A method for manufacturing a gate-controlled transistor and a gate-controlled transistor

By using FZ-n drift region, SiO2 layer etching and ion implantation to form an isolated structure in the gated transistor, the problem of electron enhancement injection is solved, efficient control of electronic channels and reduction of switching losses are achieved, and the performance of transistors is improved .

CN117153680BActive Publication Date: 2024-11-26SHANGHAI KUNCHENG ELECTRONIC TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311040522.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-08-17
Publication Date
2024-11-26
Estimated Expiration
2043-08-17

AI Technical Summary

Technical Problem

The prior art is difficult to implement a gated transistor manufacturing method for electronic enhanced injection, resulting in poor electronic channel control and large switching losses.

Method used

The n-drift region was made using FZ-n (100), the SiO2 layer was deposited and the left oxide layer and the right oxide layer were formed by CMD chemical dry etching, the n-type polycrystalline silicon was deposited to form the n-region, and the ion implantation and Thermal annealing forms p- and n+ regions, forming an isolation structure, and finally forming a gate and collector to ensure control of the electronic channel and enhanced injection.

Benefits of technology

The electron enhancement injection of the gated transistor is realized, which improves the control capability of the electronic channel and reduces switching losses, ensuring efficient on- and off-transmitter performance of the transistor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117153680B_ABST
    Figure CN117153680B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for manufacturing a gate-controlled transistor, comprising the following steps: using FZ-n (100) to make an n-drift region; depositing a first oxide layer of 0.3-0.7 μm on the n-drift region; the first oxide layer is a SiO2 layer; using CMD chemical dry etching to remove the middle of the first oxide layer to form a groove, and the first oxide layer is separated to form a left oxide layer and a right oxide layer; depositing n-type polysilicon on the first oxide layer to form an n region, and forming a protrusion placed in the groove in the middle of the bottom of the n region; forming a p region and an n+ region at positions corresponding to the left oxide layer and the right oxide layer; the p region above the left oxide layer is isolated from the n-drift region, and the p region above the right oxide layer is isolated from the n-drift region. After adopting the above isolation measures of the present invention, the p region is not in direct contact with the n-drift region, so the sudden conduction phenomenon that may occur between the p region, the n-drift region and the p region can be reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of transistors, and in particular to a method for manufacturing a gate-controlled transistor and the gate-controlled transistor. Background Art

[0002] At present, the new generation of high-power devices developed on the basis of IGBT - injection enhanced gate transistor (IEGT) has entered the practical stage. The rated capacity of IEGT reaches 4.5kV / 3kA. It has many advantages such as low on-state voltage, small gate drive current, high power density, low switching loss, and high speed. It can be predicted that it will be widely used in high-power converters and other fields like IGCT. IEGT is developed on the basis of IGBT. Figure 1 It can be seen that the gate width Lg of IEGT is relatively large. The conduction process of IEGT is as follows: forward bias the tube (i.e., positive voltage is applied to the collector and gate, and the emitter is grounded). GS When it reaches a certain critical value, a layer with opposite conductivity to the original semiconductor is formed on the surface of the P-type layer near SiO2, namely the N channel, which creates an electron channel between the emitter and the collector. In this way, electrons are emitted from the emitter, pass through the N+ layer and the N channel, and enter the N-base region. At the same time, holes are also emitted from the collector to the P-base region. Since the electron concentration in the N-layer is not large, some holes pass through the PN junction here and also enter the N-base region. The holes move along the direction of the electric field. Only a small part of them directly reaches the P+ layer and eventually enters the emitter, while most of the holes reach the opposite side near the gate and accumulate there. Figure 1 The accumulation layer in the N-tunnel attracts the electrons coming out of the N-tunnel, so the electron emission is enhanced, and the electron concentration in the N-base region is improved, which is the meaning of electron enhanced injection in the name of IEGT. The above process continues and eventually reaches a dynamic balance, the N-base region is filled with electrons, and the conduction process is completed.

[0003] IEGT turn-off process: When a negative voltage is applied to the gate, the N channel in the P+ base region disappears, the electron flow channel is cut off, the electron emission of the emitter stops, and the electron concentration in the N-base region drops rapidly. The electrons in the N-base region recombine with the holes here and disappear, so the hole concentration also drops significantly, and the PN junction between the P+ base region and the N-base region has a chance to recover. At this time, the hole flow path is blocked, and part of the carriers in the N-base region enters the emitter or collector, and the other part recombine in the N-base region. When the carrier concentration drops to a certain level, the turn-off process is completed. Summary of the invention

[0004] The technical problem to be solved by the present invention is to provide a method for manufacturing a gate-controlled transistor and a gate-controlled transistor, wherein the manufactured gate-controlled transistor realizes electron enhanced injection.

[0005] The technical solution adopted by the present invention to solve the above technical problem is: a method for manufacturing a gate-controlled transistor, comprising the following steps:

[0006] FZ-n (100) was used to make the n-drift region;

[0007] Depositing a first oxide layer of 0.3-0.7 μm on the n-drift region; the first oxide layer is a SiO2 layer;

[0008] CMD chemical dry etching is used to remove the middle of the first oxide layer to form a groove, and the first oxide layer is separated to form a left oxide layer and a right oxide layer;

[0009] n-type polysilicon is deposited on the first oxide layer to form an n-region, and a protrusion disposed in the groove is formed in the middle of the bottom of the n-region;

[0010] Ion implantation and thermal annealing are performed at positions corresponding to the left oxide layer and the right oxide layer to form a p region and an n+ region; the p region above the left oxide layer is isolated from the n-drift region, and the p region above the right oxide layer is isolated from the n-drift region.

[0011] Preferably, the method for manufacturing a gate-controlled transistor further comprises the following steps:

[0012] forming a second oxide layer, wherein the second oxide layer covers the n region, the p region and the n+ region;

[0013] forming a gate, wherein a side edge of the gate corresponds to an area above the n+ region;

[0014] A BPSG borophosphosilicate glass layer is deposited on the second oxide layer to cover the gate electrode;

[0015] A contact hole is opened on the BPSG borophosphosilicate glass layer to make an emitter leading out of the n+ region;

[0016] A p-region is formed under the n-drift region as a collector, or an N buffer region is formed under the n-drift region, and a p-region is formed under the N buffer region as a collector.

[0017] Preferably, the method for manufacturing a gate-controlled transistor further comprises the following step: injecting phosphorus ions into the bottom of the protrusion formed in the middle of the bottom of the n-region to form a hole blocking layer.

[0018] In a second aspect, a gate-controlled transistor is manufactured using the above-mentioned method for manufacturing a gate-controlled transistor.

[0019] Preferably, the gate-controlled transistor includes an n-drift region, a first oxide layer is formed on the n-drift region, the middle portion of the first oxide layer is removed to form a groove so as to form a left oxide layer and a right oxide layer, the first oxide layer has an n region, a protrusion placed in the groove is formed in the middle portion of the bottom of the n region, a p region is formed corresponding to the positions of the left oxide layer and the right oxide layer, an n+ region is partially formed above the p region, the p region above the left oxide layer is isolated from the n-drift region, and the p region above the right oxide layer is isolated from the n-drift region; a second oxide layer is formed on the n region, a gate is formed on the second oxide layer, and the side edge of the gate corresponds to the top of the n+ region.

[0020] Preferably, the width of the downward protrusion formed in the middle of the bottom of the n-type polysilicon layer is 1 μm.

[0021] Preferably, the edge of the left oxide layer facing the protrusion is located below the gate, and the edge of the right oxide layer facing the protrusion is located below the gate.

[0022] Preferably, a p+ region is implanted in the top between the n+ region and the edge of the n region located below the gate.

[0023] The beneficial effects of the present invention are as follows: after a positive voltage is applied to the gate, an inversion layer is formed on the top of the p region (if there is a p+ region, an inversion layer is formed on the top of the p+ region), an electron channel is formed between the n+ region and the n region, and the electrons in the n+ region enter the n region and then enter the n-drift region to the collector to turn on the transistor, and some holes accumulate at the top of the n-drift region and below the left oxide layer and the right oxide layer. In order to ensure the electrical neutrality of the n-drift region, the n+ emitter region will inject more electrons into the n-drift region, thereby enhancing the electron injection. The gate-controlled transistor of the present invention adopts a new structure and also achieves the effect of electron enhanced injection. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 It is a partial structural diagram of an existing gate-controlled transistor;

[0025] Figure 2 It is a schematic diagram of the structure of the gate-controlled transistor of the present invention. DETAILED DESCRIPTION

[0026] The present invention will now be described in further detail in conjunction with the accompanying drawings and preferred embodiments. These drawings are simplified schematic diagrams, which only illustrate the basic structure of the present invention in a schematic manner, and therefore only show the components related to the present invention.

[0027] A method for manufacturing a gate-controlled transistor comprises the following steps:

[0028] FZ-n (100) was used to make the n-drift region;

[0029] Depositing a first oxide layer of 0.3-0.7 μm on the n-drift region; the first oxide layer is a SiO2 layer;

[0030] CMD chemical dry etching is used to remove the middle of the first oxide layer to form a groove, and the first oxide layer is separated to form a left oxide layer and a right oxide layer;

[0031] n-type polysilicon is deposited on the first oxide layer to form an n-region, and a protrusion disposed in the groove is formed in the middle of the bottom of the n-region;

[0032] Ion implantation and thermal annealing are performed at positions corresponding to the left oxide layer and the right oxide layer to form a p region and an n+ region; the p region above the left oxide layer is isolated from the n-drift region, and the p region above the right oxide layer is isolated from the n-drift region.

[0033] Specifically, in an optional implementation manner, the method for manufacturing a gate-controlled transistor further includes the following steps:

[0034] forming a second oxide layer, wherein the second oxide layer covers the n region, the p region and the n+ region;

[0035] forming a gate, wherein a side edge of the gate corresponds to an area above the n+ region;

[0036] A BPSG borophosphosilicate glass layer is deposited on the second oxide layer to cover the gate electrode;

[0037] A contact hole is opened on the BPSG borophosphosilicate glass layer to make an emitter leading out of the n+ region;

[0038] A p-region is formed under the n-drift region as a collector, or an N buffer region is formed under the n-drift region, and a p-region is formed under the N buffer region as a collector.

[0039] Specifically, in an optional embodiment, the method for manufacturing a gate-controlled transistor further includes the following step: injecting phosphorus ions into the bottom of a protrusion formed in the middle of the bottom of the n region to form a hole blocking layer for blocking holes in the n-drift region from entering the n region.

[0040] The first oxide layer is separated by deposition and chemical etching to form a left oxide layer, a right oxide layer and a groove. Compared with using a Si3N4 mask deposited on SiO2 and a LOCOS oxidation process to perform local thermal growth of SiO2, the spacing between the left oxide layer and the right oxide layer formed by the LOCOS oxidation process is difficult to accurately control. The present invention does not require a LOCOS oxidation process, and the present invention can accurately control the width of the protrusion only by deposition and chemical etching.

[0041] The p region above the left oxide layer is isolated from the n-drift region, and the p region above the right oxide layer is isolated from the n-drift region. In some existing structures, the p region is in contact with the n-drift region, so the PN junction there may be suddenly turned on, causing the entire transistor to suddenly turn off. After adopting the above isolation measures of the present invention, the p region is not in direct contact with the n-drift region, so the sudden conduction phenomenon that may occur between the p region, the n-drift region and the p-region can be reduced.

[0042] like Figure 2 As shown, a gate-controlled transistor includes an n-drift region, a first oxide layer is formed on the n-drift region, the middle of the first oxide layer is removed to form a groove so as to form a left oxide layer and a right oxide layer, the first oxide layer has an n region, a protrusion placed in the groove is formed in the middle of the bottom of the n region, a p region is formed corresponding to the position of the left oxide layer and the right oxide layer, an n+ region is partially formed above the p region, the p region above the left oxide layer is isolated from the n-drift region, and the p region above the right oxide layer is isolated from the n-drift region; a second oxide layer is formed on the n region, a gate is formed on the second oxide layer, and the side edge of the gate corresponds to the top of the n+ region.

[0043] Specifically, in an optional implementation manner, the width of the downward protrusion formed in the middle of the bottom of the n-type polysilicon layer is 1 μm.

[0044] Specifically, in an optional implementation manner, the edge of the left oxide layer facing the protrusion is located below the gate, and the edge of the right oxide layer facing the protrusion is located below the gate.

[0045] Specifically, in an optional implementation manner, a p+ region is implanted in the top portion between the n+ region and the edge of the n region located below the gate.

[0046] The working principle of the gate-controlled transistor of the present invention is as follows: after a positive voltage is applied to the gate, an inversion layer is formed on the top of the p region (if there is a p+ region, the inversion layer is formed on the top of the p+ region), an electron channel is formed between the n+ region and the n region, and the electrons in the n+ region enter the n region and then enter the n-drift region to the collector to turn on the transistor, and some holes accumulate at the top of the n-drift region and below the left oxide layer and the right oxide layer. In order to ensure the electrical neutrality of the n-drift region, the n+ emitter region will inject more electrons into the n-drift region, thereby enhancing the electron injection and achieving the effect of electron enhanced injection. After a negative voltage is applied to the gate, the inversion layer formed on the top of the p region disappears (if there is a p+ region, the inversion layer formed on the top of the p+ region disappears), the electron channel formed between the n+ region and the n region is disconnected, and the transistor is disconnected.

[0047] The above description only describes the specific implementation mode of the present invention. Various examples do not limit the essential content of the present invention. After reading the description, ordinary technicians in the relevant technical field can modify or deform the specific implementation modes described above without departing from the essence and scope of the invention.

Claims

1. A method for manufacturing a gate-controlled transistor, characterized in that: The steps include: FZ-n (100) was used to make the n-drift region; Depositing a first oxide layer of 0.3-0.7 μm on the n-drift region; the first oxide layer is a SiO2 layer; CMD chemical dry etching is used to remove the middle of the first oxide layer to form a groove, and the first oxide layer is separated to form a left oxide layer and a right oxide layer; n-type polysilicon is deposited on the first oxide layer to form an n-region, and a protrusion disposed in the groove is formed in the middle of the bottom of the n-region; Ion implantation and thermal annealing are performed at positions corresponding to the left oxide layer and the right oxide layer to form a p region and an n+ region; the p region above the left oxide layer is isolated from the n-drift region, and the p region above the right oxide layer is isolated from the n-drift region; forming a second oxide layer, wherein the second oxide layer covers the n region, the p region and the n+ region; forming a gate, wherein a side edge of the gate corresponds to an area above the n+ region; implanting phosphorus ions into the bottom of a protrusion formed in the middle of the bottom of the n region to form a hole blocking layer; The gate-controlled transistor includes an n-drift region, a first oxide layer is formed on the n-drift region, a middle portion of the first oxide layer is removed to form a groove so as to form a left oxide layer and a right oxide layer, an n region is provided on the first oxide layer, a protrusion placed in the groove is formed in the middle portion of the bottom of the n region, a p region is formed corresponding to the position of the left oxide layer and the right oxide layer, an n+ region is partially formed above the p region, the p region above the left oxide layer is isolated from the n-drift region, and the p region above the right oxide layer is isolated from the n-drift region; a second oxide layer is formed on the n region, a gate is formed on the second oxide layer, and a side edge of the gate corresponds to the top of the n+ region.

2. The method for manufacturing a gate-controlled transistor according to claim 1, characterized in that: The following steps are also included: A BPSG borophosphosilicate glass layer is deposited on the second oxide layer to cover the gate electrode; A contact hole is opened on the BPSG borophosphosilicate glass layer to make an emitter leading out of the n+ region; A p-region is formed under the n-drift region as a collector, or an N buffer region is formed under the n-drift region, and a p-region is formed under the N buffer region as a collector.

3. A gate-controlled transistor manufactured by the method for manufacturing a gate-controlled transistor according to any one of claims 1 to 2.

4. The gate-controlled transistor according to claim 3, characterized in that: The width of the downward protrusion formed in the middle of the bottom of the n-type polysilicon layer is 1 μm.

5. The gate-controlled transistor according to claim 3, characterized in that: The edge of the left oxide layer facing the protrusion is located below the gate electrode, and the edge of the right oxide layer facing the protrusion is located below the gate electrode.

6. The gate-controlled transistor according to claim 3, characterized in that: A p+ region is implanted on the top between the n+ region and the edge of the n region under the gate.