the test piece is calculated in real time, as shown below: X = floor height / 2 - L; S5. Determine the sign of the sintering neck radius X of the test piece. If X≤0, it is determined that the sintering neck of the test piece has not been formed, and the forming process is terminated. If X>0, proceed to S6. S6. Based on the constraint threshold, determine the mechanical property defects. If the sintering neck radius X of the test piece is less than the constraint threshold Xmin, it is determined that the mechanical properties of the corresponding area have defects, and the forming is terminated. If the sintering neck radius X of the test piece is greater than or equal to the constraint threshold Xmin, proceed to S7. S7. Query the model database to obtain and record the mechanical property value corresponding to the sintering neck radius X of the test piece; S8. Check the end time. If the end time has not arrived, repeat steps S4-S7. Otherwise, determine that the forming is completed normally.

2. The additive manufacturing mechanical property defect prediction method based on non-contact displacement sensing as described in claim 1, characterized in that, The measured mechanical properties of the molded part include: The mechanical properties include at least tensile properties, bending properties, compressive properties, impact properties, tearing properties, torsional properties, shear properties, hardness properties, impact toughness, fracture toughness, fatigue properties, high-temperature mechanical properties, corrosion brittle fracture properties, corrosion fatigue properties, wear resistance, and friction properties.

3. The additive manufacturing mechanical property defect prediction method based on non-contact displacement sensing as described in claim 1, characterized in that, The non-contact displacement sensor includes: The non-contact displacement sensor includes at least a laser sensor, a dispersive confocal sensor, a white light interferometer sensor, an ultrasonic sensor, and an eddy current sensor.

4. The additive manufacturing mechanical property defect prediction method based on non-contact displacement sensing as described in claim 1, characterized in that, The additive manufacturing process, which employs a non-contact displacement sensor to monitor the workpiece in real time, includes: The non-contact displacement sensor is used to integrate with the additive manufacturing device to achieve synchronous scanning and detection during the additive manufacturing process.

5. The additive manufacturing mechanical property defect prediction method based on non-contact displacement sensing as described in claim 4, characterized in that, The non-contact displacement sensor is used for integration with the additive manufacturing apparatus, including: The non-contact displacement sensor is used to be directly integrated with the printhead of the additive manufacturing device; or it can be first installed on a separate single-axis or multi-axis motion mechanism, and then integrated with the additive manufacturing device along with the single-axis or multi-axis motion mechanism.

6. The additive manufacturing mechanical property defect prediction method based on non-contact displacement sensing as described in any one of claims 1-5, wherein the step of acquiring the surface contour features of the newly formed portion of the workpiece layer by layer includes: The surface contour features are either two-dimensional planar features or three-dimensional solid features.

Citation Information

Patent Citations

  • Online detection method and system for surface defects of additive manufacturing part

    CN113781585A

  • Method for evaluating influence of internal defect on performance of additive manufacturing part

    CN113959829A