A method for preparing outer layer circuit of carrier board
By forming pads and circuit patterns on the outside of the carrier plate and bonding them to the carrier plate, the problems of cumbersome and insufficient precision of the outer circuit preparation process of the carrier plate in the prior art are solved, and the production efficiency of the carrier plate is improved and Product stability.
Patent Information
- Application Number
- CN202311325018.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-10-13
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2043-10-13
AI Technical Summary
In the prior art, the preparation process of the outer layer line of the carrier plate is cumbersome, the production line is lengthened and the accuracy of the outer layer line cannot be guaranteed, resulting in the risk of defects caused by the internal device line after packaging, reducing product stability.
The pad is formed on the protective film outside the carrier plate, and the circuit grooves are etched out by hot melt adhesive to form a circuit pattern. Then the pad is bonded to the carrier plate, and the protective film and hot melt adhesive are used to load. The pads and circuit patterns are formed on the outside of the board, so that the preparation and packaging of the circuit patterns are carried out simultaneously.
It improves the connection and packaging efficiency of the carrier board, improves the production efficiency of the carrier board, ensures the accuracy and stability of the outer circuit, and reduces the risk of defects caused by the packaged circuit.
Smart Images

Figure CN117395894B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor carrier circuit preparation, and in particular to a method for preparing an outer layer circuit of a carrier. Background Art
[0002] The carrier board is the packaging substrate, which provides support, heat dissipation and protection for the chip, and is a key carrier in the packaging and testing of PCB products. The carrier board can be divided into hard packaging substrates (BT resin / ABF resin / MIS), flexible packaging substrates and ceramic packaging substrates. During the packaging process, the carrier board not only needs to protect and package the internal devices, but also needs to ensure that the pads in the internal devices are led out through the outer layer circuit to ensure that the internal devices can achieve normal electrical connection after packaging.
[0003] In the prior art, the outer layer circuit is directly formed on the carrier, which makes the preparation process of the carrier more complicated, lengthens the production line, and cannot guarantee the accuracy of the outer layer circuit, resulting in the risk of circuit lead-out defects in the internal devices after packaging, reducing product stability. Summary of the invention
[0004] The present invention aims to solve at least one of the problems in the related art to a certain extent. To this end, the purpose of the present invention is to provide a method for preparing an outer layer circuit of a carrier board, generate a circuit pattern on the outer side of the carrier board, and then bond it in the carrier board through a pad, thereby improving the connection and packaging efficiency of the carrier board, thereby improving the production efficiency of the carrier board.
[0005] In order to achieve the above-mentioned purpose, the present application adopts the following technical solution: a method for preparing an outer layer circuit of a carrier board, comprising:
[0006] forming a pad on the protective film;
[0007] Coating hot melt adhesive on the protective film and etching circuit grooves in the hot melt adhesive;
[0008] Electroplating the circuit groove to form a circuit pattern, wherein the circuit pattern is electrically connected to the pad;
[0009] Remove the protective film and connect the pads to the carrier board.
[0010] Furthermore, the circuit groove is prepared by laser processing.
[0011] Furthermore, a pad is formed on the protective film by a laser 3D forming process.
[0012] Furthermore, before forming the pad on the protective film, the method further includes: performing a roughening treatment on the protective film.
[0013] Furthermore, before etching the circuit grooves in the hot melt adhesive, the method further includes: mechanically grinding the solidified hot melt adhesive.
[0014] Furthermore, the mechanical grinding is performed in a grinding liquid, and the grinding liquid includes abrasive particles, a dispersant, a modifier and a surfactant.
[0015] Further, the circuit groove is electroplated to form a circuit pattern, including:
[0016] Depositing an initial copper layer at the bottom of the circuit groove by vapor deposition;
[0017] The circuit pattern is formed by horizontal electroplating on the initial copper layer.
[0018] Further, horizontal electroplating is performed on the initial copper layer to form a circuit pattern, specifically comprising:
[0019] The support frame is fixedly connected to the line groove, and the support frame includes a top plate, and probes arranged on one side of the top plate corresponding to the line grooves one by one. When the top plate is located above the line grooves, the probes abut against the bottom of the line grooves one by one; all the probes are energized at the same time to achieve synchronous electroplating of all the line grooves.
[0020] Furthermore, the probe comprises a spring assembly, and the spring assembly can drive the probe to move toward or away from the circuit groove.
[0021] Furthermore, after removing the protective film, the method further includes:
[0022] Perform plasma cleaning and AOI inspection on the exposed pads;
[0023] Apply hot melt adhesive on the surface of the pad;
[0024] Mechanical grinding is performed until the pad is exposed; the pad is bonded to the pad in the carrier board.
[0025] The above technical solution provided by the embodiment of the present application has the following advantages compared with the prior art: the present application forms a pad on the protective film on the outside of the carrier, applies hot melt adhesive on the protective film, etches a circuit groove in the hot melt adhesive; electroplates the circuit groove to form a circuit pattern, and the circuit pattern is electrically connected to the pad; finally removes the protective film, and connects the pad to the carrier. The present application forms a pad and a circuit pattern on the outside of the carrier with the help of a protective film and hot melt adhesive, and bonds the circuit pattern to the carrier through the pad; at the same time, the hot melt adhesive can also encapsulate the circuit pattern. The preparation and encapsulation of the circuit pattern of the present application can be carried out simultaneously, and are independent of the production process of the carrier. The preparation of the carrier, the preparation and encapsulation of the outer layer circuit pattern can be completed at the same time, which effectively improves the electrical connection efficiency of the carrier and improves the production efficiency of the carrier. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the invention and, together with the description, serve to explain the principles of the invention.
[0027] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.
[0028] In the attached figure:
[0029] Figure 1 Flow chart of the preparation method in Example 2. DETAILED DESCRIPTION
[0030] In order to have a clearer understanding of the technical features, purposes and effects of the present invention, the specific embodiments of the present invention are now described in detail with reference to the accompanying drawings. In the following description, it should be understood that the directions or positional relationships indicated by "front", "back", "up", "down", "left", "right", "longitudinal", "horizontal", "vertical", "horizontal", "top", "bottom", "inside", "outside", "head", "tail", etc. are based on the directions or positional relationships shown in the accompanying drawings, are constructed and operated in a specific direction, and are only for the convenience of describing the present technical solution, rather than indicating that the mechanism or element referred to must have a specific direction, and therefore cannot be understood as a limitation to the present invention.
[0031] It should also be noted that, unless otherwise clearly specified and limited, the terms such as "installed", "connected", "connected", "fixed", "set" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. When an element is referred to as being "on" or "under" another element, the element can be "directly" or "indirectly" located on the other element, or there may be one or more intermediate elements. The terms "first", "second", "third", etc. are only for the convenience of describing the present technical solution, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first", "second", "third", etc. can explicitly or implicitly include one or more of the features. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to the specific circumstances.
[0032] In the following description, specific details such as specific system structures, technologies, etc. are provided for the purpose of illustration rather than limitation, so as to provide a thorough understanding of the embodiments of the present invention. However, it should be clear to those skilled in the art that the present invention may be implemented in other embodiments without these specific details. In other cases, detailed descriptions of well-known systems, mechanisms, circuits, and methods are omitted to prevent unnecessary details from obstructing the description of the present invention.
[0033] Example 1
[0034] The present application provides a method for preparing an outer layer circuit of a carrier board, comprising:
[0035] forming a pad on the protective film;
[0036] Coating hot melt adhesive on the protective film and etching circuit grooves in the hot melt adhesive;
[0037] Electroplating the circuit groove to form a circuit pattern, wherein the circuit pattern is electrically connected to the pad;
[0038] Remove the protective film and connect the pads to the carrier board.
[0039] The protective film in this application can be made of materials such as PET film.
[0040] The present application forms pads and circuit patterns on the outside of the carrier board with the help of a protective film and hot-melt adhesive, and bonds the circuit patterns to the carrier board through the pads; at the same time, the hot-melt adhesive can also encapsulate the circuit patterns. The preparation and packaging of the circuit patterns of the present application can be carried out simultaneously, and are independent of the production process of the carrier board. The preparation of the carrier board, the preparation of the outer layer circuit pattern and the packaging can be completed at the same time, which effectively improves the electrical connection efficiency of the carrier board and improves the production efficiency of the carrier board.
[0041] Example 2
[0042] The present application provides a method for preparing an outer layer circuit of a carrier board, such as Figure 1 As shown, including:
[0043] S1: forming a pad on the protective film. Specifically including:
[0044] First, the protective film is roughened. The protective film may be a PET film, etc. The roughening process includes plasma etching or liquid etching. The protective film after the roughening process has a certain degree of roughness, which is convenient for the subsequent formation of the pad.
[0045] The pads are formed on the protective film through the laser 3D forming process. The pad areas are defined on the protective film in sequence, and the laser is used to melt the copper slurry so that the molten copper slurry drips onto the pad area and solidifies to form the pad. In the laser 3D forming process, the pads are formed by the accumulation of molten copper slurry drop by drop, and copper pillars can be accurately formed at the pre-defined pad positions.
[0046] Laser polishing is performed on the pad formed by solidification and accumulation of copper slurry to form a cylindrical pad. The pad formed by dropwise accumulation of copper slurry has an irregular shape, and a cylindrical pad can be formed by laser polishing. Among them, laser polishing refers to controlling the laser power to cut or melt the irregular pad so that its final shape is cylindrical.
[0047] The present application adopts a laser 3D forming method to form the pad, which can ensure the accuracy of the pad position, shape and size. The pad is used to connect the circuit pattern and the pad in the carrier, avoiding the tedious operation of wire connection or wiring connection, and improving the electrical connection accuracy between the carrier and the circuit pattern.
[0048] The pads formed in this step are used to connect the subsequent circuit patterns and pads in the carrier board.
[0049] S2: Apply hot melt adhesive on the protective film and etch circuit grooves in the hot melt adhesive. Specifically include:
[0050] The solidified hot melt adhesive is mechanically ground. The grinding fluid includes solid abrasive particles and liquid medium, wherein the liquid medium includes a dispersant, a modifier and a surfactant.
[0051] The solid-phase abrasive particles may be particles having a hardness greater than that of the hot melt adhesive after curing, for example, abrasive particles such as boron carbide and diamond powder may be used.
[0052] Dispersants are used to ensure that the abrasive particles are evenly dispersed in the grinding fluid, and also to prevent the abrasive particles from settling and agglomerating to form a stable suspension.
[0053] The modifier can be adsorbed on the abrasive particles or the surface of the workpiece to be ground, which can have a wetting and lubricating effect and improve the grinding efficiency.
[0054] Surfactants can reduce interfacial tension and make the wetting angle θ close to zero, so that solid powder can be dispersed spontaneously in the surfactant solution. At the same time, surfactants can help liquids wet the inner surface of solids, allowing liquids to penetrate into the channels and gaps between the internal aggregates of particles, provide a certain pressure, and under the action of machinery, destroy the strong chemical bonding force of the particle aggregates. At the same time, surfactants can help grinding, reduce the surface energy of particles, and prevent the damaged surface from restoring bonding, thereby achieving the purpose of preventing particle agglomeration. Surfactants can also play a lubricating role as grinding aids, which can increase the specific surface area of the product and shorten the grinding time.
[0055] In summary, the grinding liquid in this application has the following effects:
[0056] (1) Suspension effect: The addition of free abrasives requires the grinding fluid to have good suspension properties, ensuring that the abrasives are evenly distributed and do not flocculate or precipitate within a certain period of use, thereby greatly improving the quality and efficiency of the grinding process.
[0057] (2) Lubrication: The liquid environment provided by the grinding fluid can reduce the friction between the abrasive particles, grinding chips and the workpiece surface, playing a lubricating role. The high pressure resistance can be improved by adding some active elements such as sulfur and chlorine to the grinding fluid.
[0058] (3) Cooling effect: The grinding fluid can penetrate into the high-temperature grinding area during the processing, effectively reducing the temperature of the grinding area and preventing burns and cracks on the workpiece surface.
[0059] (4) Cleaning effect: During the grinding process, a large amount of fine grinding chips and abrasive powder will be generated, which are easy to adhere to the surface of the grinder workpiece table, thereby affecting the surface quality of the grinding pad and reducing the accuracy. The liquid environment of the grinding fluid can remove excess debris through its fluidity, while ensuring the smoothness of the contact surface between the workpiece and the grinder.
[0060] After mechanical grinding, the hot melt adhesive has a smooth surface and uniform thickness. A circuit groove is prepared in the hot melt adhesive after grinding. The specific circuit groove preparation process can adopt a laser process or a laser drilling process to form a circuit groove corresponding to the circuit pattern.
[0061] S3: Electroplating the circuit groove to form a circuit pattern, wherein the circuit pattern is electrically connected to the pad. Specifically comprising:
[0062] S31: Deposit an initial copper layer at the bottom of the circuit groove by vapor deposition. The vapor deposition method is a global deposition process, and its purpose is to deposit a thin initial copper layer at the bottom of the circuit groove. The initial copper layer can provide a reference for the subsequent electroplated copper layer, ensuring that the circuit pattern formed by electroplating can be stably deposited in the circuit groove.
[0063] S32: Horizontally electroplating on the initial copper layer to form a circuit pattern. Specifically including:
[0064] The support frame is fixedly connected to the line groove, and the support frame includes a top plate, and probes arranged on one side of the top plate corresponding to the line grooves one by one. When the top plate is located above the line grooves, the probes abut against the bottom of the line grooves one by one; all the probes are energized at the same time to achieve synchronous electroplating of all the line grooves.
[0065] Since the circuit groove contains multiple grooves that are connected or adjacent to each other, in order to perform horizontal electroplating copper deposition on multiple grooves at the same time, multiple probes are set in the support frame of the present application, each probe corresponds to a groove, and when the probe is located in the groove and powered on, horizontal electroplating of the groove can be achieved. Powering on multiple probes at the same time can ensure that multiple grooves are powered on at the same time, ensuring the uniformity and stability of the circuit pattern formation.
[0066] Specifically, the probe of the present application includes a spring assembly, which can drive the probe to move toward or away from the circuit groove. During the horizontal electroplating process, the probe can rise as the thickness of the metal plating layer in the circuit groove increases. At the same time, when the depression depth of the circuit groove at different positions is different, the elastic force of the spring assembly can also be used to make the bottom of the probe always abut against the bottom of the circuit groove.
[0067] During the horizontal electroplating process, the probe will continue to retract as the height of the horizontal copper deposit changes. In the initial stage of horizontal electroplating, the probe abuts against the bottom of the groove. When the electroplated copper layer is deposited in the groove, the probe continues to retract upward under the elastic force of the spring assembly, ensuring that during the deposition of the electroplated copper layer, the probe always abuts against the bottom of the groove and will not be buried in the deposited copper layer.
[0068] In the horizontal electroplating copper deposition process of the present application, multiple probes are deposited with copper at the same time, and the end point of the copper deposition is the moment when the groove is just filled. In other words, when the probe rises with the copper layer in the groove to a position flush with the upper surface of the hot melt adhesive, the power supply to the probe can be stopped, and the copper deposition process of the probe is stopped. In the present application, corresponding control switches are respectively set for multiple probes. When the probe rises with the copper layer in the groove to a position flush with the upper surface of the hot melt adhesive, the corresponding control switch is closed, and the power supply to the probe is stopped.
[0069] Furthermore, the present application sets a sensor receiving end at the top of the circuit groove and a sensor transmitting end at the bottom of the probe. When the sensor receiving end receives the signal transmitted by the sensor transmitting end, the probe is controlled to be powered off and the horizontal electroplating is stopped.
[0070] Furthermore, in order to avoid confusion of sensor signals corresponding to adjacent probes, the present application may set an isolation piece between adjacent grooves to ensure that the sensor receiving end at the top of the groove can only receive the signal emitted by the sensor transmitting end at the bottom of the corresponding probe.
[0071] During the horizontal electroplating process of the circuit pattern of the present application, the height of the final horizontal electroplated layer may be inconsistent due to slight differences in the depth of each position of the circuit groove. Mechanical grinding can be performed again after the horizontal electroplating is completed to obtain a circuit pattern with a flush top. The specific mechanical grinding process can refer to the grinding process in step S2. During the grinding process, there is a difference in the hardness of the circuit pattern and the hot melt adhesive after curing. During the grinding process, the horizontal electroplated copper layer protruding from the circuit groove is first removed, and then the initial copper layer deposited globally on the upper surface of the hot melt adhesive is removed; after the excess copper layer is ground and removed, the solidified hot melt adhesive is finally ground. When grinding to the position of the hot melt adhesive, the grinding pressure and rate will change significantly. The present application can monitor the changes in pressure and rate during the grinding process in real time to monitor the end point of the grinding process.
[0072] S4: Remove the protective film and connect the pads to the carrier board. Specifically include:
[0073] The exposed pads are then plasma cleaned and inspected by AOI. Plasma cleaning is used to remove the residual protective film.
[0074] Hot melt adhesive is applied on the surface of the pad; the purpose of applying hot melt adhesive is to facilitate subsequent mechanical grinding to obtain a smooth pad.
[0075] Mechanical grinding is performed until the pad is exposed. In the mechanical grinding process, the hot melt adhesive part is ground in the initial stage, and the pad is ground later. Since the pad is formed on the protective film and the pad is formed after the surface of the protective film is roughened, that is, the side of the pad away from the circuit pattern has a larger roughness, when grinding to the pad position, it is necessary to over-grind so that the rougher part of the bottom of the pad is also removed, and then the pad is bonded to the pad in the carrier board.
[0076] The specific mechanical grinding process can refer to the grinding process in step S2. During the grinding process, the hardness of the pad and the cured hot melt adhesive is different. During the grinding process, the cured hot melt adhesive is removed first, and then the rougher part of the pad is removed; when grinding to the pad position, the grinding pressure and rate will change significantly. This application can monitor the pressure and rate changes during the grinding process in real time to monitor the end point of the grinding process.
[0077] The present application forms pads and circuit patterns on the outside of the carrier board with the help of a protective film and hot-melt adhesive, and bonds the circuit patterns to the carrier board through the pads; at the same time, the hot-melt adhesive can also encapsulate the circuit patterns. The preparation and packaging of the circuit patterns of the present application can be carried out simultaneously, and are independent of the production process of the carrier board. The preparation of the carrier board, the preparation of the outer layer circuit pattern and the packaging can be completed at the same time, which effectively improves the electrical connection efficiency of the carrier board and improves the production efficiency of the carrier board.
[0078] It can be understood that the above embodiments only express the preferred implementation modes of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the patent scope of the present invention. It should be pointed out that, for ordinary technicians in this field, the above technical features can be freely combined without departing from the concept of the present invention, and several deformations and improvements can be made, which all belong to the protection scope of the present invention. Therefore, all equivalent changes and modifications made to the scope of the claims of the present invention should belong to the coverage of the claims of the present invention.
Claims
1. A method for preparing an outer layer circuit of a carrier board, characterized in that: include: forming a pad on the protective film; Coating hot melt adhesive on the protective film and etching circuit grooves in the hot melt adhesive; Hot melt adhesive is used to achieve both circuit preparation and packaging; The circuit groove is electroplated to form a circuit pattern, and the circuit pattern is electrically connected to the pad; specifically, the method comprises: depositing an initial copper layer at the bottom of the circuit groove by a vapor deposition method; horizontally electroplating on the initial copper layer to form a circuit pattern; fixing a support frame to the circuit groove, the support frame comprising a top plate, and probes arranged on one side of the top plate corresponding to the circuit grooves, and when the top plate is located above the circuit grooves, the probes abut against the bottom of the circuit grooves in a one-to-one manner; all the probes are energized at the same time to achieve synchronous electroplating of all the circuit grooves; the probes comprise a spring assembly, and the spring assembly can drive the probes to move toward or away from the circuit grooves; Remove the protective film and connect the pads to the carrier board.
2. The method for preparing an outer layer circuit of a carrier board according to claim 1, characterized in that: The circuit groove is prepared by laser processing.
3. The method for preparing an outer layer circuit of a carrier board according to claim 1, characterized in that: The pads are formed on the protective film by a laser 3D forming process.
4. The method for preparing an outer layer circuit of a carrier board according to claim 1, characterized in that: Before forming the pad on the protective film, the method further includes: performing a roughening treatment on the protective film.
5. The method for preparing an outer layer circuit of a carrier board according to claim 1, characterized in that: Before etching the circuit grooves in the hot melt adhesive, the method also includes: mechanically grinding the cured hot melt adhesive.
6. The method for preparing an outer layer circuit of a carrier board according to claim 5, characterized in that: The mechanical grinding is performed in a grinding solution, which includes abrasive particles, a dispersant, a modifier and a surfactant.
7. The method for preparing an outer layer circuit of a carrier board according to claim 1, characterized in that: After removing the protective film, it also includes: Perform plasma cleaning and AOI inspection on the exposed pads; Apply hot melt adhesive on the surface of the pad; Mechanical grinding is performed until the pad is exposed; the pad is bonded to the pad in the carrier board.