Test structure, semiconductor device, wafer, electronic product and method

By designing a test structure that reduces metal density, and using alternately set test metal block gaps to reduce thermal stress during laser cutting, the problem of dielectric layer delamination caused by stress in the wafer test structure is solved, and more efficient inter-metal dielectric striking is achieved. Penetration testing and device stability.

CN117174695BActive Publication Date: 2024-10-15HONOR DEVICE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311414400.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-10-30
Publication Date
2024-10-15
Estimated Expiration
2043-10-30

AI Technical Summary

Technical Problem

The existing wafer test structure causes delamination of the low dielectric constant dielectric layer inside the chip due to stress during laser cutting, resulting in device failure.

Method used

Design a test structure that reduces the metal density and uses alternating first test metal blocks and second test metal blocks to form gaps to reduce thermal stress conduction and ensure that low dielectric constant materials do not delaminate due to thermal expansion coefficient mismatch. .

Benefits of technology

It effectively reduces the thermal stress during laser cutting, prevents the delamination of low-dielectric constant materials inside the chip, maintains device stability, and improves the accuracy and reliability of inter-metal dielectric breakdown testing within the same area.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117174695B_ABST
    Figure CN117174695B_ABST
Patent Text Reader

Abstract

The embodiments of the present application provide a test structure, a semiconductor device, a wafer, an electronic product and a method, wherein the test structure comprises: at least one first metal pad coupled to a high-level voltage; at least one second metal pad coupled to a low-level voltage, each second metal pad being alternately arranged with the first metal pad, and an interlayer dielectric being accommodated between adjacent first metal pads and second metal pads; a plurality of test layers fixed in the interlayer dielectric between adjacent first metal pads and second metal pads, each of the test layers comprising: a first test metal block and a second test metal block alternately arranged. The present application reduces the metal density of the test structure, thereby generating less thermal stress during subsequent laser cutting, and the generated heat is not easily conducted to the inside of the chip, and the low dielectric constant material inside the chip is not easily delaminated due to the mismatch of the thermal expansion coefficient.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the semiconductor field, and specifically to a test structure, a semiconductor device, a wafer, an electronic product and a method. Background Art

[0002] The chip wafer-level reliability test structure is generally used to monitor the process stability of the wafer production line and identify qualified chips before the wafer is sent to the packaging plant. During the design stage, some test structures are usually designed in the wafer's scribe grooves, including some device-related and metal routing-related structures. Through electrical measurement, data analysis, and data distribution on the wafer, the process stability and volatility of the production line are judged. Since the wafer test structure is generally placed in the scribe groove, when the subsequent packaging plant cuts, whether it is laser cutting or knife cutting, the wafer test structure will generally be touched. In the existing wafer test structure, due to stress during cutting, such as thermal stress generated by the heat generated by the laser, it will act on the inside of the chip, and it is easy for the low dielectric constant dielectric layer inside the chip to be delaminated, thereby causing device failure. Therefore, there are many deficiencies. Summary of the invention

[0003] In order to solve the problem of device failure caused by dielectric layer delamination due to stress in current wafer test structures, the embodiments of the present application provide a test structure, a semiconductor device, a wafer, an electronic product and a method. By reducing the metal density of the test structure, the thermal stress generated during subsequent laser cutting is smaller, and the generated heat is not easily conducted to the inside of the chip. The low dielectric constant material inside the chip is not easily delaminated due to the mismatch of thermal expansion coefficients.

[0004] A first aspect of the present application provides a test structure, comprising: at least one first metal pad, coupled to a high-level voltage; at least one second metal pad, coupled to a low-level voltage, each second metal pad being alternately arranged with the first metal pad, and an interlayer dielectric being accommodated between adjacent first metal pads and second metal pads; a plurality of test layers, fixed in the interlayer dielectric between adjacent first metal pads and second metal pads, each of the test layers comprising: a first test metal block and a second test metal block alternately arranged at intervals; wherein the first test metal block is coupled to the first metal pad, and the second test metal block is coupled to the second metal pad.

[0005] In the present application, the test layer between the first metal pad and the second metal pad is configured as a first test metal block and a second test metal block that are alternately arranged at intervals. The first test metal block is coupled to a high level, and the second test metal block is coupled to a low level, so that a breakdown test is performed between the two metal blocks, and a wafer-level metal-to-metal dielectric breakdown test can be achieved. Since a gap is formed between the first test metal block and the second test metal block, compared with configuring a complete test metal layer structure between the first metal pad and the second metal pad, the metal density is greatly reduced, and the effective side length of the metal is not reduced. The probability of effectively capturing production line abnormalities has basically not changed. At the same time, due to the reduced metal density, the thermal stress generated during subsequent laser cutting is small, and the generated heat is not easily conducted to the inside of the chip. The low dielectric constant material inside the chip is not easily stratified due to the mismatch of the coefficient of thermal expansion (CTE).

[0006] In some embodiments, the number of the first metal pads and the number of the second metal pads are the same or different.

[0007] Specifically, the number of the first metal pads is N, the number of the second metal pads is N+1, and N is an integer greater than or equal to 1. In this way, when N is equal to 1, the test structure of the present application includes two second metal pads and one first metal pad, and a structure of 2 groups of test units can be formed. From this point of view, this embodiment can form a structure of 2N groups of test units, so that the test structure of the present application can be extended to more metal pads, thereby achieving a further increase in the effective side length of the metal, thereby increasing the probability of capturing metal-to-metal dielectric anomalies in the production line.

[0008] Specifically, the number of the first metal pads is N, the number of the second metal pads is N, and N is an integer greater than or equal to 1. In this way, when N is equal to 2, the test structure of the present application includes two second metal pads and two first metal pads, and a structure of three groups of test units can be formed. From this point of view, this embodiment can form a structure of 2N-1 groups of test units, so that the test structure of the present application can be extended to more metal pads, thereby achieving a further increase in the effective side length of the metal, thereby increasing the probability of capturing intermetallic dielectric anomalies in the production line.

[0009] In some embodiments, the number of the first metal pads is N+1, and the number of the second metal pads is N, where N is an integer greater than or equal to 1. Thus, when N is equal to 1, the test structure of the present application includes two first metal pads and one first metal pad, and a structure of 2 groups of test units can be formed. Therefore, the present embodiment can form a structure of 2N groups of test units, so that the test structure of the present application can be extended to more metal pads, thereby achieving a further increase in the effective side length of the metal, thereby increasing the probability of capturing intermetallic dielectric anomalies in the production line.

[0010] In some embodiments, in at least a portion of the test layer, the number of the first test metal blocks and the number of the second test metal blocks are the same or different.

[0011] For example, in some embodiments, in at least part of the test layer, the number of the first test metal blocks is M, and the number of the second test metal blocks is M+1. In this way, a test gap is formed between 2M first test metal blocks and the second test metal blocks, and a metal-to-metal dielectric breakdown test can be performed in the test gap.

[0012] The intermetallic dielectric (IMD) structure is used to characterize the weak links of the intermetallic dielectric in the back-end process (BEOL). The currently commonly used intermetallic dielectric (IMD) breakdown test structure is to pressurize the structure of all layers at the same time during the test. Generally, the breakdown mainly occurs at the small spacing between the metals in the same layer and the misalignment defects of the two metal layers. The implementation method of the present application forms 2M test gaps by forming 2M test gaps between the first test metal blocks and the second test metal blocks. Since the first test metal block is coupled to a high level and the second test metal block is coupled to a low level, after the alternating setting, the gap forms a certain voltage difference, and the intermetallic dielectric (IMD) breakdown test can be performed by continuously adjusting the applied voltage.

[0013] In some embodiments, in at least part of the test layer, the number of the first test metal blocks is M, the number of the second test metal blocks is M, and M is an integer greater than or equal to 1. In this way, 2M+1 test gaps between the first test metal block and the second test metal block can be formed between the first metal pad and the second metal pad, and the metal interlayer dielectric breakdown test can be performed in the test gap. The embodiment of the present application forms 2M+1 test gaps by forming 2M+1 test gaps between the first test metal block and the second test metal block. Since the first test metal block is coupled to a high level and the second test metal block is coupled to a low level, after the alternating setting, the gap forms a certain voltage difference, and the metal interlayer dielectric (IMD) breakdown test can be performed by continuously adjusting the applied voltage.

[0014] In some embodiments, in at least one test layer, the test metal block adjacent to the first metal pad is the second test metal block, and the test metal block adjacent to the second metal pad is the first test metal block. In this way, since the first test metal block is coupled to a high level and the second test metal block is coupled to a low level, and the first metal pad is coupled to a high level and the second metal pad is coupled to a low level, after such a setting, the first metal pad and the second test metal block also form a high-low level difference, so that the first metal pad and the adjacent test metal block can also perform an intermetallic dielectric (IMD) breakdown test by continuously adjusting the applied voltage.

[0015] In some embodiments, in the same test layer, all the first test metal blocks have the same length, and / or all the second test metal blocks have the same length. In this embodiment, all the first test metal blocks have the same length, or all the second test metal blocks have the same length. On the one hand, the same etching parameters can be used for etching during production, without the need for step-by-step etching, which simplifies the production process. On the other hand, the first test metal blocks or second test metal blocks of equal length have the same effect on voltage, so there is no need to consider the effect of resistance factors such as length on voltage output during testing, thereby making the test results of the intermetallic dielectric (IMD) breakdown test more accurate and the measured breakdown voltage more precise.

[0016] In some embodiments, each test layer includes at least two first test metal blocks of different lengths, and / or each test layer includes at least two second test metal blocks of different lengths. In this way, multiple different tests can be performed in the same test structure, and the second test metal blocks of different lengths can be set to adjust different metal densities and metal effective side lengths. For example, part of the first test metal blocks or part of the second test metal blocks can be set to a longer structure, so that the metal effective side length can be increased to a certain multiple of the original, and the metal density can be adjusted as needed.

[0017] In some embodiments, the lengths of all the first test metal blocks and the second test metal blocks are the same, and in two adjacent test layers, the position of the first test metal block is set in the upper test layer, and the position of the second test metal block is set in the corresponding test layer in the lower layer. In this way, the positive projection of the position of the first test metal block coupled to the high point level in the upper test layer overlaps with the positive projection of the position of the second test metal block coupled to the low level in the lower test layer, so that a high-low voltage difference is formed between the two, so that the metal dielectric breakdown test can also be performed, thereby realizing the metal dielectric breakdown test between the upper and lower layers.

[0018] In some embodiments, in each test layer, the length of K first test metal blocks is the first length, the length of NK first test metal blocks is the second length, K is a positive integer less than or equal to N / 2, and N is the number of first test metal blocks; wherein the K first test metal blocks of the first length are separated by at least one first test metal block of the second length. In this way, first test metal blocks of different lengths can be set separately.

[0019] In some embodiments, the length of the second test metal block is different from the length of the first test metal block. In this way, the metal density and the effective metal side length can be adjusted as needed, providing a higher degree of freedom for adjusting the metal density and the effective metal side length.

[0020] In some embodiments, each of the test layers further includes: a first metal layer and a second metal layer, the first metal layer includes a first connector for electrically connecting to the first test metal block, and the second metal layer includes a second connector for electrically connecting to the second test metal block. In this way, the first test metal block is coupled to the first metal pad through the first connector, so that a high level can be applied to the first test metal block through the first metal pad, and a low level can be applied to the second test metal block through the second metal pad, thereby completing the metal-to-metal dielectric breakdown test of the first test metal block and the second test metal block.

[0021] In some embodiments, the spacing between the adjacent first test metal blocks and the second test metal blocks is the same or different. In this way, when the spacing is different, the metal dielectric thickness is higher, which is more difficult to break down. Therefore, the dielectric breakdown can be tested by the thickness of the spacing, and the breakdown effect of different dielectric thicknesses can be tested. The metal dielectric thickness between the test metal blocks with the same spacing is the same, so that the influencing factors of the breakdown test can be uniformed, and the difference in the breakdown effect of different positions can be tested under the same voltage.

[0022] In some embodiments, the multi-layer test layer is the top metal layer of the semiconductor device, and / or the thickness of each test layer is greater than or equal to 3 microns. In this way, the embodiments of the present application can be applied to devices whose back-end metal dielectric is a low-k (k<3.9) material to prevent damage to the chip during cutting, and to the metal dielectric breakdown test structure design where the back-end metal interconnect dielectric layer is an ultra-thick metal layer (generally about 3um) of a low-k material to prevent cracks in the dielectric during cutting.

[0023] A second aspect of the present application provides a semiconductor device, including a substrate, and a semiconductor structure formed on the substrate and the test structure as described above.

[0024] The semiconductor device provided by the present application, because it includes the above-mentioned test structure, can realize the basic function of monitoring metal dielectric defects in the production line. Compared with the traditional metal-to-metal dielectric breakdown test structure, within the same area, the metal density of the new metal-to-metal dielectric breakdown test structure is reduced to 55% of the original, but the effective side length of the metal has not decreased, which is basically the same as the original. The probability of being able to capture abnormal production line situations has not changed basically. Since this structure reduces the metal density, the thermal stress generated during subsequent laser cutting is small, and the generated heat is not easily conducted to the inside of the chip. The low k material inside the chip is not easy to be delaminated due to CTE mismatch.

[0025] A third aspect of the present application provides an electronic product, including a housing, multiple functional hardware, and the semiconductor device as described above.

[0026] The multifunctional hardware may include functional hardware such as cameras, displays, microphones and gyroscopes. The thermal stress generated by the above-mentioned semiconductor devices during the laser cutting process is small, so the low-k material inside the chip is not easily delaminated due to CTE mismatch, which can ensure the stability of the subsequent use of the product.

[0027] A fourth aspect of the present application provides a semiconductor wafer, including a wafer panel, in which a plurality of semiconductor devices as described above are formed.

[0028] The multifunctional hardware may include functional hardware such as cameras, displays, microphones and gyroscopes. The thermal stress generated by the above-mentioned semiconductor devices during the laser cutting process is small, so the low-k material inside the chip is not easily delaminated due to CTE mismatch, which can ensure the stability of the subsequent use of the product.

[0029] A fifth aspect of the present application provides a method for performing a metal-to-metal dielectric breakdown test using the test structure as described above, comprising:

[0030] Writing a high level voltage to the first metal pad and a first test metal block in each test layer, and writing a low level voltage to the second metal pad and a second test metal block in each test layer;

[0031] The test structure is used to monitor the stability of the metal interconnect medium of the production line.

[0032] Specifically, in some embodiments, the potential difference between the two metal pads can be gradually increased from 0, and the current between the two metal pads can be tested. When the current rises sharply, the potential difference between the two metal pads (that is, the potential difference between the adjacent first test metal block and the second test metal block) can be considered as the breakdown voltage of the interlayer dielectric. The measured breakdown voltage is compared with the threshold range to monitor the stability of the metal interconnect medium of the production line. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] Figure 1 A schematic diagram of a process structure for configuring a test structure in a scribe line before wafer dicing provided for an example technology;

[0034] Figure 2 A schematic diagram of the process structure when the scribe line is opened after wafer dicing provided for the exemplary technology;

[0035] Figure 3 A schematic diagram of a test structure used as a comparison for this application;

[0036] Figure 4 Based on Figure 3 Schematic diagram of the defect photo shown;

[0037] Figure 5 This is one of the test structure schematic diagrams in the implementation mode of this application;

[0038] Figure 6 This is the second test structure schematic diagram in the implementation mode of the present application;

[0039] Figure 7 This is the third test structure schematic diagram in the implementation manner of this application;

[0040] Figure 8 This is the fourth test structure schematic diagram in the implementation manner of the present application;

[0041] Fig. 9 This is the fifth test structure schematic diagram in the implementation manner of the present application;

[0042] Fig.10 It is a schematic diagram of the flow chart of the testing method in the embodiment of the present application;

[0043] Fig.11 One of the structural schematic diagrams of a semiconductor wafer including the test structure provided in the embodiment of the present application;

[0044] Fig.12 The second structural schematic diagram of a semiconductor wafer including the test structure provided in the embodiment of the present application;

[0045] Fig.13 A top view of a semiconductor wafer provided in accordance with an embodiment of the present application.

[0046] Figure numerals: 20 - test structure, vx - etch stop layer, 11 - first metal pad, 12 - second metal pad, 21 - metal strip, 22 - first test metal block, 23 - second test metal block, 24 - first metal layer, 25 - first connector, 26 - second metal layer, 27 - second connector, 28 - cross-structure metal connection layer. DETAILED DESCRIPTION

[0047] In order to make the purpose, technical solution and advantages of the implementation mode of the present application clearer, the specific technical solution of the present application will be further described in detail below in conjunction with the drawings in the implementation mode of the present application. The following implementation mode is used to illustrate the present application, but is not used to limit the scope of the present application.

[0048] Figure 1 The schematic diagram of the structure before wafer cutting is shown. Figure 2 The schematic diagram of the structure after wafer cutting is shown. Figure 1 and Figure 2 As shown, during the design stage, some test structures 20 are usually designed in the wafer's scribe grooves, including some device-related and metal routing-related structures. Electrical measurements, data analysis, and data distribution on the wafer are used to determine the process stability and volatility of the production line. Since the wafer test structure is generally placed in the scribe groove, when the subsequent packaging plant cuts, whether it is laser cutting or knife cutting, the test structure 20 will generally be touched. On a wafer, hundreds or thousands of chips are usually formed, and there will be a certain gap between them, such as 60μm to 150μm, and this gap is called a cutting groove. After the semiconductor manufacturing process is completed and the test chip is tested, these chips are cut from the wafer along the cutting groove to form a separate chip. In some embodiments, the test structure 20 of the present application is located in the chip area, and the structure for detecting defects in the intermetallic dielectric layer is located in the cutting groove area, which can save chip area.

[0049] Figure 3 FIG. 1 shows a schematic diagram of a test structure for metal-to-metal dielectric breakdown in an example technology. Figure 4 The schematic diagram of the metal interlayer dielectric being broken down is shown in FIG. Figure 3As shown, the structure is a comb-to-comb comb structure, and the long metal strips 21 are staggered with the first metal pad 11 and the second metal pad 12 to meet the minimum size of the metal spacing and metal size in the design rules. This test structure is used for ultra-thick metal layers (UTM for short), which can be about 3um and are the top metal of the chip. In the specific test, the first metal pad 11 of this structure is connected to a high voltage, and the second metal pad 12 is grounded. By sweeping the voltage from low to high, the test current changes with the voltage until the intermetallic dielectric occurs as shown in the following example. Figure 4 The breakdown shown in the figure completes the metal-to-metal dielectric breakdown test, but the test structure is prone to cause delamination of the dielectric layer with low dielectric constant inside the chip during laser cutting, and the cause of this phenomenon has not been found yet.

[0050] After research, the inventors of the present application found that the high metal density of the scribe groove is an important reason affecting the delamination of the back-end dielectric layer. If the test structure in the scribe groove is an area with relatively high metal density, and the back-end metal dielectric layer of the chip is made of low-k (k<3.9, low Young's modulus, low hardness, low toughness, and insufficient adhesion to the underlying material) material, due to stress, such as thermal stress generated by the heat generated by the laser, it will act on the inside of the chip. If this stress is greater than the adhesion between the materials, delamination is likely to occur in the low-k dielectric layer inside the chip, thereby causing device failure.

[0051] Based on the above findings of the inventors of this application, this application designs a new type of metal dielectric breakdown test structure by reducing the metal density of the test structure. This structure generates less thermal stress during subsequent laser cutting, and the generated heat is not easily conducted to the inside of the chip. The low dielectric constant material inside the chip is also not easily delaminated due to the mismatch of the thermal expansion coefficient.

[0052] In order to detect defects in the interlayer dielectric, the embodiment of the present application provides a test structure for detecting interlayer dielectric defects. Through the special design of the structure, the structure can detect defects generated in the metal interlayer dielectric under certain process conditions. When the structure for detecting interlayer dielectric defects and the chip to be produced are manufactured on the same wafer, the stability of the metal interconnect medium of the production line is monitored by using the test structure.

[0053] According to some embodiments of the present application, Figure 5A structural schematic diagram of a test structure is shown, including: a first metal pad 11, coupled to a high-level voltage; a second metal pad 12, coupled to a low-level voltage, the second metal pad 12 and the first metal pad 11 are alternately arranged, and an interlayer dielectric is accommodated between the first metal pad 11 and the second metal pad 12; a plurality of test layers, fixed in the interlayer dielectric between the first metal pad 11 and the second metal pad 12, each of the test layers including: a first test metal block 22 and a second test metal block 23 alternately arranged at intervals; wherein the first test metal block 22 is coupled to the first metal pad 11, and the second test metal block 23 is coupled to the second metal pad 12.

[0054] In the present application, the test layer between the first metal pad 11 and the second metal pad 12 is configured as a first test metal block 22 and a second test metal block 23 that are alternately arranged. The first test metal block 22 is coupled to a high level, and the second test metal block 23 is coupled to a low level, so that the breakdown test is performed between the two metal blocks, and a wafer-level metal-to-metal dielectric breakdown test can be achieved. Since a gap is formed between the first test metal block 22 and the second test metal block 23, compared with configuring a complete test metal layer structure between the first metal pad 11 and the second metal pad 12, the metal density is greatly reduced, and the effective side length of the metal is not reduced. The probability of effectively capturing the abnormal situation of the production line has basically not changed. At the same time, due to the reduction in metal density, the thermal stress generated during subsequent laser cutting is small, and the generated heat is not easily conducted to the inside of the chip. The low dielectric constant material inside the chip is not easily delaminated due to the mismatch of the coefficient of thermal expansion (CTE).

[0055] It should be noted that the embodiments of the present application can be used in devices whose back-end metal dielectric is a low-k (k<3.9) material to prevent damage to the chip during cutting.

[0056] In addition, the embodiments of the present application can be used for performance testing of interlayer dielectrics. Specifically, in the process of integrated circuit manufacturing, a multi-layer metal interconnect structure is usually used to achieve circuit connection. Dielectric materials, so-called interlayer dielectrics (IMDs), are used between multilayer metal interconnects to achieve electrical isolation. Commonly used dielectric materials include silicon oxide and low dielectric constant (low-k) materials. However, due to the complexity of semiconductor manufacturing processes, it is easy to form defects in the interlayer dielectric, such as cracks, pinholes, particles, etc., which affect the dielectric properties of the interlayer dielectric, causing leakage, and leading to yield and reliability problems.

[0057] In the embodiment of the present application, the material of the test metal block (including the first test metal block 22 and the second test metal block 23 mentioned above) may include aluminum and / or copper, but the present application is not limited thereto, and the test metal block may also be other suitable materials in the art.

[0058] In the embodiment of the present application, the material of the interlayer dielectric is silicon oxide or a low-k material.

[0059] In the embodiment of the present application, the metal density is the sum of the metal areas between the first metal pad 11 and the second metal pad 12 / the total area between the first metal pad 11 and the second metal pad 12 .

[0060] In the embodiment of the present application, the effective metal side length is the sum of the relative metal side lengths of the first test metal block 22 and the adjacent second test metal block 23 .

[0061] Please continue to combine Figure 5 As shown, when the test structure of the present application is used specifically, a high level is connected through the first metal pad 11, and a low level is connected through the second metal pad 12. At the same time, the first test metal block 22 is coupled to the first metal pad 11, and the second test metal block 23 is coupled to the second metal pad 12, so that the voltage of the first metal pad 11 and the first test metal block 22 is high, and the voltage of the second metal pad 12 and the second test metal block 23 is low. Since the first test metal block 22 and the second test metal block 23 are alternately arranged, a voltage difference is formed therebetween. By continuously adjusting the applied voltage, the size of the voltage difference can be controlled to achieve a breakdown voltage test of the gap between the first test metal block 22 and the second test metal block 23.

[0062] During the specific test, different test voltages are applied to the first metal pad 11 and the second metal pad 12. Since the first metal pad 11 is electrically connected to the first test metal block 22, and the second metal pad 12 is electrically connected to the second test metal block 23, different test voltages are applied to detect the current between the adjacent first test metal block 22 and the second test metal block 23. For example, the steps of applying the test voltage and monitoring the current can be performed through the first metal pad 11 and the second metal pad 12, and then judging whether there is a defect in the dielectric layer based on the current.

[0063] Specifically, in some embodiments, the potential difference between the two metal pads can be gradually increased from 0, and the current between the two metal pads can be tested. When the current rises sharply, the potential difference between the two metal pads (that is, the potential difference between the adjacent first test metal block 22 and the second test metal block 23) can be considered as the breakdown voltage of the interlayer dielectric. The measured breakdown voltage is compared with the threshold range. When the breakdown voltage is less than the above threshold, the production line may be unstable.

[0064] It should be noted that the above threshold range can be determined according to specific processes and dielectric materials, and can also be determined by testing the breakdown voltage of an interlayer dielectric without defects determined by other means.

[0065] In other embodiments, a preset test voltage may be applied between two metal pads, and the voltage value may be kept constant to test the change of the current between the two metal pads over time. If there are defects in the interlayer dielectric, metal (such as copper) will diffuse into it and form a conductive path in the interlayer dielectric. In this case, if the test current increases significantly with the increase of the pressure test time, it means that the insulation performance of the interlayer dielectric has decreased significantly and there are defects in the interlayer dielectric.

[0066] In order to further expand the test structure of the present application to more metal pads, increase the effective side length of the metal, and thus increase the probability of capturing the abnormality of the dielectric between metals in the production line, Figure 6 The embodiment of the present application is extended based on the test structure, such as Figure 6 As shown, in the implementation manner of the present application, two or more (more than two implementation manners are not shown in this application due to the length of the drawings) test structures can be combined together to form a structure. Specifically, three different implementation manners can be included at this time: 1. The number of first metal pads 11 and second metal pads 12 is equal, 2. The number of first metal pads 11 is one more than the number of second metal pads 12, and 3. The number of second metal pads 12 is one more than the number of first metal pads 11.

[0067] The above three implementation modes are described in detail below.

[0068] 1. The number of the first metal pads 11 and the second metal pads 12 is equal:

[0069] Figure 5 and Figure 8 FIG. 1 shows a schematic diagram of a structure in which the number of first metal pads 11 and second metal pads 12 is equal in the embodiment of the present application. Figure 7As shown, in this embodiment, the number of the first metal pads 11 is N, and the number of the second metal pads 12 is N, where N is an integer greater than or equal to 1. In this way, when N is equal to 2, the test structure of the present application includes two second metal pads 12 and two first metal pads 11, and a structure of three groups of test units can be formed. From this point of view, this embodiment can form a structure of 2N-1 groups of test units, so that the test structure of the present application can be extended to more metal pads, thereby achieving a further increase in the effective side length of the metal, thereby increasing the probability of capturing intermetallic dielectric anomalies in the production line.

[0070] 2. The number of the first metal pad 11 is one more than the number of the second metal pad 12:

[0071] Figure 7 FIG. 1 shows a schematic diagram of a structure in which the number of the first metal pad 11 is one more than the number of the second metal pad 12 in an embodiment of the present application, as shown in FIG. Figure 8 As shown, in this embodiment, the number of the first metal pads 11 is N+1, and the number of the second metal pads 12 is N, where N is an integer greater than or equal to 1. In this way, when N is equal to 1, the test structure of the present application includes two first metal pads 11 and one first metal pad 11, and a structure of 2 groups of test units can be formed. From this point of view, this embodiment can form a structure of 2N groups of test units, so that the test structure of the present application can be extended to more metal pads, thereby achieving a further increase in the effective side length of the metal, thereby increasing the probability of capturing metal-to-metal dielectric anomalies in the production line.

[0072] 3. The number of the second metal pads 12 is one more than the number of the first metal pads 11:

[0073] Figure 6 FIG. 1 shows a schematic diagram of a structure in which the number of the second metal pad 12 is one more than the number of the first metal pad 11 in an embodiment of the present application, as shown in FIG. Figure 6 As shown, in this embodiment, the number of the first metal pads 11 is N, and the number of the second metal pads 12 is N+1, where N is an integer greater than or equal to 1. In this way, when N is equal to 1, the test structure of the present application includes two second metal pads 12 and one first metal pad 11, and a structure of two groups of test units can be formed. From this point of view, this embodiment can form a structure of 2N groups of test units, so that the test structure of the present application can be extended to more metal pads, thereby achieving a further increase in the effective side length of the metal, thereby increasing the probability of capturing intermetallic dielectric anomalies in the production line.

[0074] It should be noted that in the above structure, in order not to introduce unnecessary voltage access pins, all first metal pads 11 can be electrically connected on the top layer through the cross-structure metal connection layer 28, so that each first metal pad 11 can be written with a high level. Similarly, all second metal pads 12 can be electrically connected on the bottom layer through the cross-structure metal connection layer 28, so that each second metal pad 12 can be written with a low level.

[0075] The first test metal block 22 and the second test metal block 23 of the present application are described in detail below.

[0076] Figures 5 to 8 One of the schematic diagrams showing the number of the first test metal blocks 22 and the second test metal blocks 23 of the present application is shown. Specifically, the present application can be set in at least part of the test layer, and the number of the first test metal blocks 22 is M ( Figures 5 to 8 Where M is equal to 2), the number of the second test metal blocks 23 is M+1. In this way, 2M test gaps are formed between the first test metal blocks 22 and the second test metal blocks 23, and the metal-to-metal dielectric breakdown test can be performed in the test gap. The intermetallic dielectric (IMD) structure is used to characterize the weak links of the intermetallic dielectric in the back-end process (BEOL). The currently commonly used intermetallic dielectric (IMD) breakdown test structure is to pressurize the structure of all layers at the same time during the test. Generally, the breakdown mainly occurs at the small spacing of the metal in the same layer and the misalignment defects of the two metal layers. The embodiment of the present application forms 2M test gaps by forming test gaps between 2M first test metal blocks 22 and the second test metal blocks 23. Since the first test metal block 22 is coupled to a high level and the second test metal block 23 is coupled to a low level, after the alternating setting, the gap forms a certain voltage difference, and the intermetallic dielectric (IMD) breakdown test can be performed by continuously adjusting the applied voltage.

[0077] at the same time, Figures 5 to 8 In the illustrated embodiment, since the number of the second test metal blocks 23 is one more than the number of the first test metal blocks 22, it is equivalent to that the second test metal blocks 23 are located at the first and last in a test layer when arranged, and the middle part is the alternation of the first test metal blocks 22 and the second test metal blocks 23, so that at this time one of the second test metal blocks 23 is close to the first metal pad 11, and at this time since the first metal pad 11 is coupled to a high-level voltage and the second test metal block 23 is coupled to a low-level voltage, the first and last test metal blocks (both second test metal blocks 23) located in a test layer form a high-low voltage difference with one of the metal pads, so that a breakdown test of the dielectric between metal layers can also be performed.

[0078] Fig. 9 It is shown that in at least part of the test layer, the number of the first test metal blocks 22 is M ( Fig. 9 Where M is equal to 2), the number of the second test metal blocks 23 is M, and M is an integer greater than or equal to 1. In this way, 2M+1 test gaps between the first test metal block 22 and the second test metal block 23 can be formed between the first metal pad 11 and the second metal pad 12, and the metal-to-metal dielectric breakdown test can be performed in the test gaps. The embodiment of the present application forms 2M+1 test gaps by forming 2M+1 test gaps between the first test metal block 22 and the second test metal block 23. Since the first test metal block 22 is coupled to a high level and the second test metal block 23 is coupled to a low level, after the alternating setting, the gap forms a certain voltage difference, and the metal-to-metal dielectric (IMD) breakdown test can be performed by continuously adjusting the applied voltage.

[0079] according to Fig. 9 In the embodiment shown, since the first test metal layer and the second test metal layer are both M, it is equivalent to that when the first one in a test layer is the first test metal layer, the last one in a test layer is the second test metal layer, and vice versa, when the first one is the second test metal layer, the last one is the first test metal layer, and the middle part is the alternation of the first test metal block 22 and the second test metal block 23, so there are two situations at this time, one is that the test metal block close to the first metal pad 11 is the first test metal block 22, and the test metal block close to the second metal pad 12 is the second metal block. In this case, since the first test metal block 22 and the first metal pad 11 are both coupled to a high level, and the second test metal block 23 and the second metal pad 12 are coupled to a low level, no voltage difference is formed between the two, so the first metal pad 11 and the second metal pad 12 are connected. First, no breakdown test will be performed between the test metal blocks 22; second, the test metal block close to the first metal pad 11 is the second test metal block 23, and the test metal block close to the second metal pad 12 is the first metal block. In this case, since the first test metal block 22 and the first metal pad 11 are both coupled to a high level, and the second test metal block 23 and the second metal pad 12 are coupled to a low level, a voltage difference is formed between the first metal pad 11 and the second test metal block 23, and between the second metal pad 12 and the first test metal block 22. Therefore, the first and last test metal blocks (both are the second test metal blocks 23) located in a test layer form a high and low voltage difference with one of the metal pads, so that the first metal pad 11 and the adjacent test metal blocks can also perform an intermetallic dielectric (IMD) breakdown test by continuously adjusting the applied voltage.

[0080] Similarly, the number of the first test metal blocks 22 may be set to M+1, and the number of the second test metal blocks 23 may be set to M, which will not be elaborated in this application.

[0081] also, Figures 5 to 8 It can be seen that in the same test layer, all the first test metal blocks 22 have the same length, and / or, all the second test metal blocks have the same length. In this embodiment, all the first test metal blocks 22 have the same length, or all the second test metal blocks 23 have the same length. On the one hand, the same etching parameters can be used for etching during production, without the need for step-by-step etching, which simplifies the production process. On the other hand, the first test metal blocks 22 or the second test metal blocks 23 of equal length have the same effect on the voltage. Therefore, during the test, there is no need to consider the effect of resistance factors such as length on the voltage output, thereby making the test results of the intermetallic dielectric (IMD) breakdown test more accurate and the measured breakdown voltage more precise.

[0082] Fig. 9 A schematic diagram of the test structure provided in the embodiment of the present application is shown. Fig.12 As shown, the present application can also set the lengths of the test metal blocks to be different, that is, each test layer includes at least two first test metal blocks 22 with different lengths, and / or, each test layer includes at least two second test metal blocks 23 with different lengths. In this way, multiple different tests can be performed in the same test structure, and the second test metal blocks 23 with different lengths can be set to adjust different metal densities and metal effective side lengths. For example, part of the first test metal blocks 22 or part of the second test metal blocks 23 can be set to be a longer structure, so that the metal effective side length can be increased to a certain multiple of the original, and the metal density can be adjusted as needed.

[0083] Since the test structure provided by the present application includes multiple test layers, the influence between the adjacent upper and lower test layers can be further considered. In this embodiment, the lengths of all the first test metal blocks 22 and the second test metal blocks 23 are the same, and in the two adjacent test layers, the position of the first test metal block 22 is set in the test layer located in the upper layer, and the position of the second test metal block 23 is set in the test layer located in the lower layer. In this way, the positive projection of the position of the first test metal block 22 coupled to the high point level in the upper test layer overlaps with the position of the second test metal block 23 coupled to the low level in the lower test layer, so that a high and low voltage difference is formed between the two, so the metal dielectric breakdown test can also be performed, thereby realizing the upper and lower metal dielectric breakdown test.

[0084] Please continue to see Fig. 9As shown, it can be seen that the local metal density of the test metal block with a longer length is greater. Therefore, in order to ensure the uniformity of the local metal density and the effective metal side length, in some embodiments of the present application, in each test layer, the length of K first test metal blocks 22 is the first length, the length of NK first test metal blocks 22 is the second length, K is a positive integer less than or equal to N / 2, and N is the number of first test metal blocks 22; wherein the K first test metal blocks 22 of the first length are separated by at least one first test metal block 22 of the second length. In this way, the first test metal blocks 22 of different lengths can be set separately, so that the situation where the local metal density is high and the metal effective side length is longer and the metal density is low and the metal effective side length is shorter in other places will not occur, and the uniformity of the local metal density and the effective metal side length is ensured.

[0085] It can be seen from the above embodiments that in the present application, the length of the second test metal block 23 is different from the length of the first test metal block 22. In this way, the metal density and the effective metal side length can be adjusted as needed, providing a higher degree of freedom for adjusting the metal density and the effective metal side length.

[0086] Please continue to combine Figure 5 As shown, the coupling method in the embodiment of the present application can be specifically achieved by etching vias on the metal layer and the test metal block, then depositing conductive metal in the vias, and then leading the metal layer to the metal pad or a voltage terminal, so as to achieve the coupling of high and low voltages of the test metal block. In this embodiment, each test layer also includes: a first metal layer 24 and a second metal layer 26, the first metal layer 24 includes a first connector 25 for electrically connecting to the first test metal block 22, and the second metal layer 26 includes a second connector 27 for electrically connecting to the second test metal block 23. In this way, the first test metal block 22 is coupled to the first metal pad 11 through the first connector 25, so that a high level can be applied to the first test metal block 22 through the first metal pad 11, and a low level can be applied to the second test metal block 23 through the second metal pad 12, so as to complete the metal-to-metal dielectric breakdown test of the first test metal block 22 and the second test metal block 23.

[0087] Furthermore, in the embodiment of the present application, the spacing between the adjacent first test metal blocks 22 and the second test metal blocks 23 is the same, and the minimum spacing size in the design rules should be adopted, so that the breakdown voltage under the most stringent structural conditions can be detected.

[0088] Furthermore, the embodiments of the present application can be applied to devices whose back-end metal dielectric is a low-k (k<3.9) material, that is, on the one hand, it can be used for the top metal layer of the chip, and the multi-layer test layer is the top metal layer of the semiconductor device, and / or the thickness of each test layer is greater than or equal to 3 microns. In this way, the embodiments of the present application can be applied to devices whose back-end metal dielectric is a low-k (k<3.9) material to prevent damage to the chip during cutting, and can be applied to ultra-thick metal layers (generally around 3um), that is, the top metal of the chip.

[0089] The following is the application Figure 5 The embodiment shown in the figure is further described in detail. Figure 5 In the embodiment shown, the original UTM metal is in the shape of comb to comb strips, and the UTM of the new structure is in the shape of a square. The voltage applied to each metal square is opposite to that of the adjacent square. For example, the first metal pad 11 is connected to a low voltage, and the second metal pad 12 is connected to a high voltage. The high voltage end is connected to the first metal pad 11 through the lower metal layer (i.e., the first metal layer 24) and the top through hole (with a first connector 25), and the low voltage end is connected to the second metal pad 12 through the lower metal layer (i.e., the second metal layer 26) and the lower through hole (with a second connector 27). Since there is space between each metal square in the new structure, the metal density is small, from 45.9% of the metal density of the original structure to 25.5% of the new structure. Similarly, the first metal pad 11 is connected to a high voltage, and the second metal pad 12 is connected to a low voltage. In the new structure, since each metal block and the surrounding metal blocks can capture the abnormality of the metal dielectric of the production line, through calculation, the effective metal side length of the new structure (that is, the metal side length that can detect the breakdown of the metal dielectric of the production line) is 1.09 times that of the original structure, which is basically the same as the original structure, but the metal density is only 55% of the original structure. Such a structure not only meets the demand for the effective metal side length (the longer the metal side length, the easier it is to capture the abnormality of the production line), but also reduces the metal density, reducing the risk of low k dielectric layer delamination during cutting. This wafer-level intermetallic dielectric breakdown test structure can realize the basic function of monitoring the defects of the metal dielectric of the production line, and compared with the traditional intermetallic dielectric breakdown test structure, within the same area, the metal density of the new intermetallic dielectric breakdown test structure is reduced to 55% of the original, but the effective metal side length has not decreased, which is basically the same as the original. The probability of being able to capture the abnormality of the production line has basically not changed. This structure reduces the metal density, so the thermal stress generated during subsequent laser cutting is small, and the generated heat is not easily transferred to the inside of the chip. The low-k material inside the chip is not easily delaminated due to CTE mismatch.

[0090] exist Fig. 9In the embodiment shown, the square test metal block is changed into a rectangular shape, the effective side length of the metal in this design is 1.17 times of the original one, and the metal density is 30%, which is reduced to 55% of the original one. The risk of cutting cracks can also be reduced.

[0091] Fig.11 and Fig.12 The embodiment of the present application provides Figure 5 A1-A2 cross-sectional view, where Fig.11 It is a cross-sectional view from B1 to B2. Fig.12 is a cross-sectional view from A2 to A1, such as Fig.11 and Fig.12 As shown, the test structure forms M1-Mn test layers, V1-Vn are the first metal layer and the second metal layer corresponding to each test layer, for example, V1 is the first metal layer and the second metal layer corresponding to the M1 test layer, V2 is the first metal layer and the second metal layer corresponding to the M2 test layer, UTM is an ultra-thick metal layer in this structure, and this application will not go into details here.

[0092] Specifically, the semiconductor device is obtained by cutting a semiconductor wafer, and the test structure is included inside the semiconductor device. The semiconductor device provided by the present application, because it includes the above-mentioned test structure, can realize the basic function of monitoring metal dielectric defects in the production line. Compared with the traditional metal-to-metal dielectric breakdown test structure, within the same area, the metal density of the new metal-to-metal dielectric breakdown test structure is reduced to 55% of the original, but the effective side length of the metal has not decreased, which is basically the same as the original. The probability of being able to capture the abnormal situation of the production line has basically not changed. Since this structure reduces the metal density, the thermal stress generated during subsequent laser cutting is small, and the generated heat is not easily conducted to the inside of the chip. The low k material inside the chip is not easy to be delaminated due to CTE mismatch.

[0093] Fig.13 A semiconductor wafer provided in an embodiment of the present application is shown, and the semiconductor wafer is used to manufacture the semiconductor device in the above embodiment. Specifically, the semiconductor wafer is subjected to layer-by-layer masking and etching to form a layer structure of the semiconductor device, and then a plurality of semiconductor devices are obtained by cutting on the semiconductor wafer, wherein a test structure is placed in the scribe groove.

[0094] An electronic product provided in an embodiment of the present application includes a housing, multiple functional hardware, and the semiconductor device as described above.

[0095] The multifunctional hardware may include functional hardware such as cameras, displays, microphones and gyroscopes. The thermal stress generated by the above-mentioned semiconductor devices during the laser cutting process is small, so the low-k material inside the chip is not easily delaminated due to CTE mismatch, which can ensure the stability of the subsequent use of the product.

[0096] Fig.10 The present invention shows a method for performing a metal-to-metal dielectric breakdown test using the fixed test structure in the above embodiment, including:

[0097] S1: writing a high level voltage to the first metal pad and a first test metal block in each test layer, and writing a low level voltage to the second metal pad and a second test metal block in each test layer;

[0098] S2: Using the test structure, monitor the stability of the metal interconnect medium of the production line. It can be understood that when the test structure of the present application is used specifically, the first metal pad is connected to a high level, and the second metal pad is connected to a low level. At the same time, the first test metal block is coupled to the first metal pad, and the second test metal block is coupled to the second metal pad, so that the voltage of the first metal pad and the first test metal block is high, and the voltage of the second metal pad and the second test metal block is low. Since the first test metal block and the second test metal block are alternately arranged, a voltage difference is formed between the two. By continuously adjusting the applied voltage, the size of the voltage difference can be controlled to achieve the breakdown voltage test of the gap between the first test metal block and the second test metal block. If no defects are detected in the interlayer dielectric in all gaps in a test layer, it can be considered that other semiconductor devices arranged in the same layer in the chip produced at the same time do not have interlayer dielectric defects.

[0099] During the specific test, different test voltages are applied to the first metal pad and the second metal pad. Since the first metal pad is electrically connected to the first test metal block, and the second metal pad is electrically connected to the second test metal block, different test voltages are applied to detect the current between the adjacent first test metal block and the second test metal block. For example, the steps of applying the test voltage and monitoring the current can be performed through the first metal pad and the second metal pad, and then judging whether there is a defect in the dielectric layer based on the current.

[0100] Specifically, in some embodiments, the potential difference between the two metal pads can be gradually increased from 0, and the current between the two metal pads can be tested. When the current rises sharply, the potential difference between the two metal pads (that is, the potential difference between the adjacent first test metal block and the second test metal block) can be considered as the breakdown voltage of the interlayer dielectric. The measured breakdown voltage is compared with the threshold range. When the breakdown voltage is less than the above threshold, it is considered that there is a defect in the interlayer dielectric between the first metal pad and the second metal pad. This is because after the dielectric layer defect occurs, metal (such as copper) will diffuse into it to form a conductive path or reduce the effective isolation distance.

[0101] In combination with the test method for reliability analysis of the interlayer dielectric in the embodiment of the present application, the test method at least includes the following steps:

[0102] 1) A test structure is provided, the test structure comprising: at least one first metal pad coupled to a high level voltage; at least one second metal pad coupled to a low level voltage, each second metal pad is alternately arranged with the first metal pad, and an interlayer dielectric is accommodated between adjacent first metal pads and second metal pads; multiple test layers are fixed in the interlayer dielectric between adjacent first metal pads and second metal pads, each of the test layers comprises: a first test metal block and a second test metal block alternately arranged; wherein the first test metal block is coupled to the first metal pad, and the second test metal block is coupled to the second metal pad.

[0103] 2) applying a bias voltage to the first metal pad, the second metal pad, all first test metal blocks, and all second test metal blocks, and detecting the readout values ​​of the first metal pad, the second metal pad, all first test metal blocks, and all second test metal blocks, thereby detecting the interlayer dielectric located between the first metal pad and the second metal pad.

[0104] It should be noted that the test structure provided in the present test method is consistent with the test structure described in the above-mentioned test structure implementation mode of the present application, wherein, for the specific description of the test structure, please refer to the above-mentioned implementation mode, which will not be repeated here one by one.

[0105] The voltage ramp methodology and the time dependent dielectric breakdown voltage (TDDB) method can be applied to the reliability inspection of the interlayer dielectric.

[0106] The voltage boost method is to apply a voltage that increases in a constant step to both ends of the interlayer dielectric (i.e., the first metal pad, the second metal pad, all the first test metal blocks, and all the second test metal blocks), and continuously detect the current read value. When the voltage increases to a certain level, the interlayer dielectric is broken down, and then the reliability of the tested interlayer dielectric is evaluated based on the corresponding read value data recorded in this process. This test result can usually also reflect the number of defects in the material.

[0107] The time-based dielectric breakdown voltage (TDDB) is when the test structure is in the ambient temperature range of 80 to 150°C, a constant high voltage is applied to the test structure (i.e., the first metal pad, the second metal pad, all the first test metal blocks, and all the second test metal blocks), and the current reading value is continuously detected. After a period of time, if the detected dielectric layer leakage (current reading value) exceeds a certain predetermined value, it is considered that the dielectric layer has failed, and the time point is recorded. It is the time to failure (TTF) of this test sample. Based on the TTF values ​​of the time to failure of a large number of samples, the actual service life (lifetime) of the dielectric layer corresponding to the tested structure under normal working conditions can be calculated through the model, thereby evaluating the reliability of the tested interlayer dielectric.

[0108] It can be seen that the above-mentioned implementation method of the present application can realize the basic function of monitoring metal dielectric defects in the production line, and compared with the traditional metal-to-metal dielectric breakdown test structure, within the same area, the metal density of the new metal-to-metal dielectric breakdown test structure is reduced to 55% of the original, but the effective side length of the metal has not decreased, which is basically the same as before. The probability of being able to capture abnormal production line situations has not changed basically. Since this structure reduces the metal density, the thermal stress generated during subsequent laser cutting is small, and the generated heat is not easily conducted to the inside of the chip. The low k material inside the chip is not easy to be delaminated due to CTE mismatch.

[0109] The above embodiments are merely illustrative of the principles and effects of the present application and are not intended to limit the present application. Anyone familiar with the technology may modify or change the above embodiments without violating the spirit and scope of the present application. Therefore, all equivalent modifications or changes made by a person of ordinary skill in the art without departing from the spirit and technical ideas disclosed in the present application shall still be covered by the claims of the present application.

Claims

1. A test structure, It is characterized in that Applied to devices whose back-end metal dielectric is low-k material to prevent damage to the chip during cutting, including: At least one first metal pad coupled to a high level voltage; at least one second metal pad coupled to a low level voltage, each second metal pad being arranged alternately with the first metal pad, and an interlayer dielectric being accommodated between adjacent first metal pads and second metal pads; A multi-layer test layer is fixed in the interlayer dielectric between the adjacent first metal pad and the second metal pad, each of the test layers comprising: a first test metal block and a second test metal block arranged alternately at intervals; The first test metal block is coupled to the first metal pad, the second test metal block is coupled to the second metal pad, the test structure is used for performance testing of interlayer dielectrics, and a breakdown test is performed between the two metal blocks, so that a wafer-level metal-to-metal dielectric breakdown test can be achieved; Each of the test layers also includes: a first metal layer and a second metal layer, the first metal layer comprising a first connector for electrically connecting to the first test metal block, and the second metal layer comprising a second connector for electrically connecting to the second test metal block, so as to apply a high level to the first test metal block through the first metal pad and apply a low level to the second test metal block through the second metal pad; In two adjacent test layers, the position of the first test metal block is set in the upper test layer, and the position of the second test metal block is set correspondingly in the lower test layer. The position of the first test metal block coupled to the high point in the upper test layer overlaps with the positive projection of the position of the second test metal block coupled to the low level in the lower test layer.

2. The test structure according to claim 1, It is characterized in that The number of the first metal pads and the number of the second metal pads are the same or different.

3. The test structure according to claim 1, It is characterized in that In at least a portion of the test layer, the number of the first test metal blocks and the number of the second test metal blocks are the same or different.

4. The test structure according to claim 2, It is characterized in that The number of the first metal pads is N, and the number of the second metal pads is N+1; or, the number of the first metal pads is N, and the number of the second metal pads is N, where N is an integer greater than or equal to 1; or, the number of the first metal pads is N+1, and the number of the second metal pads is N, where N is an integer greater than or equal to 1.

5. The test structure according to claim 3, It is characterized in that In at least part of the test layer, the number of the first test metal blocks is M, and the number of the second test metal blocks is M+1; or, the number of the first test metal blocks is M, and the number of the second test metal blocks is M; or, the number of the first test metal blocks is M+1, and the number of the second test metal blocks is M, where M is an integer greater than or equal to 1.

6. The test structure according to claim 3, It is characterized in that The number of the first test metal blocks is M, the number of the second test metal blocks is M, and in at least one test layer, the test metal block adjacent to the first metal pad is the second test metal block, and the test metal block adjacent to the second metal pad is the first test metal block.

7. The test structure according to claim 1, It is characterized in that In each test layer, the length of K first test metal blocks is the first length, the length of NK first test metal blocks is the second length, K is a positive integer less than or equal to N / 2, and N is the number of first test metal blocks; The K first test metal blocks of the first length are spaced apart by at least one first test metal block of the second length.

8. The test structure according to any one of claims 1 to 7, It is characterized in that The intervals between adjacent first test metal blocks and second test metal blocks are the same or different.

9. The test structure according to any one of claims 1 to 7, Features , the multi-layer test layer is the top metal layer of the semiconductor device, and / or the thickness of each test layer is greater than or equal to 3 microns.

10. A semiconductor device, It is characterized in that The invention comprises a substrate, a semiconductor structure formed on the substrate and a test structure as claimed in any one of claims 1 to 9.

11. An electronic product, It is characterized in that The invention comprises a housing, various functional hardware and the semiconductor device as claimed in claim 10.

12. A semiconductor wafer, It is characterized in that A wafer panel is provided, wherein a plurality of semiconductor devices as claimed in claim 10 are formed in the wafer panel.

13. A method for performing a metal-to-metal dielectric breakdown test using the test structure according to any one of claims 1 to 9, It is characterized in that include: Writing a high level voltage to the first metal pad and a first test metal block in each test layer, and writing a low level voltage to the second metal pad and a second test metal block in each test layer; The test structure is used to monitor the stability of the metal interconnect medium of the production line.