Glass-based circuit board and its preparation method and maintenance method
By using optical adhesive layers and film layers containing thermal expansion materials on glass-based circuit boards, the problem that the glass substrate is easily broken and difficult to repair during the packaging process is solved, and the effect is achieved that is not easy to break and is easy to repair.
Patent Information
- Application Number
- CN202311868553.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-29
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2043-12-29
AI Technical Summary
During the packaging process of traditional LED substrates, the glass substrate is easily broken due to the pressure exerted and the curing shrinkage of the epoxy resin. Moreover, it is difficult to repair after being film-coated and encapsulated, resulting in failed LED chips that cannot be replaced.
A glass-based circuit board including a laminated first optical adhesive layer and an optical film layer is used. The first optical adhesive layer contains thermal expansion materials such as vermiculite and thermal expansion microspheres. The bonding force between the adhesive layer and the substrate surface is reduced by heating to facilitate peeling, thereby realizing glass The base plate is fragile and easy to repair.
It effectively prevents the glass substrate from shattering due to pressure and shrinkage during the packaging process, allows subsequent reliable repair of faulty LED chips, and avoids the problem of splinters caused by peeling off the adhesive film.
Smart Images

Figure CN117812820B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of circuit boards, and in particular to a glass-based circuit board and a preparation method and a maintenance method thereof. Background Art
[0002] At present, the packaging of traditional LED substrates generally adopts two methods. Method 1: Molding packaging, which adopts epoxy resin curing packaging. Method 2: Film packaging, which adopts semi-cured film bonding and curing packaging. For method 1, it has at least two technical defects: First, the molding process needs to apply a large pressure, which may easily cause the glass substrate to break during the pressure application process; Second, due to the obvious shrinkage phenomenon in the epoxy resin curing process, the glass substrate warps and generates stress, which leads to the breakage of the glass substrate. For method 2, it has at least one technical defect: First, after laminating, the semi-cured film cannot be removed, or during the removal process, tearing off the semi-cured film may easily cause the glass substrate to crack due to stress, resulting in the inability to perform subsequent repairs on the faulty LED chips on the glass-based circuit board.
[0003] Therefore, there is an urgent need to provide a glass-based circuit board whose glass substrate is not easy to break and is easy to subsequently repair, as well as a preparation method and a repair method thereof. Summary of the invention
[0004] The present invention aims at the shortcomings of the existing glass-based circuit boards in the prior art that the glass substrates are easy to break and difficult to repair subsequently. To achieve one purpose of the present invention, a glass-based circuit board is provided, comprising: a glass substrate, which includes a substrate surface, on which a conductive circuit and a plurality of light-emitting chips are arranged; an optical adhesive film, which includes a stacked first optical adhesive layer and an optical film layer, the first optical adhesive layer includes a thermal expansion material, and the optical film layer has a transmittance of 30 to 90%; the optical adhesive film is adhered to the substrate surface through the first optical adhesive layer.
[0005] Furthermore, the thermal expansion material includes at least one of vermiculite and thermal expansion microspheres. The first optical adhesive layer uses acrylic optical adhesive as a base material. Vermiculite and / or thermal expansion microspheres are mixed inside the acrylic optical adhesive. The diameter of the vermiculite is set to 20 to 100 μm, the diameter of the thermal expansion microspheres is set to 20 to 40 μm, the outer shell of the thermal expansion microspheres is thermoplastic plastic, and alkane gas is sealed inside.
[0006] Furthermore, the total thickness of the first optical adhesive layer and the second optical adhesive layer is 150-300 μm, the thickness of the first optical adhesive layer is ≥40 μm, and the thickness of the second optical adhesive layer is >0 μm.
[0007] Furthermore, the glass-based circuit board also includes a bottom black ink layer arranged on the substrate surface and a carbon black layer arranged between the optical film layer and the second optical adhesive layer, and the first optical adhesive layer is attached to the bottom black ink layer.
[0008] Furthermore, the optical film layer is made of a polymer film, and the surface of the optical film layer is treated with AG or / and HC and has a glossiness of 60°≤10%.
[0009] To achieve another object of the present invention, a method for preparing a glass-based circuit board is provided, which is applicable to any of the above glass-based circuit boards and includes the following steps: S110: providing a glass substrate having a conductive circuit and a plurality of light-emitting chips arranged on its substrate surface; S130: preparing an optical adhesive film, which includes: S131: providing an optical film layer with a transmittance of 30 to 90%; S133: arranging a first optical adhesive layer including a thermal expansion material on a first side of the optical film layer; S150: attaching the first optical adhesive layer of the optical adhesive film to the substrate surface to cover the conductive circuit and the plurality of light-emitting chips arranged on the substrate surface.
[0010] Furthermore, step S132 is included between step S131 and step S133, and step S132 includes: coating a second optical adhesive layer on the optical film layer; S133 includes: coating the first optical adhesive layer on the second optical adhesive layer, so that the first optical adhesive layer is arranged on the first side of the optical film layer; step S130 also includes: S135: performing AG treatment and / or HC treatment on the surface of the optical film layer.
[0011] To achieve another object of the present invention, a repair method for a glass-based circuit board is provided, which is applied to any of the above glass-based circuit boards, where there is at least one faulty light-emitting chip that cannot work normally among multiple light-emitting chips, and the repair method includes: S210: heating the glass substrate to cause the heat-expanding material in the first optical adhesive layer of the optical adhesive film to expand due to the heat until the bonding force between the first optical adhesive layer and the substrate surface is reduced to the point where the two can be relatively peeled off; S220: peeling the first optical adhesive layer and the optical film layer together relative to the glass substrate; S230: removing the faulty light-emitting chip and replacing it with a new light-emitting chip; S240: pasting a new optical adhesive film on the substrate surface.
[0012] Furthermore, the heating of the glass substrate in step S210 includes: when the thermal expansion material in the first optical adhesive layer is vermiculite, heating is performed at a heating temperature of 150 to 300°C and a heating time of 10 to 15 minutes; when the thermal expansion material in the first optical adhesive layer is thermal expansion microspheres, heating is performed at a heating temperature of 120 to 180°C and a heating time of 10 to 15 minutes; when the thermal expansion material in the first optical adhesive layer is a mixture of vermiculite and thermal expansion microspheres, heating is performed at a heating temperature of 150 to 180°C and a heating time of 10 to 15 minutes.
[0013] The beneficial effects of the present invention are:
[0014] The glass-based circuit board and its preparation method and maintenance method ensure that the glass substrate is not easy to break by pasting a stacked first optical adhesive layer and an optical film layer on the substrate surface of the glass substrate without using epoxy resin in the prior art to cure the package; if at least one light-emitting chip of the glass-based circuit board fails and needs to be repaired, the glass substrate is heated to expand the thermal expansion material of the first optical adhesive layer so that the bonding force between the first optical adhesive layer and the substrate surface can be reduced to the point where the two can be relatively peeled off, thereby ensuring that the glass-based circuit board is not only easy to repair later but also the glass substrate will not be cracked due to stress. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] In order to more clearly illustrate the technical solution of the embodiment of the present invention, the drawings required for use in the embodiment of the present invention will be briefly introduced below. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work, and these are all within the protection scope of the present invention.
[0016] Figure 1 A schematic diagram of the layer structure of an embodiment of a glass-based circuit board provided by an embodiment of the present invention, omitting the thermosetting anti-glare layer;
[0017] Figure 2 A schematic diagram of another embodiment of a glass-based circuit board provided by an embodiment of the present invention and omitting the layer structure of the glass substrate;
[0018] Figure 3 Schematic diagram of a process for preparing a glass-based circuit board provided in an embodiment of the invention
[0019] Figure 4 Schematic diagram of a process for repairing a glass-based circuit board provided by an embodiment of the invention
[0020] Description of reference numerals:
[0021] 1-glass substrate; 2-first optical adhesive layer; 3-second optical adhesive layer; 4-optical film layer; 5-thermosetting anti-glare layer; 6-thermal expansion material; 7-diffusion powder; 8-light-emitting chip. DETAILED DESCRIPTION
[0022] In order to make the purpose, technical solution and advantages of the embodiment of the present invention clearer, the technical solution in the embodiment of the present invention will be clearly and completely described in conjunction with the drawings in the embodiment of the present invention. It should be noted that, in this article, relational terms such as first and second are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply that there is any such actual relationship or order between these entities or operations. In the description of the present invention, it should be understood that the orientation or position relationship indicated by the terms "center", "upper", "lower", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc. is based on the orientation or position relationship shown in the drawings, which is only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present invention. Moreover, the term "include", "comprise" or any other variant thereof is intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also includes other elements not explicitly listed, or also includes elements inherent to such a process, method, article or device. In the absence of further restrictions, the elements defined by the phrase "comprising..." do not exclude the existence of other identical elements in the process, method, article or device comprising the elements. If there is no conflict, the embodiments of the present invention and the various features in the embodiments can be combined with each other and are all within the protection scope of the present invention.
[0023] refer to Figure 1As an object of the present invention, a glass-based circuit board is provided. In one embodiment, the glass-based circuit board includes a glass substrate 1 and an optical adhesive film, and the optical adhesive film includes a stacked first optical adhesive layer 2 and an optical film layer 4. The optical adhesive film includes various adhesive layers and film layers located in the light emitting direction of the light-emitting chip and can be independently prepared by the following preparation method. Among them, the glass substrate 1 includes a substrate surface, on which a conductive circuit and a plurality of light-emitting chips 8 are arranged. The light-emitting chip 8 can specifically be Mini LED or Micro LED. The first optical adhesive layer 2 includes a thermal expansion material 6. It should be noted that the thermal expansion material 6 is uniformly distributed in the first optical adhesive layer 2. The optical film layer 4 has a transmittance of 30 to 90%. The first optical adhesive layer 2 is attached to the substrate surface so that the optical adhesive film is attached to the substrate surface, so that the optical film layer 4 is located on the side of the first optical adhesive layer 2 facing away from the substrate surface. It should be noted that the various layers of the optical adhesive film described herein may be directly or indirectly connected to each other when there is no conflict or impracticability. In addition, the first optical adhesive layer attached to the substrate surface includes being directly attached to the substrate surface or being indirectly attached to the substrate surface by being attached to, for example, a bottom black ink layer on the substrate surface. Specifically, in this embodiment, the first optical adhesive layer 2 and the optical film layer 4 may be directly or indirectly disposed on the adjacent substrate surface and the side surface of the first optical adhesive layer 2, respectively. Therefore, the glass-based circuit board of the present invention is configured to attach an optical adhesive film having a first optical adhesive layer 2 and an optical film layer 4 stacked in parallel above the substrate surface of the glass substrate 1. On the one hand, since epoxy resin curing encapsulation is not used, it can prevent the unfavorable situation that the glass substrate 1 is broken due to the application of a large pressure during the molding process using epoxy resin in the prior art, and the glass substrate 1 will not be warped and broken due to the obvious shrinkage phenomenon of epoxy resin curing, thereby ensuring that the glass substrate 1 is not easy to break. On the other hand, since the first optical adhesive layer attached to the glass substrate 1 The optical adhesive layer 2 contains heat expansion material 6, so if at least one light emitting chip 8 of the glass-based circuit board fails and needs to be repaired later, the glass substrate 1 is heated to expand the heat expansion material 6, so that the bonding force between the first optical adhesive layer 2 and the substrate surface can be reduced to the point where the two can be relatively peeled off, so that the optical adhesive film can be relatively peeled off relative to the glass substrate, thereby avoiding the unfavorable situation of traditional film packaging that the glass substrate 1 is easily cracked due to force when the semi-cured adhesive film is torn off, resulting in the failure of the light emitting chip 8 being unable to be repaired, thereby ensuring that the glass-based circuit board is easy to repair later.
[0024] Specifically, the heat expansion material 6 includes at least one of vermiculite and heat expansion microspheres. The first optical adhesive layer 2 uses acrylic optical adhesive as a base material. In addition, inorganic or organic diffusion powder can be mixed in the acrylic optical adhesive to play a role in light uniformity. Vermiculite and / or heat expansion microspheres are mixed inside the acrylic optical adhesive. The vermiculite and / or heat expansion microspheres are evenly distributed in the acrylic optical adhesive. The diameter of the vermiculite is set to 20 to 100 μm, and the diameter of the heat expansion microspheres is set to 20 to 40 μm. Due to the characteristics of the vermiculite itself, when, for example, the glass substrate 1 is heated and heat is transferred to the first optical adhesive layer 2 to heat the vermiculite, its volume will expand. The shell of the heat expansion microsphere is a thermoplastic plastic, and an alkane gas is sealed inside. Similarly, when, for example, the glass substrate 1 is heated, the shell of the heat expansion microsphere becomes soft due to the heat, and the alkane gas inside expands due to the heat. Therefore, both vermiculite and heat-expandable microspheres can expand in volume when heated, thereby reducing or even eliminating the bonding force between the first optical adhesive layer 2 and the glass substrate 1, so that the first optical adhesive layer 2 can be separated from the glass substrate 1 while minimizing the risk of cracking of the glass substrate 1 due to uneven force.
[0025] Preferably, combined with reference Figure 2 , the optical adhesive film also includes a second optical adhesive layer 3 arranged between the first optical adhesive layer 2 and the optical film layer 4. It should be noted that the second optical adhesive layer 3 does not have the above-mentioned thermal expansion material 6, thereby preventing the glass substrate 1 from being heated and causing the thermal expansion material 6 in the second optical adhesive layer 3 to expand and apply force to press the first optical adhesive layer 2 against the glass substrate 1, resulting in the first optical adhesive layer 2 being difficult to separate from the glass substrate 1. The second optical adhesive layer 3 uses acrylic optical adhesive as a base material, and inorganic or organic diffusion powder 7 can be mixed inside the acrylic optical adhesive. The mass percentage of the diffusion powder 7 in the acrylic optical adhesive is 5 to 20wt%, and the particle size of the diffusion powder 7 is 1.5 to 3μm. By mixing the diffusion powder 7 that meets the mass percentage and particle size value inside the acrylic optical adhesive, for example, the RGB three-color Mini LED and MicroLED light can be homogenized, so that the light intensity of each monochromatic light at each angle remains relatively consistent.
[0026] The total thickness of the first optical adhesive layer 2 and the second optical adhesive layer 3 is 150 to 300 μm, the thickness of the first optical adhesive layer 2 is ≥40 μm and the thickness of the second optical adhesive layer 3 is >0 μm. After repeated experimental tests by the applicant, when the thickness of the first optical adhesive layer 2 and the second optical adhesive layer 3 meet the above-mentioned specific numerical range, the first optical adhesive layer 2 can be easily separated from the glass substrate 1 by the pulling force, and the two optical adhesive layers can be ensured to be separated from the glass substrate 1 together without being separated from each other.
[0027] Specifically, the glass-based circuit board also includes, for example, an ink-colored base black ink layer (not shown) arranged on the substrate surface by laminating, and a carbon black layer (not shown) arranged between the optical film layer 4 and the second optical adhesive layer 3. In this way, by setting the base black ink layer, the ink color of the glass substrate 1 can be adjusted relatively directly, and by setting the carbon black layer, the ink color of the glass substrate 1 can be adjusted relatively indirectly.
[0028] Specifically, the optical film layer 4 uses a polymer film such as PET, PI, PC, etc., and different transmittances of 30 to 90% can be obtained by adding different pigments or pigment mass percentages in the optical film layer 4. The surface of the optical film layer 4 is treated with AG or / and HC and the 60° glossiness is ≤10%. When the surface of the optical film layer 4 is treated with AG or HC, a thermosetting anti-glare layer or a hardness-enhancing layer can be obtained on the side of the optical film layer 4 facing away from the first optical adhesive layer 2. Moreover, when the surface of the optical film layer 4 is treated with AG and HC at the same time, a hardness-enhancing layer and a thermosetting anti-glare layer can be obtained on the optical film layer 4 in sequence, and the thermosetting anti-glare layer is located at the outermost layer. In this way, the surface hardness of the optical film layer 4 can be improved, the surface glossiness can be adjusted, and the glossiness can be controlled.
[0029] As another object of the present invention, in combination with reference 3, the present invention also provides a method for preparing a glass-based circuit board. In the absence of conflict, the preparation method described below is applied to the above glass-based circuit board embodiments, and the relevant repeated contents are not repeated here. The preparation method comprises the following steps:
[0030] S110: Provide a glass substrate 1 on which conductive circuits and a plurality of light-emitting chips 8 are arranged.
[0031] S130: preparing an optical adhesive film, which includes: S131: providing an optical film layer 4 with a transmittance of 30-90%; S133: arranging a first optical adhesive layer 2 including a thermal expansion material on a first side of the optical film layer 4;
[0032] Specifically, the optical film layer 4 is used as a substrate, and the first optical adhesive layer 2 can be arranged on the first side of the optical film layer 4 by directly coating on the first side of the optical film layer 4 or indirectly coating on the second optical adhesive layer 3 (further detailed description will be given below) located on the first side of the optical film layer 4. By using an optical film layer 4 with a transmittance of 30 to 90%, an optical film layer 4 with a suitable transmittance can be selected according to actual needs to adapt to light-emitting chips 8 with different luminous colors or luminous brightness. It is known that there is no sequential relationship between S110 and S130. In addition, in the present invention, the sequence numbers of each step are only an exemplary preparation or maintenance sequence. In the absence of conflict, each step can be selectively combined and the sequence can be adjusted. It can be understood that the first optical adhesive layer 2 can be directly attached to the substrate surface or attached to the bottom black ink layer located on the substrate surface. The thermal expansion material 6 in the first optical adhesive layer 2 can provide an expansion force to reduce the bonding force between the first optical adhesive layer 2 and the glass substrate 1 when the glass substrate 1 is heated, which not only facilitates the separation of the first optical adhesive layer 2 and the optical adhesive film as a whole from the glass substrate 1, but also minimizes the cracks of the glass substrate 1.
[0033] S150: Adhere the first optical adhesive layer 2 of the optical adhesive film to the substrate surface to cover the conductive circuits and multiple light-emitting chips arranged on the substrate surface.
[0034] The glass-based circuit board of the present invention can be obtained by the preparation method of the glass-based circuit board of the present invention, so that the glass-based circuit board directly obtained by the preparation method also has the above-mentioned beneficial technical effects. In addition, the preparation method also has the advantages of strong operability and compact steps.
[0035] Preferably, the preparation method further comprises:
[0036] Step S132 is included between step S131 and step S133. Step S132 includes: coating a second optical adhesive layer 3 on the optical film layer 4;
[0037] In addition, step S132 may have another implementation method, which includes: first coating a carbon black layer on the optical film layer 4, and then coating a second optical adhesive layer on the carbon black layer.
[0038] S133 includes: coating the first optical adhesive layer 2 on the second optical adhesive layer 3, so that the first optical adhesive layer 2 is arranged on the first side of the optical film layer 4;
[0039] Step S130 includes: S135: performing AG treatment or / and HC treatment on the surface of the optical film layer 4;
[0040] Specifically, when the surface of the optical film layer 4 is subjected to AG treatment, a thermosetting anti-glare layer 5 can be coated on the side of the optical film layer 4 facing away from the first optical adhesive layer 2. Therefore, the arrangement of the thermosetting anti-glare layer 5 can change the light direction of the light-emitting chip 8 by, for example, diffuse reflection, thereby achieving an anti-glare effect, avoiding flash points and blooming on the glass-based circuit board, and ensuring the high quality of the glass-based circuit board.
[0041] In addition, the above step S150 may have another implementation, which includes: first coating a bottom black ink layer on the substrate surface, and then attaching the first optical adhesive layer 2 to the bottom black ink layer to cover the conductive circuits and multiple light-emitting chips arranged on the substrate surface.
[0042] As described above, as a further improvement on the preparation method of the glass-based circuit board, corresponding steps are taken to correspondingly obtain at least one of the second optical adhesive layer 3, the carbon black layer, the bottom black ink layer, the thermosetting anti-glare layer and the hardness enhancement layer, so that the prepared glass-based circuit board can obtain the beneficial effects of the corresponding layer. For details, please refer to the above text and will not be repeated here.
[0043] As another object of the present invention, in conjunction with reference Figure 4 The present invention also provides a glass-based circuit board maintenance method. In the absence of conflicts, the maintenance method described below is applied to the glass-based circuit boards of the above glass-based circuit board embodiments and the glass-based circuit boards prepared by the above preparation method embodiments. The repeated contents are not repeated here. Since it is difficult to avoid the glass-based circuit board requiring maintenance due to a faulty light-emitting chip 8, when there is at least one faulty light-emitting chip 8 that cannot work properly among the multiple light-emitting chips 8, the maintenance method includes the following steps:
[0044] S210: heating the glass substrate 1 to expand the heat-expandable material 6 in the first optical adhesive layer 2 of the optical adhesive film until the bonding force between the first optical adhesive layer 2 and the substrate surface is reduced to the point where the two can be relatively peeled off. The specific method of heating the glass substrate 1 may be to heat the packaging surface side, i.e., the light emitting surface side, using a heating platform or an oven;
[0045] S220: peeling the first optical adhesive layer 2 and the optical film layer 4 together from the glass substrate 1;
[0046] S230: taking out the faulty light emitting chip and replacing it with a new light emitting chip 8 by, for example, using SMT technology;
[0047] S240: attaching a new optical adhesive film on the substrate surface;
[0048] It is known that the optical adhesive film in step S240 can refer to the relevant description of the preparation method of the optical adhesive film mentioned above, which will not be repeated here. In addition, the maintenance method of the present invention can also be based on actual needs. After replacing and installing the new light-emitting chip 8, according to the actual needs of display effect, light output intensity, etc., the relevant steps in the above-mentioned preparation method embodiments of the optical adhesive film can be used to obtain an optical adhesive film including a first optical adhesive layer and an optical film layer, and further including at least one of the second optical adhesive layer 3, a carbon black layer, a thermosetting anti-glare layer and a hardness-enhancing layer. Accordingly, regardless of any type of optical adhesive film that the glass-based circuit board has before maintenance, the heat expansion material 6 in the first optical adhesive layer 2 can be expanded by heating the glass substrate 1, so that the bonding force between the first optical adhesive layer 2 and the substrate surface can be reduced to the point that various optical adhesive films can be relatively peeled off relative to the glass substrate, thereby ensuring that the glass-based circuit board is reliably repaired.
[0049] In summary, the glass-based circuit board repair method of the present invention heats the glass substrate 1 to expand the thermal expansion material 6 in the first optical adhesive layer 2 of the optical film layer, so that the bonding force between the first optical adhesive layer 2 and the substrate surface can be reduced to the point where the two can be relatively peeled off, thereby replacing the faulty light-emitting chip 8 with a new light-emitting chip 8 without causing the glass substrate 1 to crack due to stress, thereby achieving the purpose of easily repairing the glass-based circuit board.
[0050] Preferably, heating the glass substrate 1 in step S210 includes: when the thermal expansion material 6 in the first optical adhesive layer 2 is vermiculite, heating is performed at a heating temperature of 150 to 300° C. and a heating time of 10 to 15 minutes; when the thermal expansion material 6 in the first optical adhesive layer 2 is thermal expansion microspheres, heating is performed at a heating temperature of 120 to 180° C. and a heating time of 10 to 15 minutes; when the thermal expansion material 6 in the first optical adhesive layer 2 is a mixture of vermiculite and thermal expansion microspheres, heating is performed at a heating temperature of 150 to 180° C. and a heating time of 10 to 15 minutes. Through repeated experimental tests by the applicant, the above-mentioned numerical range is adopted for the heating temperature and heating time of the heating according to the different thermal expansion materials in the first optical adhesive layer 2. In particular, when the first optical adhesive layer contains both vermiculite and thermal expansion microspheres, 150-300°C and 120-180°C are intersected to obtain 150-180°C, and different suitable temperatures are selected from 150-180°C according to the different proportions of vermiculite and thermal expansion microspheres in the first optical adhesive layer. In addition, the suitable temperature and the specific values of the above-mentioned heating temperatures and heating times can be obtained based on the numerical range obtained by the present invention and experimental means known to those skilled in the art. Therefore, when the corresponding heating temperature and heating time are adopted, the glass substrate 1 can be prevented from being overheated and damaged, and it can also ensure that substantially all the thermal expansion materials 6 in the first optical adhesive layer 2 are expanded, thereby sufficiently reducing the bonding force between the first optical adhesive layer 2 and the substrate surface or / and the bottom black ink layer coated on the substrate surface, thereby facilitating their relative peeling.
[0051] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein by equivalents. These modifications or replacements do not make the essence of the corresponding technical solutions deviate from the scope of the technical solutions of the embodiments of the present invention. Any modifications, equivalent replacements and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A glass-based circuit board, characterized in that: include: A glass substrate, comprising a substrate surface, on which a conductive circuit and a plurality of light-emitting chips are arranged; An optical adhesive film, comprising a stacked first optical adhesive layer and an optical film layer, wherein the first optical adhesive layer comprises a heat-expandable material, the optical film layer has a transmittance of 30 to 90%, and the heat-expandable material in the first optical adhesive layer can expand by heating the glass substrate, thereby reducing the bonding force between the first optical adhesive layer and the substrate surface to the point where the two can be relatively peeled off; The optical adhesive film is adhered to the substrate surface through the first optical adhesive layer.
2. The glass-based circuit board according to claim 1, characterized in that: The thermal expansion material includes at least one of vermiculite and thermal expansion microspheres. The first optical adhesive layer uses acrylic optical adhesive as a substrate. Vermiculite and / or thermal expansion microspheres are mixed inside the acrylic optical adhesive. The diameter of the vermiculite is set to 20 to 100 μm, and the diameter of the thermal expansion microspheres is set to 20 to 40 μm. The shell of the thermal expansion microspheres is thermoplastic plastic and alkane gas is sealed inside.
3. The glass-based circuit board according to claim 1, characterized in that: The optical adhesive film also includes a second optical adhesive layer arranged between the first optical adhesive layer and the optical film layer. The second optical adhesive layer uses acrylic optical adhesive as a base material, and inorganic or organic diffusion powder is mixed inside the acrylic optical adhesive. The mass percentage of the diffusion powder in the acrylic optical adhesive is 5 to 20wt%, and the particle size of the diffusion powder is 1.5 to 3μm.
4. The glass-based circuit board according to claim 3, characterized in that: The total thickness of the first optical adhesive layer and the second optical adhesive layer is 150-300 μm, the thickness of the first optical adhesive layer is ≥40 μm, and the thickness of the second optical adhesive layer is >0 μm.
5. The glass-based circuit board according to claim 3, characterized in that: The glass-based circuit board also includes a bottom black ink layer arranged on the substrate surface and a carbon black layer arranged between the optical film layer and the second optical adhesive layer, and the first optical adhesive layer is attached to the bottom black ink layer.
6. The glass-based circuit board according to claim 1, characterized in that: The optical film layer is made of a polymer film, and the surface of the optical film layer is treated with AG or / and HC and has a glossiness of ≤10% at 60°.
7. A method for preparing a glass-based circuit board, applied to the glass-based circuit board according to any one of claims 1 to 6, characterized in that: The steps include: S110: providing a glass substrate on which a conductive circuit and a plurality of light-emitting chips are arranged; S130: preparing an optical adhesive film, which includes: S131: providing an optical film layer with a transmittance of 30-90%; S133: arranging a first optical adhesive layer including a thermal expansion material on a first side of the optical film layer; S150: Adhere the first optical adhesive layer of the optical adhesive film to the substrate surface to cover the conductive circuits and the plurality of light-emitting chips arranged on the substrate surface.
8. The method for preparing a glass-based circuit board according to claim 7, characterized in that: Step S132 is included between step S131 and step S133, and step S132 includes: coating a second optical adhesive layer on the optical film layer; The S133 includes: coating the first optical adhesive layer on the second optical adhesive layer, so that the first optical adhesive layer is arranged on the first side of the optical film layer; The step S130 further includes: S135: performing AG treatment and / or HC treatment on the surface of the optical film layer.
9. A method for repairing a glass-based circuit board, applied to the glass-based circuit board according to any one of claims 1 to 6, characterized in that: There is at least one faulty light-emitting chip that cannot work normally among the plurality of light-emitting chips, and the repair method comprises: S210: heating the glass substrate to cause the heat-expandable material in the first optical adhesive layer of the optical adhesive film to expand due to the heat until the bonding force between the first optical adhesive layer and the substrate surface is reduced so that the two can be relatively peeled off; S220: peeling the first optical adhesive layer and the optical film layer together from the glass substrate; S230: removing the faulty light emitting chip and replacing it with a new light emitting chip; S240: Paste the new optical adhesive film on the substrate surface.
10. The glass-based circuit board repair method according to claim 9, characterized in that: The heating of the glass substrate in step S210 includes: when the thermal expansion material in the first optical adhesive layer is vermiculite, heating is performed at a heating temperature of 150 to 300° C. and a heating time of 10 to 15 minutes; when the thermal expansion material in the first optical adhesive layer is thermal expansion microspheres, heating is performed at a heating temperature of 120 to 180° C. and a heating time of 10 to 15 minutes; when the thermal expansion material in the first optical adhesive layer is a mixture of vermiculite and thermal expansion microspheres, heating is performed at a heating temperature of 150 to 180° C. and a heating time of 10 to 15 minutes.
Citation Information
Patent Citations
Packaging structure and packaging method, electronic device and packaging film recovery method
CN109686854A