Axle counter cable preparation method and axle counter cable
By heating the shielding layer and coating it with aerogel and melamine materials to form a multi-layer protective structure, the problem of gaps between the insulation layer and the shielding layer of the reel cable is solved, improving the bonding strength and insulation performance.
Patent Information
- Application Number
- CN202311310744.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-10-10
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2043-10-10
AI Technical Summary
Gaps can easily appear between the insulation and shielding layers of existing reel cables, affecting the protective effect of the insulation layer.
A heated shielding layer is heated to 110°C to 150°C, and molten aerogel is coated on its outside to form an aerogel protective layer. A mixture of silicate aerogel, heat insulation filler and modifier is used, and the aerogel protective layer is formed by extrusion through a screw extruder. Melamine material is then coated on the outside to form a multi-layer protective structure.
It improves the bonding strength between the aerogel and the shielding layer, reduces gaps, enhances the adhesion and stability, improves insulation performance, and provides good insulation and protection.
Smart Images

Figure CN117497255B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of cables, and in particular to a method for preparing an axle counting cable and the axle counting cable. Background Art
[0002] The axle counting cable generally includes a unit cable core and a protective layer wrapped around the outer side of the unit cable core. The protective layer of the current axle counting cable generally includes a shielding layer and an insulating layer arranged outside the shielding layer. In the prior art, the insulating layer and the shielding layer are easily separated, resulting in a gap between the insulating layer and the shielding layer, which affects the protective effect of the insulating layer. Summary of the invention
[0003] The invention provides a method for preparing an axle counter cable and the axle counter cable, so as to solve the problem that gaps are easily formed between the insulating layer and the shielding layer of the axle counter cable in the prior art.
[0004] According to one aspect of the present invention, a method for preparing an axle counting cable is provided, which comprises the following steps: step 1: preparing a unit cable core of the axle counting cable; step 2: coating a shielding layer on the outside of the unit cable core; step 3: heating the shielding layer to 110°C to 150°C; step 4: coating aerogel in a molten state on the outside of the heated shielding layer to form an aerogel protective layer.
[0005] Furthermore, step 4 also includes: mixing the silicate aerogel, the insulation layer filler and the modifier to form a mixed material, and then extruding the mixed material through a screw extruder to form an aerogel in a molten state.
[0006] Furthermore, the silicate aerogel accounts for 45wt% to 55wt% of the mixed material; the heat insulation layer filler accounts for 25wt% to 35wt% of the mixed material; and the modifier accounts for 15wt% to 25wt% of the mixed material.
[0007] Furthermore, the filler of the heat insulation layer is silicon dioxide; and the modifier is polyethylene resin.
[0008] Furthermore, the extrusion temperature of the aerogel by the screw extruder is set to 50°C to 150°C; the extrusion speed of the aerogel by the screw extruder is set to 1mm / s to 100mm / s; and the extrusion pressure of the aerogel by the screw extruder is set to 10MPa to 100MPa.
[0009] Furthermore, the preparation method also includes: Step 5: coating the melamine material in a molten state on the outer side of the aerogel protective layer to form a melamine protective layer.
[0010] Furthermore, step 5 specifically includes: step 51: coating the melamine material in a molten state and having flame-proof bubbles on the outside of the aerogel protective layer to form a melamine bubble layer; step 52: coating the melamine material in a molten state on the outside of the melamine bubble layer to form a melamine sheath surface layer.
[0011] Furthermore, the thickness of the melamine protective layer is set to 2 mm to 3 mm; the ratio of the thickness of the surface layer of the melamine sheath to the thickness of the melamine protective layer is set to 0.2 to 0.3.
[0012] Furthermore, step 5 specifically includes: step 501: selecting a screw extruder having a first extrusion tube and a second extrusion tube, wherein the second extrusion tube is sleeved on the outside of the first extrusion tube, the first extrusion tube is sleeved on the outside of the aerogel protective layer, melamine material is added to the first extrusion tube and the second extrusion tube respectively, and the first extrusion tube and the second extrusion tube are heated to make the melamine material in the first extrusion tube and the melamine material in the second extrusion tube in a molten state; step 502: injecting flame-retardant gas into the first extrusion tube to form a molten melamine material with flame-retardant bubbles, extruding the molten melamine material with flame-retardant bubbles and coating it on the outside of the aerogel protective layer to form a melamine bubble layer; at the same time, the second extrusion tube is The melamine material in the molten state in the tube is extruded and coated on the outside of the melamine bubble layer to form a melamine sheath surface layer; wherein the first extruded tube has a first feed section, a first melting section and a first discharge section arranged in sequence along the conveying direction of the melamine material, the temperature of the first feed section is set to 80°C to 120°C, the temperature of the first melting section is set to 100°C to 150°C, and the temperature of the first discharge section is set to 110°C to 160°C; the second extruded tube has a second feed section, a second melting section and a second discharge section arranged in sequence along the conveying direction of the melamine material, the temperature of the second feed section is set to 80°C to 120°C, the temperature of the second melting section is set to 100°C to 150°C, and the temperature of the second discharge section is set to 110°C to 160°C.
[0013] Further, step 502 specifically includes: injecting flame retardant gas into the first melting section to form flame retardant bubbles in the molten melamine material in the first extrusion tube, and the injection rate of the flame retardant gas is set to 20 mL / min to 200 mL / min.
[0014] Furthermore, the pore size of the fire-proof bubble is set to 0.08 mm to 0.2 mm; the porosity of the fire-proof bubble is set to 40% to 60%.
[0015] According to another aspect of the present invention, an axle counter cable is provided, which is prepared by the above method.
[0016] By applying the technical solution of the present invention, the molten aerogel is coated on the outside of the heated shielding layer, which can improve the bonding strength of the interface between the aerogel and the shielding layer, reduce the possibility of gaps between the aerogel protective layer and the shielding layer, and improve the firmness and stability of the bonding between the aerogel and the shielding layer. Specifically, when the heating temperature of the shielding layer is lower than 110°C, the effect of improving the interface bonding ability of the shielding layer is limited; when the heating temperature of the shielding layer is higher than 150°C, it may cause damage to the unit cable core. Therefore, this solution sets the heating temperature of the shielding layer to the above range, which will not cause damage to the unit cable core, and can also improve the interface bonding strength between the shielding layer and the aerogel protective layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] The drawings constituting a part of the present application are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings:
[0018] Figure 1 A schematic structural diagram of an axle counting cable prepared according to the method of Embodiment 1 of the present invention is shown.
[0019] The above drawings include the following reference numerals:
[0020] 10. Unit cable core;
[0021] 20. Shielding layer;
[0022] 30. Aerogel protective layer;
[0023] 40. Melamine protective layer; 41. Melamine bubble layer; 42. Melamine sheath surface layer. DETAILED DESCRIPTION
[0024] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. The following description of at least one exemplary embodiment is actually only illustrative and is by no means intended to limit the present invention and its application or use. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0025] Embodiment 1 of the present invention provides a method for preparing an axle counter cable. The structural schematic diagram of the axle counter cable prepared by the method is shown in FIG. Figure 1 As shown, the preparation method comprises the following steps:
[0026] Step 1: preparing a unit cable core 10 of an axle counting cable;
[0027] Step 2: Wrap the shielding layer 20 on the outside of the unit cable core 10;
[0028] Step 3: Heat the shielding layer at 20 to 110°C to 150°C;
[0029] Step 4: Wrap the molten aerogel on the outside of the heated shielding layer 20 to form the aerogel protective layer 30 .
[0030] By applying the technical solution of the present invention, the molten aerogel is coated on the outside of the heated shielding layer 20, which can improve the bonding strength of the interface between the aerogel and the shielding layer 20, reduce the possibility of gaps between the aerogel protective layer 30 and the shielding layer 20, and improve the firmness and stability of the bonding between the aerogel protective layer 30 and the shielding layer 20. Specifically, when the heating temperature of the shielding layer 20 is lower than 110°C, the effect of improving the interface bonding ability of the shielding layer 20 is limited; when the heating temperature of the shielding layer 20 is higher than 150°C, it may cause damage to the unit cable core 10. Therefore, the present solution sets the heating temperature of the shielding layer 20 to the above range, which will not cause damage to the unit cable core 10, and can also improve the interface bonding strength between the shielding layer 20 and the aerogel protective layer 30.
[0031] The present solution does not limit the specific heating method of the shielding layer 20, which can be heated by electric induction heating and open flame heating. In this embodiment, the shielding layer 20 is heated by microwave heating. Heating the shielding layer 20 by microwave heating can make the heat act directly on the shielding layer 20, avoiding adverse effects on the unit cable core 10, and the heating temperature is easy to control, ensuring the uniformity of heating of the shielding layer 20.
[0032] The heating temperature of the shielding layer 20 can be set to 110° C., 120° C., 130° C., 140° C. or 150° C. In this embodiment, the heating temperature of the shielding layer 20 is set to 125° C.
[0033] In this embodiment, the shielding layer 20 is a double steel belt armor layer, the thickness of which is set to 0.2 mm to 0.8 mm, and the gap ratio is set to 30% to 45%. The above setting makes the surface of the shielding layer 20 a non-smooth structure, which can further increase the interface bonding force between the shielding layer 20 and the aerogel protective layer 30.
[0034] The thickness of the double steel belt armor layer can be set to 0.2 mm, 0.3 mm, 0.4 mm, 0.5 mm, 0.6 mm, 0.7 mm or 0.8 mm. In this embodiment, the thickness of the double steel belt armor layer is set to 0.55 mm.
[0035] When the gap ratio of the double steel belt armor layer is less than 30%, it may lead to slow production speed, low production efficiency and waste of materials; when the gap ratio of the double steel belt armor layer is greater than 45%, it may lead to a decrease in shielding performance and the overall ideal shielding coefficient of the cable has the risk of being greater than 0.1. Therefore, this solution sets the gap ratio of the double steel belt armor layer within the above range.
[0036] The gap ratio of the double steel belt armor layer can be set to 30%, 35%, 40% or 45%. In this embodiment, the gap ratio of the double steel belt armor layer is set to 37%.
[0037] Furthermore, step 4 also includes: mixing the silicate aerogel, the insulation layer filler and the modifier to form a mixed material, and then extruding the mixed material through a screw extruder to form an aerogel in a molten state.
[0038] Specifically, in this embodiment, the insulation layer filler is silicon dioxide; the modifier is polyethylene resin. Silicate aerogel accounts for 45wt% to 55wt% of the mixed material; the insulation layer filler accounts for 25wt% to 35wt% of the mixed material; the modifier accounts for 15wt% to 25wt% of the mixed material. By selecting the above materials and proportions, the fire-resistant temperature can be 800℃ to 1000℃, the thermal conductivity is between 0.02W(m·k) and 0.06W(m·k), and the density reaches 0.1g / cm 3 Up to 1.5g / cm 3 , that is, low density and light weight.
[0039] Silicate aerogel has good thermal stability and can withstand high temperature environments. Silica has low thermal conductivity. Adding silica filler can further improve the thermal insulation performance of silicate aerogel and prevent heat conduction. Adding polyethylene resin can improve the flexibility of silicate aerogel and improve the mechanical strength and tear resistance of silicate aerogel. Polyethylene resin has good fluidity and low density. Under the action of polyethylene resin, the fluidity and shape retention ability of aerogel in a molten state can be improved, the overall density of aerogel can be reduced, the weight of the axle meter cable can be reduced, and the suspension ability of the aerogel protective layer 30 can be improved.
[0040] Among them, if the polyethylene resin exceeds the above range, it will affect the hardness and stability of the silicate aerogel, and affect the shape retention and durability of the material. Too much polyethylene resin may increase the thermal conductivity of the material and affect the thermal insulation performance. In addition, too much polyethylene resin may also affect the reactivity and curing process of the silicate aerogel, resulting in incomplete formation of the gel network or insufficient curing, affecting the thermal insulation effect of the aerogel.
[0041] The silicate aerogel may account for 45wt% or 55wt% of the mixed material; the heat insulation layer filler may account for 25wt% or 35wt% of the mixed material; and the modifier may account for 15wt% or 25wt% of the mixed material.
[0042] In this embodiment, the silicate aerogel accounts for 50wt% of the mixed material; the heat insulation layer filler accounts for 30wt% of the mixed material; and the modifier accounts for 20wt% of the mixed material.
[0043] In this embodiment, the porosity of the aerogel protective layer 30 is 5% to 50%. Setting the porosity of the aerogel protective layer 30 within the above range can reduce the thermal conductivity as much as possible while ensuring its mechanical strength. Specifically, setting the ratio of silicate aerogel, silicon dioxide and polyethylene resin within the above range can make the porosity of the aerogel protective layer 30 5 to 50%.
[0044] Specifically, the extrusion temperature of the aerogel by the screw extruder is set to 50°C to 150°C; the extrusion speed of the aerogel by the screw extruder is set to 1mm / s to 100mm / s; the extrusion pressure of the aerogel by the screw extruder is set to 10MPa to 100MPa. In this solution, the experimental parameters of the screw extruder are set within the above range, which can make the aerogel extruded uniformly and with good consistency, so that it has excellent thermal insulation, fire resistance and mechanical properties. The thermal conductivity reaches 0.02-0.06W / (m·K), the resistance performance can reach 800 to 1000°C, and the compression strength can reach 1 to 10MPa.
[0045] In this scheme, the extrusion temperature of the aerogel by the screw extruder can be set to 90°C, 100°C, 110°C, 120°C, 125°C, 130°C, 135°C, 140°C, 145°C or 150°C; the extrusion speed of the aerogel by the screw extruder can be set to 1mm / s, 10mm / s, 20mm / s, 30mm / s, 40mm / s, or 100mm / s; the extrusion pressure of the aerogel by the screw extruder can be set to 10MPa, 30MPa, 60MPa, 80MPa or 100MPa.
[0046] Furthermore, the difference between the temperature of the molten aerogel extruded by the screw extruder and the temperature of the heated shielding layer 20 does not exceed 15° C. Since the shielding layer 20 is made of metal, when the difference between the temperature of the molten aerogel and the temperature of the heated shielding layer 20 exceeds 15° C., the interface bonding force between the molten aerogel and the heated shielding layer 20 may be affected, that is, thermal stress is generated. Under the action of long-term thermal stress, the interface will crack or separate, thereby affecting the bonding stability of the two.
[0047] In this solution, the preparation method further includes: Step 5: coating the molten melamine material on the outside of the aerogel protective layer 30 to form a melamine protective layer 40. The provision of the melamine protective layer 40 can further enhance the protection effect of the shielding layer 20 and the unit cable core 10.
[0048] Specifically, step 5 includes:
[0049] Step 51: coating the outer side of the aerogel protective layer 30 with a melamine material having flame-retardant bubbles in a molten state to form a melamine bubble layer 41;
[0050] Step 52 : coating the melamine material in a molten state on the outside of the melamine bubble layer 41 to form a melamine jacket surface layer 42 ; the melamine bubble layer 41 and the melamine jacket surface layer 42 form a melamine protective layer 40 .
[0051] In this solution, the melamine bubble layer 41 is arranged between the melamine jacket surface layer 42 and the aerogel protective layer 30, which can provide good insulation performance, and the bubble structure can prevent the conduction of heat and electricity, protecting the safe operation of the cable. The setting of the melamine bubble layer 41 can also achieve a lower density, so that the axle counting cable can be lightweight, reduce the overall weight, and facilitate installation and transportation. In addition, the melamine bubble layer 41 has good softness and elasticity, can adapt to axle counting cables of different shapes and curves, and provide good anti-obstruction performance.
[0052] In this solution, the melamine sheath surface layer 42 is arranged on the outside of the melamine bubble layer 41, which can protect the melamine bubble layer 41, provide better sealing performance, and reduce or avoid the influence of moisture, dust and other external factors on the cable.
[0053] Furthermore, the thickness of the melamine protective layer 40 is set to 2 mm to 3 mm; the ratio of the thickness of the melamine sheath surface layer 42 to the thickness of the melamine protective layer 40 is set to 0.2 to 0.3.
[0054] The thickness of the melamine protective layer 40 can be set to 2 mm, 2.3 mm, 2.5 mm, 2.7 mm or 3 mm. In this embodiment, the thickness of the melamine protective layer 40 is set to 2.5 mm.
[0055] In the present embodiment, when the ratio of the thickness of the melamine sheath surface layer 42 to the thickness of the melamine protective layer 40 is lower than 0.2, the thickness of the melamine sheath surface layer 42 may be too thin, affecting the protective effect of the melamine bubble layer 41; when the ratio of the thickness of the melamine sheath surface layer 42 to the thickness of the melamine protective layer 40 is higher than 0.3, the thickness of the melamine bubble layer 41 may be too thin, affecting the flame retardant effect of the melamine bubble layer 41.
[0056] The ratio of the thickness of the melamine sheath surface layer 42 to the melamine protective layer 40 can be set to 0.2, 0.25 or 0.3. In this embodiment, the ratio of the thickness of the melamine sheath surface layer 42 to the melamine protective layer 40 is set to 0.25.
[0057] In this embodiment, step 5 specifically includes:
[0058] Step 501: selecting a screw extruder having a first extrusion tube and a second extrusion tube, wherein the second extrusion tube is sleeved on the outside of the first extrusion tube, the first extrusion tube is sleeved on the outside of the aerogel protective layer 30, adding melamine material to the first extrusion tube and the second extrusion tube respectively, and heating the first extrusion tube and the second extrusion tube so that the melamine material in the first extrusion tube and the melamine material in the second extrusion tube are in a molten state;
[0059] Step 502: injecting flame-retardant gas into the first extrusion tube to form a molten melamine material with flame-retardant bubbles, extruding the molten melamine material with flame-retardant bubbles and coating it on the outside of the aerogel protective layer 30 to form a melamine bubble layer 41; at the same time, extruding the molten melamine material in the second extrusion tube and coating it on the outside of the melamine bubble layer 41 to form a melamine sheath surface layer 42;
[0060] The first extrusion tube has a first feeding section, a first melting section and a first discharging section which are sequentially arranged along the conveying direction of the melamine material, the temperature of the first feeding section is set to 80°C to 120°C, the temperature of the first melting section is set to 100°C to 150°C, and the temperature of the first discharging section is set to 110°C to 160°C;
[0061] The second extrusion tube has a second feed section, a second melting section and a second discharge section arranged in sequence along the conveying direction of the melamine material. The temperature of the second feed section is set to 80°C to 120°C, the temperature of the second melting section is set to 100°C to 150°C, and the temperature of the second discharge section is set to 110°C to 160°C.
[0062] In this solution, the melamine material in the first extrusion tube and the melamine material in the second extrusion tube are the same material, and the temperature range of the first extrusion tube is the same as the temperature range of the second extrusion tube. Such an arrangement can ensure processing efficiency. In addition, the above arrangement can improve the firmness of the connection between the melamine bubble layer 41 and the melamine sheath surface layer 42 during molding, and improve the chemical corrosion resistance, waterproof and moisture-proof performance of the melamine protective layer 40 as a whole.
[0063] The temperature of the first feeding section can be set to 80°C, 90°C, 110°C or 120°C, the temperature of the first melting section can be set to 100°C, 110°C, 120°C, 130°C or 150°C, and the temperature of the first discharging section can be set to 110°C, 120°C, 130°C, 150°C or 160°C;
[0064] The temperature of the second feeding section can be set to 80°C, 90°C, 110°C or 120°C, the temperature of the second melting section can be set to 100°C, 110°C, 120°C, 130°C or 150°C, and the temperature of the second discharging section can be set to 110°C, 120°C, 130°C, 150°C or 160°C;
[0065] In this embodiment, the temperature of the first feed section is set to 110°C, the temperature of the first melting section is set to 120°C, and the temperature of the first discharging section is set to 150°C; the temperature of the second feed section is set to 110°C, the temperature of the second melting section is set to 110°C, and the temperature of the second discharging section is set to 160°C.
[0066] In this solution, the aerogel protective layer, the melamine bubble layer 41 and the melamine jacket surface layer 42 are formed at one time by three-layer co-extrusion.
[0067] Specifically, the screw extruder also includes a third extrusion tube, which is inserted into the first extrusion tube, and the third extrusion tube is coaxially arranged with the first extrusion tube. The third extrusion tube is used to be sleeved on the outside of the shielding layer 20, and a mixture formed by mixing silicate aerogel, thermal insulation layer filler and modifier is added to the third extrusion tube. Such an arrangement can improve the processing efficiency of the aerogel protective layer, the melamine bubble layer 41 and the melamine sheath surface layer 42, and improve the coaxiality of the three. In addition, during molding, the stability of the connection between the molten aerogel and the molten polyurethane is stronger.
[0068] Further, step 502 specifically includes: injecting flame retardant gas into the first melting section to form flame retardant bubbles in the melted melamine material in the first extrusion tube, and the injection rate of the flame retardant gas is set to 20mL / min to 200mL / min. The injection of the flame retardant gas can increase the stirring and dispersion effect of the melamine material in the first extrusion tube, promote the melting and mixing of the material, help improve the melting efficiency, and reduce the processing time of the first melting section.
[0069] In this scheme, when the injection speed of the flame-retardant gas is lower than 20 mL / min, the gas may not be able to enter effectively and the pores may not be dense; when the injection speed of the flame-retardant gas is higher than 200 mL / min, the generated pores may stick to each other and bubble. Therefore, this scheme sets the injection speed of the flame-retardant gas within the above range.
[0070] The injection rate of the flame retardant gas can be set to 20 mL / min, 60 mL / min, 80 mL / min, 100 mL / min, 120 mL / min, 160 mL / min or 200 mL / min. In this embodiment, the injection rate of the flame retardant gas is set to 150 mL / min.
[0071] This solution injects flame-retardant gas into the first extrusion tube by supersonic pumping. This arrangement can ensure that the bubbles are evenly distributed throughout the material, avoiding bubble aggregation and local unevenness, improving the density and uniformity of the material, and improving the balance between its density and strength. In addition, supersonic pumping can introduce a cooling effect in the first melting section, and the injection of gas will take away some heat, thereby reducing the temperature of the material and improving the thermal stability and anti-aging performance of the material.
[0072] Furthermore, the pore size of the fire-proof bubble is set to 0.08 mm to 0.2 mm; the porosity of the fire-proof bubble is set to 40% to 60%.
[0073] When the pore diameter of the flame-retardant bubble is less than 0.08 mm, it may be difficult to form a flame-retardant bubble. When the pore diameter of the flame-retardant bubble is greater than 0.2 mm, the pore diameter of the flame-retardant bubble may be too large, causing the melamine bubble layer 41 to be easily damaged and the structural strength to be low. Therefore, this scheme sets the pore diameter of the flame-retardant bubble within the above range.
[0074] When the porosity of the flame retardant bubble is lower than 40%, there may be too little flame retardant gas to effectively achieve the flame retardant effect. When the porosity of the flame retardant bubble is higher than 60%, the mechanical properties may be reduced and the cable may break during installation. Therefore, the porosity of the flame retardant bubble is set within the above range in this solution.
[0075] In summary, the method for preparing an axle counter cable provided in this solution specifically includes:
[0076] 1. preparing a unit cable core 10 of an axle counting cable;
[0077] 2. Wrap the shielding layer 20 on the outside of the unit cable core 10;
[0078] 3. Heating shield layer 20 to 110°C to 150°C;
[0079] Fourth, the third extrusion tube of the screw extruder is set on the outside of the shielding layer 20, the working parameters of the screw extruder are set, the screw extruder is started, and the mixture of silicate aerogel, silicon dioxide and polyethylene resin is added into the third extrusion tube of the screw extruder; the melamine material is added into the first extrusion tube and the second extrusion tube of the screw extruder respectively; the flame-retardant gas is injected into the first melting section of the first extrusion tube; the first extrusion tube, the second extrusion tube and the third extrusion tube extrude the materials at the same time to form the aerogel protective layer 30, the melamine bubble layer 41 and the melamine sheath surface layer 42 respectively.
[0080] The flame retardant gas may be carbon dioxide or nitrogen. In this embodiment, the flame retardant gas is carbon dioxide.
[0081] A second embodiment of the present invention provides an axle counting cable, which is prepared by the above method.
[0082] It should be noted that the terms used herein are only for describing specific embodiments and are not intended to limit the exemplary embodiments according to the present application. As used herein, unless the context clearly indicates otherwise, the singular form is also intended to include the plural form. In addition, it should be understood that when the terms "comprise" and / or "include" are used in this specification, it indicates the presence of features, steps, operations, devices, components and / or combinations thereof.
[0083] Unless otherwise specifically stated, the relative arrangement of the parts and steps described in these embodiments, numerical expressions and numerical values do not limit the scope of the present invention. At the same time, it should be understood that, for ease of description, the sizes of the various parts shown in the accompanying drawings are not drawn according to the actual proportional relationship. The technology, method and equipment known to ordinary technicians in the relevant field may not be discussed in detail, but in appropriate cases, the technology, method and equipment should be regarded as a part of the authorization specification. In all examples shown and discussed here, any specific value should be interpreted as being merely exemplary, rather than as a limitation. Therefore, other examples of exemplary embodiments may have different values. It should be noted that similar reference numerals and letters represent similar items in the following drawings, so once a certain item is defined in an accompanying drawing, it does not need to be further discussed in subsequent drawings.
[0084] In the description of the present invention, it is necessary to understand that the directions or positional relationships indicated by directional words such as "front, back, up, down, left, right", "lateral, vertical, perpendicular, horizontal" and "top, bottom" are usually based on the directions or positional relationships shown in the drawings. They are only for the convenience of describing the present invention and simplifying the description. Unless otherwise specified, these directional words do not indicate or imply that the devices or elements referred to must have a specific direction or be constructed and operated in a specific direction. Therefore, they cannot be understood as limiting the scope of protection of the present invention. The directional words "inside and outside" refer to the inside and outside relative to the contours of each component itself.
[0085] For ease of description, spatially relative terms such as "above", "above", "on the upper surface of", "above", etc. may be used here to describe the spatial positional relationship between a device or feature and other devices or features as shown in the figure. It should be understood that spatially relative terms are intended to include different orientations of the device in use or operation in addition to the orientation described in the figure. For example, if the device in the accompanying drawings is inverted, the device described as "above other devices or structures" or "above other devices or structures" will be positioned as "below other devices or structures" or "below other devices or structures". Thus, the exemplary term "above" can include both "above" and "below". The device can also be positioned in other different ways (rotated 90 degrees or in other orientations), and the spatially relative descriptions used here are interpreted accordingly.
[0086] In addition, it should be noted that the use of terms such as "first" and "second" to limit components is only for the convenience of distinguishing the corresponding components. If not otherwise stated, the above terms have no special meaning and therefore cannot be understood as limiting the scope of protection of the present invention.
[0087] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A method for preparing an axle counting cable, characterized in that: The following steps are involved: Step 1: preparing a unit cable core (10) of an axle counting cable; Step 2: Wrapping a shielding layer (20) on the outside of the unit cable core (10); Step 3: heating the shielding layer (20) to 110° C. to 150° C.; Step 4: coating the molten aerogel on the outside of the heated shielding layer (20) to form an aerogel protective layer (30), wherein the difference between the temperature of the molten aerogel and the temperature of the heated shielding layer (20) does not exceed 15° C.; Step 5: coating the outer side of the aerogel protective layer (30) with melamine material in a molten state to form a melamine protective layer (40); The step 5 specifically includes: Step 51: coating the outer side of the aerogel protective layer (30) with a melamine material in a molten state and having flame-proof bubbles to form a melamine bubble layer (41); Step 52: Covering the outer side of the melamine bubble layer (41) with molten melamine material to form a melamine sheath surface layer (42); The aerogel protective layer (30), the melamine bubble layer (41) and the melamine jacket surface layer (42) are formed at one time by three-layer co-extrusion; the melamine bubble layer (41) and the melamine jacket surface layer (42) are made of the same melamine material, and the temperature ranges of the extrusion processes of the melamine bubble layer (41) and the melamine jacket surface layer (42) are the same.
2. The preparation method according to claim 1, characterized in that: The step 4 also includes: The silicate aerogel, the insulation layer filler and the modifier are mixed to form a mixed material, and then the mixed material is extruded through a screw extruder to form the aerogel in a molten state.
3. The preparation method according to claim 2, characterized in that: The silicate aerogel accounts for 45wt% to 55wt% of the mixed material; The insulation layer filler accounts for 25wt% to 35wt% of the mixed material; The modifier accounts for 15 wt % to 25 wt % of the mixed material.
4. The preparation method according to claim 2, characterized in that: The heat insulation layer filler is silicon dioxide; The modifier is polyethylene resin.
5. The preparation method according to claim 2, characterized in that: The screw extruder sets the extrusion temperature of the aerogel to 100° C. to 150° C.; The screw extruder is configured to extrude the aerogel at a speed of 1 mm / s to 100 mm / s; The extrusion pressure of the screw extruder on the aerogel is set to 10 MPa to 100 MPa.
6. The preparation method according to claim 1, characterized in that: The thickness of the melamine protective layer (40) is set to 2 mm to 3 mm; The ratio of the thickness of the melamine sheath surface layer (42) to the thickness of the melamine protective layer (40) is set to 0.2 to 0.
3.
7. The preparation method according to claim 6, characterized in that: The step 5 specifically includes: Step 501: selecting a screw extruder having a first extrusion tube and a second extrusion tube, wherein the second extrusion tube is sleeved on the outside of the first extrusion tube, the first extrusion tube is sleeved on the outside of the aerogel protective layer (30), melamine material is added to the first extrusion tube and the second extrusion tube respectively, and the first extrusion tube and the second extrusion tube are heated so that the melamine material in the first extrusion tube and the melamine material in the second extrusion tube are in a molten state; Step 502: injecting flame-retardant gas into the first extrusion tube to form the melamine material in a molten state with flame-retardant bubbles, extruding the melamine material in a molten state with flame-retardant bubbles and coating the melamine bubble layer (41) on the outside of the aerogel protective layer (30); at the same time, extruding the melamine material in a molten state in the second extrusion tube and coating the melamine bubble layer (41) on the outside of the melamine bubble layer (41) to form the melamine sheath surface layer (42); Wherein, the first extrusion tube has a first feeding section, a first melting section and a first discharging section which are sequentially arranged along the conveying direction of the melamine material, the temperature of the first feeding section is set to 80°C to 120°C, the temperature of the first melting section is set to 100°C to 150°C, and the temperature of the first discharging section is set to 110°C to 160°C; The second extrusion tube has a second feed section, a second melting section and a second discharge section which are sequentially arranged along the conveying direction of the melamine material. The temperature of the second feed section is set to 80°C to 120°C, the temperature of the second melting section is set to 100°C to 150°C, and the temperature of the second discharge section is set to 110°C to 160°C.
8. The preparation method according to claim 7, characterized in that: The step 502 specifically includes: A flame retardant gas is injected into the first melting section to form flame retardant bubbles in the molten melamine material in the first extrusion tube, and the injection rate of the flame retardant gas is set to 20 mL / min to 200 mL / min.
9. The preparation method according to claim 1, characterized in that: The aperture of the flame retardant bubble is set to 0.08 mm to 0.2 mm; The porosity of the fire-resistant bubbles is set to 40% to 60%.
10. An axle counting cable, characterized in that: The axle counter cable is prepared by the preparation method according to any one of claims 1 to 9.