A flocculant and its preparation method

A type of amide is prepared by polymerizing acrylamide, cationic monomer, 2-acrylamide-2-methylpropanesulfonic acid and (E)-3-(furan-2-yl)acrylic acid in sodium hydroxide solution. The flocculants of the group, sulfonic acid group and cationic group solve the problem of poor effect of the existing flocculants and achieve efficient sewage treatment effect.

CN116715808BActive Publication Date: 2024-11-12SHANDONG NUOER BIOLOGICAL TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310798751.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-06-30
Publication Date
2024-11-12
Estimated Expiration
2043-06-30

AI Technical Summary

Technical Problem

The existing flocculants have poor effects when treating sewage, and lack an excellent flocculant and their preparation method.

Method used

The polymerization reaction of acrylamide, cationic monomer, 2-acrylamide-2-methylpropanesulfonic acid and (E)-3-(furan-2-yl)acrylic acid in sodium hydroxide solution was prepared to prepare amides Flocculants of radicals, sulfonic acid groups and cationic groups have the characteristics of being insensitive to salts, strong hydration ability and stable chemical properties.

Benefits of technology

The obtained flocculant has a significant improvement in the flocculation effect and hydration ability, and can quickly settle, improve the clarity of the upper clear liquid, reduce the moisture content of the lower mud cake, and significantly reduce CODCr and turbidity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116715808B_ABST
    Figure CN116715808B_ABST
Patent Text Reader

Abstract

The present invention relates to the technical field of polymer functional polymer compounds, and in particular to a flocculant and a preparation method thereof. An embodiment of the present invention provides a preparation method of a flocculant, comprising: dissolving acrylamide, a cationic monomer, 2-acrylamide-2-methylpropanesulfonic acid and (E)-3-(furan-2-yl) acrylic acid in a sodium hydroxide solution to obtain a polymerization solution; and subjecting the polymerization solution to a polymerization reaction to obtain the flocculant. An embodiment of the present invention provides a flocculant and a preparation method thereof, and can provide a flocculant and a preparation method thereof with excellent effects.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of polymer functional macromolecular compounds, in particular to a flocculant and a preparation method thereof. Background Art

[0002] Flocculant is a commonly used reagent for sewage treatment.

[0003] In the related art, the flocculant has poor effect.

[0004] Therefore, in view of the above shortcomings, there is an urgent need for a flocculant with excellent effect and a preparation method thereof. Summary of the invention

[0005] The embodiment of the present invention provides a flocculant and a preparation method thereof, which can provide a flocculant and a preparation method thereof with excellent effects.

[0006] In a first aspect, an embodiment of the present invention provides a method for preparing a flocculant, comprising:

[0007] dissolving acrylamide, a cationic monomer, 2-acrylamide-2-methylpropanesulfonic acid and (E)-3-(furan-2-yl)acrylic acid in a sodium hydroxide solution to obtain a polymerization solution;

[0008] The polymerization solution is subjected to a polymerization reaction to obtain the flocculant.

[0009] In one possible design, the cationic monomer is:

[0010]

[0011] In one possible design, the method for preparing the cationic monomer includes:

[0012] (1) N,N-diisopropylethylamine and 1,4-dibromobutane are mixed and reacted to obtain a prepolymer;

[0013] (2) The prepolymer and dimethylaminopropyl acrylamide are mixed to obtain the cationic monomer after reaction.

[0014] In one possible design, the molar ratio of N,N-diisopropylethylamine to 1,4-dibromobutane is (1.2-1.5):1.

[0015] In a possible design, the molar ratio of the prepolymer to the dimethylaminopropyl acrylamide is 1:(1.1-1.3).

[0016] In one possible design, the catalyst for the reaction of step (1) is at least one of dibutyltin, dibutyltin dilaurate or dibutyltin dilaurate;

[0017] The mass of the catalyst in the reaction of step (1) is 0.03% to 0.05% of the sum of the mass of N,N-diisopropylethylamine and 1,4-dibromobutane;

[0018] The reaction temperature of step (1) is 50-60° C., and the reaction time is 2-4 h;

[0019] The N,N-diisopropylethylamine and 1,4-dibromobutane in step (1) are mixed in a solvent. The solvent in step (1) is dimethyl sulfoxide, and its mass is 40%-45% of the total mass of N,N-diisopropylethylamine and 1,4-dibromobutane.

[0020] In one possible design, step (2) includes:

[0021] The prepolymer, dimethylaminopropyl acrylamide and a polymerization inhibitor are mixed in a solvent, and after the reaction, the cationic monomer is obtained by evaporation and purification through a condensation reflux device;

[0022] The polymerization inhibitor is 2,6-di-tert-butyl-p-cresol, and the mass of the polymerization inhibitor is 0.01%-0.02% of the mass of dimethylaminopropyl acrylamide;

[0023] In step (2), the solvent is dimethyl sulfoxide, and its mass is 30%-40% of the total mass of the prepolymer and dimethylaminopropyl acrylamide;

[0024] The reaction temperature in step (2) is 65-70° C., and the reaction time is 5-7 hours.

[0025] In a possible design, the polymerization solution further includes water as a solvent, a dispersant, a regulator, a high temperature initiator and a low temperature initiator;

[0026] The dispersant is ethylene (octyl polyoxyethylene) ammonium bromide;

[0027] The regulator includes at least one of dihydrogenated tallow dimethyl ammonium salt and dipalmitoyl carboxyethyl hydroxyethyl methyl sulfate ammonium salt;

[0028] The high-temperature initiator is at least one of azobisisoheptanenitrile, azobisisobutyronitrile, azobisisobutyramidine hydrochloride, and azobisisobutylimidazoline hydrochloride; the low-temperature initiator is a redox composite initiator, and the redox composite initiator includes an oxidant and a reductant; the oxidant is at least one of potassium persulfate, ammonium persulfate, peroxydiphosphate, tert-butyl peroxide, isopropylbenzene hydroperoxide, diisopropylbenzene peroxide, tert-butyl perbenzoate, and tert-amyl hydroperoxide; the reductant is at least one of sodium bisulfite, sodium pyrosulfite, thiosulfate, and ferrous sulfate.

[0029] In a possible design, the pH value of the polymerization solution is 3.8-4.2, the reaction environment of the polymerization reaction is a nitrogen environment, and the reaction temperature of the polymerization reaction is 0-2°C;

[0030] The weight proportions of the raw materials for preparing the flocculant are: 150-200 parts of acrylamide, 120-180 parts of cationic monomer, 180-200 parts of 2-acrylamide-2-methylpropanesulfonic acid, 100-120 parts of (E)-3-(furan-2-yl)acrylic acid, 5-15 parts of dispersant, 3-8 parts of regulator, 25-38 parts of sodium hydroxide, 400-600 parts of deionized water, 1-3 parts of high-temperature initiator and 1-6 parts of low-temperature initiator.

[0031] In a second aspect, an embodiment of the present invention further provides a flocculant prepared by any of the above-mentioned preparation methods.

[0032] Compared with the prior art, the present invention has at least the following beneficial effects:

[0033] In this embodiment, acrylamide, 2-acrylamide-2-methylpropanesulfonic acid, and (E)-3-(furan-2-yl) acrylic acid all have functional groups that can react with double bonds, and they all have amide groups and sulfonic acid groups. Through the reaction with cationic monomers, the obtained flocculant not only has amide groups, sulfonic acid groups, and cationic groups, but also has rigid groups, so that the polymer has positive and negative charges, and the polymer has the advantages of being insensitive to salt, having strong hydration ability, and having stable chemical properties. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0035] Figure 1 The present invention provides a flow chart of a method for preparing a flocculant. DETAILED DESCRIPTION

[0036] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0037] In the description of the embodiments of the present invention, unless otherwise clearly specified and limited, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance; unless otherwise specified or explained, the term "multiple" refers to two or more; the terms "connected" and "fixed" should be understood in a broad sense, for example, "connected" can be a fixed connection, a detachable connection, an integral connection, or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0038] like Figure 1 As shown, an embodiment of the present invention provides a method for preparing a flocculant, comprising:

[0039] dissolving acrylamide, a cationic monomer, 2-acrylamide-2-methylpropanesulfonic acid and (E)-3-(furan-2-yl)acrylic acid in a sodium hydroxide solution to obtain a polymerization solution;

[0040] The polymerization solution is subjected to polymerization reaction to obtain a flocculant.

[0041] In this embodiment, acrylamide, 2-acrylamide-2-methylpropanesulfonic acid, and (E)-3-(furan-2-yl) acrylic acid all have functional groups that can react with double bonds, and they all have amide groups and sulfonic acid groups. Through the reaction with cationic monomers, the obtained flocculant not only has amide groups, sulfonic acid groups, and cationic groups, but also has rigid groups, so that the polymer has positive and negative charges, and the polymer has the advantages of being insensitive to salt, having strong hydration ability, and having stable chemical properties.

[0042] It should be noted that after the polymerization reaction, there should be steps of filtration, washing and drying, and the washing agent is isopropanol.

[0043] In some embodiments of the present invention, the cationic monomer is:

[0044]

[0045] In this embodiment, the cationic monomer carries a double cationic group, which can hydrolyze the polymer to produce more positive charges and negative charges, and can significantly improve the flocculation effect and increase the hydration capacity.

[0046] In some embodiments of the present invention, the method for preparing the cationic monomer comprises:

[0047] (1) N,N-diisopropylethylamine and 1,4-dibromobutane are mixed and reacted to obtain a prepolymer;

[0048] (2) The prepolymer and dimethylaminopropyl acrylamide are mixed and reacted to obtain a cationic monomer.

[0049] In this embodiment, the chemical formula for the preparation process of the cationic monomer is as follows:

[0050]

[0051]

[0052] The reaction equation of the polymerization reaction of the present invention is as follows:

[0053]

[0054] In some embodiments of the present invention, the molar ratio of N,N-diisopropylethylamine to 1,4-dibromobutane is (1.2-1.5):1 (eg, 1.2:1, 1.3:1, 1.4:1 or 1.5:1).

[0055] In some embodiments of the present invention, the molar ratio of the prepolymer to dimethylaminopropyl acrylamide is 1:(1.1-1.3) (for example, it can be 1:1.1, 1:1.15, 1:1.2, 1:1.25 or 1:1.3).

[0056] In some embodiments of the present invention, the catalyst for the reaction of step (1) is at least one of dibutyltin, dibutyltin dilaurate or dibutyltin dilaurate;

[0057] The mass of the catalyst in the reaction of step (1) is 0.03% to 0.05% of the sum of the mass of N,N-diisopropylethylamine and 1,4-dibromobutane;

[0058] The reaction temperature of step (1) is 50-60° C., and the reaction time is 2-4 h;

[0059] The N,N-diisopropylethylamine and 1,4-dibromobutane in step (1) are mixed in a solvent. The solvent in step (1) is dimethyl sulfoxide, and its mass is 40%-45% of the total mass of N,N-diisopropylethylamine and 1,4-dibromobutane.

[0060] In some embodiments of the present invention, step (2) comprises:

[0061] The prepolymer, dimethylaminopropyl acrylamide and a polymerization inhibitor are mixed in a solvent, and after the reaction, the cationic monomer is obtained by evaporation and purification through a condensation reflux device;

[0062] The polymerization inhibitor is 2,6-di-tert-butyl-p-cresol, and the mass of the polymerization inhibitor is 0.01%-0.02% of the mass of dimethylaminopropyl acrylamide;

[0063] In step (2), the solvent is dimethyl sulfoxide, and its mass is 30%-40% of the total mass of the prepolymer and dimethylaminopropyl acrylamide;

[0064] The reaction temperature in step (2) is 65-70° C., and the reaction time is 5-7 hours.

[0065] In some embodiments of the present invention, the polymerization solution further includes water as a solvent, a dispersant, a regulator, a high temperature initiator and a low temperature initiator;

[0066] The dispersant is ethylene (octyl polyoxyethylene) ammonium bromide;

[0067] The conditioning agent includes at least one of dihydrogenated tallow dimethyl ammonium salt and dipalmitoyl carboxyethyl hydroxyethyl methyl sulfate ammonium salt;

[0068] The high-temperature initiator is at least one of azobisisoheptanonitrile, azobisisobutyronitrile, azobisisobutyramidine hydrochloride, and azobisisobutylimidazoline hydrochloride; the low-temperature initiator is a redox composite initiator, which includes an oxidant and a reductant; the oxidant is at least one of potassium persulfate, ammonium persulfate, peroxydiphosphate, tert-butyl peroxide, isopropylbenzene hydroperoxide, diisopropylbenzene peroxide, tert-butyl perbenzoate, and tert-amyl hydroperoxide; the reductant is at least one of sodium bisulfite, sodium pyrosulfite, thiosulfate, and ferrous sulfate.

[0069] In this embodiment, the dispersant is a Gemini-type cationic surfactant with high surface activity, so that the present invention has the ability of rapid dissolution and solubilization, and is suitable for various salt-containing and high-oil wastewater.

[0070] In some embodiments of the present invention, the pH value of the polymerization solution is 3.8 to 4.2, the reaction environment of the polymerization reaction is a nitrogen environment, and the reaction temperature of the polymerization reaction is 0 to 2°C;

[0071] The weight proportions of the raw materials for preparing the flocculant are: 150-200 parts of acrylamide (for example, 150 parts, 160 parts, 170 parts, 180 parts, 190 parts or 200 parts), 120-180 parts of cationic monomer (for example, 120 parts, 130 parts, 140 parts, 150 parts, 160 parts, 170 parts or 180 parts), 180-200 parts of 2-acrylamide-2-methylpropanesulfonic acid, 100-120 parts of (E)-3-(furan-2-yl)acrylic acid, 5-15 parts of dispersant, 3-8 parts of regulator, 25-38 parts of sodium hydroxide, 400-600 parts of deionized water, 1-3 parts of high-temperature initiator and 1-6 parts of low-temperature initiator.

[0072] It should be noted that at least one is any one or a mixture of any several in any proportion.

[0073] It should be noted that the water used as a solvent in the present application is deionized water.

[0074] The embodiment of the present invention further provides a flocculant, which is prepared by any preparation method in the above embodiments.

[0075] In order to more clearly illustrate the technical solution and advantages of the present invention, a method for preparing a flocculant is described in detail below through several embodiments.

[0076] Example 1

[0077] In this embodiment, cationic monomers and flocculants are prepared by the following method:

[0078] Preparation of cationic monomers:

[0079] (1) In a closed reaction kettle equipped with a stirrer and a thermometer, 155 parts of N,N-diisopropylethylamine, 216 parts of 1,4-dibromobutane, 140 parts of dimethyl sulfoxide, and 0.11 parts of dibutyltin dilaurate were added, nitrogen was passed through for 20 minutes, and then the reaction was sealed. The temperature was controlled at 50° C. by an electronic temperature control system, and the reaction was carried out for 2 hours to obtain a prepolymer.

[0080] (2) In a closed reaction kettle equipped with a stirrer and a thermometer, 222 parts of a cationic monomer, 110 parts of dimethylaminopropyl acrylamide, 112 parts of dimethyl sulfoxide, and 0.03 parts of 2,6-di-tert-butyl-p-cresol were added, nitrogen was passed through for 20 minutes and then the reaction was sealed. The temperature was controlled at 65° C. by an electronic temperature control system and the reaction was carried out for 5 hours. The product was placed in a condensation reflux device (rotary evaporator) and purified by evaporation to obtain a cationic monomer.

[0081] Preparation of flocculant:

[0082] The flocculant is composed of the following raw materials in parts by weight: 150 parts of acrylamide, 120 parts of cationic monomers, 180 parts of 2-acrylamide-2-methylpropanesulfonic acid, 100 parts of (E)-3-(furan-2-yl) acrylic acid, 5 parts of ethylene (octyl polyoxyethylene) ammonium bromide, 3 parts of dihydrogenated tallow dimethyl ammonium salt, 25 parts of sodium hydroxide, 400 parts of deionized water, 1 part of azobisisoheptonitrile, 0.5 parts of tert-butyl peroxide and 0.5 parts of sodium pyrosulfite.

[0083] The preparation method comprises the following steps: uniformly dissolving acrylamide, cationic monomer, (E)-3-(furan-2-yl) acrylic acid, ethylenic (octyl polyoxyethylene) ammonium bromide and dihydrogenated tallow dimethyl ammonium salt in a sodium hydroxide solution composed of deionized water and sodium hydroxide to obtain a polymerization solution, adjusting the pH value of the polymerization solution to 3.8, transferring the aqueous solution into a reaction kettle, passing nitrogen for 45 minutes to remove dissolved oxygen in the aqueous solution, cooling the aqueous solution to 0°C, adding azobisisoheptanenitrile, tert-butyl peroxide and sodium pyrosulfite to initiate polymerization, reacting for 2 hours, and obtaining a flocculant block when the reaction temperature rises to the highest temperature and does not rise any more, and granulating, drying, grinding and sieving the block to obtain a flocculant.

[0084] Example 2

[0085] In this embodiment, cationic monomers and flocculants are prepared by the following method

[0086] Preparation of cationic monomers:

[0087] (1) In a closed reaction kettle equipped with a stirrer and a thermometer, 169 parts of N,N-diisopropylethylamine, 216 parts of 1,4-dibromobutane, 149 parts of dimethyl sulfoxide, and 0.15 parts of dibutyltin dilaurate were added, nitrogen was passed through for 20 minutes, and then the reaction was sealed. The temperature was controlled at 55° C. by an electronic temperature control system, and the reaction was carried out for 3 hours to obtain a prepolymer.

[0088] (2) In a closed reaction kettle equipped with stirring, condensation reflux and a thermometer, 222 parts of cationic monomer, 120 parts of dimethylaminopropyl acrylamide, 130 parts of dimethyl sulfoxide and 0.045 parts of 2,6-di-tert-butyl-p-cresol were added, nitrogen was passed through for 20 minutes and then sealed, the temperature was controlled at 68° C. by an electronic temperature control system, the reaction was carried out for 6 hours, and the product was placed in a condensation reflux device (rotary evaporator) for purification by evaporation to obtain a cationic monomer.

[0089] Preparation of flocculant:

[0090] The flocculant is composed of the following raw materials in parts by weight: 180 parts of acrylamide, 150 parts of cationic monomers, 190 parts of 2-acrylamide-2-methylpropanesulfonic acid, 105 parts of (E)-3-(furan-2-yl) acrylic acid, 8 parts of ethylene (octyl polyoxyethylene) ammonium bromide, 5 parts of dihydrogenated tallow dimethyl ammonium salt, 29 parts of sodium hydroxide, 500 parts of deionized water, 2 parts of azobisisoheptonitrile, 1.5 parts of tert-butyl peroxide and 1.5 parts of sodium pyrosulfite.

[0091] The preparation method comprises the following steps: uniformly dissolving acrylamide, a cationic monomer, 2-acrylamide-2-methylpropanesulfonic acid, (E)-3-(furan-2-yl) acrylic acid, ethylenic (octyl polyoxyethylene) ammonium bromide and dihydrogenated tallow dimethyl ammonium salt in a sodium hydroxide solution composed of deionized water and sodium hydroxide to obtain a polymerization solution; adjusting the pH value of the polymerization solution to 4.0; transferring the aqueous solution into a reaction kettle; passing nitrogen gas for 45 minutes to remove dissolved oxygen in the aqueous solution; cooling the aqueous solution to 1°C; adding azobisisoheptanenitrile, tert-butyl peroxide and sodium pyrosulfite to initiate polymerization; reacting for 2 hours; and obtaining a flocculant block when the reaction temperature rises to the highest temperature and does not rise any more; and granulating, drying, grinding and screening the block to obtain a flocculant.

[0092] Example 3

[0093] In this embodiment, cationic monomers and flocculants are prepared by the following method

[0094] Preparation of cationic monomers:

[0095] (1) In a closed reaction kettle equipped with a stirrer and a thermometer, 195 parts of N,N-diisopropylethylamine, 216 parts of 1,4-dibromobutane, 156 parts of dimethyl sulfoxide, and 0.2 parts of dibutyltin dilaurate were added, nitrogen was passed through for 20 minutes, and then the reaction was sealed. The temperature was controlled at 60° C. by an electronic temperature control system, and the reaction was carried out for 4 hours to obtain a prepolymer.

[0096] (2) In a closed reaction kettle equipped with a stirrer and a thermometer, 222 parts of a cationic monomer, 130 parts of dimethylaminopropyl acrylamide, 150 parts of dimethyl sulfoxide, and 0.06 parts of 2,6-di-tert-butyl-p-cresol were added, nitrogen was passed through for 20 minutes and then the reaction was sealed. The temperature was controlled at 70° C. by an electronic temperature control system and the reaction was carried out for 7 hours. The product was placed in a condensation reflux device (rotary evaporator) and purified by evaporation to obtain a cationic monomer.

[0097] Preparation of flocculant:

[0098] The flocculant is composed of the following raw materials in parts by weight: 200 parts of acrylamide, 180 parts of cationic monomers, 200 parts of 2-acrylamide-2-methylpropanesulfonic acid, 110 parts of (E)-3-(furan-2-yl) acrylic acid, 10 parts of ethylene (octyl polyoxyethylene) ammonium bromide, 8 parts of dihydrogenated tallow dimethyl ammonium salt, 38 parts of sodium hydroxide, 600 parts of deionized water, 3 parts of azobisisoheptonitrile, 3 parts of tert-butyl peroxide, and 3 parts of sodium pyrosulfite.

[0099] The preparation method comprises the following steps: uniformly dissolving acrylamide, a cationic monomer, 2-acrylamide-2-methylpropanesulfonic acid, (E)-3-(furan-2-yl) acrylic acid, ethylenic (octyl polyoxyethylene) ammonium bromide and dihydrogenated tallow dimethyl ammonium salt in a sodium hydroxide solution composed of deionized water and sodium hydroxide to obtain a polymerization solution; adjusting the pH value of the polymerization solution to 4.2; transferring the aqueous solution into a reaction kettle; passing nitrogen gas for 45 minutes to remove dissolved oxygen in the aqueous solution; cooling the aqueous solution to 2°C; adding azobisisoheptanenitrile, tert-butyl peroxide and sodium pyrosulfite to initiate polymerization; reacting for 2 hours; and obtaining a flocculant block when the reaction temperature rises to the highest temperature and does not rise any more; and granulating, drying, grinding and screening the block to obtain a flocculant.

[0100] Comparative Example 1

[0101] The difference between this comparative example and Example 1 is that in this comparative example, no polymerization inhibitor 2,6-di-tert-butyl-p-cresol is added when preparing the cationic monomer, and the rest is the same as in Example 1 to prepare the flocculant.

[0102] Comparative Example 2

[0103] The difference between this comparative example and Example 1 is that in this comparative example, the catalyst dibutyltin dilaurate is not added when preparing the cationic monomer, and the rest is the same as in Example 1 to prepare the flocculant.

[0104] Comparative Example 3

[0105] The difference between this comparative example and Example 1 is that in this comparative example, no cationic monomer is added when preparing the cationic flocculant, and the amount thereof is replaced by methacryloyloxyethyltrimethylammonium chloride. The rest is the same as in Example 1 to prepare the flocculant.

[0106] Comparative Example 4

[0107] The difference between this comparative example and Example 1 is that in this comparative example, no (E)-3-(furan-2-yl) acrylic acid is added when preparing the amphoteric cationic flocculant, and its amount is replaced by acrylamide. The rest is the same as in Example 1 to prepare the flocculant.

[0108] Comparative Example 5

[0109] The difference between this comparative example and Example 1 is that in this comparative example, dihydrogenated tallow dimethyl ammonium salt is not added when preparing the cationic monomer, and the rest is the same as in Example 1 to prepare the flocculant.

[0110] Comparative Example 6

[0111] The difference between this comparative example and Example 1 is that in this comparative example, ethylene (octyl polyoxyethylene) ammonium bromide is not added when preparing the amphoteric cationic flocculant, and the rest is the same as in Example 1 to prepare the flocculant.

[0112] The effects of the flocculants prepared in the examples and the comparative examples were compared and evaluated, and at the same time, compared with the inorganic flocculants ferric chloride and aluminum chloride.

[0113] The selected wastewater to be treated is the white water from the newsprint production line of Shandong Huatai Group, with a pH value of 6.9 and a COD Cr It is 1148.3 mg / L, the turbidity is 155.3 NTU, and the sewage to be treated is maintained at 25℃.

[0114] Static sedimentation experiments were performed in a 100 ml measuring cylinder to measure the transmittance of the suspension (the upper clear liquid), sedimentation velocity and COD at different time periods. Cr And measure the floc height; COD of the sewage to be treated before and after flocculant treatment Cr The percentage of reduction is an indicator to characterize the COD reduction. Cr Rate; The percentage of turbidity reduction of the sewage to be treated before and after flocculant treatment is used as an indicator to characterize the turbidity reduction rate.

[0115] Adjust the pH value of the mud cake (lower sediment) to 6.8, raise the temperature to 40°C, stir for 5 minutes, separate the mud cake from the water, and test the moisture content of the mud cake.

[0116] The test results are as follows:

[0117]

[0118]

[0119] It can be seen from the experimental data that the sedimentation rate of the flocculant synthesized in Example 1 is above 80m / h, which is several times the sedimentation rate of inorganic flocculants such as ferric chloride and aluminum chloride; the light transmittance is above 95%; the floc height is less than 5cm; the moisture content of the mud cake is not more than 50%; the COD reduction Cr The rate of flocculation is greater than 85%; the rate of turbidity reduction is greater than 90%. Similar effects are also seen in Examples 2 and 3. It can be seen that the flocculant synthesized by the present invention has a fast flocculation speed, high clarity of the upper clear liquid, and low moisture content of the lower mud cake, and can significantly reduce COD Cr and turbidity.

[0120] By comparing Example 1 with Comparative Example 1, it can be seen that when the inhibitor 2,6-di-tert-butyl-p-cresol is not added during the preparation of the cationic monomer, the cationic monomer in the obtained flocculant is not completely reacted, the cationic group content contained in the flocculant is small, the sedimentation rate and light transmittance are significantly deteriorated, and the COD reduction is Cr The turbidity reduction rate and the turbidity reduction rate decreased, while the water content increased significantly (48% higher than that of Example 1).

[0121] By comparing Example 1 with Comparative Example 2, it can be seen that when preparing the cationic monomer, the catalyst dibutyltin dilaurate is not added, and the cationic monomer reaction in the obtained flocculant is not complete, the cationic group content contained in the flocculant is small, the sedimentation rate and light transmittance are significantly deteriorated, and the COD reduction is Cr The turbidity reduction rate and the turbidity reduction rate decreased, while the water content increased significantly (44% higher than that of Example 1).

[0122] By comparing Example 1 with Comparative Example 3, it can be seen that when preparing the cationic monomer, the cationic monomer is not added, and methacryloyloxyethyl trimethyl ammonium chloride is used instead. The obtained polyacrylamide flocculant has a smaller number of cationic groups than the flocculant, and the sedimentation rate and light transmittance are significantly worse, and the COD reduction is Cr The turbidity reduction rate and the turbidity reduction rate decreased, while the water content increased significantly (38% higher than that of Example 1).

[0123] By comparing Example 1 with Comparative Example 4, it can be seen that when preparing the cationic monomer, without adding (E)-3-(furan-2-yl) acrylic acid, the obtained flocculant lacks rigid groups, has poor sedimentation rate and transmittance, and reduces COD Cr The rate of turbidity reduction and the rate of turbidity reduction decreased, while the water content increased (19% higher than that of Example 1).

[0124] By comparing Example 1 with Comparative Example 5, it can be seen that when preparing the flocculant, without adding dihydrogenated tallow dimethyl ammonium salt, the obtained flocculant has a disordered structure, poor sedimentation rate and light transmittance, and low COD reduction. Cr The rate of turbidity reduction and the rate of turbidity reduction decreased, while the water content increased (56% higher than that of Example 1).

[0125] By comparing Example 1 with Comparative Example 6, it can be seen that when preparing the flocculant, ethylene (octyl polyoxyethylene) ammonium bromide is not added, the insoluble particles in the obtained flocculant are significantly increased, the sedimentation rate and light transmittance are poor, and the COD reduction is Cr The rate of turbidity reduction and the rate of turbidity reduction decreased, while the water content increased (75% higher than that of Example 1).

[0126] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method for preparing a flocculant, characterized in that: include: dissolving acrylamide, a cationic monomer, 2-acrylamide-2-methylpropanesulfonic acid and (E)-3-(furan-2-yl)acrylic acid in a sodium hydroxide solution to obtain a polymerization solution; Performing a polymerization reaction on the polymerization solution to obtain the flocculant; The cationic monomer is:

2. The preparation method according to claim 1, characterized in that: The preparation method of the cationic monomer comprises: (1) N,N-diisopropylethylamine and 1,4-dibromobutane are mixed and reacted to obtain a prepolymer; (2) The prepolymer and dimethylaminopropyl acrylamide are mixed to obtain the cationic monomer after reaction.

3. The preparation method according to claim 2, characterized in that: The molar ratio of N,N-diisopropylethylamine to 1,4-dibromobutane is (1.2-1.5):

1.

4. The preparation method according to claim 3, characterized in that: The molar ratio of the prepolymer to the dimethylaminopropyl acrylamide is 1:(1.1-1.3).

5. The preparation method according to claim 2, characterized in that: The catalyst for the reaction in step (1) is dibutyltin dilaurate; The mass of the catalyst in the reaction of step (1) is 0.03% to 0.05% of the sum of the mass of N,N-diisopropylethylamine and 1,4-dibromobutane; The reaction temperature of step (1) is 50-60° C., and the reaction time is 2-4 h; The N,N-diisopropylethylamine and 1,4-dibromobutane in step (1) are mixed in a solvent. The solvent in step (1) is dimethyl sulfoxide, and its mass is 40%-45% of the total mass of N,N-diisopropylethylamine and 1,4-dibromobutane.

6. The preparation method according to claim 3, characterized in that: Step (2) comprises: The prepolymer, dimethylaminopropyl acrylamide and a polymerization inhibitor are mixed in a solvent, and after the reaction, the cationic monomer is obtained by evaporation and purification through a condensation reflux device; The polymerization inhibitor is 2,6-di-tert-butyl-p-cresol, and the mass of the polymerization inhibitor is 0.01%-0.02% of the mass of dimethylaminopropyl acrylamide; In step (2), the solvent is dimethyl sulfoxide, and its mass is 30%-40% of the total mass of the prepolymer and dimethylaminopropyl acrylamide; The reaction temperature in step (2) is 65-70° C., and the reaction time is 5-7 hours.

7. The preparation method according to claim 1, characterized in that: The polymerization solution also includes water as a solvent, a dispersant, a regulator, a high-temperature initiator and a low-temperature initiator; The dispersant is ethylene (octyl polyoxyethylene) ammonium bromide; The conditioning agent includes at least one of dihydrogenated tallow dimethyl ammonium salt and dipalmitoyl carboxyethyl hydroxyethyl methyl sulfate ammonium salt; The high-temperature initiator is at least one of azobisisoheptanenitrile, azobisisobutyronitrile, azobisisobutyramidine hydrochloride, and azobisisobutylimidazoline hydrochloride; the low-temperature initiator is a redox composite initiator, and the redox composite initiator includes an oxidant and a reductant; the oxidant is at least one of potassium persulfate, ammonium persulfate, peroxydiphosphate, tert-butyl peroxide, isopropylbenzene hydroperoxide, diisopropylbenzene peroxide, tert-butyl perbenzoate, and tert-amyl hydroperoxide; the reductant is at least one of sodium bisulfite, sodium pyrosulfite, thiosulfate, and ferrous sulfate.

8. The preparation method according to claim 7, characterized in that: The pH value of the polymerization solution is 3.8-4.2, the reaction environment of the polymerization reaction is a nitrogen environment, and the reaction temperature of the polymerization reaction is 0-2°C; The weight proportions of the raw materials for preparing the flocculant are: 150-200 parts of acrylamide, 120-180 parts of cationic monomer, 180-200 parts of 2-acrylamide-2-methylpropanesulfonic acid, 100-120 parts of (E)-3-(furan-2-yl)acrylic acid, 5-15 parts of dispersant, 3-8 parts of regulator, 25-38 parts of sodium hydroxide, 400-600 parts of deionized water, 1-3 parts of high-temperature initiator and 1-6 parts of low-temperature initiator.

9. A flocculant, characterized in that: The preparation method is described in any one of claims 1 to 8.