A high linearity device employing a T-type dual-channel structure and its fabrication method

By employing a T-type Fin structure array design in GaN-based HEMT devices, the problems of poor coupling and decreased linearity in dual-channel devices are solved, achieving a combination of high linearity and high breakdown voltage.

CN117457495BActive Publication Date: 2026-11-10XIDIAN UNIV
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311567963.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-11-22
Publication Date
2026-11-10
Estimated Expiration
2043-11-22

AI Technical Summary

Technical Problem

The dual-channel structure of existing GaN-based HEMT devices exhibits poor coupling on the transconductance curve, leading to a decrease in linearity, and the traditional N-type doping method results in a loss of breakdown voltage.

Method used

A T-type dual-channel structure is adopted. By forming a T-type Fin structure array in the device, gate control of different channels is performed using Fin structures with different Fin widths. By combining dry and wet etching techniques, T-type Fin structures with different threshold characteristics are formed.

Benefits of technology

A flatter transconductance curve was achieved, improving the linearity of the device while maintaining high breakdown voltage characteristics without compromising the device's breakdown characteristics.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117457495B_ABST
    Figure CN117457495B_ABST
Patent Text Reader

Abstract

This invention discloses a high-linearity device employing a T-type dual-channel structure and its fabrication method, comprising: obtaining an epitaxial structure from bottom to top including a SiC substrate, a GaN buffer layer, a first GaN channel layer, a first AlGaN back barrier layer, a second GaN channel layer, and a second AlGaN back barrier layer; forming a source electrode and a drain electrode on the second AlGaN back barrier layer; etching the second AlGaN back barrier layer until the first AlGaN back barrier layer forms the upper part of the T-type Fin structure; continuing to etch the first AlGaN back barrier layer until it reaches the first GaN channel layer, and etching the first AlGaN back barrier layer and the first GaN channel layer directly below the upper part of the T-type Fin structure to form the lower part of the corresponding T-type Fin structure; forming a gate electrode on the periphery of the T-type Fin structure and on the surface of the first GaN channel layer. This invention can fabricate devices with high linearity.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of semiconductor technology, specifically relating to a high linearity device employing a T-type dual-channel structure and its fabrication method. Background Technology

[0002] With wireless communication technologies increasingly requiring high frequency, high voltage, and high power, GaN-based HEMTs (High Electron Mobility Transistors) are widely used in applications such as 5G communication, WIMAX (World Interoperability for Microwave Access), and satellite communication due to their excellent material properties, including wide bandgap, high breakdown electric field, high saturation electron velocity, and high mobility.

[0003] Conventional single-channel devices have a limited theoretical saturation current limit compared to multi-channel devices due to their limited carrier concentration. To further improve the saturation current and achieve high-linearity, high-current RF devices, dual-channel gallium nitride (GaN) high-electron-mobility transistors (HEMTs) have attracted widespread attention. For example, in terms of heterostructure, the most common choice is the AlGaN / GaN double heterojunction, which fabricates a dual-channel device. The additional channel provides extra carriers, ensuring an increase in saturation current. Because the two channels are at different distances from the gate and are controlled by different gate voltages, their DC characteristics show sequential turn-on. However, the coupling between the two channels is often not very good, with a noticeable dip between the two peaks of the transconductance curve, which affects the overall linearity of the device. Currently, the coupling characteristics of the dual channels can be improved by N-type doping of the underlying barrier layer, thus increasing the flatness of the transconductance.

[0004] However, the breakdown voltage of devices fabricated by N-type doping of the bottom barrier layer is significantly reduced. Therefore, it is imperative to fabricate dual-channel devices that do not compromise the breakdown characteristics and have high linearity. Summary of the Invention

[0005] To address the aforementioned problems in the prior art, this invention provides a high linearity device employing a T-type dual-channel structure and its fabrication method. The technical problem to be solved by this invention is achieved through the following technical solution:

[0006] In a first aspect, embodiments of the present invention provide a method for fabricating a high linearity device employing a T-type dual-channel structure, comprising:

[0007] An epitaxial structure is obtained, which consists of a SiC substrate, a GaN buffer layer, a first GaN channel layer, a first AlGaN back barrier layer, a second GaN channel layer, and a second AlGaN back barrier layer, from bottom to top.

[0008] Source and drain metals are deposited on the surface of the second AlGaN back barrier layer to form source and drain electrodes, respectively.

[0009] Electrically isolated regions are formed at both ends of the device; wherein the electrically isolated regions are adjacent to the source electrode and the drain electrode;

[0010] A SiN passivation layer is grown on the surface of the source electrode, the drain electrode, the second AlGaN back barrier layer, and the electrically isolated region.

[0011] The SiN passivation layer is etched to form a photolithographic pattern of a T-type Fin structure array on the surface of the second AlGaN back barrier layer between the source electrode and the drain electrode; wherein the distance between adjacent T-type Fin structures in the T-type Fin structure array is W1;

[0012] According to the photolithography pattern, the second AlGaN back barrier layer is etched until the surface of the first AlGaN back barrier layer forms the upper part of each T-type Fin structure; wherein, the Fin width of the upper part of each T-type Fin structure is W2, and W2 = 2*W1;

[0013] The etching process continues until the first AlGaN back barrier layer is reached into the first GaN channel layer, and the portion of the first AlGaN back barrier layer and the portion of the first GaN channel layer directly below the upper part of the T-shaped Fin structure are etched to form the lower part of each T-shaped Fin structure. The upper part of each T-shaped Fin structure and the lower part of its corresponding T-shaped Fin structure constitute the entire T-shaped Fin structure. The Fin width of the lower part of each T-shaped Fin structure is W3, and W3 = 0.6 * W2.

[0014] Gate metal is deposited around each T-shaped Fin structure and on the surface of the first GaN channel layer to form a gate electrode.

[0015] In one embodiment of the present invention, electrically isolated regions are formed at both ends of the device, including:

[0016] Ion implantation is performed on the surface of the second AlGaN back barrier layer at both ends of the device, with the implantation depth extending into a portion of the GaN buffer layer to form the electrically isolated region.

[0017] In one embodiment of the present invention, etching the second AlGaN back barrier layer until the surface of the first AlGaN back barrier layer forms the upper part of each T-shaped Fin structure includes:

[0018] The second AlGaN back barrier layer is etched using a dry etching method until the upper part of each T-shaped Fin structure is formed on the surface of the first AlGaN back barrier layer.

[0019] In one embodiment of the present invention, the process of etching the second AlGaN back barrier layer down to the surface of the first AlGaN back barrier layer using a dry etching method includes:

[0020] The process parameters used in the ICP etching equipment include: etching gas is BCl3 / Cl2, flow rate is 20 / 8 sccm, pressure is 5 mTorr, ICP power is 50W, and RF power is 15W.

[0021] In one embodiment of the present invention, etching the first AlGaN back barrier layer down to the first GaN channel layer includes:

[0022] The first AlGaN back barrier layer is etched into the first GaN channel layer using a dry etching method.

[0023] In one embodiment of the present invention, the process of etching the first AlGaN back barrier layer down to the first GaN channel layer using a dry etching method includes:

[0024] The process parameters used in the ICP etching equipment include: etching gas is BCl3 / Cl2, flow rate is 20 / 8 sccm, pressure is 10 mTorr, ICP power is 50W, and RF power is 15W.

[0025] In one embodiment of the present invention, etching a portion of the first AlGaN back barrier layer and a portion of the first GaN channel layer directly below the upper part of the T-shaped Fin structure includes:

[0026] The first AlGaN back barrier layer and part of the first GaN channel layer are etched directly below the upper part of the T-shaped Fin structure using a wet etching method.

[0027] In one embodiment of the present invention, the thickness of the upper part of each T-shaped Fin structure is H1, where H1 is the sum of the thicknesses of the second AlGaN back barrier layer and the second GaN channel layer; the thickness of the lower part of each T-shaped Fin structure is H2, where H2 is the sum of the thicknesses of the first AlGaN back barrier layer and a portion of the first GaN channel layer, and H2...

[0028] Secondly, embodiments of the present invention provide a high linearity device employing a T-type dual-channel structure, the device comprising:

[0029] The epitaxial structure includes, from bottom to top, a SiC substrate, a GaN buffer layer, a first GaN channel layer, a first AlGaN back barrier layer, a second GaN channel layer, and a second AlGaN back barrier layer. ​

[0030] The source electrode and drain electrode are located on the upper surface of the second AlGaN back barrier layer, respectively.

[0031] An electrical isolation region is located at both ends of the device and is adjacent to the source electrode and the drain electrode;

[0032] A SiN passivation layer is located on the source electrode, the drain electrode, the second AlGaN back barrier layer, and the upper surface of the electrically isolated region;

[0033] Several T-shaped Fin structures are provided, with a distance of W1 between adjacent T-shaped Fin structures. Each T-shaped Fin structure includes an upper part and a lower part. The upper part of each T-shaped Fin structure penetrates the SiN passivation layer and includes the second AlGaN back barrier layer and the second GaN channel layer. The lower part of each T-shaped Fin structure includes the first AlGaN back barrier layer and part of the first GaN channel layer. The Fin width of the upper part of each T-shaped Fin structure is W2, and the Fin width of the lower part of each T-shaped Fin structure is W3, where W2 = 2 * W1 and W3 = 0.6 * W2.

[0034] The gate electrode is located on the periphery of each T-shaped Fin structure and on the upper surface of the first GaN channel layer.

[0035] In one embodiment of the present invention, the thickness of the upper part of each T-shaped Fin structure is H1, where H1 is the sum of the thicknesses of the second AlGaN back barrier layer and the second GaN channel layer; the thickness of the lower part of each T-shaped Fin structure is H2, where H2 is the sum of the thicknesses of the first AlGaN back barrier layer and a portion of the first GaN channel layer, and H2...

[0036] The beneficial effects of this invention are:

[0037] ​The fabrication method of the high linearity device using a T-type dual-channel structure proposed in this invention can be applied to the fabrication of high linearity devices with different channel widths and different Fin structures. Its implementation includes: obtaining an epitaxial structure comprising, from bottom to top, a SiC substrate, a GaN buffer layer, a first GaN channel layer, a first AlGaN back barrier layer, a second GaN channel layer, and a second AlGaN back barrier layer; depositing source and drain metals on the surface of the second AlGaN back barrier layer to form source and drain electrodes, respectively; forming electrically isolated regions at both ends of the device, wherein the electrically isolated regions are adjacent to the source and drain electrodes; growing a SiN passivation layer on the surface of the source electrode, drain electrode, second AlGaN back barrier layer, and the electrically isolated regions; etching the SiN passivation layer; and forming a photolithographic pattern of a T-type Fin structure array on the surface of the second AlGaN back barrier layer between the source and drain electrodes; wherein the T-type Fin structure... The distance between adjacent T-type Fin structures in the array is W1. According to the photolithography pattern, the second AlGaN back barrier layer is etched up to the surface of the first AlGaN back barrier layer to form the upper part of each T-type Fin structure. The Fin width of the upper part of each T-type Fin structure is W2, and W2 = 2 * W1. The first AlGaN back barrier layer is etched further up to the first GaN channel layer, and the portion of the first AlGaN back barrier layer and the portion of the first GaN channel layer directly below the upper part of the T-type Fin structure are etched to form the lower part of each corresponding T-type Fin structure. The upper part of each T-type Fin structure and the lower part of its corresponding T-type Fin structure constitute the entire T-type Fin structure. The Fin width of the lower part of each T-type Fin structure is W3, and W3 = 0.6 * W2. Gate metal is deposited around each T-type Fin structure and on the surface of the first GaN channel layer to form a gate electrode. As can be seen, the fabrication method proposed in this invention, based on the fabrication of a dual-channel device with a T-type Fin structure, uses different Fin widths for different channels, which allows for different gate control for different channels, thereby achieving a flatter transconductance curve, improving the device's GVS (Gate Voltage Swing), and thus improving the device's linearity, resulting in a device with high linearity. Compared with the traditional N-type doping method, the fabrication method provided by this invention does not damage the device's breakdown characteristics; that is, for GaN devices with high breakdown voltage, it still maintains the device's high breakdown voltage characteristics.

[0038] The present invention will be further described in detail below with reference to the accompanying drawings and embodiments. Attached Figure Description

[0039] Figure 1 This is a schematic flowchart of a method for fabricating a high linearity device using a T-type dual-channel structure according to an embodiment of the present invention;

[0040] Figure 2 (a)~ Figure 2 (l) is a schematic diagram of the process structure corresponding to the fabrication method of the high linearity device with T-type dual-channel structure provided in the embodiment of the present invention;

[0041] Figure 3 This is a schematic diagram showing the performance comparison between devices based on traditional Fin structures and devices based on the T-type Fin structure proposed in this invention.

[0042] Figure 4 (a)~ Figure 4 (b) is a schematic diagram of the high linearity device with a T-type dual-channel structure provided in an embodiment of the present invention;

[0043] Figure 5 This is a three-dimensional structural schematic diagram of a high linearity device with a T-type dual-channel structure provided in an embodiment of the present invention.

[0044] Explanation of reference numerals in the attached figures:

[0045] 1-SiC substrate; 2-GaN buffer layer; 3-First GaN channel layer; 4-First AlGaN back barrier layer; 5-Second GaN channel layer; 6-Second AlGaN back barrier layer; 7-Source electrode; 8-Drain electrode; 9-Electrically isolated region; 10-SiN passivation layer; 11-Gate electrode. Detailed Implementation

[0046] The present invention will be further described in detail below with reference to specific embodiments, but the implementation of the present invention is not limited thereto.

[0047] Firstly, please see Figure 1 This invention provides a method for fabricating a high linearity device using a T-type dual-channel structure, comprising the following steps:

[0048] S10. Obtain an epitaxial structure consisting of, from bottom to top, a SiC substrate 1, a GaN buffer layer 2, a first GaN channel layer 3, a first AlGaN back barrier layer 4, a second GaN channel layer 5, and a second AlGaN back barrier layer 6.

[0049] The epitaxial structure provided in this embodiment of the invention can be an existing integrated structure, such as... Figure 2 As shown in (a), structures that can also be produced through manufacturing processes are as follows: Figure 2 As shown in (a), the fabrication process can use MOCVD (Metal-Organic Chemical Vapor Deposition) technology to grow SiC substrate 1, GaN buffer layer 2, first GaN channel layer 3, first AlGaN back barrier layer 4, second GaN channel layer 5, and second AlGaN back barrier layer 6 from bottom to top.

[0050] Preferably, the SiC substrate 1 has a thickness of 0.375 mm, the GaN buffer layer has a thickness of 1 μm, the first GaN channel layer 3 has a thickness of 400 nm, the first AlGaN back barrier layer 4 (30% Al content) has a thickness of 10 nm, the second GaN channel layer 5 has a thickness of 10 nm, and the second AlGaN back barrier layer 6 (30% Al content) has a thickness of 20 nm.

[0051] S20. Source and drain metals are deposited on the surface of the second AlGaN back barrier layer 6 to form source electrode 7 and drain electrode 8, respectively.

[0052] In this embodiment of the invention, photoresist is coated onto the surface of the second AlGaN back barrier layer 6, and the source and drain electrode markings are aligned using a stepper lithography machine. Then, source and drain metals (Ti / Al / Ni / Au) are deposited in the source and drain electrode regions of the device using electron beam evaporation. Subsequently, rapid annealing at 880°C for 50 seconds under a nitrogen atmosphere forms the source electrode 7 and drain electrode 8. Figure 2 As shown in (b), ohmic contacts are formed at the drain electrode 8 and the source electrode 7, respectively.

[0053] S30. Electrically isolated regions 9 are formed at both ends of the device; wherein, the electrically isolated regions 9 are adjacent to the source electrode 7 and the drain electrode 8.

[0054] This invention provides an optional solution for forming electrically isolated regions 9 at both ends of the device, including: performing ion implantation on the surface of the second AlGaN back barrier layer 6 at both ends of the device, with the implantation depth extending into a portion of the GaN buffer layer 2, to form the electrically isolated regions 9 as shown. Figure 2 As shown in (c), for example, the implanted ions can be boron ions. After ions are implanted on both sides of the drain electrode 8 and the source electrode 7, a high-resistivity state is formed, which can achieve active region isolation of the device. Compared with the method of etching to form the electrical isolation region 9, this isolation method can ensure better isolation performance of the device and will not affect the performance of the device itself.

[0055] S40, a SiN passivation layer 10 is grown on the surface of the source electrode 7, the drain electrode 8, the second AlGaN back barrier layer 6, and the electrically isolated region 9.

[0056] In this embodiment of the invention, a 120 nm thick SiN passivation layer 10 is grown on the surface of the source electrode 7, drain electrode 8, second AlGaN back barrier layer 6, and electrically isolated region 9 using PECVD (Plasma Enhanced Chemical Vapor Deposition). Figure 2 As shown in (d).

[0057] S50, etch the SiN passivation layer 10 to form a photolithographic pattern of a T-type Fin structure array on the surface of the second AlGaN back barrier layer 6 between the source electrode 7 and the drain electrode 8; wherein, the distance between adjacent T-type Fin structures in the T-type Fin structure array is W1.

[0058] In this embodiment of the invention, photoresist is coated on the surface of the SiN passivation layer 10, and the SiN passivation layer 10 is etched. A photolithographic pattern of the T-type Fin structure array designed in this invention is formed on the surface of the second AlGaN back barrier layer 6 between the source electrode 7 and the drain collector. The distance between adjacent T-type Fin structures in the T-type Fin structure array is W1. Preferably, the distance W1 between adjacent T-type Fin structures in the T-type Fin structure array is 50 nm.

[0059] S60. According to the photolithography pattern, etch the second AlGaN back barrier layer 6 until the surface of the first AlGaN back barrier layer 4 forms the upper part of each T-type Fin structure; wherein, the Fin width of the upper part of each T-type Fin structure is W2, and W2 = 2*W1.

[0060] According to the photolithography pattern formed in S50, the second AlGaN back barrier layer 6 is etched up to the surface of the first AlGaN back barrier layer 4 (i.e., etched down to below the first two-dimensional electron gas layer formed by the second AlGaN back barrier layer 6 and the second GaN channel layer 5) to form the upper part of each T-type Fin structure. That is, the upper part of each T-type Fin structure includes the second AlGaN back barrier layer 6 and the second GaN channel layer 5, as shown below. Figure 2 As shown in (e). Figure 2 Another cross-sectional view corresponding to the area marked by the blue box in (e) is shown below. Figure 2 As shown in (f), from Figure 2 As shown in (f), the upper Fin width of each T-shaped Fin structure is W2, and W2 = 2 * W1. The upper thickness of each T-shaped Fin structure is H1, where H1 is the sum of the thicknesses of the second AlGaN back barrier layer 6 and the second GaN channel layer 5. Preferably, the upper Fin width W2 of each T-shaped Fin structure is 100 nm, and the upper thickness H1 of each T-shaped Fin structure is 30 nm.

[0061] This invention provides an optional solution, employing dry etching to etch the second AlGaN back barrier layer 6 up to the surface of the first AlGaN back barrier layer 4, forming the upper part of each T-shaped Fin structure. Correspondingly, the process of etching the second AlGaN back barrier layer 6 up to the surface of the first AlGaN back barrier layer 4 using dry etching includes:

[0062] The etching equipment used in the ICP (Inductively Coupled Plasma) process had the following parameters: etching gas was BCl3 / Cl2, flow rate was 20 / 8 sccm, pressure was 5 mTorr, ICP power was 50 W, and RF power was 15 W.

[0063] S70. Continue etching the first AlGaN back barrier layer 4 until it reaches the first GaN channel layer 3, and etch the portion of the first AlGaN back barrier layer 4 and the portion of the first GaN channel layer 3 directly below the upper part of the T-type Fin structure to form the lower part of each T-type Fin structure. The upper part of each T-type Fin structure and the lower part of its corresponding T-type Fin structure constitute the entire T-type Fin structure. The Fin width of the lower part of each T-type Fin structure is W3, and W3 = 0.6 * W2.

[0064] In this embodiment of the invention, S60 continues etching the first AlGaN back barrier layer 4 until it reaches the first GaN channel layer 3 (i.e., etching down to below the second two-dimensional electron gas formed by the first AlGaN back barrier layer 4 and the first GaN channel layer 3). Figure 2 As shown in (g) Figure 2 Another cross-sectional view corresponding to the area marked by the red box in (g) is shown below. Figure 2 As shown in (h). Fin structures are typically designed for single-channel devices, which effectively ensures the high linearity of single-channel structures. If such a Fin structure is directly applied to a dual-channel device, as shown in (h),... Figure 2 (h) The device structure formed by etching, for this dual-channel HEMT device, mainly reduces the two-dimensional electron gas surface density below the gate electrode by reducing the thickness of the lower back barrier layer, so that the threshold voltage of the device drifts in the positive direction. Figure 2 In addition to the upper gate control, the Fin structure shown also generates additional gate controls on both sides of the Fin, which is equivalent to generating two devices with different thresholds. During operation, the two devices are turned on in sequence, so that the gate is always effectively controlled. Two obvious peaks can be seen on the transconductance curve. Combining the Fin structure with the dual channel can generate more devices with different thresholds. The coupling between them is a qualitative leap in improving the transconductance flatness of the device.

[0065] However, dual-channel devices typically have poor coupling, limiting their GVS and exhibiting a noticeable dip between the two peaks of the transconductance curve, thus affecting the device's linearity. Therefore, this invention proposes a T-type Fin structure... Figure 2Based on (h), further etching makes the Fin structure T-shaped. This allows for the combination of different Fin widths into a single device by utilizing the different threshold characteristics corresponding to different Fin widths. Since Fin structures with different gate widths are sequentially activated, the gate control effects on the two channels differ, widening the GVS, improving the flatness of the transconductance curve, and enhancing the coupling effect between the two channels, thereby improving the device's linearity. It is evident that the T-shaped Fin structure proposed in this embodiment has the aforementioned advantages. However, since no Fin structure has been designed in this way before, the design of various process parameters during the fabrication process of the T-shaped Fin structure is particularly important. For example, the design of etching process parameters and the design of the Fin width of the T-shaped Fin structure are crucial. Inappropriate parameter design cannot improve the device's linearity; on the contrary, it may lead to a deterioration in linearity. Based on research and multiple experiments, the inventors have provided the following specific implementation scheme:

[0066] This invention provides an optional solution, which first employs dry etching to etch the first AlGaN back barrier layer 4 down to the first GaN channel layer 3, as shown in the following embodiment. Figure 2 As shown in (h). Correspondingly, the process of etching the first AlGaN back barrier layer 4 up to the first GaN channel layer 3 using a dry etching method includes:

[0067] The process parameters used in the ICP etching equipment include: etching gas is BCl3 / Cl2, flow rate is 20 / 8 sccm, pressure is 10 mTorr, ICP power is 50W, and RF power is 15W.

[0068] Furthermore, embodiments of the present invention in Figure 2 Based on (h), a wet etching method is used, such as the TMAH wet etching process, to form isotropic etching. The etching time is controlled to be 90 minutes. The portion of the first AlGaN back barrier layer 4 and the portion of the first GaN channel layer 3 directly below the upper part of the T-shaped Fin structure are etched to form the lower part of each T-shaped Fin structure, as shown in Figure 3. Figure 2 As shown in (i), the upper part of each T-shaped Fin structure and the lower part of its corresponding T-shaped Fin structure constitute the entire T-shaped Fin structure. Figure 2 As shown in (i), the width of the lower Fin of each T-shaped Fin structure is W3, and W3 = 0.6 * W2. The thickness of the lower part of each T-shaped Fin structure is H2, where H2 is the sum of the thicknesses of the first AlGaN back barrier layer 4 and part of the first GaN channel layer 3.

[0069] from Figure 2 ​(j) It can be seen that: the present invention proposes a distribution form of multiple T-type Fin structures in the device structure, and the distance between adjacent T-type Fin structures is W1, that is, the distance between adjacent T-type Fin structures in the T-type Fin structure array mentioned in S50.

[0070] S80. A gate electrode 11 is formed by depositing gate metal on the periphery of each T-shaped Fin structure and on the surface of the first GaN channel layer 3.

[0071] In this embodiment of the invention, photoresist is applied to the gate electrode region, and a stepper lithography machine is used to align the gate marking metal. Then, an electron beam evaporation method is used to deposit gate metal (Ni / Au) in the gate electrode region of the device to form the gate electrode 11. Figure 2 As shown in (k), from Figure 2 Another cross-sectional view corresponding to the red line marked in (k) is shown below. Figure 2 As shown in (l), it can be seen that the gate metal is deposited on the periphery of each T-type Fin structure and on part of the surface of the first GaN channel layer 3.

[0072] It should be noted that the T-type dual-channel embodiment of the present invention is used as an example for protection description. However, for other multi-channel devices, such as three-channel and four-channel devices, the above-described fabrication process of S10 to S80 can still be used. The difference is that etching continues after S60 to S70. If the device is a three-channel device, etching continues below the third layer of two-dimensional electron gas after S70. The first layer of two-dimensional electron gas and the second layer of two-dimensional electron gas are etched to form a T-type Fin structure, and the third layer of two-dimensional electron gas and the second layer of two-dimensional electron gas are etched to form a T-type Fin structure, and so on.

[0073] Figure 3 For based on Figure 2 (h) shows the Fin structure dual-channel structure device (shown by the black line) and the device based on the present invention. Figure 2 (i) shows a performance comparison of dual-channel devices with a T-type Fin structure (shown by the red line). Figure 3 The horizontal axis represents the transconductance value (g) m (Unit: mS / mm), with the vertical axis representing the gate voltage (V). g (unit V), from Figure 3 It can be seen that, compared with traditional Fin structure devices, the method proposed in this invention produces Fin structures with flatter transconductance curves, enabling the fabrication of dual-channel devices with higher linearity. Regarding... Figure 3 The inventor discovered through research that: traditional Figure 2 The device with the Fin structure shown in (h) has a transconductance g m After reaching its peak value, as the gate voltage continues to increase, the parasitic resistance R of the source electrode 7... s The increase of g leads to the transconductance g mThe parasitic resistance R of the source electrode 7 is reduced. The fin-shaped gate, i.e., the T-type Fin structure proposed in this invention, can effectively reduce the parasitic resistance R of the source electrode 7. s Suppress transconductance g m The reduction. Meanwhile, to further improve GVS, embodiments of the present invention combine different Fin widths onto a single device. Different Fin widths correspond to different threshold characteristics, achieving different gate control for different channels. This allows T-shaped Fin structures with different gate widths to turn on sequentially, thus widening the GVS; while... Figure 2 The Fin structure shown in (h) can theoretically improve the linearity of dual-channel devices when directly applied, but due to the transconductance curve g m The concavity phenomenon still exists, and the improvement in device linearity is not significant. Therefore, embodiments of the present invention propose a method based on... Figure 2 The T-shaped Fin structure shown in (i) adjusts the gate control of the two channels by changing the Fin width of the upper and lower channels. This results in different gate control effects on the two channels without compromising the device's breakdown characteristics, widening the GVS and improving the flatness of the transconductance curve. Furthermore, this T-shaped Fin structure design enhances the coupling between the two channels, further improving the device's linearity. Therefore, the T-shaped Fin structure design of this invention can effectively improve the linearity of the device, resulting in a device with high linearity.

[0074] In summary, the fabrication method for a high-linearity device employing a T-type dual-channel structure proposed in this invention can be applied to the fabrication of high-linearity devices with different channel widths using different Fin structures. Its implementation includes: obtaining an epitaxial structure comprising, from bottom to top, a SiC substrate 1, a GaN buffer layer 2, a first GaN channel layer 3, a first AlGaN back barrier layer 4, a second GaN channel layer 5, and a second AlGaN back barrier layer 6; depositing source and drain metals on the surface of the second AlGaN back barrier layer 6 to form source electrodes 7 and drain electrodes 8; forming electrically isolated regions 9 at both ends of the device; wherein the electrically isolated regions 9 are adjacent to the source electrodes 7 and drain electrodes 8; growing a SiN passivation layer 10 on the surfaces of the source electrodes 7, drain electrodes 8, the second AlGaN back barrier layer 6, and the electrically isolated regions 9; etching the SiN passivation layer 10 to form a photolithographic pattern of a T-type Fin structure array on the surface of the second AlGaN back barrier layer 6 between the source electrodes 7 and drain electrodes 8. In this process, the distance between adjacent T-type Fin structures in the T-type Fin structure array is W1. According to the photolithography pattern, the second AlGaN back barrier layer 6 is etched up to the surface of the first AlGaN back barrier layer 4 to form the upper part of each T-type Fin structure. The Fin width of the upper part of each T-type Fin structure is W2, and W2 = 2 * W1. The first AlGaN back barrier layer 4 is etched up to the first GaN channel layer 3, and the portion of the first AlGaN back barrier layer 4 and the portion of the first GaN channel layer 3 directly below the upper part of the T-type Fin structure are etched to form the lower part of each T-type Fin structure. The upper part of each T-type Fin structure and the lower part of its corresponding T-type Fin structure constitute the entire T-type Fin structure. The Fin width of the lower part of each T-type Fin structure is W3, and W3 = 0.6 * W2. Gate metal is deposited on the periphery of each T-type Fin structure and on the surface of the first GaN channel layer 3 to form a gate electrode 11. As can be seen, the fabrication method proposed in this embodiment of the invention is based on the fabrication of a dual-channel device with a T-type Fin structure. By using different Fin widths for different channels, different gate control can be achieved for different channels, thereby achieving a flatter transconductance curve, improving the device's GVS, and thus improving the device's linearity, resulting in a device with high linearity. Compared with the traditional N-type doping method, the fabrication method provided in this embodiment of the invention does not damage the device's breakdown characteristics, that is, for GaN devices with high breakdown voltage, it still maintains the device's high breakdown voltage characteristics.

[0075] Secondly, high linearity devices fabricated based on the manufacturing method in the first aspect, such as... Figure 4 (a)~ Figure 4 As shown in (b) Figure 4 (a) Figure 4 (b) Two cross-sectional views from different angles are shown. This embodiment of the invention provides a high linearity device employing a T-type dual-channel structure. The device includes:

[0076] The epitaxial structure includes, from bottom to top, a SiC substrate 1, a GaN buffer layer 2, a first GaN channel layer 3, a first AlGaN back barrier layer 4, a second GaN channel layer 5, and a second AlGaN back barrier layer 6.

[0077] The source electrode 7 and the drain electrode 8 are located on the upper surface of the second AlGaN back barrier layer 6, respectively.

[0078] Electrical isolation region 9 is located at both ends of the device and is adjacent to source electrode 7 and drain electrode 8;

[0079] The SiN passivation layer 10 is located on the upper surface of the source electrode 7, the drain electrode 8, the second AlGaN back barrier layer 6, and the electrical isolation region 9.

[0080] Several T-shaped Fin structures are provided, with the distance between adjacent T-shaped Fin structures being W1. Each T-shaped Fin structure includes an upper part and a lower part. The upper part of each T-shaped Fin structure penetrates the SiN passivation layer and includes a second AlGaN back barrier layer 6 and a second GaN channel layer 5. The lower part of each T-shaped Fin structure includes a first AlGaN back barrier layer 4 and a portion of the first GaN channel layer 3. The Fin width of the upper part of each T-shaped Fin structure is W2, and the Fin width of the lower part of each T-shaped Fin structure is W3, where W2 = 2 * W1 and W3 = 0.6 * W2.

[0081] The gate electrode 11 is located on the periphery of each T-type Fin structure and on the upper surface of the first GaN channel layer 3.

[0082] In this embodiment of the invention, the thickness of the upper part of each T-shaped Fin structure is H1, where H1 is the sum of the thicknesses of the second AlGaN back barrier layer 6 and the second GaN channel layer 5; the thickness of the lower part of each T-shaped Fin structure is H2, where H2 is the sum of the thicknesses of the first AlGaN back barrier layer 4 and a portion of the first GaN channel layer 3, and H2...

[0083] Figure 5 The three-dimensional structure of the device proposed in the embodiments of the present invention provides a more intuitive understanding of the device's structure. Figure 5 The three-dimensional structure is more important in demonstrating the T-shaped Fin structure proposed in this invention; other structures are not shown here.

[0084] As for the device structure embodiment of the second aspect, since it is basically similar to the fabrication method embodiment of the first aspect, the description is relatively simple. For relevant details, please refer to the description of the fabrication method embodiment of the first aspect.

[0085] ​In the description of this invention, it should be understood that the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more of that feature. In the description of this invention, "a plurality of" means two or more, unless otherwise explicitly specified.

[0086] Although the invention has been described herein in conjunction with various embodiments, those skilled in the art, by reviewing the specification and accompanying drawings, will understand and implement other variations of the disclosed embodiments in carrying out the claimed invention. In the specification, the word "comprising" does not exclude other components or steps, and "a" or "an" does not exclude a plurality. While certain measures are described in different embodiments, this does not mean that these measures cannot be combined to produce good results.

[0087] The above description, in conjunction with specific preferred embodiments, provides a further detailed explanation of the present invention. It should not be construed that the specific implementation of the present invention is limited to these descriptions. For those skilled in the art, various simple deductions or substitutions can be made without departing from the concept of the present invention, and all such modifications and substitutions should be considered within the scope of protection of the present invention.

Claims

1. A method for fabricating a high linearity device employing a T-type dual-channel structure, characterized in that, include: An epitaxial structure is obtained, which consists of a SiC substrate, a GaN buffer layer, a first GaN channel layer, a first AlGaN back barrier layer, a second GaN channel layer, and a second AlGaN back barrier layer, from bottom to top. Source and drain metals are deposited on the surface of the second AlGaN back barrier layer to form source and drain electrodes, respectively. Electrically isolated regions are formed at both ends of the device; wherein the electrically isolated regions are adjacent to the source electrode and the drain electrode; A SiN passivation layer is grown on the surface of the source electrode, the drain electrode, the second AlGaN back barrier layer, and the electrically isolated region. The SiN passivation layer is etched to form a photolithographic pattern of a T-type Fin structure array on the surface of the second AlGaN back barrier layer between the source electrode and the drain electrode; wherein the distance between adjacent T-type Fin structures in the T-type Fin structure array is W1; According to the photolithography pattern, the second AlGaN back barrier layer is etched until the surface of the first AlGaN back barrier layer forms the upper part of each T-type Fin structure; wherein, the Fin width of the upper part of each T-type Fin structure is W2, and W2 = 2*W1; The etching continues until the first AlGaN back barrier layer is reached into the first GaN channel layer, and the portion of the first AlGaN back barrier layer and the portion of the first GaN channel layer directly below the upper part of the T-shaped Fin structure are etched to form the lower part of each T-shaped Fin structure. The upper part of each T-shaped Fin structure and the lower part of its corresponding T-shaped Fin structure constitute the entire T-shaped Fin structure. The Fin width of the lower part of each T-shaped Fin structure is W3, and W3 = 0.6 * W2. Gate metal is deposited around each T-shaped Fin structure and on the surface of the first GaN channel layer to form a gate electrode.

2. The method for fabricating a high linearity device employing a T-type dual-channel structure according to claim 1, characterized in that, Electrically isolated regions are formed at both ends of the device, including: Ion implantation is performed on the surface of the second AlGaN back barrier layer at both ends of the device, with the implantation depth extending into a portion of the GaN buffer layer to form the electrically isolated region.

3. The method for fabricating a high linearity device employing a T-type dual-channel structure according to claim 1, characterized in that, Etching the second AlGaN back barrier layer until the surface of the first AlGaN back barrier layer forms the upper part of each T-type Fin structure includes: The second AlGaN back barrier layer is etched using a dry etching method until the upper part of each T-shaped Fin structure is formed on the surface of the first AlGaN back barrier layer.

4. The method for fabricating a high linearity device employing a T-type dual-channel structure according to claim 3, characterized in that, The process of etching the second AlGaN back barrier layer down to the surface of the first AlGaN back barrier layer using a dry etching method includes: The process parameters used in the ICP etching equipment include: etching gas is BCl3 / Cl2, flow rate is 20 / 8 sccm, pressure is 5 mTorr, ICP power is 50W, and RF power is 15W.

5. The method for fabricating a high linearity device employing a T-type dual-channel structure according to claim 1, characterized in that, Etching the first AlGaN back barrier layer down to the first GaN channel layer includes: The first AlGaN back barrier layer is etched into the first GaN channel layer using a dry etching method.

6. The method for fabricating a high linearity device employing a T-type dual-channel structure according to claim 5, characterized in that, The process of etching the first AlGaN back barrier layer down to the first GaN channel layer using a dry etching method includes: The process parameters used in the ICP etching equipment include: etching gas is BCl3 / Cl2, flow rate is 20 / 8 sccm, pressure is 10 mTorr, ICP power is 50W, and RF power is 15W.

7. The method for fabricating a high linearity device employing a T-type dual-channel structure according to claim 1, characterized in that, Etching a portion of the first AlGaN back barrier layer and a portion of the first GaN channel layer directly below the upper part of the T-shaped Fin structure, including: The first AlGaN back barrier layer and part of the first GaN channel layer are etched directly below the upper part of the T-shaped Fin structure using a wet etching method.

8. The method for fabricating a high linearity device employing a T-type dual-channel structure according to claim 1, characterized in that, The upper part of each T-shaped Fin structure has a thickness of H1, where H1 is the sum of the thicknesses of the second AlGaN back barrier layer and the second GaN channel layer; the lower part of each T-shaped Fin structure has a thickness of H2, where H2 is the sum of the thicknesses of the first AlGaN back barrier layer and a portion of the first GaN channel layer, and H2... <H1。 9. A high linearity device employing a T-type dual-channel structure, characterized in that, The device includes: The epitaxial structure includes, from bottom to top, a SiC substrate, a GaN buffer layer, a first GaN channel layer, a first AlGaN back barrier layer, a second GaN channel layer, and a second AlGaN back barrier layer. The source electrode and drain electrode are located on the upper surface of the second AlGaN back barrier layer, respectively. An electrical isolation region is located at both ends of the device and is adjacent to the source electrode and the drain electrode; A SiN passivation layer is located on the source electrode, the drain electrode, the second AlGaN back barrier layer, and the upper surface of the electrically isolated region; Several T-shaped Fin structures are provided, with a distance of W1 between adjacent T-shaped Fin structures. Each T-shaped Fin structure includes an upper part and a lower part. The upper part of each T-shaped Fin structure penetrates the SiN passivation layer and includes the second AlGaN back barrier layer and the second GaN channel layer. The lower part of each T-shaped Fin structure includes the first AlGaN back barrier layer and part of the first GaN channel layer. The Fin width of the upper part of each T-shaped Fin structure is W2, and the Fin width of the lower part of each T-shaped Fin structure is W3, where W2 = 2 * W1 and W3 = 0.6 * W2. The gate electrode is located on the periphery of each T-shaped Fin structure and on the upper surface of the first GaN channel layer.

10. The high linearity device employing a T-type dual-channel structure according to claim 9, characterized in that, The upper part of each T-shaped Fin structure has a thickness of H1, where H1 is the sum of the thicknesses of the second AlGaN back barrier layer and the second GaN channel layer; the lower part of each T-shaped Fin structure has a thickness of H2, where H2 is the sum of the thicknesses of the first AlGaN back barrier layer and a portion of the first GaN channel layer, and H2... <H1。

Citation Information

Patent Citations

  • GaN-based nanometer channel transistor with high electron mobility and manufacture method

    CN105762078A

  • AlGaN / GaN high electron mobility transistor with multi-channel fin-type structure

    CN109285885A